A Raman spectroscopy detection method based on colloidal silver gradient aggregation effect

By introducing a coagulation agent into the silver nanoparticle sol to form a layered interface, the problem of insufficient detection signals in the existing technology is solved, high-sensitivity Raman spectrum detection is achieved, the process is simplified and the cost is reduced.

CN115184334BActive Publication Date: 2024-10-25XI AN JIAOTONG UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210797173.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-07-08
Publication Date
2024-10-25
Estimated Expiration
2042-07-08

AI Technical Summary

Technical Problem

Existing Raman spectroscopy detection technology is difficult to achieve high-sensitivity detection, especially under the influence of the selection and addition amount of coagulation agent on the detection results, which leads to the aggregation of nanoparticles to reduce molecular adsorption sites and reduce the detection signal.

Method used

Add a coagulation agent to the silver nanoparticle sol so that it naturally aggregates to form a layered interface. Use a portable Raman spectrometer to detect the interface to avoid mixing the coagulation agent with the liquid to be tested and ensure that the silver particles are partially aggregated and dispersed. , improve the detection signal.

Benefits of technology

This method significantly improves the detection sensitivity of molecules, simplifies the process, reduces costs, shortens detection time, and improves detection repeatability and accuracy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115184334B_ABST
    Figure CN115184334B_ABST
Patent Text Reader

Abstract

The present invention discloses a Raman spectrum detection method based on the gradient aggregation effect of colloidal silver, comprising the following steps: (1) synthesizing enhanced reagent silver nanoparticles, using sodium citrate as a reducing agent, and synthesizing silver nanoparticles by reducing silver nitrate. (2) preparing standard samples of molecules to be tested of different concentrations as test solutions; putting an appropriate amount of silver nanoparticles and the test solution into a sample detection pool and mixing them evenly, then adding a small amount of coagulant, keeping the sample pool still to avoid the coagulant mixing evenly in the sol, so that the lower layer of the sol naturally agglomerates while the upper layer remains in a dispersed state, the sample presents a stratified phenomenon, and produces an obvious interface; (3) using a Raman spectrometer, aiming the laser at the interface of the sol stratification for detection, and obtaining the Raman spectrum of the molecules to be tested. The method has excellent detection capabilities for molecules such as crystal violet, methylene blue, diquat, etc., and has the advantages of being simple, rapid, highly sensitive, and low cost.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of Raman spectroscopy technology detection, and in particular relates to a Raman spectroscopy detection method based on the gradient aggregation effect of colloidal silver. Background Art

[0002] Aromatic dye molecules such as crystal violet, rhodamine 6G, methylene blue, malachite green, etc. are a class of organic pollutants present in the environment. They have a wide range of applications and can be used as dyes in textiles. In addition, they are also favored in the aquaculture industry because of their bactericidal and antibacterial effects. However, when these dyes enter the body, they will produce harmful hidden dye molecules, such as hidden crystal violet and hidden malachite green, which are serious pollutants in water bodies and have high residues, high carcinogenicity, and high toxicity. In addition, in order to meet the needs of agricultural production, a large amount of pesticides are used in production activities, which brings serious harm to the environment and humans. Realizing rapid, real-time, and highly sensitive detection of different molecules such as pesticide residues, dyes, and drugs is very important for environmental pollution monitoring, aquatic food safety, and human health.

[0003] Surface enhanced Raman spectroscopy (SERS) is a molecular detection technology with excellent characteristics such as non-destructive detection, convenience, and fingerprint recognition. Using gold and silver nanoparticle colloids as an enhanced substrate to perform Raman detection on molecules is a convenient and fast method. However, in actual detection, it is difficult to achieve highly sensitive SERS detection. At present, the coagulation method for Raman detection mainly adds the enhanced substrate, the test liquid and the coagulation agent into the sample pool, mixes them and then performs detection. The type selection and amount of coagulation agent added will have a great impact on the detection results. Excessive coagulation agent addition will cause a large number of nanoparticles to aggregate, which will not only produce competitive adsorption of the molecules to be tested, but also reduce the molecular adsorption sites due to excessive aggregation, so that good detection sensitivity cannot be obtained. Therefore, it is crucial to detect the molecules to be tested under the optimal aggregation conditions to obtain the best signal. Developing new detection methods in the system of Raman detection by sol method is of great significance to improving the detection ability of molecules. Summary of the invention

[0004] The purpose of the present invention is to provide a method for adding a coagulation agent to a silver nanoparticle sol, causing the silver particles to aggregate in a gradient along the distribution of the coagulation agent without mixing, causing the solution to be stratified after the silver particles are naturally coagulated, and obtaining a highly sensitive Raman spectroscopy detection method based on the gradient aggregation effect of colloidal silver by detecting at the stratification interface.

[0005] A method in which a coagulation agent is added to a mixed solution of silver nanoparticles and a test liquid to partially aggregate and stratify the silver particles, and the molecules to be tested are detected at the stratification interface.

[0006] To achieve the above object, the technical solution of the present invention is as follows:

[0007] Step 1, preparation of silver nanoparticle sol

[0008] Add 75 mL of ultrapure water and 10-30 mL of sodium citrate with a mass fraction of 1-2% into a conical flask, stir and heat to 70° C., then add 1.5-2.5 mL of silver nitrate with a mass fraction of 1% and 2 mL of sodium borohydride with a mass fraction of 0.1-1%, and continue to stir evenly to obtain a seed solution of silver nanoparticles;

[0009] The second step growth of silver nanoparticles: 2 mL of 1-2% sodium citrate is added to 75 mL of ultrapure water, stirred and heated to 110° C., and then 10-20 mL of seed solution and 1.5-2.5 mL of 1% silver nitrate are added, and after fully stirring, 2 mL of 1-2% sodium citrate and 1.5-2.5 mL of 1% silver nitrate solution are added and the reaction is continued for 30 minutes to obtain silver nanoparticles grown in the second step;

[0010] 2 mL of 1-2% sodium citrate was added to 80 mL of ultrapure water, and the mixture was heated to 110° C. with stirring, and then 10-20 mL of the silver nanoparticles grown in the second step and 1.5-2.5 mL of 1% silver nitrate were added, and the reaction was continued for 30 minutes to obtain a silver nanoparticle sol;

[0011] Step 2, prepare standard solutions of the molecules to be tested with different concentrations as test solutions:

[0012] Take 250-500uL of silver nanoparticle sol and 1-2mL of the standard solution of the molecule to be tested, add them into the detection cell and mix them evenly, then add 25-100uL of a coagulant solution with a concentration of 1-1.5mol / L, keep the sample cell still to prevent the coagulant from mixing in the solution, so that the lower layer of the sol naturally agglomerates while the upper layer remains dispersed, the sample shows a stratified phenomenon, and a clear interface is produced. Use a portable Raman spectrometer to detect at the stratified interface of the sample to obtain the final test result.

[0013] The coagulation agent is sodium chloride, sodium bromide, sodium iodide or magnesium sulfate, potassium chloride, potassium bromide, potassium iodide, magnesium chloride, magnesium bromide, magnesium iodide, calcium chloride, calcium bromide, and aluminum sulfate.

[0014] The amount of silver nanoparticle sol added in step 2 is 500uL.

[0015] In step 2, the amount of the standard solution of the molecule to be tested added is 2 mL.

[0016] The amount of the coagulation agent added in step 2 is 100uL.

[0017] The concentration of the coagulant in step 2 is 1.5 mol / L.

[0018] Compared with the prior art, the present invention has the following beneficial effects:

[0019] The present invention first adds silver nanoparticle sol and a standard solution of a molecule to be tested into a sample pool and mixes them, then adds a small amount of coagulation agent, and keeps the sample pool still to prevent the coagulation agent from mixing with the silver colloid and the solution to be tested. The coagulation agent naturally sinks to the bottom of the sample pool, causing the silver particles at the bottom to aggregate and darken in color; while the silver particles at the top remain dispersed and present the original light yellow color. Therefore, the silver particles in the sample pool are partially aggregated, and the lower aggregated area and the upper non-aggregated area present an obvious interface due to different colors. The sample is detected by a portable Raman detector, and detection signals of different intensities are obtained at different positions of the sample detection pool. When the laser is aligned at the interface of the sol stratification, the best detection signal can be obtained. Compared with adding a large amount of coagulation agent to cause the solution to aggregate as a whole, the detection sensitivity of the molecule is increased. The obvious interface generated is conducive to locating the best detection position for detection. The method has simple process, low cost, short time consumption, high repeatability, and greatly improves the sensitivity of molecular detection. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 Optical photographs of silver sol precipitating after adding different amounts of coagulation agent into a mixed solution of silver nanoparticle sol and a molecule to be tested;

[0021] Figure 2 a is a schematic diagram of Raman detection when 100uL of sodium chloride is added to a mixed solution of silver nanoparticle sol and the molecule to be detected;

[0022] Figure 2 b is the Raman spectrum detected by focusing the laser at different positions of the solution when 100uL of sodium chloride is added to the mixed solution of silver nanoparticle sol and crystal violet;

[0023] Figure 3 The Raman spectra of the mixed solution of silver nanoparticle sol and crystal violet molecules were detected when different volumes of sodium chloride were added;

[0024] Figure 4 The Raman spectra of the mixed solution of silver nanoparticle sol and crystal violet of different concentrations were detected when 100uL of sodium chloride was added;

[0025] Figure 5 The Raman spectra of the mixed solution of silver nanoparticle sol and crystal violet of different concentrations were detected when 100uL sodium iodide was added;

[0026] Figure 6 The Raman spectra of the mixed solution of silver nanoparticle sol and crystal violet of different concentrations were detected when 100uL sodium bromide was added;

[0027] Figure 7 The Raman spectra of the mixed solution of silver nanoparticle sol and crystal violet of different concentrations were detected when 100uL magnesium sulfate was added;

[0028] Figure 8 The Raman spectra of mixed solutions of silver nanoparticle sol and different concentrations of rhodamine 6G were detected when 100uL of sodium chloride was added;

[0029] Fig. 9 The Raman spectra of the mixed solution of silver nanoparticle sol and methylene blue of different concentrations were detected when 100uL of sodium chloride was added;

[0030] Fig.10 This is the Raman spectrum detected when 100uL of sodium chloride was added to a mixed solution of silver nanoparticle sol and malachite green of different concentrations.

[0031] Fig.11 The Raman spectra were detected when 100uL of sodium chloride was added to the mixed solution of silver nanoparticle sol and diquat of different concentrations.

[0032] Fig.12 This is the Raman spectrum detected when 100uL of sodium chloride was added to the mixed solution of silver nanoparticle sol and different concentrations of thiabendazole. DETAILED DESCRIPTION

[0033] The present invention is further described in detail below with reference to the accompanying drawings and embodiments.

[0034] Preparation of silver nanoparticle sol

[0035] Add 75 mL of ultrapure water and 10-30 mL of sodium citrate with a mass fraction of 1-2% into a conical flask, stir and heat to 70° C., then add 1.5-2.5 mL of silver nitrate with a mass fraction of 1% and 2 mL of sodium borohydride with a mass fraction of 0.1-1%, and continue to stir evenly to obtain a seed solution of silver nanoparticles;

[0036] The second step growth of silver nanoparticles: 2 mL of 1-2% sodium citrate is added to 75 mL of ultrapure water, stirred and heated to 110° C., and then 10-20 mL of seed solution and 1.5-2.5 mL of 1% silver nitrate are added, and after fully stirring, 2 mL of 1-2% sodium citrate and 1.5-2.5 mL of 1% silver nitrate solution are added and the reaction is continued for 30 minutes to obtain silver nanoparticles grown in the second step;

[0037] 2 mL of 1-2% sodium citrate was added to 80 mL of ultrapure water, and the mixture was heated to 110° C. with stirring. Then, 10-20 mL of the silver nanoparticles grown in the second step and 1.5-2.5 mL of 1% silver nitrate were added. The reaction was continued for 30 minutes to obtain a silver nanoparticle sol.

[0038] Figure 1 These are optical photographs of silver nanoparticle sol in the sample pool after different volumes of coagulants were induced to aggregate. After adding silver nanoparticle sol and the sample to be tested into the sample pool and mixing them evenly, after adding the coagulant, the solution was kept still so that the coagulant would not mix with the sample solution and coagulation would occur naturally. When the amount of coagulant added exceeded 100uL, all the sol in the sample pool aggregated and the overall color of the sol darkened. When the amount of coagulant added did not exceed 100uL, only the lower part of the sol aggregated. The color of the aggregated part darkened and formed a clear interface with the non-aggregated part.

[0039] Figure 2 a is a schematic diagram of Raman detection after adding 100uL of coagulation agent to the mixed solution of silver nanoparticle sol and test liquid. The laser is aimed at the layered interface for detection.

[0040] Embodiment 1:

[0041] Step 1, preparation of silver nanoparticle sol

[0042] Add 75 mL of ultrapure water and 20 mL of 1% sodium citrate in a conical flask, stir and heat to 70°C, then add 1.7 mL of 1% silver nitrate and 2 mL of 1% sodium borohydride, continue stirring to obtain a silver nanoparticle seed solution;

[0043] The second growth of silver nanoparticles: 2 mL of 1% sodium citrate was added to 75 mL of ultrapure water, stirred and heated to 110° C., and then 10 mL of seed solution and 1.7 mL of 1% silver nitrate were added. After fully stirring, 2 mL of 1% sodium citrate and 1.7 mL of 1% silver nitrate solution were added and the reaction was continued for 30 minutes to obtain silver nanoparticles grown in the second step.

[0044] 2 mL of 1% sodium citrate was added to 80 mL of ultrapure water, and the mixture was heated to 110° C. with stirring, and then 10 mL of the silver nanoparticles grown in the second step and 1.7 mL of 1% silver nitrate were added, and the reaction was continued for 30 minutes to obtain a silver nanoparticle sol;

[0045] Step 2, prepare standard solutions of the molecules to be tested with different concentrations as test solutions:

[0046] Prepare a 0.01 mol / L crystal violet standard solution and dilute it to obtain 10 -8 mol / L standard test solution. Take 500uL of silver nanoparticle sol and 2mL of standard test solution and add them to the detection cell to mix well. Then add 100uL of 1.5mol / L coagulation agent sodium chloride. Do not mix the sample. Keep the sample cell still to allow the sol to aggregate naturally. The lower part of the sol aggregates and forms a clear interface with the unaggregated part of the upper layer. The laser is focused on different positions of the solution, starting from the bottom and moving upwards, and detection is performed every 1mm. The Raman spectrometer power is 300mW, the laser wavelength is 785nm, and the integration time is 20s.

[0047] In Example 1, after adding 100uL of sodium chloride to the sample to produce stratification, the Raman spectra detected at different positions of the solution are as follows: Figure 2 As shown in b, when the laser is focused at the interface, the optimal detection signal is obtained.

[0048] Example 2

[0049] Step 1, preparation of silver nanoparticle sol

[0050] Add 75 mL of ultrapure water and 10 mL of 2% sodium citrate in a conical flask, stir and heat to 70°C, then add 1.5 mL of 1% silver nitrate and 2 mL of 0.5% sodium borohydride, and continue to stir to obtain a seed solution of silver nanoparticles;

[0051] The second growth of silver nanoparticles: 2 mL of 2% sodium citrate was added to 75 mL of ultrapure water, stirred and heated to 110° C., and then 15 mL of seed solution and 1.5 mL of 1% silver nitrate were added. After fully stirring, 2 mL of 2% sodium citrate and 1.5 mL of 1% silver nitrate solution were added and the reaction was continued for 30 minutes to obtain silver nanoparticles grown in the second step.

[0052] 2 mL of 2% sodium citrate was added to 80 mL of ultrapure water, and the mixture was heated to 110° C. with stirring, and then 15 mL of the silver nanoparticles grown in the second step and 1.5 mL of 1% silver nitrate were added, and the reaction was continued for 30 minutes to obtain a silver nanoparticle sol;

[0053] Step 2, prepare standard solutions of the molecules to be tested with different concentrations as test solutions:

[0054] Prepare a 0.01 mol / L crystal violet standard solution and dilute the solution to obtain 10 -7 mol / L-10 -16mol / L standard test solution. Take 500uL of silver nanoparticle colloid and put it into the sample detection pool, add 2mL of 10 -8 mol / L crystal violet test solution was mixed. Then 500uL, 400uL, 300uL, 200uL, 100uL, 75uL, 50uL, and 25uL of 1.5mol / L sodium chloride solution were added respectively, without mixing the sample, so that the sol was naturally aggregated. When the volume of sodium chloride exceeded 100uL, the silver nanoparticles aggregated as a whole, and the color turned dark gray. The solution was detected using a portable Raman spectrometer; when the volume of sodium chloride did not exceed 100uL, the lower part of the sol aggregated, and a clear interface was formed with the unaggregated part of the upper layer. The laser was focused on the interface for detection. The power of the Raman spectrometer was 300mW, the laser wavelength was 785nm, and the integration time was 20s.

[0055] In Example 2, the Raman spectra of the samples detected when different volumes of sodium chloride were added are as follows: Figure 3 As shown, when the volume of the coagulation agent is 100uL, the optimal detection signal is obtained.

[0056] Example 3

[0057] Step 1, preparation of silver nanoparticle sol

[0058] Add 75 mL of ultrapure water and 15 mL of 1.5% sodium citrate in a conical flask, stir and heat to 70° C., then add 2.3 mL of 1% silver nitrate and 2 mL of 0.8% sodium borohydride, and continue to stir to obtain a seed solution of silver nanoparticles;

[0059] The second growth of silver nanoparticles: 2 mL of 1.5% sodium citrate was added to 75 mL of ultrapure water, stirred and heated to 110° C., and then 13 mL of seed solution and 2.3 mL of 1% silver nitrate were added. After fully stirring, 2 mL of 1.5% sodium citrate and 2.3 mL of 1% silver nitrate solution were added and the reaction was continued for 30 minutes to obtain silver nanoparticles grown in the second step.

[0060] 2 mL of 1.5% sodium citrate was added to 80 mL of ultrapure water, and the mixture was heated to 110° C. with stirring, and then 13 mL of the silver nanoparticles grown in the second step and 2.3 mL of 1% silver nitrate were added, and the reaction was continued for 30 minutes to obtain a silver nanoparticle sol;

[0061] Step 2, prepare standard solutions of the molecules to be tested with different concentrations as test solutions:

[0062] Prepare a 0.01 mol / L crystal violet standard solution and dilute the solution to obtain 10-8 mol / L-10 -16 mol / L standard test solution. Take 500uL of silver nanoparticle sol and put it into the sample detection cell, add 2mL of crystal violet test solution of different concentrations and mix well. Then add 100uL of 1.5mol / L sodium chloride solution as a coagulant. The lower part of the sol aggregates and forms a clear interface with the unaggregated part of the upper layer. The laser is focused on the interface of the layers for detection. The Raman spectrometer power is 300mW, the laser wavelength is 785nm, and the integration time is 20s.

[0063] After adding 100uL of sodium chloride to the samples of different concentrations in Example 3, the Raman spectra detected at the interface where the sol is delaminated are as follows: Figure 4 As shown, in this embodiment, 10 -15 mol / L crystal violet signal.

[0064] Example 4

[0065] Step 1, preparation of silver nanoparticle sol

[0066] Add 75 mL of ultrapure water and 25 mL of 1.8% sodium citrate in a conical flask, stir and heat at 70°C, then add 2.5 mL of 1% silver nitrate and 2 mL of 0.6% sodium borohydride, and continue to stir to obtain a silver nanoparticle seed solution;

[0067] The second growth of silver nanoparticles: 2 mL of 1.8% sodium citrate was added to 75 mL of ultrapure water, stirred and heated to 110° C., and then 18 mL of seed solution and 2.5 mL of 1% silver nitrate were added. After fully stirring, 2 mL of 1.8% sodium citrate and 2.5 mL of 1% silver nitrate solution were added and the reaction was continued for 30 minutes to obtain silver nanoparticles grown in the second step.

[0068] 2 mL of 1.8% sodium citrate was added to 80 mL of ultrapure water, and the mixture was heated to 110° C. with stirring, and then 18 mL of the silver nanoparticles grown in the second step and 2.5 mL of 1% silver nitrate were added, and the reaction was continued for 30 minutes to obtain a silver nanoparticle sol;

[0069] Step 2, prepare standard solutions of the molecules to be tested with different concentrations as test solutions:

[0070] Prepare a 0.01 mol / L crystal violet standard solution and dilute the solution to obtain 10 -8 mol / L-10 -16mol / L standard test solution. Take 500uL of silver nanoparticle sol and put it into the sample detection cell, add 2mL of crystal violet test solution of different concentrations and mix well. Then add 100uL of 1.5mol / L sodium iodide solution as a coagulant. The lower part of the sol aggregates and forms a clear interface with the unaggregated part of the upper layer. The laser is focused on the interface of the layers for detection. The Raman spectrometer power is 300mW, the laser wavelength is 785nm, and the integration time is 20s.

[0071] After adding 100uL of sodium iodide to the samples of different concentrations in Example 4, the Raman spectra detected at the interface where the sol is delaminated are as follows: Figure 5 As shown, in this embodiment, 10 -13 mol / L crystal violet signal.

[0072] Embodiment 5:

[0073] Step 1, preparation of silver nanoparticle sol

[0074] Add 75 mL of ultrapure water and 30 mL of 1.3% sodium citrate in a conical flask, stir and heat to 70°C, then add 2 mL of 1% silver nitrate and 2 mL of 0.1% sodium borohydride, and continue to stir to obtain a silver nanoparticle seed solution;

[0075] The second growth of silver nanoparticles: 2 mL of 1.3% sodium citrate was added to 75 mL of ultrapure water, stirred and heated to 110° C., and then 20 mL of seed solution and 2 mL of 1% silver nitrate were added. After fully stirring, 2 mL of 1.3% sodium citrate and 2 mL of 1% silver nitrate solution were added and the reaction was continued for 30 minutes to obtain silver nanoparticles grown in the second step.

[0076] 2 mL of 1.3% sodium citrate was added to 80 mL of ultrapure water, and the mixture was stirred and heated to 110° C., and then 20 mL of the silver nanoparticles grown in the second step and 2 mL of 1% silver nitrate were added, and the reaction was continued for 30 minutes to obtain a silver nanoparticle sol;

[0077] Prepare a 0.01 mol / L crystal violet standard solution and dilute the solution to obtain 10 -8 mol / L-10 -16mol / L standard test solution. Take 400uL of silver nanoparticle sol and put it into the sample detection cell, add 1.8mL of crystal violet test solution of different concentrations and mix well. Then add 100uL of 1mol / L sodium bromide solution as a coagulation agent. The lower part of the sol aggregates and forms a clear interface with the unaggregated part of the upper layer. The laser is focused on the interface of the stratification for detection. The Raman spectrometer power is 300mW, the laser wavelength is 785nm, and the integration time is 20s.

[0078] After adding 100uL of sodium bromide to the samples of different concentrations in Example 5, the Raman spectra detected at the interface where the sol is delaminated are as follows: Figure 6 As shown, in this embodiment, 10 -15 mol / L crystal violet signal.

[0079] Example 6

[0080] Step 1, preparing silver nanoparticle sol, the same as in Example 1;

[0081] Prepare a 0.01 mol / L crystal violet standard solution and dilute the solution to obtain 10 -8 mol / L-10 -16 mol / L standard test solution. Take 500uL of silver nanoparticle sol and put it into the sample detection cell, add 2mL of crystal violet test solution of different concentrations and mix well. Then add 100uL of 1.5mol / L coagulation agent magnesium sulfate solution. The lower part of the sol aggregates and forms a clear interface with the unaggregated part of the upper layer. The laser is focused on the interface of the stratification for detection. The Raman spectrometer power is 300mW, the laser wavelength is 785nm, and the integration time is 20s.

[0082] After adding 100uL of magnesium sulfate to the samples of different concentrations in Example 6, the Raman spectra detected at the interface where the sol is stratified are as follows: Figure 7 As shown, in this embodiment, 10 -15 mol / L crystal violet signal.

[0083] Example 7

[0084] Step 1, preparing silver nanoparticle sol, the same as in Example 1;

[0085] Prepare 0.01 mol / L Rhodamine 6G standard solution, dilute the solution to obtain 10 -8 mol / L-10 -16mol / L standard test solution. Take 500uL of silver nanoparticle sol and put it into the sample detection cell, add 2mL of rhodamine 6G test solution of different concentrations and mix them. Then add 100uL of 1.5mol / L sodium chloride solution as a coagulant. The lower part of the sol aggregates and forms a clear interface with the unaggregated part of the upper layer. The laser is focused on the interface of the layers for detection. The Raman spectrometer power is 300mW, the laser wavelength is 785nm, and the integration time is 20s.

[0086] After adding 100uL of sodium chloride to the samples of different concentrations in Example 7, the Raman spectra detected at the interface where the sol is delaminated are as follows: Figure 8 As shown, in this embodiment, 10 -14 mol / L of Rhodamine 6G signal.

[0087] Example 8

[0088] Step 1, preparing silver nanoparticle sol, the same as in Example 1;

[0089] Prepare a 0.01 mol / L methylene blue standard solution and dilute the solution to obtain 10 -8 mol / L-10 -16 mol / L standard test solution. Take 500uL of silver nanoparticle sol and put it into the sample detection cell, add 2mL of methylene blue test solution of different concentrations and mix well. Then add 100uL of 1.5mol / L sodium chloride solution as a coagulant. The lower part of the sol aggregates and forms a clear interface with the unaggregated part of the upper layer. The laser is focused on the interface of the layers for detection. The Raman spectrometer power is 300mW, the laser wavelength is 785nm, and the integration time is 20s.

[0090] After adding 100uL of sodium chloride to the samples of different concentrations in Example 8, the Raman spectra detected at the interface where the sol is stratified are as follows: Fig. 9 As shown, in this embodiment, 10 -15 mol / L methylene blue signal.

[0091] Example 9

[0092] Step 1, preparing silver nanoparticle sol, the same as in Example 1;

[0093] Prepare a 0.01 mol / L malachite green standard solution and dilute the solution to obtain 10 -8 mol / L-10 -16mol / L standard test solution. Take 500uL of silver nanoparticle sol and put it into the sample detection cell, add 2mL of malachite green test solution of different concentrations and mix well. Then add 100uL of 1.5mol / L sodium chloride solution as a coagulant. The lower part of the sol aggregates and forms a clear interface with the unaggregated part of the upper layer. The laser is focused on the interface of the layers for detection. The Raman spectrometer power is 300mW, the laser wavelength is 785nm, and the integration time is 20s.

[0094] After adding 100uL of sodium chloride to the samples of different concentrations in Example 9, the Raman spectra detected at the interface where the sol is delaminated are as follows: Fig.10 As shown, in this embodiment, 10 -14 mol / L of malachite green signal.

[0095] Example 10

[0096] Step 1, preparing silver nanoparticle sol, the same as in Example 1;

[0097] Prepare a 0.01 mol / L diquat standard solution and dilute the solution to obtain 10 -8 mol / L-10 -13 mol / L standard test solution. Take 500uL of silver nanoparticle sol and put it into the sample detection cell, add 2mL of diquat test solution of different concentrations and mix well. Then add 100uL of 1.5mol / L sodium chloride solution as a coagulant. The lower part of the sol aggregates and forms a clear interface with the unaggregated part of the upper layer. The laser is focused on the interface of the stratification for detection. The Raman spectrometer power is 300mW, the laser wavelength is 785nm, and the integration time is 20s.

[0098] After adding 100uL of sodium chloride to the samples of different concentrations in Example 10, the Raman spectra detected at the interface where the sol is delaminated are as follows: Fig.11 As shown, in this embodiment, 10 -12 mol / L of diquat signal.

[0099] Embodiment 11

[0100] Step 1, preparing silver nanoparticle sol, the same as in Example 1;

[0101] Prepare a 0.01 mol / L thiabendazole standard solution and dilute the solution to obtain 10 -8 mol / L-10 -12mol / L standard test solution. Take 500uL of silver nanoparticle sol and put it into the sample detection cell, add 2mL of different concentrations of thioconazole test solution and mix well. Then add 100uL of 1.5mol / L sodium chloride solution as a coagulant. The lower part of the sol aggregates and forms a clear interface with the unaggregated part of the upper layer. The laser is focused on the interface of the stratification for detection. The Raman spectrometer power is 300mW, the laser wavelength is 785nm, and the integration time is 20s.

[0102] After adding 100uL of sodium chloride to the samples of different concentrations in Example 11, the Raman spectra detected at the interface where the sol is delaminated are as follows: Fig.12 As shown, in this embodiment, 10 -11 mol / L thiabendazole signal.

Claims

1. A Raman spectroscopy detection method based on colloidal silver gradient aggregation effect, characterized in that: The following steps are involved: Step 1, preparation of silver nanoparticle sol Add 75 mL of ultrapure water and 10-30 mL of sodium citrate with a mass fraction of 1-2% into a conical flask, stir and heat to 70° C., then add 1.5-2.5 mL of silver nitrate with a mass fraction of 1% and 2 mL of sodium borohydride with a mass fraction of 0.1-1%, and continue to stir evenly to obtain a seed solution of silver nanoparticles; The second step growth of silver nanoparticles: 2 mL of 1-2% sodium citrate is added to 75 mL of ultrapure water, stirred and heated to 110° C., and then 10-20 mL of seed solution and 1.5-2.5 mL of 1% silver nitrate are added, and after fully stirring, 2 mL of 1-2% sodium citrate and 1.5-2.5 mL of 1% silver nitrate solution are added and the reaction is continued for 30 minutes to obtain silver nanoparticles grown in the second step; 2 mL of 1-2% sodium citrate was added to 80 mL of ultrapure water, and the mixture was heated to 110° C. with stirring, and then 10-20 mL of the silver nanoparticles grown in the second step and 1.5-2.5 mL of 1% silver nitrate were added, and the reaction was continued for 30 minutes to obtain a silver nanoparticle sol; Step 2, prepare standard solutions of the molecules to be tested with different concentrations as test solutions: Take 250-500uL of silver nanoparticle sol and 1-2mL of the standard solution of the molecule to be tested, add them into the detection cell and mix them evenly, then add 25-100uL of a coagulant solution with a concentration of 1-1.5mol / L, keep the sample cell still to prevent the coagulant from mixing in the solution, so that the lower layer of the sol naturally agglomerates while the upper layer remains dispersed, the sample shows a stratified phenomenon, and a clear interface is produced. Use a portable Raman spectrometer to detect at the stratified interface of the sample to obtain the final test result.

2. The Raman spectroscopy detection method based on colloidal silver gradient aggregation effect according to claim 1, characterized in that: The coagulation agent is sodium chloride, sodium bromide, sodium iodide, magnesium sulfate, potassium chloride, potassium bromide, potassium iodide, magnesium chloride, magnesium bromide, magnesium iodide, calcium chloride, calcium bromide, and aluminum sulfate.

3. The Raman spectroscopy detection method based on colloidal silver gradient aggregation effect according to claim 1, characterized in that: The amount of silver nanoparticle sol added in step 2 is 500uL.

4. The Raman spectroscopy detection method based on colloidal silver gradient aggregation effect according to claim 1, characterized in that: In step 2, the amount of the standard solution of the molecule to be tested added is 2 mL.

5. The Raman spectroscopy detection method based on colloidal silver gradient aggregation effect according to claim 1, characterized in that: The amount of the coagulation agent added in step 2 is 100uL.