A foam slag improvement method suitable for shield construction in fine sand strata
By injecting water and foam liquid into the shield soil silo, and adjusting the injection of foam liquid according to the consistency and collapse of the residue, the difficulty of unearthing and cutting blade wear in the shield construction in the fine sand formation was solved, and the problem of cutting wheel wear was improved. Construction efficiency and soil stability.
Patent Information
- Application Number
- CN202210863966.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-07-21
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2042-07-21
AI Technical Summary
In fine sand formations, due to large internal friction angle and poor fluid plasticity during construction, it leads to difficulty in unearthing, severe wear of the cutter tool, and causes great disturbance to the soil. The existing slag improvement technology is mainly concentrated in sand There is a lack of research on fine sand formations in pebbles and clay formations.
By using the foam slag improvement method, by injecting water into the shield silo and adding foam liquid, adjusting the injection ratio of the foam liquid according to the consistency and slump value of the slag, monitoring the slag status to meet the preset parameters, and improving the slag Soil fluid plasticity and stability.
It effectively solved the problem of difficulty in unearthing of shield structures in fine sand formations and serious wear of cutter cutting tools in fine sand formations, improved the excavation speed and construction efficiency, and reduced disturbance to the soil.
Smart Images

Figure CN115247562B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of shield construction, and in particular to a foam slag improvement method suitable for shield construction in fine sand strata. Background Art
[0002] With the acceleration of urbanization, urban subway facilities have been rapidly developed as the focus of underground space development and utilization. The construction methods of urban subways are usually open excavation and dark excavation. Dark excavation includes pipe jacking and shield tunneling. The shield tunneling method is widely used because of its fast construction speed, small impact on the surrounding environment and relatively simple construction process. Due to the characteristics of sand, silt and fine sand with large internal friction angle and poor flow plasticity, shield tunneling often encounters problems such as difficulty in excavation and severe wear of cutterheads when excavating in fine sand strata, resulting in large fluctuations in the thrust and torque of the shield cutterhead, slow excavation speed, and large disturbance to the surrounding soil. This has led to increasing attention to soil improvement. Making the soil have good flow plasticity during construction is an important guarantee for the smooth and efficient excavation of the earth pressure balance shield.
[0003] At present, the technology for improving shield slag is mainly concentrated on sand and gravel layers and clay layers, with less research on silt and fine sand layers. When shield tunneling in silt and fine sand layers, due to the large internal friction angle, large permeability, low compressibility and poor plasticity of sand and silt, a series of problems such as failure to meet water-stopping requirements, difficulty in shield slag discharge, high sensitivity of the stratum to the soil bin pressure during excavation and severe wear of the cutterhead tools occur. Summary of the invention
[0004] In view of the defects in the prior art, the present invention provides a foam slag improvement method suitable for shield construction in silt and fine sand strata, so as to solve the problems that the existing shield slag improvement methods mainly focus on sand and gravel and clay strata, lack of research on silt and fine sand strata, resulting in difficulty in shield slag discharge in silt and fine sand strata during shield construction, great sensitivity of the strata to soil bin pressure during excavation, and serious wear of the cutterhead tools.
[0005] The present invention provides a foam slag improvement method suitable for shield construction in fine sand strata, comprising:
[0006] S1. Inject a certain amount of water into the shield soil bin to make the soil moisture content within the preset range;
[0007] S2. Add foam liquid prepared according to the moisture content of the slag through the nozzles on the soil bin partition and the cutter head; the adding rate of the foam liquid is determined according to the consistency value C and the slump value T of the slag at the target moisture content, and the adding rate is the volume of foam liquid to be injected for each ring of shield excavation;
[0008] S3. Monitor the state of the slag when excavating in the fine sand stratum and adjust the injection ratio of the foam liquid according to the state of the slag; when the foam slag parameters of the shield in the fine sand stratum meet the preset values, determine that the slag meets the improvement requirements.
[0009] It can be seen from the above technical scheme that the present invention provides a foam slag improvement method suitable for shield construction in fine sand strata. According to the characteristics of large internal friction angle and poor plasticity of fine sand strata, consistency and slump are used as evaluation indicators, which can effectively solve the problems of difficult shield slag discharge and serious wear of cutterhead tools.
[0010] Optionally, in step S1, in order to make the soil moisture content within a preset range, the amount of water injected into the shield soil bin is determined according to the following formula: m L is the amount of water injected into the shield soil bin,
[0011]
[0012] Among them, m s is the mass of each ring of slag, w s is the current soil moisture content, and w is the target soil moisture content for improvement.
[0013] Optionally, step S2 includes:
[0014] The relationship models between the consistency value C and the soil moisture content w, and the foam addition amount FIR, and the relationship models between the slump value T and the soil moisture content w, and the foam addition amount FIR are established respectively;
[0015] Obtain the foam addition amount FIR when the consistency value C, slump value T and soil moisture content w are within the preset range;
[0016] According to the foam addition amount FIR and the volume of each ring of slag V s , determine the volume of foam liquid V that needs to be added for each shield excavation ring f .
[0017] Optionally, the relationship model expression of the consistency value C, the soil moisture content w, and the foam addition amount FIR is:
[0018] C=30.7FIR 2 -302.75w 2 +242.05w+10.96FIR-41.08;
[0019] The relationship model expression of the slump value T, soil moisture content w, and foam addition amount FIR is:
[0020] T=86.8FIR 2 -1272.64w 2+902.12w+20.28FIR-148.56;
[0021] Among them, C is the consistency value, T is the slump value, FIR is the foam dosage, and w is the moisture content of the slag.
[0022] Optionally, the volume of foam liquid V to be added for each ring of shield excavation is f Determined according to the following formula:
[0023] V f =V S ×FIR,
[0024] The volume of each ring of slag is D is the shield excavation diameter / m, L is the width of each ring of segments / m, and ε is the loose coefficient of slag.
[0025] Optionally, step S2 further includes:
[0026] According to the volume of foam liquid V that needs to be added for each ring of shield tunneling f Determine the volume of foaming agent V required for each excavation ring g ;in, W is the volume fraction of the foam liquid, and EFR′ is the foaming ratio of the foaming agent at the soil bin pressure P.
[0027] Optionally, the foaming ratio EFR′ of the foaming agent at the soil bin pressure P is determined according to the following formula:
[0028]
[0029] Here, FER is the foaming ratio at standard atmospheric pressure P0.
[0030] By adopting the above technical solution, the present application has the following beneficial effects:
[0031] Aiming at the characteristics of large internal friction angle and poor flow plasticity of fine sand strata, the present invention adopts consistency and slump as evaluation indicators, and from the two dimensions of consistency and slump, forms relationship model expressions of foam external admixture FIR and consistency value C and foam external admixture FIR and slump value T for slag in fine sand strata, so as to take into account the influence of consistency and slump of fine sand strata during construction. The consistency determines the flow plasticity of slag, and the slump determines the sensitivity of the stratum to the soil bin pressure during excavation, which can effectively solve the problems of difficult shield slag discharge and severe wear of cutterhead tools. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] In order to more clearly illustrate the specific embodiments of the present invention or the technical solutions in the prior art, the following is a brief introduction to the drawings required for the specific embodiments or the description of the prior art. In all the drawings, similar elements or parts are generally identified by similar reference numerals. In the drawings, the elements or parts are not necessarily drawn according to the actual scale.
[0033] Figure 1 A flow chart of a foam slag improvement method applicable to shield construction in fine sand strata provided by an embodiment of the present invention is shown;
[0034] Figure 2 A flow chart of a foam slag improvement method suitable for shield construction in fine sand strata provided by an embodiment of the present invention is shown. DETAILED DESCRIPTION
[0035] The following embodiments of the technical solution of the present invention are described in detail in conjunction with the accompanying drawings. The following embodiments are only used to more clearly illustrate the technical solution of the present invention, and are therefore only used as examples, and cannot be used to limit the protection scope of the present invention.
[0036] It should be noted that, unless otherwise specified, the technical terms or scientific terms used in this application should have the common meanings understood by those skilled in the art to which the invention belongs.
[0037] The shield slag of this embodiment is taken from a shield section of Nantong Rail Transit Line 2. The diameter D of the tunnel in this shield section is 6.2m, the width L of each ring segment is 1.2m, the shield soil bin pressure P is about 1.5bar, and the soil layer is a silty sand and sandy silty soil layer. The natural moisture content is 25% determined by on-site sampling. Through geotechnical tests such as screening method and densimeter method, the uneven coefficient Cu and curvature coefficient CC of fine sand are measured to be 2.39 and 0.99 respectively. According to the geotechnical test regulations, when the uneven coefficient Cu≥5 and the curvature coefficient 1≤CC≤3, it is a well-graded soil, otherwise it is a poorly graded soil. According to the test results, it is determined that the shield slag of this embodiment is poorly graded fine sand, so it needs to be improved.
[0038] Figure 1 The flowchart of a foam slag improvement method for shield construction in fine sand strata provided by an embodiment of the present invention is shown. Figure 1 As shown, a foam slag improvement method suitable for shield construction in fine sand strata according to an embodiment of the present invention comprises:
[0039] S1. Inject a certain amount of water into the shield soil bin to make the moisture content of the slag within the preset range.
[0040] In step S1, in order to make the soil moisture content within the preset range, the amount of water injected into the shield soil bin is determined according to the following formula: mL is the amount of water injected into the shield soil bin,
[0041]
[0042] In the above formula, m s is the mass of each ring of slag, w s is the current soil moisture content, i.e., the natural moisture content of 25%, and w is the target moisture content of the improved soil, i.e., the optimal soil moisture content of 32.5% in this embodiment. Based on the above formula, the amount of water injected into the shield soil bin is further obtained to be 2.4m 3 .
[0043] S2. Add foam liquid prepared according to the moisture content of the slag through the nozzles on the soil bin partition and the cutter head; the rate of adding foam liquid is determined according to the consistency value C and slump value T when the slag is at the target moisture content, and the adding rate is the volume of foam liquid that needs to be injected for each ring of shield excavation.
[0044] Among them, Figure 2 As shown, step S2 specifically includes:
[0045] S201, respectively establishing the relationship model between the consistency value C and the soil moisture content w, and the foam external admixture FIR, and the relationship model between the slump value T and the soil moisture content w, and the foam external admixture FIR.
[0046] Specifically, the relationship model expression between the consistency value C, the soil moisture content w, and the foam addition amount FIR is:
[0047] C=30.7FIR 2 -302.75w 2 +242.05w+10.96FIR-41.08;
[0048] The relationship model expression of slump value T, soil moisture content w, and foam addition amount FIR is:
[0049] T=86.8FIR 2 -1272.64w 2 +902.12w+20.28FIR-148.56;
[0050] Among them, C is the consistency value, T is the slump value, FIR is the foam dosage, and w is the moisture content of the slag.
[0051] S202, obtaining the foam admixture amount FIR when the consistency value C, the slump value T and the soil moisture content w are within a preset range.
[0052] Through preliminary measurement, the consistency value C should be in the range of 8-10cm, and the slump value T should be in the range of 15-20cm. Therefore, the measured foam admixture FIR and the aforementioned predetermined target moisture content w of improved slag are 32.5%, and the target foam admixture FIR is determined to be 15%.
[0053] S203, according to the foam addition amount FIR and the volume V of each ring of slag s , determine the volume of foam liquid V that needs to be added for each shield excavation ring f .
[0054] Based on the determined target foam addition amount FIR, the volume of foam liquid V to be added for each tunneling ring of the shield is f Determined according to the following formula:
[0055] V f =V S ×FIR,
[0056] The volume of each ring of slag is D is the shield excavation diameter / m, L is the width of each ring segment / m, and ε is the loose coefficient of the slag. In this embodiment, the volume of each ring of slag V s 40.56m 3 , the volume of foam liquid V that needs to be added for each ring of shield excavation f 6.08m 3 , the loose coefficient ε of the slag is 1.12.
[0057] In view of the large internal friction angle and poor flow plasticity of fine sand formations, this embodiment adopts consistency and slump as evaluation indicators. Starting from the two dimensions of consistency and slump, a relationship model expression between the foam external admixture FIR and the consistency value C and between the foam external admixture FIR and the slump value T is formed for the slag in the fine sand formation, so as to take into account the influence of consistency and slump of the fine sand formation during construction. The consistency determines the flow plasticity of the slag, and the slump determines the sensitivity of the formation to the soil bin pressure during excavation. The above two indicators can effectively solve the problems of difficult shield slag discharge and severe wear of the cutterhead tool.
[0058] In a possible implementation, step S2 further includes:
[0059] According to the volume of foam liquid V that needs to be added for each ring of shield tunneling f Determine the volume of foaming agent V required for each excavation ring g ;in, W is the volume fraction of the foaming agent in the foam liquid, and EFR′ is the foaming ratio of the foaming agent at the soil bin pressure P.
[0060] Optionally, the expansion ratio EFR′ of the foaming agent at the soil bin pressure P is determined according to the following formula:
[0061]
[0062] Here, FER is the foaming ratio at standard atmospheric pressure P0.
[0063] The volume fraction W of the foaming agent in the foam liquid and the foaming ratio FER of the foaming agent at the standard atmospheric pressure P0 depend on the properties of the foaming agent itself. In this embodiment, the volume fraction W = 3%, the foaming ratio EFR' is 11.5 when the current soil bin pressure P is 1.5 bar, and the volume of foaming agent V required for each excavation ring is g 1.59×10 -2 m 3 .
[0064] S3. Monitor the state of the slag when excavating in the fine sand stratum and adjust the injection ratio of the foam liquid according to the state of the slag; when the foam slag parameters of the shield in the fine sand stratum meet the preset values, determine that the slag meets the improvement requirements.
[0065] Based on the method of this embodiment, the optimal foam slag improvement parameters for shield tunneling in fine sand strata under the current construction environment are: slag moisture content w = 32.5%, foam admixture amount FIR = 15%, at this time the foaming ratio of the foaming agent is maintained at about 12 times, the half-life is about 10 minutes, the slump value of the improved slag is about 16.5cm, which meets the requirements of the range of 15-20cm, and when there is no water and foam precipitation, the slag flow plasticity is good, which can well meet the requirements of shield construction.
[0066] The technical features of the above embodiments may be combined arbitrarily. To make the description concise, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0067] The above-mentioned embodiments only express several implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present application, and these all belong to the protection scope of the present application. Therefore, the protection scope of the patent of the present application shall be subject to the attached claims.
Claims
1. A foam slag improvement method suitable for shield construction in fine sand strata, characterized in that: include: S1. Inject a certain amount of water into the shield soil bin to make the soil moisture content within the preset range; S2. Add foam liquid prepared according to the moisture content of the slag through the nozzles on the soil bin partition and the cutter head; the adding rate of the foam liquid is determined according to the consistency value C and the slump value T of the slag at the target moisture content, and the adding rate is the volume of foam liquid to be injected for each ring of shield excavation; S3. Monitor the soil state when excavating in the fine sand stratum, and adjust the injection ratio of the foam liquid according to the soil state; when the foam soil parameter of the shield in the fine sand stratum meets the preset value, determine that the soil meets the improvement requirements; In step S1, in order to make the soil moisture content within the preset range, the amount of water injected into the shield soil bin is determined according to the following formula: is the amount of water injected into the shield soil bin, , in, m s is the mass of each ring of slag, w s is the current soil moisture content, w is the target moisture content of the slag; Step S2 includes: The relationship models between the consistency value C and the target soil moisture content w, and the foam admixture FIR, and the relationship models between the slump value T and the target soil moisture content w, and the foam admixture FIR are established respectively; Obtain the foam addition amount FIR when the consistency value C, slump value T and target soil moisture content w are within the preset range; According to the foam addition amount FIR and the volume of each ring of slag V s , determine the volume of foam liquid to be added for each shield tunneling ring ; The relationship model expression of the consistency value C, the target soil moisture content w, and the foam addition amount FIR is: ; The relationship model expression of the slump value T, the target soil moisture content w, and the foam addition amount FIR is: ; The volume of foam liquid that needs to be added for each ring of shield excavation Determined according to the following formula: , The volume of each ring of slag is , D is the shield excavation diameter / m, L is the width of each ring segment / m, is the loose coefficient of soil; Step S2 also includes: According to the volume of foam liquid that needs to be added for each ring of shield excavation Determine the volume of foaming agent required for each ring of excavation ;in, , W is the volume fraction of foam liquid, is the foaming ratio of the foaming agent at the soil bin pressure P; The foaming ratio of the foaming agent at the soil bin pressure P Determined according to the following formula: , in, Standard atmospheric pressure The foaming ratio below.
Citation Information
Cited By
Soil pressure shield muck improving material and preparation method thereof
CN121293711A