Particle sorting system and method

By guiding electromagnetic radiation on the micropore array to destroy the surface material, combined with laser technology and surface modification layer, the problems of cell sorting efficiency and purity in the existing technology are solved, and efficient, sterile and rapid cell sorting are achieved. , suitable for clinical applications.

CN115461153BActive Publication Date: 2024-11-26ORCA BIOSYSTEMS INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202180031428.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2020-03-04
Filing Date
2021-03-03
Publication Date
2024-11-26
Estimated Expiration
2041-03-03

AI Technical Summary

Technical Problem

The prior art is difficult to quickly and sterilely sort cells, especially to achieve high-efficiency cell sorting while maintaining cell viability and high purity, especially in clinical applications where there are challenges to the isolation of rare stem cells and immune cells.

Method used

Using micropore arrays with specific pore structures and surface materials, the surface material is destroyed by directing electromagnetic radiation, thereby releasing target cells, combining laser technology and surface modification layers to improve cell extraction efficiency and purity.

Benefits of technology

It achieves efficient, sterile and rapid cell sorting, significantly improves cell viability and extraction efficiency, and can achieve high sorting rate without damaging cell function, which is suitable for clinical applications.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115461153B_ABST
    Figure CN115461153B_ABST
Patent Text Reader

Abstract

Systems and methods for particle sorting are described. An array may include a substrate having a first surface and a second surface opposite the first surface. The substrate may include a plurality of holes defining a lumen extending from the first surface to the second surface. The plurality of holes may be configured to receive a sample solution comprising a plurality of particles. The array may also include a surface material disposed at or adjacent to the first surface or the second surface. The surface material may include a plurality of materials configured to modify the wetting behavior of a sample solution or a plurality of particles at or adjacent to the first surface or the second surface such that one of the first surface or the second surface is hydrophilic and the other of the first surface or the second surface is hydrophobic.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Cross-references

[0002] This application claims the benefit of U.S. Provisional Patent Application No. 62 / 985,257, filed on March 4, 2020, which is incorporated herein by reference. Background Art

[0003] Cell-based therapies represent the foundation of regenerative medicine and immunotherapy. Although many non-therapeutic cells carried over into therapy are harmless, even small amounts of specific abnormal cell types can cause serious adverse consequences for patients. Therefore, it is critical to purify therapeutic cells from harmful cells before transplanting them into patients. To accelerate the translation of cell-based regenerative medicine technologies to the clinic, high-throughput, high-purity methods for isolating rare stem cells and other immune cell types based on differential surface marker expression in a sterile and clinically applicable format may be necessary. Summary of the invention

[0004] Embodiments disclosed herein provide systems, methods and devices for sorting cells. In some cases, cells can be sorted by means of lasers (e.g., laser extraction) and / or microwell arrays. The microwell array may include a coating that can interact with the laser to help extract target cells. In some cases, the coating can peel off while destroying the meniscus of the liquid held in the microwell array. Advantageously, the methods described herein can improve cell viability and extraction efficiency, for example, because the laser is directed to the surface of the array, rather than being directed directly to the liquid holding the target particles.

[0005] In some aspects, the present disclosure provides an array comprising a substrate having a first surface and a second surface opposite to the first surface, wherein the substrate comprises a substrate material and a surface material, wherein the surface material is located at or adjacent to the first surface or the second surface, and the substrate comprises a plurality of holes defining an inner cavity extending from the first surface to the second surface, and wherein the substrate is characterized in that: each of the plurality of holes has a maximum diameter of 500 microns or less, each of the plurality of holes has an aspect ratio of 5 or greater, and the surface material is selected from a material that absorbs greater than 10% of incident electromagnetic radiation.

[0006] In some aspects, the present disclosure provides an array comprising: a substrate having a first surface and a second surface opposite to the first surface, wherein the substrate comprises a substrate material and a surface material, wherein the surface material is located at or adjacent to the first surface or the second surface, and the substrate comprises a plurality of holes extending from the first surface to the second surface, and wherein the substrate is characterized in that: the hole density is 100 or more holes / square millimeter, the aspect ratio of each hole in the plurality of holes is 10 or greater, and the surface material is selected from a material that absorbs greater than 10% of incident electromagnetic radiation.

[0007] In certain embodiments, the maximum cross-sectional area of ​​each hole is about 0.008 mm 2 In some embodiments, the aperture of each hole in the plurality of holes is in the range of 5 microns to 100 microns. In some embodiments, the aperture of each hole in the plurality of holes is in the range of 15 microns to 50 microns. In some embodiments, each hole has a length selected from about 1mm to about 500mm. In some embodiments, each hole has a length selected from about 1mm to about 100mm. In some embodiments, each hole has a length selected from the range of about 0.1mm to about 10mm.

[0008] In certain embodiments, the hole density is in the range of 100 holes / square millimeter to 2500 holes / square millimeter. In certain embodiments, the hole density is in the range of 500 holes / square millimeter to 1500 holes / square millimeter. In certain embodiments, the surface material is substantially similar to the substrate material. In certain embodiments, the surface material is different from the substrate material. In certain embodiments, the substrate material is glass, and the surface material is not glass. In certain embodiments, the surface material comprises metal. In certain embodiments, the surface material absorbs greater than 10% of the incident electromagnetic radiation, and the wavelength of the incident electromagnetic radiation is selected from 0.4 microns to 2.5 microns. In certain embodiments, the surface material absorbs greater than 50% of the incident radiation. In certain embodiments, the surface material absorbs greater than 50% of the incident electromagnetic radiation, and the wavelength of the incident electromagnetic radiation is selected from 0.4 microns to 1.5 microns.

[0009] In certain embodiments, the aspect ratio is in the range of 5 to 100. In certain embodiments, the aspect ratio is 20 or greater. In certain embodiments, the aspect ratio is 50 or greater. In certain embodiments, the aspect ratio is 100 or greater. In certain embodiments, the surface material coats or partially coats the second surface. In certain embodiments, the surface material coats or partially coats the first surface. In certain embodiments, the surface material does not block the lumen entering the hole. In certain embodiments, the surface material has an average thickness of about 20nm to 500nm. In certain embodiments, the surface material has an average thickness of about 100nm to 500nm. In certain embodiments, the surface material is hydrophobic.

[0010] In certain embodiments, the first surface and the second surface are substantially parallel planes. In certain embodiments, the plurality of holes extend at an angle relative to the surface normal from the first surface to the second surface. In certain embodiments, the angle is larger in the range of 0 to 90 degrees. In certain embodiments, the plurality of holes extend orthogonally from the first surface to the second surface. In certain embodiments, the plurality of holes traverse an indirect path from the first surface to the second surface.

[0011] In some aspects, the present disclosure provides a system for sorting components of a mixture, the system comprising an array according to any aspect of the present disclosure; and a housing comprising an inner surface configured to receive selected contents released from the array. In some embodiments, the inner surface is located below the second surface of the substrate.

[0012] In some aspects, the present disclosure provides a method for releasing selected contents from a hole in an array, the method comprising: identifying a hole in an array having selected contents, wherein the array comprises a substrate having a first surface and a second surface opposite to the first surface, wherein the substrate comprises a substrate material and a surface material, wherein the surface material is located at or adjacent to the first surface or the second surface, and the substrate comprises a plurality of holes defining an inner cavity extending from the first surface to the second surface, wherein the substrate is characterized by one or more of the following: (a) a maximum diameter of each of the plurality of holes is 500 microns or less; (b) an aspect ratio of each of the plurality of holes is 5 or greater; (c) a hole density of 100 or more holes / square millimeter; and (d) the surface material is selected from materials that absorb greater than 10% of incident electromagnetic radiation; and removing a portion of the surface material from the first surface or the second surface of the array using electromagnetic radiation directed to the surface material within or adjacent to the identified hole, thereby releasing the contents of the identified hole.

[0013] In certain embodiments, the electromagnetic radiation is selected from a wavelength of 0.2 microns to 2.5 microns, a flux level sufficient to disrupt adhesion between the contents and the pores, and a pulse duration in the range of 1 ns to 1 millisecond. In certain embodiments, removing surface material comprises ablation. In certain embodiments, removing surface material comprises mechanical removal. In certain embodiments, mechanical removal comprises exfoliation. In certain embodiments, removing surface material comprises photothermal removal. In certain embodiments, removing surface material comprises photochemical removal. In certain embodiments, removing surface material comprises photoacoustic removal.

[0014] In certain embodiments, the selected contents include cells in an aqueous solution. In certain embodiments, the cells are selected from INKT cells, Tmem, Treg, HSPC, and combinations thereof. In certain embodiments, the cross-sectional area of ​​each of the plurality of holes is each about 0.008 mm 2 In some embodiments, the aperture of each hole in the plurality of holes is in the range of 5 microns to 100 microns. In some embodiments, the aperture of each hole in the plurality of holes is in the range of 15 microns to 50 microns. In some embodiments, each hole has a length selected from about 1mm to about 500mm. In some embodiments, each hole has a length selected from about 1mm to about 100mm. In some embodiments, each hole has a length selected from about 0.1mm to about 10mm.

[0015] In some embodiments, the hole density on the array is in the range of 100 holes / mm2 to 2500 holes / mm2. In some embodiments, the hole density of the array is in the range of 500 holes / mm2 to 1500 holes / mm2. In some embodiments, the array has greater than 1000 holes / mm2. 2 In certain embodiments, the pore density is 5000 pores / mm 2 In some embodiments, the aspect ratio is in the range of 5 to 100. In some embodiments, the aspect ratio of the hole is 20 or more. In some embodiments, the aspect ratio of the hole is 50 or more. In some embodiments, the aspect ratio of the hole is 100 or more. In some embodiments, the surface material absorbs greater than 10% at a wavelength selected from about 0.4 microns to about 2.5 microns. In some embodiments, the surface material absorbs greater than 50% of the incident radiation. In some embodiments, the surface material absorbs greater than 50% of the incident radiation, and the wavelength of the incident radiation is selected from about 0.4 microns to about 2.5 microns.

[0016] In certain embodiments, the array is characterized by two or more of the following: (a) the maximum diameter of each hole in the plurality of holes is 500 microns or less, (b) the aspect ratio of each hole in the plurality of holes is 5 or more, (c) the hole density is 100 or more holes / square millimeter, and (d) the surface material is selected from a material that absorbs more than 10% of the incident electromagnetic radiation. In certain embodiments, a portion of the surface material is adjacent to the identified hole. In certain embodiments, a portion of the surface includes the luminal surface of the identified hole. In certain embodiments, a portion of the surface is removed to a depth of 100 microns or less. In certain embodiments, a portion of the surface is removed to a depth of 50 microns or less. In certain embodiments, the method further comprises loading the array with a solution containing the selected contents before identifying the hole with the selected contents. In certain embodiments, identifying the hole with the selected contents comprises analyzing electromagnetic radiation emitted from the hole of the array. In certain embodiments, releasing the contents comprises releasing the contents at a rate of about 5,000 pores / second to about 100,000,000 pores / second.

[0017] In some aspects, the present disclosure provides a bead comprising: an infrared absorbing core; and a non-infrared absorbing shell, wherein the non-infrared absorbing shell has an outer diameter equal to or less than about 10 microns.

[0018] In certain embodiments, the non-infrared absorbing shell comprises agarose, dextran, or both. In certain embodiments, the infrared absorbing core comprises an infrared absorbing dye. In certain embodiments, the bead has a diameter equal to or less than about 20 microns.

[0019] In some aspects, the present disclosure provides a solution comprising: a plurality of beads according to any aspect of the present disclosure; and a target particle. In some embodiments, the target particle is a cell. In some embodiments, the ratio of the number of the plurality of beads to the number of the plurality of cells is about 1:1 to 10:1.

[0020] In another aspect of the present disclosure, an array includes a substrate having a first surface and a second surface opposite to the first surface, wherein the substrate includes a plurality of holes defining an inner cavity extending from the first surface to the second surface, and wherein the plurality of holes are configured to receive a sample solution comprising a plurality of particles; and a surface material disposed at or adjacent to the first surface or the second surface, wherein the surface material includes a plurality of materials configured to modify the wetting behavior of the sample solution or the plurality of particles at or adjacent to the first surface or the second surface, such that one of the first surface or the second surface is hydrophilic and the other of the first surface or the second surface is hydrophobic.

[0021] In some embodiments, the plurality of materials include a metal layer (such as sputtered, physically sputtered, chemically coated, functionally modified (i.e., surface hydrophilic modified, surface hydrophobic modified), etc.). The metal layer may have a thickness in the range of about 50 nm to about 1 mm. The metal layer may include titanium and / or gold. A first portion of the metal layer may be coated with a first chemical coating. A second portion of the metal layer may be coated with a second chemical coating different from the first chemical coating. In some embodiments, the first chemical coating may be disposed on a vertical sidewall of the plurality of holes at or adjacent to the first surface or the second surface. The first chemical coating may be configured to reduce or eliminate adhesion of the particles to the vertical sidewalls of the holes. The second chemical coating may be configured to reduce or prevent unwanted leakage of the sample solution from the holes. In some embodiments, the second chemical coating is hydrophobic. The second chemical coating may be disposed on a portion of the first surface or the second surface of the substrate or adjacent to the first surface or the second surface. The portion of the substrate may be adjacent to the vertical sidewalls of the plurality of holes. In some cases, the portion of the substrate can be substantially orthogonal to the vertical sidewalls of the plurality of holes.

[0022] In some embodiments, the first chemical coating may include methoxy-poly(ethylene glycol)-thiol. The second chemical coating may include 1H,1H,2H,2H-perfluorodecanethiol.

[0023] In some embodiments, the plurality of materials further comprises a chemical coating that is not on the metal layer (such as sputtered, physically sputtered, chemically coated, functionally modified (i.e., surface hydrophilicity modified, surface hydrophobicity modified), etc.). The chemical coating may be disposed on one or more portions of the substrate or the plurality of holes that do not have the metal layer (such as sputtered, physically sputtered, chemically coated, functionally modified (i.e., surface hydrophilicity modified, surface hydrophobicity modified), etc.). In some embodiments, the chemical coating comprises methoxy-poly(ethylene glycol)-silane.

[0024] In some embodiments, the second surface can be configured to receive the sample solution comprising the plurality of particles. The first surface can be configured to be destroyed to release one or more of the particles from one or more of the holes. In some embodiments, the second surface can be hydrophilic to enhance absorption of the sample solution comprising the plurality of particles into the plurality of holes. The first surface can be hydrophobic to reduce or eliminate undesirable leakage of the sample solution from the holes.

[0025] In some embodiments, the first surface can be configured to be disrupted by directing electromagnetic radiation at one or more portions of the second surface. In some embodiments, each of the plurality of holes has a maximum diameter of 500 microns or less. Each of the plurality of holes can have an aspect ratio of 5 or more. The surface material can be selected from a material that absorbs greater than 10% of incident electromagnetic radiation. The substrate can have a hole density of 100 or more holes / square millimeter.

[0026] In some embodiments, the particle extraction yield of the array is at least 70%. The particle extraction yield of the array having a functionally modified surface layer (i.e., a chemically coated metal layer) (i.e., a surface hydrophilic modification, a surface hydrophobic modification) can be higher than another array without the functionally modified surface layer (i.e., a chemically coated metal layer) (i.e., a surface hydrophilic modification, a surface hydrophobic modification). For example, the particle extraction yield of the array having the functionally modified surface layer (i.e., a chemically coated metal layer) (i.e., a surface hydrophilic modification, a surface hydrophobic modification) can be at least 5% higher than another array without the functionally modified surface layer (i.e., a chemically coated metal layer) (i.e., a surface hydrophilic modification, a surface hydrophobic modification). In some cases, the particle extraction yield of the array having the functionally modified surface layer (i.e., chemically coated metal layer) (i.e., surface hydrophilicity modified, surface hydrophobic modified) is at least 20% higher than that of the other array without the functionally modified surface layer (i.e., chemically coated metal layer) (i.e., surface hydrophilicity modified, surface hydrophobic modified).

[0027] In some embodiments, the plurality of particles include living cells. The live cell extraction yield of the array having the functionally modified surface layer (i.e., chemically coated metal layer) (i.e., surface hydrophilic modification, surface hydrophobic modification) may be higher than another array without the functionally modified surface layer (i.e., chemically coated metal layer) (i.e., surface hydrophilic modification, surface hydrophobic modification). For example, the live cell extraction yield of the array having the functionally modified surface layer (i.e., chemically coated metal layer) (i.e., surface hydrophilic modification, surface hydrophobic modification) may be at least 5% higher than another array without the functionally modified surface layer (i.e., chemically coated metal layer) (i.e., surface hydrophilic modification, surface hydrophobic modification). In some cases, the live cell extraction yield of the array having the functionally modified surface layer (i.e., chemically coated metal layer) (i.e., surface hydrophilicity modified, surface hydrophobic modified) is at least 20% higher than that of the other array without the functionally modified surface layer (i.e., chemically coated metal layer) (i.e., surface hydrophilicity modified, surface hydrophobic modified).

[0028] Incorporation by reference

[0029] All publications, patents, and patent applications mentioned in this specification are herein incorporated by reference to the same extent as if each individual publication, patent, or patent application was specifically and individually indicated to be incorporated by reference. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] The novel features of the present invention are particularly set forth in the appended claims. A better understanding of the features and advantages of the present invention will be obtained by reference to the following detailed description and accompanying drawings which set forth illustrative embodiments in which the principles of the invention are utilized, wherein:

[0031] Figure 1A is a side cross-sectional view of an array for sorting cells according to some embodiments.

[0032] Figure 1B is a top view of an array for sorting particles according to some embodiments.

[0033] Figure 1C Example images of arrays with different cell concentrations are shown according to some embodiments.

[0034] Figure 2A is a side cross-sectional view of an example array for sorting particles according to some embodiments.

[0035] Figure 2B is an orthogonal view of an example substrate of an example array according to some embodiments.

[0036] Figure 3A are orthogonal views of example arrays for sorting particles according to some embodiments.

[0037] Figure 3B is an orthogonal view of an example array for sorting particles that include a coating removed by a laser at locations adjacent to the holes, according to some embodiments.

[0038] Figure 4A are orthogonal views of PBMCs stained with an IR energy absorbing fluorescent dye in an exemplary first array according to some embodiments.

[0039] Figure 4B is an orthogonal view of an example first array after extraction of PBMCs according to some embodiments.

[0040] Figure 5A Shown is a side cross-sectional view of an array comprising microspheres according to some embodiments.

[0041] Figure 5B Shown is a side cross-sectional view of an array including microspheres and an aqueous sample solution according to some embodiments.

[0042] Fig. 6A Shown is a bright field image of a microwell array filled with microspheres and cells according to some embodiments.

[0043] Figure 6B Shown is a bright field image of cells extracted from a single well, according to some embodiments.

[0044] Figure 6C Shown is an image of an array of wells filled with microspheres and one cell, according to some embodiments.

[0045] Fig.6D Shown is an image of an array after extraction of cells from a single microwell, according to some embodiments.

[0046] Fig. 7A Example bright field images of extracted cells are shown according to some embodiments.

[0047] Figure 7B Example images of extracted cells are shown according to some embodiments.

[0048] Figure 8 Shown is a bright field image of example microspheres comprising agarose and dextran according to some embodiments.

[0049] Fig. 9 Shown is a high magnification infrared image of example microspheres comprising agarose and dextran, according to some embodiments.

[0050] Fig. 10A Shown is a bright field image of example microspheres comprising agarose and an IR absorbing dye, according to some embodiments.

[0051] Fig. 10B An infrared image of example microspheres comprising agarose and an IR absorbing dye is shown according to some embodiments.

[0052] Fig.11A A flow chart of a coating procedure according to some embodiments is illustrated.

[0053] Fig. 11B Illustrated according to some embodiments Fig.11A Additional details of the coating procedure.

[0054] Fig. 12A is a top view of an array for sorting particles according to some embodiments.

[0055] Fig. 12B Shown is a cross-sectional view of an array having a surface modification at the bottom end of the array according to some embodiments.

[0056] Fig.13A Shown is a cross-sectional view of the bottom end of an array prior to surface modification, according to some embodiments.

[0057] Fig. 13B A cross-sectional view of the bottom end of an array coated with a layer of pretreatment material is shown according to some embodiments.

[0058] Fig. 13CA cross-sectional view of the bottom end of an array coated with a first material and a second material is shown according to some embodiments.

[0059] Fig.13D Shown is a cross-sectional view of the bottom end of an array having two layers of coating material and surface modification according to some embodiments.

[0060] Fig.14A A side cross-sectional view of a system including an array, a housing, and an inner surface is shown according to some embodiments.

[0061] Fig. 14B A side cross-sectional view of a system including an array, a housing, an interior surface, and an electromagnetic radiation source is shown according to some embodiments.

[0062] Fig.15A is an orthogonal initial view of a leak test of an example system at 0 hours, according to some embodiments.

[0063] Fig. 15B is an orthogonal end view of a leak test of an example system at 5 hours, according to some embodiments.

[0064] Fig.16A A side cross-sectional view of providing an array including a plurality of holes is shown according to some embodiments.

[0065] Fig. 16B A side cross-sectional view of depositing an aqueous solution within an array is shown, according to some embodiments.

[0066] Fig. 16C Insertion of the cartridge into the cartridge according to some embodiments is shown. Figure 1A Side cross-sectional view of an example array.

[0067] Fig.16D An image showing a plot of signals of a first cell and a second cell according to some embodiments.

[0068] Fig.16E A side cross-sectional view of extracting a second cell is shown according to some embodiments.

[0069] Fig.16F Shown is a side cross-sectional view of collected cells according to some embodiments.

[0070] Fig.17 Shown are example raw fluorescence images of cell arrays according to some embodiments.

[0071] Fig.18 According to some embodiments, Fig.17 Example scatter plot of 500,000 wells of the array shown.

[0072] Figure 19A-Figure 19CA comparison of performance (extraction yield and cell viability) between Au-coated and Cr-coated well plates according to some embodiments is shown.

[0073] Fig. 20 Contact angle images and measurements of different coatings according to some embodiments are shown. DETAILED DESCRIPTION

[0074] It is necessary to provide a cell sorting system with high speed and asepticity. Therefore, systems, devices and methods for sorting cells by laser extraction from arrays (such as microwell arrays) are provided herein. The microwell sorting adopted by the system, device and method herein can be configured to a high sorting rate of about 10,000 cells / second, or 100-1000 times faster than the prior art. In addition, the embodiments described herein can achieve such a sorting rate without compromising cell viability or function, while maintaining asepticity and operator biosafety, reducing contamination between samples, and eliminating any flow rate time limit. In particular, the surface materials of microwell arrays and the systems and methods used therein allow the release of the contents of the wells, while the thermal effects on the contents of the wells can be ignored. Various systems and methods disclosed herein can be combined with other systems and methods or modified with other systems and methods, such as, for example, those described in International Patent Application No. PCT / US2019 / 049221 entitled "ULTRAFAST PARTICLE SORTING", which is incorporated herein by reference in its entirety.

[0075] Array

[0076] An array is provided herein. The array described herein can be used to sort particles. The particles can be target particles, such as cells that need to be enriched for therapeutic use. The array can include a substrate. The substrate can include a first surface, such as a top surface; a second surface opposite the first surface, such as a bottom surface; and a plurality of holes extending from the first surface to the second surface. The holes can define a lumen, which can have different shapes as described herein. The holes can be micropores or microchannels.

[0077] In one non-limiting example, the substrate comprising a plurality of holes is characterized in that each hole has a maximum diameter of 500 microns or less, each hole has an aspect ratio of 10 or more, and the surface material is selected from materials that absorb more than 10% of incident electromagnetic radiation. In an additional or alternative non-limiting example, the substrate comprising a plurality of holes is characterized in that the hole density is 100 or more holes / square millimeter, each hole has an aspect ratio of 10 or more, and the surface material is selected from materials that absorb more than 10% of incident electromagnetic radiation.

[0078] Figure 1Ais a vertical cross-section of an array for sorting particles according to some embodiments. Figure 1A As shown, the array 100 may include a substrate 110, the substrate 110 including (a) a first surface 111 and a second surface 112 opposite to the first surface 111, and (b) a plurality of holes 113 extending from the first surface 111 to the second surface 112. The plurality of holes may be substantially parallel to each other and may be configured to hold the particles together with the liquid. For example, the liquid may be held in the hole by surface tension, and in some cases a meniscus may be formed at one or both ends of each hole.

[0079] The substrate 110 may include a substrate material. The substrate material may be glass, such as silicate glass, fused silica, fused quartz, etc. The substrate material may be plastic, such as PETG, PEEK, etc. In some embodiments, the substrate may be a metal, such as aluminum, steel, chromium, titanium, gold, etc.

[0080] Substrate 110 may include a plurality of holes 113. In some cases, plurality of holes 113 includes about 100,000 to about 100 billion holes. In some cases, plurality of holes 113 includes about 100 to about 1 billion holes. In some cases, plurality of holes 113 includes about 1 million to about 100 billion holes.

[0081] The substrate 110 may include a certain density of holes. The density of the holes may include the number of holes per square millimeter array. The density of the holes may be measured at the first surface 111 or the second surface 112. Optionally, in some embodiments, the first array 100 has an open array fraction (packing density) of about 66% or about 40% to about 75%. In some cases, the hole density may be in the range of 100 to 2500 holes / square millimeter. In some cases, the hole density may be in the range of 500 to 1500 holes / square millimeter. A method of manufacturing a high hole density may be by melting a tube such as a capillary. The hole density may be changed by changing the wall thickness and center diameter of the tube.

[0082] In one non-limiting example, the first array 110 has a width and length of 10×10 inches respectively and includes 240 million holes 113 , each hole 113 having a diameter of 15 um.

[0083] In addition, according to Figure 1A, the first array 100 has an array height 110a measured as a normal distance between the first surface 111 and the second surface 112. In some embodiments, the array height 110a can be measured as the maximum or minimum normal distance between the first surface 111 and the second surface 112. In some embodiments, the array height 110a can be measured as the normal height of the hole 113. In some embodiments, the array height 110a can be measured as the maximum or minimum length of the hole 113. Each hole can have a height (or longitudinal length) 113a. The length between the holes can be uniform, or the length between the holes can vary, such as through deformation or irregularity during the manufacturing process. Optionally, each of the holes 113 has a length equal to or less than about 50mm. In some cases, each hole can have a length selected from about 1mm to about 500mm. In some cases, each hole can have a length selected from about 1mm to about 100mm. In some cases, each hole can have a length selected from about 1mm to about 10mm.

[0084] Optionally, a plurality of holes 113 may be substantially orthogonal to the first surface 111 and the second surface 112. In some embodiments, a plurality of holes 113 may be substantially parallel to each other. In some embodiments, the first surface opposite to the second surface may be substantially parallel planes. A plurality of holes may extend orthogonally from the first surface to the second surface. The holes may extend vertically from the first surface to the second surface. Alternatively, a plurality of holes may extend at an angle relative to the surface normal from the first surface to the second surface. The angle may be less than 90 degrees with respect to the normal. The angle may be less than 60 degrees, less than 45 degrees, less than 30 degrees or less. The angle may be in the range of from 5 degrees to 90 degrees.

[0085] In some embodiments, a plurality of holes can traverse an indirect path from the first surface to the second surface. In such embodiments, the holes can be tangled, braided, or staggered. The holes can include one or more bends such that the path through the holes substantially changes direction relative to a direct path from the first surface to the second surface.

[0086] Figure 1B A top view of an array 100 for sorting particles is shown. In some examples, the array 100 has a plurality of holes 113. Each hole can include a cross section. The cross section can be circular, can be elliptical, can be a polyhedron (e.g., square, hexagonal, octagonal, dodecagonal, etc.), or can have an irregular shape. The shape between the holes can be uniform, or the holes can vary from hole to hole, such as through deformation or irregularity during the manufacturing process.

[0087] refer to Figure 1A, the cross-section of each hole 113 may include a cross-sectional dimension 113b. The cross-sectional dimension may be measured at either of the two surfaces of the array or at an intermediate position. The cross-sectional dimension may be measured at a single cross-section. Additionally or alternatively, the cross-sectional dimension may be averaged over many positions along the hole. The dimension may be measured in a variety of ways, such as using a reference under a microscope, by an interferometer, from flow calculations, etc. In some examples, each hole of the array may have a cross-sectional dimension in the range of 5 microns to 100 microns. In some examples, each hole may have a cross-sectional dimension in the range of 15 microns to 50 microns.

[0088] In some cases, the cross-sectional dimension may be a diameter. The term diameter is intended to encompass the maximum cross-sectional distance of a circular, approximately circular, or elliptical hole. In some examples, each hole of the array may have an aperture in the range of 5 microns to 100 microns. In some examples, each hole may have a diameter in the range of 10 microns to 50 microns.

[0089] Each hole 113 may have a cross-sectional area. The cross-sectional area may be measured at a single cross section. Additionally or alternatively, the cross-sectional area may be averaged over a number of locations along the hole. Figure 1B The white area of ​​the hole 113 shown can define the cross-sectional area at the first surface of the hole. Optionally, each micropore 113 has a cross-sectional area equal to or less than about 1 square millimeter. In some cases, each hole in the plurality of holes can have a cross-sectional area of ​​about 0.008 mm. 2 or smaller maximum cross-sectional area.

[0090] Each hole 113 of the array can have an aspect ratio. The aspect ratio can be the fraction of the length of the hole relative to the maximum cross-sectional dimension of the hole. The aspect ratio can be the fraction of the length of the hole relative to the diameter of the hole. In some cases, the aspect ratio can be in the range of 10 to 100. In some cases, the aspect ratio can be 10 or more. In some cases, the aspect ratio can be 20 or more. In some cases, the aspect ratio can be 100 or more.

[0091] Figure 1C Example images of arrays with different cell concentrations are shown. As shown in the illustrated embodiment, each hole can include one or more target particles, such as cells. A particle or multiple particles can include a cell or multiple cells. The number of multiple cells can be about 1, about 5, about 25 or more. In some examples, the number of multiple cells can be less than about 100 or less than about 1000.

[0092] In some embodiments, the aqueous sample solution can be deposited onto the array 100, such as by spreading the aqueous sample solution onto the array 100. In some embodiments, the first surface 111 of the array 100 can be hydrophilic, and the aqueous sample solution can be absorbed into the wells 113. In some embodiments, the first surface 111 of the array 100 can distribute target particles, such as cells, in the aqueous sample solution between the microwells 113. In some embodiments, the first surface 111 of the array 100 can randomly distribute the target particles in the aqueous sample solution between the microwells 113. In some embodiments, one or more target particles can move through the wells and settle at the bottom of each microwell 113. Optionally, in some embodiments, the target particles can be retained in each well 113 by the surface tension of the aqueous sample solution.

[0093] One or more surface portions of the substrate may be coated with material. The coated material may be configured to be destroyed in response to electromagnetic radiation directed to the coated portion of the substrate or adjacent to the coated portion of the substrate. Therefore, once the target particle is identified as being held in a specific microchannel (hole) of the array, electromagnetic radiation may be directed to the coated portion of the substrate to destroy the surface material, which may cause the meniscus of the liquid held in the microchannel to rupture to release the target particle. In certain embodiments, electromagnetic radiation may remove (e.g., ablate) a portion of the coating material in the hole in the microarray or adjacent to the hole, thereby destroying the meniscus of the liquid held in the microchannel of the hole.

[0094] Surface material

[0095] Non-limiting examples of arrays 100 including surface materials are provided herein, such as Figures 2A to 17 As shown in . Figure 2A , the surface material 120 may include a coating. The coating may be coupled to the first surface 111 of the substrate 110. In some embodiments, the surface material 120 may include a material different from the substrate material. In one example, the coating may include a metal, such as a transition metal (e.g., gold, and a metal that can provide adhesion to gold (such as chromium, titanium, nickel, or nickel-chromium)). In some embodiments, the surface material may include multiple layers. The surface material may include a combination of metal coatings (e.g., Ti-Au). In some embodiments, the surface material may include a metalloid or a metal oxide. In some embodiments, the surface material may include scandium, titanium, vanadium, chromium, manganese, iron, cobalt, nickel, copper, zinc, yttrium, zirconium, platinum, gold, mercury, niobium, iridium, molybdenum, silver, cadmium, tantalum, tungsten, aluminum, silicon, phosphorus, tin, an oxide of any of the foregoing, or any combination thereof.

[0096] In some embodiments, the surface material 120 may include a polymer. In some embodiments, the surface material may include a combination of any coating materials described herein. The surface material or coating may be configured to be disrupted from the first surface 111 of the array in response to electromagnetic radiation directed to or adjacent to a portion of the surface material. Thus, once a target particle is identified as being held within a particular microchannel of the array, electromagnetic radiation may be directed to the surface to disrupt and / or strip the coating, which may disrupt the meniscus of the liquid held in the microchannel to release one or more target particles.

[0097] Figure 2A is a side cross-sectional view of an example array for sorting particles according to some embodiments. Figure 2A As shown in , array 100 may include substrate 110. The substrate may include a plurality of holes 113. Substrate 110 may include a second surface 112 and a first surface 111 opposite second surface 112. Optionally, the plurality of holes 113 may extend from first surface 111 to second surface 112. In some embodiments, coating 120 may be coupled to first surface 111.

[0098] In some embodiments, the array 100 has an open array fraction (packing density) of about 66%. In some embodiments, each hole 113 has a cross-sectional area equal to or less than about 1 square millimeter. In some embodiments, each hole 113 has a diameter of about 50um to about 150um. In some embodiments, each hole 113 has a length equal to or less than about 50mm. In some embodiments, a plurality of holes 113 are orthogonal to the second surface 112 and the first surface 111. In some embodiments, each hole 113 in the plurality of holes 113 can be substantially parallel to each other. In some embodiments, the plurality of holes 113 includes about 1 million to about 100 billion holes.

[0099] In addition, according to Figure 2A , the array 100 can have an array height 110a measured as the distance from the second surface 112 to the surface material 120. In some embodiments, the array height 110a can be measured as the normal distance between the first surface 111 and the second surface 112. In some embodiments, the array height 110a can be measured as the maximum or minimum normal distance between the first surface 111 and the second surface 112. In some embodiments, the array height 110a can be measured as the normal height of the hole 113. In some embodiments, the array height 110a can be measured as the maximum or minimum height of the hole 113.

[0100] Figure 2B is a top view of an example array according to some embodiments. Figure 2B, the plurality of holes 113 within the array 100 are arranged in an orthogonal pattern. In some embodiments, the pattern comprises a linear pattern, a triangular pattern, a hexagonal pattern, an irregular pattern, or any combination thereof. Figure 2B , the orthogonal pattern of holes 113 has at least one of a first spacing 113b and a second spacing 113c, wherein the first spacing 113b and the second spacing are measured between center points of consecutive holes 113. In some embodiments, at least one of the first spacing 113b and the second spacing is measured as a normal distance between opposite points on the surface of the consecutive holes 113. In some embodiments, at least one of the first spacing 113b and the second spacing 113c can be about 10 mm to about 40 mm.

[0101] The arrays described herein may include a coating 120. The coating may be coupled to one or more surface portions of the substrate. The coating may be configured to be destroyed when subjected to electromagnetic radiation. For example, in response to electromagnetic radiation from a laser directed at a portion of the coating, the coating may be peeled off or stripped. Optionally, the coating may include a material different from the substrate. For example, the substrate 110 may include a first material, and the coating 120 may include a second material different from the first material.

[0102] In some cases, the surface material (coating 120) can coat or partially coat the second surface 112 of the array. In addition or in lieu thereof, the surface material can coat or partially coat the first surface 111 of the array. In some cases, the surface material can substantially not hinder access to the lumen of the hole. However, in some cases, some clogging of the holes may occur, such as due to variations in coating thickness during manufacturing. The surface material can have an average thickness of about 20 nanometers (nm) to 500nm. The surface material can have an average thickness of about 100nm to 500nm.

[0103] In some cases, the surface material (coating 120) can be substantially similar to the substrate material 110. In some cases, the array can be homogeneous. In some embodiments, the homogeneous array does not include or need not include a coating. In some embodiments, the homogeneous array includes a uniform agglomerate or alloy material. In one example, the array includes a metalloid, a metal (e.g., chromium, titanium, gold, iron, nickel, copper, platinum or palladium) (e.g., gold and a metal (such as chromium, titanium, nickel or nickel-chromium) that can provide adhesion to gold) or any combination thereof. In some embodiments, the substrate material includes glass, plastic, aluminum, steel, stainless steel or any combination thereof.

[0104] In some cases, the surface material (coating 120) can be substantially different from the substrate material 110. The substrate material can be glass, and the surface material can be a material other than glass. In some cases, the surface material (coating 120) can include a metal. In some cases, the metal can include titanium, gold, chromium, silver, aluminum, or any other one or more metals. In some cases, the surface material can include a metal oxide, such as magnesium fluoride, calcium fluoride, silicon dioxide, etc. The surface material can include a metal layer and / or a metal oxide layer to form a customized optical property, such as reflection or absorption.

[0105] In some embodiments, the surface material (coating 120) comprises a transition metal (e.g., titanium, gold, etc.). In some embodiments, the second material comprises a metalloid. In some embodiments, the second material comprises a metal oxide. In some embodiments, the second material comprises scandium, titanium, vanadium, chromium, manganese, iron, cobalt, nickel, copper, zinc, yttrium, zirconium, platinum, gold, mercury, niobium, iridium, molybdenum, silver, cadmium, tantalum, tungsten, aluminum, silicon, phosphorus, tin, an oxide of any of the foregoing, or any combination thereof.

[0106] In some embodiments, the surface material (coating 120) is selected from materials that will not have a negative impact on cell viability. For example, the surface material can be biocompatible. The surface material can be non-toxic. In certain embodiments, the surface material is selected from materials that will not cause cell damage or cell death when in contact with electromagnetic radiation. For example, the product produced by the surface material in contact with electromagnetic radiation itself may not cause cell damage or cell death. That is to say, the product produced by the ablation of the surface material, for example, can be biocompatible and / or non-toxic to cells. In certain embodiments, the impact on cell viability is assessed by measuring cell viability before and after the cell is exposed to the surface material. In certain embodiments, cell viability remains unchanged or decreases by less than 40%, less than 30%, less than 20%, less than 15%, less than 10% or even less than 5%. In certain embodiments, cell viability can be assessed by measuring cell viability before and after the surface material is in contact with electromagnetic radiation. For example, before cells are loaded into the array and after the cells are released from the holes of the array by contacting the surface material with electromagnetic radiation, cell viability is assessed. In some examples, after the surface material is contacted with electromagnetic radiation, the activity remains unchanged or decreases by less than 40%, less than 30%, less than 20%, less than 15%, less than 10%, less than 5%, or even less than 1%.

[0107] In some cases, the array can have a customized hydrophobicity. In one example, the second surface 112 can be hydrophilic. Optionally, the second surface 112 itself need not be hydrophilic, but can be operably coupled to a hydrophilic coating. In some embodiments, a portion of the coating 120 can be configured to be destroyed from the first surface 111. In some embodiments, a portion of the coating 120 can be configured to be destroyed from the first surface 111 in response to electromagnetic radiation directed to the portion of the coating. In some embodiments, the coating 120 can be hydrophobic.

[0108] The coating 120 can be configured to be destroyed in response to electromagnetic radiation directed to a portion of the surface material. Thus, once a target particle is identified as being held within a particular microchannel (well) of the array, electromagnetic radiation can be directed to the coating to destroy and / or strip the coating 120, which can destroy the meniscus of the liquid held in the microchannel (well 113) to release the target particle. The coating 120 can absorb a wavelength or range of wavelengths corresponding to the wavelength emitted by the electromagnetic radiation source.

[0109] Thus, once a target particle is identified as being held within a particular well of the array, electromagnetic radiation may be directed near or adjacent to the particular well to release the target particle. In some embodiments, the disruption of the surface material comprises removing at least a portion of the material of the array, a coating on the array, or both.

[0110] In some embodiments, destruction of the array can be caused by local heating. Such a mechanism is possible when the pulse duration is long, the peak power density is low, and / or the wavelength of the incident radiation is in the infrared range. Local heating can cause sublimation of the surface material (coating 120) or the array material. In some embodiments, the substrate material and the coating 120 have different thermal expansion coefficients, which can cause peeling.

[0111] Additionally or alternatively, destruction of the array can be caused by ablation. Such a mechanism is possible when the incident peak power density is high, the pulse duration is short, the incident power is high, and / or the incident radiation is in the visible range. Ablation can include local bond breaking and / or vaporization of the array or substrate material.

[0112] Additionally or alternatively, destruction of the array can be caused by plasma generation. Such a mechanism is possible when the pulse duration of the incident radiation is particularly short, the wavelength of the incident radiation is resonant with the multiphoton ionization mechanism, and / or the wavelength of the incident radiation is very short. Pulse durations on the order of picoseconds to femtoseconds can result in faster plasma generation than local heating, resulting in optical etching of substrate or surface materials.

[0113] Additionally or alternatively, destruction of the array may occur through shock wave generation. Such a mechanism may be more likely when peak power density is high, phonon resonances, and / or pulse durations are short. Shock may cause physical vibration, flaking, or shaking of the surface or array material.

[0114] In one example, the surface material (coating 120) absorbs a range of wavelengths in the visible or infrared range. In some embodiments, the surface material may be opaque. The surface material may absorb a band of at least 5 nanometers selected in the visible and infrared ranges. The surface material may absorb greater than 10% of the incident radiation selected from at least 5 nanometer bands of 0.4 to 2.5 microns. The surface material may absorb greater than 10% of the incident electromagnetic radiation selected from wavelengths of 0.4 microns to 2.5 microns. In some cases, the surface material may absorb greater than 50% of the incident radiation in at least 5 nanometer bands. A 5 nanometer band may be selected within a wavelength range of 0.4 to 2.5 microns. The surface material may absorb greater than 50% of the incident electromagnetic radiation selected from wavelengths of 0.4 microns to 1.5 microns. The surface material may absorb greater than 10% of the incident radiation selected from harmonics of doped ytterbium orthovanadate or ytterbium aluminum garnet solid-state lasers. The surface material may absorb greater than 10% of the incident 1064 nanometer radiation.

[0115] In one example, the coating 120 of the array 100 has an average thickness of about 600 nm. The thickness of the coating 120 can be reduced in thickness by an infrared (IR) laser to about 100 nm or less, such as about 75 nm or less, or even about 50 nm or less. The coating thickness may be between 10 and 1000 nm. In some embodiments, the thickness of the coating or any discernible layer thereof is or is about, 10 nm, 20 nm, 30 nm, 40 nm, 50 nm, 60 nm, 70 nm, 80 nm, 90 nm, 100 nm, 150 nm, 200 nm, 250 nm, 300 nm, 300 nm, 400 nm, 450 nm, 500 nm, 550 nm, 600 nm, 650 nm, 700 nm, 750 nm, 800 nm, 850 nm, 900 nm, 950 nm, or 1000 nm, or any range between two of the above values. In some embodiments, the coating, or any discernible layer thereof, has a thickness of at least or is at least about 10 nm, 20 nm, 30 nm, 40 nm, 50 nm, 60 nm, 70 nm, 80 nm, 90 nm, 100 nm, 150 nm, 200 nm, 250 nm, 300 nm, 300 nm, 400 nm, 450 nm, 500 nm, 550 nm, 600 nm, 650 nm, 700 nm, 750 nm, 800 nm, 850 nm, 900 nm, 950 nm, or 1000 nm. In some embodiments, the coating, or any discernible layer thereof, has a thickness of at least or is at least about 10 nm, 20 nm, 30 nm, 40 nm, 50 nm, 60 nm, 70 nm, 80 nm, 90 nm, 100 nm, 150 nm, 200 nm, 250 nm, 300 nm, 300 nm, 400 nm, 450 nm, 500 nm, 550 nm, 600 nm, 650 nm, 700 nm, 750 nm, 800 nm, 850 nm, 900 nm, 950 nm, or 1000 nm. In some embodiments, the coating thickness may be at least 10 nm, 20 nm, 30 nm, 40 nm, 50 nm, 100 nm, 200 nm, 300 nm, 400 nm, 500 nm, 600 nm, 800 nm, 1000 nm, or more. In some embodiments, the coating thickness may be at most 1000nm, 800nm, 600nm, 500nm, 400nm, 300nm, 200nm, 100nm, 50nm, 40nm, 30nm, 20nm, 10nm or less. Energy dispersive X-ray spectroscopy (EDS or EDX) can be used to determine one or more layer structures of the coating.

[0116] In some embodiments, the electromagnetic radiation source can be configured to reduce the average thickness of the coating 120 from about 1 nm to about 5 nm, from about 1 nm to about 10 nm, from about 1 nm to about 20 nm, from about 1 nm to about 30 nm, from about 1 nm to about 40 nm, from about 1 nm to about 60 nm, from about 1 nm to about 70 nm, from about 1 nm to about 80 nm, from about 1 nm to about 90 nm, or from about 1 nm to about 100 nm.

[0117] In some embodiments, the electromagnetic radiation source can be configured to ablate a portion of the array at an average depth of about 1 nm to about 5 nm, about 1 nm to about 10 nm, about 1 nm to about 20 nm, about 1 nm to about 30 nm, about 1 nm to about 40 nm, about 1 nm to about 60 nm, about 1 nm to about 70 nm, about 1 nm to about 80 nm, about 1 nm to about 90 nm, or about 1 nm to about 100 nm.

[0118] In some embodiments, the electromagnetic radiation source can be configured to remove a portion of the coating 120 or array having a thickness of about 1 μm. 2 to about 30 μm 2 , 1μm 3 to about 20 μm 2 , about 1μm 2 to about 10 μm 2 or about 1 μm 2 to about 5 μm 2 surface area.

[0119] In some embodiments, the electromagnetic radiation source can be configured to ablate a portion of the array at an average distance from about 1 nm to about 5 nm, about 1 nm to about 10 nm, about 1 nm to about 20 nm, about 1 nm to about 30 nm, about 1 nm to about 40 nm, about 1 nm to about 60 nm, about 1 nm to about 70 nm, about 1 nm to about 80 nm, about 1 nm to about 90 nm, or about 1 nm to about 100 nm from the perimeter of the microwells.

[0120] Figure 3A A top view of an example array for sorting particles including a coating is shown according to some embodiments. Figure 3B A top view of a non-limiting example array for sorting particles including a coating removed by laser is shown according to some embodiments. Figure 3A and Figure 3B , the coating 120 can absorb electromagnetic energy, which causes it to break apart from the substrate 110, which disturbs the meniscus of the fluid within each well 113 to eject the cells therein. Figure 3B Fragments of coating 120 are shown being removed from substrate 110 by electromagnetic energy. Figure 3B, the laser can be focused at or near a single hole, between two adjacent holes, or equidistant from three holes. In some embodiments, the infrared laser is focused near a single hole, between two adjacent holes, or equidistant from three holes to disturb the meniscus of the fluid in one, two, or three holes 113, respectively, to eject the cells therein. In some embodiments, focusing the laser closer to a specific hole reduces the possibility of inadvertently ejecting cells in adjacent holes. In some embodiments, at least one of the intensity and duration of the infrared laser can be configured to control the ejection of cells in one, two, or three holes.

[0121] In some embodiments, the surface material (coating 120) can be formed by sputtering material on array 100. In some embodiments, the surface material can include one or more metals (e.g., titanium, gold). The thickness of the surface material can be between 10 and 1000nm. In some embodiments, the thickness of the surface material can be at least 10nm, 20nm, 30nm, 40nm, 50nm, 100nm, 200nm, 300nm, 400nm, 500nm, 600nm, 800nm, 1000nm or larger. In some embodiments, the thickness of the surface material can be at most 1000nm, 800nm, 600nm, 500nm, 400nm, 300nm, 200nm, 100nm, 50nm, 40nm, 30nm, 20nm, 100nm or smaller. In some embodiments, the surface material can include a Ti-Au stack. The thickness of the titanium layer may be at least 10 nm, 20 nm, 30 nm, 40 nm, 50 nm, 100 nm, 200 nm or greater. The gold layer may be formed directly on the titanium layer. The thickness of the gold layer may be at least 100 nm, 200 nm, 300 nm, 400 nm, 500 nm, 600 nm, 700 nm or greater. In some embodiments, the surface material may include a titanium layer, and the gold layer may be optional.

[0122] In some embodiments, sputtering can be carried out under vacuum. In some embodiments, vacuum can be about 0.08 to about 0.02 mbar. In some embodiments, sputtering can be carried out under a voltage of about 100V to 3kV. In some embodiments, the voltage can be at least about 100V, 110V, 130V, 150V, 170V, 220V, 280V, 500V, 1000V, 2000V, 3000V or more. In some embodiments, the voltage can be at most about 3000V, 2000V, 1000V, 500V, 280V, 220V, 170V, 150V, 130V, 110V, 100V or less. In some embodiments, sputtering can be carried out under electric current: 0 to 50mA. In some embodiments, the electric current may be at least about 0.01mA, 0.1mA, 1mA, 5mA, 10mA, 20mA, 30mA, 40mA, 50mA or more. In some embodiments, the electric current may be at most about 50mA, 40mA, 30mA, 20mA, 10mA, 1mA, 0.1mA, 0.01mA or less. Optionally, in some embodiments, the surface material (coating 120) can be sputtered only on one side (111 or 112) or both sides (111 and 112) of the array. For example, in some embodiments, the surface material can be sputtered on the first side (e.g., 111) of the array. In other embodiments, the surface material can be sputtered on the second side (e.g., 112) of the glass array. In some further embodiments, the surface material can be sputtered on the first side (e.g., 111) and the second side (e.g., 112) of the array.

[0123] In some embodiments, the extraction of PBMCs includes adding a surfactant and a receiving medium to the coated array; inserting the array into a box with the coated side of the box facing down, toward the receiving medium; dropping PBMCs onto the array and allowing the PBMCs to settle into the wells. In some embodiments, the surfactant protects the integrity of the cell membrane and improves the stability under liquid shear. In some embodiments, the surfactant includes a nonionic surfactant. In some embodiments, the nonionic surfactant includes 0.1% pluoronic F68. In some embodiments, the receiving medium includes OptiPEAK T cell medium. In some embodiments, the receiving medium also includes streptavidin. In some embodiments, PBMCs are allowed to settle into the microwells for a period of about 5 minutes.

[0124] In some embodiments, infrared (IR) energy emitted from the laser and absorbed by the surface material coating 120 (e.g., Ti-Au stack, Ti layer, or Au layer) can cause the coating to spread and delaminate at the bottom edge of each microwell to extract PBMCs from each microwell. The separation of the coating at the bottom edge of each microwell disrupts the meniscus of the fluid therein to release the PBMCs.

[0125] Figure 4A is a top view of PBMCs stained with an IR energy absorbing fluorescent dye in a non-limiting example of an array including a surface material coating (eg, a Ti—Au stack, a Ti layer, or an Au layer) according to some embodiments. Figure 4B is a top view of an example of an array including a coating of a surface material after extraction of PBMCs according to some embodiments.

[0126] Beads

[0127] In certain embodiments, the holes of the array may include beads that absorb electromagnetic radiation and affect the meniscus rupture of the fluid in the hole. In some cases, the beads may be bound to the inner cavity surface of the hole or may be unbound (added to the hole in the liquid mixture). A bead including a core and a shell is provided herein. The beads of the present disclosure may be referred to as "microspheres". The core may include an infrared (IR) absorbing core. The shell may include a non-IR absorbing shell. The beads of the present disclosure may be associated with the holes of the array, and the beads may absorb electromagnetic radiation. The non-infrared absorbing shell may isolate the infrared absorbing core from nearby particles (e.g., cells), thereby protecting the particles from the destructive effects of infrared absorbed radiation on the core. The beads may also include agarose. The non-infrared absorbing shell may include agarose. The beads may also include dextran. The beads may be dyed with infrared absorbing dyes. The diameter of the beads may be equal to or less than about 20 μm, such as about 1 μm to about 20 μm, or about 5 μm to about 20 μm. The beads may include an absorbing shell that may be equal to or less than about 10 microns. In some embodiments, the surface material of the arrays described herein may include beads comprising an infrared absorbing core and a non-infrared absorbing shell, wherein the outer diameter of the non-infrared absorbing shell is equal to or less than about 10 microns.

[0128] Figure 5A An array 100 is shown including beads disposed therein. In some cases, the beads can be disposed inside the lumen of the wells. In some cases, the beads can be disposed on the first surface 111. In some cases, the beads can be disposed within the lumen of the wells. Figure 5B Shows Figure 5A100. In some embodiments, depositing the aqueous sample solution 521 onto the array 100 includes spreading the aqueous sample solution 521 onto the array 100. In some embodiments, the hydrophilic first surface 111 of the array 100 absorbs the aqueous sample solution 521 into the wells 113. In some embodiments, the hydrophilic first surface 111 of the array 100 uniformly distributes the first cells 522 and the second cells 523 within the aqueous sample solution 521 among the wells 113. In some embodiments, the hydrophilic first surface 111 of the array 100 randomly distributes the first cells 522 and the second cells 523 within the aqueous sample solution 521 among the wells 113. In some embodiments, the first cells 522 and the second cells 523 settle to the bottom of each well 113. Optionally, in some embodiments, the first cells 522 and the second cells 523 are retained in each well 113 by the surface tension of the aqueous sample solution 521.

[0129] Fig. 6A A bright field image of a microwell array filled with microspheres and cells according to some embodiments is shown. Fig. 6A As seen in FIG. 6 , each microwell 601 within array 600 may be clogged with microbeads and cells in each corresponding microwell 601 . Figure 6B A bright field image of cells extracted from a single microwell is shown according to some embodiments. Figure 6B As can be seen in FIG. 6 , only one microwell 601 in array 600 is not blocked by cells, indicating that only the cells in a single microwell 601 have been removed. Figure 6C An image of a microwell array filled with microspheres and cells according to some embodiments is shown. Figure 6C As seen in FIG. 6 , only one of the microwells 601 within array 600 contains a cell. Fig.6D An image of array 600 is shown after cells have been extracted from a single microwell, according to some embodiments. Fig.6D As can be seen in FIG. 6 , none of the microwells 601 within array 600 contain a cell, indicating that a single cell in a single microwell 601 has been removed.

[0130] Fig. 7A Example bright field images of extracted cells are shown according to some embodiments. Figure 7B Example images of extracted cells are shown according to some embodiments.

[0131] according to Figure 8 , Fig. 9 , Fig. 10A and Fig. 10B , example beads or microspheres are provided herein. Figure 8Bright field images of example agarose and dextran microspheres are shown. In some embodiments, agarose and dextran microspheres 800 are configured to absorb infrared light. In some embodiments, agarose and dextran microspheres 800 are opaque, black, or both. In some embodiments, agarose and dextran microspheres 800 include polymer shell iron oxide microspheres 800. In some embodiments, the diameter of agarose and dextran microspheres 800 is about 6um to about 20um.

[0132] Fig. 9 High magnification infrared images of example agarose and dextran microspheres are shown. Fig. 9 As seen, agarose and dextran microspheres 800 include an infrared (IR) absorbing core 910 and a non-IR absorbing shell 920. In some embodiments, the IR absorbing core 910 includes an IR absorbing dye. In some embodiments, the IR absorbing dye includes Epolight 1178. In some embodiments, the non-IR absorbing shell 920 comprises agarose and dextran.

[0133] The use of IR core-dyed particles can be advantageous for efficient cell extraction. First, the dye integrated into the molecular structure of the agarose core can increase IR absorption compared to the dye coating. In addition, the non-IR absorbing soft shell can act as a buffer layer to protect cells from stress and thermal shock associated with any potential absorbed heat, volume expansion and / or microbubble formation. Both can lead to increased extraction efficiency (greater number of successful extraction events) and high cell viability.

[0134] Fig. 10A Brightfield images of example agarose and IR dye microspheres are shown. Fig. 10B Infrared images of example agarose and IR dye microspheres are shown. Fig. 10B As seen, agarose and IR dye microspheres 1000 can be infrared (IR) absorbing. In some embodiments, agarose and IR dye microspheres 1000 comprise agarose. In some embodiments, agarose and IR dye microspheres 1000 comprise IR absorbing dyes. In some embodiments, IR absorbing dyes include Epolight. In some embodiments, the dye comprises green fluorescent protein. In some embodiments, the dye comprises red fluorescent protein. In some embodiments, the dye comprises cyanine dyes, acridine dyes, fluorone dyes, oxazine dyes, rhodamine dyes, coumarin dyes, phenanthridine dyes, BODIPY dyes, ALEXA dyes, perylene dyes, anthracene dyes, naphthalene dyes, and the like. In some embodiments, the diameter of agarose and IR dye microspheres 1000 is about 2 μm to about 16 μm.

[0135] Fig.11A and Fig. 11B An example procedure for modifying all or part of one or more surfaces of substrate 110 is shown. In some embodiments, the bottom surface and a portion of the vertical sidewalls of the well plate may first be coated with a surface coating (step 1111), such as Fig. 13B and / or Fig. 13C The surface coating may include one or more thermally or electrically conductive materials. Step 1111 may include metal deposition. The surface coating may include one or more metals selected from chromium, titanium, gold, iron, nickel, copper, platinum, and palladium. The surface coating may include one or more metal layers (e.g. Fig. 13C 1320 and 1322 shown in ), each layer is independently selected from chromium, titanium, gold, iron, nickel, copper, platinum, palladium, any mixture thereof and any alloy thereof. The surface coating may include a metal layer and an adhesion layer for the metal layer below. The adhesion layer can be used to promote adhesion to the substrate material. The surface coating may include a gold layer and a gold adhesion layer (such as chromium, titanium, nickel or nickel-chromium) below the gold. Surface coating (step 1111) can be performed using any suitable coating method, such as sputtering, spin coating, chemical vapor deposition (CVD), physical vapor deposition, pulsed laser deposition, atomic layer deposition, low-pressure CVD or any combination thereof. In some embodiments, the surface coating may be the same as coating 120. In some embodiments, the coating process (step 1111) may include metal deposition. In some cases, the metal coating may include one or more metals (e.g., Cr, Ni, Ti, Au). In some embodiments, the metal coating may include a Ti-Au stack. In some embodiments, the metal coating may include a Cr-Au stack. In some embodiments, the metal coating may include a Ni-Au stack.

[0136] Next, the surface of the orifice plate can then be cleaned and / or activated by physical or chemical means (step 1113), such as by plasma cleaning, by immersing the plate in an alkaline solution or a combination thereof. Physical or chemical means (step 1113) can enhance the attachment of subsequent layers on the coating obtained from step 1111. In some embodiments, the alkaline solution may include NaOH with a predetermined concentration. In some embodiments, the predetermined concentration may be about 1M to 3M. In some embodiments, the predetermined concentration may be or may be about, any range between any two of 3M, 2.5M, 2M, 1.5M, 1M or the aforementioned values ​​(including). In some embodiments, the predetermined concentration may be at least 1M, 1.5M, 2M, 2.5M, 3M or greater. In some embodiments, the predetermined concentration may be at most 3M, 2.5M, 2M, 1.5M, 1M or less. In some embodiments, the orifice plate may be immersed in an alkaline solution for a predetermined period of time. In some embodiments, the predetermined period of time may be between about 15 minutes and 12 hours. In some embodiments, the predetermined time period can be at most 12 hours, 10 hours, 8 hours, 7 hours, 6 hours, 5 hours, 4 hours, 3 hours, 2 hours, 1 hour, 50 minutes, 40 minutes, 35 minutes, 30 minutes, 25 minutes, 20 minutes, 15 minutes or less. In some embodiments, the predetermined time period can be at least 15 minutes, 20 minutes, 25 minutes, 30 minutes, 35 minutes, 40 minutes, 50 minutes, 1 hour, 2 hours, 3 hours, 4 hours, 5 hours, 6 hours, 8 hours, 10 hours, 12 hours or more.

[0137] Next, the orifice plate may then be cleaned to remove impurities, such as residual alkaline solution, by, for example, washing with deionized water (step 1115). The orifice plate may be dried using, for example, pressurized air from a pressurized air gun.

[0138] In some embodiments, orifice plate can carry out plasma cleaning with any suitable plasma in chamber for a predetermined time period.Suitable plasma can be argon plasma, compressed air plasma, plasma or vacuum plasma based on flame.The predetermined time period can be or can be about, 10 seconds, 20 seconds, 30 seconds, 40 seconds, 50 seconds, 1 minute, 70 seconds, 80 seconds, 90 seconds, 100 seconds, 110 seconds, 2 minutes, 130 seconds, 140 seconds, 150 seconds, 160 seconds, 170 seconds, 3 minutes, 3.5 minutes, 4 minutes, 4.5 minutes, 5 minutes, 5.5 minutes, 6 minutes, 6.5 minutes, 7 minutes, 7.5 minutes, 8 minutes, 8.5 minutes, 9 minutes, 9.5 minutes, 10 minutes, 11 minutes, 12 minutes, 13 minutes, 14 minutes or 15 minutes or any two of the aforementioned values ​​between any scope (including). The predetermined time period may be at least or at least about, 10 seconds, 20 seconds, 30 seconds, 40 seconds, 50 seconds, 1 minute, 70 seconds, 80 seconds, 90 seconds, 100 seconds, 110 seconds, 2 minutes, 130 seconds, 140 seconds, 150 seconds, 160 seconds, 170 seconds, 3 minutes, 3.5 minutes, 4 minutes, 4.5 minutes, 5 minutes, 5.5 minutes, 6 minutes, 6.5 minutes, 7 minutes, 7.5 minutes, 8 minutes, 8.5 minutes, 9 minutes, 9.5 minutes, 10 minutes, 11 minutes, 12 minutes, 13 minutes, 14 minutes or 15 minutes. The predetermined time period may be at most or at most about, 10 seconds, 20 seconds, 30 seconds, 40 seconds, 50 seconds, 1 minute, 70 seconds, 80 seconds, 90 seconds, 100 seconds, 110 seconds, 2 minutes, 130 seconds, 140 seconds, 150 seconds, 160 seconds, 170 seconds, 3 minutes, 3.5 minutes, 4 minutes, 4.5 minutes, 5 minutes, 5.5 minutes, 6 minutes, 6.5 minutes, 7 minutes, 7.5 minutes, 8 minutes, 8.5 minutes, 9 minutes, 9.5 minutes, 10 minutes, 11 minutes, 12 minutes, 13 minutes, 14 minutes, or 15 minutes. The chamber used for plasma cleaning may be an ultra-high vacuum (UHV) chamber.

[0139] In some embodiments, the orifice plate after step 1113 can be washed in one or more passes using one or more washing liquids (step 1115). In each pass, the washing liquid can be independently selected from water, alcohol (such as methanol, ethanol, isopropanol, butanol), acetonitrile, acetone, toluene, and mixtures thereof. Each pass can independently last for a predetermined period of time. The predetermined time period may be, or may be about, 10 seconds, 20 seconds, 30 seconds, 40 seconds, 50 seconds, 1 minute, 70 seconds, 80 seconds, 90 seconds, 100 seconds, 110 seconds, 2 minutes, 130 seconds, 140 seconds, 150 seconds, 160 seconds, 170 seconds, 3 minutes, 3.5 minutes, 4 minutes, 4.5 minutes, 5 minutes, 5.5 minutes, 6 minutes, 6.5 minutes, 7 minutes, 7.5 minutes, 8 minutes, 8.5 minutes, 9 minutes, 9.5 minutes, 10 minutes, 11 minutes, 12 minutes, 13 minutes, 14 minutes, 15 minutes, 20 minutes, 25 minutes, 30 minutes, 35 minutes, 40 minutes, 45 minutes, 50 minutes, 55 minutes, or 1 hour, or any range between, inclusive, any two of the foregoing values. The predetermined time period may be at least or may be at least about, 10 seconds, 20 seconds, 30 seconds, 40 seconds, 50 seconds, 1 minute, 70 seconds, 80 seconds, 90 seconds, 100 seconds, 110 seconds, 2 minutes, 130 seconds, 140 seconds, 150 seconds, 160 seconds, 170 seconds, 3 minutes, 3.5 minutes, 4 minutes, 4.5 minutes, 5 minutes, 5.5 minutes, 6 minutes, 6.5 minutes, 7 minutes, 7.5 minutes, 8 minutes, 8.5 minutes, 9 minutes, 9.5 minutes, 10 minutes, 11 minutes, 12 minutes, 13 minutes, 14 minutes, 15 minutes, 20 minutes, 25 minutes, 30 minutes, 35 minutes, 40 minutes, 45 minutes, 50 minutes, 55 minutes or 1 hour. The predetermined time period may be at most or may be at most about, 10 seconds, 20 seconds, 30 seconds, 40 seconds, 50 seconds, 1 minute, 70 seconds, 80 seconds, 90 seconds, 100 seconds, 110 seconds, 2 minutes, 130 seconds, 140 seconds, 150 seconds, 160 seconds, 170 seconds, 3 minutes, 3.5 minutes, 4 minutes, 4.5 minutes, 5 minutes, 5.5 minutes, 6 minutes, 6.5 minutes, 7 minutes, 7.5 minutes, 8 minutes, 8.5 minutes, 9 minutes, 9.5 minutes, 10 minutes, 11 minutes, 12 minutes, 13 minutes, 14 minutes, 15 minutes, 20 minutes, 25 minutes, 30 minutes, 35 minutes, 40 minutes, 45 minutes, 50 minutes, 55 minutes or 1 hour.

[0140] In some embodiments, the well plate with the activated and cleaned surface ready for surface functionalization (after step 1115) can then be coated with one or more surface modifying materials (step 1117). The one or more surface modifying materials can include one or more polymers. The one or more surface modifying materials can include one or more hydrophilic materials (such as one or more hydrophilic oligomers or one or more hydrophilic polymers), one or more hydrophobic materials (such as one or more hydrophobic oligomers or one or more hydrophobic polymers), or any combination thereof.

[0141] In some embodiments, a portion of the vertical sidewall of the orifice plate (e.g., the sidewall of hole 113) can be functionalized with hydrophilic oligomers or polymers such as polyethylene glycol (PEG), poly (hydroxyethyl methacrylate) (PHEMA), polyacrylamide (PAM), polyacrylic acid (PAA), polyvinyl pyrrolidone (PVP), polysaccharides, polylactic acid (PLA), etc. The hydrophilic oligomer or polymer can be linear or branched. The hydrophilic oligomer or polymer can include a first end group. The hydrophilic oligomer or polymer including the first end group can include a second end group. One of the first end group and the second end group can be configured to react with an activated and cleaned surface, or to form a self-assembled layer thereon (after step 1117), and the other of the first end group and the second end group (if present) can be configured to remain on the hydrophilic oligomer or polymer after surface functionalization. The first end group or the second end group configured to remain on the hydrophilic oligomer or polymer after surface functionalization can be an alkoxy group (e.g., methoxy, ethoxy), a hydroxyl group, an amine, or an ionic hydrophilic group. The first end group or the second end group configured to react with the activated and cleaned surface or to form a self-assembled layer thereon (after step 1117) can be selected from silane, thiol, primary amine (-NH2), carboxylic acid (-COOH), aldehyde, vinyl, epoxy, and chloro. The first end group or the second end group configured to react with the activated and cleaned surface or to form a self-assembled layer thereon (after step 1117) can be a silane or thiol. After step 1117, the vertical sidewalls of the orifice plate can be functionalized by a hydrophilic oligomer or polymer (such as poly (ethylene glycol) (PEG)) terminated by an alkoxy group (such as a methoxy group) at the end. The hydrophilic oligomer or polymer having a first end and a second end may be a functionalized PEG, such as silane-PEG-methoxy (PEG-silane) or thiol-PEG-methoxy (PEG-SH).

[0142] In some embodiments, the hydrophilic oligomer or polymer (such as PEG-silane or PEG-SH) has a molecular weight of or about 250, 500, 750, 1000, 1250, 1500, 1750, 2000, 2250, 2500, 2750, 3000, 3250, 3500, 3750, 4000, 4250, 4500, 4750, 5000, 5250, 5500, 5750, or 6000 Daltons, or any range between any two of the foregoing values. In some embodiments, the hydrophilic oligomer or polymer (such as PEG-silane or PEG-SH) has a molecular weight of at least or at least about 250, 500, 750, 1000, 1250, 1500, 1750, 2000, 2250, 2500, 2750, 3000, 3250, 3500, 3750, 4000, 4250, 4500, 4750, 5000, 5250, 5500, 5750, or 6000 Daltons. In some embodiments, the hydrophilic oligomer or polymer (such as PEG-silane or PEG-SH) has a molecular weight of at most or at most about 250, 500, 750, 1000, 1250, 1500, 1750, 2000, 2250, 2500, 2750, 3000, 3250, 3500, 3750, 4000, 4250, 4500, 4750, 5000, 5250, 5500, 5750, or 6000 Daltons. In some embodiments, the PEG-silane used in step 1117 can be a solution dissolved in an alcohol (e.g., ethanol), for example, 0.5 g / 100 mL PEG-silane. In some embodiments, the functionalized PEG can include methoxy-poly(ethylene glycol)-thiol (PEG-SH). In some embodiments, PEG-SH can be a solution dissolved in an alcohol (e.g., dehydratase ethanol), such as 0.5 g / 100 mL PEG-SH. In some embodiments, a hydrophilic oligomer or polymer (such as a functionalized PEG) can be configured to reduce nonspecific binding of charged particles (e.g., cells) to different surfaces of the orifice plate 113, such as adhesion. The silane groups present in the PEG-silane can promote selective affinity to the glass surface of the orifice plate. The thiol groups present in the PEG-SH can promote selective affinity to the orifice plate surface coated with a transition metal (e.g., Ti-Au). In some embodiments, PEG-SH can be specifically attached to the metal coating portion of the substrate 110, such as Ti-Au. In some embodiments, PEG-silane can be specifically attached to the glass portion of the substrate 110 without any metal coating.

[0143] Fig. 12A A top view of the array 100 is shown, and Fig. 12BA cross-sectional view of an array according to some embodiments is shown. Fig. 12B The diagram illustrates that one or more surface modifying materials (such as one or more hydrophilic materials) can be added to a first portion and a second portion of substrate 110. In some embodiments, the first portion can be a top portion of substrate 110, which is a portion closer to surface 112. In some embodiments, the second portion can be a bottom portion of substrate 110, which is a portion closer to surface 111. In some embodiments, the first portion of substrate 110 (e.g., Fig. 13B The portions of the vertical sidewalls not covered by 1320 / 1322 in the well 113) can be coated with a material 1231 to change the surface properties of the substrate 110. The surface material 1231 may include a hydrophilic material, such as a hydrophilic oligomer or polymer (such as a functionalized PEG), as described above. In some embodiments, the surface material 1231 may be a functionalized PEG, for example, a PEG-silane (such as described above with respect to FIG. 11 or anywhere else herein). In some embodiments, the functionalized PEG can reduce non-specific binding (e.g., adhesion) of charged particles (e.g., cells) to the walls of the well 113. In some embodiments, the silane groups in the PEG-silane can be used to change the surface properties of the glass portion of the substrate 110. In some embodiments, the second portion (bottom portion) of the substrate 110 can be coated with a plurality of materials 1300, as described in reference to Figures 13A-13D Described in more detail.

[0144] Figures 13A-13D A method for forming a multilayer coating 1300 on a bottom portion of a substrate 110 (see Fig.13D 11 or any other place described herein). In some embodiments, the multilayer coating 1300 can enhance or change the surface properties of the substrate 110. In addition, the multilayer coating 1300 can, in some cases, delaminate and simultaneously destroy the meniscus of the liquid held in the microwell array. In some embodiments, the multilayer coating 1300 or at least one or more portions of the coating 1300 can be destroyed using electromagnetic radiation (e.g., laser).

[0145] In some embodiments, the first layer 1320 may be formed on the surface of the substrate 110, such as Fig. 13B In some embodiments, the first layer may include a transition metal, such as Au, Ti, or Cr. Optionally, in some embodiments, the second layer 1322 may be formed on the first layer 1320, such as Fig. 13CIn some embodiments, the second layer can be a material different from the first layer. In some embodiments, the second layer can include a noble metal, such as Au. In some embodiments, the first layer can help to attach at least one or more subsequent coating material layers to the substrate. In some embodiments, the first layer can be titanium, which can promote the attachment of the second layer (e.g., gold) of different coating materials. In some embodiments, the second layer (e.g., gold) can be coated with other materials, such as polymers. As an example, thiol (-SH) groups have a high affinity for gold. In some embodiments, the second layer (e.g., gold) can be suitable for surface functionalization, such as by using thiol (-SH) derivatives of functional surface coating materials, such as PEG-SH.

[0146] Then, if Fig.13D As shown in , a third layer 1332 covering the vertical sidewall portion of the hole (e.g., extending along the Z axis) can be formed. The vertical sidewall portion may include a first layer 1320 and / or a second layer 1322 (such as described above with respect to FIG. 11 or described anywhere else herein). The first and / or second layer 1320 / 1322 may include a Ti layer, a Ti-Au stack, or an Au layer. In some embodiments, the third layer 1332 may include a polymer. In some embodiments, the polymer may include PEG or a derivative of PEG, such as PEG-thiol. The thiol groups present in PEG-SH may promote selective affinity to the surface of the orifice plate coated with a metal (e.g., Ti-Au). In some embodiments, functionalized PEG may reduce nonspecific binding (e.g., adhesion) of charged particles (e.g., cells) to the wall of the hole 113.

[0147] In some embodiments, such as in Fig.13D As shown in FIG. 1 , a fourth layer 1333 covering a bottom portion of the substrate may be formed on the first layer 1320 and / or the second layer 1322. The bottom portion may be adjacent to a vertical sidewall of the hole. The fourth layer 1333 may be formed along Fig.13DThe Y-axis shown in extends. In some embodiments, the fourth layer 1333 may include an oligomer or polymer. In some embodiments, the fourth layer may include a hydrophobic oligomer or polymer, such as a fluorinated or perfluorinated oligomer or polymer. Fluorinated or perfluorinated oligomers or polymers may be formed by monomers selected from fluorinated dioxoles, fluorinated dioxolanes, fluorinated cyclopolymerizable alkyl ethers and combinations thereof. Fluorinated or perfluorinated oligomers or polymers may be perfluoroalkyl thiols, such as perfluorohexanethiol, perfluorooctanethiol or perfluorodecanethiol. Fluorinated or perfluorinated oligomers or polymers may include 1H, 1H, 2H, 2H-perfluorodecanethiol (PF-SH). The thiol groups present in PF-SH may have a high affinity for a previous coating (e.g., gold). Hydrophobic oligomers or polymers may be linear or branched. Hydrophobic oligomers or polymers may include a first end group. The hydrophobic oligomer or polymer comprising the first end group may include the second end group. One of the first end group and the second end group may be configured to react with the surface of activation and cleaning or to form a self-assembled layer (such as a monolayer) thereon (after step 1117), and another one of the first end group and the second end group (if present) may be configured to remain on the hydrophobic oligomer or polymer after surface functionalization. The first end group or the second end group configured to react with the surface of activation and cleaning or to form a self-assembled layer thereon may be selected from silane, thiol, primary amine (-NH2), carboxylic acid (-COOH), aldehyde, vinyl, epoxy and chloro. The first end group or the second end group configured to react with the surface of activation and cleaning or to form a self-assembled layer thereon (after step 1117) may be thiol. The hydrophobic oligomer or polymer, such as a fluorinated or perfluorinated oligomer or polymer, can have a molecular weight of or about 250, 480, 500, 750, 1000, 1250, 1500, 1750, 2000, 2250, 2500, 2750, 3000, 3250, 3500, 3750, 4000, 4250, 4500, 4750, 5000, 5250, 5500, 5750, or 6000 Daltons, or any range between any two of the foregoing values. The hydrophobic oligomer or polymer, such as a fluorinated or perfluorinated oligomer or polymer, may have a molecular weight of at least or at least about 250, 480, 500, 750, 1000, 1250, 1500, 1750, 2000, 2250, 2500, 2750, 3000, 3250, 3500, 3750, 4000, 4250, 4500, 4750, 5000, 5250, 5500, 5750, or 6000 Daltons.Hydrophobic oligomers or polymers (such as fluorinated or perfluorinated oligomers or polymers) can have a molecular weight of up to or about 250, 480, 500, 750, 1000, 1250, 1500, 1750, 2000, 2250, 2500, 2750, 3000, 3250, 3500, 3750, 4000, 4250, 4500, 4750, 5000, 5250, 5500, 5750, or 6000 daltons. In some embodiments, the hydrophobic surface coating can form a self-assembled monolayer (SAM). In some embodiments, the self-assembled monolayer can reduce wettability. In some embodiments, the self-assembled monolayer can reduce surface energy. In some embodiments, the hydrophobic surface coating, such as PF-SH, can have a water contact angle of about 120 °. In some embodiments, the hydrophobic surface coating, such as PF-SH, can have a water contact angle of 90° to 150°. In some embodiments, the hydrophobic surface coating, such as PF-SH, can have a water contact angle of 100°, 105°, 110°, or 115°. In some embodiments, the hydrophobic coating can be used as a sealing layer. In some embodiments, the sealing layer can prevent leakage from the end of the hole on the surface 111. In some embodiments, the thiol group can improve the adhesion of the hydrophobic coating (such as PF-SH) to the lower surface (such as Au in Ti-Au).

[0148] In some embodiments, the surface material 1320 and / or 1322 (such as described above with respect to FIG. 11 or described anywhere else herein) can be applied to the surface of the substrate 110 by metal sputtering. In some embodiments, the thickness of the surface material 1320 and / or 1322 can be from 10 nm to 1000 nm. In some embodiments, the thickness of the surface material 1320 and / or 1322 can be at least 10 nm, 20 nm, 30 nm, 40 nm, 50 nm, 100 nm, 200 nm, 300 nm, 400 nm, 500 nm, 600 nm, 800 nm, 1000 nm, or more. In some embodiments, the thickness of surface material 1320 and / or 1322 may be at most about 1000 nm, 800 nm, 600 nm, 500 nm, 400 nm, 300 nm, 200 nm, 100 nm, 50 nm, 40 nm, 30 nm, 20 nm, 10 nm, or less.

[0149] In some embodiments, sputtering can be carried out under vacuum. In some embodiments, vacuum can be about 0.08 to about 0.02 mbar. In some embodiments, vacuum can be at most about 0.01 mbar, 0.02 mbar, 0.03 mbar, 0.04 mbar, 0.05 mbar, 0.06 mbar, 0.07 mbar, 0.08 mbar, 0.09 mbar, 0.1 mbar or less. In some embodiments, vacuum can be at least about 0.1 mbar, 0.09 mbar, 0.08 mbar, 0.07 mbar, 0.06 mbar, 0.05 mbar, 0.04 mbar, 0.03 mbar, 0.02 mbar, 0.01 mbar or more. In some embodiments, sputtering can be carried out at a voltage of about 100V to 3kV. In some embodiments, the voltage may be at least about 100V, 110V, 130V, 150V, 170V, 220V, 280V, 500V, 1000V, 2000V, 3000V or more. In some embodiments, the voltage may be at most about 3000V, 2000V, 1000V, 500V, 280V, 220V, 170V, 150V, 130V, 110V, 100V or less. In some embodiments, sputtering can be carried out at a current of 0 to 50mA. In some embodiments, the current may be at least about 0.01mA, 0.1mA, 1mA, 5mA, 10mA, 20mA, 30mA, 40mA, 50mA or more. In some embodiments, the current may be at most about 50 mA, 40 mA, 30 mA, 20 mA, 10 mA, 1 mA, 0.1 mA, 0.01 mA, or less. In some embodiments, the surface material may be sputtered on one or both sides of the glass array (e.g., the top and / or bottom of the plate).

[0150] Also provided herein is a method for forming infrared absorbing beads. In some embodiments, the method includes: washing agarose beads; dyeing agarose beads; and forming the core of agarose beads. In some embodiments, washing agarose beads includes suspending agarose beads in a first solvent and centrifuging agarose beads and the first solvent. In some embodiments, the first solvent includes an organic solvent (e.g., acetone), or an aqueous solvent (e.g., water) or a combination thereof. In some embodiments, centrifugation can be performed at a speed of about 1,000 rpm to about 4,000 rpm. In some embodiments, centrifugation can be performed at a speed of about 2,000 rpm. In some embodiments, 1 mL of the first solvent can be used for every 50 mg of agarose beads. In some embodiments, agarose beads include Superdex beads.

[0151] In some embodiments, dyeing agarose beads includes: forming a dyeing solution, centrifuging the dyeing solution, and adding the dyeing solution to agarose beads. The dyeing solution can include Epolin 1178 and a second solvent. In some embodiments, the second solvent includes acetone, water, deionized water, or any combination thereof. Centrifugation can be performed at a speed of about 2,000rpm to about 10,000rpm, for example, about 5,000rpm. In some embodiments, dyeing agarose beads also includes incubating agarose beads and the dyeing solution. Incubation can be performed for about 15 minutes to about 1 hour, for example, about 30 minutes. In some embodiments, incubation can be performed at room temperature. Incubation can be performed under continuous mixing. In some embodiments, dyeing agarose beads also includes centrifuging agarose beads after incubation, for example, at a speed of about 750rpm to about 3,000rpm. In some embodiments, dyeing agarose beads also includes separating dark beads from bright beads. In some embodiments, staining the agarose beads further comprises suspending the agarose beads in 0.2% BSA-PBS.

[0152] In some embodiments, forming the core of the agarose beads comprises suspending the agarose beads in a third solvent and centrifuging the agarose beads and the third solvent. In some embodiments, the third solvent comprises a 1:1 acetone-water mixture. In some embodiments, centrifugation can be performed at a rate of about 500 rpm to about 2,000 rpm. In some embodiments, centrifugation can be performed for about 10 seconds to about 60 seconds.

[0153] Alternatively, in some embodiments, forming the core of the agarose bead comprises incubating the beads in a buffer. In some embodiments, the buffer comprises BSA-PBS. In some embodiments, the buffer has a concentration of about 0.2%. In some embodiments, the beads may be incubated in the buffer at a temperature of about 4°C. In some embodiments, the beads may be incubated in the buffer for a period of at least about 5 days. Forming the core of the agarose bead may also comprise changing the buffer every day.

[0154] Provided herein is a solution comprising a plurality of beads as described herein and a target particle as described herein. In some cases, the target particle is a cell. In some cases, the solution has a ratio of the number of a plurality of beads to the number of a plurality of cells of about 1:1 to 10:1. The solution comprising the target particle can be embedded in one or more holes of an array as described herein. Exemplary solutions are further described with respect to Examples 5 and 6.

[0155] system

[0156] Another aspect provided herein is a system for sorting particles. A system for sorting mixture components is provided herein. The system may include any embodiment, variation or example of an array as described herein.

[0157] Fig.14A A system is shown including an array 100, a housing 1431, and an inner surface 1432. A system for sorting particles may include an array 100, the array 100 including: a substrate 110 including a first surface 111; a second surface 112 opposite the first surface 111; and a plurality of holes 113 extending from the first surface 111 to the second surface 112, each hole 113 having a cross-sectional area equal to or less than about 1 square millimeter and a length equal to or less than about 10 mm, wherein the substrate 110 comprises a first material; and a coating 120 operably coupled to the second surface 112, wherein the coating 120 comprises a second material different from the first material, and wherein a portion of the coating 120 may be configured to be disrupted from the second surface 112 in response to electromagnetic radiation directed at a portion of the coating 120; and a fluid within the plurality of holes 113 of the array 100, wherein a meniscus of the fluid within the plurality of holes 113 is substantially adjacent to the coating 120.

[0158] In some embodiments, the first surface 111 or the second surface 112 may be hydrophilic. In some embodiments, the first surface 111 or the second surface 112 may be coupled to a hydrophilic coating 120. In some embodiments, the coating 120 may be hydrophobic. In some embodiments, the coating 120 may be capable of preventing leakage from the hole for a period of time equal to or greater than 1 hour. In some embodiments, the coating 120 covers the first surface 111 or the second surface 112 in its entirety.

[0159] In some embodiments, the surface coating material may be titanium. In some embodiments, the surface coating material includes silver, gold, aluminum, copper, platinum, nickel, or cobalt. In some embodiments, the substrate material may be glass. In some embodiments, the cross-sectional area may be equal to or less than about 0.03 mm 2 In some embodiments, the length may be equal to or less than about 1.5 mm. In some embodiments, coating 120 has a thickness equal to or less than about 200 nm. In some embodiments, substrate 110 has a thickness of about 0.5 nm. -1In some embodiments, a portion of coating 120 may be configured to absorb electromagnetic radiation and detach from second surface 112 in response to electromagnetic radiation directed to the portion of coating 120. In some embodiments, a plurality of micropores 113 are orthogonal to first surface 111 and second surface 112. In some embodiments, a plurality of micropores 113 are substantially parallel to each other. In some embodiments, a plurality of micropores 113 are from about 1 million to about 100 billion micropores 113. In some embodiments, the second material is opaque. The second material may be configured to absorb infrared (IR) energy. Substrate 110 and coating 120 may have different coefficients of thermal expansion.

[0160] Optionally, the system can further include a housing 1431 including an inner surface 1432 configured to receive selected contents released from the array. The system can include any embodiment, variation, or example of an array as described herein, and a housing including an inner surface. The inner surface can be located below the second surface of the substrate. The system can further include a cell sorter. The array is mounted on the cell sorter.

[0161] Optionally, the system for sorting particles may include a source of electromagnetic radiation.

[0162] Fig. 14B A system for sorting particles is shown, the system comprising an array 100 and an electromagnetic radiation source 1451. The array can be configured to be damaged at a first surface or a second surface in response to electromagnetic radiation directed to a portion of the first surface or the second surface. In some cases, it is beneficial to enable a sorting system to release particles held in a particular compartment of the array without directing a laser or other energy source directly to the compartment holding the target particle (e.g., when the target particle is a cell, it helps to increase cell viability). Focusing the laser energy on the surface of the array rather than the interior of the pores of the array can avoid or reduce possible damage to the pore contents due to thermal shock, thermal expansion, microbubble generation, and local shear stress.

[0163] The source generating electromagnetic radiation may include a laser. The laser may be a doped solid-state laser. The laser may be a fiber laser. The laser may be a semiconductor diode laser. The laser may be a gas laser, such as a HeNe laser or an excimer laser. The laser may emit electromagnetic radiation within a wavelength range. In some embodiments, the electromagnetic radiation may be emitted within the visible and / or infrared range. The electromagnetic radiation may then be emitted within a 5 nanometer band within the visible or infrared range. The electromagnetic radiation may be emitted as a harmonic of a doped solid-state laser, such as doped ytterbium orthovanadate or ytterbium aluminum garnet. The electromagnetic radiation may include 1064nm radiation.

[0164] The electromagnetic radiation may include incident energy. The incident energy may be greater than 0.1 microjoules per pulse. The incident energy may be less than 1 millijoule per pulse. The incident energy may be in the range of 1 picojoule per pulse to 1 joule per pulse. The average power may be less than 10 watts. The average power may be less than 100 milliwatts. The average power may be greater than 1 microwatt.

[0165] The electromagnetic radiation may have an incident peak power density. The peak power density may be less than 10 terawatts per square centimeter. The peak power may be less than 10 gigawatts per square centimeter.

[0166] The electromagnetic radiation may have an incident spot diameter. The spot diameter may be small enough so that an area adjacent to the aperture may be irradiated without significantly irradiating the cell contents. The spot diameter may be adjusted based on the size of the aperture and the aperture spacing. The spot diameter may be small enough so that an inner wall of the aperture lumen may be irradiated without significantly irradiating the aperture contents (such as cells inside the lumen). The spot diameter may be less than 10 millimeters (mm), less than 1 millimeter, less than 100 micrometers (μm), less than 10 μm, or less.

[0167] The electromagnetic radiation may have an incident pulse duration. The pulse duration may be greater than about 5 femtoseconds. The pulse duration may be greater than about 100 femtoseconds. The pulse duration may be greater than about 1 nanosecond or longer. The pulse duration may be less than about 1 microsecond.

[0168] Exemplary electromagnetic radiation sources include a source with a power of 0.1 mJ and a power density of 10 8 -10 9 W / mm 2 A 1064 nm Ytterbium fiber laser with a spot diameter of 20 μm is capable of delivering 30-90 J / cm to the array at 10%-30% of the maximum laser power with a pulse duration of 4 ns. 2 .

[0169] The system may further include one or more lenses for focusing the electromagnetic radiation source. The one or more lenses may include a microscope objective. The microscope objective may be raster scanned over the surface of the array to target a specific portion of the array. The system may include one or more translation stages that may control the positioning of the objective relative to the array surface.

[0170] The system may include one or more beam splitters, filters or dichroic filters. A system including one or more beam splitters, filters or dichroic filters may allow a user to monitor the surface of the array while aligning or directing an electromagnetic radiation source to the surface of the array. Alignment may be performed at a lower power than would damage the array or at the same power of electromagnetic radiation. The system may include one or more position-sensitive optical detectors, such as a CCD, to monitor the alignment of the electromagnetic radiation source.

[0171] The system may include a second electromagnetic radiation source. The second electromagnetic radiation source may be used for alignment. The second electromagnetic radiation source may be used to excite an absorber such as a fluorophore. The second electromagnetic radiation source may be coherent or incoherent. The second electromagnetic radiation source may be broadband or narrowband. The second electromagnetic radiation source may have any of the properties described herein for electromagnetic radiation sources, such as power, pulse duration, wavelength, etc.

[0172] Fig.15A and Fig. 15B An example system 1400 is shown that includes an array and a housing. Fig.15A is a top down initial view of the leak test at 0 hours. Fig.18 B is a top down initial view of the leak test of an example array at 5 hours. FIG. 15A to FIG. 15B , the example array 100 in the frame 1510 was leak tested with deionized water over a period of about 5 hours, wherein no deionized water leaked through the micropores of the array. In some embodiments, the coating of the example array 100 is capable of preventing leakage from the pores for a period of time equal to or greater than about 1 hour. In some embodiments, the coating of the example array 100 is capable of preventing leakage from the pores for a period of time equal to or greater than about 1 hour, 2 hours, 3 hours, 4 hours, 5 hours, 6 hours, 7 hours, 8 hours, 9 hours, or 10 hours.

[0173] method

[0174] Embodiments, examples, and variations of the arrays described herein can be used in methods for releasing particles from the holes of the array. Embodiments, examples, and variations of the systems described herein can be used in methods for releasing particles from the holes of the array. A method for releasing particles from the holes of the array is provided herein, the method comprising: filling the holes, retaining a portion of the solution in the holes, directing electromagnetic radiation to a portion of the array, destroying a portion of the array, and releasing a portion of the solution containing the target particle. The holes can be filled with at least a portion of the solution. The solution can contain the target particle. A portion of the solution can be retained in the holes by surface tension. Destroying a portion of the array can destroy the surface tension of a portion of the solution retained in the holes.

[0175] Provided herein is a method for releasing selected contents from holes in an array, the method comprising: identifying holes in an array having selected contents, wherein the array comprises a substrate having a first surface and a second surface opposite to the first surface, wherein the substrate comprises a substrate material and a surface material, wherein the surface material is located at or adjacent to the first surface or the second surface, and the substrate comprises a plurality of holes defining an inner cavity extending from the first surface to the second surface, wherein the substrate is characterized by one or more of the following: (a) a maximum diameter of each of the plurality of holes is 500 microns or less; (b) an aspect ratio of each of the plurality of holes is 10 or greater; (c) a hole density of 100 or more holes per square millimeter, and (d) the surface material is selected from materials that absorb greater than 10% of incident electromagnetic radiation; and removing a portion of the surface material from the first surface or the second surface of the array using electromagnetic radiation directed to the surface material within or adjacent to the identified hole, thereby releasing the contents of the identified hole.

[0176] In some examples, the array can be characterized by two or more of the following: (a) a maximum diameter of each of the plurality of holes is 500 microns or less, (b) an aspect ratio of each of the plurality of holes is 10 or greater; (c) a hole density of 100 or more holes per square millimeter; and (d) a surface material selected from materials that absorb greater than 10% of incident electromagnetic radiation.

[0177] Figures 16A-16F As described herein, the use of Figure 1A A side cross-sectional view of an example method for sorting cells from an example array. Figures 16A-16F , an example method 1600 for sorting cells using an example first array 100 includes providing 1610 an array 100 including a plurality of wells 113. In some embodiments, operation 1610 may also include sorting cells according to Figure 5A Covering a portion of the first surface 111 of the array 100 closest to the wells 113 with microspheres. Operation 1620 of method 1600 may include depositing an aqueous solution 1621 within the array. In some cases, according to Fig. 16B , the array may include depositing first cells 1622 and second cells 1623 onto the first array 100. Fig. 16C , operation 1630 of method 1600 may include inserting array 100 into housing 1631. In some cases, the housing may include a box. The housing may include inner surface 1632. Operation 1640 of method 100 may include capturing a signal plot of the selected particle. Fig.16D , the selected particles may include a first cell 1622 and a second cell 1623. Fig.16E, the method 1600 may further include locating 1640 the signal map of the first cell 1622 within the signal map of the first cell and the second cell 1623. The method 1600 may further include extracting 1640 the second cell 1623 from the array 100; and Fig.16F , collecting 1650 second cells 1623. The step of extracting cells from the array may include disrupting a coating on or near the surface of the array 100. The step of disrupting may include providing electromagnetic radiation to the surface of the array at selected locations. Fig.16A A side cross-sectional view of providing an array including a plurality of holes including a coating according to an example method is shown.

[0178] Fig. 16B A side cross-sectional view of depositing an aqueous sample solution within the example array of FIG1 is shown. In some embodiments, depositing 1620 an aqueous sample solution 1621 onto the array 100 includes spreading the aqueous sample solution 1621 onto the array 100. In some embodiments, the hydrophilic second surface 112 of the array 100 absorbs the aqueous sample solution 1621 into the wells 113. In some embodiments, the hydrophilic second surface 112 of the array 100 uniformly distributes the first cells 1622 and the second cells 1623 within the aqueous sample solution 1621 among the wells 113. In some embodiments, the hydrophilic second surface 112 of the array 100 randomly distributes the first cells 1622 and the second cells 1623 within the aqueous sample solution 1621 among the wells 113. In some embodiments, the first cells 1622 and the second cells 1623 settle to the bottom of each well 113. Optionally, in some embodiments, the first cell 1622 and the second cell 1623 are retained in each hole 113 by the surface tension of the aqueous sample solution 1621. In some examples, the cells are selected from INKT cells, Tmem, Treg, HSPC and combinations thereof. The first surface 111 of the array 100 can be hydrophobic. For example, the bottom side of the well plate can be coated with 1H, 1H, 2H, 2H-perfluorodecanethiol as a hydrophobic layer to prevent the well plate from leaking, as described elsewhere herein. The vertical sidewalls of the wells near the bottom of the well plate can be coated with methoxy-poly (ethylene glycol)-thiol to reduce cell viscosity, as described elsewhere herein.

[0179] Fig. 16C Insertion of the device into a closure or housing according to some embodiments is shown. Figure 1A A side cross-sectional view of an exemplary array of. Fig. 16C, the box 1631 includes a humidifying membrane 1633 located on top of the array 100 and a collection tray 1632 for collecting the second cells 1623. Optionally, in some embodiments, the box 1631 includes a closed box 1631. Optionally, in some embodiments, the box 1631 includes a humidity controlled box 1631. Optionally, in some embodiments, the humidifying membrane 1633 reduces evaporation from the wells 113. Optionally, in some embodiments, the collection tray 1632 can be placed below the array 100 within the box 1631. Optionally, in some embodiments, the collection tray 1632 includes a transparent collection tray 1632.

[0180] Fig.16D An image showing a signal plot of a first cell and a second cell according to some embodiments. Fig.16D , a signal graph 1641 of a second cell may be determined. In some embodiments, a signal graph 1642 of a first cell may be determined. In some embodiments, a graph may be captured by quantifying an image taken by an automated fluorescence scanning system. The first cell may be fluorescent at a first wavelength, and the second cell may be fluorescent at a second wavelength. In some embodiments, a combined image may be determined. Fig.17 Example non-limiting raw fluorescence images of cell arrays are shown. Fig.18 Shown as Fig.17 Example non-limiting scatter plot of 500,000 microwells of the array shown.

[0181] Fig.16E A side cross-sectional view of extracting a second cell is shown according to some embodiments. Fig.16E , by placing the well 113 (according to Fig.16D 1623 in the array 100) is exposed to a pulse of a laser 1651, extracting the second cell 1623 from the array 100. The laser excites the coating 120. In some embodiments, a microsphere can be provided within a particular well 113. Optionally, in some embodiments, the laser 1651 comprises a nanosecond laser 1651.

[0182] Fig.16F A side cross-sectional view of a collected cell is shown according to some embodiments. Fig.16F , second cells 1623 extracted from array 100 by laser 1651 can be collected in collection tray 1661.

[0183] Another aspect provided herein is a method of releasing particles from a hole of an array, the method comprising: filling the hole with at least a portion of a solution, wherein the portion of the solution contains a target particle; maintaining the portion of the solution in the hole by surface tension; directing electromagnetic radiation at a portion of the array; destroying the portion of the array, thereby destroying the surface tension of the portion of the solution held in the hole; and releasing the portion of the solution containing the target particle. In some embodiments, the array comprises a substrate and a coating operably coupled to the substrate. In some embodiments, the substrate comprises a first surface, a second surface opposite to the first surface, and a hole, wherein the hole extends from the first surface to the second surface. In some embodiments, the first surface is hydrophilic and the coating is hydrophobic. In some embodiments, a portion of the array is a coating of the array. In some embodiments, a portion of the array is a coating of the array near the hole. In some embodiments, the coating may include one or more metals selected from chromium, titanium, gold, iron, nickel, copper, platinum, and palladium. In some embodiments, the coating may include one or more metal layers, each layer independently selected from chromium, titanium, gold, iron, nickel, copper, platinum, palladium, any mixture thereof, and any alloy thereof. In some embodiments, the coating may include a metal layer (such as gold) and an attachment layer for the metal layer below it. The attachment layer of the gold layer below the gold may include chromium, titanium, nickel, or nickel chromium. In some embodiments, the coating includes a titanium-gold stack or a titanium layer. In some embodiments, the array includes a plurality of holes. In some embodiments, the method also includes filling the plurality of holes with a solution. In some embodiments, the method also includes releasing the solution held in a subset of the plurality of holes, wherein the subset of the plurality of holes holds a solution containing target particles. The method may also include analyzing a plurality of fluorescent features of each particle. In some embodiments, the method also includes determining based on the analysis the holes of the portion of the solution containing the target particles. In some embodiments, the particles are released at a rate of about 5,000 to about 100,000,000 target particles per second. In some embodiments, the target particles include cells. In some embodiments, the release activity is equal to or greater than 60% of the cells. In some embodiments, the method also includes receiving the target particles in a housing, wherein the housing includes an inner surface for receiving the target particles. In some embodiments, the inner surface accommodates a receiving medium. In some embodiments, the receiving medium includes pluoronic F68.

[0184] In some embodiments, the method also includes utilizing electromagnetic radiation directed to the surface material in the hole of identification or adjacent to the hole of identification, removing a part of the surface material from the first surface or second surface of the array, thereby releasing the contents in the hole of identification. In some examples, a part of the surface material can be adjacent to the hole of identification. A part of the surface can include the lumen surface of the hole of identification. A part of the surface can be removed to a depth of 100 microns or less. A part of the surface can be removed to a depth of 50 microns or less.

[0185] In some cases, prior to identifying the wells with the selected contents, a step of loading the array with a solution comprising the selected contents is performed. In some cases, the step of identifying the wells with the selected contents comprises analyzing electromagnetic radiation emitted from the wells of the array. In some cases, the step of releasing the contents comprises releasing the contents at a rate of about 5,000 to about 100,000,000 wells / second.

[0186] The source generating electromagnetic radiation may include a laser. The laser may be a doped solid-state laser. The laser may be a fiber laser. The laser may be a semiconductor diode laser. The laser may be a gas laser, such as a HeNe laser or an excimer laser. The laser may emit electromagnetic radiation within a wavelength range. In some embodiments, the electromagnetic radiation may be emitted within the visible and / or infrared range. The electromagnetic radiation may then be emitted within a 5 nanometer band within the visible or infrared range. The electromagnetic radiation may be emitted as a harmonic of a doped solid-state laser, such as doped ytterbium orthovanadate or ytterbium aluminum garnet. The electromagnetic radiation may include 1064nm radiation.

[0187] The electromagnetic radiation may be selected from a wavelength of 0.2 microns to 2.5 microns, a flux level sufficient to disrupt adhesion between the contents and the pores, and a pulse duration in the range of 1 ns to 1 millisecond.

[0188] Thus, once it is identified that the target particle is held within a particular hole of the array, electromagnetic radiation can be directed near or adjacent to the particular hole to release the target particle. In some embodiments, the destruction of the second surface comprises removing at least a portion of the array material, a coating on the array, or both.

[0189] In some embodiments, the step of removing a portion of the surface material can be caused by local heating. This mechanism may be possible when the pulse duration is long, the peak power density is low, and / or the wavelength of the incident radiation is in the infrared range. Local heating can cause the surface material or the array material to sublime. In some embodiments, the substrate material and the coating have different thermal expansion coefficients, which can cause peeling.

[0190] In some cases, the step of removing a portion of the surface material can be caused by ablation. Such a mechanism may be possible when the incident peak power density is high, the pulse duration is short, the incident power is high, and / or the incident radiation is in the visible light range. Ablation may include local bond breaking and / or vaporization of the array or substrate material.

[0191] In some cases, the step of removing a portion of the surface material can be caused by plasma generation. Such a mechanism may be possible when the pulse duration of the incident radiation is particularly short, the wavelength of the incident radiation is resonant with the multiphoton ionization mechanism, and / or the wavelength of the incident radiation is very short. Compared to local heating, pulse durations on the order of picoseconds to femtoseconds can result in faster plasma generation, resulting in optical etching of the substrate or surface material.

[0192] In some cases, the step of removing a portion of the surface material may occur by shock wave generation. Such a mechanism may be more likely when the peak power density is high, the phonon resonance and / or the pulse duration is short. The shock may cause physical vibration, flaking or shaking of the surface or array material.

[0193] In some cases, the step of removing a portion of the surface material is photochemical removal, such as photoionization. In some cases, the step of removing a portion of the surface material includes photoacoustic removal, such as by optical generation of shock waves.

[0194] Terms and Definitions

[0195] Unless otherwise defined, all technical terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which the present disclosure belongs.

[0196] As used herein, the singular forms "a," "an," and "the" include plural referents unless the context clearly dictates otherwise. Any reference to "or" herein is intended to include "and / or" unless stated otherwise.

[0197] As used herein, the term "about" refers to an amount that is close to the stated amount by 10%, 5%, or 1%, including increments therein.

[0198] As used herein, the term "PBMC" refers to peripheral blood mononuclear cells.

[0199] As used herein, the term "orthogonal" refers to a perpendicular arrangement or relationship.

[0200] Example

[0201] The following illustrative examples represent implementations of the software applications, systems, and methods described herein and are not meant to be limiting in any way.

[0202] Example 1 - Ti-Au coated microwell array preparation :

[0203] First, 100 nm thick titanium (Ti) was sputtered onto a glass microwell array (20 μm holes, 60% hole coverage), followed by 500 nm thick gold (Au) (vacuum: 8×10-2 to 2×10-2 mbar, sputtering pressure: 100 V to 3 kV, current: 0 to 50 mA). Ti / Au was sputtered onto one side of the well plate. It should be noted that Ti / Au can be sputtered onto both sides or either side of the well plate, as described elsewhere herein.

[0204] The Ti / Au coated microwell array was then immersed in 2M NaOH solution for 20 minutes at room temperature. Any residual NaOH was washed off using deionized water (DI) and ethanol, and the well plate was blown dry.

[0205] PEG-Silane Coating

[0206] Methoxy-poly(ethylene glycol)-silane (PEG-silane) is dissolved in alcohol at a concentration of 0.1 to 5 g / 100 mL. Acetic acid is added to the solution at a volume ratio of 0.1 to 5 mL / 100 mL. The dried well plate from the previous step is immersed in the solution and incubated in an oven at a temperature of 60 to 80° C. for 10 to 60 minutes. The well plate is then washed with deionized water (DI) and ethanol, and blown dry.

[0207] PEG-SH coating

[0208] 0.5 g / 100 mL of methoxy-poly(ethylene glycol)-thiol (PEG-SH) was dissolved in anhydrous ethanol (100% alcohol) by ultrasonic treatment. The dried plate from the previous step was immersed in the solution and incubated in an oven at 30°C for 1 hour. The plate was then washed with deionized water (DI) and ethanol and blown dry.

[0209] Hydrophobic coating on the Au side of the aperture plate

[0210] 100 μL of PF-SH was added to 5 mL of 95% ethanol. The solution was then evenly distributed on an 8x8 inch PDMS sheet while the ethanol evaporated. When there was no visually detectable liquid on the PDMS sheet, the PDMS sheet (PF-SH side down) was applied to the top of the Au side of the orifice plate for 5 minutes. The PDMS sheet was then peeled off. The orifice plate was left to stand for 10 minutes.

[0211] The well plate was immersed in the PEG-SH coating solution and incubated in an oven for 15 minutes at 30° C. The well plate was then washed with deionized water (DI) and / or ethanol and blown dry using a pressurized air gun.

[0212] Example 2 - Box Assembly:

[0213] The box includes (from top to bottom): glass sealed on the top of the box; aluminum alloy frame for holding the microplate; receiving glass plate spaced at a consistent or variable distance from the microplate. Different volumes (depending on the box size) of receiving medium (OptiPEAKT cell medium, InVitria, Junction City, KS) containing 0.1% pluoronic F68 (catalog number 24040032, ThermoFisher Scientific Inc.) are added to the receiving plate. The coated microwell array is assembled into the box with the coated side facing down (facing the receiving medium). Pluoronic F68 added to the receiving medium can greatly improve the viability of cells extracted from the wells, from 0% viability to> 75% viability.

[0214] Example 3 - Cell Sorting Using Coated Microwell Arrays:

[0215] PBMCs at a density of 2 million / mL in OptiPEAK T Cell Media were dropped on top of the microwell array and allowed to settle for 5 minutes to trap single cells at the bottom of the microwells by surface tension. The cartridge was then mounted on a cell sorter. 10-100% laser power was used to extract cells from the microwells. The Ti-Au coating at the bottom edge of the microwells absorbed the IR laser energy and the thin Ti-Au layer was removed. The meniscus ruptured and the cells were released from the desired microwells.

[0216] Example 4 - Fabrication of agarose beads with IR absorbing core:

[0217] This procedure describes the preparation of agarose beads with a transparent shell and an IR-absorbing core.

[0218] Step 1: Suspend 50 mg of Superdex beads (Superdex 75 100 / 300 GL, GE Healthcare LifeSciences) in 1 mL of acetone. Centrifuge at 2000 rpm to collect the Superdex beads. Discard the acetone. Prepare 1 mL of a saturated IR absorbing dye (Epolight 1178, Epolin, New Jersey, USA) solution in acetone. Centrifuge at 5000 rpm to remove all undissolved IR dye. Add the IR dye solution to the Superdex beads. Incubate at room temperature for 30 minutes under constant stirring. Centrifuge the mixture at 1500 rpm. Discard the top liquid. Only the dark precipitate is saved at the bottom. Without further washing with acetone, the resulting dark precipitate is suspended in 0.2% BSA-PBS. This results in Superdex beads uniformly incorporated with IR dye.

[0219] Step 2: To remove the dye from the outside of the beads, wash the beads in a 1:1 acetone-water mixture by pipetting in less than 15 seconds. Immediately afterwards, centrifuge the mixture at 1000 rpm for 30 seconds and discard the top liquid. This will yield the IR core structure.

[0220] Alternatively, the IR absorbing core can be prepared by incubating the beads from step 1 in 0.2% BSA-PBS at 4 degrees for >5 days. Change the buffer once a day. This will slowly dissolve the IR dye from the Superdex beads simply by molecular diffusion.

[0221] The efficacy of IR dye microspheres is shown in Table 1 below.

[0222]

[0223]

[0224] The efficacy of chromium microspheres is shown in Table 2 below.

[0225]

[0226] Example 5 - Single PBMC viability using pluronic F68 as media supplement:

[0227] This procedure describes media supplements used to enhance cell viability during cell sorting.

[0228] The cells were suspended and harvested in OptiPEAK T lymphocyte complete medium (777OPT069) supplemented with 0.1% pluronic F68 and 1X penicillin / streptomycin for cell loading and harvesting. In this example, for an example array with a 20 μm microwell size, the percent viability of each of the three samples was measured to be 81%, 74%, and 65%, respectively.

[0229] Example 6 - PBMC extraction:

[0230] The process describes a solution containing target particles and beads.

[0231] The solution containing human PBMC cells is dripped on the top of the microwell array. After 10 minutes, a single PBMC is loaded into the microwell. Then, a solution containing control beads (TiO2 beads coated with IR dye), or agarose and dextran beads, or agarose and IR dye microspheres is loaded into the top of the microwell array. After 15-30 minutes, beads are loaded into the microwell by gravity. The hole array with cells and beads is installed on the top of the receiving reservoir containing cell culture medium. The IR pulse laser is guided to the bottom of the hole aligned with the loaded beads, and cells are extracted into the cell culture medium. After extraction, the cell culture medium containing the extracted cells is harvested to carry out viability determination.

[0232] Example 7 - Cell Viability:

[0233] This procedure describes determining cell viability.

[0234] Cell viability was determined by quantitative sandwich ELISA assay (human IFN-γ ELISpot kit, R&D Systems Inc., number EL285). The assay used a capture antibody specific for human cytokine interferon γ (IFN-γ), which was pre-coated on a PVDF-supported microplate. The harvested cells were directly pipetted into the wells, and the fixed antibodies near the secreting cells were combined with the secreted human IFN-γ. After the washing step and incubation with the biotinylated detection antibody, alkaline phosphatase conjugated with streptavidin was added. Unbound enzymes were subsequently removed by washing, and substrate solution was added. Blue colored precipitation can be formed at the site of the cytokine and appears in the form of spots, wherein each individual spot represents a single human IFN-γ secreting cell. Spots were counted. Standard cell samples with a series of dilutions of known viable cells were also plated in the same manner as the harvested cell samples. A standard curve was drawn by counting the blue spots in each well. The number of viable cells in the harvested sample was determined by the standard curve.

[0235] Example 8 - Comparison of performance (extraction rate and cell viability) between different coatings:

[0236] Figure 19A-Figure 19C A comparison of the performance (extraction yield and cell viability) between Au-coated well plates and Cr-coated well plates is shown. The Au-coated core plates may include those described herein by reference Figures 11A-13D The surface modification described above. For example, an Au-coated aperture plate may include Fig. 12B and Fig.13D Materials described and shown. Fig.19AIn an array of Au-coated holes, the upper sidewall portion (glass portion) of the holes in the array can be coated with PEG-silane. The lower vertical sidewall portion of the holes in the array can be coated with Au and PEG-thiol. The bottom portion of the array (adjacent to the vertical sidewalls of the holes) can be coated with Au and stamped with perfluorooctane thiol. Reference Fig.19A In a Cr-coated hole array, the bottom portion and bottom vertical sidewalls of the holes of the array can be coated with Cr only, and the upper sidewall portion (glass portion) of the holes in the array can be coated with PEG-silane.

[0237] Au-coated well plates with different surface PEG modifications can provide improvements in extraction yield and cell viability over Cr-coated well plates. For example, the extraction yield of the Au-coated well plate was 73%, while the extraction yield of the Cr-coated well array was 66%. Although the viability of the extracted cells between the Au-coated well plate and the Cr-coated well plate was similar (66% vs. 68%), the number of viable cells obtained using the Au-coated well plate was higher than that obtained with the Cr-coated well plate because the Au-coated core plate had a higher extraction yield compared to the Cr-coated well plate.

[0238] Fig.19B Another example of the yield between Au coated well plates and Cr coated well plates is shown. Ti-Au-PEG coated well plates improve extraction yield and cell viability as well as total viable cell yield. Peripheral blood mononuclear cells (PBMCs) stained with CD4 / 8-APC T cell markers were loaded on Au coated and Cr coated plates and extracted to compare their extraction yield and viability by dye exclusion. Compared with the chemically coated Au plates, only the PEG-silane coated Cr plates showed high viability based on dye exclusion, but due to their laser power limitations, the extraction yield could not be improved. The total yield (i.e., extraction yield and viability) of the Cr coated plates appears to be much lower than that of the Au coated plates. Fig.19C An image of the extraction yield from a whole plate coated with Ti-Au-PEG and a hydrophobic coating is shown (the bright spots are cells stained with fluorescent antibodies under fluorescence imaging). Fig.19C As shown in , comparison of images before and after extraction showed a high extraction yield consistent with the quantitative results above.

[0239] Example 9 - Contact angle images and measurements of different coatings:

[0240] Fig. 20 Images and contact angle measurements of bare Au surface, mPEG-SH coated surface and PF-SH coated surface are shown. Images and measurements were performed on glass plates and well plates. Fig. 20As shown in , different surface coatings can be used to change the wetting behavior of liquids. For example, a hydrophobic coating can be formed on the bottom of the well plate (e.g., by stamping PF-SH on the bottom portion of the array) to prevent leakage from the wells and form a meniscus sufficient to keep the liquid and particles within the wells.

[0241] Although preferred embodiments of the present invention have been shown and described herein, it will be apparent to those skilled in the art that such embodiments are provided by way of example only. Without departing from the present invention, those skilled in the art will now appreciate that many variations, changes and replacements may be employed in practicing the present invention. It should be understood that various alternatives to the embodiments of the present invention described herein may be employed.

Claims

1. An array comprising: a substrate having a first surface and a second surface opposite the first surface, wherein the substrate comprises a plurality of holes defining an inner cavity extending from the first surface to the second surface, and wherein the plurality of holes are configured to receive a sample solution comprising a plurality of particles; and A surface material coated on the first surface or on the vertical sidewalls of the holes adjacent to the first surface, wherein the surface material includes a plurality of materials configured to modify the wetting behavior of the sample solution or the plurality of particles such that one of the first surface or the second surface is hydrophilic and the other of the first surface or the second surface is hydrophobic, the plurality of materials including a functionally modified surface layer including a transition metal and a first chemical coating configured to reduce or eliminate adhesion of the particles to the vertical sidewalls of the holes, the first chemical coating including methoxy-poly(ethylene glycol)-thiol, wherein the surface material is configured to be destroyed from the first surface of the array in response to electromagnetic radiation directed at or adjacent to the surface material.

2. The array of claim 1, wherein the functionally modified surface layer is a hydrophilic modified surface layer, a hydrophobic modified surface layer, or a combination thereof.

3. The array of claim 1, wherein the transition metal of the functionally modified surface layer is a chemically coated metal layer comprising a thickness in the range of 50 nm to 1 mm.

4. The array of claim 1, wherein the transition metal is titanium.

5. The array of claim 1, wherein the transition metal is gold.

6. The array of claim 1, wherein a second portion of the functionally modified surface layer is coated with a second chemical coating different from the first chemical coating.

7. The array of claim 6, wherein the second chemical coating is configured to reduce or prevent unwanted leakage of the sample solution from the wells.

8. The array of claim 6, wherein the second chemical coating is hydrophobic.

9. The array of claim 6, wherein the second chemical coating is disposed on a portion of the substrate at or adjacent to the first surface.

10. The array of claim 6, wherein the second chemical coating comprises 1H,1H,2H,2H-perfluorodecanethiol.

11. The array of claim 1, wherein the plurality of materials further comprises a chemical coating not on the functionally modified surface layer.

12. The array of claim 11, wherein the chemical coating is disposed on one or more portions of the substrate or the plurality of wells that do not have the functionally modified surface layer.

13. The array of claim 11, wherein the chemical coating comprises methoxy-poly(ethylene glycol)-silane.

14. The array of claim 1, wherein the second surface is configured to receive the sample solution comprising the plurality of particles.

15. The array of claim 1, wherein the first surface is configured to be disrupted to release one or more of the particles from one or more of the pores.

16. The array of claim 15, wherein the second surface is hydrophilic to enhance absorption of the sample solution comprising the plurality of particles into the plurality of wells.

17. The array of claim 15, wherein the first surface is hydrophobic to reduce or eliminate unwanted leakage of the sample solution from the wells.

18. The array of claim 15, wherein the first surface is configured to be disrupted by directing electromagnetic radiation at one or more portions of the second surface.

19. The array of claim 1, wherein each hole in the plurality of holes has a maximum diameter of 500 microns or less.

20. The array of claim 1, wherein each hole in the plurality of holes has an aspect ratio of 10 or greater.

21. The array of claim 1, wherein the surface material is selected from materials that absorb greater than 10% of incident electromagnetic radiation.

22. The array of claim 1, wherein the substrate has a hole density of 100 or more holes per square millimeter.

23. The array of claim 1, wherein the array has a particle extraction yield of at least 70%.

24. The array of claim 1, wherein the particle extraction yield of the array having the functionally modified surface layer is higher than another array without the functionally modified surface layer.

25. The array of claim 24, wherein the particle extraction yield of the array having the functionally modified surface layer is at least 5% higher than the other array without the functionally modified surface layer.

26. The array of claim 25, wherein the particle extraction yield of the array having the functionally modified surface layer is at least 20% higher than the other array without the functionally modified surface layer.

27. The array of claim 1, wherein the plurality of particles comprises living cells, and wherein the array having the functionally modified surface layer has a higher live cell extraction yield than another array without the functionally modified surface layer.

28. The array of claim 27, wherein the live cell extraction yield of the array having the functionally modified surface layer is at least 5% higher than that of the other array without the functionally modified surface layer.

29. The array of claim 27, wherein the live cell extraction yield of the array having the functionally modified surface layer is at least 20% higher than that of the other array without the functionally modified surface layer.

30. The array of claim 1, wherein the functionally modified surface layer has a thickness in the range of 50 nm to 1 mm.