A method for improving water absorption profile in multi-level near-wellbore zones

Through multi-particle size and multi-step process technology, combined with large-particle size sealing and small-particle size diversion, the water absorption profile of the water injection well in oil mining is adjusted, which solves the problem of poor injection and degradability of the water injection well and improves oil discharging Efficiency and construction efficiency reduce costs.

CN115717514BActive Publication Date: 2024-11-01CHINA NAT PETROLEUM CORP +1
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
CN202211458501.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-11-17
Publication Date
2024-11-01
Estimated Expiration
2042-11-17

AI Technical Summary

Technical Problem

The prior art in oil mining has poor injection properties and degradability, resulting in under-injection and uneven profiles, reducing oil displacement efficiency, and low efficiency of conventional disassembly process and low efficiency of temporary blocking agent sealing agent. The problem of intra-layer heterogeneity in the reservoir cannot be effectively solved.

Method used

The method of improving the water absorption profile in multiple stages near well zones is adopted, and through multi-particle size and multi-step process operation, combined with the technology of sealing wide joints and real-time diversion of large-particle sizes, solid particle type temporary plugging agent and pH value are used. The controlled temporary blocking agent adjusts the water absorption profile through multiple steps to achieve all-round adjustment of the profile.

Benefits of technology

The oil discharging efficiency of the water injection well is improved, the pump injection cost is reduced, and the uniform and comprehensive profile adjustment is achieved, which significantly improves construction efficiency and reduces resource waste and economic losses.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115717514B_ABST
    Figure CN115717514B_ABST
Patent Text Reader

Abstract

The present invention relates to a method for improving the water absorption profile in a multi-stage near-wellbore zone, and the specific steps are as follows: step one, pushing a solid particle-type temporary plugging agent into a wellbore to plug large cracks and pores in the near-wellbore zone; step two, injecting chelated acid and a pH-controlled temporary plugging agent into the oil pipe in the wellbore respectively through two acid injection skids, and injecting water into the wellhead through a water injection pipeline at the same time; the chelated acid, the pH-controlled temporary plugging agent and the injected water are injected and mixed in the oil pipe; the pH-controlled temporary plugging agent is mixed in the wellbore to precipitate particles, and the process of acidification-temporary plugging is realized in the formation, and the water absorption profile is adjusted by plugging a high-permeability water-absorbing layer in multiple steps and acidifying and transforming a low-permeability water-absorbing layer. In the present invention, a solid water-soluble temporary plugging agent is used for temporary plugging, and a solid oil-soluble temporary plugging agent is used for long-term plugging of the water injection layer to save time. The present invention realizes the process of acidification-temporary plugging in the formation through chelated acid, injected water and a pH-controlled temporary plugging agent, thereby improving the water absorption profile.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of improving oil recovery, and in particular to a method for improving water absorption profiles in multi-level near-wellbore zones. Background Art

[0002] At present, there are nearly 20,000 water injection wells in Changqing Oilfield. Affected by the water quality and reservoir heterogeneity, the proportion of water injection wells with high pressure under-injection and uneven profile exceeds 15%, and the trend is increasing year by year. Conventional profile control technology has problems such as long operation cycle, low efficiency, and short effective period. At the same time, the pressure before and after the operation is on the rise, which aggravates the degree of under-injection and reduces the oil recovery efficiency. In addition, the temporary plugging agent used in the acidizing process has low plugging efficiency, poor acid resistance, and incomplete dissolution of the temporary plugging agent after transformation, which pollutes the reservoir. As a result, a large amount of acid enters the high permeability zone, further aggravating the heterogeneity between layers or sections, wasting resources and causing huge economic losses. Diverter acidizing is popular because of its diversion and economic friendliness. Granular temporary plugging agent is the most commonly used type of plugging agent in many diverter acidizing. At present, granular temporary plugging agent has high strength, high temporary plugging strength, and can plug the conical profile for a long time. However, it is easy to get stuck in the pumping process, and the injection process generally requires viscous liquid, and it is difficult to inject at the same time.

[0003] 1. The existing water-soluble temporary plugging agents disclosed in Chinese patents have a large particle size (for example, the finished water-soluble fracturing acidification temporary plugging agent disclosed in CN1597873A has a particle size of 3-6 mm). When applied to low-permeability oil fields, it is difficult to enter the reservoir to temporarily plug the high-permeability layer, especially unable to solve the problem of intra-layer heterogeneity in the reservoir. The current acid injection skid has a small pumping diameter and cannot simultaneously pump such large-diameter temporary plugging agents.

[0004] 2. Water-soluble temporary plugging agent for acidification of low-permeability oil field water injection wells and its preparation method and application (application number: CN201310139554.5). The water-soluble temporary plugging agent precipitates temporary plugging agent particles after encountering acid, and the particle size range is between 5μm-30μm. Take 20g sodium benzoate, 1g methanol, and 0.2g ATMP and add water to 100g. While adding water, slowly stir until all components are completely dissolved, that is, 100g of water-soluble temporary plugging agent sample with a solid content of about 20%. The disadvantage is that the use of this particle size temporary plugging agent cannot form a rapid temporary plugging for high permeability and water-absorbing layers with wide cracks. Summary of the invention

[0005] In order to overcome the existing problems of poor injectability and degradation, the present invention provides a method for improving the water absorption profile in the near-wellbore zone at multiple levels. The present invention adopts multi-particle size and multi-step process operation according to the reservoir characteristics, combining the characteristics of large particle size blocking wide seams and high permeability layers with good effects, and small particle size with real-time diversion and real-time adjustment; water-soluble temporary blocking, oil-soluble long-term blocking of water injection layers. The characteristics of all-round profile adjustment are achieved, and the multi-step process operation greatly reduces the pumping cost.

[0006] The technical solution adopted by the present invention is:

[0007] A method for improving the water absorption profile in a multi-stage near-wellbore zone, comprising the following specific steps: Step 1, injecting a solid particle-type temporary plugging agent into the wellbore to plug large cracks and pores in the near-wellbore zone;

[0008] Step 2: Inject chelated acid and pH-controlled temporary plugging agent into the oil pipe in the wellbore respectively, and inject water into the wellhead through the water injection pipeline at the same time; the chelated acid, pH-controlled temporary plugging agent and injection water are injected and mixed in the oil pipe; the pH-controlled temporary plugging agent is mixed in the wellbore to precipitate particles, and the process of acidification-temporary plugging is realized in the formation, and the water absorption profile is adjusted by plugging the high permeability water-absorbing layer in multiple steps and acidizing and transforming the low permeability water-absorbing layer.

[0009] In the step 2, the specific method of adjusting the water absorption profile by plugging the high permeability water absorption layer in multiple steps and acidifying and transforming the low permeability water absorption layer is:

[0010] The first step is to determine the time when all the solid particle type temporary plugging agent enters the formation according to the injection speed of the solid particle type temporary plugging agent, and record the wellhead pressure P1 at that time;

[0011] In the second step, as the temporary plugging particles precipitated by the pH-controlled temporary plugging agent in the wellbore gradually enter the reservoir with relatively high permeability, the wellhead pressure will continue to rise. When the pressure rises to P1 plus 2-4MPa, the injection of the pH-controlled temporary plugging agent is stopped;

[0012] The third step is to continue injecting chelated acid and allow the chelated acid to enter the near-wellbore area to transform the relatively low-permeability water-absorbing layer; as the chelated acid continues to enter the formation, the wellhead pressure decreases. When the wellhead pressure drops to pressure P1, continue to inject the pH-controlled temporary plugging agent. As the particles of the pH-controlled temporary plugging agent precipitated in the wellbore enter the formation, when the pressure rises to P1 plus 4-6MPa, stop injecting the pH-controlled temporary plugging agent and continue acidizing to transform the low-permeability water-absorbing layer;

[0013] The fourth step is that when the wellhead pressure drops to pressure P1 again, continue to inject the pH-controlled temporary plugging agent. As the particles of the pH-controlled temporary plugging agent precipitated in the wellbore enter the formation, when the pressure rises to P1 plus 6-8MPa, stop injecting the pH-controlled temporary plugging agent and continue to acidify the low-permeability water-absorbing layer. In this way, different high-permeability water-absorbing layers are plugged and the low-permeability water-absorbing layer is acidified through multiple pressure steps to adjust the water absorption profile.

[0014] In the step 2, the mixing volume ratio of the chelating acid and the injected water is 1:1-2.50.

[0015] In the step 1, the solid particle type temporary plugging agent includes a solid oil-soluble temporary plugging agent and a solid water-soluble temporary plugging agent, and the volume ratio of the solid oil-soluble temporary plugging agent to the solid water-soluble temporary plugging agent is 1:5-10.

[0016] The solid oil-soluble temporary plugging agent comprises the following components by mass ratio: 40%-50% petroleum resin, 20%-25% petroleum asphalt, 10%-15% rock asphalt, 5%-10% xanthan gum, 4%-8% nanofiber, and 2%-6% surfactant.

[0017] The solid water-soluble temporary plugging agent comprises the following components by mass ratio: 80% to 85% of PLGA-PEG-PLGA polymer, 5% to 8% of polytrimethylene carbonate, 6% to 9% of nano-enhanced material, 3% of plasticizer, 0.5% of antioxidant and 0.5% of lubricant; the nano-enhanced material is SiO2, the plasticizer is polyethylene glycol, the antioxidant is tetrakis[β-(3.5-di-tert-butyl, 4-hydroxyphenyl) propionate] pentaerythritol; and the lubricant is ethylene bisstearamide.

[0018] The pH value controlled temporary plugging agent comprises the following components by mass ratio: 10.0%-15.0% of melamine, 10.0%-20.0% of sodium lignin sulfonate, 3.0%-5.0% of lauryl amide propyl dimethyl tertiary amine, 12.0%-15.0% of methanol, 5.0%-8.0% of lauryl amide propyl amine oxide, and the rest is monomer A, wherein monomer A is one of N,N-dimethylhexylamide, dimethyltetradecylamine, N-methyldidecylamine, and dodecyldimethyl tertiary amine.

[0019] In step one, the process of pushing the solid particle type temporary plugging agent into the wellbore is as follows: first, the 700-type fracturing truck is connected to the water injection well oil pipe, the casing gate is opened, and the solid particle type temporary plugging agent is pushed into the wellbore with a large displacement. The 700-type fracturing truck removes the pipeline and leaves, completing the injection of the solid particle type temporary plugging agent. The solid particle type temporary plugging agent pushed into the wellbore seals the 0.5-20mm cracks near the wellbore.

[0020] In the step 1, chelated acid and pH-controlled temporary plugging agent are respectively injected into the oil pipe in the wellbore by two acid injection skids, and the acid injection skid is an acid-resistant three-cylinder plunger pump with a maximum pump discharge pressure greater than 30MPa.

[0021] The chelating acid is composed of the following substances in percentage by mass: 20-25% hydrochloric acid, 25-35% hydrofluoric acid, 15-25% acetic acid, 0.5% fluorine surfactant, 1-2% corrosion inhibitor, and the rest is water.

[0022] The beneficial effects of the present invention are:

[0023] In the present invention, the solid particle type temporary plugging agent includes a solid oil-soluble temporary plugging agent and a solid water-soluble temporary plugging agent. The particle sizes of the solid oil-soluble temporary plugging agent and the solid water-soluble temporary plugging agent are both 3-6 mm, which effectively plugs the 0.5-20 mm near-wellbore cracks. At the same time, a large displacement speed injection is adopted to ensure that the solid particle type temporary plugging agent can be quickly injected, the solid water-soluble temporary plugging agent performs temporary plugging, and the solid oil-soluble temporary plugging agent performs long-term plugging of the injection layer, saving time and ensuring the effectiveness of the construction.

[0024] The present invention realizes a process of acidification and temporary plugging in a formation by using chelated acid, injected water and a pH-controlled temporary plugging agent. In the present invention, the chelated acid and injected water are mixed while being injected, and the pH-controlled temporary plugging agent is a liquid. After mixing in the wellbore, particles are precipitated, and the precipitated particles are small in diameter. The pH-controlled temporary plugging agent is mixed with the acid in the chelated acid, and will combine with the hydrogen ions in the acid to precipitate particles to form a temporary plugging agent. When the pH value increases, the hydrogen ions are separated, and the precipitated particles are dissolved in the liquid again. The present invention realizes the process of real-time diversion and real-time adjustment of small particle diameters by injecting and stopping the pH-controlled temporary plugging agent, thereby effectively adjusting the water absorption profile.

[0025] The invention reduces labor intensity, greatly improves construction efficiency, and achieves the purpose of uniform comprehensive profile adjustment construction.

[0026] The following is a further description with reference to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] Figure 1 This is a schematic diagram of the on-site construction process.

[0028] Figure 2 Inject pressure variation diagram for on-site construction.

[0029] Figure 3 This is a comparison diagram of the water absorption profile before and after construction. DETAILED DESCRIPTION

[0030] Embodiment 1:

[0031] In order to overcome the existing problems of poor injectability and degradation, the present invention provides a method for improving the water absorption profile in the near-wellbore zone at multiple levels. The present invention adopts multi-particle size and multi-step process operation according to the reservoir characteristics, combining the characteristics of large particle size blocking wide seams and high permeability layers with good effects, and small particle size with real-time diversion and real-time adjustment; water-soluble temporary blocking, oil-soluble long-term blocking of water injection layers. The characteristics of all-round profile adjustment are achieved, and the multi-step process operation greatly reduces the pumping cost.

[0032] A method for improving the water absorption profile in a multi-stage near-wellbore zone, comprising the following specific steps: Step 1, injecting a solid particle-type temporary plugging agent into the wellbore to plug large cracks and pores in the near-wellbore zone;

[0033] Step 2: Inject chelated acid and pH-controlled temporary plugging agent into the oil pipe in the wellbore respectively, and inject water into the wellhead through the water injection pipeline at the same time; the chelated acid, pH-controlled temporary plugging agent and injection water are injected and mixed in the oil pipe; the pH-controlled temporary plugging agent is mixed in the wellbore to precipitate particles, and the process of acidification-temporary plugging is realized in the formation, and the water absorption profile is adjusted by plugging the high permeability water-absorbing layer in multiple steps and acidizing and transforming the low permeability water-absorbing layer.

[0034] In the present invention, firstly, large cracks and channels in the near-wellbore area are blocked by solid particle type temporary plugging agents, and large cracks are cracks of 0.5-20mm. In the present invention, the particle size of the solid particle type temporary plugging agent is 3-6mm, and the solid particle type temporary plugging agent is injected at a large displacement of 200-400L / min to ensure rapid injection and the effectiveness of the construction. The injected water is connected to the water injection wellhead through the water injection pipeline, and the chelated acid and the pH value controlled temporary plugging agent are respectively connected to the water injection wellhead through the acid injection skid. In the present invention, the chelated acid is arranged in the chelated acid tank of the acid tank truck. The pH value controlled temporary plugging agent is in liquid form and is in a tank on the temporary plugging truck containing the pH value controlled temporary plugging agent. When necessary, the chelated acid and the pH value controlled temporary plugging agent are injected in a small displacement through the corresponding acid injection skid.

[0035] The large displacement in the present invention is at least 200L / min, and the small displacement is less than 100L / min. In the present invention, the injection water is injected into the wellhead through the water injection pipeline. In the present invention, the chelated acid, the pH value-controlled temporary plugging agent and the injection water are mixed while being injected in the oil pipe, and the solid particle-type temporary plugging agent in the wellbore is first pushed into the large cracks and channels for plugging. At the same time, the injection water is injected into the wellhead through the water injection pipeline, and the chelated acid and the injection water are mixed while being injected temporarily. The pH value-controlled temporary plugging agent precipitates particles after mixing in the wellbore, and the process of acidification and temporary plugging is realized in the formation. In the present invention, the pH value-controlled temporary plugging agent precipitates particles after mixing in the wellbore, and the precipitated particles are small in size, and the small-size particles plug cracks less than 0.5mm. By controlling the injection and stopping of the pH value-controlled temporary plugging agent multiple times, the process of real-time diversion and real-time adjustment of small particle size is realized, thereby effectively adjusting the water absorption profile.

[0036] In the present invention, the low corrosion inhibition of the chelated acid (less than 3.0 g / (m 2 h)>, which is less than the first-level industry standard, will not corrode the pipe in the wellbore, and avoid downhole accidents. In the present invention, the injection and stop of the chelating acid and the pH value controlled temporary plugging agent are controlled multiple times to achieve the process of real-time diversion and real-time adjustment of small particle size, thereby effectively adjusting the water absorption profile.

[0037] Embodiment 2:

[0038] Based on Example 1, in this embodiment, preferably, in the step 2, the specific method for adjusting the water absorption profile by plugging the high permeability water absorption layer in multiple steps and acidifying and transforming the low permeability water absorption layer is:

[0039] The first step is to determine the time when all the solid particle type temporary plugging agent enters the formation according to the injection speed of the solid particle type temporary plugging agent, and record the wellhead pressure P1 at that time;

[0040] In the second step, as the temporary plugging particles precipitated by the pH-controlled temporary plugging agent in the wellbore gradually enter the reservoir with relatively high permeability, the wellhead pressure will continue to rise. When the pressure rises to P1 plus 2-4MPa, the injection of the pH-controlled temporary plugging agent is stopped;

[0041] The third step is to continue injecting chelated acid and allow the chelated acid to enter the near-wellbore area to transform the relatively low-permeability water-absorbing layer; as the chelated acid continues to enter the formation, the wellhead pressure decreases. When the wellhead pressure drops to pressure P1, continue to inject the pH-controlled temporary plugging agent. As the particles of the pH-controlled temporary plugging agent precipitated in the wellbore enter the formation, when the pressure rises to P1 plus 4-6MPa, stop injecting the pH-controlled temporary plugging agent and continue acidizing to transform the low-permeability water-absorbing layer;

[0042] The fourth step is that when the wellhead pressure drops to pressure P1 again, continue to inject the pH-controlled temporary plugging agent. As the particles of the pH-controlled temporary plugging agent precipitated in the wellbore enter the formation, when the pressure rises to P1 plus 6-8MPa, stop injecting the pH-controlled temporary plugging agent and continue to acidify the low-permeability water-absorbing layer. In this way, different high-permeability water-absorbing layers are plugged and the low-permeability water-absorbing layer is acidified through multiple pressure steps to adjust the water absorption profile.

[0043] The present invention realizes the process of acidification and temporary plugging in the formation by using chelated acid, injection water and pH value controlled temporary plugging agent. In the present invention, chelated acid and injection water are mixed while being injected, and the pH value controlled temporary plugging agent is mixed in the wellbore to precipitate particles, and the precipitated particles are small in size. By injecting and stopping the pH value controlled temporary plugging agent, the process of real-time diversion and real-time adjustment of small particle size is realized, thereby effectively adjusting the water absorption profile.

[0044] In the present invention, Figure 1 As shown, the chelated acid is injected into the water injection wellhead through the acid injection system. The acid injection system includes at least one acid injection vehicle and one acid injection skid. The chelated acid is in the acid injection vehicle. The injection displacement of the chelated acid is determined and adjusted through the acid injection skid and finally enters the water injection wellhead.

[0045] In the present invention, Figure 1 As shown, the pH-controlled temporary plugging agent is injected into the water injection wellhead through the pH-controlled temporary plugging agent configuration. The pH-controlled temporary plugging agent configuration includes at least the pH temporary plugging agent and an acid injection skid. The pH-controlled temporary plugging agent is injected into the water injection wellhead through the acid injection skid.

[0046] In the present invention, the outlets of the 700-type fracturing truck and the acid injection skid are connected to the wellhead of the water injection well through a three-way high-pressure acid-resistant pipeline.

[0047] In the present invention, Figure 1 As shown, the injection water is injected into the injection wellhead in a small volume through the existing daily water injection room, and the small volume is preferably 70L / min.

[0048] Preferably, in step 2, the mixing volume ratio of the chelating acid and the injected water is 1:1-2.50.

[0049] Preferably, in the step 1, the chelated acid and the pH-controlled temporary plugging agent are respectively injected into the oil pipe in the wellbore by two acid injection skids, and the acid injection skid is an acid-resistant three-cylinder plunger pump with a maximum pump discharge pressure greater than 30 MPa. In the present invention, the acid injection skid is a prior art and will not be further described in the present invention.

[0050] Preferably, the displacement of the chelated acid and the injection water after mixing and injecting into the formation is 0-100 L / min. The displacement is also selected to be small to ensure that the three can be fully mixed when the pH value controlled temporary plugging agent is injected. The chelated acid and the injection water will not be injected too quickly, resulting in the formation only undergoing an acidification reaction, and no effective and rapid precipitation of particles, and inability to effectively plug.

[0051] Preferably, the pH-controlled temporary plugging agent comprises the following components by mass ratio: 10.0%-15.0% of melamine, 10.0%-20.0% of sodium lignin sulfonate, 3.0%-5.0% of lauryl amide propyl dimethyl tertiary amine, 12.0%-15.0% of methanol, 5.0%-8.0% of lauryl amide propyl amine oxide, and the rest is monomer A, wherein monomer A is one of N,N-dimethylhexanamide, dimethyltetradecylamine, N-methyldidecylamine, and dodecyldimethyl tertiary amine.

[0052] In the present invention, monomer A is one of N,N-dimethylhexanamide (C8H17NO), dimethyltetradecylamine (C16H35N), N-methyldidecylamine (C21H45N), and dodecyldimethyl tertiary amine (C14H31N).

[0053] In the present invention, the pH value controlled temporary plugging agent is a liquid, and particles are precipitated after mixing in the wellbore. The precipitated particles are small in size. The system of the pH value controlled temporary plugging agent is mixed with the acid in the chelated acid, and will combine with the hydrogen ions in the acid to precipitate particles to form a temporary plugging agent. When the pH value increases, the hydrogen ions are separated and the precipitated particles are dissolved in the liquid again.

[0054] Preferably, the chelating acid is composed of the following substances in the following mass percentages: 20-25% hydrochloric acid, 25-35% hydrofluoric acid, 15-25% acetic acid, 0.5% fluorine surfactant, 1-2% corrosion inhibitor, and the rest is water.

[0055] In the present invention, the chelated acid preparation process is:

[0056] Add the water of formula amount to the reactor, then add the hydrochloric acid, hydrofluoric acid, acetic acid, fluorine surfactant and corrosion inhibitor of formula amount to the reactor in sequence, stir for 10-15min each time adding one component, make each component fully mixed, stir for 30-35min after adding all components to obtain chelated acid. In the present embodiment, the mixing volume ratio of the chelated acid and water is 1:1-1:2.50. After the chelated acid and the injected water are mixed, the injection formation displacement is preferably 50-100L / min.

[0057] In the present invention, 20-25% hydrochloric acid, 25-35% hydrofluoric acid, 15-25% acetic acid, 1.5% fluorine surfactant, and 1-2% corrosion inhibitor are used as the main acid, and the fluorine surfactant is used as the penetration enhancer. When the main acid remains unchanged, the amount of fluorine surfactant is changed to improve the penetration effect. In the present invention, the low corrosion inhibition of the chelated acid (less than 3.0g / (m 2 h)>, which is lower than the industry's first-class standard and will not cause corrosion to the pipe in the wellbore and cause downhole accidents.

[0058] Preferably, in step 1, the solid particle type temporary plugging agent includes a solid oil-soluble temporary plugging agent and a solid water-soluble temporary plugging agent, and the volume ratio of the solid oil-soluble temporary plugging agent to the solid water-soluble temporary plugging agent is 1:5-10.

[0059] Preferably, in step one, the process of pushing the solid particle type temporary plugging agent into the wellbore is: firstly connect the 700-type fracturing truck with the oil pipe of the water injection well, open the casing gate, push the solid particle type temporary plugging agent into the wellbore with a large displacement, remove the pipeline and leave the 700-type fracturing truck, complete the injection of the solid particle type temporary plugging agent, and the solid particle type temporary plugging agent pushed into the wellbore seals the 0.5-20 mm cracks near the wellbore.

[0060] Preferably, the solid oil-soluble temporary plugging agent comprises the following components by mass ratio: 40% to 50% petroleum resin, 20% to 25% petroleum asphalt, 10% to 15% rock asphalt, 5% to 10% xanthan gum, 4% to 8% nanofiber, and 2% to 6% surfactant. In the present invention, the solid oil-soluble temporary plugging agent is a prior art, and each component is an existing mature substance, and will not be further described in the present invention.

[0061] In the present invention, the petroleum resin is preferably C9 petroleum resin. C9 petroleum resin does not contain polar groups in its structure, has good water resistance, acid and alkali resistance, weather resistance and light aging resistance, good solubility in organic solvents, good compatibility with other resins, and also has brittleness, tackification, adhesion and plasticity.

[0062] Preferably, the solid water-soluble temporary plugging agent comprises the following components by mass ratio: 80% to 85% of PLGA-PEG-PLGA polymer, 5% to 8% of polytrimethylene carbonate, 6% to 9% of nano-reinforcement material, 3% of plasticizer, 0.5% of antioxidant and 0.5% of lubricant; the nano-reinforcement material is SiO2, the plasticizer is polyethylene glycol, the antioxidant is pentaerythritol tetrakis[β-(3.5-di-tert-butyl, 4-hydroxyphenyl) propionate]; the lubricant is ethylene bisstearamide.

[0063] In the present invention, the solid particle type temporary plugging agent includes a solid oil-soluble temporary plugging agent and a solid water-soluble temporary plugging agent. The particle sizes of the solid oil-soluble temporary plugging agent and the solid water-soluble temporary plugging agent are both 3-6 mm, which effectively plugs the 0.5-20 mm near-wellbore cracks. At the same time, a large displacement of 200-400L / min is used for injection to ensure that the solid particle type temporary plugging agent can be quickly injected, the solid water-soluble temporary plugging agent performs temporary plugging, and the solid oil-soluble temporary plugging agent performs long-term plugging of the injection layer to save time and ensure the effectiveness of the construction.

[0064] like Figure 1 As shown, the injection of solid particle type temporary plugging agent requires a temporary plugging agent injection system, which includes at least a water distribution vehicle and a 700 type fracturing vehicle. The water distribution vehicle is used for mixing water when water is needed. The solid particle type temporary plugging agent is injected into the water injection wellhead through the 700 type fracturing vehicle. At the same time, during construction, according to the construction design requirements, the daily water injection room on site is connected to the water injection wellhead, and a small amount of water is injected according to the design requirements. The 700 type fracturing vehicle and its supporting equipment, working principle and process in the present invention are all prior art, and will not be further described in the present invention.

[0065] After the method provided by the present invention is used specifically, Figure 2 As shown in the figure, the construction injection pressure change diagram. Figure 2 After the injection of chelated acid and pH-controlled temporary plugging agent, the following is obtained: Figure 3 Schematic diagram of the comparison of water absorption profiles shown. Figure 3 As shown, after construction according to the method provided by the present invention, the change of the water absorption profile is as follows Figure 3 As shown in the figure, the left side is the water absorption profile before the measures, and the right side is the water absorption profile after the measures. It can be seen from the figure that the water absorption profile on the right side becomes balanced, and the section that did not absorb water originally also begins to absorb water. After the measures, the water injection pressure dropped from 10.7 to 8MPa, and the water injection volume was 30m 3 / d rise to 35m 3 / d; the water absorption in the upper section increased from 0 to 45%, and in the lower section decreased from 100% to 55%; the water absorption thickness increased from 4m to 10m; the water absorption profile changed from no water absorption + peak shape to uniform water absorption, and the water absorption condition improved significantly. The upper part of the perforation section was opened and began to absorb water; the heterogeneity coefficient of the water absorption profile changed from the baseline heterogeneity coefficient of 0.5 to the heterogeneity coefficient of 0.65 before and after improvement. 0.36, the homogeneity increased by 29%.

[0066] The invention reduces labor intensity, greatly improves construction efficiency, and achieves the purpose of uniform comprehensive profile adjustment construction. The invention can reduce construction procedures, reduce labor intensity, and greatly improve construction efficiency.

[0067] The above examples are merely illustrative of the present invention and do not constitute a limitation on the protection scope of the present invention. Any design that is the same or similar to the present invention belongs to the protection scope of the present invention. The device structure and method steps not described in detail in the present invention are all prior art and will not be further described in the present invention.

Claims

1. A method for improving water absorption profile in multi-level near-wellbore zones, characterized in that: The specific steps are as follows: Step 1, pushing a solid particle type temporary plugging agent into the wellbore to plug large cracks and pores near the wellbore; the solid particle type temporary plugging agent includes a solid oil-soluble temporary plugging agent and a solid water-soluble temporary plugging agent, and the volume ratio of the solid oil-soluble temporary plugging agent to the solid water-soluble temporary plugging agent is 1:5-10; Step 2: Inject chelated acid and pH-controlled temporary plugging agent into the oil pipe in the wellbore respectively, and inject water into the wellhead through the water injection pipeline at the same time; the chelated acid, pH-controlled temporary plugging agent and injected water are mixed while being injected in the oil pipe; the pH-controlled temporary plugging agent is mixed in the wellbore to precipitate particles, and the acidification-temporary plugging process is realized in the formation, and the high-permeability water-absorbing layer is plugged by steps of multiple different pressures and the low-permeability water-absorbing layer is transformed by acidification, so as to adjust the water absorption profile; The specific method of adjusting the water absorption profile by step-sealing the high permeability water absorption layer with multiple different pressures and acidizing the low permeability water absorption layer is as follows: The first step is to determine the time when all the solid particle type temporary plugging agent enters the formation according to the injection speed of the solid particle type temporary plugging agent, and record the wellhead pressure P1 at that time; In the second step, as the temporary plugging particles precipitated by the pH-controlled temporary plugging agent in the wellbore gradually enter the reservoir with relatively high permeability, the wellhead pressure will continue to rise. When the pressure rises to P1 plus 2-4MPa, the injection of the pH-controlled temporary plugging agent is stopped; The third step is to continue injecting chelated acid and allow the chelated acid to enter the near-wellbore area to transform the relatively low-permeability water-absorbing layer; as the chelated acid continues to enter the formation, the wellhead pressure decreases. When the wellhead pressure drops to pressure P1, continue to inject the pH-controlled temporary plugging agent. As the particles of the pH-controlled temporary plugging agent precipitated in the wellbore enter the formation, when the pressure rises to P1 plus 4-6MPa, stop injecting the pH-controlled temporary plugging agent and continue acidizing to transform the low-permeability water-absorbing layer; The fourth step is that when the wellhead pressure drops to pressure P1 again, continue to inject the pH-controlled temporary plugging agent. As the particles of the pH-controlled temporary plugging agent precipitated in the wellbore enter the formation, when the pressure rises to P1 plus 6-8MPa, stop injecting the pH-controlled temporary plugging agent and continue to acidify the low-permeability water-absorbing layer. In this way, different high-permeability water-absorbing layers are plugged and the low-permeability water-absorbing layer is acidified through multiple pressure steps to adjust the water absorption profile.

2. A method for improving water absorption profile in a multi-stage near-wellbore zone according to claim 1, characterized in that: In the step 2, the mixing volume ratio of the chelating acid and the injected water is 1:1-2.

50.

3. The method for improving water absorption profile in multi-level near-wellbore zones according to claim 1, characterized in that: The solid oil-soluble temporary plugging agent comprises the following components by mass ratio: 40% to 50% petroleum resin, 20% to 25% petroleum asphalt, 10% to 15% rock asphalt, 5% to 10% xanthan gum, 4% to 8% nanofiber, and 2% to 6% surfactant.

4. The method for improving water absorption profile in multi-level near-wellbore zones according to claim 1, characterized in that: The solid water-soluble temporary plugging agent comprises the following components by mass ratio: 80% to 85% of PLGA-PEG-PLGA polymer, 5% to 8% of polytrimethylene carbonate, 6% to 9% of nano-enhanced material, 3% of plasticizer, 0.5% of antioxidant and 0.5% of lubricant; the nano-enhanced material is SiO2, the plasticizer is polyethylene glycol, the antioxidant is tetrakis[β-(3.5-di-tert-butyl, 4-hydroxyphenyl) propionate] pentaerythritol; and the lubricant is ethylene bisstearamide.

5. The method for improving water absorption profile in multi-level near-wellbore zones according to claim 1, characterized in that: The pH value controlled temporary plugging agent comprises the following components by mass ratio: 10.0%-15.0% of melamine, 10.0%-20.0% of sodium lignin sulfonate, 3.0%-5.0% of lauryl amide propyl dimethyl tertiary amine, 12.0%-15.0% of methanol, 5.0%-8.0% of lauryl amide propyl amine oxide, and the rest is monomer A, wherein monomer A is one of N,N-dimethylhexylamide, dimethyltetradecylamine, N-methyldidecylamine, and dodecyldimethyl tertiary amine.

6. The method for improving water absorption profile in multi-level near-wellbore zones according to claim 1, characterized in that: In step 1, the process of pushing the solid particle type temporary plugging agent into the wellbore is as follows: first, the 700-type fracturing truck is connected to the water injection well oil pipe, the casing gate is opened, and the solid particle type temporary plugging agent is pushed into the wellbore with a large displacement. The 700-type fracturing truck removes the pipeline and leaves, completing the injection of the solid particle type temporary plugging agent. The solid particle type temporary plugging agent pushed into the wellbore seals the 0.5-20mm cracks near the wellbore.

7. The method for improving water absorption profile in multi-level near-wellbore zones according to claim 1, characterized in that: In the step 2, chelated acid and pH-controlled temporary plugging agent are respectively injected into the oil pipe in the wellbore by two acid injection skids, and the acid injection skid is an acid-resistant three-cylinder plunger pump with a maximum pump discharge pressure greater than 30MPa.

8. The method for improving water absorption profile in multi-level near-wellbore zones according to claim 1, characterized in that: The chelating acid is composed of the following substances in percentage by mass: 20-25% hydrochloric acid, 25-35% hydrofluoric acid, 15-25% acetic acid, 0.5% fluorine surfactant, 1-2% corrosion inhibitor, and the rest is water.

Citation Information

Patent Citations

  • Water soluble temporary plugging agent for acidification of water injection well in low permeability oilfield, and preparation method and application thereof

    CN103224773A

  • Cleaning gasoline with alcohol ether base

    CN1597873A

  • Well treating compositions containing polymer plugging or fluid loss reducing agents

    CA1050743A

  • Temporary plugging agent for acidization of water injection well of low permeability reservoir

    CN101993684A

  • Temporary plugging turnaround fracture method

    CN107100607A