Inorganic compound crystal and its preparation method and application
By preparing the ternary gallium-based inorganic compound crystal Cs5Ga9S16, the problem of performance balance of infrared second-order nonlinear optical materials has been solved, the combination of high second-order frequency multiplication coefficient and wide optical band gap has been achieved, and the laser damage threshold and application value have been improved.
Patent Information
- Application Number
- CN202111238403.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-10-25
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2041-10-25
AI Technical Summary
Due to the inverse relationship between the second-order frequency multiplication coefficient and the optical band gap, existing infrared second-order nonlinear optical crystal materials are difficult to achieve a balance of performance, resulting in performance defects in practical applications.
Provides a ternary gallium-based inorganic compound crystal Cs5Ga9S16, which has a three-dimensional diamond-like grid structure and a wide optical band gap. It is prepared by a high-temperature solid-state method and combined with the alkali metal element Cs and rare earth elements to achieve large second-order times. A balance between frequency coefficient and wide optical bandgap.
The powder frequency doubling strength of this material reaches 0.8 times that of commercial material AgGaS2, and the laser damage threshold reaches 75 times that of AgGaS2. It is suitable for the infrared band and achieves phase matching. It has important application value in infrared detectors, lasers and photorefractive information processing. and other fields.
Smart Images

Figure CN116024667B_ABST
Abstract
Description
Technical Field
[0001] The present application belongs to the technical field of inorganic nonlinear optical materials, and specifically relates to an inorganic compound crystal and a preparation method and application thereof. Background Art
[0002] Second-order nonlinear optical (NLO) crystals are a very important type of functional material, which are widely used in laser communications, optical information processing, integrated circuits and military technology. Generally speaking, an ideal second-order NLO crystal must meet the following conditions: (1) a large second-order harmonic coefficient; (2) a high laser damage threshold; (3) an appropriate birefringence; (4) a wide optical transmission range; (5) good physical, chemical and mechanical properties. Nonlinear optical materials can be divided into inorganic materials, organic materials, polymer materials and organometallic complex materials according to their physical and chemical properties. Currently, most of the second-order NLO crystals on the market are inorganic materials. According to their different application bands, they can be divided into three categories: ultraviolet band, visible band and infrared band. Among them, the second-order NLO crystal materials in the ultraviolet and visible bands can already meet the requirements of practical applications.
[0003] Currently, commercial infrared second-order NLO crystals are mainly chalcopyrite-type materials, such as AgGaS2, AgGaSe2 and ZnGeP2, but a series of performance defects caused by low optical band gaps affect their practical application range. Excellent infrared second-order NLO crystal materials require both large second-order frequency harmonic coefficient (>0.5×AgGaS2) and wide optical band gap (E g >3.5eV). However, the second-order harmonic generation coefficient of the material is inversely proportional to the optical band gap. How to achieve the performance balance of the material has become a difficulty and hot spot in exploring new infrared second-order NLO crystal materials with excellent performance. Summary of the invention
[0004] The present application aims to provide a ternary gallium-based infrared nonlinear optical crystal, a preparation method and use thereof. The optical crystal material has excellent second-order nonlinear optical properties, can achieve phase matching in the infrared band, has a wide optical band gap, and its powder frequency doubling intensity can reach 0.8 times that of the commercial material AgGaS2, and its laser damage threshold is 75 times that of the AgGaS2 crystal, achieving a good balance between a large second-order frequency doubling coefficient and a wide optical band gap.
[0005] This application provides the following technical solutions:
[0006] According to one aspect of the present application, an inorganic compound crystal is provided, wherein the chemical formula of the inorganic compound crystal is Cs5Ga9S 16 .
[0007] The inorganic compound crystal has a three-dimensional diamond-like grid structure; the three-dimensional diamond-like grid structure is composed of [Ga9S 20 ] The polyhedral groups serve as basic repeating units and are interconnected through shared vertices S; the alkali metal elements Cs are dispersed and filled in the three-dimensional diamond-like grid structure as a charge balance.
[0008] The inorganic compound crystal belongs to the monoclinic system, the space group is Pc, and the unit cell parameters are α=90°, β=100.474±0.1°, γ=90°, Z=2.
[0009] Furthermore, the unit cell parameters are α=90°, β=100.474(6)°, γ=90°, Z=2.
[0010] The powder frequency-doubled intensity of the inorganic compound crystal when the incident laser is 2050nm is 0.6 to 1.0 times that of the AgGaS2 crystal;
[0011] Optionally, the powder frequency-doubled intensity of the inorganic compound crystal when the incident laser is 2050nm is 0.8 times that of the AgGaS2 crystal.
[0012] The laser damage threshold of the inorganic compound crystal when the incident laser is 1064nm is 65 to 85 times that of the AgGaS2 crystal;
[0013] Optionally, the laser damage threshold of the inorganic compound crystal when the incident laser is 1064 nm is 75 times that of the AgGaS2 crystal;
[0014] The inorganic compound crystal has an optical band gap of 3.9-4.1 eV and can achieve phase matching in the infrared band.
[0015] According to another aspect of the present application, a method for preparing the above-mentioned inorganic compound crystal is provided, which comprises at least the following steps: uniformly mixing raw materials containing a cesium source, a gallium source, a sulfur source and a rare earth element, and preparing the inorganic compound crystal by a high temperature solid phase method;
[0016] The high temperature solid phase method comprises the following steps: heating the raw material under vacuum conditions to a holding temperature of 700-1100° C. and keeping the temperature for 50-150 hours, cooling the temperature to 200-500° C. at a cooling rate of 1-3° C. / hour, and then cooling.
[0017] The cesium source is selected from cesium halides; the cesium halides are selected from at least one of cesium chloride, cesium bromide or cesium iodide;
[0018] The gallium source is selected from gallium element;
[0019] The sulfur source is selected from elemental sulfur;
[0020] The rare earth element single substance is selected from at least one of lanthanum single substance, cerium single substance, praseodymium single substance, neodymium single substance or samarium single substance;
[0021] The molar ratio of the cesium source, gallium source, sulfur source and rare earth element is 25-45:27:48:3-13;
[0022] The molar amounts of the cesium source, gallium source, sulfur source and rare earth element are measured in terms of the molar amounts of the single substances;
[0023] The molar amount of the cesium source is based on the molar amount of the cesium element;
[0024] Optionally, the molar ratio of the cesium source, gallium source, sulfur source and rare earth element is 30-40:27:48:5-10;
[0025] Optionally, the molar ratio of the cesium source, gallium source, sulfur source and rare earth element is 35:27:48:5;
[0026] Optionally, the molar ratio of the cesium source, gallium source, sulfur source and rare earth element is 37:27:48:7.
[0027] The vacuum condition is a vacuum pressure of 10 -4 ~10 -3 Pa;
[0028] The insulation temperature is 800-1000° C.; the insulation time is 70-120 hours;
[0029] Optionally, the insulation temperature is 850-950°C;
[0030] Optionally, the insulation temperature is 850° C.; the insulation time is 120 hours;
[0031] Optionally, the insulation temperature is 900° C. and the insulation time is 100 hours.
[0032] Furthermore, the vacuum environment is in a closed container;
[0033] Optionally, the sealed container is a sealed quartz reaction tube.
[0034] Optionally, the preparation method further comprises washing and drying the product obtained by naturally cooling to room temperature to obtain the optical crystal, for example, washing with water (such as deionized water) and drying with ethanol.
[0035] According to another aspect of the present application, an infrared nonlinear optical crystal is provided, comprising the above-mentioned inorganic compound crystal or the inorganic compound crystal prepared by the above-mentioned preparation method.
[0036] According to another aspect of the present application, an application of the above-mentioned infrared nonlinear optical crystal is provided, which is used for infrared detectors, infrared lasers, photorefractive information processing, near-infrared probes or laser frequency conversion.
[0037] Beneficial effects of this application:
[0038] The present application provides a ternary gallium-based infrared nonlinear optical crystal material, which has excellent second-order nonlinear optical properties, namely, it can achieve phase matching in the infrared band and has a wide optical band gap. Its powder frequency doubling intensity can reach 0.8 times that of the commercial material AgGaS2 when the incident laser is 2050nm, and its laser damage threshold can reach 75 times that of the AgGaS2 crystal when the incident laser is 1064nm, thus achieving a good balance between a large second-order frequency doubling coefficient and a wide optical band gap.
[0039] This infrared nonlinear optical crystal has important application value in high-tech fields such as laser frequency conversion, near-infrared probes, and photorefractive information processing, especially in infrared detectors and infrared lasers. BRIEF DESCRIPTION OF THE DRAWINGS
[0040] Figure 1 This is a schematic diagram of the sample structure obtained in Example 1 of the present application.
[0041] Figure 2 is the X-ray diffraction pattern of the sample prepared in Example 1. DETAILED DESCRIPTION
[0042] The technical solution of the present application will be further described in detail below in conjunction with specific embodiments. It should be understood that the following embodiments are only exemplary illustrations and explanations of the present application and should not be construed as limiting the scope of protection of the present application. All technologies implemented based on the above content of the present application are included in the scope that the present application is intended to protect.
[0043] Unless otherwise specified, the raw materials and reagents used in the following examples are commercially available or can be prepared by known methods.
[0044] Example 1
[0045] The total mass of 1g of CsCl, Ga, S and Pr was mixed evenly in a molar ratio of 36:27:48:5 to obtain a raw material. The raw material was placed in a quartz crucible, and the quartz crucible containing the raw material was placed in a quartz reaction tube, and the vacuum was pumped to 10 -3 Pa and melt the sealed quartz reaction tube with hydrogen-oxygen flame. Place the quartz reaction tube in a tube furnace with a temperature controller, heat it to 900°C, and keep it warm for 100 hours. Then cool it down to 400°C at a rate of 2°C / hour, stop heating, and cool it naturally to room temperature. The product is washed with deionized water and dried with ethanol to obtain the sample.
[0046] Test Example 1
[0047] (1) Structural characterization of the sample obtained in Example 1
[0048] The sample obtained in Example 1 was subjected to X-ray single crystal diffraction test, and the test conditions were: on a Saturn 724 single crystal diffractometer, Mo target, Kα radiation source (λ=0.07107nm), and test temperature 293K. The sample was structurally analyzed by Shelx-2014. The crystallographic data results of the sample are shown in Table 1, and the crystal structure schematic diagram is shown in Figure 1 shown.
[0049] Table 1 Crystallographic data of the samples obtained in Example 1
[0050]
[0051] like Figure 1 As shown, the obtained crystal is mainly composed of [Ga9S 20 ] The polyhedral groups serve as the basic repeating units, which are interconnected through shared vertices S to form a three-dimensional grid structure, and the alkali metal ions Cs that serve as charge balance are dispersed and filled in the three-dimensional grid structure.
[0052] The sample was subjected to X-ray powder diffraction phase analysis (XRD) under the following test conditions: on a Rigaku MiniFlexII X-ray diffractometer, Cu target, Kα radiation source (λ = 0.154184 nm). The powder XRD pattern of the sample was fitted with the single crystal diffraction data as shown in the figure below: Figure 2 As shown. Figure 2 It can be seen that the XRD pattern of sample 1 is consistent with the XRD spectrum simulated from single crystal diffraction data. Figure 1 This indicates that the sample obtained in Example 1 is Cs5Ga9S 16 , and has high crystallinity and purity.
[0053] (2) Characterization of optical properties of samples
[0054] The optical properties of sample 1 were tested under the following conditions: characterization on a Perkin-Elmer FT-IR infrared spectrometer and a Perkin-Elmer Lambda 950 UV-visible (near infrared) absorption or diffuse reflectance spectrometer. The light transmission performance, frequency doubling performance, laser damage threshold and optical band gap of sample 1 are shown in Table 2.
[0055] Table 2 Optical performance data of samples
[0056]
[0057] The above are only a few embodiments of the present application and do not constitute any form of limitation to the present application. Although the present application is disclosed as above with preferred embodiments, it is not intended to limit the present application. Any technician familiar with the profession, without departing from the scope of the technical solution of the present application, using the technical content disclosed above to make slight changes or modifications are equivalent to equivalent implementation cases and fall within the scope of the technical solution.
Claims
1. An inorganic compound crystal, characterized in that: The chemical formula of the inorganic compound crystal is Cs5Ga9S 16 ; The inorganic compound crystal belongs to the monoclinic system, and the space group is Pc , the unit cell parameters are a=9.467±0.1Å, b=9.719±0.1Å, c=18.835±0.1Å, α=90°, β=100.474±0.1°, γ=90°, V=1704±1Å 3 , Z=2.
2. The inorganic compound crystal according to claim 1, characterized in that: The unit cell parameters are a=9.467(3)Å, b=9.719(3)Å, c=18.835(6)Å, α=90°, β=100.474(6)°, γ=90°, V=1704.3(9)Å 3 , Z=2.
3. The inorganic compound crystal according to claim 1, characterized in that: The powder frequency-doubled intensity of the inorganic compound crystal when the incident laser is 2050nm is 0.6 to 1.0 times that of the AgGaS2 crystal; The laser damage threshold of the inorganic compound crystal when the incident laser is 1064nm is 65-85 times that of the AgGaS2 crystal; The optical band gap of the inorganic compound crystal is 3.9-4.1 eV.
4. The method for preparing an inorganic compound crystal according to any one of claims 1 to 3, characterized in that: At least the following steps are included: The raw materials containing cesium source, gallium source, sulfur source and rare earth element are uniformly mixed, and the inorganic compound crystal is prepared by a high temperature solid phase method; The high temperature solid phase method comprises the following steps: heating the raw material under vacuum conditions to a holding temperature of 700-1100° C. and keeping the temperature for 50-150 hours, cooling the temperature to 200-500° C. at a cooling rate of 1-3° C. / hour, and then cooling; The cesium source is selected from cesium halides; the cesium halides are selected from at least one of cesium chloride, cesium bromide or cesium iodide; The gallium source is selected from gallium element; The sulfur source is selected from elemental sulfur; The rare earth element single substance is selected from at least one of lanthanum single substance, cerium single substance, praseodymium single substance, neodymium single substance or samarium single substance; The molar ratio of the cesium source, gallium source, sulfur source and rare earth element is 25-45:27:48:3-13; The molar amounts of the gallium source, sulfur source and rare earth element are measured in terms of the molar amounts of the single substances; The molar amount of the cesium source is based on the molar amount of the cesium element.
5. The method according to claim 4, characterized in that The molar ratio of the cesium source, the gallium source, the sulfur source and the rare earth element is 30-40:27:48:5-10.
6. The method according to claim 4, characterized in that The molar ratio of the cesium source, the gallium source, the sulfur source and the rare earth element is 35:27:48:
5.
7. The method according to claim 4, characterized in that The molar ratio of the cesium source, the gallium source, the sulfur source and the rare earth element is 37:27:48:
7.
8. The method according to claim 4, characterized in that The vacuum condition is a vacuum pressure of 10 -4 ~10 -3 Pa; The insulation temperature is 800-1000° C.; the insulation time is 70-120 hours.
9. The method according to claim 4, characterized in that The insulation temperature is 850-950°C.
10. The method according to claim 4, characterized in that The insulation temperature is 850° C. and the insulation time is 120 hours.
11. The method according to claim 4, characterized in that The insulation temperature is 900° C. and the insulation time is 100 hours.
12. An infrared nonlinear optical crystal, characterized in that: Contains the inorganic compound crystal according to any one of claims 1 to 3 or the inorganic compound crystal prepared by the preparation method according to any one of claims 4 to 11.
13. An application of the infrared nonlinear optical crystal according to claim 12, characterized in that: Used in infrared detectors, infrared lasers, photorefractive information processing, near-infrared probes or laser frequency conversion.
Citation Information
Patent Citations
Mid-infrared nonlinear optical crystal, preparation method and applications thereof
CN105603531A
Infrared nonlinear optical crystal CsZn4Ga5S12 as well preparation method and application thereof
CN106087063A