A solar cell and a photovoltaic module
By gradually reducing the doping concentration of the doped conductive layer in TOPCon solar cells, the light absorption capacity and lateral transmission loss are reduced, the optical loss and efficiency reduction problems caused by the doped conductive layer are solved, and the front-side efficiency and double-sided efficiency of the cell are improved. Rate.
Patent Information
- Application Number
- CN202310214703.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-03-01
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2043-03-01
AI Technical Summary
The doped conductive layer in TOPCon solar cells causes optical loss and reduced cell efficiency due to its light absorption capacity, especially when using double-sided power generation, resulting in a decrease in double-sided power generation.
The doping concentration of the doped conductive layer is designed to gradually decrease from the first electrode to the symmetry axis of the two adjacent electrodes without changing the thickness, which reduces the light absorption capacity and lateral transmission loss, and improves the current density and cell efficiency.
It effectively reduces the optical loss and current lateral transmission loss of the doped conductive layer, and improves the front-side cell efficiency and cell double-sided ratio.
Smart Images

Figure CN116093191B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of solar cells, and more particularly to a solar cell and a photovoltaic module. Background Art
[0002] TOPCon (Tunnel Oxide Passivated Contact) is a tunnel oxide passivated contact solar cell technology based on the principle of selective carriers. Its cell structure is an N-type silicon substrate cell. An ultra-thin layer of silicon oxide is prepared on the back of the cell, and then a thin layer of doped silicon is deposited. The two together form a passivated contact structure, which effectively reduces surface recombination and metal contact recombination, providing greater room for further improving cell conversion efficiency.
[0003] Among them, the doped conductive layer in the TOPCon battery has the ability to absorb light, which will cause certain optical losses and reduce the efficiency of the front battery. After the sunlight reaches the back, it is mainly a long-wave spectrum. The doped conductive layer on the back will absorb the long-wave spectrum, causing short-circuit current losses and reduced front battery efficiency. The reason for the difference in the light absorption capacity of the doped conductive layer is that, on the one hand, the higher the absorption coefficient, the stronger the light absorption capacity; on the other hand, the longer the absorption path, the more absorption, and at the same time, because the doped conductive layer has the ability to absorb light, it will also cause a decrease in the efficiency of the back battery, that is, the battery bifaciality decreases, resulting in a decrease in the bifacial power generation power when the battery is used for bifacial power generation. In order to reduce the optical loss caused by the absorption of the doped conductive layer and improve the short-circuit current and battery efficiency, it is usually used to thin the thickness of the doped conductive layer. By reducing the absorption path and reducing the light absorption capacity, however, as the thickness of the doped conductive layer is thinned, the sheet resistance will increase and the lateral transmission capacity of the current will decrease, resulting in a decrease in the fill factor of the battery, affecting the battery efficiency. Summary of the invention
[0004] In view of this, the present invention provides a solar cell and a photovoltaic module, which reduce the optical loss of the doped conductive layer and reduce the lateral transmission loss of the current, thereby improving the front cell efficiency and the cell bifaciality.
[0005] A solar cell provided by the present invention comprises: a silicon substrate and a first electrode;
[0006] A tunneling oxide layer, a doped conductive layer and a first passivation layer are sequentially stacked on one side of the silicon substrate in a direction away from the silicon substrate; the first electrode penetrates the first passivation layer and is electrically connected to the doped conductive layer; the doping concentration of the doped conductive layer gradually decreases from the first electrode to the symmetry axis of two adjacent first electrodes.
[0007] Optionally, the doping concentration of the doped conductive layer decreases from the first electrode to the symmetry axis of two adjacent first electrodes in a range of (1.7-17)×10 19 cm -3 .
[0008] Optionally, the doping concentration of the doped conductive layer at the first electrode is in the range of (1-10)×10 20 cm -3 .
[0009] Optionally, the doping concentration of the doped conductive layer at the symmetry axis of two adjacent first electrodes is in the range of (1-10)×10 19 cm -3 .
[0010] Optionally, the thickness of the doped conductive layer along a direction perpendicular to the silicon substrate ranges from 10 nm to 300 nm.
[0011] Optionally, a diffusion doping layer is further provided between the silicon substrate and the tunneling oxide layer, and a doping concentration in the diffusion doping layer on a side away from the silicon substrate is greater than a doping concentration in the diffusion doping layer on a side close to the silicon substrate.
[0012] Optionally, the doping concentration in the diffusion doping layer gradually decreases from a side away from the silicon substrate to a side close to the silicon substrate.
[0013] Optionally, the doping concentration range of the diffuse doping layer away from the silicon substrate is 10 17 cm -3 ~10 21 cm -3 .
[0014] Optionally, the doping concentration range of the diffuse doping layer close to the silicon substrate is 10 17 cm -3 ~10 19 cm -3 .
[0015] Optionally, the thickness of the diffuse doping layer along a direction perpendicular to the silicon substrate ranges from 40 nm to 200 nm.
[0016] Optionally, the silicon substrate includes a base region and an emitter located on the surface of the base region away from the diffuse doping layer; the emitter is sequentially stacked with a second passivation layer and an anti-reflection layer along a direction away from the base region; the second electrode sequentially penetrates the anti-reflection layer and the second passivation layer and is electrically connected to the emitter.
[0017] The present invention provides a photovoltaic module, comprising a front cover plate, a first packaging film, a battery string, a second packaging film and a back cover plate which are stacked; the battery string is formed by connecting a plurality of solar cells described in any one of the above items.
[0018] Compared with the prior art, the solar cell and photovoltaic module provided by the present invention achieve at least the following beneficial effects:
[0019] The present invention provides a solar cell and a photovoltaic module, in which the thickness of the doped conductive layer remains unchanged from the first electrode to the symmetry axis of two adjacent first electrodes, but the total doping concentration gradually decreases, thereby reducing the optical loss of the doped conductive layer and the lateral transmission loss of the current, thereby improving the front cell efficiency and the cell bifaciality.
[0020] Of course, any product implementing the present invention does not necessarily need to achieve all of the technical effects described above at the same time.
[0021] Further features and advantages of the present invention will become apparent from the following detailed description of exemplary embodiments of the present invention with reference to the attached drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] The accompanying drawings, which are incorporated in and constitute a part of the specification, illustrate embodiments of the invention and, together with the description, serve to explain the principles of the invention.
[0023] Figure 1 is a schematic structural diagram of a solar cell provided in this embodiment;
[0024] Figure 2 is a flow chart of a method for preparing a solar cell provided in this embodiment;
[0025] Figure 3 is a schematic structural diagram of a photovoltaic module provided in this embodiment;
[0026] Figure 4 This is a schematic diagram of the structure of another photovoltaic module provided in this embodiment. DETAILED DESCRIPTION
[0027] Various exemplary embodiments of the present invention will now be described in detail with reference to the accompanying drawings. It should be noted that the relative arrangement of components and steps, numerical expressions and numerical values set forth in these embodiments do not limit the scope of the present invention unless otherwise specifically stated.
[0028] The following description of at least one exemplary embodiment is merely illustrative in nature and is in no way intended to limit the invention, its application, or uses.
[0029] Technologies, methods, and equipment known to ordinary technicians in the relevant art may not be discussed in detail, but where appropriate, the technologies, methods, and equipment should be considered as part of the specification.
[0030] In all examples shown and discussed herein, any specific values should be interpreted as merely exemplary and not limiting. Therefore, other examples of the exemplary embodiments may have different values.
[0031] It should be noted that like reference numerals and letters refer to similar items in the following figures, and therefore, once an item is defined in one figure, it need not be further discussed in subsequent figures.
[0032] See also Figure 1 As shown, Figure 1 is a schematic diagram of the structure of a solar cell provided in this embodiment; a solar cell 18 provided in this embodiment comprises: a silicon substrate 1 and a first electrode 2;
[0033] A tunnel oxide layer 3, a doped conductive layer 4 and a first passivation layer 5 are sequentially stacked on one side of the silicon substrate 1 in a direction away from the silicon substrate 1; the first electrode 2 penetrates the first passivation layer 5 and is electrically connected to the doped conductive layer 4; the doping concentration of the doped conductive layer 4 gradually decreases from the first electrode 2 to the symmetry axis 6 of two adjacent first electrodes 2;
[0034] The silicon substrate 1 includes: a base region 11 and an emitter 12 located on the surface of the base region 11 on a side away from the diffuse doping layer 7; the emitter 12 is sequentially stacked with a second passivation layer 8 and an anti-reflection layer 9 in a direction away from the base region 11; the second electrode 10 sequentially penetrates the anti-reflection layer 9 and the second passivation layer 8 and is electrically connected to the emitter 12.
[0035] In the above scheme, the front surface of the silicon substrate 1 facing the sun is the light-receiving surface, and the back surface of the silicon substrate 1 facing away from the sun is the backlight surface; the silicon substrate 1 can be an N-type silicon substrate 1, specifically, it can be one of a polycrystalline silicon substrate, a single crystal silicon substrate, a microcrystalline silicon substrate or a silicon carbide substrate, and this embodiment does not limit the specific type of the silicon substrate 1; the doping elements of the silicon substrate 1 can be group V elements such as phosphorus, arsenic, and antimony; the thickness of the silicon substrate 1 along the direction perpendicular to the silicon substrate 1 can be 60μm~240μm, specifically, it can be 60μm, 80μm, 90μm, 100μm, 120μm, 150μm, 200μm or 240μm, which is not limited here.
[0036] The emitter 12 can be a P-type emitter, which is a boron-doped diffusion layer; the boron-doped diffusion layer is a P-type emitter (i.e., P+ layer) formed by diffusing boron atoms to a certain depth on the front surface through a diffusion process using a boron source; for example, the boron source can be liquid boron tribromide or boron trichloride.
[0037] The tunneling oxide layer 3 may be an ultra-thin oxide layer; for example, it may be silicon oxide or metal oxide, and may contain other additional elements, such as nitrogen; the thickness of the silicon oxide (SiOx) layer in the direction perpendicular to the silicon substrate 1 is generally 1 nm to 2 nm, and its main function is to serve as a tunneling layer for majority carriers, while chemically passivating the surface of the silicon wafer to reduce interface states; illustratively, the tunneling oxide layer 3 may be a stacked structure of one or more of a silicon oxide layer, an aluminum oxide layer, a silicon oxynitride layer, a molybdenum oxide layer, and a hafnium oxide layer; in other embodiments, the tunneling oxide layer 3 may also be an oxygen-containing silicon nitride layer, an oxygen-containing silicon carbide layer, and the like.
[0038] The doped conductive layer 4 includes at least one of silicon carbide and polycrystalline silicon, that is, the doped conductive layer 4 can be a doped polycrystalline silicon layer, a silicon carbide layer, or a composite layer of a doped polycrystalline silicon layer and a silicon carbide layer; when the doped conductive layer 4 is doped polycrystalline silicon (Doped poly-Si), its main function is to serve as a field passivation layer, forming a band bending on the surface of the silicon wafer, realizing the selective transmission of carriers, and reducing the recombination loss; in the metal electrode covering area of the back silicon oxide / doped polycrystalline silicon, the metal electrode will penetrate the first passivation layer 5 and contact with the doped polycrystalline silicon, but will not penetrate the silicon oxide; the metal electrode contacts the doped polycrystalline silicon to achieve electrical connection, and the metal electrode does not penetrate the silicon oxide to maintain good interface passivation; in the non-metallic electrode covering area, the recombination current on the surface of the silicon substrate 1 can reach a very low level; the first passivation layer 5 generally uses silicon nitride (SiNx) as a hydrogen passivation layer and an optical matching layer.
[0039] The second passivation layer 8 may include but is not limited to at least one of silicon oxide, silicon nitride, silicon oxynitride, aluminum oxide, etc., or any combination thereof. The second passivation layer 8 can produce a good passivation effect on the silicon substrate 1, which is helpful to improve the conversion efficiency of the battery. It should be noted that the second passivation layer 8 can also reduce the reflection of incident light. The thickness of the second passivation layer 8 along the direction perpendicular to the silicon substrate 1 ranges from 10nm to 120nm, and can be specifically 10nm, 20nm, 30nm, 42nm, 50nm, 60nm, 70nm, 80nm, 90nm, 100nm or 120nm, etc., and of course it can also be other values within the above range, which is not limited here.
[0040] The first passivation layer 5 may include but is not limited to at least one of silicon oxide, silicon nitride, silicon oxynitride, aluminum oxide, etc., or any combination thereof; the thickness of the first passivation layer 5 along the direction perpendicular to the silicon substrate 1 ranges from 70nm to 120nm, specifically 70nm, 80nm, 90nm, 100nm or 120nm, etc., and of course may also be other values within the above range, which is not limited here.
[0041] The first electrode 2 and the second electrode 10 are both metal grid line electrodes, and the material of the metal grid line electrode includes at least one of copper, silver, aluminum, and nickel; the metal grid line electrode includes: a main grid line and a secondary grid line, the secondary grid line is connected to the main grid line, the secondary grid line is used to gather the current generated by the solar cell, and the main grid line is used to collect the current on the secondary grid line; as an optional technical solution of this embodiment, multiple main grid lines are distributed at equal intervals, so that the current collected by each main grid line is more uniform.
[0042] In order to form a good ohmic contact with the metal, the metal region requires a higher doping concentration; but the non-metal region requires a lower light absorption performance; for example, the doping elements in the doped polysilicon will affect its light absorption ability, and the higher the element doping concentration, the stronger the light absorption ability and the lower the current, so the non-gate line region requires a relatively low doping concentration; this embodiment proposes a design in which the doping concentration of the doped conductive layer 4 gradually decreases from the first electrode 2 to the symmetry axis 6 of the two adjacent first electrodes 2; the thickness of the doped conductive layer 4 along the direction perpendicular to the silicon substrate 1 remains unchanged, but the doping concentration gradually decreases, and the light absorption ability also gradually decreases, compared with the conventional The doped conductive layer 4 with the same thickness and uniform doping has a weakened total light absorption capacity. Overall, the light absorption loss of the doped conductive layer 4 is greatly reduced, the back current is increased, and the overall current of the battery is increased; and the doping concentration from the symmetry axis 6 of the two adjacent first electrodes 2 to the first electrode 2 gradually increases, and the regionalized lateral transmission resistance gradually decreases accordingly, which is more conducive to the lateral transmission of photogenerated carriers and the lateral transmission of current. The current gradually increases, the current density gradually increases, the front efficiency of the battery is improved, and the battery bifaciality is improved; the battery bifaciality is the ratio of the back efficiency of the battery to the front efficiency of the battery.
[0043] It can be seen from the above embodiments that the solar cell provided in this embodiment achieves at least the following beneficial effects:
[0044] In a solar cell provided in this embodiment, the thickness of the doped conductive layer 4 remains unchanged from the first electrode 2 to the symmetry axis 6 of two adjacent first electrodes 2, but the total doping concentration gradually decreases, thereby reducing the optical loss of the doped conductive layer 4 and the lateral transmission loss of the current, thereby improving the front cell efficiency and the cell bifaciality.
[0045] In some optional embodiments, see Figure 1 As shown, the doping concentration of the doped conductive layer 4 can be uniformly reduced based on the distance from the first electrode 2 to the symmetry axis 6 of two adjacent first electrodes 2; that is, from the first electrode 2 to the symmetry axis 6 of two adjacent first electrodes 2, the doping concentration of the doped conductive layer 4 can be reduced by the same distance at each interval; for example, the doping concentration of the doped conductive layer 4 decreases by (1.7~17)×10 per millimeter from the first electrode 2 to the symmetry axis 6 of two adjacent first electrodes 2.19 cm -3 The doping concentration of the doped conductive layer 4 may also be unevenly reduced from the first electrode 2 to the symmetry axis 6 of two adjacent first electrodes 2 based on the distance; that is, from the first electrode 2 to the symmetry axis 6 of two adjacent first electrodes 2, the doping concentration of the doped conductive layer 4 may be reduced at different intervals of the same distance; for example, the doping concentration of the doped conductive layer 4 may be exponentially reduced per millimeter from the first electrode 2 to the symmetry axis 6 of two adjacent first electrodes 2.
[0046] Specifically, if the doping concentration of the doped conductive layer 4 decreases by less than 1.7×10 19 cm -3 , the doping concentration at the symmetry axis 6 of the two adjacent first electrodes 2 is too high, and the light absorption capacity is strong, resulting in a decrease in current; if the doping concentration of the doped conductive layer 4 decreases by more than 17×10 19 cm -3 , the doping concentration at the symmetry axis 6 of the two adjacent first electrodes 2 is too low, the lateral transmission capability is weakened, the current density is deteriorated, and the battery performance is affected; therefore, the doping concentration of the doped conductive layer 4 decreases from the first electrode 2 to the symmetry axis 6 of the two adjacent first electrodes 2 by (1.7~17)×10 19 cm -3 , it can not only reduce the light absorption capacity and increase the current, but also improve the lateral transmission capacity and current density, thereby improving the battery performance; Optionally, the doping concentration of the doped conductive layer 4 can be reduced by 1.7×10 19 cm -3 , 4×10 19 cm -3 , 8×10 19 cm -3 , 10×10 19 cm -3 , 15×10 19 cm -3 and 17×10 19 cm -3 .
[0047] In some optional embodiments, see Figure 1 As shown, the doping concentration of the doped conductive layer 4 at the first electrode 2 is in the range of (1 to 10)×10 20 cm -3 .
[0048] Specifically, if the doping concentration of the doped conductive layer 4 at the first electrode 2 is greater than 10×1020 cm -3 , the doping concentration is too high, Auger recombination increases, and the passivation performance decreases; if the doping concentration of the doped conductive layer 4 at the first electrode 2 is less than 1×10 20 cm -3 , the doping concentration is too low to achieve the field passivation effect, and the contact with the metallization becomes poor, and the fill factor is reduced; therefore, the doping concentration of the doped conductive layer 4 at the first electrode 2 ranges from (1 to 10)×10 20 cm -3 , which can not only reduce Auger recombination and ensure the passivation effect, but also improve the contact with metallization and improve the fill factor; Optionally, the doping concentration of the doped conductive layer 4 at the first electrode 2 can be 1×10 20 cm -3 , 3×10 20 cm -3 , 5×10 20 cm -3 , 8×10 20 cm -3 and 10×10 20 cm -3 .
[0049] In some optional embodiments, see Figure 1 As shown, the doping concentration of the doped conductive layer 4 at the symmetry axis 6 of two adjacent first electrodes 2 ranges from (1 to 10)×10 19 cm -3 .
[0050] Specifically, if the doping concentration of the doped conductive layer 4 at the symmetry axis 6 of two adjacent first electrodes 2 is greater than 10×10 19 cm -3 , the doping concentration is too high, the Auger recombination increases, and the passivation performance decreases; if the doping concentration of the doped conductive layer 4 at the symmetry axis 6 of two adjacent first electrodes 2 is less than 1×10 19 cm -3 , the doping concentration is too low to achieve the field passivation effect, and the contact with the metallization becomes poor, and the fill factor is reduced; therefore, the doping concentration range of the doped conductive layer 4 at the symmetry axis 6 of two adjacent first electrodes 2 is (1~10)×10 19 cm -3 , which can not only reduce Auger recombination and ensure the passivation effect, but also improve the contact with metallization and improve the fill factor; Optionally, the doping concentration of the doped conductive layer 4 at the symmetry axis 6 of two adjacent first electrodes 2 can be 1×10 19 cm -3 , 3×10 19 cm -3 , 5×10 19 cm-3 , 8×10 19 cm -3 and 10×10 19 cm -3 .
[0051] In some optional embodiments, see Figure 1 As shown, the thickness of the doped conductive layer 4 along the direction perpendicular to the silicon substrate 1 ranges from 10 nm to 300 nm.
[0052] Specifically, if the thickness of the doped conductive layer 4 along the direction perpendicular to the silicon substrate 1 is greater than 300nm, it will cause excessive light absorption ability, resulting in reduced current; if the thickness of the doped conductive layer 4 along the direction perpendicular to the silicon substrate 1 is less than 10nm, the passivation performance will be reduced, and at the same time, the metallization requirements will be too high, making it difficult to achieve mass production; therefore, the thickness range of the doped conductive layer 4 along the direction perpendicular to the silicon substrate 1 is 10nm~300nm, which can avoid excessive light absorption ability and reduced current, and can also improve passivation performance, reduce metallization requirements, and facilitate mass production; optionally, the thickness of the doped conductive layer 4 along the direction perpendicular to the silicon substrate 1 can be 10nm, 100nm, 150nm, 200nm and 300nm.
[0053] In some optional embodiments, see Figure 1 As shown, a diffusion doping layer 7 is further provided between the silicon substrate 1 and the tunneling oxide layer 3 , and the doping concentration in the diffusion doping layer 7 on the side away from the silicon substrate 1 is greater than the doping concentration in the diffusion doping layer 7 on the side close to the silicon substrate 1 .
[0054] Specifically, the doping concentration in the diffusion doping layer 7 gradually decreases from the side far away from the silicon substrate 1 to the side close to the silicon substrate 1; the doping concentration of the diffusion doping layer 7 decreases from the side far away from the silicon substrate 1 to the doping concentration close to the silicon substrate 1, and an electric field is formed between the high doping and the low doping, which plays a field passivation role and improves the passivation performance.
[0055] In some optional embodiments, see Figure 1 As shown, the doping concentration range of the diffusion doping layer 7 away from the side of the silicon substrate 1 is 10 17 cm -3 ~10 21 cm -3 .
[0056] Specifically, if the doping concentration in the diffusion doping layer 7 on the side away from the silicon substrate 1 is greater than 10 21 cm -3 , the doping concentration of the diffusion doping layer 7 is too high, indicating that the tunneling oxide layer 3 has a poor effect and the passivation performance is reduced; if the doping concentration in the diffusion doping layer 7 on the side away from the silicon substrate 1 is less than 10 17 cm -3, the doping amount of the diffusion doping layer 7 is too low, the metal contact performance deteriorates, and the filling factor deteriorates; therefore, the doping concentration range of the diffusion doping layer 7 away from the side of the silicon substrate 1 is 10 17 cm -3 ~10 21 cm -3 , it can ensure the tunneling oxide layer 3 effect and passivation performance, and can also improve the metal contact performance and fill factor; Optionally, the doping concentration in the diffusion doping layer 7 away from the side of the silicon substrate 1 can be 10 17 cm -3 , 10 18 cm -3 , 10 19 cm -3 , 10 20 cm -3 and 10 21 cm -3 .
[0057] In some optional embodiments, see Figure 1 As shown, the doping concentration range of the diffuse doping layer 7 close to the silicon substrate 1 is 10 17 cm -3 ~10 19 cm -3 .
[0058] Specifically, if the doping concentration in the diffusion doping layer 7 close to the silicon substrate 1 is greater than 10 19 cm -3 , the doping concentration of the diffusion doping layer 7 is too high, indicating that the tunneling oxide layer 3 has a poor effect and the passivation performance is reduced; if the doping concentration in the diffusion doping layer 7 close to the silicon substrate 1 is less than 10 17 cm -3 , the doping amount of the diffusion doping layer 7 is too low, the metal contact performance deteriorates, and the filling factor deteriorates; therefore, the doping concentration range of the diffusion doping layer 7 close to the side of the silicon substrate 1 is 10 17 cm -3 ~10 19 cm -3 , it can not only ensure the tunneling oxide layer 3 effect and passivation performance, but also improve the metal contact performance and fill factor; Optionally, the doping concentration in the diffusion doping layer 7 close to the side of the silicon substrate 1 can be 10 17 cm -3 , 10 18 cm -3 and 10 19 cm -3 In some optional embodiments, see Figure 1 As shown, the thickness of the diffusion doping layer 7 along the direction vertical to the silicon substrate 1 ranges from 40 nm to 200 nm.
[0059] Specifically, the thickness of the diffusion doping layer 7 along the direction perpendicular to the silicon substrate 1 is the doping depth of the doping element in the silicon substrate 1; if the thickness of the diffusion doping layer 7 along the direction perpendicular to the silicon substrate 1 is greater than 200nm, the thickness is too large, the doping amount in the silicon substrate 1 is too high, and the passivation effect is poor; if the thickness of the diffusion doping layer 7 along the direction perpendicular to the silicon substrate 1 is less than 40nm, the thickness is too small, the doping amount is too low, and the metal contact is poor; therefore, the thickness range of the diffusion doping layer 7 along the direction perpendicular to the silicon substrate 1 is 40nm~200nm, which can ensure that the doping amount in the silicon substrate is appropriate and improve the passivation effect and the metal contact effect; optionally, the thickness of the diffusion doping layer 7 along the direction perpendicular to the silicon substrate 1 can be 40nm, 80nm, 100nm, 150nm, 180nm and 200nm.
[0060] See also Figure 2 As shown, Figure 2 It is a flow chart of a method for preparing a solar cell provided in this embodiment; this embodiment also provides a method for preparing a solar cell, which can be used to prepare an N-type solar cell, and further can be used to prepare an N-type TOPCon cell. The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the method for preparing the N-type TOPCon cell of the present invention. The described embodiments are only part of the embodiments of the present invention, not all of the embodiments.
[0061] Step S100, forming an emitter 12 on the front surface of the textured silicon substrate 1;
[0062] Specifically, the silicon substrate 1 is an N-type silicon substrate 1, and the silicon substrate 1 can be one of a polycrystalline silicon substrate, a single crystal silicon substrate, a microcrystalline silicon substrate or a silicon carbide substrate. The present embodiment does not limit the specific type of the silicon substrate 1; the doping elements of the silicon substrate 1 can be group V elements such as phosphorus, arsenic, and tellurium; in some other embodiments, the front and rear surfaces of the silicon substrate 1 can also be subjected to a texturing treatment to form a velvet surface or surface texture structure, such as a pyramid structure; the texturing treatment method can be chemical etching, laser etching, mechanical method, and plasma etching, etc., which are not limited here; illustratively, the front and rear surfaces of the silicon substrate 1 can be subjected to a texturing treatment using a NaOH solution, and since the corrosion of the NaOH solution is anisotropic, a pyramid velvet surface structure can be prepared; it can be understood that the surface of the silicon substrate 1 has a velvet structure through the texturing treatment, which produces a light trapping effect, increases the amount of light absorbed by the solar cell, and thus improves the conversion efficiency of the solar cell.
[0063] In some embodiments, before the texturing process, a step of cleaning the N-type silicon substrate 1 may be further included to remove metal and organic pollutants on the surface.
[0064] In some other embodiments, the emitter 12 can be formed on the front side of the silicon substrate 1 by any one or more methods of high-temperature diffusion, slurry doping or ion implantation; specifically, the emitter 12 is formed by diffusing boron atoms through a boron source; the emitter 12 is designed as a selective emitter structure; the boron source can be, for example, diffused with boron tribromide to transform the microcrystalline silicon phase of the crystalline silicon into a polycrystalline silicon phase; since the surface of the silicon substrate 1 has a high concentration of boron, a borosilicate glass layer (BSG) is usually formed, and this borosilicate glass layer has a metal gettering effect, which will affect the normal operation of the solar cell and needs to be removed later.
[0065] Step S200 , forming a tunneling oxide layer 3 and a conductive layer on the back side of the silicon substrate 1 , and performing doping treatment and local laser treatment on the conductive layer to form a doped conductive layer 4 .
[0066] Specifically, a tunneling oxide layer 3 can be first formed on the back side of the silicon substrate 1, and then a doped polysilicon layer can be formed on the surface of the tunneling oxide layer 3; wherein, the laser processing method of the doped polysilicon layer is to gradually decrease the laser energy from the first electrode 2 to the symmetry axis 6 of two adjacent first electrodes 2, thereby realizing a structure in which the doping concentration decreases from the first electrode 2 to the symmetry axis 6 of two adjacent first electrodes 2.
[0067] This embodiment does not limit the specific operation method for forming the oxide layer; illustratively, any one of ozone oxidation, high-temperature thermal oxidation and nitric acid oxidation can be used to oxidize the rear surface of the silicon substrate 1; this embodiment does not limit the specific operation method for forming the conductive layer; illustratively, any one of low-pressure chemical vapor deposition, plasma-enhanced chemical vapor deposition and atmospheric pressure chemical vapor deposition can be used to deposit a conductive layer on the surface of the tunneling layer to protect the oxide layer. Secondly, the conductive layer is doped to form a high-low junction (n / n+-Si), which can effectively reduce the recombination rate of carriers on the back of the battery and further improve the conversion efficiency of the solar cell.
[0068] In some embodiments, an in-situ doping treatment can be performed while depositing the conductive layer to form a doped conductive layer 4, and the doped conductive layer 4 includes at least one of silicon carbide and polycrystalline silicon, that is, the doped conductive layer 4 can be a doped polycrystalline silicon layer, a silicon carbide layer, or a composite layer of a doped polycrystalline silicon layer and a silicon carbide layer.
[0069] When the doped conductive layer 4 is a phosphorus-doped polysilicon layer, the phosphorus doping source can be prepared by any one or more methods of high-temperature diffusion, slurry doping or ion implantation; the doping source for local laser treatment is the phosphorus silicon glass on the surface of the doped polysilicon layer and the unactivated phosphorus in the polysilicon layer, and these phosphorus are activated by laser to form a heavily doped polysilicon layer with a higher phosphorus concentration; the laser for local laser treatment includes green light with a wavelength of 532nm, and of course it can also be lasers in other wavelength ranges, which are not limited here; the pulse width of local laser treatment is 15ns~40ns, Specifically, the pulse width of the local laser treatment can be, for example, 15ns, 18ns, 20ns, 25ns, 26ns, 29ns, 30ns, 32ns, 35ns and 40ns; the laser frequency of the local laser treatment is 100KHz~400KHz, specifically, the laser frequency of the local laser treatment can be, for example, 100KHz, 150KHz, 200KHz, 250KHz, 300KHz, 350KHz and 400KHz; the comprehensive laser energy of the local laser treatment is 0.1J·cm -2 ~0.2J·cm -2 Specifically, the comprehensive laser energy of the local laser treatment may be, for example, 0.1 J·cm -2 , 0.13J·cm -2 , 0.15J·cm -2 , 0.18J·cm -2 and 0.2 J·cm -2 .
[0070] Step S300 , forming a first passivation layer 5 on the surface of the doped conductive layer 4 , and forming a second passivation layer 8 and an anti-reflection layer 9 on the surface of the emitter 12 .
[0071] Specifically, a first passivation layer 5 is formed on the surface of the doped conductive layer 4; the first passivation layer 5 may include but is not limited to at least one of silicon oxide, silicon nitride, silicon oxynitride, aluminum oxide, etc., or any combination thereof; for example, the first passivation layer 5 is composed of silicon nitride, and the silicon nitride thin film layer can play the role of an anti-reflection film, and the silicon nitride thin film has good insulation, density, stability and masking ability for impurity ions, and the silicon nitride thin film layer can have a passivation effect on the silicon substrate 1, thereby significantly improving the photoelectric conversion efficiency of the solar cell.
[0072] The thickness range of the first passivation layer 5 along the direction perpendicular to the silicon substrate 1 is 70nm~120nm. The thickness of the first passivation layer 5 along the direction perpendicular to the silicon substrate 1 can specifically be 70nm, 80nm, 90nm, 100nm or 120nm, etc., and of course it can also be other values within the above range, which is not limited here; when the first passivation layer 5 is a stacked silicon nitride layer and a silicon oxide layer or a stacked silicon nitride layer and a silicon oxynitride layer, the silicon nitride layer is located on the surface of the doped conductive layer 4, and the silicon oxide layer or the silicon oxynitride layer is located on the surface of the silicon nitride layer.
[0073] The second passivation layer 8 may include but is not limited to at least one of silicon oxide, silicon nitride, silicon oxynitride, aluminum oxide, etc., or any combination thereof; the second passivation layer 8 can produce a good passivation effect on the silicon substrate 1, which is helpful to improve the conversion efficiency of the battery; it should be noted that the second passivation layer 8 can also play a role in reducing the reflection of incident light; the thickness range of the second passivation layer 8 along the direction perpendicular to the silicon substrate 1 is 10nm~120nm, and the thickness of the second passivation layer 8 along the direction perpendicular to the silicon substrate 1 can specifically be 10nm, 20nm, 30nm, 42nm, 50nm, 60nm, 70nm, 80nm, 90nm, 100nm or 120nm, etc., of course, it can also be other values within the above range, which is not limited here.
[0074] Step S400 , penetrating the first passivation layer 5 to form a first electrode 2 in contact with the doped polysilicon layer, and penetrating the surface of the second passivation layer 8 to form a second electrode 10 in contact with the emitter 12 .
[0075] Specifically, a front main grid and a front sub-grid are printed on the front side of the silicon substrate 1 using a slurry, and the slurry is dried to form a corresponding second electrode 10, and a back main grid and a back sub-grid are printed on the back side of the silicon substrate 1 using a slurry, and the slurry is dried to form a corresponding first electrode 2, and finally the dried cell is sintered to obtain a solar cell; the specific material of the second electrode 10 and the first electrode 2 is not limited in this embodiment; for example, the second electrode 10 is a silver electrode or a silver / aluminum electrode, and the first electrode 2 is a silver electrode or a silver / aluminum electrode.
[0076] It should be noted that, unless otherwise specified in the present application, the various operation steps may be performed in sequence or not; this embodiment does not limit the sequence of steps for preparing solar cells, and it may be adjusted according to the actual production process.
[0077] See also Figure 3 As shown, Figure 3It is a schematic diagram of the structure of a photovoltaic module provided in this embodiment; a photovoltaic module provided in this embodiment includes a front cover plate 13, a first packaging film 14, a battery string 15, a second packaging film 16 and a back cover plate 17 arranged in a stacked manner; the battery string 15 is formed by connecting multiple solar cells 18 of any of the above embodiments.
[0078] Specifically, the photovoltaic module includes a front cover plate 13, a first packaging film 14, a battery string 15, a second packaging film 16 and a back cover plate 17 which are stacked; the battery string includes a plurality of solar cells 18 as described above which are connected by a conductive tape (not shown in the figure), and the connection between the solar cells 18 can be partial stacking or splicing; that is, the TOPCon cells are electrically connected in the form of a whole piece or multiple pieces to form a plurality of battery strings 15, and the plurality of battery strings 15 are then electrically connected in series and / or in parallel.
[0079] The front cover plate 13 can be made of glass with high light transmittance, which can reach more than 92%. Low-iron tempered embossed glass is generally used. The thickness of the front cover plate 13 along the direction perpendicular to the silicon substrate 1 can range from 2.7 mm to 3.2 mm. The thickness of the front cover plate 13 along the direction perpendicular to the silicon substrate 1 can be 2.7 mm, 3 mm, 3.1 mm or 3.2 mm. The thickness of the front cover plate 13 can be set according to actual conditions, and this embodiment does not specifically limit this. Within the wavelength range of 380 nm to 1100 nm of the spectral response of the solar cell, the light transmittance can reach more than 91%. For large 12 00nm infrared light has a higher reflectivity; the front cover plate 13 can be a conventional flat glass, and the shape of the front cover plate 13 is no longer limited in this embodiment, and can be square, round or other shapes, as long as it can achieve the purpose of this embodiment; of course, the front cover plate 13 can also be special-shaped glass, such as curved glass. This embodiment no longer limits the curvature angle corresponding to the curved glass, and can be set according to actual conditions, which can be 5 degrees, 10 degrees, 15 degrees, 20 degrees, or other degrees. It can be understood that the back cover plate 17 can be consistent with the front cover plate 13, of course, it can also be different.
[0080] The back cover 17 can be made of glass, TPT (polyvinyl fluoride composite film) or TPE (thermoplastic elastomer). The back cover 17 is used to protect the internal packaging materials and batteries from mechanical damage and external environmental corrosion. It also has good insulation properties, which largely determines the working life of the component. It has excellent weather resistance, low water vapor permeability, good electrical insulation, and a certain bonding strength. The thickness of the back cover 17 along the direction perpendicular to the silicon substrate 1 can range from 0.2mm to 3.2mm. The thickness of the back cover 17 along the direction perpendicular to the silicon substrate 1 can be 0.2mm, 1mm, 2mm, 3mm or 3.2mm.
[0081] The two sides of the first encapsulation film 14 are respectively in contact with the front cover plate 13 and the battery string 15, and the two sides of the second encapsulation film 16 are respectively in contact with the back cover plate 17 and the battery string 15; wherein, the first encapsulation film 14 and the second encapsulation film 16 can be ethylene-vinyl acetate copolymer (EVA) film, polyethylene octene co-elastic (POE) film or polyethylene terephthalate (PET) film. EVA (ethylene-vinyl acetate copolymer) has the advantages of excellent bonding performance, low melting temperature, good melt fluidity and softness, low cost, and easy construction. EVA material introduces vinyl acetate monomer into the molecular chain, which can reduce high crystallinity, improve toughness, impact resistance, filler solubility and heat sealing performance; POE (random copolymer elastomer of ethylene and high-carbon α-olefin); the molecular structure of POE material gives it excellent mechanical properties, rheological properties and UV resistance, and it also has good affinity with polyolefins, good low-temperature toughness, and high performance-price ratio; PVB (polyvinyl butyral) material, PVB material is soluble in methanol, ethanol, ketones, halogenated alkanes, and aromatic hydrocarbon solvents, and has good solubility with phthalates, sebacate plasticizers, as well as nitrocellulose, phenolic resin, epoxy resin, etc. It has high transparency, cold resistance, impact resistance, UV radiation resistance, and good adhesion to metals, glass, wood, ceramics, fiber products, etc.
[0082] The photovoltaic module can also adopt the full side encapsulation, that is, the side of the photovoltaic module is completely encapsulated by the encapsulation tape (not shown in the figure) to prevent the photovoltaic module from laminating and shifting during the lamination process. The photovoltaic module also includes an edge sealing component (not shown in the figure), which is fixedly encapsulated on part of the edge of the photovoltaic module; the edge sealing component can be fixedly encapsulated on the edge near the corner of the photovoltaic module. The edge sealing component can be a high-temperature resistant tape, which has excellent high-temperature resistance and will not decompose or fall off during the lamination process, and can ensure the reliable encapsulation of the photovoltaic module; wherein, the two ends of the high-temperature resistant tape are respectively fixed to the back cover plate 17 and the front cover plate 13; the two ends of the high-temperature resistant tape can be bonded to the back cover plate 17 and the front cover plate 13 respectively, and the middle part can realize the limitation of the side of the photovoltaic module to prevent the photovoltaic module from laminating and shifting during the lamination process.
[0083] See also Figure 4 As shown, Figure 4It is a structural schematic diagram of another photovoltaic module provided in this embodiment; the photovoltaic module also includes a frame 19, and the frame 19 can be made of aluminum alloy or stainless steel; when the frame 19 is made of aluminum alloy, the strength and corrosion resistance of the frame 19 are very good, and the frame 19 can support and protect the entire solar panel; the photovoltaic module can also be connected to an external photovoltaic bracket through the frame 19, and multiple photovoltaic modules can be connected to each other to form a photovoltaic power station.
[0084] It can be seen from the above embodiments that the solar cell and photovoltaic module provided by the present invention achieve at least the following beneficial effects:
[0085] The present invention provides a solar cell and a photovoltaic module, in which the thickness of the doped conductive layer remains unchanged from the first electrode to the symmetry axis of two adjacent first electrodes, but the total doping concentration gradually decreases, thereby reducing the optical loss of the doped conductive layer and the lateral transmission loss of the current, thereby improving the front cell efficiency and the cell bifaciality.
[0086] Although some specific embodiments of the present invention have been described in detail by way of example, it will be appreciated by those skilled in the art that the above examples are for illustration only and are not intended to limit the scope of the present invention. It will be appreciated by those skilled in the art that the above embodiments may be modified without departing from the scope and spirit of the present invention. The scope of the present invention is defined by the appended claims.
Claims
1. A solar cell, characterized in that: include: A silicon substrate and a first electrode; One side of the silicon substrate is provided with a tunneling oxide layer, a doped conductive layer and a first passivation layer in a stacked order in a direction away from the silicon substrate; the first electrode penetrates the first passivation layer and is electrically connected to the doped conductive layer; the doped conductive layer comprises at least one of silicon carbide and polycrystalline silicon, the thickness of the doped conductive layer along the direction perpendicular to the silicon substrate is constant, the doping concentration of the doped conductive layer gradually decreases from the first electrode to the symmetry axis of two adjacent first electrodes, and the doping concentration of the doped conductive layer decreases from the first electrode to the symmetry axis of two adjacent first electrodes by (1.7 to 17)×10 19 cm -3 ; The thickness of the doped conductive layer in a direction perpendicular to the silicon substrate ranges from 10 nm to 100 nm; A diffusion doping layer is further provided between the silicon substrate and the tunneling oxide layer, and the doping concentration in the diffusion doping layer gradually decreases from a side away from the silicon substrate to a side close to the silicon substrate.
2. A solar cell according to claim 1, characterized in that: The doping concentration of the doped conductive layer at the first electrode is in the range of (1 to 10)×10 20 cm -3 .
3. A solar cell according to claim 1, characterized in that: The doping concentration of the doped conductive layer at the symmetry axes of two adjacent first electrodes is in the range of (1 to 10)×10 19 cm -3 .
4. A solar cell according to claim 1, characterized in that: The doping concentration range of the diffuse doping layer away from the silicon substrate is 10 17 cm -3 ~10 21 cm -3 .
5. A solar cell according to claim 1, characterized in that: The doping concentration range of the diffusion doping layer close to the silicon substrate is 10 17 cm -3 ~10 19 cm -3 .
6. A solar cell according to claim 1, characterized in that: The thickness of the diffusion doping layer along a direction perpendicular to the silicon substrate ranges from 40 nm to 200 nm.
7. A solar cell according to any one of claims 2 to 6, characterized in that: The silicon substrate includes a base region and an emitter located on the surface of the base region away from the diffuse doping layer; the emitter is sequentially stacked with a second passivation layer and an anti-reflection layer in a direction away from the base region; the second electrode sequentially penetrates the anti-reflection layer and the second passivation layer and is electrically connected to the emitter.
8. A photovoltaic module, characterized in that: It comprises a front cover plate, a first packaging film, a battery string, a second packaging film and a back cover plate which are stacked; the battery string is formed by connecting the solar cells according to any one of claims 1 to 7.
Citation Information
Patent Citations
Solar cell, preparation method thereof and photovoltaic module
CN114975648A
Solar cell
CN210926046U