Solar cell detection method and detection device
By using high concentration of NaOH etching liquid and alkali-throwing additives, combined with temperature adjustment, the problem of large error and high cost of detection of thickness of TOPCon solar cell tunneling oxide layer is solved, and fast and accurate detection efficiency is achieved, suitable for mass production .
Patent Information
- Application Number
- CN202310331837.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-03-30
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2043-03-30
AI Technical Summary
The existing detection methods cannot effectively monitor the thickness of the tunneled oxide layer in TOPCon solar cells. The traditional methods have large errors and high costs, so they cannot be used in mass production.
The solar cell was soaked with an etching liquid containing high concentration of NaOH. By recording the time and bubbling of the etching liquid, the thickness of the tunneled oxide layer was calculated, and the color of the silicon base layer was observed uniformly. The uniformity is determined by combining optional alkali-throwing additives and temperature adjustment to improve detection efficiency and accuracy.
It realizes rapid and accurate detection of the thickness and uniformity of the tunneled oxide layer without complex equipment, improves detection efficiency, reduces costs, and is suitable for mass production.
Smart Images

Figure CN116344377B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of photovoltaic technology, and in particular to a detection method and a detection device for solar cells. Background Art
[0002] TOPCon cell technology is a breakthrough experimental progress made by Frank Feldmann and others from the Fraunhofer ISE Institute in Germany in 2013. Compared with other traditional solar cells, TOPCon solar cells can significantly improve the photoelectric conversion efficiency. Moreover, the domestic TOPCon solar cell market has already occupied a certain market share, and many photovoltaic companies can already conduct independent research and development and mass production. Therefore, TOPCon cell technology has extremely high industrial value.
[0003] The core technology of TOPCon battery is to use tunnel oxide layer and poly process to passivate the back of the battery. The thickness of the tunnel oxide layer is only about 1-2nm, which makes it difficult to monitor its thickness.
[0004] The error of the ellipsometer used to test the film thickness is greater than 1nm, so it cannot be used to detect the thickness of the tunnel oxide layer. When the laboratory tests the thickness of the tunnel oxide layer, it is generally necessary to use a TEM (transmission electron microscope) to test it. The cost and difficulty are too high, and the efficiency is also very low, so it cannot be used in mass production. Summary of the invention
[0005] The purpose of the present application is to provide a solar cell detection method and detection device, so as to partially or completely improve the problem of detecting the thickness of the tunneling oxide layer of the solar cell in the related art.
[0006] In a first aspect, an embodiment of the present application provides a method for detecting a solar cell, wherein the solar cell includes a substrate, the substrate includes a silicon-based layer, a tunneling oxide layer disposed on a first surface of the silicon-based layer, and a covering layer disposed on a second surface of the silicon-based layer; the detection method includes:
[0007] The substrate is immersed in an etching solution, and the time when the etching solution does not bubble is recorded as the first etching time; the first etching time is the time for the etching solution to etch the tunnel oxide layer, and the etching solution has a first etching speed for etching the tunnel oxide layer, and the product of the first etching speed and the first etching time is used to detect the thickness of the tunnel oxide layer; wherein the etching solution includes NaOH with a mass concentration of not less than 1%.
[0008] In the above implementation process, the substrate is immersed in an etching solution containing NaOH with a mass concentration of not less than 1%, and then the etching solution is observed, and the time when the etching solution does not bubble is recorded as the first etching time. Since the second surface of the silicon-based layer is provided with a covering layer, and the silicon-based layer is usually thin at the micron level, when the substrate is immersed in the etching solution, the tunneling oxide layer located on the surface will contact the etching solution and react slowly, and at this time, no bubbling phenomenon can be observed in the etching solution. After the tunneling oxide layer is etched, the first surface of the silicon-based layer under the tunneling oxide layer will contact the etching solution and react quickly, and the reaction speed is fast, and a large number of bubbles can be observed in the etching solution. Therefore, the time when the etching solution does not bubble is the time when the etching solution etches the tunneling oxide layer. Since the etching solution has a first etching speed for etching the tunneling oxide layer, the approximate thickness of the tunneling oxide layer can be calculated by multiplying the first etching time and the first etching speed.
[0009] By using the above detection method, the approximate thickness of the tunnel oxide layer can be quickly detected without the need for complex detection equipment, thereby improving detection efficiency.
[0010] In combination with the first aspect, in an optional implementation of the present application, the detection method further includes: after the etching solution etches the silicon base layer for a preset time, observing the color uniformity of the surface of the silicon base layer to determine the uniformity of the tunneling oxide layer.
[0011] Optionally, the preset time is 20-30s.
[0012] In the above implementation process, by observing the uniformity of the surface color of the silicon-based layer after etching in the etching solution, the uniformity of the thickness of the tunneling oxide layer can be determined. If the brightness of the silicon-based layer surface is different, it indicates that the thickness of the tunneling oxide layer is uneven.
[0013] In combination with the first aspect, in an optional implementation manner of the present application, the chemical composition of the tunneling oxide layer includes silicon oxide, and the etching solution includes NaOH with a mass concentration of not less than 3%.
[0014] In the above implementation process, the etching solution contains NaOH with a mass concentration of not less than 3%, which can further accelerate the reaction speed of the silicon base layer in the etching solution without accelerating the speed of etching the tunneling oxide layer. Therefore, the time when the etching solution starts to bubbling can be more clearly observed, and the bubbling phenomenon is more obvious, so as to improve the detection efficiency and detection accuracy.
[0015] In combination with the first aspect, in an optional embodiment of the present application, the etching solution also includes an alkali polishing additive.
[0016] In the above implementation process, adding an alkali polishing additive can make the bubbling phenomenon more obvious, and can more easily distinguish the phenomenon before and after the etching solution bubbling, thereby improving the accuracy of the recorded first etching time and reducing the detection error.
[0017] In combination with the first aspect, in an optional embodiment of the present application, the etching solution includes an alkali polishing additive with a mass concentration of 1% and NaOH with a mass concentration of not less than 3%, and the temperature of the etching solution is 40-60°C.
[0018] Optionally, the etching solution includes 1% by mass concentration of an alkali polishing additive and 3% by mass concentration of NaOH, the temperature of the etching solution is 48-52° C., and the first etching speed is 0.01 nm / s.
[0019] In the above implementation process, the etching solution contains NaOH with a mass concentration of not less than 3% and an alkali polishing additive with a mass concentration of 1%. At an etching temperature of 50±2° C., the etching solution can etch the tunnel oxide layer at an etching speed of 0.01 nm / s.
[0020] In combination with the first aspect, in an optional embodiment of the present application, the substrate further includes a polycrystalline / amorphous silicon layer disposed on the tunneling oxide layer; and the detection method includes:
[0021] The substrate is immersed in the etching solution until the first bubble appears in the etching solution; the time when the immersion starts is recorded as the first moment, and the end time of the first bubble is recorded as the second moment; then the time when the etching solution starts to bubble for the second time is recorded as the third moment; the difference between the third moment and the second moment is the first etching time.
[0022] Optionally, the difference between the second moment and the first moment is a second etching time of the etching solution etching the polycrystalline / amorphous silicon layer, the etching solution has a second etching speed for etching the polycrystalline / amorphous silicon layer, and the thickness of the polycrystalline / amorphous silicon layer is detected using the product of the second etching time and the second etching speed.
[0023] In the above implementation process, when detecting a solar cell with a polycrystalline / amorphous silicon layer disposed on the surface of the tunneling oxide layer, the substrate of the solar cell can be immersed in an etching solution. Since the etching speeds of the polycrystalline / amorphous silicon layer, the tunneling oxide layer and the silicon-based layer in the etching solution are different, after the substrate of the solar cell is immersed in the etching solution, first, the etching solution will react rapidly with the polycrystalline / amorphous silicon layer on the surface, and a large number of bubbles will be observed to appear in the etching solution for the first time; after the etching of the polycrystalline / amorphous silicon layer is completed, the tunneling oxide layer is exposed to the etching solution and reacts slowly with the etching solution, and bubbles cannot be observed in the etching solution at this time; after the etching of the tunneling oxide layer is completed, the first surface of the silicon-based layer will be exposed to the etching solution and react rapidly with the etching solution, and at this time, a large number of bubbles can be observed to appear in the etching solution for the second time. The etching solution has a specific second etching speed when etching the polycrystalline / amorphous silicon layer. Therefore, the difference between the second moment and the first moment can be used as the second etching time for the etching solution to etch the polycrystalline / amorphous silicon layer, and the thickness of the polycrystalline / amorphous silicon layer can be calculated by the product of the second etching time and the second etching speed. The difference between the start time of the second bubbling (i.e., the third moment) and the end time of the first bubbling (i.e., the second moment) is the first etching time when no bubbling occurs.
[0024] In combination with the first aspect, in an optional embodiment of the present application, the substrate also includes a phosphosilicate glass layer arranged on the polycrystalline / amorphous silicon layer; before immersing the substrate in the etching solution, the substrate is pretreated with a pretreatment agent to remove the phosphosilicate glass layer; the pretreatment agent includes HF.
[0025] In the solar cell, a phosphosilicate glass layer is also provided on the surface of the polycrystalline / amorphous silicon layer. When detecting the thickness of the tunneling oxide layer and the polycrystalline / amorphous silicon layer of the solar cell, the phosphosilicate glass layer can be first removed using a pretreatment agent containing HF, so that the solar cell can be treated with an etching solution to obtain the thickness data of the tunneling oxide layer or the polycrystalline / amorphous silicon layer of the solar cell.
[0026] In a second aspect, an embodiment of the present application provides a solar cell detection device, comprising:
[0027] A transparent etching tank, configured to contain etching liquid;
[0028] A temperature regulator is disposed on the wall of the etching tank and is configured to adjust the temperature of the etching solution in the etching tank;
[0029] A clamp, equipped to hold the solar cell in and out of the etching tank;
[0030] A timer is provided to record the time when the solar cell is immersed in the etching solution, and the start time and the end time when the etching solution bubbles.
[0031] In the above implementation process, a transparent etching tank is set so that the solar cell to be tested can be immersed in the etching solution in the transparent etching tank using a clamp, and the bubbling of the etching solution in the etching tank is observed. At the same time, a timer is used to record the time when the solar cell is immersed in the etching solution, as well as the time when the etching solution starts to bubble and the time when the bubbling phenomenon ends, so that the operator can obtain the etching time of the corresponding layer structure according to the time difference before and after the bubbling, and calculate the corresponding layer thickness of the solar cell, such as the tunneling oxide layer or the polycrystalline / amorphous silicon layer, according to the etching time and etching speed.
[0032] In addition, a temperature regulator is provided to adjust the reaction temperature during the etching process, thereby further reducing the detection error.
[0033] In combination with the second aspect, in an optional embodiment of the present application, the temperature regulator includes a heating tank and a heating element; the heating tank is configured to place the etching tank and to contain the heating medium filled between the outer wall of the etching tank and the inner wall of the heating tank; the heating element is configured to heat the heating medium.
[0034] In the above implementation process, the etching tank is placed in the heating tank, and the temperature of the etching tank can be adjusted by heating the heating medium through the heating element.
[0035] In combination with the second aspect, in an optional implementation of the present application, the detection device includes a slot cover, which can selectively close and expose the etching slot; and the clamp is connected to the slot cover.
[0036] In the above implementation process, a slot cover is provided at the etching slot to further maintain the etching temperature in the etching slot. In addition, the clip is connected to the slot cover, and the etching slot can be closed by the slot cover while the solar cell in the clip is immersed in the etching solution, simplifying the operation process. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the drawings required for use in the embodiments will be briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present application and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without paying creative work.
[0038] Figure 1 is a schematic cross-sectional view of a solar cell;
[0039] Figure 2 A schematic diagram of the operation flow of the detection method provided for the example of this application;
[0040] Figure 3 A schematic diagram of the structure of the detection device provided for the example of this application;
[0041] Figure 4This is an optical picture of the silicon-based layer after detection by the detection method provided in Example 1 of the present application.
[0042] Icons: 100 - solar cell; 110 - substrate; 111 - silicon base layer; 112 - tunneling oxide layer; 113 - cover layer; 114 - polycrystalline / amorphous silicon layer; 115 - phosphosilicate glass layer;
[0043] 1-detection device; 10-etching tank; 20-temperature regulator; 21-heating tank; 22-heating element; 30-clip holder; 40-timer; 50-tank cover. DETAILED DESCRIPTION
[0044] The following embodiments of the technical solution of the present application are described in detail in conjunction with the accompanying drawings. The following embodiments are only used to more clearly illustrate the technical solution of the present application, and are therefore only used as examples, and cannot be used to limit the scope of protection of the present application.
[0045] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by technicians in the technical field to which this application belongs; the terms used herein are only for the purpose of describing specific embodiments and are not intended to limit this application; the terms "including" and "having" in the specification of this application and the above-mentioned drawings and any variations thereof are intended to cover non-exclusive inclusions.
[0046] In the description of the embodiments of the present application, technical terms such as "first" and "second" are only used to distinguish different objects and cannot be understood as indicating or implying relative importance or implicitly indicating the number, specific order or primary and secondary relationship of the indicated technical features.
[0047] Reference to "embodiments" herein means that a particular feature, structure, or characteristic described in conjunction with the embodiments may be included in at least one embodiment of the present application. The appearance of the phrase in various locations in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments. It is explicitly and implicitly understood by those skilled in the art that the embodiments described herein may be combined with other embodiments.
[0048] In the description of the embodiments of the present application, the orientations or positional relationships indicated by technical terms such as "middle", "bottom", and "inside" are based on the orientations or positional relationships shown in the accompanying drawings and are only for the convenience of describing the embodiments of the present application and simplifying the description. They do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the embodiments of the present application.
[0049] In the description of the embodiments of the present application, unless otherwise clearly specified and limited, technical terms such as "connection" and "fixation" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, and it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the embodiments of the present application can be understood according to specific circumstances.
[0050] TOPCon cells have a high photoelectric conversion efficiency. The core technology of TOPCon cells is to use tunneling oxide layer and poly process to passivate the back of the cell. Figure 1 The solar cell 100 includes a substrate 110 , which includes a silicon-based layer 111 , a tunneling oxide layer 112 disposed on a first surface of the silicon-based layer 111 , and a capping layer 113 disposed on a second surface of the silicon-based layer 111 .
[0051] The present application does not limit the specific type of the covering layer 113. One purpose of providing the covering layer on the second surface of the silicon-based layer 111 is to prevent the second surface of the silicon-based layer 111 from rapidly reacting with the etching solution and generating a large number of bubbles.
[0052] For example, the cover layer 113 may include a doping layer, a passivation layer, and an anti-reflection layer stacked in sequence.
[0053] It is worth noting that the chemical composition of the covering layer 113 can react slowly with the etching solution, and no bubbling phenomenon can occur during the reaction. In addition, if the covering layer 113 can react slowly with the etching solution, the thickness of the covering layer 113 cannot be less than the sum of the thicknesses of the tunneling oxide layer 112 and the polycrystalline / amorphous silicon layer 114. That is, the covering layer 113 cannot be completely etched before the first surface of the silicon-based layer 111 is exposed to the etching solution, and before the first surface of the silicon-based layer 111 is exposed to the etching solution, the second surface of the silicon-based layer 111 is always covered with the covering layer 113.
[0054] For example, the chemical composition of the capping layer 113 may be silicon oxide, but the thickness of the capping layer 113 is greater than the sum of the thicknesses of the tunneling oxide layer 112 and the polycrystalline / amorphous silicon layer 114 .
[0055] Furthermore, a polycrystalline / amorphous silicon layer 114 may be disposed on the tunneling oxide layer 112. Furthermore, a phosphorus silicon glass layer 115 may be disposed on the polycrystalline / amorphous silicon layer 114. The thickness of the tunneling oxide layer 112 is only about 1 to 2 nm, and it is difficult to monitor its thickness.
[0056] The thickness measuring instrument using the existing technology has a large error. For example, the error of the ellipsometer used to test the film thickness is greater than 1nm, so it cannot be used to test the thickness of the tunneling oxide layer 112. Alternatively, a TEM (transmission electron microscope) is used to test the thickness of the tunneling oxide layer 112. However, the operation of the transmission electron microscope is complicated, the testing cost and difficulty are too high, and the efficiency is also very low, so it cannot be mass-produced.
[0057] Therefore, the present application provides a detection method of a solar cell 100 to improve the problem of detecting the thickness of the tunnel oxide layer 112 of the solar cell 100 .
[0058] When testing a solar cell 100 in which the substrate 110 includes a silicon-based layer 111, a tunneling oxide layer 112 disposed on a first surface of the silicon-based layer 111, and a capping layer 113 disposed on a second surface of the silicon-based layer 111, refer to Figure 2 , detection methods include:
[0059] S1, immersing the substrate 110 in an etching solution, recording the time when the etching solution does not bubble, and recording it as a first etching time; the first etching time is the time for the etching solution to etch the tunnel oxide layer 112, and the etching solution has a first etching speed for etching the tunnel oxide layer 112. The thickness of the tunnel oxide layer 112 is calculated by the product of the first etching speed and the first etching time.
[0060] Wherein, the etching solution includes NaOH with a mass concentration of not less than 1%.
[0061] The substrate 110 is immersed in the etching solution. Since the second surface of the silicon-based layer 111 is provided with a covering layer 113, and the thickness of the covering layer 113 is thicker than the tunneling oxide layer 112, the second surface of the silicon-based layer 111 will not contact the etching solution during etching. In addition, the layer thickness of the silicon-based layer 111 is relatively thin, at the micron level, so even if the surrounding of the silicon-based layer 111 contacts the etching solution, a large amount of bubbling will not be observed in the etching solution. Since the tunneling oxide layer 112 is located on the surface layer of the substrate 110, the tunneling oxide layer 112 will react with the etching solution after contacting with the etching solution. The main chemical component of the tunneling oxide layer 112 is silicon oxide. After the tunneling oxide layer 112 contacts with the etching solution, the tunneling oxide layer 112 will react slowly with the etching solution, and no bubbling can be observed in the etching solution.
[0062] After the tunnel oxide layer 112 is etched, the silicon base layer 111 is exposed to the etching solution. The chemical composition of the silicon base layer 111 is mainly silicon. After silicon contacts the etching solution, a rapid reaction will occur, and obvious bubbling can be observed in the etching solution.
[0063] Therefore, the time when the etching solution does not bubble is recorded as the etching time of the tunnel oxide layer 112. Since the etching solution has a first etching speed for etching the tunnel oxide layer 112, the approximate thickness of the tunnel oxide layer 112 can be calculated by multiplying the first etching time and the first etching speed.
[0064] Furthermore, the thickness uniformity of the tunnel oxide layer 112 can be determined by observing the light and dark colors at different locations on the surface of the silicon-based layer 111 after the etching solution bubbles. If the light and dark colors on the surface of the silicon-based layer 111 are uneven, it indicates that the thickness of the tunnel oxide layer 112 is uneven.
[0065] By using the detection method provided in this example, taking advantage of the different reaction characteristics of the tunneling oxide layer 112 and the silicon-based layer 111 when reacting with the same etching solution, the approximate thickness and thickness uniformity of the tunneling oxide layer 112 can be quickly detected without the need for complex detection equipment such as a transmission electron microscope, thereby improving detection efficiency.
[0066] Furthermore, in the solar cell 100 , a POLY layer, ie, a polycrystalline / amorphous silicon layer 114 is often provided on the surface of the tunnel oxide layer 112 .
[0067] When testing the thickness of the tunnel oxide layer 112 in the solar cell 100 provided with the polycrystalline / amorphous silicon layer 114, please continue to refer to Figure 1 , detection methods include:
[0068] S101, immersing the substrate 110 in an etching solution, and the etching solution bubbles for the first time. Recording the time when the immersion starts, which is recorded as the first moment, and recording the time when the first bubble ends, which is recorded as the second moment.
[0069] The difference between the second moment and the first moment is a second etching time for the etching solution to etch the polycrystalline / amorphous silicon layer 114, and the etching solution has a second etching speed for etching the polycrystalline / amorphous silicon layer 114. In a possible implementation, the thickness of the polycrystalline / amorphous silicon layer 114 can be calculated using the product of the second etching time and the second etching speed.
[0070] S102, then record the time when the etching solution starts to bubble for the second time, which is recorded as the third moment. The difference between the third moment and the second moment is the first etching time.
[0071] When testing a substrate 110 having a polycrystalline / amorphous silicon layer 114 disposed on the surface of the tunnel oxide layer 112, the substrate 110 can be immersed in an etching solution. The etching speeds of the polycrystalline / amorphous silicon layer 114, the tunnel oxide layer 112 and the silicon-based layer 111 in the etching solution are different. Therefore, when the substrate 110 is immersed in the etching solution, the etching solution will react quickly with the surface polycrystalline / amorphous silicon layer 114, and a large number of bubbles are observed in the etching solution. Therefore, the time when the substrate 110 starts to be immersed is recorded as the first moment, and the first moment is the time when the polycrystalline / amorphous silicon layer 114 just starts to contact with the etching solution.
[0072] After the etching of the polycrystalline / amorphous silicon layer 114 is completed, the tunnel oxide layer 112 located under the polycrystalline / amorphous silicon layer 114 is exposed to the etching solution and reacts slowly with the etching solution. At this time, no bubbles can be observed in the etching solution. Therefore, the time when the first bubbling of the etching solution is recorded is the time when the etching of the polycrystalline / amorphous silicon layer 114 is completed, and it is also the time when the tunnel oxide layer 112 begins to contact the etching solution, which is recorded as the second moment. Therefore, the difference between the second moment and the first moment is the second etching time of the polycrystalline / amorphous silicon layer 114. Since the etching solution has a second etching speed for etching the polycrystalline / amorphous silicon layer 114, the thickness value of the polycrystalline / amorphous silicon layer 114 can be calculated using the product of the second etching time and the second etching speed.
[0073] After the tunnel oxide layer 112 is etched, the first surface of the silicon-based layer 111 below the tunnel oxide layer 112 will be exposed to the etching solution and react rapidly with the etching solution. At this time, a large amount of bubbling can be observed in the etching solution for the second time. Therefore, the time when the etching solution bubbles for the second time is the time when the tunnel oxide layer 112 is etched, and the time when the second bubble appears is recorded as the third moment. Therefore, the difference between the third moment and the second moment is the first etching time of the tunnel oxide layer 112. The thickness value of the tunnel oxide layer 112 can be calculated by using the product of the first etching time and the first etching rate.
[0074] Furthermore, in the solar cell 100, a phosphosilicate glass layer 115 may be provided on the polycrystalline / amorphous silicon layer 114. When testing the solar cell 100 provided with the phosphosilicate glass layer 115, the phosphosilicate glass layer 115 may be removed by using a pretreatment agent to expose the polycrystalline / amorphous silicon layer 114 to the surface. Then, the substrate 110 after the phosphosilicate glass layer 115 is removed is immersed in an etching solution, and the bubbling of the etching solution and the corresponding time are observed.
[0075] Exemplarily, the pretreatment agent is HF.
[0076] Furthermore, in order to further improve the detection quality, in a possible implementation manner, an alkali polishing additive is also added to the etching solution.
[0077] Exemplarily, the etching solution includes 1% by mass concentration of an alkali polishing additive and not less than 3% by mass concentration of NaOH.
[0078] Exemplarily, the etching solution includes 1% by mass concentration of the alkaline polishing additive and 3% by mass concentration of NaOH.
[0079] Further, the present application does not limit how to obtain the first etching rate of the etching solution for etching the tunnel oxide layer 112, and the second etching rate of the etching solution for etching the polycrystalline / amorphous silicon layer 114. In a possible implementation, the etching solution is used to etch the tunnel oxide layer 112 or the polycrystalline / amorphous silicon layer 114 of known thickness, and the etching time is recorded. The corresponding first etching rate or second etching rate is obtained by dividing the known thickness by the etching time.
[0080] For example, using 1% mass concentration of alkaline polishing additive and 3% mass concentration of NaOH, a 1 nm thick tunnel oxide layer 112 is etched at an etching temperature of 40-60° C., and the etching time is recorded as 100 s. The first etching rate is calculated to be 0.01 nm / s.
[0081] Furthermore, in order to facilitate the detection of the solar cell 100 using the detection method provided in this example, in a possible implementation, the example of the present application also provides a detection device 1.
[0082] See also Figure 3 The detection device 1 includes a transparent etching tank 10, a temperature regulator 20, a clamp 30 and a timer 40. The etching tank 10 is configured to contain etching liquid. The temperature regulator 20 is arranged outside the tank wall of the etching tank 10, and is configured to adjust the temperature of the etching liquid in the etching tank 10. The clamp 30 is configured to clamp the solar cell 100 in and out of the etching tank 10. The timer 40 is configured to record the time when the solar cell 100 is immersed in the etching liquid, as well as the start time and end time of the bubbling of the etching liquid.
[0083] A transparent etching groove 10 is provided to facilitate observation of the bubbling of the etching solution in the etching groove 10 .
[0084] The present application does not limit the specific configuration of the etching groove 10 . In a possible implementation, the etching groove 10 is made of a transparent heat-resistant PP material.
[0085] Further, the present application does not limit the specific configuration of the temperature regulator 20. In a possible implementation, the temperature regulator 20 includes a heating tank 21 and a heating element 22. The heating tank 21 is configured to place the etching tank 10 and to contain a heating medium filled between the outer wall of the etching tank 10 and the inner wall of the heating tank 21. The heating element 22 is configured to heat the heating medium.
[0086] Furthermore, the heating tank 21 is made of transparent tempered glass to facilitate observation of the bubbling of the etching liquid in the etching tank 10 .
[0087] Furthermore, the heating medium is water, and the heating element 22 is a heating wire.
[0088] Furthermore, a circulation pump may be provided in the heating tank 21 to increase the fluidity and temperature uniformity of the heating medium.
[0089] Furthermore, thermometers may be placed in the heating medium and the etching solution to facilitate observation of the temperatures of the heating medium and the etching solution.
[0090] The clamp 30 is used to clamp the solar cell 100 to be tested and immerse the solar cell 100 into the etching solution.
[0091] Exemplarily, the clip 30 includes a first clip and a second clip that are movably connected. The first clip and the second clip are close to each other to clamp the solar cell 100 between the first clip and the second clip.
[0092] Furthermore, the first clamp and the second clamp are used to clamp the side of the solar cell 100 to prevent the solar cell 100 from falling out of the clamp 30 due to the reduction of the thickness of the solar cell 100 caused by etching.
[0093] Furthermore, in order to facilitate the fixation of the clip 30 and maintain the temperature of the etching solution, in a possible implementation, a slot cover 50 may be provided. When the solar cell 100 needs to be processed, the clip 30 is connected to the inner wall of the slot cover 50, the solar cell 100 is clamped in the clip 30, and the etching slot 10 is closed by the slot cover 50, so that the solar cell 100 is immersed in the etching solution.
[0094] The timer 40 is used to record time as needed.
[0095] Exemplarily, when the detection device 1 provided in this example is used to detect the solar cell 100 provided with the polycrystalline / amorphous silicon layer 114, the etching solution can be poured into the etching tank 10, and the etching tank 10 can be placed in the heating tank 21. The heating medium is heated by the heating element 22, and the thermometer is observed to maintain the temperature of the etching solution at 30-40°C. Then the solar cell 100 can be clamped in the clamp 30, and the tank cover 50 is closed to immerse the solar cell 100 in the etching solution. The timer 40 is used to record the time when the solar cell 100 is immersed in the etching solution, which is recorded as the first moment. At the same time, it is observed that the etching solution begins to bubble for the first time. Continue to observe the bubbling of the etching solution in the etching tank 10. When the bubbling of the etching solution ends, the timer 40 is used to record the time when the first bubbling ends, which is recorded as the second moment. Then, continue to observe the etching solution. After a period of time, the etching solution begins to bubble for the second time, and the timer 40 is used to record the start time of the second bubbling phenomenon, which is recorded as the third moment.
[0096] The second etching time is calculated using the difference between the second moment and the first moment, and the thickness of the polycrystalline / amorphous silicon layer 114 can be calculated using the product of the second etching time and the second etching speed.
[0097] The first etching time is calculated by using the difference between the third moment and the second moment. The thickness of the tunnel oxide layer 112 can be calculated by using the product of the first etching time and the first etching speed.
[0098] In order to make the purpose, technical scheme and advantages of the embodiments of the present application clearer, the technical scheme in the embodiments of the present application will be described clearly and completely below. If the specific conditions are not specified in the embodiments, they are carried out according to the conventional conditions or the conditions recommended by the manufacturer. If the manufacturer is not specified for the reagents or instruments used, they are all conventional products that can be purchased commercially.
[0099] Example 1
[0100] Embodiment 1 of the present application provides a detection method for a solar cell 100, wherein the solar cell 100 includes a substrate 110, a polycrystalline / amorphous silicon layer 114 disposed on a tunneling oxide layer 112, and a phosphosilicate glass layer 115 disposed on the polycrystalline / amorphous silicon layer 114. The thickness of the polycrystalline / amorphous silicon layer 114 and the thickness of the tunneling oxide layer 112 are detected using the detection device 1 provided in the example of the present application. The detection method is as follows:
[0101] HF is used to wash away the phosphosilicate glass layer 115 on the surface of the solar cell 100. The temperature regulator 20 is adjusted to make the temperature of the etching solution between 40-60°C. Then, the solar cell 100 after washing away the phosphosilicate glass layer 115 using the clamp 30 is immersed in the etching solution. The time for immersing the solar cell 100 in the etching solution is recorded using the timer 40, which is recorded as the first moment. At the same time, the first bubbling phenomenon of the etching solution in the etching tank 10 is observed. When the first bubbling phenomenon of the etching solution ends, the time when the first bubbling ends is recorded using the timer 40, which is recorded as the second moment. The bubbling of the etching solution in the etching tank 10 is continued to be observed. After a period of time, the etching solution has a second bubbling phenomenon, and the time when the second bubbling starts is recorded using the timer 40, which is recorded as the third moment.
[0102] The etching solution includes 1% mass concentration of NaOH and 1% mass concentration of alkali polishing additive. The difference between the second moment and the first moment is the second etching time: 50s. The difference between the third moment and the second moment is the first etching time: 150s.
[0103] The thickness of the tunnel oxide layer 112 is calculated to be 1.5 nm using the product of the first etching time 150 s and the first etching rate 0.01 nm / s.
[0104] The surface morphology of the silicon-based layer 111 in the etching solution after the second bubbling phenomenon is observed. The observation time is 30 seconds after the second bubbling begins. Figure 4 As shown. Figure 4 It can be seen that the edge of the silicon-based layer 111 shows obvious color unevenness compared with the middle portion, indicating that there is a large deviation in thickness between the edge and middle portions of the tunnel oxide layer 112 on the silicon-based layer 111 .
[0105] The above description is only the preferred embodiment of the present application and is not intended to limit the present application. For those skilled in the art, the present application may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present application shall be included in the protection scope of the present application.
Claims
1. A method for detecting a solar cell, characterized in that: The solar cell comprises a substrate, wherein the substrate comprises a silicon-based layer, a tunneling oxide layer disposed on a first surface of the silicon-based layer, and a covering layer disposed on a second surface of the silicon-based layer; the detection method comprises: The substrate is immersed in an etching solution, and the time when the etching solution does not bubble is recorded as a first etching time; the first etching time is the time for the etching solution to etch the tunnel oxide layer, and the etching solution has a first etching speed for etching the tunnel oxide layer, and the thickness of the tunnel oxide layer is calculated using the product of the first etching speed and the first etching time; wherein the etching solution includes NaOH with a mass concentration of not less than 1%.
2. The solar cell detection method according to claim 1, characterized in that: The detection method further includes: after the etching solution etches the silicon-based layer for a preset time, observing the color uniformity of the surface of the silicon-based layer to determine the uniformity of the tunneling oxide layer.
3. The solar cell detection method according to claim 2, characterized in that: The preset time is 20-30s.
4. The solar cell detection method according to claim 1, characterized in that: The chemical composition of the tunnel oxide layer includes silicon oxide, and the etching solution includes NaOH with a mass concentration of not less than 3%.
5. The solar cell detection method according to claim 1, characterized in that: The etching solution also includes an alkali polishing additive.
6. The solar cell detection method according to claim 5, characterized in that: The etching solution comprises an alkali polishing additive with a mass concentration of 1% and NaOH with a mass concentration of not less than 3%, and the temperature of the etching solution is 40-60°C.
7. The solar cell detection method according to claim 6, characterized in that: The etching solution includes 1% by mass concentration of an alkali polishing additive and 3% by mass concentration of NaOH. The temperature of the etching solution is 48-52° C., and the first etching speed is 0.01 nm / s.
8. The solar cell detection method according to any one of claims 1 to 7, characterized in that: The substrate further includes a polycrystalline / amorphous silicon layer disposed on the tunneling oxide layer; and the detection method includes: The substrate is immersed in the etching solution until the etching solution bubbles for the first time; the time when the immersion starts is recorded as the first moment; the time when the first bubble ends is recorded as the second moment; and the time when the etching solution starts to bubble for the second time is recorded as the third moment; The difference between the third moment and the second moment is the first etching time.
9. The solar cell detection method according to claim 8, characterized in that: The difference between the second moment and the first moment is a second etching time of the etching solution etching the polycrystalline / amorphous silicon layer. The etching solution has a second etching speed for etching the polycrystalline / amorphous silicon layer. The product of the second etching time and the second etching speed is used to detect the thickness of the polycrystalline / amorphous silicon layer.
10. The solar cell detection method according to claim 9, characterized in that: The substrate also includes a phosphosilicate glass layer disposed on the polycrystalline / amorphous silicon layer; before the substrate is immersed in the etching solution, the substrate is pretreated with a pretreatment agent to remove the phosphosilicate glass layer; the pretreatment agent includes HF.