A rare earth-containing additive and preparation method thereof
By using a gas-solid two-phase structure and a streamlined shell in rare earth additives, the problem of mixing uniformity of rare earths in molten steel is solved, the yield and distribution uniformity of rare earths are improved, the influence of oxide inclusions is overcome, and the rare earth Efficient use in steel.
Patent Information
- Application Number
- CN202310478230.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-04-28
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2043-04-28
AI Technical Summary
The mixing uniformity of rare earths in molten steel is poor, resulting in serious segregation of components, and the excellent effects of rare earths cannot be fully exerted. In addition, the oxide inclusions in commercially available rare earth additives are generally large and difficult to control.
A rare earth additive with a gas-solid two-phase structure sealed inside the shell is used. The gas at a preset pressure pushes the internal rare earth alloy when the shell becomes thinner, so that it is evenly distributed in the molten steel. A streamlined shell is used to reduce resistance and improve penetration. depth.
It achieves the uniform dispersion of rare earths in steel, improves the yield and distribution uniformity of rare earths, reduces the impact of oxide inclusions on steel properties, and significantly enhances the role of rare earths in steel.
Smart Images

Figure CN116574864B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of rare earth alloys, and in particular to an additive containing rare earth and a preparation method thereof. Background Art
[0002] Adding rare earth to steel can deoxidize and purify the molten steel, spheroidize sulfide inclusions, reduce the anisotropy of the material, and improve the transverse impact performance of the rolled material; it can also be used as a microalloying element to affect the evolution of the material's microstructure. Since the density, melting point, and reactivity of rare earth and other physical and chemical properties are very different from those of the steel matrix, it is difficult to mix the rare earth evenly after adding it to the molten steel, and the components are severely segregated, which greatly reduces the effect of rare earth addition and makes it impossible to give full play to the excellent role of rare earth. Therefore, how to add rare earth to the molten steel evenly and effectively to maximize the role of rare earth is a difficult problem that needs to be solved in this field.
[0003] At present, the commonly used method in industry is to put rare earth intermediate alloys in the form of solid blocks, ingots, filaments, powders, rods or rare earth cored wires into molten steel, and rely on self-diffusion and soft blowing of the molten steel after it melts to evenly mix the rare earth and molten steel. However, considering that a bag of molten steel often weighs hundreds of tons, and the time from rare earth addition to casting is short, the above rare earth additives often cause uneven distribution and severe segregation after being added to molten steel, which makes it impossible to fully exert the role of rare earth. Secondly, the oxide inclusions in the rare earth additives have a great influence on the final performance of the steel. The rare earth oxide inclusions in the rare earth additives currently on the market are generally large and difficult to control. Summary of the invention
[0004] The purpose of the embodiment of the present invention is to provide a rare earth-containing additive and a preparation method thereof. By adopting a gas-solid two-phase structure sealed inside a shell, after the additive is added to molten steel, as the outer shell wall becomes thinner, the gas breaks through the shell and pushes the internal solid additive in all directions, thereby improving the uniformity of rare earth distribution in the final product and the rare earth yield.
[0005] To solve the above technical problems, the first aspect of the embodiments of the present invention provides a rare earth-containing additive and a preparation method thereof, comprising: a sealed shell and a plurality of master alloys arranged inside the shell; wherein the master alloy contains rare earth elements;
[0006] The shell is filled with gas at a preset pressure.
[0007] Furthermore, the shell has a shape of a cuboid, a sphere, a cylinder, a truncated cone, a cone, or a streamline.
[0008] Further, the housing comprises: a front housing and a rear housing;
[0009] The front shell is integrally connected to the edge of the rear shell, and the plurality of intermediate alloys and the gas are located in a closed space between the front shell and the rear shell.
[0010] Furthermore, the counterweight of the front shell is greater than the counterweight of the rear shell.
[0011] Furthermore, the profile of the streamlined front housing satisfies the following mathematical expression obtained by rotating one circle around the x-axis:
[0012]
[0013] Wherein, x is the coordinate value of the front shell in the X-axis direction, y is the coordinate value of the Y-axis direction perpendicular to the axial direction of the front shell, the origin of the XY-axis coordinates is at the center point of the interface between the front shell and the rear shell, R is the minor axis radius value of the ellipse where the central axis section of the front shell is located, and L is the major axis radius value of the ellipse where the central axis section of the front shell is located;
[0014] The length of the front shell along the length direction of the shell is greater than the length of the rear shell along the length direction of the shell, and the maximum diameter B of the rear shell along the Y-axis direction is less than or equal to 2R.
[0015] Further, the master alloy includes: rare earth metal and iron;
[0016] The rare earth metal content is 8wt% to 90wt%, and the iron content is 10wt% to 92wt%;
[0017] Among them, the oxygen content is less than 150ppm, the maximum size of inclusions is less than 30μm, and the total amount of inclusions is less than 0.5wt%.
[0018] Further, the intermediate alloy composition is RE-Fe-M, M is a transition metal, and the transition metal includes: at least one of nickel, chromium, tungsten, molybdenum, cobalt, manganese, vanadium, niobium, and titanium; preferably, the transition metal includes: at least one of chromium, tungsten, molybdenum, vanadium, niobium, and titanium;
[0019] In the master alloy, the rare earth metal content is 15wt% to 70wt%, the transition metal content is 0.1wt% to 15wt%, and the iron content is 20wt% to 70wt%;
[0020] The oxygen content of the rare earth-containing additive is less than 100 ppm, the carbon content is less than 300 ppm, the maximum size of inclusions is less than 25 μm, and the total amount of inclusions is less than 0.1 wt%.
[0021] Further, the rare earth metal includes at least one of lanthanum, cerium, praseodymium, neodymium, samarium, europium, gadolinium, terbium, dysprosium, holmium, erbium, thulium, ytterbium, lutetium, scandium and yttrium;
[0022] Preferably, the rare earth metal includes at least one of lanthanum, cerium and yttrium.
[0023] Furthermore, the material of the shell is iron alloy;
[0024] The proportion of iron in the ferroalloy is greater than 95wt%;
[0025] The shell wall thickness has a numerical range of 2.5 mm to 50 mm, and a length / diameter ratio of 1 to 5;
[0026] Preferably, the shell wall thickness has a value ranging from 5 mm to 30 mm, and a length / diameter ratio of 1 to 3.
[0027] Furthermore, the ratio of the sum of the volumes of the plurality of master alloys to the volume of the inner cavity of the housing is greater than or equal to a preset value;
[0028] Preferably, the preset value is 70%.
[0029] Further, the gas includes: at least one of argon, nitrogen, helium, neon, krypton, radon, xenon, carbon dioxide, and carbon monoxide;
[0030] Preferably, the gas includes: argon;
[0031] Furthermore, the oxygen in the gas is ≤10ppm.
[0032] Further, the preset pressure value of the gas is 0.04MPa-0.3MPa;
[0033] Preferably, the preset pressure value of the gas is 0.08MPa-0.12MPa.
[0034] Accordingly, a second aspect of an embodiment of the present invention includes a method for preparing a rare earth-containing additive, which is used to prepare the rare earth-containing additive, comprising the following steps:
[0035] Adding iron to a vacuum induction melting furnace and filling it with inert gas to a first preset pressure value;
[0036] After the temperature reaches a first preset temperature, rare earth metal is added to the iron solution, and the temperature is heated until the alloy is completely melted;
[0037] The alloy solution is poured into a mold and cooled in a furnace under the protection of an inert gas to obtain a rare earth alloy;
[0038] After the rare earth alloy is loaded into the shell, a gas with a second preset pressure value is charged into the shell, and the shell is sealed to obtain the rare earth-containing additive.
[0039] Further, the numerical range of the first preset pressure value is 10000Pa-90000Pa;
[0040] The numerical range of the second preset pressure value is 0.04-0.3MPa; preferably, the preset pressure value is 0.08-0.12MPa;
[0041] The numerical range of the first preset temperature value is 1550°C-1800°C.
[0042] The above technical solution of the embodiment of the present invention has the following beneficial technical effects:
[0043] 1. The gas in the additive generates thrust by thermal expansion, so that the rare earth metals can be evenly dispersed in the steel, which can effectively solve the problems of unstable control, uneven distribution and low yield of rare earth components in rare earth steel;
[0044] 2. By adopting a streamlined shell with a special shape, compared with ordinary rare earth additives on the market, it has a smaller resistance coefficient, can achieve a deeper penetration depth in the molten steel, penetrate into the middle and lower part of the ladle, and achieve the purpose of evenly mixing the rare earth and molten steel. BRIEF DESCRIPTION OF THE DRAWINGS
[0045] Figure 1 It is a schematic diagram of the structure of a rare earth-containing additive provided in an embodiment of the present invention.
[0046] 1. Front shell, 2. Rear shell, 3. Shell, 4. Intermediate alloy, 5. Gas. DETAILED DESCRIPTION
[0047] In order to make the purpose, technical scheme and advantages of the present invention clearer, the present invention is further described in detail below in conjunction with specific embodiments and with reference to the accompanying drawings. It should be understood that these descriptions are only exemplary and are not intended to limit the scope of the present invention. In addition, in the following description, the description of well-known structures and technologies is omitted to avoid unnecessary confusion of the concept of the present invention.
[0048] Please refer to Figure 1 The embodiment of the present invention provides a rare earth-containing additive, including: a sealed shell 3 and a plurality of intermediate alloys 4 arranged inside the shell 3; wherein the intermediate alloy 4 contains rare earth elements; and the shell 3 is filled with a gas 5 of a preset pressure.
[0049] By making the rare earth-containing additive contain gas-solid two phases, it expands due to heat after being added to the molten steel, forming a positive pressure inside. As the shell of the additive continues to melt and the shell wall becomes thinner, the internal gas pressure breaks through the shell, generating a driving force, pushing the internal solid phase rare earth additive to the surroundings, further fully mixing the rare earth additive evenly, and significantly improving the rare earth recovery rate.
[0050] Optionally, the wall thickness of the shell 3 containing the rare earth additive is selected in the range of 2.5-50mm, preferably 5-30mm, the length / diameter (width) is 1-5, the longest side is 400mm, preferably the length / diameter (width) is 1-3, and the longest side is 300mm. If the size of the rare earth additive is too small, the overall addition time will be too long, and if the size of the rare earth additive is too large, the melting time will be prolonged and the danger will increase. Therefore, the size range is preferably determined based on a comprehensive assessment of the addition time, melting time and production safety of the rare earth additive.
[0051] Optionally, the shell 3 has a shape of a cuboid, a sphere, a cylinder, a truncated cone, a cone, or a streamline.
[0052] Preferably, the housing 3 comprises: a front housing 1 and a rear housing 2; the front housing 1 and the rear housing 2 are connected at their edges, and a plurality of intermediate alloys 4 and gas 5 are located in a closed space between the front housing 1 and the rear housing 2; the shapes of the front housing and the rear housing are different. Preferably, the weight of the front housing is greater than that of the rear housing.
[0053] Furthermore, the front shell 1 is a semi-ellipsoid, and the rear shell 2 is a cylinder, a cone or a semi-ellipsoid.
[0054] The front shell 1 adopts a streamlined semi-ellipsoidal structure. The streamlined shell reduces the resistance coefficient of the rare earth additive, thereby reducing the viscous resistance of the rare earth additive in the steel. Compared with ordinary blocks, it can achieve a deeper penetration depth of the molten steel and increase the uniformity of the rare earth mixing.
[0055] Specifically, the cross-sectional profile of the front housing 1 satisfies:
[0056]
[0057] Among them, x is the axial X-axis coordinate value of the front shell 1, y is the Y-axis coordinate value perpendicular to the streamlined axial direction of the front shell 1, the origin of the XY axis coordinates is at the center point of the interface between the front shell and the rear shell, R is the short axis radius value of the ellipse where the central axis section of the front shell is located, and L is the long axis radius value of the ellipse where the central axis section of the front shell is located; the maximum diameter of the rear shell 2 along the Y-axis direction is B≤2R.
[0058] When R / L=1, it is a sphere; when R / L≠1, it is an ellipsoid, and the first part is ≤ a semi-ellipsoid; the preferred L / R range is 1-5. The front shell shape in this range is sharper, penetrates deeper into the molten steel, and has a better addition effect.
[0059] Preferably, the length of the front shell accounts for more than 50% of the entire length of the rare earth additive, so as to achieve a "top-heavy" effect and ensure that the first shell is plunged downward into the molten steel.
[0060] Furthermore, the intermediate alloy 4 includes rare earth metal and iron; the rare earth metal content is 8wt% to 90wt%, and the iron content is 10wt% to 92wt%; wherein the oxygen content is less than 150ppm, the maximum size of inclusions is less than 30μm, and the total amount of inclusions is less than 0.5wt%.
[0061] Furthermore, the rare earth metal includes at least one of lanthanum, cerium, praseodymium, neodymium, samarium, europium, gadolinium, terbium, dysprosium, holmium, erbium, thulium, ytterbium, lutetium, scandium and yttrium; preferably, the rare earth metal includes at least one of lanthanum, cerium and yttrium. Among the rare earth species, lanthanum, cerium and yttrium are highly abundant, inexpensive and have good addition effects.
[0062] In addition, in another embodiment of the present invention, the intermediate alloy 4 further includes: a transition metal; the transition metal includes: at least one of nickel, chromium, tungsten, molybdenum, cobalt, manganese, vanadium, niobium, and titanium. Preferably, the transition metal includes: at least one of chromium, tungsten, molybdenum, vanadium, niobium, and titanium. The transition metal is derived from the common trace elements in steel and will not introduce new impurities; secondly, the transition metal plays a role in microalloying the rare earth additive and preventing the rare earth additive from oxidizing.
[0063] Specifically, the rare earth metal content in the master alloy 4 is 15wt% to 70wt%, the transition metal content is 0.1wt% to 15wt%, and the iron content is 20wt% to 70wt%. At this time, the oxygen content is less than 100ppm, the carbon content is less than 300ppm, the maximum size of inclusions is less than 25μm, and the total amount of inclusions is less than 0.1wt%. The controllable size and quantity of inclusions have a significant impact on the final addition effect. Within this range, the rare earth additive has a better addition effect.
[0064] Furthermore, the material of the shell is an iron alloy; the proportion of iron in the iron alloy is greater than 95wt%.
[0065] Furthermore, the ratio of the volume of the plurality of master alloys 4 to the volume of the inner cavity of the shell is greater than or equal to a preset value; preferably, the preset value is 70%. The volume of the rare earth alloy filled inside accounts for ≥70% of the volume of the entire inner cavity, based on the fact that the amount of additive added at one time is larger and the addition efficiency is higher, and the larger the volume of the rare earth alloy filled inside, the greater the overall density of the additive, and the deeper the rare earth and the molten steel are, the purpose of mixing the rare earth and the molten steel evenly is achieved.
[0066] Specifically, gas 5 includes at least one of argon, nitrogen, helium, neon, krypton, radon, xenon, carbon dioxide, and carbon monoxide. Preferably, gas 5 includes argon. Argon is preferred because it is an inert gas and does not react with rare earth metals when used as a filling gas. It is cheaper than inert gases such as helium, neon, krypton, radon, and xenon, and is more suitable for industrial production. Nitrogen easily reacts with rare earth metals, and carbon dioxide and carbon monoxide easily increase the carbon content of molten steel, and carbon monoxide easily causes human poisoning, which is not within the preferred range. The oxygen content is ≤10ppm to minimize the introduction of oxygen.
[0067] Optionally, the preset pressure value of the gas 5 is 0.04MPa-0.3MPa; preferably, the preset pressure value of the gas 5 is 0.08MPa-0.12MPa. The pressure of the gas 5 is determined by comprehensively considering the pressure of the molten steel, the explosion feasibility and the production safety.
[0068] Accordingly, a second aspect of an embodiment of the present invention provides a method for preparing a rare earth-containing additive, which is used to prepare the rare earth-containing additive, comprising the following steps:
[0069] Step S100, adding iron into a vacuum induction melting furnace, and filling it with inert gas to a first preset pressure value.
[0070] Step S200, adding rare earth metal to the iron solution after the temperature is raised to a first preset temperature value, and heating until the alloy is completely melted.
[0071] Step S300, pouring the alloy solution into a mold, and cooling it in a furnace under the protection of an inert gas to obtain a rare earth alloy.
[0072] Step S400, after the rare earth alloy is loaded into the shell, a gas with a second preset pressure value is filled into the shell, and the shell is sealed to obtain the rare earth-containing additive.
[0073] Furthermore, the numerical range of the first preset pressure value is 10000Pa-90000Pa; the numerical range of the second preset pressure value is 0.04-0.3MPa; preferably, the preset pressure value is 0.08-0.12MPa; the numerical range of the first preset temperature value is 1550℃-1800℃.
[0074] The rare earth-containing additives are further described below with reference to several embodiments:
[0075] Example 1
[0076] Pure iron and rare earth cerium obtained by thermal reduction are prepared according to the mass percentages of 92% and 8% respectively. Put the pure iron raw material into the crucible of the vacuum induction melting furnace, and put the rare earth cerium into the trough of the vacuum induction melting furnace; evacuate to below 0.2Pa, and fill with high-purity argon gas to make the vacuum degree in the furnace reach 10000Pa. Fill with high-purity argon gas, when the vacuum degree in the furnace is maintained at 10000Pa, raise the temperature to 1700℃, and after the metal in the crucible is melted, add rare earth cerium to the metal iron liquid through the trough, and refine for 10 minutes after melting. Pour the alloy solution into the mold and cool it with the furnace under the protection of the argon atmosphere in the furnace. After analysis, the average size of inclusions in the rare earth alloy is 20μm, the oxygen content is 66ppm, and the carbon content is 200ppm. The rare earth alloy is loaded into a streamlined (L / R=1) pure iron shell with a rare earth alloy filling ratio of 85%, a shell wall thickness of 2.5mm, a maximum (diameter) length of 100mm, and an aspect ratio of 2:1. The air in the shell is emptied and filled with 0.04MPa Ar, which is then added to the ladle. The rare earth recovery rate in the tested product is 60.1%, the standard deviation of the rare earth composition at the edge, 1 / 4 radius, 1 / 2 radius, and middle of the slab is 4.5ppm, and the average size of inclusions in the steel is 15.1μm.
[0077] Comparative Example 1
[0078] Pure iron and rare earth cerium obtained by thermal reduction are prepared according to the mass percentages of 92% and 8% respectively. Put the pure iron raw material into the crucible of the vacuum induction melting furnace, and put the rare earth cerium into the trough of the vacuum induction melting furnace; evacuate to below 0.2Pa, and fill with high-purity argon gas to make the vacuum degree in the furnace reach 10000Pa. Fill with high-purity argon gas, when the vacuum degree in the furnace is maintained at 10000Pa, raise the temperature to 1700℃, and after the metal in the crucible is melted, add rare earth cerium to the metal iron liquid through the trough, and refine for 10 minutes after melting. Pour the alloy solution into the mold and cool it with the furnace under the protection of the argon atmosphere in the furnace. After analysis, the average size of inclusions in the rare earth alloy is 50μm, the oxygen content is 200ppm, and the carbon content is 200ppm. The rare earth alloy is loaded into a streamlined (L / R=1) pure iron shell with a rare earth alloy filling ratio of 85%, a shell wall thickness of 2.5mm, a maximum (diameter) length of 100mm, and an aspect ratio of 2:1. The air in the shell is emptied and filled with 0.04MPa Ar, which is then added to the ladle. The rare earth recovery rate in the tested product is 49.5%, and the standard deviation of the rare earth composition at the edge, 1 / 4 radius, 1 / 2 radius, and middle of the slab is 6ppm. The average size of inclusions in the steel is 30.2μm.
[0079] Example 2
[0080] Pure iron and rare earth lanthanum obtained by molten salt electrolysis are prepared according to the mass percentages of 10% and 90% respectively. Put the pure iron raw material into the crucible of the vacuum induction melting furnace, and put the rare earth lanthanum into the material trough of the vacuum induction melting furnace; evacuate to below 0.2Pa, and fill with high-purity argon gas to make the vacuum degree in the furnace reach 20000Pa. Fill with high-purity argon gas, when the vacuum degree in the furnace is maintained at 20000Pa, raise the temperature to 1550℃, and after the metal in the crucible is melted, add rare earth lanthanum to the metal iron liquid through the material trough, and refine for 10 minutes after melting. Pour the alloy solution into the mold and cool it with the furnace under the protection of the argon atmosphere in the furnace. After analysis, the average size of inclusions in the rare earth alloy is 12.4μm, the oxygen content is 55ppm, and the carbon content is 150ppm. The rare earth alloy is loaded into a streamlined (L / R=2) pure iron shell with a rare earth alloy filling ratio of 75%, a shell wall thickness of 50mm, a maximum (diameter) length of 180mm, and an aspect ratio of 2.5:1. The air in the shell is emptied and filled with 0.3MPa Ar, which is then added to the ladle. The rare earth recovery rate in the tested product is 55%, the standard deviation of the rare earth composition at the edge, 1 / 4 radius, 1 / 2 radius, and middle of the slab is 4.2ppm, and the average size of inclusions in the steel is 12.4μm.
[0081] Comparative Example 2
[0082] An irregular block of lanthanum-iron alloy with the same composition as that of Comparative Example 2 was prepared, with a maximum (diameter) length of 180 mm, an aspect ratio of 2.5:1, an average size of inclusions in the rare earth alloy of 12.4 μm, an oxygen content of 55 ppm, and a carbon content of 150 ppm. It was added to a ladle, and the rare earth yield in the tested product was 35.1%, the standard deviation of the rare earth composition at the edge, 1 / 4 radius, 1 / 2 radius, and middle of the slab was 15 ppm, and the average size of inclusions in the steel was 14.6 μm.
[0083] Example 3
[0084] Prepare pure iron and rare earth metal yttrium using molten salt electrolysis according to the mass percentage of 60% and 40% respectively. Put the pure iron raw material into the crucible of the vacuum induction melting furnace, and put the rare earth metal yttrium into the trough of the vacuum induction melting furnace; evacuate to below 0.2Pa, and fill with high-purity argon gas to make the vacuum degree in the furnace reach 30000Pa. Fill with high-purity argon gas, when the vacuum degree in the furnace is maintained at 30000Pa, raise the temperature to 1600℃, and after the metal in the crucible is melted, add rare earth metal yttrium to the metal iron liquid through the trough, and refine for 10 minutes after melting. Pour the alloy solution into the mold and cool it with the furnace under the protection of the argon atmosphere in the furnace. After analysis, the average size of inclusions in the rare earth alloy is 25μm, the oxygen content is 56ppm, and the carbon content is 180ppm. The rare earth alloy is loaded into a streamlined (L / R=3) pure iron shell with a rare earth alloy filling ratio of 80%, a shell wall thickness of 10mm, a maximum (diameter) length of 200mm, and an aspect ratio of 3.5:1. The air in the shell is emptied and filled with 0.1MPa Ar, which is then added to the ladle. The rare earth recovery rate in the tested product is 62.2%, the standard deviation of the rare earth composition at the edge, 1 / 4 radius, 1 / 2 radius, and middle of the slab is 2.3ppm, and the average size of inclusions in the steel is 10.7μm.
[0085] Comparative Example 3
[0086] Prepare pure iron and rare earth metal yttrium using molten salt electrolysis according to the mass percentage of 60% and 40% respectively. Put the pure iron raw material into the crucible of the vacuum induction melting furnace, and put the rare earth metal yttrium into the trough of the vacuum induction melting furnace; evacuate to below 0.2Pa, and fill with high-purity argon gas to make the vacuum degree in the furnace reach 30000Pa. Fill with high-purity argon gas, when the vacuum degree in the furnace is maintained at 30000Pa, raise the temperature to 1600℃, and after the metal in the crucible is melted, add rare earth metal yttrium to the metal iron liquid through the trough, and refine for 10 minutes after melting. Pour the alloy solution into the mold and cool it with the furnace under the protection of the argon atmosphere in the furnace. After analysis, the average size of inclusions in the rare earth alloy is 25μm, the oxygen content is 56ppm, and the carbon content is 180ppm. The rare earth alloy is loaded into a streamlined (L / R=3) pure iron shell with a shell wall thickness of 10mm, a maximum (diameter) length of 200mm, an aspect ratio of 3.5:1, and no gas is filled. The rare earth recovery rate in the tested product is 46.4%, and the standard deviation of the rare earth composition at the edge, 1 / 4 radius, 1 / 2 radius, and middle of the slab is 14.4ppm. The average size of inclusions in the steel is 23.2μm.
[0087] All embodiments and comparative examples of the present invention are listed in Table 1 and Table 2. The effect of adding gas-containing rare earth additives to steel is significantly better than that of ordinary solid rare earth additives, which is specifically reflected in higher rare earth recovery rate and better uniformity; the average size and oxygen content of inclusions in the rare earth additives have a significant impact on the size of inclusions in the final steel, and the rare earth additives with small average inclusion size and low oxygen content have smaller inclusion sizes in the final steel. The rare earth-containing additive provided by the present invention has a simple preparation method, excellent addition effect, and has the prospect of large-scale industrial production.
[0088] Table 1
[0089]
[0090]
[0091] Table 2
[0092]
[0093] The embodiment of the present invention aims to protect a rare earth-containing additive, comprising: a sealed shell and a plurality of master alloys disposed inside the shell; wherein the master alloy contains rare earth elements, and the shell is filled with gas at a preset pressure. The above technical solution has the following effects:
[0094] 1. The gas in the additive generates thrust by thermal expansion, so that the rare earth metals can be evenly dispersed in the steel, which can effectively solve the problems of unstable control, uneven distribution and low yield of rare earth components in rare earth steel;
[0095] 2. By adopting a streamlined shell with a special shape, compared with ordinary rare earth additives on the market, it has a smaller resistance coefficient, can achieve a deeper penetration depth in the molten steel, penetrate into the middle and lower part of the ladle, and achieve the purpose of evenly mixing the rare earth and molten steel.
[0096] It should be understood that the above specific embodiments of the present invention are only used to illustrate or explain the principles of the present invention, and do not constitute a limitation of the present invention. Therefore, any modifications, equivalent substitutions, improvements, etc. made without departing from the spirit and scope of the present invention should be included in the protection scope of the present invention. In addition, the appended claims of the present invention are intended to cover all changes and modifications that fall within the scope and boundaries of the appended claims, or the equivalent forms of such scope and boundaries.
Claims
1. An additive containing rare earth, It is characterized in that include: A sealed shell and a plurality of master alloys disposed inside the shell; wherein the master alloy contains rare earth elements; The shell is filled with gas at a preset pressure, and the preset pressure value of the gas is 0.04-0.3 MPa.
2. The rare earth-containing additive according to claim 1, It is characterized in that The shell has a shape of a cuboid, a sphere, a cylinder, a truncated cone, a cone, or a streamline.
3. The rare earth-containing additive according to claim 2, It is characterized in that The housing comprises: a front housing and a rear housing; The front shell is integrally connected with the rear shell, and the plurality of master alloys and the gas are located in a closed space between the front shell and the rear shell.
4. The rare earth-containing additive according to claim 3, It is characterized in that The counterweight of the front housing is greater than the counterweight of the rear housing.
5. The rare earth-containing additive according to claim 3, It is characterized in that The streamlined front shell profile satisfies the following mathematical expression obtained by rotating one circle around the x-axis: Wherein, x is the coordinate value of the front shell in the X-axis direction, y is the coordinate value of the Y-axis direction perpendicular to the axial direction of the front shell, the origin of the XY-axis coordinates is at the center point of the interface between the front shell and the rear shell, R is the minor axis radius value of the ellipse where the central axis section of the front shell is located, and L is the major axis radius value of the ellipse where the central axis section of the front shell is located; The length of the front shell along the length direction of the shell is greater than the length of the rear shell along the length direction of the shell, and the maximum diameter B of the rear shell along the Y-axis direction is less than or equal to 2R.
6. The rare earth-containing additive according to claim 1, It is characterized in that The master alloy comprises: rare earth metal and iron; The rare earth metal content is 8wt%~90wt%, and the iron content is 10wt%~92wt%; Among them, the oxygen content is <150 ppm, the maximum size of inclusions is <30 μm, and the total amount of inclusions is <0.5 wt %.
7. The rare earth-containing additive according to claim 6, It is characterized in that The intermediate alloy composition is RE-Fe-M, where M is a transition metal, and the transition metal includes at least one of nickel, chromium, tungsten, molybdenum, cobalt, manganese, vanadium, niobium, and titanium; In the master alloy, the rare earth metal content is 15wt%~70wt%, the transition metal content is 0.1wt%~15wt%, and the iron content is 20wt%~70wt%; The oxygen content of the rare earth-containing additive is less than 100 ppm, the carbon content is less than 300 ppm, the maximum size of inclusions is less than 25 μm, and the total amount of inclusions is less than 0.1 wt %.
8. The rare earth-containing additive according to claim 7, It is characterized in that The transition metal includes at least one of chromium, tungsten, molybdenum, vanadium, niobium and titanium.
9. The rare earth-containing additive according to claim 6, It is characterized in that The rare earth metal includes at least one of lanthanum, cerium, praseodymium, neodymium, samarium, europium, gadolinium, terbium, dysprosium, holmium, erbium, thulium, ytterbium, lutetium, scandium and yttrium.
10. The rare earth-containing additive according to claim 9, It is characterized in that The rare earth metal includes at least one of lanthanum, cerium and yttrium.
11. The rare earth-containing additive according to any one of claims 1 to 8, It is characterized in that The material of the shell is iron alloy; The proportion of iron in the ferroalloy is greater than 95wt%; The shell wall thickness has a numerical range of 2.5 mm to 50 mm, and a length / diameter ratio of 1 to 5.
12. The rare earth-containing additive according to claim 11, It is characterized in that The shell wall thickness has a numerical range of 5 mm to 30 mm, and a length / diameter ratio of 1 to 3.
13. The rare earth-containing additive according to any one of claims 1 to 8, It is characterized in that The ratio of the sum of the volumes of the plurality of master alloys to the volume of the inner cavity of the housing is greater than or equal to a preset value; The preset value is 70%.
14. The rare earth-containing additive according to any one of claims 1 to 9, It is characterized in that The gas includes at least one of argon, nitrogen, helium, neon, krypton, radon, xenon, carbon dioxide and carbon monoxide.
15. The rare earth-containing additive according to claim 14, It is characterized in that The gas includes: argon.
16. The rare earth-containing additive according to claim 14, It is characterized in that Oxygen in the gas ≤10 ppm.
17. The rare earth-containing additive according to claim 14, It is characterized in that The preset pressure value of the gas is 0.08-0.12 MPa.
18. A method for preparing a rare earth-containing additive, It is characterized in that The method for preparing the rare earth-containing additive according to any one of claims 1 to 17 comprises the following steps: Adding iron to a vacuum induction melting furnace and filling it with inert gas to a first preset pressure value; After the temperature reaches a first preset temperature, rare earth metal is added to the iron solution, and the temperature is heated until the alloy is completely melted; The alloy solution is poured into a mold and cooled in a furnace under the protection of an inert gas to obtain a rare earth alloy; After the rare earth alloy is loaded into the shell, a gas with a second preset pressure value is charged into the shell, and the shell is sealed to obtain the rare earth-containing additive.
19. The method for preparing a rare earth-containing additive according to claim 18, It is characterized in that The numerical range of the first preset pressure value is 10000Pa-90000Pa; The numerical range of the second preset pressure value is 0.04-0.3 MPa; The numerical range of the first preset temperature value is 1550°C-1800°C.
20. The method for preparing a rare earth-containing additive according to claim 19, It is characterized in that The second preset pressure value is 0.08-0.12 MPa.
Citation Information
Cited By
Preparation method of green and efficient rare earth additive
CN121518738A