Semiconductor devices and their manufacturing methods

By forming a capping layer in the MRAM cell and removing its patterning process, electrical interference is improved by using a low dielectric constant dielectric material, thus solving the electrical problems caused by the increase in MRAM cell density and improving device performance and process yield.

CN116669524BActive Publication Date: 2026-11-17UNITED MICROELECTRONICS CORP
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202310561422.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2018-11-05
Publication Date
2026-11-17
Estimated Expiration
2038-11-05

AI Technical Summary

Technical Problem

As MRAM cell density increases, electrical issues between adjacent cells, such as RC delay effect and crosstalk, become more severe, and existing structural designs and manufacturing processes are difficult to improve effectively.

Method used

A capping layer is formed on the first intermetallic dielectric layer, and the capping layer is removed in the patterning fabrication process of the magnetic tunneling junction structure, so that the second intermetallic dielectric layer surrounds the magnetic tunneling junction structure, and the electrical interference is improved by using a dielectric material with a low dielectric constant.

Benefits of technology

By using materials with low dielectric constants, electrical interference between magnetic tunnel junction structures and with other conductive structures is reduced, thereby improving the operational performance and manufacturing yield of semiconductor devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116669524B_ABST
    Figure CN116669524B_ABST
Patent Text Reader

Abstract

This invention discloses a semiconductor device and its fabrication method. The fabrication method includes the following steps: forming a first intermetallic dielectric layer on a substrate; forming a capping layer on the first intermetallic dielectric layer; forming an interconnect structure on the substrate penetrating the capping layer and the first intermetallic dielectric layer; forming a magnetic tunneling junction stack on the interconnect structure and the capping layer; performing a patterning fabrication process on the magnetic tunneling junction stack to form a magnetic tunneling junction structure on the interconnect structure and removing the capping layer; forming a second intermetallic dielectric layer on the first intermetallic dielectric layer; and the second intermetallic dielectric layer surrounding the magnetic tunneling junction structure. A semiconductor device includes a substrate, an interconnect structure, a first intermetallic dielectric layer, a magnetic tunneling junction structure, and a second intermetallic dielectric layer. The dielectric constant of the first intermetallic dielectric layer is lower than the dielectric constant of the second intermetallic dielectric layer.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] This application is a divisional application of Chinese invention patent application (application number: 201811306131.7, application date: November 5, 2018, invention title: semiconductor device and method of manufacturing thereof). Technical Field

[0002] This invention relates to a semiconductor device and a method for manufacturing the same, and more particularly to a semiconductor device having a magnetic tunnel junction (MTJ) structure and a method for manufacturing the same. Background Technology

[0003] Data storage devices used in electronic products are basically of two types: non-volatile and volatile. Magnetic random access memory (MRAM) is a type of non-volatile memory technology. Unlike current standard memory devices, MRAM uses magnetism to store data instead of using electric charge. Typically, an MRAM cell consists of a data layer and a reference layer. The data layer is made of a magnetic material, and its magnetization can be switched between two opposing states by an applied magnetic field, thereby storing binary information. The reference layer can be made of a magnetic material, and its magnetization can be locked so that the magnetic field applied to the data layer and partially penetrating the reference layer is insufficient to switch the magnetization in the reference layer. During a read operation, the resistance of the MRAM cell differs when the magnetization directions of the data layer and the reference layer are the same or different, thus allowing the identification of the magnetic polarity of the data layer.

[0004] The distance between adjacent MRAM cells decreases as the storage cell density increases. However, if the MRAM cells are too close together, electrical problems such as resistive-capacitive delay (RC delay) and crosstalk will become more serious. Therefore, improvements need to be made in terms of structural design and / or manufacturing process. Summary of the Invention

[0005] The present invention provides a semiconductor device and a method thereof, which utilizes the formation of a capping layer on a first intermetallic dielectric layer and the removal of the capping layer in a patterning process for forming a magnetic tunneling junction structure, so that a second intermetallic dielectric layer surrounding the magnetic tunneling junction structure can be formed on the first intermetallic dielectric layer, thereby improving the electrical interference between the magnetic tunneling junction structure and other conductive structures.

[0006] An embodiment of the present invention provides a method for fabricating a semiconductor device, comprising the following steps: First, a first intermetallic dielectric layer is formed on a substrate. A capping layer is formed on the first intermetallic dielectric layer. An interconnect structure is formed on the substrate, the interconnect structure penetrating the capping layer and the first intermetallic dielectric layer. A magnetic tunneling junction stack is formed on the interconnect structure and the capping layer. A patterning process is performed on the magnetic tunneling junction stack to form a magnetic tunneling junction structure on the interconnect structure, and the capping layer is removed by the patterning process. A second intermetallic dielectric layer is formed on the first intermetallic dielectric layer, and the second intermetallic dielectric layer surrounds the magnetic tunneling junction structure.

[0007] An embodiment of the present invention provides a semiconductor device including a substrate, a connection structure, a first intermetallic dielectric layer, a magnetic tunneling junction structure, and a second intermetallic dielectric layer. The connection structure is disposed on the substrate. The first intermetallic dielectric layer is disposed on the substrate and surrounds the connection structure. The magnetic tunneling junction structure is disposed on the connection structure. The second intermetallic dielectric layer is disposed on the first intermetallic dielectric layer and surrounds the magnetic tunneling junction structure. The dielectric constant of the first intermetallic dielectric layer is lower than the dielectric constant of the second intermetallic dielectric layer. Attached Figure Description

[0008] Figures 1 to 5 This is a schematic diagram of a method for manufacturing a semiconductor device according to an embodiment of the present invention, wherein...

[0009] Figure 2 for Figure 1 A diagram illustrating the subsequent situation;

[0010] Figure 3 for Figure 2 A diagram illustrating the subsequent situation;

[0011] Figure 4 for Figure 3 A diagram illustrating the subsequent situation;

[0012] Figure 5 for Figure 4 A diagram illustrating the subsequent situation.

[0013] Explanation of main component symbols

[0014] 10 base

[0015] 11 First dielectric layer

[0016] 21 Second dielectric layer

[0017] 22 Interconnection Structure

[0018] 23 Stop Layer

[0019] 31 First intermetallic dielectric layer

[0020] 31T First Upper Surface

[0021] 32 cap layer

[0022] 40 Connection Structure

[0023] 40T Second Upper Surface

[0024] 41 Barrier Layer

[0025] 42 Metal Layer

[0026] 50 magnetic tunneling junction stack

[0027] 50S magnetic tunnel junction structure

[0028] 51 First conductive layer

[0029] 52 Locked Layer

[0030] 53 First Barrier Layer

[0031] 54 Free Layer

[0032] 55 Second Barrier Layer

[0033] 56 Second conductive layer

[0034] 61 First mask layer

[0035] 62 Second mask layer

[0036] 63 Organic dielectric layer

[0037] 64 Anti-reflective layer

[0038] 65 Patterned photoresist layer

[0039] 66. Spacer wall material layer

[0040] 66S spacer wall

[0041] 70 Second intermetallic dielectric layer

[0042] 80 Contact plug

[0043] 90 Patterned Production Process

[0044] 100 Semiconductor Devices

[0045] D1 First Direction

[0046] D2 Second Direction

[0047] T1 First Thickness

[0048] T2 Second Thickness Detailed Implementation

[0049] Please see Figures 1 to 5 . Figures 1 to 5 The illustration is a schematic diagram of a method for manufacturing a semiconductor device according to an embodiment of the present invention, wherein... Figure 2 It is illustrated Figure 1 A diagram illustrating the subsequent situation. Figure 3 It is illustrated Figure 2 A diagram illustrating the subsequent situation. Figure 4 It is illustrated Figure 3 The following is a diagram illustrating the situation, and Figure 5 It is illustrated Figure 4 A schematic diagram of the subsequent situation. The method for manufacturing the semiconductor device in this embodiment may include the following steps. First, as... Figure 1 As shown, a first inter-metal dielectric (IMD) layer 31 is formed on a substrate 10, and a capping layer 32 is formed on the first IMD layer 31. Then, a connection structure 40 is formed on the substrate 10, and the connection structure 40 is oriented in the thickness direction of the substrate 10 (e.g., ...). Figure 1 The first direction D1) shown in the figure penetrates the capping layer 32 and the first intermetallic dielectric layer 31. In some embodiments, a magnetic tunnel junction (MTJ) region and a logic region may be defined on the substrate 10. The first intermetallic dielectric layer 31 and the capping layer 32 may be formed on the MTJ region and the logic region simultaneously, and the connection structure 40 may be formed on the MTJ region, but is not limited thereto.

[0050] In some embodiments, the first intermetallic dielectric layer 31 may include a low dielectric constant (low-k) dielectric material and / or an ultra-low dielectric constant (ULK) dielectric material, such as benzocyclclobutene (BCB), HSQ (hydrogen silsesquioxane), MSQ (methyl silesquioxane), silicon oxyhydrocarbon (SiOC-H), or / or a porous dielectric material. The dielectric constant of the first intermetallic dielectric layer 31 may be lower than 2.9 (e.g., a general requirement for low-k dielectric materials), and preferably lower than 2.7 (e.g., a general requirement for ULK dielectric materials), but is not limited thereto. Furthermore, generally, low-dielectric-constant dielectric materials have relatively low hardness (e.g., when using porous structures to reduce the dielectric constant). Therefore, to avoid affecting the fabrication yield when forming the connection structure 40, it is preferable to use a material with a relatively high dielectric constant but also high hardness to form the capping layer 32, thereby avoiding the inability to successfully form the desired shape of the connection structure 40. In some embodiments, the capping layer 32 may include silicon oxide, tetraethoxysilane (TEOS) oxide, or other suitable dielectric materials, but is not limited thereto. Therefore, the capping layer 32 may be a dielectric capping layer, and the hardness of the capping layer 32 may be higher than the hardness of the first intermetallic dielectric layer 31, and the dielectric constant of the first intermetallic dielectric layer 31 may be lower than the dielectric constant of the capping layer 32. However, in some embodiments, the capping layer 32 may also include other dielectric or conductive materials that have a high etch selectivity with the material of the connection structure 40, as needed.

[0051] In some embodiments, substrate 10 may include a semiconductor substrate or a non-semiconductor substrate. The semiconductor substrate may include, for example, a silicon substrate, a silicon-germanium semiconductor substrate, or a silicon-on-insulator (SOI) substrate, while the non-semiconductor substrate may include a glass substrate, a plastic substrate, or a ceramic substrate, but is not limited thereto. For example, when substrate 10 includes a semiconductor substrate, multiple silicon-based field-effect transistors (not shown) may be formed on the semiconductor substrate as needed, along with a dielectric layer covering the silicon-based field-effect transistors (e.g., [insert dielectric layer here]). Figure 1The diagram shows a first dielectric layer 11 and a second dielectric layer 21, an interconnect structure 22, and then a first intermetallic dielectric layer 31. The first dielectric layer 11 and the second dielectric layer 21 may include silicon oxide, a low-dielectric-constant dielectric material, or other suitable dielectric materials. In some embodiments, the connection structure 40 may be electrically connected to a portion of the interconnect structure 22 and may be electrically connected downwards to the aforementioned silicon-based field-effect transistor via a portion of the interconnect structure 22, but this is not a limitation. In some embodiments, the interconnect structure 22 may include a trench conductor, and the connection structure 40 may include a via conductor. Furthermore, the interconnect structure 22 and the connection structure 40 may be formed of a barrier layer and a metal layer; for example, the connection structure 40 may include a barrier layer 41 and a metal layer 42, but this is not a limitation. The barrier layer 41 may include titanium (Ti), titanium nitride (TiN), tantalum (Ta), tantalum nitride (TaN) or other suitable barrier materials, while the metal layer 42 may include tungsten (W), copper (Cu), aluminum (Al), titanium-aluminum alloy (TiAl), cobalt tungsten phosphide (CoWP) or other suitable metal materials.

[0052] In some embodiments, a stop layer 23 may be formed on the substrate 10 before forming the first intermetallic dielectric layer 31. The stop layer 23 may cover the second dielectric layer 21 and the interconnect structure 22. The first intermetallic dielectric layer 31 may be formed on the stop layer 23, and the connection structure 40 may penetrate the stop layer 23 to contact the interconnect structure 22 and form an electrical connection. The stop layer 23 may include a nitrogen-doped carbide (NDC), silicon nitride, silicon carbon nitride (SiCN), or other suitable insulating materials. In some embodiments, the stop layer 23 may be an insulating material with relatively high hardness, and the dielectric constant of the first intermetallic dielectric layer 31 may be lower than that of the stop layer 23, but is not limited thereto. Furthermore, it is worth noting that since the capping layer 32 will be removed in subsequent fabrication processes, the thickness of the capping layer 32 (e.g., Figure 1 The second thickness T2 shown should not be too thick to avoid residual capping layer 32 affecting the equivalent dielectric constant of the overall dielectric material. However, when forming the connection structure 40, the capping layer 32 must have a certain thickness to achieve the required support effect. Therefore, in some embodiments, the thickness of the first intermetallic dielectric layer 31 (e.g., Figure 1 The first thickness T1 shown may be greater than or equal to the second thickness T2 of the capping layer 32, but is not limited thereto.

[0053] Then, as Figure 2 and Figure 3As shown, a magnetic tunneling junction (MTJ) stack 50 can be formed on the connecting structure 40 and the capping layer 32, and a patterning fabrication process 90 is performed on the magnetic tunneling junction stack 50 to form a magnetic tunneling junction (MTJ) structure 50S on the connecting structure 40. In some embodiments, the magnetic tunneling junction stack 50 may include a first conductive layer 51, a pinned layer 52, a first barrier layer 53, a free layer 54, a second barrier layer 55, and a second conductive layer 56 sequentially stacked in the first direction D1, but is not limited thereto. In some embodiments, the magnetic tunneling junction stack 50 may also include a stacked structure of materials different from the above-described material layers and / or other material layers as needed. In some embodiments, the first conductive layer 51 and the second conductive layer 56 may include metallic materials such as tantalum (Ta), platinum (Pt), ruthenium (Ru), composite layers or alloys of the above materials, or other suitable conductive materials. The pinned layer 52 may include an antiferromagnetic layer and a reference layer. The antiferromagnetic layer may include antiferromagnetic materials, such as iron-manganese (FeMn), platinum-manganese (PtMn), iridium-manganese (IrMn), nickel oxide (NiO), cobalt / platinum (Co / Pt) composite layers, or other suitable antiferromagnetic materials. The reference layer in free layer 54 and locked layer 52 may include ferromagnetic materials, such as iron, cobalt, nickel, cobalt-iron (CoFe) alloy, cobalt-iron-boron (CoFeB), or other suitable ferromagnetic materials. The first barrier layer 53 and the second barrier layer 55 may include insulating materials, such as magnesium oxide (MgO), aluminum oxide, or other suitable insulating materials. The material layers in the aforementioned magnetic tunneling junction stack 50 may be formed using deposition processes such as sputtering, but are not limited thereto.

[0054] In some embodiments, the patterning fabrication process 90 may include sequentially forming a first mask layer 61, a second mask layer 62, an organic dielectric layer 63, an anti-reflection layer 64, and a patterned photoresist layer 65 on a magnetic tunneling junction stack 50. The first mask layer 61 and the second mask layer 62 preferably comprise different materials; for example, the first mask layer 61 may comprise silicon nitride and the second mask layer 62 may comprise silicon oxide, but this is not a limitation. The organic dielectric layer 63 may comprise an organic distribution layer (ODL) or other suitable organic dielectric material, and the anti-reflection layer 64 may comprise a silicon-containing hard mask bottom anti-reflecting coating (SHB) or other suitable anti-reflection material. Then, one or more etching steps can be used to remove portions of the first mask layer 61, portions of the second mask layer 62, portions of the magnetic tunneling junction stack 50, the capping layer 32, and portions of the first intermetallic dielectric layer 31, thereby forming a magnetic tunneling junction structure 50S on the interconnect structure 40.

[0055] It is worth noting that the capping layer 32 can be removed by the etching step in the patterning process 90. For example, in some embodiments, the patterning process 90 may include a reactive ion etching (RIE) process and an ion beam etching (IBE) process. The reactive ion etching process can be used to etch the first mask layer 61, the second mask layer 62, and a portion of the magnetic tunneling junction stack 50, while the ion beam etching process can be performed after the reactive ion etching process, using the second mask layer 62 as a mask to etch the magnetic tunneling junction stack 50 to form the magnetic tunneling junction structure 50S. The capping layer 32 and a portion of the first intermetallic dielectric layer 31 can be removed by the ion beam etching process in the patterning process 90, but are not limited thereto. Due to the characteristics of the ion beam etching process, after the patterning process 90, the upper surface of the remaining first intermetallic dielectric layer 31 (e.g., Figure 3 The first upper surface 31T shown may include a recessed surface, such as a concave arcuate surface, and the first upper surface 31T of the first intermetallic dielectric layer 31 may be lower than an upper surface of the connection structure 40 in the thickness direction of the substrate 10 (e.g., the first direction D1). Figure 3 The second upper surface 40T shown. Furthermore, in some embodiments, the capping layer 32 is preferably completely removed by the patterning process 90 to prevent the capping layer 32 from remaining on the first intermetallic dielectric layer 31 after the patterning process 90 and affecting the magnetic tunnel junction structure 50S and the connection structure 40 in the horizontal direction (e.g., ...). Figure 3 The dielectric material isolation effect between the magnetic tunneling junction structure 50S and the connecting structure 40 and other adjacent magnetic tunneling junction structures 50S and connecting structures 40 in the second direction (D2) parallel to the surface of the substrate 10, and / or the dielectric material isolation effect between the magnetic tunneling junction structure 50S and the connecting structure 40 and other subsequently formed conductive structures in the second direction (D2).

[0056] Then, as Figure 4 and Figure 5 As shown, a second inter-metal dielectric layer 70 is formed on the first inter-metal dielectric layer 31, and the second inter-metal dielectric layer 70 may surround the magnetic tunneling junction structure 50S in a horizontal direction (e.g., the second direction D2). In some embodiments, a spacer wall 66S may be formed on the sidewall of the magnetic tunneling junction structure 50S before forming the second inter-metal dielectric layer 70. The spacer wall 66S may include, but is not limited to, first conformally forming a spacer wall material layer 66 on the magnetic tunneling junction structure 50S, the connection structure 40, and the first inter-metal dielectric layer 31, and then etching the spacer wall material layer 66 to remove a portion of the spacer wall material layer 66 (e.g., the spacer wall material layer 66 located on the first inter-metal dielectric layer 31), and the spacer wall material layer 66 remaining on the sidewall of the magnetic tunneling junction structure 50S forms the spacer wall 66S. The spacer wall material layer 66 may include silicon oxide, silicon oxynitride, silicon carbide nitride, aluminum oxide, or other insulating materials that have a more protective effect than the second inter-metal dielectric layer 70. Furthermore, in some embodiments, the upper part of the connection structure 40 may be etched by the patterning process described above for forming the magnetic tunnel junction structure 50S to have sidewalls not covered by the first intermetallic dielectric layer 31, and the gap wall 66S may further cover the sidewalls of the upper part of the connection structure 40 to achieve a protective effect, especially when the sidewalls directly expose the metal layer 42 in the connection structure 40.

[0057] In some embodiments, the second intermetallic dielectric layer 70 may include a low-dielectric-constant dielectric material and / or an ultra-low-dielectric-constant dielectric material, such as benzocyclobutene, HSQ, MSQ, siloxane hydrocarbons, or / or porous dielectric materials. The dielectric constant of the second intermetallic dielectric layer 70 may be lower than 2.9, and preferably lower than 2.7, but is not limited thereto. Since the spacer wall 66S is preferably formed of a material that effectively blocks external substances from entering the magnetic tunneling junction structure 50S, and the low dielectric constant characteristic of the second intermetallic dielectric layer 70 is mainly used to improve the electrical interference between multiple magnetic tunneling junction structures 50S and / or between the magnetic tunneling junction structure 50S and other conductive structures, the dielectric constant of the second intermetallic dielectric layer 70 may be lower than the dielectric constant of the spacer wall 66S and the aforementioned Figure 2 The dielectric constant of the capping layer 32 in the middle.

[0058] like Figure 2 , Figure 3 as well as Figure 5 As shown, in some embodiments, the capping layer 32 is preferably completely removed by the patterning process 90, so that the second intermetallic dielectric layer 70 can directly contact the first intermetallic dielectric layer 31, and the second intermetallic dielectric layer 70 can completely cover the first upper surface 31T of the first intermetallic dielectric layer 31, but this is not a limitation. Furthermore, in some embodiments, the material composition of the first intermetallic dielectric layer 31 may be the same as that of the second intermetallic dielectric layer 70, but this is not a limitation. In some embodiments, the material composition of the first intermetallic dielectric layer 31 may also be different from that of the second intermetallic dielectric layer 70. For example, in some embodiments, after the second intermetallic dielectric layer 70 is formed, a planarization process such as chemical mechanical polishing (CMP) can be performed to remove the second intermetallic dielectric layer 70 located on the magnetic tunneling junction structure 50S and to make the upper surface of the second intermetallic dielectric layer 70 substantially flush with the upper surface of the magnetic tunneling junction structure 50S. Then, a patterning process is performed to form a contact hole penetrating the second intermetallic dielectric layer 70, the first intermetallic dielectric layer 31, and the stop layer 23, exposing a portion of the interconnect structure 22 (e.g., the interconnect structure 22 located on the logic region) that does not correspond to the connection structure 40, and a contact plug 80 is formed in the contact hole. The contact plug 80 may include barrier materials such as titanium, titanium nitride, tantalum, or tantalum nitride, and low-resistance materials such as tungsten, copper, aluminum, titanium-aluminum alloy, or cobalt-tungsten phosphide. Therefore, when performing the fabrication process to form the contact plug 80, the upper second intermetallic dielectric layer 70 preferably has higher hardness to avoid the inability to form the required shape of the contact hole corresponding to the contact plug 80, which would affect the fabrication yield. Therefore, the material composition of the second intermetallic dielectric layer 70 may be different from the material composition of the first intermetallic dielectric layer 31. For example, in some embodiments, the dielectric constant of the first intermetallic dielectric layer 31 may be lower than that of the second intermetallic dielectric layer 70, while the hardness of the second intermetallic dielectric layer 70 may be higher than that of the first intermetallic dielectric layer 31.

[0059] Using the above-described manufacturing method, the following can be obtained: Figure 5 The semiconductor device 100 shown is illustrated. Figure 5As shown, the semiconductor device 100 may include a substrate 10, a connection structure 40, a first intermetallic dielectric layer 31, a magnetic tunneling junction structure 50S, and a second intermetallic dielectric layer 70. The connection structure 40 is disposed on the substrate 10. The first intermetallic dielectric layer 31 is disposed on the substrate 10 and surrounds the connection structure 40. The magnetic tunneling junction structure 50S is disposed on the connection structure 40. The second intermetallic dielectric layer 70 is disposed on the first intermetallic dielectric layer 31 and surrounds the magnetic tunneling junction structure 50S. In some embodiments, the semiconductor device 100 may be considered as a magnetoresistive random access memory (MRAM) device, but is not limited thereto. Furthermore, in some embodiments, the semiconductor device 100 may also include a contact plug 80 penetrating the second intermetallic dielectric layer 70, the first intermetallic dielectric layer 31, and the stop layer 23 in a first direction D1. By utilizing a first intermetallic dielectric layer 31 and a second intermetallic dielectric layer 70 with low dielectric constant characteristics between adjacent connection structures 40, between adjacent magnetic tunnel junction structures 50S, between contact plugs 80 and connection structures 40, and between contact plugs 80 and connection structures 40, the electrical interference between adjacent magnetic tunnel junction structures 50S and / or between magnetic tunnel junction structures 50S and contact plugs 80 can be reduced, thereby improving the operational performance of the semiconductor device 100.

[0060] In summary, in the semiconductor device and its fabrication method, a capping layer is formed on a first intermetallic dielectric layer, and then removed during the patterning process for forming a magnetic tunneling junction structure, allowing a second intermetallic dielectric layer surrounding the magnetic tunneling junction structure to be formed on the first intermetallic dielectric layer. By using a first intermetallic dielectric layer and a second intermetallic dielectric layer with low dielectric constants, electrical interference between magnetic tunneling junction structures and / or between magnetic tunneling junction structures and other conductive structures can be improved, thereby enhancing the operational performance of the semiconductor device. Furthermore, in some embodiments, the dielectric constant of the first intermetallic dielectric layer may be lower than that of the second intermetallic dielectric layer, while the hardness of the second intermetallic dielectric layer may be higher than that of the first intermetallic dielectric layer, thereby improving the yield of the related fabrication processes.

[0061] The above description is only a preferred embodiment of the present invention. All equivalent changes and modifications made in accordance with the claims of the present invention should be included within the scope of the present invention.

Claims

1. A method for manufacturing a semiconductor device, comprising: A first intermetallic dielectric layer is formed on the substrate; A capping layer is formed on the first intermetallic dielectric layer; A connection structure is formed on the substrate, wherein the connection structure penetrates the capping layer and the first intermetallic dielectric layer; A magnetic tunneling junction stack is formed on the connection structure and the capping layer; A patterning process is used to fabricate the magnetic tunneling junction stack to form a magnetic tunneling junction structure on the connection structure. The capping layer is completely removed by the patterning process, a portion of the first intermetallic dielectric layer is removed by the patterning process, and the upper part of the connection structure is etched by the patterning process to have sidewalls not covered by the first intermetallic dielectric layer. A gap wall is formed on the sidewall of the magnetic tunneling junction structure and the sidewall of the connecting structure; as well as A second intermetallic dielectric layer is formed on the first intermetallic dielectric layer, wherein the second intermetallic dielectric layer surrounds the magnetic tunneling junction structure, and the second intermetallic dielectric layer directly contacts the first intermetallic dielectric layer, and the dielectric constant of the second intermetallic dielectric layer is lower than the dielectric constant of the spacer wall.

2. The method for manufacturing a semiconductor device as claimed in claim 1, wherein the capping layer is a dielectric capping layer, and the dielectric constant of the first intermetallic dielectric layer is lower than the dielectric constant of the capping layer.

3. The method for manufacturing a semiconductor device as claimed in claim 2, wherein the dielectric constant of the second intermetallic dielectric layer is lower than the dielectric constant of the capping layer.

4. The method for manufacturing a semiconductor device as claimed in claim 1, wherein the hardness of the capping layer is higher than the hardness of the first intermetallic dielectric layer.

5. The method for fabricating a semiconductor device as claimed in claim 1, wherein the patterning process includes an ion beam etching process.

6. The method for manufacturing a semiconductor device as claimed in claim 1, wherein the thickness of the first intermetallic dielectric layer is greater than or equal to the thickness of the capping layer.

7. The method for manufacturing a semiconductor device as claimed in claim 1, further comprising: Before forming the first intermetallic dielectric layer, a stop layer is formed on the substrate, wherein the first intermetallic dielectric layer is formed on the stop layer, the connection structure also extends through the stop layer, and the dielectric constant of the first intermetallic dielectric layer is lower than the dielectric constant of the stop layer.

8. The method for manufacturing a semiconductor device as claimed in claim 1, further comprising: The gap wall is formed before the second intermetallic dielectric layer is formed.

9. The method of fabricating a semiconductor device as claimed in claim 1, wherein the step of forming the spacer wall comprises: A spacer wall material layer is conformally formed on the magnetic tunnel junction structure, the connection structure, and the first intermetallic dielectric layer; as well as An etching process is performed on the spacer wall material layer to remove a portion of the spacer wall material layer.

10. The method for manufacturing a semiconductor device as claimed in claim 1, wherein the dielectric constant of the first intermetallic dielectric layer and the dielectric constant of the second intermetallic dielectric layer are both less than 2.

9.

11. The method for manufacturing a semiconductor device as claimed in claim 1, wherein the material composition of the first intermetallic dielectric layer is the same as the material composition of the second intermetallic dielectric layer.

12. The method for manufacturing a semiconductor device as claimed in claim 1, wherein the material composition of the first intermetallic dielectric layer is different from the material composition of the second intermetallic dielectric layer.

13. A semiconductor device, characterized by comprising: include: Base; A connection structure is provided on this base; A first intermetallic dielectric layer is disposed on the substrate and surrounds the connection structure; A magnetic tunnel junction structure is disposed on the connection structure; Spacer walls are provided on the sidewalls of the magnetic tunneling junction structure and the sidewalls of the connecting structure; as well as A second intermetallic dielectric layer is disposed on the first intermetallic dielectric layer and surrounds the magnetic tunneling junction structure, wherein the dielectric constant of the first intermetallic dielectric layer is lower than that of the second intermetallic dielectric layer, the hardness of the second intermetallic dielectric layer is higher than that of the first intermetallic dielectric layer, the second intermetallic dielectric layer is in direct contact with the first intermetallic dielectric layer, and the dielectric constant of the second intermetallic dielectric layer is lower than that of the spacer wall.

14. The semiconductor device of claim 13, wherein the dielectric constant of the first intermetallic dielectric layer and the dielectric constant of the second intermetallic dielectric layer are both less than 2.

9.

15. The semiconductor device of claim 13, wherein the upper surface of the first intermetallic dielectric layer includes a recessed surface, and the second intermetallic dielectric layer completely covers the upper surface of the first intermetallic dielectric layer.

16. The semiconductor device of claim 13, wherein the upper surface of the first intermetallic dielectric layer is lower than the upper surface of the interconnect structure in a thickness direction of the substrate.

Citation Information

Patent Citations

  • Self-aligned top contact for MRAM fabrication

    CN106104829A

  • MTJ structure and integration scheme

    US20130119494A1