Soft-pack secondary batteries with excellent insulation and heat dissipation properties

By bonding an insulating coating containing high thermal conductivity heat dissipation particles to the curved sealing part and platform part of the soft-pack secondary battery, the problems of insufficient sealing and insulation are solved, achieving excellent sealing, insulation and heat dissipation effects, and improving the overall safety of the battery.

CN116802893BActive Publication Date: 2026-11-10LG ENERGY SOLUTION LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202280008458.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2022-07-18
Filing Date
2022-08-22
Publication Date
2026-11-10
Estimated Expiration
2042-08-22

AI Technical Summary

Technical Problem

Existing soft-pack secondary batteries suffer from insufficient sealing, poor insulation, and inadequate heat dissipation. In particular, they are prone to contamination and dielectric breakdown during the heat sealing process, and existing external insulation methods are easily peeled off.

Method used

A curved seal is formed at the curved portion of the electrode assembly housing, and an insulating coating is bonded between the inner and outer surfaces. The coating contains an adhesive and heat dissipation particles with high thermal conductivity to ensure bonding strength and heat dissipation effect. An insulating coating is also applied to the platform portion to enhance sealing and insulation.

Benefits of technology

It significantly improves the sealing performance, insulation properties, and heat dissipation properties of the sealing part, enhances the safety and reliability of the battery, and prevents moisture penetration and electrolyte leakage.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116802893B_ABST
    Figure CN116802893B_ABST
Patent Text Reader

Abstract

The present invention provides a pouch-type secondary battery, comprising a pouch-type battery housing including an electrode assembly receiving portion and a sealing portion; an electrode assembly housed in the electrode assembly receiving portion; and an insulating coating laminated on the sealing portion, wherein the insulating coating comprises an adhesive and heat dissipation particles having a thermal conductivity of 0.2 W / (mk) or higher.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application claims priority based on Korean Patent Application No. 10-2021-0115869 filed on August 31, 2021 and Korean Patent Application No. 10-2022-0088456 filed on July 18, 2022, the entire contents of which are incorporated herein by reference.

[0002] This invention relates to a pouch-type secondary battery with excellent insulation and heat dissipation properties. Background Technology

[0003] Among the recently increasing use of secondary batteries, there is a growing demand for rectangular and pouch-type batteries. Considering their shape, these batteries are suitable for use in products such as mobile phones due to their thinness. In terms of materials, there is an increasing demand for lithium-ion batteries, such as lithium-ion polymer batteries, which offer advantages such as high energy density, discharge voltage, and output stability.

[0004] The secondary battery can be classified according to the structure of the electrode assembly forming an anode / separation membrane / cathode structure. Examples of such electrode assemblies include gel roll (wound type) electrode assemblies in which long sheet-like anodes and cathodes are wound with a separation membrane inserted between them; stacked (laminated type) electrode assemblies in which a large number of anodes and cathodes cut into predetermined sizes are sequentially laminated with a separation membrane inserted between them; and stacked / folded type electrode assemblies, etc., in which dual cells or full cells (in which predetermined units of anodes and cathodes are laminated with a separation membrane inserted between them) are wound together with the separation membrane.

[0005] In recent years, pouch cells, in which stacked / folded electrode assemblies are incorporated into a pouch cell housing made of aluminum laminates, have attracted much attention due to their low manufacturing rate, light weight, and ease of deformation, and their usage has gradually increased.

[0006] Figure 1 The general structure of a typical pouch-type secondary battery in the prior art is shown. (Refer to...) Figure 1 The pouch-type secondary battery 100 includes an electrode assembly 20, an electrode sheet 50 extending from the electrode assembly 20, electrode leads 40 welded to the electrode sheet 50, and a battery housing 10 housing the electrode assembly. A lead insulation coating 60 is attached to a portion of the upper and lower surfaces of the electrode leads 40 to improve the seal with the battery housing 10 and simultaneously ensure electrical insulation.

[0007] This type of pouch cell battery is manufactured by housing electrode components within a laminate, injecting electrolyte, and sealing it using methods such as heat sealing. In this manufacturing process, there are problems such as the heat-sealed area (the sealing part) potentially becoming contaminated during electrolyte injection, or the resin layer potentially protruding outwards due to excessive melting and / or compression of the innermost resin layer of the laminate. Contamination of the sealing part and the outward protrusion of the inner resin layer contribute to an incomplete seal, and defects in the sealing part cause serious problems such as moisture penetration and electrolyte leakage.

[0008] Furthermore, it is known that pouch cells suffer from dielectric breakdown due to metal exposure at the ends of the laminates that form the battery casing.

[0009] To address this issue, existing technologies have proposed methods for externally insulating the heat-sealed portion using PET labels, tapes, etc. However, when using PET labels, tapes, etc. to externally insulate the heat-sealed portion, it is known that the labels and tapes may peel off, and defects such as bubbles and wrinkles may occur.

[0010] In recent years, pouch cells have also introduced methods to improve sealing by applying sealing agents to the exterior of the heat-sealed portion. However, it is not easy to apply a sealing agent with a predetermined viscosity and flowability to the exterior of the heat-sealed portion on a thin vertical cross-section. Because the sealing agent flows downwards during the curing process after application, and the desired effect is difficult to achieve, it seems difficult to apply it to actual large-scale production processes.

[0011] Therefore, there is a need to develop a technology that can improve the sealing performance of thermally sealed parts by solving the problems of existing technologies and reliably prevent dielectric breakdown.

[0012] [Existing Technical Documents]

[0013] [Patent Literature]

[0014] Korean Patent No. 10-1216422 Summary of the Invention

[0015] Technical issues

[0016] The present invention aims to solve the above-mentioned problems of the prior art.

[0017] One object of the present invention is to provide a pouch-type secondary battery with improved sealing and insulation properties of the sealing portion.

[0018] Another object of the present invention is to provide a pouch-type secondary battery in which the heat dissipation characteristics of the sealing portion are improved.

[0019] Technical solution

[0020] To achieve the above objectives, the present invention provides a pouch-type secondary battery, comprising:

[0021] A soft-pack battery casing including an electrode assembly housing and a sealing portion; and

[0022] The electrode assembly housed in the electrode assembly housing.

[0023] The sealing portion includes a curved portion formed by bending the sealing portion toward the electrode assembly receiving portion.

[0024] An insulating coating is bonded to the inner and outer surfaces of the curved portion based on the electrode assembly housing, as well as the curved end face that forms a boundary between the inner and outer surfaces.

[0025] The outer surface of the insulating coating bonded to the inner surface of the bend is bonded to the outer surface of the wall of the electrode assembly housing, and

[0026] The insulating coating includes an adhesive and heat dissipation particles having a thermal conductivity of 0.2 W / (mk) or higher, and the joints bonded to the outer surface of the wall of the electrode assembly housing do not include the heat dissipation particles.

[0027] In one embodiment of the invention, the joint may have a thickness of 1 μm to 100 μm from the outer surface of the wall of the electrode assembly receiving portion.

[0028] In one embodiment of the present invention, the insulating coating on the inner and outer surfaces of the curved portion of the electrode assembly receiving portion and the end face of the curved portion forming a boundary between the inner and outer surfaces can be formed by bending and bonding the insulating coating film.

[0029] In one embodiment of the present invention, the insulating coating film can be bonded by heat sealing.

[0030] In one embodiment of the present invention, the sealing portion may further include a terrace portion positioned parallel to the upper or lower surface of the electrode assembly receiving portion.

[0031] The insulating coating is further laminated into the space formed between the outer surface of the platform portion and the outer surface of the electrode assembly housing portion, and

[0032] The insulating coating includes an adhesive and heat dissipation particles having a thermal conductivity of 0.2 W / (mk) or higher, and the joints bonded to the outer surface of the wall of the electrode assembly housing do not include heat dissipation particles.

[0033] In one embodiment of the invention, the joint may have a thickness of 1 μm to 100 μm from the outer surface of the wall of the electrode assembly receiving portion.

[0034] In one embodiment of the present invention, the height of the insulating coating may be equal to or less than the height of the wall of the electrode assembly receiving portion.

[0035] In one embodiment of the invention, the electrode leads may be located at the tip of the platform portion.

[0036] In one embodiment of the invention, the portion of the insulating coating containing heat-dissipating particles may include 10% to 90% by weight of an adhesive and 10% to 90% by weight of heat-dissipating particles.

[0037] In one embodiment of the present invention, the heat dissipation particles may have an average particle size of 0.1 μm to 10 μm.

[0038] In one embodiment of the invention, the curved portion may include a portion formed by folding and overlapping the sealing portion more than twice.

[0039] Beneficial effects

[0040] The pouch-type secondary battery of the present invention provides excellent sealing performance, excellent insulation properties, and particularly excellent heat dissipation properties.

[0041] Therefore, the pouch-type secondary battery of the present invention provides a significant improvement in battery safety. Attached Figure Description

[0042] Figure 1 This is an exploded perspective view of a traditional pouch-type secondary battery.

[0043] Figure 2 This is a perspective view schematically illustrating one embodiment of the pouch-type secondary battery of the present invention.

[0044] Figure 3 It is cut along section AA. Figure 2 A cross-sectional view of a pouch-type secondary battery.

[0045] Figure 4 This is a schematic cross-sectional view illustrating the form of an insulating coating film as an embodiment of the present invention.

[0046] Figure 5 This is a perspective view schematically illustrating one embodiment of the pouch-type secondary battery of the present invention.

[0047] Figure 6 It is cut along section BB. Figure 5 A cross-sectional view of a pouch-type secondary battery.

[0048] Figure 7 This is a perspective view schematically illustrating the form of an insulating coated rod as an embodiment of the present invention.

[0049] Figures 8 to 10 This is a cross-sectional view schematically illustrating one embodiment of the pouch-type secondary battery of the present invention. Detailed Implementation

[0050] The embodiments of the present invention will now be described in detail with reference to the accompanying drawings to enable those skilled in the art to readily implement the invention. However, the present invention can be implemented in many different forms and is not limited to the embodiments set forth herein. Similar components are designated by the same reference numerals throughout this specification.

[0051] When a component is described as being "connected to, set up, or installed" in another component, it can be directly connected to or installed in the other component, but it should be understood that other structures may also exist between them. On the other hand, when a component is described as being "directly connected to, set up, or installed" in another component, it should be understood that there are no other components between them. Furthermore, other expressions describing the relationship between constituent elements, namely "on" and "directly on," or "between" and "exactly between," or "adjacent to" and "directly adjacent," should also be interpreted in the same way.

[0052] Figure 1 This also applies to the exploded perspective view of the conventional pouch-type secondary battery of the present invention. Figure 2 and Figure 5 This is a perspective view schematically illustrating one embodiment of the pouch-type secondary battery of the present invention.

[0053] like Figure 1 and Figure 2 The pouch-type secondary battery 100 of the present invention shown includes: a pouch-type battery housing 10 including an electrode assembly receiving portion 11 and a sealing portion 12; and an electrode assembly 20 housed in the electrode assembly receiving portion 11.

[0054] The sealing portion 12 includes a curved portion 12-1 formed by bending toward the electrode assembly receiving portion 11.

[0055] The insulating coating 30 is bonded to the inner and outer surfaces of the curved portion 12-1 based on the electrode assembly receiving portion 11, and to the curved portion end face that forms a boundary between the inner and outer surfaces.

[0056] The outer surface of the insulating coating 30, which is bonded to the inner surface of the bent portion 12-1, is bonded to the outer surface of the wall of the electrode assembly receiving portion 11.

[0057] The insulating coating 30 includes an adhesive and heat dissipation particles 32 having a thermal conductivity of 0.2 W / (mk) or higher, and the joint 30a bonded to the outer surface of the electrode assembly housing does not include the heat dissipation particles 32.

[0058] Despite efforts to improve the sealing and insulation properties of the sealing portion in existing pouch-type secondary batteries, the improvement has been insufficient. The present invention is characterized by improved sealing and insulation properties of the sealing portion and significantly improved heat dissipation characteristics. In particular, a drawback of the insulating layer formed on the conventional sealing portion is that the overall adhesive strength of the pouch-type battery casing is insufficient due to the inclusion of heat-dissipating particles, and the adhesive state cannot be maintained for a long period. The present invention has technical features that solve the aforementioned problems of the prior art.

[0059] The joint 30a may have a thickness of 1 μm to 100 μm, preferably 5 μm to 20 μm, from the outer surface of the wall of the electrode assembly receiving portion 11. If the thickness of the joint 30a is less than 1 μm, the adhesive strength is reduced; if the thickness of the joint 30a exceeds 100 μm, the heat dissipation effect is reduced.

[0060] The insulating coating 30 of the inner and outer surfaces of the curved portion 12-1 of the electrode assembly receiving portion 11 and the curved end face that forms a boundary between the inner and outer surfaces can be connected to each other.

[0061] The insulating coating 30, based on the inner and outer surfaces of the curved portion of the electrode assembly receiving portion 11, and the curved portion end face forming the boundary between the inner and outer surfaces, can be as follows: Figure 4 The insulating coating film 34 is formed by bending and bonding. At this time, the bent portion of the insulating coating film 34 can be bonded so that it is located on the end face of the bent portion that forms a boundary between the inner surface and the outer surface.

[0062] The adhesion of the insulating coating film 34 can be achieved by thermal fusion.

[0063] In one embodiment of the present invention, it can be used as Figure 4 The insulating coating film 34 is manufactured in the form shown. The insulating coating film 34 can be manufactured, for example, by preparing an insulating coating heat-dissipating composition containing an adhesive and heat-dissipating particles having a thermal conductivity of 0.2 W / (mK) or higher; applying the heat-dissipating composition to a substrate and curing the composition to form a first coating; then dividing the upper surface of the first coating, coating a portion of the upper surface with the insulating coating heat-dissipating composition, and coating and curing the adhesive composition in another portion. The insulating coating film 34 can be manufactured by known extrusion (injection) methods.

[0064] Furthermore, the insulating coating film 34 can be manufactured by forming a first coating, then dividing the upper surface of the first coating, and applying and curing an adhesive composition only in a portion thereof (joint portion 30a only). The insulating coating film 34 can also be manufactured by known extrusion (injection) methods.

[0065] In one embodiment of the present invention, the thickness of the insulating coating film 34 can be from 20 μm to 1 μm, preferably from 40 μm to 200 μm.

[0066] In one embodiment of the invention, the sealing portion 12 further includes a platform portion (non-bent portion) positioned in a direction parallel to the upper or lower surface of the electrode assembly receiving portion 11. At this time, as... Figure 5 and Figure 6 As shown, the insulating coating 30' can be further laminated in the space formed between the platform portion and the outer surface of the wall of the electrode assembly receiving portion 11.

[0067] The insulating coating 30' includes an adhesive and heat dissipation particles 32 having a thermal conductivity of 0.2 W / (mk) or higher, and the joint 30'a bonded to the outer surface of the wall of the electrode assembly housing may be in the form of not including the heat dissipation particles 32.

[0068] The joint 30'a may have a thickness of 1 μm to 100 μm, preferably 5 μm to 20 μm, from the outer surface of the wall of the electrode assembly receiving portion 11. If the thickness of the joint 30'a is less than 1 μm, the adhesive strength is reduced; if the thickness of the joint 30'a exceeds 100 μm, the heat dissipation effect is reduced.

[0069] The insulating coating 30' can be formed in the form of a space suitable for forming between the platform portion and the outer surface of the wall of the electrode assembly receiving portion 11, and can be, for example, in a manner similar to... Figure 5 and 6 The square column form shown is not limited to this.

[0070] Insulating coating 30' can be used as follows Figure 7 The insulating coating rod 36 shown is formed. The insulating coating rod 36 can have a shape similar to a square column, but can have a suitable shape according to the shape of the pouch battery casing.

[0071] The insulating coated rod 36 can be bonded by heat fusion, or it can be bonded using another adhesive.

[0072] In one embodiment of the invention, the insulating coating 30' may be formed only on the platform portion in the direction where the electrode lead 40 is located, or as... Figure 5 and Figure 6 As shown, the insulating coating 30' can be formed on the platform portion in the direction where the electrode lead 40 is located and on the platform portion on its opposite side.

[0073] In one embodiment of the present invention, such as Figure 9As shown, the insulating coating 30' can be formed in the form of covering the top of the platform portion, or it can be formed in the form of covering the top of the platform portion and part or all of the lower surface of the platform portion.

[0074] In one embodiment of the present invention, the height of the insulating coating 30' may be the same as or lower than the height of the wall of the electrode assembly receiving portion 11.

[0075] In one embodiment of the present invention, such as Figure 5 and 6 As shown, electrode lead 40 can be placed at the top of the platform.

[0076] In one embodiment of the invention, portions 30b and 30'b of the insulating coatings 30 and 30' containing heat-dissipating particles may comprise 10% to 90% by weight of an adhesive and 10% to 90% by weight of heat-dissipating particles. Preferably, it may comprise 30% to 70% by weight of an adhesive and 30% to 70% by weight of heat-dissipating particles, more preferably 40% to 60% by weight of an adhesive and 40% to 60% by weight of heat-dissipating particles. Furthermore, in addition to the above-described components, it may further comprise known components in the art for insulating coatings.

[0077] If the heat dissipation particles are less than 10% by weight, heat dissipation may not be expected. If the heat dissipation particles exceed 10% by weight, the adhesive strength of the insulating coatings 30 and 30' may deteriorate, and therefore is not preferred.

[0078] Photocurable or thermosetting polymers can be used as adhesives. Polyurethane resins, polyethylene resins, polypropylene resins, polybutene resins, polystyrene resins, polyethylene terephthalate resins, polycarbonate resins, polybutadiene resins, unsaturated polyester resins, polyimide resins, and polyacrylate resins can be used alone or in mixtures of two or more, but are not limited thereto. Examples of polyacrylate resins may include polyester acrylates, epoxy acrylates, and polyurethane acrylates.

[0079] Examples of heat dissipation particles with a thermal conductivity of 0.2 W / (mk) or higher include aluminum, carbon, copper, chromium, titanium, stainless steel particles, etc., which can be used alone or in combination of two or more.

[0080] The heat dissipation particles can have an average particle size of 0.1 μm to 10 μm, but are not limited to this range.

[0081] The heat dissipation particles preferably have a conductivity of 0.2 S / cm or less. If the conductivity is higher than this range, the insulation properties may deteriorate, which is not preferred.

[0082] In one embodiment of the invention, the joints 30a and 30'a on the outer surfaces of the walls of the electrode assembly housings, which do not include heat dissipation particles in the insulating coatings 30 and 30', may include adhesives and additives conventionally used in the art to improve adhesive strength, and may consist only of the aforementioned adhesives.

[0083] In one embodiment of the present invention, such as Figure 2 , Figure 3 and Figure 8 As shown, the sealing portion 12 includes a curved portion 12-1 formed by bending the sealing portion toward the electrode assembly receiving portion.

[0084] Based on the non-bent portion of the sealing portion, the bent portion 12-1 can be bent by 80 to 180 degrees, preferably 85 to 145 degrees, and more preferably 90 to 100 degrees.

[0085] In one embodiment of the present invention, such as Figure 8 As shown, the curved portion 12-1 may include a portion in which the sealing portion is folded and overlapped more than twice.

[0086] In one embodiment of the invention, since the electrode assembly 20 can have any form known in the art without limitation, its detailed description will be omitted.

[0087] There are no special restrictions on the electrode assembly 20, as long as it has a structure that connects multiple electrode plates to form an anode and a cathode, and it can have a stacked / folded structure or a laminated stacked structure.

[0088] In addition, the battery housing 10 is made of a laminate including a metal layer and a resin layer, such as an aluminum laminate, and may be a soft-pack battery housing including an electrode assembly housing and a sealing portion.

[0089] The battery housing 10 can be made from a single-cell laminate, in which case a housing body portion including an electrode assembly receiving portion surrounding a bend and a cover portion attached to the housing body to surround the electrode assembly receiving portion can be formed.

[0090] A platform portion having electrode terminals (the electrode terminals having a structure where electrode plates protruding from the electrode assembly are connected to electrode leads) can be located at the portion facing the bend of the laminate, and side sealing portions adjacent to each of the two ends of the platform portion can be located there. The bend can be formed in the side sealing portions.

[0091] Example 1: Manufacturing an insulating coating film

[0092] An insulating coating heat dissipation composition was prepared by adding polyurethane adhesive and aluminum / carbon composite material (particle size: 0.1 μm) as heat dissipation particles with a thermal conductivity of 0.2 W / (mk) or higher to acetone solvent in a weight ratio of 1:9.

[0093] In addition, polyurethane adhesives are added to acetone solvents to prepare insulating coating adhesive compositions.

[0094] An insulating coating heat dissipation composition is applied to a substrate and cured to form a first coating.

[0095] Next, according to Figure 4 The insulating coating film shown is used to divide the upper surface of the first coating, and an insulating coating adhesive composition is applied to a portion of the outer surface of the wall of the electrode assembly to be bonded to it. The remaining portion is then coated with an insulating coating heat dissipation composition and cured to prepare the coating. Figure 4 The insulating coating film shown.

[0096] Comparative Example 1: Manufacturing an insulating coating film

[0097] The heat dissipation composition for insulating coating prepared in Example 1 was applied to the same thickness as the insulating coating film prepared in Example 1 and cured to prepare the insulating coating film.

[0098] Example 2: Forming an insulating layer on the sealing portion of a pouch-type secondary battery

[0099] In the sealing portion of the pouch cell housing that houses the electrode assembly, a portion of the side of the electrode assembly housing is left unsealed, and the remaining portion is bent at 90 degrees toward the electrode assembly housing to form a bend. Subsequently, the insulating coating film prepared in Example 1 is folded and then heat-sealed to form a shape as shown in the image. Figure 2 The insulating coating shown.

[0100] Comparative Example 2: Forming an insulating layer on the sealing part of a pouch-type secondary battery

[0101] An insulating coating was formed in the same manner as in Example 2, except that the insulating coating film prepared in Preparation Example 1 was used.

[0102] Test Example 1: Evaluation of the Adhesion Performance of Insulating Coatings

[0103] While storing the pouch-type secondary batteries of Example 2 and Comparative Example 2 at temperatures below 65°C, the insulation coating was checked for peeling. The results are shown in Table 1 below.

[0104] [Table 1]

[0105]

[0106] Although the invention has been described with reference to limited embodiments and accompanying drawings, it is not limited thereto, and it will be apparent to those skilled in the art that various modifications and variations can be made within the scope of the technical spirit of the invention and the claims described below.

[0107] [Explanation of reference numerals in the attached figures]

[0108] 10: Battery casing; 11: Electrode assembly housing.

[0109] 12: Sealing part; 12-1: Bending part;

[0110] 20: Electrode assembly; 30, 30': Insulating coating.

[0111] 30a, 30'a: The joint between the insulating coating and the outer surface of the wall of the electrode assembly housing; 30b, 30'b: The portion of the insulating coating containing heat dissipation particles.

[0112] 32: Heat dissipation particles; 34: Insulating coating film.

[0113] 36: Insulating coated rod,

[0114] 40: Electrode lead; 50: Electrode plate.

[0115] 60: Lead wire insulation coating

Claims

1. A pouch-type secondary battery, comprising: A pouch battery casing, including an electrode assembly housing and a sealing portion; as well as Electrode assembly, housed within the electrode assembly housing. The sealing portion includes a curved portion formed by bending the sealing portion toward the electrode assembly receiving portion. An insulating coating is bonded to the inner and outer surfaces of the electrode assembly housing of the curved portion, and to the curved end face forming a boundary between the inner and outer surfaces. The outer surface of the insulating coating, which is bonded to the inner surface of the bent portion, is bonded to the outer surface of the wall of the electrode assembly receiving portion, and The insulating coating comprises: a portion containing an adhesive and heat-dissipating particles having a thermal conductivity of 0.2 w / (mk) or higher; and a joint containing an adhesive but not heat-dissipating particles. The joint is bonded to the outer surface of the wall of the electrode assembly receiving portion.

2. The soft-pack secondary battery according to claim 1, wherein, The joint portion has a distance of 1 from the outer surface of the wall of the electrode assembly receiving portion. m to 100 The thickness is m.

3. The soft-pack secondary battery according to claim 1, wherein, The insulating coating bonded to the inner and outer surfaces of the electrode assembly housing, and the insulating coating bonded to the end face of the bent portion forming the boundary between the inner and outer surfaces, are connected to each other.

4. The soft-pack secondary battery according to claim 3, wherein, The insulating coating bonded to the inner and outer surfaces of the electrode assembly housing, and the insulating coating bonded to the end face of the bent portion forming the boundary between the inner and outer surfaces, are formed by bending and bonding an insulating coating film.

5. The soft-pack secondary battery according to claim 4, wherein, The insulating coating film is bonded by heat sealing.

6. The soft-pack secondary battery according to claim 1, wherein, The sealing portion further includes a platform portion extending in a direction parallel to the upper or lower surface of the electrode assembly receiving portion. The insulating coating is further laminated in the space formed between the outer surface of the wall of the platform portion and the electrode assembly receiving portion, and the insulating coating includes: a portion containing an adhesive and heat-dissipating particles having a thermal conductivity of 0.2 w / (mk) or higher; and a bonding portion containing an adhesive but not heat-dissipating particles. The joint is bonded to the outer surface of the wall of the electrode assembly receiving portion.

7. The soft-pack secondary battery according to claim 6, wherein, The joint portion has a distance of 1 from the outer surface of the wall of the electrode assembly receiving portion. m to 100 The thickness is m.

8. The soft-pack secondary battery according to claim 6, wherein, The height of the insulating coating is equal to or less than the length between the upper and lower surfaces of the electrode assembly housing.

9. The soft-pack secondary battery according to claim 8, wherein, The electrode leads are located at the top of the platform section.

10. The pouch-type secondary battery according to claim 1 or 6, wherein, The portion of the insulating coating comprising adhesive and heat-dissipating particles includes 10% to 90% by weight of adhesive and 10% to 90% by weight of heat-dissipating particles.

11. The soft-pack secondary battery according to claim 10, wherein, The heat dissipation particles have a density of 0.

1. m to 10 The average particle size is m.

12. The soft-pack secondary battery according to claim 1, wherein, The curved portion includes the portion formed by folding and overlapping the sealing portion more than twice.

Citation Information

Patent Citations

  • Secondary Battery Having Sealing Portion of Improved Insulating Property

    KR101216422B1

  • Repeelable adhesive sheet

    KR1020210115869A

  • Dy2O3 particles with intermediate particle size distribution

    KR1020220088456A

  • Graphene nonstick paint

    CN103214897A

  • High-capacity battery of electric motorcycle for competition