A self-aligned contact area processing method, slot structure and chip
By removing interlayer dielectrics (ILDs) and filling intermediate dielectrics at the top of the shallow trench isolation (STI) structure in the flash memory chip, and combining dry and wet etching to define the trench structure, the increased resistance, load effect (LE), and control gate (CG) bridging risks in the self-aligned contact (SAC) process are resolved, and the process window is expanded.
Patent Information
- Application Number
- CN202310928547.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-07-27
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2043-07-27
AI Technical Summary
Self-aligned contact (SAC) technology in flash memory chips presents several challenges, including increased resistance of the self-aligned source (SAS), limitations on drain sidewall and memory area height, increased difficulty in filling gaps between interlayer dielectrics (ILDs), severe load effect (LE) of the main etching process (T&H) of vias, and bridging risk of the control gate (CG). Furthermore, the nitride chamfering at the end caps during the CESL etching stage can lead to a short circuit risk in the control gate (CG).
By removing interlayer dielectrics (ILDs) and filling them with intermediate dielectrics at the top of a shallow trench isolation (STI) structure pre-set on the wafer, and defining the trench structure in conjunction with dry and wet etching processes, the influence of load effect (LE) is reduced, the risk of CESL etching is avoided, and the working window of self-aligned contact (SAC) is increased.
It improves the dielectric distribution in the isolation region, reduces the impact of the load effect (LE), lowers the risk of end-cap nitride chamfering during the CESL etching stage, avoids the bridging risk of the control gate (CG), and expands the process window for self-aligned contact (SAC).
Smart Images

Figure CN116847657B_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of semiconductor processing technology, and particularly relates to a self-aligned contact area processing method, a slot structure, and a chip. Background Technology
[0002] Self-aligned contact (SAC) technology has been applied in the fabrication of chips such as flash memory, including ETOX (Erase Through Oxide) NOR flash memory. However, in order to overcome the increased resistance of the self-aligned source (SAS) introduced by cell shrinkage, the limitations of drain sidewalls and memory height, and the increased difficulty of filling the gaps (GF) in the interlayer dielectrics (ILDs), it has become a bottleneck restricting the further application of SAC.
[0003] Meanwhile, in related SAC applications, the loading effect (LE) during the trench & hole (T&H) main etching process is severe. When the oxygen / nitrogen selectivity ratio is low, the control gate (CG) bridging problem caused by the capped nitride chamfer is likely to occur; while when the oxygen / nitrogen selectivity ratio is high, it is easy to cause the trench etching to stop / abort.
[0004] Furthermore, during the nitrogen treatment stage of the Contact Etch Stop Layer (CESL) at the end of the SAC etching process, the capped nitride is further removed, which may lead to a short circuit risk in the control gate (CG). Summary of the Invention
[0005] This invention discloses a self-aligned contact area processing method, including a third slot construction step; the third slot construction step is between a first prior process and a fifth subsequent process; wherein, the first prior process forms a first slot-shaped region and a second hole-shaped region with a self-aligned contact SAC structure, and a shallow trench isolation structure (STI) is constructed between the first substrate layer and the first dielectric layer in the first slot-shaped region.
[0006] Furthermore, in the third trench construction step, the seventh interlayer dielectric is defined and removed in the first trench region according to the preset pattern of the shallow trench isolation structure (STI) projected or mapped on the wafer; wherein, in the fifth step, a preset contact structure is formed in the first trench region and the second hole region respectively by a self-aligned contact (SAC) structure in the subsequent process.
[0007] Specifically, its contact structure can be obtained by filling contact metal into the first groove region and the second hole region; its contact metal includes tungsten; and its fifth post-processing includes a first planarization treatment of its contact structure.
[0008] For example, its contact structure can be prepared by metal-organic chemical vapor deposition (MOCVD).
[0009] Furthermore, the third slot construction step can also fill the area where the seventh interlayer medium has been removed with a fourth intermediate medium, and the filling process of the fourth intermediate medium includes backfilling nitride by atomic layer deposition (ALD).
[0010] The fourth intermediate medium can be removed through the fourth planarization process, with the fifth stop line on the outer surface of the sixth dielectric layer as the boundary. After the fourth planarization process is completed, the fourth intermediate medium continues to undergo an intermediate etching step to remove the sixth dielectric layer and remove the fourth intermediate medium to the seventh stop line on the side of the fifth dielectric layer away from the first substrate layer. The fifth dielectric layer is a capped nitride on the side of the fourth dielectric layer where the control gate (CG) is located away from the first substrate layer.
[0011] Furthermore, the intermediate etching step can be divided into a pre-dry etching step and a post-wet etching step; the pre-dry etching step is used to etch the portion of the fourth intermediate dielectric located in the first trench region to the seventh stop line, and the post-wet etching step is used to further remove the portion of the sixth dielectric layer that could not be removed by the pre-dry etching step from the current sixth stop line to the seventh stop line; the post-wet etching step also removes the dielectric corresponding to the sixth dielectric layer of the second aperture region that penetrates the control gate CG, the third dielectric layer, and the aperture region of the second dielectric layer.
[0012] Specifically, its second dielectric layer is a floating gate (FG) dielectric layer; and its third dielectric layer is an oxygen-nitrogen-oxygen (ONO) dielectric layer.
[0013] The sixth dielectric layer can adopt an interlayer dielectric (ILD) structure, and its material can be silicon oxide. Its contact structure also includes a sidewall spacer, a first trench bottom dielectric layer, and a second hole bottom dielectric layer constructed concurrently with the fifth dielectric layer.
[0014] Specifically, its first trench bottom dielectric layer and second hole bottom dielectric layer can be removed by a ninth dry etching process to open its first substrate layer and penetrate its first dielectric layer.
[0015] The first dielectric layer can be a gate oxide layer; after the ninth dry etching is completed, the first groove-shaped unfilled area and the second hole-shaped unfilled area in its contact structure can be obtained.
[0016] Accordingly, embodiments of the present invention also disclose a slot structure, including a first slot region and a second hole region formed by a self-aligned contact (SAC) structure. The first slot region has a shallow trench isolation structure (STI) constructed between the first substrate layer and the first dielectric layer. The first slot region defines a seventh interlayer dielectric and removes it according to a preset pattern of the projection or mapping area of the shallow trench isolation structure (STI) on the wafer. The first slot region and the second hole region are respectively used to fill a preset metal to form a preset contact structure.
[0017] Specifically, the contact structure can be obtained by filling the first groove-shaped region and the second hole-shaped region with contact metal; the contact metal includes tungsten.
[0018] Furthermore, the area where the interlayer dielectric of the seventh layer has been removed can be filled with a fourth intermediate dielectric. The fourth intermediate dielectric is removed by a fourth planarization process with the fifth stop line on the outer surface of the sixth dielectric layer as the boundary. After the fourth planarization process is completed, the fourth intermediate dielectric continues to undergo an intermediate etching step to remove the sixth dielectric layer and remove the fourth intermediate dielectric to the seventh stop line on the side of the fifth dielectric layer away from the first substrate layer. The fifth dielectric layer is a capped nitride on the side of the fourth dielectric layer where the control gate CG is located away from the first substrate layer.
[0019] The fourth intermediate dielectric is partially etched to the seventh stop line in the first trench region, and the sixth dielectric layer is removed from the current sixth stop line to the seventh stop line; the sixth dielectric layer dielectric used to penetrate the control gate CG, the third dielectric layer and the second dielectric layer aperture region is also removed.
[0020] Specifically, its second dielectric layer is a floating gate (FG) dielectric layer; its third dielectric layer is an oxygen-nitrogen-oxygen (ONO) dielectric layer.
[0021] Furthermore, its sixth dielectric layer is an interlayer dielectric (ILD) structure, and the material of its sixth dielectric layer includes silicon oxide; its contact structure also includes a sidewall spacer, a first trench bottom dielectric layer, and a second hole bottom dielectric layer constructed concurrently with the fifth dielectric layer.
[0022] Specifically, the first trench bottom dielectric layer and the second via bottom dielectric layer can be removed by a ninth dry etching process to open the first substrate layer and penetrate the first dielectric layer; the first dielectric layer can be a gate oxide layer; and the contact structure includes a first trench-shaped unfilled area and a second via-shaped unfilled area.
[0023] Similarly, embodiments of the present invention also disclose a chip including any of the above slot structures, wherein a first slot region is used to form the drain structure of the chip, and a second hole region is used to form the source structure of the chip.
[0024] In summary, this invention improves the dielectric distribution in the isolation region by pre-setting shallow trench isolation (STI) structures at the top of the drain region or by projecting and mapping regions on the wafer to remove pre-set interlayer dielectrics (ILDs) and fill them with a fourth intermediate dielectric; then, by combining the etching process to define the first trench-shaped filling region and the second hole-shaped filling region respectively, and by combining the etching process to remove the isolation dielectric of the same material as the bottom and sidewalls of the above-mentioned regions, thereby improving the dielectric distribution in the isolation region.
[0025] If wet etching is used to define the slot structure, there is no load effect (LE). In the CESL (Contact Etch Stop Layer) etching stage, the risk of the capped nitride (CN) being removed is reduced, and the bridging risk of the control gate (CG) is also avoided, which increases the working window of the self-aligned contact (SAC) process.
[0026] It should be noted that the terms "first," "second," and similar terms used in this article are merely for describing the constituent elements of the technical solution and do not constitute a limitation on the technical solution, nor should they be interpreted as an indication or implication of the importance of the corresponding elements; elements with terms such as "first," "second," or similar terms indicate that at least one of the elements is included in the corresponding technical solution. Attached Figure Description
[0027] To more clearly illustrate the technical solution of the present invention and facilitate a further understanding of its technical effects, features, and objectives, the present invention will be described in detail below with reference to the accompanying drawings. The drawings constitute an essential part of the specification and are used together with Embodiment 1 of the present invention to illustrate the technical solution of the present invention, but do not constitute a limitation on the present invention.
[0028] The same reference numerals in the attached diagrams represent the same parts, specifically: Figure 1 This is a schematic diagram of the Nor Flash layout structure in related technologies.
[0029] Figure 2 This is a schematic diagram of the Nor Flash layout structure under the self-aligned contact SAC process in related technologies.
[0030] Figure 3 This is a schematic diagram of the bridging failure structure of the hole under the load effect of the SAC process in related technologies.
[0031] Figure 4 This is a schematic diagram illustrating the phenomenon of trench etching termination under the load effect in the SAC process in related technologies.
[0032] Figure 5 This is a schematic diagram of the layout structure of an embodiment of the present invention.
[0033] Figure 6 This is a schematic diagram of the prefabricated workpiece structure according to an embodiment of the present invention.
[0034] Figure 7 This is one of the schematic diagrams of the construction process of the fourth intermediate medium in the present invention.
[0035] Figure 8 This is the second schematic diagram of the construction process of the fourth intermediate medium in the present invention.
[0036] Figure 9 This is one of the schematic diagrams of the intermediate medium removal process in the fourth embodiment of the present invention.
[0037] Figure 10 This is the second schematic diagram of the intermediate medium removal process in the fourth embodiment of the present invention.
[0038] Figure 11 This is the third schematic diagram of the intermediate medium removal process in the fourth embodiment of the present invention.
[0039] Figure 12 This is a schematic diagram illustrating the construction process of the first groove-shaped filling area and the second hole-shaped filling area in an embodiment of the present invention.
[0040] Figure 13 This is a schematic diagram of the dielectric layer structure in an embodiment of the present invention.
[0041] Figure 14 This is a schematic diagram of the core steps in the self-aligned contact SCA process in related technologies.
[0042] Figure 15 This is a flowchart illustrating an embodiment of the method of the present invention. Figure 1 .
[0043] Figure 16 This is a flowchart illustrating an embodiment of the method of the present invention. Figure 2 .
[0044] in: 010 - Word Line (WL); 020 - Bit Line (BL); 030-Source Strap (SS); 033 - Feature size; 040 - Self-Aligned Source (SAS) CT (ConTact); 050 - Diffusion source; 060 - Isolation Zone; 070-Missing Contact Drain CT (ConTact); 080-Source-Rail; 100 - First-in-class process; 101 - One of the first-in-class manufacturing processes; 103 - First-in-class process three; 110 - Related SAC structure word lines; 120-bit lines of the relevant SAC structure; 130-Related SAC structure source contact SCT (Source Contact). 133 - Feature dimensions of the relevant SCA structure; 150-Related SCA structure diffusion region; 160 - Isolation region related to the SCA structure; 170-Related SCA structure leak contact DCT; 188 - Bridging caused by top chamfering due to load effect; 199 - Trench etching halted due to load effect; 300 - Construction steps for the third slot; 301 - One of the construction steps for the third slot hole; 303 - The third step in constructing the third slot; 305 - Fifth step in constructing the third slot; 307 - The seventh step in constructing the third slot; 309 - The ninth step in constructing the third slot; 500 - Fifth in the post-process; 501 - One of the fifth post-processing steps; 610 - First groove-shaped area; 620 - Second aperture region; 810 - First basal layer; 811 - First dielectric layer; 812 - Second dielectric layer; 813 - Third dielectric layer; 814 - Fourth dielectric layer; 815 - Fifth dielectric layer; 816 - Sixth dielectric layer; 817 - Seventh interlayer medium; 820-Shallow Trench Isolation Structure (STI); 830 - Photoresist layer; 840 - Fourth Intermediate Medium; 850 - Fifth Stop Line; 860 - Sixth Stop Line; 870 - Seventh Stop Line; 871 - First trough-shaped unfilled area; 872 - Second hole type unfilled area; 880-Side wall; 881 - First tank bottom medium layer; 882 - Second hole bottom medium layer; 901 - First section line Y1; 902 - Second section line Y2; 910 - Example word line; 920 - Example bit line; 930 - Example Source Contact; 933 - Feature dimensions of the embodiment; 940 - Example: Missing Contact; 950 - Example of diffusion region; 960 - Example Implementation Isolation Area; 970 - Example Source Contact. Implementation
[0045] The present invention will be further described in detail below with reference to the accompanying drawings and embodiments. Of course, the specific embodiments described below are merely illustrative of the technical solutions of the present invention, and not intended to limit the invention. Furthermore, the parts described in the embodiments or drawings are merely illustrative examples of relevant parts of the present invention, and not the entirety of the invention.
[0046] like Figure 15The self-aligned contact area processing method shown includes a third slot construction step 300; this third slot construction step 300 is located between a first prior process 100 and a fifth subsequent process 500; wherein, the first prior process 100 forms a self-aligned contact SAC structure as shown in the figure. Figure 6 The first groove-shaped region 110 and the second hole-shaped region 120 shown have a shallow trench isolation structure 820 constructed between the first base layer 810 and the first dielectric layer 811 where the first groove-shaped region 110 is located.
[0047] Furthermore, in the third trench construction step 300, the seventh interlayer dielectric 817 is defined and removed in the first trench region 110 according to the preset pattern of the shallow trench isolation structure (STI) projected or mapped on the wafer; and in the fifth post-processing step 500, a preset contact structure is formed in the first trench region 110 and the second hole region 120 respectively using a self-aligned contact (SAC) structure.
[0048] Among them, such as Figure 6 and Figure 13 As shown, its contact structure is obtained by filling contact metal into the first groove region 110 and the second hole region 120; its contact metal includes tungsten metal; its fifth post-processing 500 includes a first planarization treatment of the contact structure.
[0049] Specifically, its contact structure can be prepared by metal-organic chemical vapor deposition (MOCVD).
[0050] Furthermore, such as Figure 7 , Figure 8 As shown, the third slot construction step 300 can also fill the area where the seventh interlayer medium 817 has been removed with a fourth intermediate medium 840. The filling process of the fourth intermediate medium 840 includes backfilling nitride by atomic layer deposition (ALD).
[0051] Among them, such as Figure 9 , Figure 10 , Figure 11 As shown, the fourth intermediate dielectric 840 is removed through a fourth planarization process with the fifth stop line 850 on the outer surface of the sixth dielectric layer 816 as the boundary. After the fourth planarization process is completed, the fourth intermediate dielectric 840 continues to undergo an intermediate etching step to remove the sixth dielectric layer 816 and remove the fourth intermediate dielectric 840 to the seventh stop line 870 on the side of the fifth dielectric layer 815 away from the first substrate layer 810. The fifth dielectric layer 815 is a capped nitride on the side of the fourth dielectric layer 814 where the control gate CG is located away from its first substrate layer 810.
[0052] Specifically, the intermediate etching step includes a pre-dry etching step and a post-wet etching step; the pre-dry etching step is used to etch the fourth intermediate dielectric 840 to the seventh stop line 870 in the first trench region 110; the post-wet etching step is used to further remove the portion of the sixth dielectric layer 816 that could not be removed by the pre-dry etching step from the current sixth stop line 860 to the seventh stop line 870; the post-wet etching step also removes the dielectric of the sixth dielectric layer 816 in the aperture region of the second aperture region 120 that penetrates the control gate CG, the third dielectric layer 813 and the second dielectric layer 812.
[0053] The second dielectric layer 812 is a floating gate (FG) dielectric layer; the third dielectric layer 813 is an oxygen-nitrogen-oxygen (ONO) dielectric layer.
[0054] Specifically, such as Figure 11 As shown, its sixth dielectric layer 816 can adopt an interlayer dielectric (ILD) structure, and the material of its sixth dielectric layer 816 can be silicon oxide; its contact structure also includes a sidewall spacer, a first trench bottom dielectric layer 881 and a second hole bottom dielectric layer 882 constructed concurrently with its fifth dielectric layer 815.
[0055] The first trench bottom dielectric layer 881 and the second hole bottom dielectric layer 882 can be removed by the ninth dry etching process to open the first substrate layer 810 and penetrate the first dielectric layer 811; the first dielectric layer 811 includes a gate oxide layer; after the ninth dry etching process is completed, the first trench-shaped unfilled area 871 and the second hole-shaped unfilled area 872 in its contact structure are obtained.
[0056] Accordingly, such as Figure 6 , Figure 13 The trench structure shown includes a first trench region 110 and a second aperture region 120 formed by a self-aligned contact SAC structure. The first trench region 110 has a shallow trench isolation structure 820 constructed between the first substrate layer 810 and the first dielectric layer 811. The first trench region 110 defines and removes the seventh interlayer dielectric 817 according to a preset pattern projected or mapped on the wafer by the shallow trench isolation structure 820. The first trench region 110 and the second aperture region 120 are respectively used to fill preset metals to form preset contact structures.
[0057] The contact structure can be obtained by filling the first groove region 110 and the second hole region 120 with contact metal; the contact metal includes tungsten.
[0058] Furthermore, the area where the seventh interlayer dielectric 817 has been removed can be filled with a fourth intermediate dielectric 840; the fourth intermediate dielectric 840 is removed by a fourth planarization process with the fifth stop line 850 on the outer surface of the sixth dielectric layer 816 as the boundary; after the fourth planarization process is completed, the fourth intermediate dielectric 840 continues to undergo an intermediate etching step to remove the sixth dielectric layer 816 and remove the fourth intermediate dielectric 840 to the seventh stop line 870 on the side of the fifth dielectric layer 815 away from the first substrate layer 810, and the fifth dielectric layer 815 is a capped nitride on the side of the fourth dielectric layer 814 where the control gate CG is located away from its first substrate layer 810.
[0059] in, Figure 8 , Figure 9 , Figure 10 , Figure 11 As shown, the fourth intermediate dielectric 840 located in the first trench region 110 is etched to the seventh stop line 870, and the sixth dielectric layer 816 is removed from the current sixth stop line 860 to the seventh stop line 870; the sixth dielectric layer 816 dielectric used to penetrate the aperture region of the control gate CG, the third dielectric layer 813 and the second dielectric layer 812 is also removed.
[0060] Specifically, its second dielectric layer 812 is a Float Gate (FG) dielectric layer; its third dielectric layer 813 is an Oxygen-Nitrogen-Oxygen (ONO) dielectric layer.
[0061] The sixth dielectric layer 816 adopts an interlayer dielectric (ILD) structure and is made of silicon oxide. Its contact structure also includes a sidewall spacer, a first trench bottom dielectric layer 881, and a second hole bottom dielectric layer 882, which are constructed concurrently with the fifth dielectric layer 815.
[0062] Furthermore, such as Figure 11 As shown, the first trench bottom dielectric layer 881 and the second via bottom dielectric layer 882 are removed by a ninth dry etching process to open the first substrate layer 810 and penetrate the first dielectric layer 811; the first dielectric layer 811 includes a gate oxide layer; its contact structure includes a first trench-shaped unfilled area 871 and a second via-shaped unfilled area 872.
[0063] Accordingly, such as Figure 6 , Figure 13 As shown, its chip embodiment includes a slot structure as described above; its first slot region 110 is used to form the drain structure of the chip, and the second hole region is used to form the source structure of the chip.
[0064] It should be noted that the above embodiments are only for more clearly illustrating the technical solution of the present invention. Those skilled in the art will understand that the implementation of the present invention is not limited to the above content. Any obvious changes, substitutions or replacements made based on the above content do not exceed the scope of the technical solution of the present invention. Other implementations will also fall within the scope of the present invention without departing from the concept of the present invention.
Claims
1. A method for processing a self-aligned contact area, characterized in that... The process includes a third via construction step (300); the third via construction step (300) is located between a first prior process (100) and a fifth subsequent process (500); wherein, the first prior process (100) forms a first trench region (610) and a second via region (620) with a self-aligned contact structure, and the first trench region (610) has a shallow trench isolation structure (820) constructed between the first substrate layer (810) and the first dielectric layer (811) thereon; the third via construction step (300) defines a seventh interlayer dielectric (817) in the first trench region (610) according to a preset pattern of the shallow trench isolation structure (820) projected or mapped on the wafer and removes it; the fifth subsequent process (500) forms preset contact structures in the first trench region (610) and the second via region (620) respectively with a self-aligned contact SAC structure. The contact structure was prepared by organometallic chemical vapor deposition. The third slot construction step (300) also fills the area where the seventh interlayer medium (817) has been removed with a fourth intermediate medium (840), the filling process of which includes backfilling nitride by atomic layer deposition.
2. The self-aligned contact area processing method as described in claim 1, wherein: The contact structure is obtained by filling contact metal into the first groove region (610) and the second hole region (620); the contact metal includes tungsten; the fifth post-processing step (500) includes a first planarization process on the contact structure.
3. The self-aligned contact area processing method as described in claim 1, wherein: The fourth intermediate medium (840) is removed by a fourth planarization process with the fifth stop line (850) on the outer surface of the sixth dielectric layer (816) as the boundary. After the fourth planarization process is completed, the fourth intermediate medium (840) continues to undergo an intermediate etching step to remove the sixth dielectric layer (816) and remove the fourth intermediate medium (840) to the seventh stop line (870) on the side of the fifth dielectric layer (815) away from the first substrate layer (810). The fifth dielectric layer (815) is a pre-defined end-capping nitride on the side of the fourth dielectric layer (814) where the control gate is located away from the first substrate layer (810).
4. The self-aligned contact area processing method as described in claim 3, wherein: The intermediate etching step includes a pre-dry etching step and a post-wet etching step; the pre-dry etching step is used to etch the portion of the fourth intermediate dielectric (840) located in the first trench region (610) to the seventh stop line (870); the post-wet etching step is used to further remove the portion of the sixth dielectric layer (816) that was not removed by the pre-dry etching step from the current sixth stop line (860) to the seventh stop line (870); the post-wet etching step also removes the dielectric of the sixth dielectric layer (816) that penetrates the control gate, the third dielectric layer (813) and the second dielectric layer (812) through the aperture region of the second aperture region (620).
5. The self-aligned contact area processing method as described in claim 4, wherein: The second dielectric layer (812) is a floating gate dielectric layer; the third dielectric layer (813) is an oxygen-nitrogen-oxygen dielectric layer.
6. The self-aligned contact area processing method as described in claim 3, wherein: The sixth dielectric layer (816) is an interlayer dielectric structure, and the material of the sixth dielectric layer (816) includes silicon oxide; the contact structure also includes sidewalls, a first trench bottom dielectric layer (881) and a second hole bottom dielectric layer (882) constructed concurrently with the fifth dielectric layer (815).
7. The self-aligned contact area processing method as described in claim 6, wherein: The first trench bottom dielectric layer (881) and the second hole bottom dielectric layer (882) are removed by a ninth dry etching process to open the first substrate layer (810) and penetrate the first dielectric layer (811); the first dielectric layer (811) includes a gate oxide layer; after the ninth dry etching process is completed, the first trench-shaped unfilled area (871) and the second hole-shaped unfilled area (872) in the contact structure are obtained.
8. A slot structure comprising a first slot region (610) and a second hole region (620) formed by a self-aligned contact structure, wherein the first slot region (610) has a shallow trench isolation structure (820) between a first substrate layer (810) and a first dielectric layer (811) thereon; the first slot region (610) defines a seventh interlayer dielectric (817) by projecting or mapping a predetermined pattern on the wafer according to the shallow trench isolation structure (820) and removes it; the first slot region (610) and the second hole region (620) are respectively used to fill a predetermined metal to form a predetermined contact structure; The area where the seventh interlayer medium (817) has been removed is filled with the fourth intermediate medium (840). The fourth intermediate medium (840) is removed by a fourth planarization process with the fifth stop line (850) on the outer surface of the sixth dielectric layer (816) as the boundary. After the fourth planarization process is completed, the fourth intermediate medium (840) continues to undergo an intermediate etching step to remove the sixth dielectric layer (816) and remove the fourth intermediate medium (840) to the seventh stop line (870) on the side of the fifth dielectric layer (815) away from the first substrate layer (810). The fifth dielectric layer (815) is a pre-defined end-capping nitride on the side of the fourth dielectric layer (814) where the control gate is located away from the first substrate layer (810).
9. The slot structure as described in claim 8, wherein: The contact structure is obtained by filling contact metal into the first groove region (610) and the second hole region (620); the contact metal includes tungsten.
10. The slot structure as described in claim 8, wherein: The fourth intermediate medium (840) located in the first trench region (610) is etched to the seventh stop line (870), and the sixth dielectric layer (816) is removed from the current sixth stop line (860) to the seventh stop line (870); the dielectric of the sixth dielectric layer (816) used to penetrate the aperture region of the control gate, the third dielectric layer (813) and the second dielectric layer (812) is also removed.
11. The slot structure as described in claim 10, wherein: The second dielectric layer (812) is a floating gate dielectric layer; the third dielectric layer (813) is an oxygen-nitrogen-oxygen dielectric layer.
12. The slot structure as described in claim 8, wherein: The sixth dielectric layer (816) is an interlayer dielectric structure, and the material of the sixth dielectric layer (816) includes silicon oxide; the contact structure also includes sidewalls, a first trench bottom dielectric layer (881) and a second hole bottom dielectric layer (882) constructed concurrently with the fifth dielectric layer (815).
13. The slot structure as described in claim 12, wherein: The first trench bottom dielectric layer (881) and the second hole bottom dielectric layer (882) are removed by a ninth dry etching process to open the first substrate layer (810) and penetrate the first dielectric layer (811); the first dielectric layer (811) includes a gate oxide layer; the contact structure includes a first trench-shaped unfilled area (871) and a second hole-shaped unfilled area (872).
14. A chip comprising a slot structure as described in any one of claims 8 to 13, wherein a first slot region (610) is used to form a drain structure of the chip, and a second slot region is used to form a source structure of the chip.
Citation Information
Patent Citations
Manufacturing method of semiconductor device
CN104347485A