Sputtering method, sputtering cathode device and sputtering equipment for improving target material utilization
By dividing the target etching track and dynamically adjusting the magnetic field intensity in vacuum magnetron sputtering coating technology, the problem of uneven target etching is solved, the target utilization rate and product yield are improved, and the increase of anode components is avoided. .
Patent Information
- Application Number
- CN202311133407.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-09-05
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2043-09-05
AI Technical Summary
In the existing vacuum magnetron sputtering coating technology, the target is prone to unevenness during the etching process, resulting in low target utilization and inflexible adjustment of the anode assembly, which increases costs and may damage the coated substrate.
By dividing the etching track on the target surface into a plasma-enhanced side track and a non-enhanced side track, the magnetic field intensity is adjusted according to the film thickness distribution of the coated substrate, and the magnetic field intensity is weakened or enhanced to achieve uniform etching of the target. The adjusting component is used to dynamically adjust the magnetic field intensity, avoiding the need for additional anode components.
It improves the utilization rate of the target material, reduces the cost, improves the product yield, achieves uniform etching of the target material, and eliminates the need for additional anode components.
Smart Images

Figure CN116855909B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of vacuum sputtering coating, and in particular to a sputtering method, a sputtering cathode device and a sputtering equipment for improving the utilization rate of a target material. Background Art
[0002] Vacuum magnetron sputtering coating is a common coating method. Vacuum magnetron sputtering coating refers to a coating technology that uses the coating material as the target cathode, bombards the target material with argon ions, produces cathode sputtering, and sputters the target material atoms onto the coating substrate to form a deposited layer.
[0003] In the prior art, the cathode device for magnetron sputtering coating usually includes a target material and a magnetron component. The magnetron component is arranged inside the target material. When the target material rotates in a vacuum chamber, it is sputtered under the combined action of the magnetic field and the electric field inside it to achieve coating of the coated substrate. Since the target material is often etched unevenly during the etching process, the utilization rate of the target material is greatly reduced. Some existing means generally add an anode component at a suitable position in the vacuum chamber to optimize the distribution of the electric field and magnetic field on the surface of the target material so that the target material is uniformly etched. However, the adjustment of the anode component is not flexible and cannot be well adapted to different cathode layouts, and a certain thickness of film layer will also be deposited on the surface of the anode component, resulting in a waste of target material, increasing costs, and there is a high probability that the film layer on the surface of the anode component will peel off after accumulating more, and falling on the coated substrate is easy to damage the coated substrate, reducing the product yield.
[0004] Therefore, there is an urgent need for a sputtering method, a sputtering cathode device and a sputtering equipment that can improve the utilization rate of the target material to solve the above problems. Summary of the invention
[0005] The object of the present invention is to provide a sputtering method, a sputtering cathode device and a sputtering equipment for improving the utilization rate of target materials, so that the target materials are uniformly etched, the utilization rate of the target materials is improved, and there is no need to add additional anode components, thereby reducing costs and improving product yield.
[0006] To achieve this object, the present invention adopts the following technical solutions:
[0007] A sputtering method for improving target material utilization, dividing a linear area of an etching track on the surface of the target material into a first side track and a second side track arranged relatively, the sputtering method for improving target material utilization comprising the following steps:
[0008] S1: Obtaining the film thickness distribution of the coating substrate on which the target material is coated;
[0009] S2: judging which of the first side track and the second side track is a plasma enhanced side track and which is a plasma non-enhanced side track according to the film thickness distribution of the coated substrate;
[0010] S3: Weakening the magnetic field strength of the plasma enhanced side runway as a whole.
[0011] As a preferred solution, the sputtering method for improving target utilization rate further comprises, after step S3:
[0012] S4: Weaken the magnetic field strength of the first side runway and the second side runway, and the weakening amount of the magnetic field strength gradually decreases along the direction of the drift current on the etched runway; or, strengthen the magnetic field strength of the first side runway and the second side runway, and the strengthening amount of the magnetic field strength gradually decreases along the opposite direction of the drift current on the etched runway.
[0013] As a preferred solution, the sputtering method for improving target utilization rate further comprises, after step S4:
[0014] After the coating process is completed, the morphology information of the target material in the vacuum chamber is obtained, and when the morphology information of the target material meets the preset requirements, the adjustment is stopped;
[0015] When the morphology information of the target material does not meet the preset requirements, step S3 or steps S3 to S4 are repeated.
[0016] As a preferred solution, obtaining the morphology information of the target material in the vacuum chamber includes:
[0017] The radial dimensions of a plurality of collection points arranged along the axial direction on the target are obtained.
[0018] As a preferred embodiment, it is characterized in that when a plurality of target materials are arranged at intervals in the vacuum chamber, the plasma enhanced side track and the plasma non-enhanced side track on each target material are judged in turn, and the magnetic field strength of the etching track on the surface of each target material is adjusted in step S3 or steps S3 to S4 in turn.
[0019] A sputtering cathode device, which uses the sputtering method for improving the utilization rate of the target material as described above to adjust the magnetic field strength at each position of the etching track on the surface of the target material, and the sputtering cathode device includes:
[0020] A target material, wherein the target material is rotatably disposed in a vacuum chamber;
[0021] A magnetron assembly is disposed inside the target material; and
[0022] An adjustment component is configured to adjust the magnetic field strength at various positions of the etching track on the surface of the target material according to the film thickness distribution of the coated substrate.
[0023] As a preferred solution, the magnetron assembly includes a first magnetic yoke, a first magnet array, a second magnetic yoke and a second magnet array, the first magnetic yoke and the second magnetic yoke are both arranged in the target material, the first magnet array is arranged on the first magnetic yoke, the second magnet array is arranged on the second magnetic yoke, the first magnet array and the second magnet array are arranged adjacent to each other, and the first magnet array and the second magnet array both extend along the axial direction of the target material;
[0024] The adjustment component includes a first adjustment member and a second adjustment member, the first adjustment member is configured to adjust the distance between each position in the extension direction of the first magnet array and the target material, and the second adjustment member is configured to adjust the distance between each position in the extension direction of the second magnet array and the target material.
[0025] As a preferred embodiment, the first adjusting member includes a plurality of first adjusting components arranged at intervals along the axial direction of the target material, the output end of the first adjusting component is connected to the first magnetic yoke, and the output end of the first adjusting component can reciprocate along the radial direction of the target material to drive the first magnetic yoke connected to the output end of the first adjusting component to approach or move away from the target material; the second adjusting member includes a plurality of second adjusting components arranged at intervals along the axial direction of the target material, the output end of the second adjusting component is connected to the second magnetic yoke, and the output end of the second adjusting component can reciprocate along the radial direction of the target material to drive the second magnetic yoke connected to the output end of the second adjusting component to approach or move away from the target material.
[0026] As a preferred solution, the magnetron assembly further includes a cooling pipe, the first magnetic yoke and the second magnetic yoke are both located on one side of the cooling pipe, the first adjustment component is a first adjustment bolt, the first adjustment bolt is threadedly connected to the cooling pipe, and the first adjustment bolt is screwed through the cooling pipe to be connected to the first magnetic yoke;
[0027] The second adjusting component is a second adjusting bolt, the second adjusting bolt is threadedly connected to the cooling pipe, and the second adjusting bolt is screwed through the cooling pipe to be connected to the second magnetic yoke.
[0028] The sputtering equipment comprises a vacuum chamber, a film-coated substrate and the sputtering cathode device as described above, wherein the film-coated substrate and the sputtering cathode device are both arranged in the vacuum chamber, and the magnetic lines of force generated by the magnetron assembly promote the atoms sputtered from the target material to be deposited on the film-coated substrate.
[0029] Beneficial effects of the present invention:
[0030] The present invention provides a sputtering method for improving the utilization rate of a target material. The method divides a linear area of an etching track on the surface of the target material into a first side track and a second side track which are arranged relatively, obtains the film thickness distribution of a coated substrate, and judges which of the first side track and the second side track is a plasma enhanced side track and which is a plasma non-enhanced side track according to the film thickness distribution of the coated substrate, and weakens the magnetic field intensity of the plasma enhanced side track as a whole, thereby weakening the influence of the enhancement effect on the plasma density on the first side track or the second side track, so that the target material is uniformly etched, and the utilization rate of the target material is improved. In addition, there is no need to additionally provide an anode assembly, thereby reducing the cost and improving the product yield.
[0031] The present invention also provides a sputtering cathode device, which, by applying the above-mentioned sputtering method for improving target material utilization, allows the target material to be uniformly etched, thereby improving the utilization of the target material, and eliminating the need for additional anode components, thereby reducing costs and improving product yield.
[0032] The present invention also provides a sputtering device, which uses the above-mentioned sputtering cathode device to uniformly etch the target material, thereby improving the utilization rate of the target material and eliminating the need for additional anode components, thereby reducing costs and improving product yield. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] Figure 1 It is a schematic diagram of the structure of forming an etching track on the surface of a target material provided in the first embodiment of the present invention;
[0034] Figure 2 is the fitting of the etching speed in the axial direction of the target surface provided by the first embodiment of the present invention Figure 1 ;
[0035] Figure 3 is the fitting of the etching speed in the axial direction of the target surface provided by the first embodiment of the present invention Figure 2 ;
[0036] Figure 4 is a flow chart of a sputtering method for improving target material utilization provided by Embodiment 1 of the present invention;
[0037] Figure 5 The film thickness distribution of the coated substrate after coating provided by the first embodiment of the present invention is fitted Figure 1 ;
[0038] Figure 6 The film thickness distribution of the coated substrate after coating provided by the first embodiment of the present invention is fitted Figure 2 ;
[0039] Figure 7is a schematic structural diagram of the sputtering cathode device provided in the second embodiment of the present invention after the target material is removed;
[0040] Figure 8 It is a structural cross-sectional view of the sputtering cathode device provided in the second embodiment of the present invention after the target material is removed.
[0041] In the figure:
[0042] 200, etching runway; 210, first side runway; 220, second side runway;
[0043] 1. Target material;
[0044] 2. Magnetron assembly; 21. First magnetic yoke; 22. First magnet array; 23. Second magnetic yoke; 24. Second magnet array; 25. Cooling pipe;
[0045] 3. Adjustment assembly; 31. First adjustment member; 311. First adjustment component; 32. Second adjustment member; 321. Second adjustment component. DETAILED DESCRIPTION
[0046] In order to make the technical problem solved by the present invention, the technical solution adopted and the technical effect achieved more clearly, the technical solution of the present invention is further explained below with reference to the accompanying drawings and through specific implementation methods.
[0047] In the description of the present invention, unless otherwise clearly specified and limited, the terms "connected", "connected", and "fixed" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0048] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.
[0049] In the description of this embodiment, the terms "upper", "lower", "left", "right" and other directions or positional relationships are based on the directions or positional relationships shown in the drawings, and are only for the convenience of description and simplification of operation, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operate in a specific direction, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are only used to distinguish in the description and have no special meaning. Embodiment 1
[0050] In the actual application process of vacuum magnetron sputtering coating, for example, in a single-target application scenario, the target material is easily affected by the enhancement effect of the vacuum chamber (grounded anode), resulting in uneven target etching. In a dual-target application scenario, the target material is easily affected by the enhancement effect of the adjacent target material and the magnetic field enhancement effect of the vacuum chamber, resulting in uneven target etching.
[0051] like Figure 1 As shown, during the vacuum magnetron sputtering coating process, when the target material 1 rotates in the vacuum chamber, an etching track 200 is formed on the surface of the target material 1 under the combined action of the magnetic field and the electric field therein, and the etching track 200 extends along the axial direction of the target material 1 (i.e., extending from the end side of the target material 1 to the support side of the target material 1), and the linear area of the etching track 200 can be divided into a first side track 210 and a second side track 220 arranged relatively, and on the etching track 200, the drift current circulates along the etching track 200. On the etching track 200, the drift current is set to flow from the end side of the target material 1 to the support side of the target material 1 as the first side track 210, and the drift current is set to flow from the support side of the target material 1 to the end side of the target material 1 as the second side track 220. It should be noted that the greater the plasma density of the area on the etching track 200, the faster the etching speed of the corresponding area position of the target material 1.
[0052] like Figure 2 As shown, through experimental verification and analysis, there is an uneven phenomenon that the plasma density gradually weakens along the direction of the drift current on the etching track 200, and if one side of the etching track 200 ( Figure 2 Taking the second side track 220 as an example), the plasma density on the track will be enhanced due to the strong enhancement effect of the adjacent target material 1 or the outer anode. Due to the existence of the drift current phenomenon, the plasma in the enhanced area will be preferentially pulled to the area with stronger plasma density, which will lead to the inhomogeneity in the direction of the drift current being enhanced. Figure 2Even though the first side track 210 shown in the figure is also affected by the enhancement effect of the adjacent target material 1 or the outer anode, its enhancement effect is relatively weak compared with the stronger enhancement effect. The etching of the rotating target material 1 is the sum of the etching amounts of the first side track 210 and the second side track 220. When the etching results of both sides are superimposed, the etching of both ends of the target material 1 in the axial direction is uneven. Figure 2 In the ideal non-enhancement condition, the sum of the first side track 210 and the second side track 220 is relatively uniform along the axial direction of the target. Under the influence of the actual enhancement effect, the target 1 is often etched unevenly during the etching process, which greatly reduces the utilization rate of the target 1. In addition, if the first side track 210 is affected by the strong enhancement effect of the adjacent target 1 or the outer anode, the target 1 will be etched unevenly. Figure 3 In order to solve the above problems, Figure 4 As shown, this embodiment provides a sputtering method for improving target material utilization, dividing the linear area of the etching track 200 on the surface of the target material 1 into a first side track 210 and a second side track 220 arranged relatively, and the sputtering method for improving target material utilization includes the following steps:
[0053] S1: Obtaining the film thickness distribution of the coating substrate coated with the corresponding target material 1;
[0054] S2: judging which of the first side track 210 and the second side track 220 is a plasma enhanced side track and which is a plasma non-enhanced side track according to the film thickness distribution of the film-coated substrate;
[0055] S3: Weaken the overall magnetic field strength of the plasma enhanced side runway.
[0056] Here, it should be stated that the fact that one side of the runway is a plasma non-enhanced side runway does not mean that this side runway has no plasma enhancement. In the vacuum chamber, this plasma non-enhanced side runway is also affected by the enhancement effect of the vacuum chamber (grounded anode) and / or the adjacent target material. It is just that compared with the side runway with high plasma enhancement intensity, its plasma enhancement intensity is relatively weak, and thus the effect of this side runway on the etching uniformity of the target material is also relatively weak.
[0057] The sputtering method for improving the utilization rate of the target material provided in this embodiment weakens the magnetic field strength of the plasma enhanced side runway as a whole, thereby weakening the influence of the enhancement effect on the plasma density on the first side runway 210 or the second side runway 220, so that the target material 1 is uniformly etched, thereby improving the utilization rate of the target material 1. In addition, this method does not require the addition of an additional anode assembly, thereby reducing costs and improving product yield.
[0058] It should be noted that the greater the plasma density in a certain area on the etching track 200 on the target material 1, the faster the etching speed of the target material 1 corresponding to the area. Correspondingly, the film layer of the coated substrate in the area of the target material 1 with a fast etching speed is relatively thicker, resulting in an uneven film layer of the coated substrate. Therefore, by obtaining the film thickness distribution of the coated substrate and the known flow direction of the drift current, it can be determined which of the first side track 210 and the second side track 220 is the plasma enhanced side track and which is the plasma non-enhanced side track. In addition, the magnetic field strength on the etching track 200 can be adjusted more accurately by the film thickness distribution of the coated substrate, and the magnetic field strength can be adjusted earlier and faster without waiting for the etching morphology of the target material 1 to be formed before adjustment, which is more proactive.
[0059] Preferably, in this embodiment, due to the phenomenon of uneven distribution of plasma in the direction of drift current, even without the enhancement effect, there is a certain degree of uneven phenomenon that the etching amount on both sides of the target is greater than that in the middle. The sputtering method for improving the utilization rate of the target further includes, after step S3:
[0060] S4: Weaken the magnetic field strength of the first side track 210 and the second side track 220, and the weakening amount of the magnetic field strength gradually decreases along the direction of the drift current on the etching track 200; or, strengthen the magnetic field strength of the first side track 210 and the second side track 220, and the strengthening amount of the magnetic field strength gradually decreases along the opposite direction of the drift current on the etching track 200.
[0061] The above adjustment method ensures the uniformity of plasma density at each position on the etching track 200, and further ensures that the target material 1 is etched uniformly.
[0062] Preferably, in this embodiment, if Figure 4 As shown, the sputtering method for improving target material utilization rate further includes, after step S4:
[0063] After the coating process is completed, the morphology information of the target material 1 in the vacuum chamber is obtained, and when the morphology information of the target material 1 meets the preset requirements, the adjustment is stopped;
[0064] When the morphology information of the target material 1 does not meet the preset requirements, steps S3 to S4 are repeated.
[0065] The above design ensures that the intensity of the magnetic field at each position on the etching track 200 is gradually revised and adjusted according to the morphology of the target material 1 being etched, until the target material 1 is uniformly etched.
[0066] It should be noted that, in other embodiments, when the morphology information of the target material 1 does not meet the preset requirements, only step S3 may be repeated.
[0067] It should be noted that obtaining the morphological information of the target material 1 in the vacuum chamber includes:
[0068] The radial dimensions of a plurality of collection points arranged along the axial direction on the target material 1 are obtained, that is, the diameter of the target material 1 at each collection point is obtained.
[0069] For example, for a single target vacuum chamber, Figure 5 As shown in Figure 2, when the film thickness distribution of the coated substrate is as follows Figure 5 As shown in FIG. 1 , that is, the film layer at the position where the coated substrate is opposite to the end side of the target material 1 is thicker, which means that the etching speed at the end side of the target material 1 is faster. It can be seen that the distribution trend of the film thickness of the coated substrate is consistent with the flow direction of the drift current of the first side track 210. It can be inferred that the first side track 210 is the plasma enhanced side track, and the second side track 220 is the plasma non-enhanced side track. When the film thickness distribution of the coated substrate is as shown in FIG. Figure 6 As shown, that is, the film layer at the position relative to the support side of the coated substrate and the target 1 is thicker, which means that the etching speed of the support side of the target 1 is faster. It can be seen that the distribution trend of the film thickness of the coated substrate is consistent with the drift current distribution of the second side runway 220. It can be inferred that the second side runway 220 is a plasma enhanced side runway, and the first side runway 210 is a plasma non-enhanced side runway.
[0070] It should be noted that when a plurality of target materials 1 are arranged at intervals in the vacuum chamber, the plasma enhanced side track and the plasma non-enhanced side track on each target material 1 are determined in turn, and the magnetic field strength of the etching track 200 on the surface of each target material 1 is adjusted in turn in step S3 or steps S3 to S4. Specifically, when the plasma enhanced side track and the plasma non-enhanced side track of the etching track 200 on one of the target materials 1 are analyzed, the power of the remaining target materials 1 can be reduced to 1 / 10 or less of the power of the target material 1 to be analyzed, so that the film thickness distribution of the coated substrate is mainly caused by the sputtering of the target material 1 to be analyzed, so that the plasma enhanced side track and the plasma non-enhanced side track on the target material 1 can be obtained more accurately. It should be noted that when one of the target materials 1 is analyzed, the power of the remaining target materials 1 is only 1 / 10 or less of the target material 1 to be analyzed. The film thickness contributed by the remaining target materials 1 has little effect on the film thickness distribution of the target material 1 to be analyzed, but can produce a plasma enhancement effect on the target material 1 to be analyzed. Therefore, this method can actually analyze the actual etching distribution of the target material 1 to be analyzed. Embodiment 2
[0071] like Figure 7 As shown, this embodiment also provides a sputtering cathode device, which uses the above-mentioned sputtering method for improving the utilization rate of the target material to adjust the magnetic field strength at each position of the etching track 200 on the surface of the target material 1. The sputtering cathode device provided in this embodiment includes a target material 1 ( Figure 7 ), a magnetron assembly 2 and an adjustment assembly 3, wherein the target 1 is rotatably arranged in the vacuum chamber, the magnetron assembly 2 is arranged inside the target 1, and the adjustment assembly 3 is used to adjust the magnetic field strength at each position of the etching track 200 on the surface of the target 1 according to the film thickness distribution of the coated substrate. The sputtering cathode device provided in this embodiment uses the above-mentioned sputtering method for improving the utilization rate of the target material, so that the target material 1 is uniformly etched, the utilization rate of the target material 1 is improved, and there is no need to add an additional anode assembly, which reduces the cost and improves the product yield.
[0072] Specifically, if Figure 7 and Figure 8 As shown, the magnetron assembly 2 includes a first magnetic yoke 21, a first magnet array 22, a second magnetic yoke 23 and a second magnet array 24. The first magnetic yoke 21 and the second magnetic yoke 23 are both arranged in the target material 1. The first magnet array 22 is arranged on the first magnetic yoke 21, and the second magnet array 24 is arranged on the second magnetic yoke 23. The first magnet array 22 and the second magnet array 24 are arranged adjacent to each other. The adjustment assembly 3 includes a first adjustment member 31 and a second adjustment member 32. The first adjustment member 31 is used to adjust the distance between each position in the extension direction of the first magnet array 22 and the target material 1, and the second adjustment member 32 is used to adjust the distance between each position in the extension direction of the second magnet array 24 and the target material 1.
[0073] In this embodiment, if Figure 7 and Figure 8As shown, the first adjusting member 31 includes a plurality of first adjusting components 311 arranged at intervals along the axial direction of the target material 1, the output end of the first adjusting component 311 is connected to the first magnetic yoke 21, and the output end of the first adjusting component 311 can reciprocate radially along the target material 1 to drive the first magnetic yoke 21 connected to the output end of the first adjusting component 311 to approach or move away from the target material 1, and the second adjusting member 32 includes a plurality of second adjusting components 321 arranged at intervals along the axial direction of the target material 1, the output end of the second adjusting component 321 is connected to the second magnetic yoke 23, and the output end of the second adjusting component 321 can reciprocate radially along the target material 1 to drive the second magnetic yoke 23 connected to the output end of the second adjusting component 321 to approach or move away from the target material 1. It should be noted that, under the action of the first magnet array 22 and the second magnet array 24, an etching runway 200 is formed on the surface of the target material 1, and the first side runway 210 is arranged relative to one of the first magnet array 22 and the second magnet array 24, and the second side runway 220 is arranged relative to the other of the first magnet array 22 and the second magnet array 24. When it is necessary to weaken the magnetic field strength of the first side runway 210 as a whole, the magnet array relative to the first side runway 210 is adjusted as a whole in a direction away from the target material 1 by adjusting the first adjustment member 31. For example, the magnet array can be moved 1.5 mm in a direction away from the target material 1 to avoid over-adjustment. When it is necessary to increase the magnetic field strength of the first side runway 210 as a whole, the magnet array relative to the first side runway 210 is adjusted as a whole in a direction close to the target material 1 by adjusting the adjustment component 3. For example, the magnet array can be moved 1.5 mm in a direction close to the target material 1 to avoid over-adjustment. In addition, the overall weakening operation and overall strengthening operation of the magnetic field strength of the second side track 220 are consistent with the adjustment method of the first side track 210, and it is only necessary to adjust the distance between the corresponding magnet array and the target material 1.
[0074] In addition, it should be noted that the first magnetic yoke 21 and the second magnetic yoke 23 are both made of soft materials, and the first magnet array 22 is composed of a plurality of independent magnetic blocks arranged in sequence along the axial direction of the target material 1, and the second magnet array 24 is also composed of a plurality of independent magnetic blocks arranged in sequence along the axial direction of the target material 1. When the magnetic field strength of the first side runway 210 and the second side runway 220 is weakened, and the weakening amount of the magnetic field strength gradually decreases along the direction of the drift current on the etching runway 200, the distance between each independent magnetic block in the magnet array corresponding to the runway and the target material 1 is adjusted by the corresponding adjusting member. Similarly, when the magnetic field strength of the first side runway 210 and the second side runway 220 is enhanced, and the enhanced amount of the magnetic field strength gradually decreases along the opposite direction of the drift current on the etching runway 200, the distance between each independent magnetic block in the magnet array corresponding to the runway and the target material 1 is also adjusted by the corresponding adjusting member. It should be noted that as long as the magnetic block corresponding to the magnetic field enhancement is adjusted in the direction close to the target material 1, the magnetic block corresponding to the magnetic field weakening is adjusted in the direction away from the target material 1. Since the magnet array is composed of multiple independent magnetic blocks and the yoke is made of soft material, the reliability of adjusting the distance between each adjustment point in the axial direction of the magnet array and the target 1 is guaranteed. It should be noted that each position where the first adjustment component 311 and the second adjustment component 321 are provided is an adjustment point.
[0075] It should be noted that, in the present embodiment, the magnetron assembly 2 further includes a cooling pipe 25, in which a cooling water channel is provided, and the cooling water channel is used to form a circulating water channel in the target material 1 to cool the magnetron assembly 2 and the target material 1, the first magnetic yoke 21 and the second magnetic yoke 23 are both located on one side of the cooling pipe 25, the first adjustment component 311 is a first adjustment bolt, the first adjustment bolt is threadedly connected to the cooling pipe 25, the first adjustment bolt is screwed through the cooling pipe 25 and connected to the first magnetic yoke 21, and the second adjustment component 321 is a second adjustment bolt, the second adjustment bolt is threadedly connected to the cooling pipe 25, and the second adjustment bolt is screwed through the cooling pipe 25 and connected to the second magnetic yoke 23. By designing the adjustment component in the form of an adjustment bolt, the adjustment of the magnetic block at the corresponding position along the radial direction of the target material 1 can be achieved by manually screwing the adjustment bolt, so that the structure is simple, the cost is low, and the adjustment operation is convenient. It should be noted that, in the present embodiment, since the adjustment needs to be made by manually screwing the adjustment bolt, the vacuum chamber needs to be broken for manual adjustment.
[0076] It should be noted that, in this embodiment, the sputtering cathode device also includes a detection component, which is used to detect the film thickness distribution of the coated substrate so that the operator can obtain the film thickness distribution of the coated substrate. Specifically, the detection component is a sensor or a probe.
[0077] It should be noted that, in other embodiments, the first adjusting component 311 and the second adjusting component 321 can also be designed as a motor screw, and the first adjusting component 311 and the second adjusting component 321 can be arranged in the vacuum chamber, and the first adjusting component 311 and the second adjusting component 321 can be communicatively connected with the detection component, so that the first adjusting component 311 and the second adjusting component 321 can automatically adjust the magnetic block at the corresponding position along the radial direction of the target material 1 according to the detection structure of the detection component, without breaking the vacuum of the vacuum chamber, making the adjustment operation more convenient and more intelligent. Embodiment 3
[0078] The present embodiment further provides a sputtering device, including a vacuum chamber, a film-coated substrate, and the above-mentioned sputtering cathode device, wherein the film-coated substrate and the sputtering cathode device are both arranged in the vacuum chamber, and the magnetic lines of force generated by the magnetron assembly 2 can cause atoms sputtered from the target material 1 to be deposited on the film-coated substrate. The sputtering device provided in the present embodiment, by applying the above-mentioned sputtering cathode device, enables the target material to be uniformly etched, thereby improving the utilization rate of the target material, and does not require an additional anode assembly, thereby reducing costs and improving product yield.
[0079] Obviously, the above embodiments of the present invention are merely examples for clearly illustrating the present invention, and are not intended to limit the embodiments of the present invention. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the embodiments here. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the claims of the present invention.
Claims
1. A sputtering method for improving target material utilization, characterized in that: Applied to a target material (1) affected by a vacuum chamber enhancement effect, a linear region of an etching track (200) on the surface of the target material (1) is divided into a first side track (210) and a second side track (220) arranged relatively to each other, and the sputtering method for improving the utilization rate of the target material comprises the following steps: S1: Obtaining the film thickness distribution of the coating substrate on which the target material (1) is coated; S2: judging which of the first side runway (210) and the second side runway (220) is a plasma enhanced side runway and which is a plasma non-enhanced side runway according to the film thickness distribution of the coated substrate; S3: weakening the magnetic field strength of the plasma enhanced side runway as a whole; The sputtering method for improving target material utilization rate further comprises, after step S3: S4: weakening the magnetic field strength of the first side track (210) and the second side track (220), and the weakening amount of the magnetic field strength gradually decreases along the direction of the drift current on the etched track (200); or strengthening the magnetic field strength of the first side track (210) and the second side track (220), and the strengthening amount of the magnetic field strength gradually decreases along the opposite direction of the drift current on the etched track (200); The sputtering method for improving target material utilization rate further comprises, after step S4: After the coating process is completed, the morphology information of the target material (1) in the vacuum chamber is obtained, and when the morphology information of the target material (1) meets the preset requirements, the adjustment is stopped; When the morphology information of the target material (1) does not meet the preset requirements, step S3 or steps S3 to S4 are repeated.
2. The sputtering method for improving target utilization according to claim 1, characterized in that: Acquiring the morphology information of the target material (1) in the vacuum chamber comprises: The radial dimensions of a plurality of collection points arranged along the axial direction on the target material (1) are obtained.
3. The sputtering method for improving target utilization according to any one of claims 1 to 2, characterized in that: When a plurality of target materials (1) are arranged at intervals in a vacuum chamber, the plasma enhanced side track and the plasma non-enhanced side track on each target material (1) are determined in turn, and the magnetic field strength of the etching track (200) on the surface of each target material (1) is adjusted in step S3 or steps S3 to S4 in turn.
4. A sputtering cathode device, characterized in that The sputtering method for improving target utilization rate according to any one of claims 1 to 3 is used to adjust the magnetic field strength at each position of the etching track (200) on the surface of the target (1), and the sputtering cathode device comprises: A target material (1), wherein the target material (1) is rotatably disposed in a vacuum chamber; A magnetron assembly (2) is arranged inside the target material (1); and An adjustment component (3), the adjustment component (3) being configured to adjust the magnetic field intensity at various positions of the etching track (200) on the surface of the target material (1) according to the film thickness distribution of the coated substrate; The magnetron assembly (2) comprises a first magnetic yoke (21), a first magnet array (22), a second magnetic yoke (23) and a second magnet array (24); the first magnetic yoke (21) and the second magnetic yoke (23) are both arranged in the target material (1); the first magnet array (22) is arranged on the first magnetic yoke (21); the second magnet array (24) is arranged on the second magnetic yoke (23); the first magnet array (22) and the second magnet array (24) are arranged adjacent to each other; and the first magnet array (22) and the second magnet array (24) both extend along the axial direction of the target material (1); The adjustment component (3) comprises a first adjustment member (31) and a second adjustment member (32), wherein the first adjustment member (31) is configured to adjust the distance between each position in the extension direction of the first magnet array (22) and the target material (1), and the second adjustment member (32) is configured to adjust the distance between each position in the extension direction of the second magnet array (24) and the target material (1).
5. The sputtering cathode device according to claim 4, characterized in that: The first adjusting member (31) comprises a plurality of first adjusting members (311) arranged at intervals along the axial direction of the target material (1), the output end of the first adjusting member (311) being connected to the first magnetic yoke (21), and the output end of the first adjusting member (311) being capable of reciprocating along the radial direction of the target material (1) so as to drive the first magnetic yoke (21) connected to the output end of the first adjusting member (311) to approach or move away from the target material (1); the second adjusting member (32) comprises a plurality of second adjusting members (321) arranged at intervals along the axial direction of the target material (1), the output end of the second adjusting member (321) being connected to the second magnetic yoke (23), and the output end of the second adjusting member (321) being capable of reciprocating along the radial direction of the target material (1) so as to drive the second magnetic yoke (23) connected to the output end of the second adjusting member (321) to approach or move away from the target material (1).
6. The sputtering cathode device according to claim 5, characterized in that: The magnetron assembly (2) further comprises a cooling pipe (25), the first magnetic yoke (21) and the second magnetic yoke (23) are both located on one side of the cooling pipe (25), the first adjustment component (311) is a first adjustment bolt, the first adjustment bolt is threadedly connected to the cooling pipe (25), and the first adjustment bolt is screwed through the cooling pipe (25) to be connected to the first magnetic yoke (21); The second adjusting component (321) is a second adjusting bolt, the second adjusting bolt is threadedly connected to the cooling pipe (25), and the second adjusting bolt is screwed through the cooling pipe (25) to be connected to the second magnetic yoke (23).
7. Sputtering equipment, characterized in that It comprises a vacuum chamber, a film-coated substrate and a sputtering cathode device as claimed in any one of claims 4 to 6, wherein the film-coated substrate and the sputtering cathode device are both arranged in the vacuum chamber, and the magnetic lines of force generated by the magnetron component (2) promote the atoms sputtered from the target material (1) to be deposited onto the film-coated substrate.
Citation Information
Cited By
Magnetron sputtering-based adjustment method, sputtering cathode device, and sputtering device
EP4775710A1
Magnetron sputtering-based adjustment method, sputtering cathode device, and sputtering device
WO2025051046A1