A method for enhancing the resolution of super-resolution lithography based on transient illumination.
By optimizing the parameters of each film layer and transient illumination parameters of the superlens, and adjusting the surface plasmon mode dispersion, the problem of insufficient resolution under material loss in traditional photolithography technology has been solved, achieving higher imaging lithography resolution and a larger working distance.
Patent Information
- Application Number
- CN202311030916.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-08-15
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2043-08-15
AI Technical Summary
Traditional photolithography is limited by the optical diffraction limit, making it difficult to significantly enhance photolithographic resolution when there is material loss in the superlens.
A super-resolution lithography method based on transient illumination is adopted. By optimizing the parameters of each film layer of the superlens and the transient illumination parameters, the surface plasmon mode dispersion at the metal-dielectric interface is adjusted, thereby enhancing the imaging lithography resolution.
Under the condition of unchanged lithographic resolution, the working distance between the mask and the wafer is extended, the requirements for face shape and nanometer gap are reduced, it is compatible with existing super-resolution lithography technology, and the imaging lithography resolution is significantly improved.
Smart Images

Figure CN117008427B_ABST
Abstract
Description
Technical Field
[0001] This disclosure relates to the field of semiconductor manufacturing technology, and more specifically to a method for enhancing the resolution of super-resolution lithography based on transient illumination. Background Technology
[0002] In the modern manufacturing process of complex integrated circuits, the first step is to design an integrated circuit mask, and then transfer this pattern onto a wafer using photolithography. Traditional photolithography is limited by the optical diffraction limit, with a resolution only reaching half a wavelength. To improve photolithographic resolution, methods such as reducing the operating wavelength or increasing the numerical aperture are commonly used. Currently, mainstream photolithography systems employ 193 nm deep ultraviolet (DUV) wavelength light sources and 13.5 nm extreme ultraviolet (EUV) wavelength light sources. Super-resolution photolithography based on surface plasmon resonance can overcome the optical diffraction limit, achieving finer photolithographic resolution without shortening the exposure light source wavelength, and is therefore considered a feasible solution for advanced photolithography technology.
[0003] Super-resolution lithography based on surface plasmons relies on superlenses. Under ideal conditions of matched optical constants and no loss, the imaging resolution of a superlens has no limit. However, the inherent losses in the metal thin films that make up the superlens limit the actual imaging resolution. Previously, researchers attempted to compensate for the effects of material losses using gain media, but this method is difficult to apply in the field of micro- and nano-lithography.
[0004] Therefore, those skilled in the art urgently need a super-resolution lithography method that has a high tolerance for material loss in superlenses, and that can significantly enhance lithographic resolution even when there is material loss in the superlenses. Summary of the Invention
[0005] (a) Technical problems to be solved
[0006] To address the aforementioned issues, this disclosure provides a super-resolution lithography enhancement method based on transient illumination, which solves the technical problem that traditional methods struggle to significantly enhance lithography resolution under conditions of material loss in superlenses.
[0007] (II) Technical Solution
[0008] This disclosure provides a method for enhancing the resolution of super-resolution lithography based on transient illumination, comprising: S1, optimizing the design of the light source wavelength and parameters of each layer of the superlens under steady-state illumination according to mask parameters, wherein the parameters of each layer of the superlens include at least material parameters and structural parameters; S2, performing imaging light field simulation under transient illumination based on the parameters of each layer of the superlens to obtain the transient illumination parameters corresponding to the maximum total light field energy ratio when the photoresist center reaches the imaging contrast requirement under the target resolution, and confirming the corresponding exposure time period; S3, fine-tuning the structural parameters of each layer of the superlens under transient illumination through parameter scanning simulation to obtain the optimized structural parameters of each layer of the superlens corresponding to the maximum total light field energy ratio when the photoresist center reaches the imaging contrast requirement under the target resolution; S4, performing imaging light field simulation based on the transient illumination parameters, exposure time period, and optimized structural parameters of each layer of the superlens to determine whether the imaging effect meets expectations. If yes, the current parameters are the target parameters; if not, repeating S1 to S4 until the imaging effect meets expectations.
[0009] According to embodiments of this disclosure, each film layer of the superlens in S1 includes at least a mask, an air gap layer, a metal layer, and a photoresist layer.
[0010] According to embodiments of this disclosure, the superlens structure composed of the various film layers includes a mask, an air spacer layer, a metal transmission layer, a photoresist layer, a metal reflection layer, and a substrate; or the superlens structure includes a mask, an air spacer layer, a photoresist layer, a metal reflection layer, and a substrate; or the superlens structure includes a mask, an air spacer layer, a metal transmission layer, a photoresist layer, and a substrate; or the superlens structure includes a mask, an air spacer layer, a surface metal layer, a photoresist layer, an intermediate metal layer, a dielectric layer, and a bottom metal layer; or the superlens structure includes a mask, a metal-dielectric multilayer film, an air spacer layer, a photoresist layer, and a metal reflection layer.
[0011] According to embodiments of this disclosure, the material of the metal layer is any one or more of gold, silver, aluminum, and copper.
[0012] According to embodiments of this disclosure, the optimization design method in S1 includes any one of the following: rigorous coupled-wave analysis, finite-difference time-domain method, and finite element method.
[0013] According to an embodiment of this disclosure, S2 includes: S21, constructing transient illumination pulses with different attenuation rates based on the parameters of each layer of the superlens; S22, performing imaging light field simulation using rigorous coupled-wave analysis, finite-difference time-domain method, or finite element method; S23, calculating the proportion of total light field energy required for the photoresist center to achieve the required imaging contrast under the target resolution; and S24, obtaining the transient illumination parameters corresponding to the maximum proportion of total light field energy and confirming the corresponding exposure time period.
[0014] According to an embodiment of this disclosure, the imaging contrast in S23 is either the average imaging contrast or the instantaneous imaging contrast; the imaging contrast requirement includes the imaging contrast exceeding a preset value, where the preset value is 0.4.
[0015] According to an embodiment of this disclosure, S3 includes: S31, fine-tuning the structural parameters in the vicinity of the superlens layer structure parameters obtained in S1 with a small step size; S32, performing imaging light field simulation using rigorous coupled-wave analysis, finite-difference time-domain method, or finite element method; S33, calculating the proportion of total light field energy at the center of the photoresist to achieve the imaging contrast requirement under the target resolution; and S34, obtaining the structural parameters of each layer of the superlens corresponding to the maximum proportion of total light field energy, as the optimization parameters of each layer structure of the superlens.
[0016] According to an embodiment of this disclosure, S4 includes: S41, performing imaging light field simulation based on transient illumination parameters, exposure time period, and optimization parameters of each layer structure of the superlens; S42, statistically analyzing the integral result of the light intensity distribution at the center of the photoresist over the exposure time period to obtain the imaging light field distribution in the photoresist; S43, calculating the imaging contrast of the super-resolution lithography and confirming the imaging effect; S44, determining whether the imaging effect meets expectations. If yes, the current parameter is the target parameter; if not, repeating S1 to S4 until the imaging effect meets expectations.
[0017] According to an embodiment of this disclosure, the imaging light field simulation in S41 includes performing typical resolution pattern imaging simulation, wherein the typical resolution pattern includes one of dense periodic line pattern and finite root line pattern.
[0018] (III) Beneficial Effects
[0019] This disclosed method for enhancing the resolution of super-resolution lithography based on transient illumination designs the parameters of each layer of a superlens based on steady-state illumination. Then, transient illumination replaces steady-state illumination to illuminate the superlens. By adjusting the surface plasmon mode dispersion at the metal-dielectric interface in the superlens, the superlens can enhance and transmit surface plasmon modes with larger transverse wave vectors, thereby achieving higher imaging lithography resolution. Furthermore, without changing the lithography resolution, the working distance between the mask and the wafer can be extended, thus reducing the stringent requirements of super-resolution lithography on mask / wafer surface shape, nanometer gap control, and environmental particle management. This method is also highly compatible with existing super-resolution lithography technologies; the main difference lies only in the illumination. Attached Figure Description
[0020] Figure 1 A flowchart illustrating a super-resolution lithography resolution enhancement method based on transient illumination according to an embodiment of the present disclosure is shown.
[0021] Figure 2A schematic diagram of a surface plasmonic cavity superlens according to an embodiment of the present disclosure is shown.
[0022] Figure 3 This schematically illustrates the increase in the transverse wave vector of a transient illumination dispersion curve according to an embodiment of the present disclosure;
[0023] Figure 4 The illustration schematically shows the illumination pulse temporal envelope shape, imaging contrast at different times, and normalized imaging light field map of a 22nm half-cycle line pattern according to Embodiment 1 of this disclosure.
[0024] Figure 5 This schematically illustrates a comparison of the steady-state and transient imaging photoresist cross-sectional light field and its cut-off line for a 22nm half-cycle line pattern according to Embodiment 1 of this disclosure;
[0025] Figure 6 The illustration schematically shows a 22nm half-cycle two-dimensional pattern arranged periodically along the x-direction according to Embodiment 1 of this disclosure, and steady-state and transient imaging results.
[0026] Figure 7 The illustration schematically shows the illumination pulse temporal envelope shape, imaging contrast at different times, and normalized imaging light field map of a 45nm half-cycle line pattern according to Embodiment 2 of this disclosure.
[0027] Figure 8 The illustration schematically shows the results of the contrast of the 45nm half-cycle line pattern imaging as a function of working distance, the steady-state imaging photoresist cross-section light field results at working distances of 20nm and 40nm, and the comparison of the light field and cut-off line of the photoresist cross-section in transient imaging at a working distance of 40nm. Detailed Implementation
[0028] To make the objectives, technical solutions, and advantages of this disclosure clearer, the following detailed description is provided in conjunction with specific embodiments and the accompanying drawings.
[0029] The terminology used herein is for the purpose of describing particular embodiments only and is not intended to limit this disclosure. The terms “comprising,” “including,” etc., as used herein indicate the presence of the stated features, steps, operations, and / or components, but do not exclude the presence or addition of one or more other features, steps, operations, or components.
[0030] Material loss in a superlens can cause inconsistent attenuation of information components at different spatial frequencies (i.e., transverse wave vectors) of the target object, leading to image field distortion at the focal plane and thus reducing the lithographic resolution of the imaging. Therefore, this disclosure aims to provide a method for enhancing the lithographic resolution of surface plasmon (SP) imaging, in order to reduce the limiting effect of superlens material loss on lithographic resolution.
[0031] This disclosure provides a method for enhancing the resolution of super-resolution lithography based on transient illumination. Please refer to [link to relevant documentation]. Figure 1 The process includes: S1, optimizing the design of the light source wavelength and parameters of each layer of the superlens under steady-state illumination based on the mask parameters. The parameters of each layer of the superlens include at least material parameters and structural parameters; S2, performing imaging light field simulation under transient illumination based on the parameters of each layer of the superlens to obtain the transient illumination parameters corresponding to the maximum total light field energy ratio when the photoresist center reaches the imaging contrast requirement under the target resolution, and confirming the corresponding exposure time period; S3, fine-tuning the structural parameters of each layer of the superlens under transient illumination through parameter scanning simulation to obtain the optimized structural parameters of each layer of the superlens corresponding to the maximum total light field energy ratio when the photoresist center reaches the imaging contrast requirement under the target resolution; S4, performing imaging light field simulation based on the transient illumination parameters, exposure time period, and optimized structural parameters of each layer of the superlens to determine whether the imaging effect meets expectations. If yes, the current parameters are the target parameters; if not, repeat S1 to S4 until the imaging effect meets expectations.
[0032] This transient illumination method is a resolution enhancement approach based on steady-state illumination. To achieve this, the initial superlens structure parameters can be optimized under steady-state illumination conditions. Then, by replacing steady-state illumination with transient illumination and adjusting the surface plasmon resonance (SPR) dispersion at the metal-dielectric interface within the superlens, the superlens can enhance and transmit SPR modes with larger transverse wave vectors, thus achieving higher imaging lithography resolution. This method reduces the limiting effect of superlens material loss on imaging lithography resolution to a certain extent. It not only enhances imaging lithography resolution but can also be used to increase the working distance between the mask and the wafer in super-resolution lithography. Here, steady-state illumination refers to the commonly used illumination method that utilizes steady-state continuous light for lithography illumination; transient illumination refers to the illumination method that utilizes transient pulsed light for lithography illumination.
[0033] Based on the above embodiments, each film layer of the superlens in S1 includes at least a mask, an air gap layer, a metal layer, and a photoresist layer. The material of the metal layer is any one or more of gold, silver, aluminum, and copper.
[0034] The physical mechanism of super-resolution imaging based on surface plasmons lies in the fact that light waves incident on a metal surface can excite surface plasmon waves, and the metal-dielectric multilayer film can propagate the evanescent light waves carrying fine structural information of the pattern to the image plane, thereby realizing super-resolution imaging. The metal layer is at least one layer, and the material of the metal layer includes, but is not limited to, Au, Ag, Al, and Cu. Other metal materials that can excite surface plasmons can also be used in this disclosure.
[0035] Based on the above embodiments, the superlens structure composed of each film layer includes a mask, an air spacer layer, a metal transmission layer, a photoresist layer, a metal reflection layer, and a substrate; or the superlens structure includes a mask, an air spacer layer, a photoresist layer, a metal reflection layer, and a substrate; or the superlens structure includes a mask, an air spacer layer, a metal transmission layer, a photoresist layer, and a substrate; or the superlens structure includes a mask, an air spacer layer, a surface metal layer, a photoresist layer, an intermediate metal layer, a dielectric layer, and a bottom metal layer; or the superlens structure includes a mask, a metal-dielectric multilayer film, an air spacer layer, a photoresist layer, and a metal reflection layer.
[0036] Figure 2 The image shows one type of superlens structure for super-resolution lithography, comprising a mask (SiO2+Cr), an air spacer layer (Air), a metal transmission layer (Ag), a photoresist (Pr), a metal reflection layer (Ag), and a substrate (SiO2).
[0037] Based on the above embodiments, the optimization design method in S1 includes any one of the following: rigorous coupled-wave analysis, finite-difference time-domain method, and finite element method.
[0038] In steps S1, S2, S3, and S4, simulations can be performed using methods such as strictly coupled-wave (RCWA), finite-difference time-domain (FDTD), and finite element method (FEM). Specifically, in step S1, for steady-state imaging design of simple periodic line patterns, the RCWA method is preferred for rapid calculation. For transient imaging design in steps S2, S3, and S4, the FDTD and FEM methods can be used to optimize the structure and calculate the specific results. Based on actual simulation results, FDTD is faster and is therefore preferred. Subsequent steps optimize the material and structural parameters of each layer of the superlens based on the linewidth of the mask pattern and the existing processing capabilities to achieve basic imaging effects.
[0039] Based on the above embodiments, S2 includes: S21, constructing transient illumination pulses with different attenuation rates according to the parameters of each film layer of the superlens; S22, performing imaging light field simulation using rigorous coupled-wave analysis, finite-difference time-domain method, or finite element method; S23, calculating the proportion of total light field energy required for the photoresist center to achieve the required imaging contrast under the target resolution; S24, obtaining the transient illumination parameters corresponding to the maximum proportion of total light field energy, and confirming the corresponding exposure time period.
[0040] Imaging improvement with transient illumination is related to exponentially decaying illumination. It is necessary to calculate the pulse decay and imaging correspondence to achieve higher pulse energy utilization when the required resolution is reached. Specifically, using the superlens structure parameters optimized in step S1 under steady-state illumination, pulses with different decay rates are constructed. Imaging light field simulation is performed using the finite-difference time-domain (FDTD) method or the finite element method (FEM). The proportion of total light field energy required for the photoresist center to achieve the required imaging contrast (e.g., 0.4) at the target resolution is calculated to meet the imaging contrast requirements typically needed for positive resist lithography. The optimal transient illumination parameters are those that reach their maximum value, primarily considering the decay rate of the falling edge, while simultaneously confirming the corresponding exposure time period. Figure 3 This diagram illustrates the transient illumination method of this disclosure for the transverse wave vector on a single metal-dielectric interface. Pulsed illumination with a decaying falling edge increases the transverse wave vector on the interface, and different falling edge decay rates γ correspond to different degrees of transverse wave vector growth. This disclosure uses a femtosecond pulse illumination superlens to optimize the temporal waveform of the transient illumination pulse, thereby achieving finer imaging lithographic resolution.
[0041] Based on the above embodiments, in S23, the imaging contrast is the average imaging contrast or the instantaneous imaging contrast; the imaging contrast requirement includes the imaging contrast exceeding a preset value, which is 0.4.
[0042] In actual simulation calculations, the contrast ratio is generally calculated as the ratio of the difference between the maximum and minimum light intensity values of the photoresist layer to the sum of the values, i.e., C = (I max -I min ) / (I max +I min This method of calculation is also known as Michelson contrast. A higher contrast ratio indicates a steeper pattern that can be produced by photolithography, meaning better resolution. For submicron patterns, a contrast ratio greater than 0.4 is generally required for positive resist patterns and greater than 0.2 for negative resist patterns.
[0043] The starting point for determining imaging contrast is the moment when the average imaging contrast exceeds 0.4. Since the illumination pulse energy weakens rapidly and subsequently makes no real contribution to the imaging results, an instantaneous imaging contrast greater than 0.4 can also be used as the starting point (see...). Figure 4(b) Contrast variation curve over time, and the cutoff time can be disregarded.
[0044] Based on the above embodiments, S3 includes: S31, fine-tuning the structural parameters near the structural parameters of each layer of the superlens obtained in S1 with a small step size; S32, performing imaging light field simulation using rigorous coupled-wave analysis, finite-difference time-domain method, or finite element method; S33, calculating the proportion of total light field energy at the center of the photoresist to achieve the imaging contrast requirement under the target resolution; S34, obtaining the structural parameters of each layer of the superlens corresponding to the maximum proportion of total light field energy, as the optimization parameters of each layer of the superlens structure.
[0045] The steady-state structural parameters obtained in step S1 may not be suitable for the transient illumination parameters selected in S2. Based on steps S1 and S2, the superlens structural parameters are fine-tuned through parameter scanning simulation to further improve the proportion of total light field energy when the photoresist center reaches the imaging contrast (0.4) requirement under the target resolution. When it reaches its maximum value, the optimized parameters of the superlens structure under transient illumination are obtained.
[0046] Based on the above embodiments, S4 includes: S41, performing imaging light field simulation based on transient illumination parameters, exposure time period, and optimized parameters of each layer structure of the superlens; S42, statistically analyzing the integral result of the light intensity distribution at the center of the photoresist over the exposure time period to obtain the imaging light field distribution in the photoresist; S43, calculating the imaging contrast of super-resolution lithography and confirming the imaging effect; S44, determining whether the imaging effect meets expectations. If yes, the current parameter is the target parameter; if not, repeating S1 to S4 until the imaging effect meets expectations. The imaging light field simulation in S41 includes performing typical resolution pattern imaging simulation, wherein the typical resolution pattern includes one of dense periodic line patterns and finite root line patterns.
[0047] Imaging simulations of dense periodic line patterns, finite root line patterns, and other typical resolution patterns were performed using the obtained transient illumination parameters and superlens structure optimization parameters. The imaging light field contrast was calculated to confirm the actual imaging effect. In some cases, phase shifting occurs, meaning the image plane of periodic lines is opposite to the positional distribution of the mask pattern, which is destructive to the imaging of non-periodic patterns. This is generally due to improper material parameter selection, resulting in interference-like phenomena. Therefore, contrast alone is insufficient to fully represent imaging quality; feedback optimization based on the imaging results of actual patterns is also necessary. When this occurs, the process can be directly reversed back to S1 to redesign parameters that have the most direct impact on imaging, such as the light source wavelength and film material thickness.
[0048] For super-resolution lithography based on surface plasmons, this disclosure significantly enhances the imaging lithography resolution by replacing steady-state continuous illumination with transient pulsed illumination and optimizing the temporal pulse envelope shape of the pulsed light, thereby enabling the lithography of patterns with smaller feature sizes. Furthermore, without changing the lithography resolution, the working distance between the mask and the wafer can be extended, thus reducing the stringent requirements of super-resolution lithography on mask / wafer surface shape, nanometer gap control, and environmental particle management. This method is also highly compatible with existing super-resolution lithography technologies, with the main difference being in the illumination aspect.
[0049] The present disclosure will be further described below through specific embodiments. The following embodiments specifically illustrate the above-described method for enhancing super-resolution lithography based on transient illumination. However, the following embodiments are merely illustrative of the present disclosure, and the scope of the present disclosure is not limited thereto.
[0050] The present invention discloses a method for enhancing the resolution of super-resolution lithography based on transient illumination, such as... Figures 1-2 As shown, the following steps are performed sequentially:
[0051] Step 1: Design the superlens structure under steady-state illumination. First, determine the materials and light source. The main lens materials available for surface plasmon super-resolution lithography are one of the noble metals gold, silver, aluminum, and copper. Referring to traditional surface plasmon super-resolution lithography, the illumination center wavelength is set, for example, to 365nm. Further optimization can be achieved by selecting the center wavelength of the femtosecond laser. Based on the target lithographic resolution, combined with the light source wavelength and film material, and considering process conditions, the superlens film structure parameters under steady-state continuous illumination are designed to achieve better imaging lithography results under steady-state conditions; this is equivalent to step S1 above.
[0052] Step 2: Design the pulse parameters for transient illumination to enhance resolution while improving pulse energy utilization efficiency. Based on the film structure parameters determined in the previous steps, construct pulses with different decay rates and falling edges. Import these pulses as transient illumination sources into the software for transient simulation calculations. Calculate the proportion of total light field energy during the time period when the imaging contrast is >0.4. Select the decay rate with the larger proportion of total light field energy as the transient light source pulse parameter and determine this time period as the exposure time period; this is equivalent to step S2 above.
[0053] Step 3: Further optimize the superlens structure parameters under transient illumination. The steady-state structure parameters obtained in step S1 may not be suitable for the transient illumination pulse selected in S2. Fine-tune the structure parameters, i.e., the film thickness, with a small step size near the steady-state structure parameters, and import them into the software to calculate and optimize the structure parameters that maximize the utilization of pulse energy; this is equivalent to step S3 above.
[0054] Step 4: Calculate and verify the actual imaging results. Based on the film and light source parameters calculated in the previous steps, and the obtained exposure time period, import the data into the software to recalculate the specified exposure pattern. Statistically analyze the integral results of the light intensity distribution within the available time period in S2 to obtain the imaging light field in the photoresist. Calculate and verify the super-resolution lithography imaging resolution. For the requirement to extend the working distance, if the energy at the moment that meets the contrast requirement is relatively small, appropriately reduce the working distance and recalculate; this is equivalent to step S4 above.
[0055] Based on steps 1 to 4 above, two specific embodiments are provided below.
[0056] Example 1:
[0057] This embodiment shows the imaging result of exposing a line pattern with a smaller linewidth, namely 22nm half-cycle line pattern. The implementation steps of this embodiment are as follows:
[0058] Step 1-1: Design the superlens structure under steady-state illumination. The superlens structure includes a mask, an air gap layer, a metal layer, a photoresist layer, a metal reflective layer, and a substrate. Silver is chosen as the lens material. The illumination center wavelength is set to 365nm, which can be further optimized by selecting the center wavelength of the femtosecond laser. The required film layer parameters are the thicknesses of the air gap layer, the surface silver layer, the photoresist layer, and the bottom silver layer. The RCWA method is used to calculate the imaging contrast under different combinations of film layer thicknesses through parameter scanning, thereby obtaining the thicknesses of the air gap layer, the surface silver layer, the photoresist layer, and the bottom silver layer. In this embodiment, the mask thickness is set to 40nm, the air gap layer thickness to 15nm, the surface silver layer thickness to 12nm, the photoresist layer thickness to 15nm, and the bottom silver layer thickness to 40nm.
[0059] Step 1-2: Design transient illumination pulse parameters. Based on the film structure parameters determined in the previous steps, pulses with different decay rates and falling edges are constructed and imported into FDTD software as transient illumination sources for transient simulation calculations. The energy proportion of the time period with an average contrast greater than 0.4 is calculated, and the decay rate with the larger energy proportion is selected as the light source pulse parameter. This time period is then determined as the exposure time period. Through parameter scanning, a suitable exponential decay rate of 0.25 on the falling edge of the light pulse is optimized.
[0060] Figure 4 Figures (a) to (c) show the transient imaging light source pulse shape, normalized intensity, and contrast over time for 22nm half-cycle line patterns, respectively. The transient illumination is indistinguishable from steady-state super-resolution lithography during the pulse stabilization period. The average contrast is greater than 0.4 during the decay phase (from 22.8 fs to the end of the pulse), which is the exposure period.
[0061] Steps 1-3: Optimize the superlens structure parameters under transient illumination. Fine-tune the structure parameters (i.e., the film thickness) with small step sizes near the steady-state structure parameters, and import the results into FDTD software to calculate and optimize the structure parameters that maximize pulse energy utilization. This optimization step is omitted here to demonstrate the improvement of transient imaging compared to steady-state imaging under the same structural conditions.
[0062] Steps 1-4: Verify the resolution enhancement effect. Using the obtained transient illumination pulse light parameters and superlens structure parameters, simulate the imaging of dense periodic line patterns, finite root line patterns, and other typical resolution patterns, and calculate the imaging light field contrast to confirm the actual imaging effect.
[0063] Figure 5 Images (a) to (b) show the steady-state and transient imaging results of the photoresist longitudinal section from 22.8 fs after the pulse ends, for a 22nm linewidth half-cycle infinitely long line. Figure 5 In the middle (c), the normalized intensity result of the corresponding photoresist center cutoff line is shown. The contrast ratio is improved from 0.17 to 0.4, and the resolution is significantly improved.
[0064] Figure 6 In the middle (a), there is a 22nm linewidth half-period two-dimensional pattern with periodic arrangement in the x direction. Figure 6 Images (b) to (c) show the steady-state and transient imaging results, respectively. As shown in the one-dimensional case, transient illumination can better distinguish the image, demonstrating the ability of this disclosure to distinguish smaller images.
[0065] Example 2:
[0066] This embodiment presents the imaging results of an exposure at an extended working distance for a 45nm half-cycle line pattern. The implementation steps of this embodiment are as follows:
[0067] Step 2-1: Design the superlens structure under steady-state illumination. The superlens structure includes a mask, an air gap layer, a metal layer, a photoresist layer, a metal reflective layer, and a substrate. Silver is chosen as the lens material. The illumination center wavelength is set to 365nm, which can be further optimized by selecting the center wavelength of the femtosecond laser. The required film layer parameters are the thicknesses of the air gap layer, the surface silver layer, the photoresist layer, and the bottom silver layer. The RCWA method is used to calculate the imaging contrast under different combinations of film layer thicknesses through parameter scanning, thereby obtaining the thicknesses of the air gap layer, the surface silver layer, the photoresist layer, and the bottom silver layer. In this embodiment, the mask thickness is set to 40nm, the air gap layer thickness to 40nm, the surface silver layer thickness to 12nm, the photoresist layer thickness to 30nm, and the bottom silver layer thickness to 40nm.
[0068] Step 2-2: Design transient illumination pulse parameters. Based on the film structure parameters determined in the previous steps, pulses with different decay rates and falling edges are constructed and imported into FDTD software as transient illumination sources for transient simulation calculations. The energy proportion of the time period with an average contrast greater than 0.4 is calculated, and the decay rate with the larger energy proportion is selected as the light source pulse parameter. This time period is then determined as the exposure time period. Through parameter scanning, a suitable exponential decay rate of 0.25 on the falling edge of the light pulse is optimized.
[0069] Figure 7 Figures (a) to (c) show the results of light source pulse shape, normalized imaging intensity, and imaging contrast over time for transient imaging of 45nm half-cycle lines, respectively. During the stable pulse period, the transient illumination is indistinguishable from that of ordinary surface plasmon lithography. The average contrast exceeding 0.4 during the decay phase (23.3 fs) until the pulse ends is considered a usable exposure period.
[0070] Steps 2-3: Optimize the superlens structure parameters under transient illumination. Fine-tune the structure parameters (i.e., the film thickness) with small step sizes near the steady-state structure parameters, and import the results into FDTD software to calculate and optimize the structure parameters that maximize pulse energy utilization. This optimization step is omitted here to demonstrate the improvement in transient imaging compared to steady-state imaging under the same structural conditions.
[0071] Steps 2-4: Verify the resolution enhancement effect. Using the obtained transient illumination pulse light parameters and superlens structure parameters, simulate the imaging of dense periodic line patterns, finite root line patterns, and other typical resolution patterns, and calculate the imaging light field contrast to confirm the actual imaging effect.
[0072] Figure 8 In Figure (a), the steady-state imaging contrast of the photoresist center cut-off line changes with the working distance. When the working distance continues to increase from 20nm, the contrast of the photoresist center cut-off line alone cannot meet the imaging requirements. Figure 8 (b) to (c) are steady-state imaging results of the longitudinal cross-section of the photoresist at working distances of 20nm and 40nm, respectively, for an infinitely long line with a half-cycle of 45nm. It can be seen that the 20nm working distance can provide good imaging with a contrast of 0.47. When the working distance is extended to 40nm, the contrast of the photoresist center is 0.15, and it is obvious that the photoresist is not completely penetrated. Figure 8 The middle (d) diagram shows the results of the normalized electric field intensity at the center cutoff of the photoresist under steady-state and transient imaging at a working distance of 40 nm. Figure 8 Image (e) shows the transient imaging results when the working distance is 40 nm. The contrast reaches 0.4 after 23.5 fs, and the light field has good uniformity at different depths in the photoresist, demonstrating the extension of the working distance under the same structural parameters.
[0073] The specific embodiments described above further illustrate the purpose, technical solutions, and beneficial effects of this disclosure. It should be understood that the above descriptions are merely specific embodiments of this disclosure and are not intended to limit this disclosure. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of this disclosure should be included within the protection scope of this disclosure.
Claims
1. A method for resolution enhancement in transient illumination based super-resolution lithography, characterized in that, include: S1, optimize the design of the light source wavelength and the parameters of each layer of the superlens under steady-state illumination based on the mask parameters. The parameters of each layer of the superlens include at least material parameters and structural parameters. S2, based on the parameters of each film layer of the superlens, perform imaging light field simulation under transient illumination, obtain the transient illumination parameters corresponding to when the photoresist center reaches the imaging contrast requirement and the total light field energy ratio is the largest under the target resolution, and confirm the corresponding exposure time period. S3, by simulating parameter scanning to fine-tune the structural parameters of each layer of the superlens under transient illumination, obtain the optimized structural parameters of each layer of the superlens when the photoresist center reaches the imaging contrast requirement and the total light field energy ratio is maximized under the target resolution. S4. Based on the transient illumination parameters, the exposure time period, and the optimized parameters of each film layer of the superlens, perform imaging light field simulation to determine whether the imaging effect meets expectations. If yes, the current parameters are the target parameters; otherwise, repeat S1~S4 until the imaging effect meets expectations.
2. The transient illumination based super-resolution lithography resolution enhancement method of claim 1, wherein, The superlens in S1 includes at least a mask, an air gap layer, a metal layer, and a photoresist layer.
3. The transient illumination based super-resolution lithography resolution enhancement method of claim 2, wherein, The superlens structure, composed of the various film layers, includes a mask, an air spacer layer, a metal transmission layer, a photoresist layer, a metal reflection layer, and a substrate; or The superlens structure includes a mask, an air gap layer, a photoresist layer, a metal reflective layer, and a substrate; or The superlens structure includes a mask, an air gap layer, a metal transmission layer, a photoresist layer, and a substrate; or The superlens structure includes a mask, an air gap layer, a top metal layer, a photoresist layer, an intermediate metal layer, a dielectric layer, and a bottom metal layer; or The superlens structure includes a mask, a metal-dielectric multilayer film, an air spacer layer, a photoresist layer, and a metal reflective layer.
4. The transient-illumination-based super-resolution lithography resolution enhancement method of claim 2, wherein, The metal layer is made of any one or more of gold, silver, aluminum, and copper.
5. The method for enhancing the resolution of super-resolution lithography based on transient illumination according to claim 1, characterized in that, The optimization design method in S1 includes any one of the following: rigorous coupled-wave analysis, finite-difference time-domain method, and finite element method.
6. The method for enhancing the resolution of super-resolution lithography based on transient illumination according to claim 1, characterized in that, S2 includes: S21, construct transient illumination pulses with different attenuation rates according to the parameters of each film layer of the superlens; S22, using rigorous coupled-wave analysis, finite-difference time-domain method or finite element method to simulate the imaging light field; S23, calculate the proportion of total light field energy at the center of the photoresist to achieve the imaging contrast requirement under the target resolution; S24, obtain the transient illumination parameters corresponding to the maximum proportion of total light field energy, and confirm the corresponding exposure time period.
7. The method for enhancing the resolution of super-resolution lithography based on transient illumination according to claim 6, characterized in that, The imaging contrast in S23 is either the average imaging contrast or the instantaneous imaging contrast; The imaging contrast requirement includes an imaging contrast exceeding a preset value, where the preset value is 0.
4.
8. The method for enhancing the resolution of super-resolution lithography based on transient illumination according to claim 1, characterized in that, S3 includes: S31, fine-tune the structural parameters of each film layer of the superlens obtained in S1 with a small step size; S32 uses rigorous coupled-wave analysis, finite-difference time-domain method or finite element method to simulate the imaging light field; S33, calculates the proportion of total light field energy at the center of the photoresist to achieve the imaging contrast requirement under the target resolution; S34, obtain the structural parameters of each layer of the superlens corresponding to the maximum proportion of the total light field energy, and use them as the optimization parameters of each layer of the superlens.
9. The method for enhancing the resolution of super-resolution lithography based on transient illumination according to claim 1, characterized in that, S4 includes: S41, Simulate the imaging light field based on the transient illumination parameters, the exposure time period, and the optimization parameters of each film layer structure of the superlens; S42, the integral result of the light intensity distribution at the center of the photoresist during the exposure time period is statistically analyzed to obtain the imaging light field distribution in the photoresist; S43, calculate the imaging contrast of super-resolution lithography and confirm the imaging effect; S44: Determine whether the imaging effect meets expectations. If yes, the current parameter is the target parameter; otherwise, repeat S1~S4 until the imaging effect meets expectations.
10. The method for enhancing the resolution of super-resolution lithography based on transient illumination according to claim 9, characterized in that, The imaging light field simulation in S41 includes performing typical resolution pattern imaging simulation, wherein the typical resolution pattern includes one of dense periodic line pattern and finite root line pattern.