A high-performance magnetic shielding device based on a nanocrystalline and permalloy composite structure

By using a multi-layer magnetic shielding layer composed of nanocrystals and permalloy, combined with magnetic flux shunting and eddy current elimination, the problem of low shielding effectiveness of existing devices in low-frequency alternating magnetic fields and geomagnetic fields is solved, achieving a highly efficient and stable broadband shielding effect.

CN117074742BActive Publication Date: 2026-11-10BEIHANG UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202311183360.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-09-14
Publication Date
2026-11-10
Estimated Expiration
2043-09-14

AI Technical Summary

Technical Problem

Existing magnetic shielding devices cannot effectively shield the Earth's magnetic field and low-frequency alternating magnetic fields. They have low shielding coefficients and high losses, which affect the stability of the equipment.

Method used

By employing a composite structure of nanocrystalline and permalloy, and through magnetic flux shunting and eddy current elimination, combined with a nanocrystalline release film and a non-magnetic pad, a multi-layer high-permeability magnetic shielding layer is formed, achieving efficient shielding over a wide frequency range.

Benefits of technology

It achieves efficient shielding against the Earth's magnetic field and low-frequency alternating magnetic field, reduces losses, improves the stability and shielding effectiveness of the device, and meets the shielding requirements of a wide frequency range.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117074742B_ABST
    Figure CN117074742B_ABST
Patent Text Reader

Abstract

This invention discloses a high-performance magnetic shielding device based on a nanocrystalline and permalloy composite structure. Specifically, it includes multiple high-permeability magnetic shielding layers of the nanocrystalline and permalloy composite structure, a release film for the nanocrystalline layers, a non-magnetic fixing device between the shielding layers, and non-magnetic pads. The high-permeability magnetic shielding layers of the nanocrystalline and permalloy composite structure have the nanocrystalline magnetic shielding layer on the outside and the permalloy magnetic shielding layer on the inside, used to shield static magnetic fields and low-frequency alternating magnetic fields. The nanocrystalline magnetic shielding layers are bonded together with a non-magnetic insulating adhesive. The release film for the nanocrystalline layers is placed on the outside of the nanocrystalline magnetic shielding layers to prevent nanocrystalline fragmentation and reduced shielding performance. The non-magnetic fixing device between the shielding layers maintains the spacing between the magnetic shielding layers. The non-magnetic pads provide flexible buffering between the non-magnetic fixing device and the magnetic shielding layers, preventing stress concentration that could lead to nanocrystalline fragmentation. This invention has a compact structure, a wide applicable frequency range, and good testing results.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of magnetic shielding, and in particular to a high-performance magnetic shielding device based on a nanocrystalline and permalloy composite structure, used to shield static magnetic fields and low-frequency alternating magnetic fields. Background Technology

[0002] The measurement of extremely weak magnetic fields relies on the "zero-magnetic" space created by various magnetic shielding devices. This is of great significance for discovering new laws governing extremely weak magnetic interactions in matter and for extreme research on the mechanisms of neural, cardiac, and brain signals. Many weak signal detection and scientific experiments depend on extremely weak magnetic field environments. For example, the most important region for applications in weak magnetic environments such as magnetoencephalography (MEG), magnetocardiography (MCG), atomic magnetometers, and biomagnetic measurements ranges from static magnetic fields to low-frequency alternating magnetic fields of 1 kHz. Therefore, magnetic shielding devices should achieve excellent shielding effects within this frequency range. Magnetic shielding in low-frequency magnetic fields (f ≤ 1 kHz) has two physical mechanisms: magnetic flux shunting and eddy current elimination. The source frequency, shielding structure, and material parameters determine which shielding mechanism is dominant.

[0003] Excellent magnetic properties and optimal structural dimensions are key to improving magnetic shielding performance. Currently widely used magnetic shielding materials cannot simultaneously provide effective electromagnetic protection against both low-frequency magnetic fields and high-frequency electromagnetic fields, failing to meet current demands for wide-frequency, high-efficiency shielding. Multilayer shielding materials can complement and correlate the properties of their components, significantly broadening the shielding frequency range. This allows for the concentration of magnetic fields, improving shielding effectiveness and reducing residual magnetism.

[0004] In the field of magnetic shielding for static and low-frequency magnetic fields (f≤1kHz), losses have a significant impact on shielding performance and equipment stability. Employing high-permeability, low-loss magnetically conductive materials, refining shielding structure design, and improving shielding processes can effectively reduce losses. Reducing losses helps improve the energy conversion efficiency of magnetically conductive materials in magnetic fields, thereby enhancing their ability to absorb, guide, and disperse magnetic fields, and ultimately significantly improving magnetic shielding performance, ensuring the normal operation and stable performance of equipment under specific environments. Summary of the Invention

[0005] To address the shortcomings of existing technologies, this invention proposes a high-performance magnetic shielding device based on a nanocrystalline and permalloy composite structure, which achieves efficient shielding of static magnetic fields and low-frequency alternating magnetic fields. This invention features a lightweight, highly effective, wide-frequency shielding range, low loss, and high reliability composite magnetic shielding structure and its manufacturing method.

[0006] The objective of this invention is achieved through the following technical solution:

[0007] A high-performance magnetic shielding device based on a nanocrystalline and permalloy composite structure includes multiple high-permeability magnetic shielding layers of nanocrystalline and permalloy composite structure, a nanocrystalline layer release film, a non-magnetic fixing device between shielding layers, and a non-magnetic pad.

[0008] The high permeability magnetic shielding layer of the nanocrystalline and permalloy composite structure includes multiple high permeability nanocrystalline and permalloy composite structures nested from the inside to the outside, which are used to shield static magnetic fields through magnetic flux shunting and to shield low-frequency alternating magnetic fields through magnetic flux shunting and eddy current elimination.

[0009] The bottom of the nanocrystalline magnetic shielding layer in the high permeability magnetic shielding layer of the nanocrystalline and permalloy composite structure is bonded to the outside of the permalloy magnetic shielding layer by the non-magnetic insulating adhesive of the nanocrystalline strip. The permalloy is inside the high permeability magnetic shielding layer of the nanocrystalline and permalloy composite structure, which realizes the mechanical support of the composite structure and the shielding of the extremely weak magnetic field after the attenuation of the magnetic field lines by the nanocrystalline layer.

[0010] The nanocrystalline magnetic shielding layer comprises multiple layers of single-sided non-magnetic insulating adhesive nanocrystalline tapes laid crosswise. The nanocrystalline magnetic shielding layers are interconnected by the non-magnetic insulating adhesive of the nanocrystalline tapes, and the nanocrystalline tapes are laid in a crosswise manner.

[0011] The nanocrystalline layer release film is placed above the nanocrystalline magnetic shielding layer to protect each of the nanocrystalline magnetic shielding layers from being crushed by force. The nanocrystalline magnetic shielding layer is tightly attached to the permalloy magnetic shielding layer.

[0012] The non-magnetic fixing device between the shielding layers is set between the non-magnetic pad and the permalloy magnetic shielding layer to maintain the spacing between the high permeability magnetic shielding layers of the nanocrystalline and permalloy composite structure. The non-magnetic fixing device between the shielding layers is placed at the bottom of the high-performance magnetic shielding device and is closely attached to the permalloy layer. The top of the non-magnetic fixing device between the shielding layers is closely connected to the non-magnetic pad.

[0013] The non-magnetic pad is fixed above the non-magnetic fixing device between the shielding layers. The non-magnetic pad is made of non-magnetic silicone material. The top layer of the non-magnetic fixing device between the shielding layers is tightly bonded to the bottom layer of the non-magnetic pad. The top of the non-magnetic pad is used to support the nanocrystalline magnetic shielding layer and is tightly connected to the nanocrystalline layer release film on the outside of the high magnetic permeability magnetic shielding layer of the nanocrystalline and permalloy composite structure. It is used to isolate the nanocrystalline magnetic shielding layer from the non-magnetic fixing device between the shielding layers and to buffer the nanocrystalline magnetic shielding layer from the non-magnetic fixing device between the shielding layers.

[0014] The nanocrystalline release film is placed outside the nanocrystalline magnetic shielding layer in the high permeability magnetic shielding layer of the nanocrystalline and permalloy composite structure. Its bottom is tightly bonded to the nanocrystalline magnetic shielding layer, and its outer side is tightly bonded to the non-magnetic pad. This avoids the nanocrystalline magnetic shielding layer from being in direct contact with the non-magnetic pad and being subjected to concentrated stress, which could lead to the fragmentation of the nanocrystalline material.

[0015] The technical solution provided by this invention brings at least the following beneficial effects:

[0016] This invention utilizes nanocrystalline and permalloy materials—which possess high permeability, low loss, low coercivity, good mechanical properties, and low cost—as composite high-performance magnetic shielding devices. The technical solution of this invention solves the problems of existing magnetic shielding devices' inability to efficiently shield the Earth's magnetic field and low-frequency alternating magnetic fields, as well as their low shielding coefficient. By setting the magnetic shielding layer as a composite structure of nanocrystalline and permalloy, both nanocrystalline and permalloy exhibit high permeability characteristics under the Earth's magnetic field, achieving efficient shielding of the Earth's magnetic field. The nanocrystalline material maintains high permeability at high frequencies, effectively compensating for the sharp decrease in permeability of permalloy at high frequencies, thus meeting the shielding requirements across a wide frequency range. Furthermore, the addition of a release film for the nanocrystalline layer and non-magnetic pads provides flexible buffering, preventing stress concentration from damaging the nanocrystalline magnetic shielding layer structure and reducing shielding performance. The thickness of the nanocrystalline and permalloy materials can be adjusted to meet different shielding requirements for the Earth's magnetic field and low-frequency alternating magnetic fields. Attached Figure Description

[0017] To more clearly illustrate the technical solutions of the embodiments of the present invention, the following description of implementation examples is provided in conjunction with the accompanying drawings. However, the drawings are only for some embodiments of the present invention, wherein:

[0018] Figure 1 This is a cross-sectional view of the overall structure of a high-performance magnetic shielding device based on a nanocrystalline and permalloy composite structure according to the present invention.

[0019] Figure 2 This is a schematic diagram of the nanocrystalline and permalloy composite structure of a high-performance magnetic shielding device based on a nanocrystalline and permalloy composite structure according to the present invention.

[0020] Figure 3 This is a three-dimensional view of a non-magnetic fixing device and a non-magnetic pad for a high-performance magnetic shielding device based on a nanocrystalline and permalloy composite structure according to the present invention.

[0021] Figure 4 This is a perspective view of the end cap of a high-performance magnetic shielding device based on a nanocrystalline and permalloy composite structure according to the present invention.

[0022] Figure 5 This is a simulation result of the static magnetic shielding coefficient of a three-layer high-performance magnetic shielding device based on a nanocrystalline and permalloy composite structure according to the present invention.

[0023] Figure 6 This is a simulation result of the magnetic shielding coefficient of a three-layer high-performance magnetic shielding device based on a nanocrystalline and permalloy composite structure under an alternating magnetic field, according to the present invention.

[0024] In the diagram: 1. First layer of high-permeability magnetic shielding layer with nanocrystalline and permalloy composite structure; 2. Second layer of high-permeability magnetic shielding layer with nanocrystalline and permalloy composite structure; 3. Third layer of high-permeability magnetic shielding layer with nanocrystalline and permalloy composite structure; 4. First layer of nanocrystalline release film; 5. First layer of nanocrystalline magnetic shielding layer; 6. First layer of permalloy magnetic shielding layer; 7. Second layer of nanocrystalline release film; 8. Second layer of nanocrystalline magnetic shielding layer; 9. Second layer of permalloy magnetic shielding layer; 10. Third layer of nanocrystalline release film; 11. Third layer of nanocrystalline magnetic shielding layer; 12. Third layer of permalloy magnetic shielding layer; 13. First layer of non-magnetic pad; 14. First non-magnetic fixing device; 15. Second layer of non-magnetic pad; 16. Second non-magnetic fixing device; 17. Single layer of nanocrystalline strip; 18. Non-magnetic insulating adhesive; 19. Limiting block; 20. End cap experimental hole. Detailed Implementation

[0025] The present invention will be described in detail below with reference to the accompanying drawings and preferred embodiments, and the purpose and effects of the present invention will become clearer. It should be understood that the specific embodiments described herein are merely for explaining the present invention and are not intended to limit the present invention.

[0026] This invention provides a high-performance magnetic shielding device based on a nanocrystalline and permalloy composite structure. The high-performance magnetic shielding device comprises multiple high-permeability magnetic shielding layers of nanocrystalline and permalloy composite structure, a release film for the nanocrystalline layers, a non-magnetic fixing device between the shielding layers, and non-magnetic pads. Each high-permeability magnetic shielding layer of nanocrystalline and permalloy composite structure comprises multiple nested high-permeability nanocrystalline and permalloy composite structures, used to shield static magnetic fields through magnetic flux shunting and to shield low-frequency alternating magnetic fields through magnetic flux shunting and eddy current elimination. Each high-permeability magnetic shielding layer of nanocrystalline and permalloy composite structure is provided with a composite structure shielding end cap, and each end cap has an end cap experimental hole for use with a testing instrument to measure the central residual magnetism of the high-performance magnetic shielding device of nanocrystalline and permalloy composite structure.

[0027] The nanocrystalline magnetic shielding layer in the high permeability magnetic shielding layer of the nanocrystalline and permalloy composite structure is bonded to the outside of the permalloy magnetic shielding layer by a non-magnetic insulating adhesive of the nanocrystalline strip. The permalloy magnetic shielding layer is located inside the high permeability magnetic shielding layer of the nanocrystalline and permalloy composite structure, thus providing mechanical support for the composite structure and shielding the extremely weak magnetic field after the attenuation of the magnetic field lines by the nanocrystalline layer. The nanocrystalline magnetic shielding layer includes multiple layers of single-sided non-magnetic insulating adhesive nanocrystalline strips that are stacked and cross-laid. The nanocrystalline magnetic shielding layers are connected to each other by the non-magnetic insulating adhesive of the nanocrystalline strips, and the nanocrystalline strips are laid in a cross-laid manner.

[0028] The nanocrystalline layer release film is placed above the nanocrystalline magnetic shielding layer to protect each of the nanocrystalline magnetic shielding layers from being subjected to force and to prevent the nanocrystals from fragmenting. The nanocrystalline magnetic shielding layer is tightly attached to the permalloy magnetic shielding layer above the nanocrystalline magnetic shielding layer.

[0029] The non-magnetic fixing device between the shielding layers is set between the non-magnetic pad and the permalloy magnetic shielding layer to maintain the spacing between the high permeability magnetic shielding layers of the nanocrystalline and permalloy composite structure. The non-magnetic fixing device between the shielding layers is placed at the bottom of the high-performance magnetic shielding device and is closely attached to the permalloy layer. The top of the non-magnetic fixing device between the shielding layers is closely connected to the non-magnetic pad.

[0030] The non-magnetic pads are made of non-magnetic silicone material. The top layer of the non-magnetic fixing device between each shielding layer is tightly bonded to the bottom layer of each non-magnetic pad. The top of each non-magnetic pad is used to support each nanocrystalline magnetic shielding layer and is tightly connected to the release film of each nanocrystalline layer outside the high magnetic permeability magnetic shielding layer of each nanocrystalline and permalloy composite structure. This is used to isolate the nanocrystalline magnetic shielding layer from the non-magnetic fixing device between the shielding layers, and to buffer the nanocrystalline magnetic shielding layer from the non-magnetic fixing device between the shielding layers.

[0031] Each nanocrystalline layer release film is placed outside the nanocrystalline magnetic shielding layer in the high permeability magnetic shielding layer of the nanocrystalline and permalloy composite structure. The bottom of the release film is tightly bonded to the nanocrystalline magnetic shielding layer. The outside of the nanocrystalline layer release film is tightly bonded to the non-magnetic pad to avoid the nanocrystalline magnetic shielding layer from being in direct contact with the non-magnetic pad and being subjected to concentrated stress, which would cause the nanocrystalline to fragment.

[0032] The technical solution of this invention solves the problems of existing magnetic shielding devices being unable to efficiently shield low-frequency alternating magnetic fields and having low shielding coefficients. It sets the magnetic shielding layer as a composite structure of nanocrystalline and permalloy materials. Both nanocrystalline and permalloy materials exhibit high magnetic permeability under geomagnetic fields, enabling efficient shielding of geomagnetic fields. The nanocrystalline material maintains high magnetic permeability at high frequencies, effectively compensating for the sharp decrease in permeability of permalloy at high frequencies, thus meeting the shielding requirements across a wide frequency range. Furthermore, the addition of a release film for the nanocrystalline layer and non-magnetic pads provides flexible buffering, preventing stress concentration from damaging the nanocrystalline magnetic shielding layer structure and reducing shielding performance. By adjusting the thickness of the nanocrystalline and permalloy materials, different shielding requirements for geomagnetic fields and low-frequency alternating magnetic fields can be met.

[0033] Each permalloy layer can be rectangular, preferably square, and the preferred grade is 1J85, requiring high permeability, high saturation magnetic induction, and low loss in the 0-1kHz frequency range. The thickness of the permalloy plate is 0.5-4mm, preferably 0.75-2mm, and the plate should be free of obvious defects. In principle, increasing the thickness of the permalloy plate can improve the shielding coefficient of the composite magnetic shielding structure. However, due to the limitations of lightweighting and performance of the magnetic shielding device, increasing the thickness of the permalloy plate can easily cause a decrease in the permeability of the nanocrystalline and permalloy composite structure, resulting in a weakening of the composite effect. More importantly, if the size of the permalloy plate is too large, the impact resistance of the overall magnetic shielding device structure will decrease. If the thickness of the permalloy plate is too small, the overall magnetic properties of the magnetic shielding structure will be reduced.

[0034] Nanocrystals possess high magnetic permeability and high saturation magnetic flux density, which are beneficial for improving the shielding coefficient of high-performance magnetic shielding devices using nanocrystals and permalloys under static magnetic fields and low-frequency alternating magnetic fields, reducing device weight, and broadening the shielding frequency domain. The nanocrystal magnetic shielding layer is composed of multiple layers of nanocrystal strips interlaced and bonded together. These multiple nanocrystal strips are laid sequentially along the thickness direction of the permalloy plate, and each strip is coated with a non-magnetic insulating adhesive 18 on one side for bonding between the strips. The nanocrystal strips in each layer are laid in the same direction, perpendicular to the laying direction of adjacent layers, to avoid magnetic leakage through gaps caused by all layers being laid in the same direction. In high-performance magnetic shielding devices, nanocrystal materials mainly provide shielding for static magnetic fields and low-frequency alternating magnetic fields; the non-magnetic insulating adhesive 18 serves as the bonding and insulation between the nanocrystal magnetic shielding layers. The system and composition of the nanocrystal strips are not limited, but good soft magnetic properties are required; the iron-based nanocrystal system 1K107B is preferred. The nanocrystalline magnetic shielding layer has an equivalent amplitude permeability of over 30,000 at a working frequency of 1 kHz. The thickness of the single-layer nanocrystalline ribbon 17 is 0.015-0.05 mm; the thickness of the non-magnetic insulating adhesive 18 is 0.003-0.01 mm, preferably 0.003-0.02 mm; the nanocrystalline magnetic shielding stacking factor is 0.5-0.95 mm, preferably 0.65-0.9.

[0035] Each nanocrystalline magnetic shielding layer requires an outermost nanocrystalline release film to prevent the nanocrystalline magnetic shielding layer from fragmentation, which would cause the magnetic permeability of the nanocrystalline material to decrease due to stress, thus reducing the shielding coefficient. Currently, the size of the single-layer nanocrystalline ribbon 17 is limited by the preparation technology and process. In this invention, the thickness of the single-layer nanocrystalline ribbon 17 and the nanocrystalline magnetic shielding stacking coefficient are limited. The non-magnetic insulating adhesive 18 between the nanocrystalline ribbons plays a bonding and insulating role. If the thickness of the non-magnetic insulating adhesive 18 is too small, it will increase the stacking coefficient and improve the shielding performance. However, if the thickness of the non-magnetic insulating adhesive 18 is too small, it will reduce the bonding effect between the nanocrystalline magnetic shielding layers and reduce reliability. If the thickness of the non-magnetic insulating adhesive 18 is too large, it will reduce the bottom coefficient of the nanocrystalline magnetic shielding layer, affecting the magnetic permeability and shielding effect of the nanocrystalline magnetic shielding layer. Therefore, the thickness of the single-layer nanocrystalline ribbon 17 and the non-magnetic insulating adhesive 18 in the nanocrystalline magnetic shielding layer need to be controlled within a certain range.

[0036] The non-magnetic fixing device between the high permeability magnetic shielding layers of the nanocrystalline and permalloy composite structure can be made by 3D printing of non-magnetic epoxy resin. The non-magnetic fixing device between the shielding layers mainly serves to fix the spacing between the high permeability magnetic shielding layers of the composite structure. The non-magnetic fixing device between the shielding layers is placed at the bottom inside the composite structure shielding device to maintain the spacing between the high permeability magnetic shielding layers of the composite structure.

[0037] Each non-magnetic pad is made of microporous non-magnetic silicone, which has the characteristics of flexibility, good thermal stability, chemical stability and high mechanical strength. Fine-porous silicone is preferred, which plays a flexible buffering role between the high magnetic permeability magnetic shielding layer and the non-magnetic fixing device.

[0038] In this invention, the shielding coefficient SF represents the shielding capability of the magnetic shielding device. The larger the shielding coefficient of a high-performance magnetic shielding device, the better its shielding effect. The static magnetic shielding coefficient SF of the magnetic shielding device... N-P The calculation formula is as follows:

[0039]

[0040] In the formula:

[0041] H0 represents the external magnetic field strength of the high-performance magnetic shielding device;

[0042] H S This indicates the strength of the magnetic field inside a high-performance magnetic shielding device.

[0043] R S This indicates the internal magnetic resistance of a high-performance magnetic shielding device;

[0044] R N-P,b This represents the equivalent magnetoresistance of the composite magnetic shielding structure along the direction of the magnetic field.

[0045] Eddy current elimination shielding coefficient SF under alternating magnetic field eddy The calculation formula is as follows:

[0046]

[0047] In the formula: δ represents skin depth; μ a,N-P The effective amplitude permeability of the composite structure is represented by μ0; the free permeability is represented by σ. N-P denoted by γ, r represents the equivalent conductivity of the composite structure; d represents the thickness of the composite structure; f represents the frequency; γ and K are two intermediate quantities in the calculation of the eddy current elimination shielding coefficient of the magnetic shielding device; x and y can be selected according to the shape of the magnetic shielding of the composite structure. For square high-performance magnetic shielding devices, x = 0.3 and y = 0.47 are preferred.

[0048] The above SF N-P and SF eddy These are formulas for calculating the static magnetic shielding coefficient and eddy current elimination shielding coefficient of single-layer high-performance magnetic shielding devices. For multi-layer composite structures, the corresponding magnetic characteristic parameters need to be substituted into the calculation formula. The calculation should be performed based on the number of layers, specific composite structure parameters, and the magnetic properties of the soft magnetic material. It is worth noting that under low-frequency alternating magnetic fields, magnetic flux shunting and eddy current elimination act simultaneously. The total shielding coefficient SF under low-frequency alternating magnetic fields needs to be calculated by substituting SF...N-P and SF eddy The coefficients are added together, and the data substituted into the formula under low-frequency alternating magnetic field are all soft magnetic material data measured under the corresponding frequency test conditions.

[0049] After the design of the high-performance magnetic shielding device with composite structure was completed, simulations were performed using the above calculation formulas to obtain the results for different nanocrystal thicknesses d in the high-performance magnetic shielding device with composite structure. N And the thickness d of the permalloy P Simulation diagram of shielding coefficient under varying conditions; Figure 5 A high-performance magnetic shielding device with a three-layer nanocrystal and permalloy composite structure, with different nanocrystal thicknesses d. N And the thickness d of the permalloy P Simulation results of the static magnetic shielding coefficient under varying conditions, with a shielding coefficient of approximately 1.3 × 10⁻⁶. 8 High-performance magnetic shielding devices have good shielding performance in static magnetic environments. Figure 6 For a high-performance magnetic shielding device with a three-layer nanocrystalline and permalloy composite structure, different nanocrystalline magnetic shielding layer thicknesses d are used. N The thickness d of the permalloy magnetic shielding layer P Simulation results of the shielding coefficient for a low-frequency alternating magnetic field with a frequency of 1kHz under varying conditions; the shielding coefficient is approximately 1.5 × 10⁻⁶. 7 The shielding performance of the high-performance magnetic shielding device under low-frequency alternation of 1kHz still meets the requirements.

[0050] In this embodiment, the multilayer nanocrystalline and permalloy composite high-permeability magnetic shielding layer includes three nanocrystalline and permalloy shielding layers. The nanocrystalline magnetic shielding layer uses iron-based nanocrystalline material 1K107B, and the permalloy shielding layer uses permalloy material 1J85. In other embodiments of this invention, the number of multiple layers in the multilayer nanocrystalline and permalloy composite high-permeability magnetic shielding layer is not limited; specifically, for example... Figure 1 , Figure 2 , Figure 3 , Figure 4 As shown, the three nanocrystalline and permalloy composite high-permeability magnetic shielding layers are respectively, from the outside to the inside, a first nanocrystalline and permalloy composite high-permeability magnetic shielding layer 1, a second nanocrystalline and permalloy composite high-permeability magnetic shielding layer 2, and a third nanocrystalline and permalloy composite high-permeability magnetic shielding layer 3. The first nanocrystalline magnetic shielding layer 5 of the first nanocrystalline and permalloy composite high-permeability magnetic shielding layer 1 is on the outermost side of the high-performance magnetic shielding device, and the third permalloy magnetic shielding layer 12 of the third nanocrystalline and permalloy composite high-permeability magnetic shielding layer 3 is on the innermost side of the high-performance magnetic shielding device. The three nanocrystalline and permalloy composite high-permeability magnetic shielding layers are used for magnetic flux diversion and eddy current elimination, so as to achieve shielding of static magnetic fields or low-frequency alternating magnetic fields.

[0051] Each nanocrystalline and permalloy composite high-permeability magnetic shielding layer has a corresponding sized end cap for a magnetic shielding device on one side. Specifically, the first nanocrystalline and permalloy composite high-permeability magnetic shielding layer 1 has a first-layer nanocrystalline and permalloy composite magnetic shielding device end cap on one side; the second nanocrystalline and permalloy composite high-permeability magnetic shielding layer 2 has a second-layer nanocrystalline and permalloy composite magnetic shielding device end cap on one side; and the third nanocrystalline and permalloy composite high-permeability magnetic shielding layer 3 has a third-layer nanocrystalline and permalloy composite magnetic shielding device end cap on one side. The nanocrystalline and permalloy composite high-permeability magnetic shielding layers and their corresponding end caps are in one-to-one correspondence, and there are strict tolerance requirements between the nanocrystalline and permalloy composite high-permeability magnetic shielding layers and their corresponding end caps to ensure normal disassembly of the end caps and to prevent magnetic leakage through gaps. Each nanocrystalline and permalloy composite structure end cap has a pre-drilled end cap test hole 20 for remanence testing. The end cap test hole 20 is located at the center of the end cap of the nanocrystalline and permalloy composite structure magnetic shielding device.

[0052] In this embodiment of the present disclosure, the non-magnetic fixing device between shielding layers is provided with limiting blocks 19 in three directions. The limiting blocks 19 are used to stabilize the position of the high magnetic permeability magnetic shielding layer of the nanocrystalline and permalloy composite structure. The non-magnetic fixing device between shielding layers includes a first non-magnetic fixing device 14 disposed above the first permalloy magnetic shielding layer 6 and a second non-magnetic fixing device 16 disposed above the second permalloy magnetic shielding layer 9. The non-magnetic pads include a first non-magnetic pad 13 disposed above the first non-magnetic fixing device 14 and a second non-magnetic pad 15 disposed above the second non-magnetic fixing device 16.

[0053] Specifically, the first non-magnetic fixing device 14 is located between the first permalloy magnetic shielding layer 6 and the first non-magnetic pad 13, that is, the bottom of the first non-magnetic fixing device 14 is above the first permalloy magnetic shielding layer 6 and below the first non-magnetic pad 13; the second non-magnetic fixing device 16 is located between the second permalloy magnetic shielding layer 9 and the second non-magnetic pad 15, that is, the bottom of the second non-magnetic fixing device 16 is above the second permalloy magnetic shielding layer 9 and below the second non-magnetic pad 15. The first non-magnetic pad 13 is located between the first non-magnetic fixing device 14 and the second nanocrystalline release film 7, that is, above the first non-magnetic fixing device 14 and below the second nanocrystalline release film 7; the second non-magnetic pad 15 is located between the second non-magnetic fixing device 16 and the third nanocrystalline release film 10, that is, the second non-magnetic pad 15 is placed above the second non-magnetic fixing device 16 and below the third nanocrystalline release film 10.

[0054] The second nanocrystalline magnetic shielding layer 8 is disposed outside the second permalloy magnetic shielding layer 9; the third nanocrystalline magnetic shielding layer 11 is disposed outside the third permalloy magnetic shielding layer 12.

[0055] In practical implementation, the thickness and number of nanocrystals and permalloy layers can be adjusted according to requirements, and the structure can be adjusted according to the shielding frequency range and target. It should be understood that the terms "upper," "lower," "bottom," "inner," and "outer," etc., indicate positional relationships or orientations and are only used for the convenience of describing the invention. They do not specifically refer to or imply the necessary orientation and operation of the device or accessory referred to, and should not be construed as limitations on the invention.

[0056] The embodiments described above are merely preferred embodiments of the present invention and are not intended to limit the scope of the present invention. Various modifications and improvements made by those skilled in the art to the technical solutions of the present invention without departing from the spirit of the present invention should fall within the protection scope defined by the claims of the present invention.

Claims

1. A high-performance magnetic shielding device based on a nanocrystalline and permalloy composite structure, characterized in that: It includes multiple high-permeability magnetic shielding layers with nanocrystalline and permalloy composite structures, nanocrystalline release film, non-magnetic fixing device between shielding layers, and non-magnetic pads; The high permeability magnetic shielding layer of the nanocrystalline and permalloy composite structure includes multiple high permeability nanocrystalline and permalloy composite structures nested from the inside to the outside, which are used to shield static magnetic fields through magnetic flux shunting and to shield low-frequency alternating magnetic fields through magnetic flux shunting and eddy current elimination. The bottom of the nanocrystalline magnetic shielding layer in the high permeability magnetic shielding layer of the nanocrystalline and permalloy composite structure is bonded to the outside of the permalloy magnetic shielding layer by the non-magnetic insulating adhesive of the nanocrystalline strip. The permalloy is inside the high permeability magnetic shielding layer of the nanocrystalline and permalloy composite structure, which realizes the mechanical support of the composite structure and the shielding of the extremely weak magnetic field after the attenuation of the magnetic field lines by the nanocrystalline layer. The nanocrystalline magnetic shielding layer comprises multiple layers of single-sided non-magnetic insulating adhesive nanocrystalline tapes laid crosswise. The nanocrystalline magnetic shielding layer is interconnected by the nanocrystalline tapes and the non-magnetic insulating adhesive, and the nanocrystalline tapes are laid in a crosswise manner. The nanocrystalline layer release film is placed above the nanocrystalline magnetic shielding layer to protect each of the nanocrystalline magnetic shielding layers from being crushed by force. The nanocrystalline magnetic shielding layer is tightly attached to the permalloy magnetic shielding layer. The non-magnetic fixing device between the shielding layers is set between the non-magnetic pad and the permalloy magnetic shielding layer to maintain the spacing between the high permeability magnetic shielding layers of the nanocrystalline and permalloy composite structure. The non-magnetic fixing device between the shielding layers is placed at the bottom of the high-performance magnetic shielding device and is closely attached to the permalloy magnetic shielding layer. The top of the non-magnetic fixing device between the shielding layers is closely connected to the non-magnetic pad. The non-magnetic pad is fixed above the non-magnetic fixing device between the shielding layers. The non-magnetic pad is made of non-magnetic silicone material. The top layer of the non-magnetic fixing device between the shielding layers is tightly bonded to the bottom layer of the non-magnetic pad. The top of the non-magnetic pad is used to support the nanocrystalline magnetic shielding layer and is tightly connected to the nanocrystalline layer release film on the outside of the high magnetic permeability magnetic shielding layer of the nanocrystalline and permalloy composite structure. It is used to isolate the nanocrystalline magnetic shielding layer from the non-magnetic fixing device between the shielding layers and to buffer the nanocrystalline magnetic shielding layer from the non-magnetic fixing device between the shielding layers. The nanocrystalline release film is placed outside the nanocrystalline magnetic shielding layer in the high permeability magnetic shielding layer of the nanocrystalline and permalloy composite structure. Its bottom is tightly bonded to the nanocrystalline magnetic shielding layer, and its outer side is tightly bonded to the non-magnetic pad. This avoids the nanocrystalline magnetic shielding layer from being in direct contact with the non-magnetic pad and being subjected to concentrated stress, which could lead to the fragmentation of the nanocrystalline material.

2. The high-performance magnetic shielding device based on a nanocrystalline and permalloy composite structure according to claim 1, characterized in that, Each layer of the high-permeability magnetic shielding layer composed of nanocrystalline and permalloy composite structures is equipped with a composite structure shielding end cap. Each composite structure shielding end cap has an end cap test hole, which is used by an instrument to measure the center residual magnetism of the high-performance magnetic shielding device composed of nanocrystalline and permalloy composite structures.

3. The high-performance magnetic shielding device based on a nanocrystalline and permalloy composite structure according to claim 1, characterized in that, The high-permeability magnetic shielding layer of the nanocrystalline and permalloy composite structure is a composite structure of nanocrystalline and permalloy. The nanocrystalline magnetic shielding layer uses 1K107B nanocrystalline material, and the permalloy layer uses 1J85 permalloy material. It plays a role in magnetic flux shunting under static magnetic field and magnetic flux shunting and eddy current elimination under low-frequency alternating magnetic field shielding.

4. The high-performance magnetic shielding device based on a nanocrystalline and permalloy composite structure according to claim 1, characterized in that, The stacking coefficient of the nanocrystalline magnetic shielding layer is not less than 0.5 and not more than 0.95, which is used to ensure the adhesion and reliability between the nanocrystalline strips in the nanocrystalline magnetic shielding layer. The nanocrystalline strips in the nanocrystalline magnetic shielding layer are laid in the same direction and are perpendicular to the laying direction of the adjacent layers to avoid magnetic leakage caused by laying in the same direction.

5. A high-performance magnetic shielding device based on a nanocrystalline and permalloy composite structure according to claim 1, characterized in that, The non-magnetic fixing device between shielding layers has limit blocks in three directions. The limit blocks are used to fix the position of the high magnetic permeability magnetic shielding layer of nanocrystal and permalloy composite structure. A non-magnetic pad is set above the non-magnetic fixing device between shielding layers to provide a flexible buffer between the device and the nanocrystal layer and prevent the nanocrystal from breaking.