Semiconductor device structure and fabrication method

By combining dry etching with a hard mask layer and an etching barrier layer using the Bosch process, a small-sized columnar structure is formed at the bottom of the deep cavity, solving the problem of corrosion damage to the step structure in the prior art and realizing the formation of a high-quality columnar structure in the deep trench.

CN117658054BActive Publication Date: 2026-11-17CSMC TECH FAB2 CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202211004913.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-08-22
Publication Date
2026-11-17
Estimated Expiration
2042-08-22

AI Technical Summary

Technical Problem

In existing technologies, when forming deep cavity structures, the stepped structure at the junction of the deep cavity and the small cavity is easily damaged during corrosion, causing the small-sized columnar structure to be corroded away, making it difficult to form a small-sized columnar structure at the bottom of the large cavity.

Method used

The Bosch dry etching process is used in combination with a hard mask layer and an etching barrier layer to form a deep trench and a small second pillar on the substrate through multiple etching steps. The hard mask layer acts as an etching barrier layer to ensure that the top of the second pillar maintains a right angle shape.

Benefits of technology

It has been achieved that small-sized second pillars can be formed in deep trenches of more than 20 micrometers, and the top of the second pillars maintains a good morphology, solving the problem of corrosion damage. The process is simple and low-cost.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117658054B_ABST
    Figure CN117658054B_ABST
Patent Text Reader

Abstract

This invention relates to a semiconductor device structure and its fabrication method. The method includes: obtaining a substrate, wherein a patterned hard mask layer is formed on a first surface of the substrate; forming a patterned first etch barrier layer on the hard mask layer and the substrate, the first etch barrier layer having trench windows; dry etching the substrate to a predetermined depth using a Bosch process to form trenches, wherein a first pillar is formed on the substrate below the first etch barrier layer adjacent to the trenches; removing the first etch barrier layer; dry etching the substrate using a Bosch process to form a cavity, wherein the first pillar is etched into a second pillar located at the bottom of the cavity, the hard mask layer serving as the etch barrier layer; the depth of the cavity is not less than 20 micrometers. This invention, combined with the Bosch process, achieves the formation of small-sized pillars in trenches deeper than 20 micrometers, and the top of the second pillar can maintain a near-right-angled, neat morphology. The process flow of this invention is simple and low-cost.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of semiconductor manufacturing, and in particular to a semiconductor device structure, and also to a method for processing the semiconductor device structure. Background Technology

[0002] In device structures such as microelectromechanical systems (MEMS), it is necessary to form deep cavity structures of varying depths. One deep cavity is a large cavity, and the other is a small cavity connected to the large cavity. The small cavity and the large cavity have different depths, forming a step at their interface. In an exemplary method for forming the aforementioned structure, during the second etching process, the step structure at the interface between the large and small cavities is damaged, resulting in an arc-shaped step, such as... Figure 1a and Figure 1b As shown. This means that if this method is used to construct a structure with small-sized columns inside a large cavity, the small-sized column structure will be corroded away due to the secondary corrosion damage to the steps, such as... Figure 2a and Figure 2b As shown. Summary of the Invention

[0003] Therefore, it is necessary to provide a method for fabricating semiconductor device structures that enables the formation of small-sized columnar structures at the bottom of large cavities.

[0004] A method for fabricating a semiconductor device structure includes: obtaining a substrate, wherein a patterned hard mask layer is formed on a first surface of the substrate; forming a patterned first etch barrier layer on the hard mask layer and the substrate, the first etch barrier layer having a trench window; dry etching the substrate to a predetermined depth using a Bosch process to form a trench, wherein a first pillar is formed on the substrate below the first etch barrier layer adjacent to the trench; removing the first etch barrier layer; dry etching the substrate using a Bosch process to form a cavity, wherein the first pillar is etched into a second pillar located at the bottom of the cavity, the hard mask layer serving as the etch barrier layer; and the depth of the cavity being not less than 20 micrometers.

[0005] The above-mentioned semiconductor device structure fabrication method, combined with the Bosch process, enables the formation of a small second pillar in a deep trench (i.e., cavity) of more than 20 micrometers, and the top of the second pillar can maintain a good morphology (i.e., the top of the second pillar has a neat structure that tends to be right angle).

[0006] In one embodiment, the height of the second column is 0.5 to 20 micrometers.

[0007] In one embodiment, the ratio of the depth of the cavity to the height of the second column is not less than 50.

[0008] In one embodiment, the step of forming a patterned first etch barrier layer on the hard mask layer and the substrate is to form a patterned photoresist layer by photolithography.

[0009] In one embodiment, the step of removing the first etch barrier layer includes removing the photoresist layer using a dry etching process.

[0010] In one embodiment, the etching gas used in the step of removing the photoresist layer using a dry etching process includes oxygen.

[0011] In one embodiment, the gas used in the step of removing the photoresist layer using a dry etching process includes oxygen and nitrogen to regulate the intensity of the reaction.

[0012] In one embodiment, the step of removing the photoresist layer using a dry etching process and the two steps of dry etching the substrate using the Bosch process are performed in the same etching apparatus.

[0013] In one embodiment, the reactive gases used in both steps of the Bosch process for dry etching the substrate include SF6 and C4F8.

[0014] In one embodiment, the material of the hard mask layer includes silicon oxide.

[0015] In one embodiment, the material of the hard mask layer includes silicon dioxide.

[0016] In one embodiment, the step of removing the hard mask layer is also included.

[0017] In one embodiment, the step of removing the hard mask layer is performed by wet etching or by using gaseous hydrofluoric acid to remove the hard mask layer.

[0018] In one embodiment, the trench window is mesh-like, thereby dividing the first etch barrier layer into multiple mesh openings.

[0019] It is also necessary to provide a semiconductor device structure.

[0020] A semiconductor device structure includes a cavity formed in a substrate and an uneven structure located at the bottom of the cavity. The semiconductor device structure is formed by the processing method described in any of the foregoing embodiments. The uneven structure includes a second pillar.

[0021] In one embodiment, the height of the second column is 0.5 to 20 micrometers.

[0022] In one embodiment, the ratio of the depth of the cavity to the height of the second column is not less than 50.

[0023] In one embodiment, the groove is mesh-like and the second column is cylindrical.

[0024] The aforementioned semiconductor device structure achieves the formation of a small second pillar in a deep trench (i.e., cavity) of more than 20 micrometers using the Bosch process, and the top of the second pillar can maintain a good morphology (i.e., the top of the second pillar has a neat structure that tends to be right angle). Attached Figure Description

[0025] To better describe and illustrate embodiments and / or examples of the inventions disclosed herein, reference may be made to one or more accompanying drawings. Additional details or examples used to describe the drawings should not be considered as limiting the scope of any of the disclosed inventions, the currently described embodiments and / or examples, or the best mode of these inventions as currently understood.

[0026] Figure 1a This is a schematic diagram of an ideal morphology of a deep cavity structure consisting of large cavities connected to smaller cavities. Figure 1b It is formed using an exemplary two-stage etching method. Figure 1a A schematic diagram of the actual structure obtained when the structure shown is presented.

[0027] Figure 2a This is a schematic diagram of an ideal morphology of a semiconductor device structure that uses a columnar structure formed at the bottom of a large cavity. Figure 2b It is formed using an exemplary two-stage etching method. Figure 2a A schematic diagram of the actual structure obtained when the structure shown is presented.

[0028] Figure 3 This is a flowchart of a method for fabricating a semiconductor device structure according to an embodiment of this application;

[0029] Figures 4a to 4g Is adopted Figure 3 A schematic cross-sectional view of the semiconductor device structure during processing in one embodiment of the method shown;

[0030] Figure 5 These are a top view and a cross-sectional view of a semiconductor device structure according to an embodiment of this application;

[0031] Figure 6a This is a microscope photograph of a semiconductor device structure according to an embodiment of this application; Figure 6b yes Figure 6a A magnified view of the central ellipse. Detailed Implementation

[0032] To facilitate understanding of the present invention, a more complete description will be given below with reference to the accompanying drawings. Preferred embodiments of the invention are shown in the drawings. However, the invention can be implemented in many different forms and is not limited to the embodiments described herein. Rather, these embodiments are provided so that this disclosure will be thorough and complete.

[0033] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this invention pertains. The terminology used herein in the description of the invention is for the purpose of describing particular embodiments only and is not intended to be limiting of the invention. The term "and / or" as used herein includes any and all combinations of one or more of the associated listed items.

[0034] It should be understood that when an element or layer is referred to as "on," "adjacent to," "connected to," or "coupled to" other elements or layers, it may be directly on, adjacent to, connected to, or coupled to other elements or layers, or there may be intervening elements or layers. Conversely, when an element is referred to as "directly on," "directly adjacent to," "directly connected to," or "directly coupled to" other elements or layers, there are no intervening elements or layers. It should be understood that although the terms first, second, third, etc., may be used to describe various elements, components, areas, layers, and / or portions, these elements, components, areas, layers, and / or portions should not be limited by these terms. These terms are only used to distinguish one element, component, area, layer, or portion from another element, component, area, layer, or portion. Therefore, without departing from the teachings of this invention, the first element, component, area, layer, or portion discussed below may be referred to as the second element, component, area, layer, or portion.

[0035] Spatial relation terms such as “below,” “under,” “below,” “under,” “above,” “above,” etc., are used herein for convenience of description to describe the relationship between one element or feature shown in the figure and other elements or features. It should be understood that, in addition to the orientation shown in the figure, spatial relation terms are intended to also include different orientations of the device in use and operation. For example, if the device in the figure is flipped, then the element or feature described as “below” or “under” the other element or feature will be oriented “above” the other element or feature. Therefore, the exemplary terms “below” and “under” can include both upper and lower orientations. The device may be otherwise oriented (rotated 90 degrees or otherwise) and the spatial descriptive terms used herein will be interpreted accordingly.

[0036] The terminology used herein is for the purpose of describing particular embodiments only and is not intended to limit the invention. When used herein, the singular forms “a,” “an,” and “the” are also intended to include the plural forms unless the context clearly indicates otherwise. It should also be understood that the terms “comprising” and / or “including,” when used in this specification, identify the presence of the stated features, integers, steps, operations, elements, and / or components, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components, and / or groups. When used herein, the term “and / or” includes any and all combinations of the associated listed items.

[0037] Embodiments of the invention are described herein with reference to cross-sectional views that serve as schematic diagrams of ideal embodiments (and intermediate structures). Thus, variations in the shape shown can be anticipated due to, for example, manufacturing techniques and / or tolerances. Therefore, embodiments of the invention should not be limited to the specific shapes of the regions shown herein, but include shape deviations due to, for example, manufacturing processes. For example, implantation regions shown as rectangular typically have rounded or curved features at their edges and / or implantation concentration gradients, rather than a binary change from implantation regions to non-implantation regions. Similarly, the buried regions formed by implantation can result in some implantation in the region between the buried region and the surface traversed during implantation. Therefore, the regions shown in the figures are substantially schematic, and their shapes are not intended to show the actual shapes of the regions of the device and are not intended to limit the scope of the invention.

[0038] The semiconductor terminology used in this article is the technical terminology commonly used by those skilled in the art. For example, for P-type and N-type impurities, in order to distinguish the doping concentration, P+ type represents heavily doped P-type, P type represents moderately doped P-type, P- type represents lightly doped P-type, N+ type represents heavily doped N-type, N type represents moderately doped N-type, and N- type represents lightly doped N-type.

[0039] This application provides a method for fabricating a semiconductor device structure that can form a small-sized cylindrical structure at the bottom of a cavity. Figure 3 This is a flowchart of a method for fabricating a semiconductor device structure according to an embodiment of this application, including the following steps:

[0040] S310, Obtain the substrate, the first surface of which has a patterned hard mask layer formed.

[0041] In one embodiment of this application, a wafer substrate 410 is first obtained, and then a hard mask layer 422 is formed on the front side of the substrate 410, as shown in the figure. Figure 4aThe wafer substrate 410 includes a semiconductor substrate. In one embodiment of this application, the semiconductor substrate material may be undoped single-crystal silicon, doped single-crystal silicon, silicon-on-insulator (SOI), silicon-on-insulator stacked (SSOI), silicon-on-insulator stacked (S-SiGeOI), silicon-on-insulator (SiGeOI), and germanium-on-insulator (GeOI), etc., and may also be at least one of the following materials: Si, Ge, SiGe, SiC, SiGeC, InAs, GaAs, InP, or other III / V compound semiconductors. Figure 4a In the illustrated embodiment, the substrate is made of monocrystalline silicon. Devices, such as NMOS and / or PMOS transistors, can be formed on the substrate. Correspondingly, conductive components can also be formed in the substrate. These conductive components can be the gate, source, or drain of a transistor, or a metal interconnect structure electrically connected to the transistor, etc. Furthermore, isolation structures such as STI (shallow trench isolation) can be formed on the substrate.

[0042] In one embodiment of this application, the hard mask layer 422 is made of silicon oxide, such as silicon dioxide. This silicon dioxide layer can be formed by thermal oxidation or deposition.

[0043] In one embodiment of this application, the patterning of the hard mask layer 422 can be accomplished by photolithography followed by etching. Specifically, a layer of photoresist is coated on the upper surface of the hard mask layer 422, and then exposed using a corresponding photomask followed by development. After development, the remaining photoresist layer 492 exposes the hard mask layer 422 that needs to be etched away. The exposed hard mask layer 422 is then etched away using an etching process. See [link to relevant documentation]. Figure 4b .

[0044] S320, a patterned first etch barrier layer is formed on the hard mask layer and the substrate.

[0045] In one embodiment of this application, the photoresist layer 492 needs to be removed before step S320 is performed. See also Figure 4c The first etch barrier layer 494 has a trench window 493. In one embodiment of this application, the first etch barrier layer 494 is a photoresist layer, which can be obtained by coating a layer of photoresist on the hard mask layer 422 and the substrate 410, and then exposing it with a corresponding photomask and developing it.

[0046] S330 uses Bosch dry etching technology to etch the substrate to a predetermined depth, forming trenches and the first pillar.

[0047] The area not covered by the first etch barrier layer 494 is etched to form a trench 411, while the area covered by the first etch barrier layer 494 is protected by the first etch barrier layer 494, forming a first pillar 412 adjacent to the trench 411. See [link / reference] Figure 4d .

[0048] The Bosch process, first proposed by Robert Bosch, is a technique used to prevent or mitigate lateral etching by depositing a thin etched film on the lateral sidewalls of the etched surface. This process first uses fluorine-based active groups to etch silicon, followed by sidewall passivation; the etching and passivation steps are performed alternately. Etching and passivation are achieved by alternating etching and passivation gases in the etching equipment. In one embodiment of this application, the etching gas in step S330 of the Bosch process is SF6, and the passivation gas is C4F8. C4F8 can form fluorinated carbon polymers in plasma, which, when deposited on the silicon surface, prevent the reaction between fluoride ions and silicon. Etching and passivation can be cycled every 5 to 10 seconds, with the newly etched silicon surface being passivated immediately after a short period of isotropic etching. Due to the physical sputtering bombardment of ions in the depth direction, the passivation film can be retained, thus preventing lateral etching in the next etching cycle. This periodic "etch-passivation-etch" process ensures that etching only occurs along the depth direction.

[0049] S340, remove the first etch barrier layer.

[0050] Figure 4e This is a schematic cross-sectional view of the device after adhesive removal in one embodiment.

[0051] In the S350, the substrate is dry-etched using the Bosch process, and the first pillar is etched into the second pillar.

[0052] The hard mask layer 422 acts as a barrier layer for etching, and the trench 411 is etched further downwards, with a portion of the first pillar 412 being etched away, forming a second pillar 414 at the bottom of the cavity 41. This application forms small-sized pillar structures within a deep trench, with the depth h of the cavity 41 not less than 20 micrometers. In one embodiment of this application, the reaction gases in step S350 of the Bosch process also include SF6 (etching gas) and C4F8 (passivation gas). See also... Figure 4f After step S350 is completed, a concave-convex structure consisting of a second column 414 and a groove 411 is finally formed at the bottom of the cavity 41.

[0053] The aforementioned semiconductor device structure fabrication method, combined with Bosch technology, enables the formation of a small-sized second pillar within a deep trench (i.e., cavity 41) exceeding 20 micrometers, while maintaining a good morphology at the top of the second pillar (i.e., the top of the second pillar has a neat, near-right-angled structure). Furthermore, the method boasts a simple process flow and low cost.

[0054] In one embodiment of this application, the height of the second pillar 414 is 0.5 to 20 micrometers. The height of the second pillar 414 is adjustable, therefore the above-described semiconductor device structure fabrication method has broad application prospects.

[0055] The above-mentioned semiconductor device structure fabrication method using Bosch process can even form a deep trench small silicon pillar structure with a cavity depth h to a second pillar 414 ratio greater than 50:1. For example, the cavity depth h is 50 micrometers and the second pillar 414 is 1 micrometer.

[0056] In one embodiment of this application, after step S350, a step of removing the hard mask layer 422 is further included. The semiconductor device structure obtained after removing the hard mask layer 422 is as follows: Figure 4g As shown.

[0057] In one embodiment of this application, the hard mask layer 422 can be removed by wet etching. The etchant used for wet etching of the hard mask layer 422 can be a BOE (Buffered Oxide Etch) solution. In another embodiment of this application, the hard mask layer 422 can be removed by VHF (vaporized hydrofluoric acid).

[0058] In one embodiment of this application, the patterning of the hard mask layer 422 is accomplished by a dry etching process.

[0059] In one embodiment of this application, the photoresist layer 492 is removed by a dry stripping process and a wet stripping process.

[0060] In one embodiment of this application, the removal of the photoresist layer (first etch barrier layer 494) in step S340 is performed using a dry etching process. Since steps S330, S340, and S350 all employ dry etching, these three steps can be performed in the same etching equipment, and the photoresist removal in step S340 is an in-situ strip.

[0061] In one embodiment of this application, the etching gas used in step S340, dry etching to remove the photoresist layer, is oxygen. In another embodiment of this application, step S340, dry etching to remove the photoresist layer, can use a mixture of oxygen and nitrogen, where nitrogen can be used to regulate the intensity of the etching reaction.

[0062] Figure 5 These are top and cross-sectional views of the semiconductor device structure obtained after removing the hard mask layer 422 in one embodiment of this application. In this embodiment, the trench window 493 formed in step S320 is a mesh, and the corresponding first etch barrier layer 494, serving as the mesh opening, is circular and arranged in an array. The second pillar 414 in the resulting semiconductor device structure is cylindrical. In other embodiments, the first etch barrier layer 422, serving as the mesh opening, can also be a square hole or other shaped hole, thereby obtaining a second pillar 414 of other shapes accordingly.

[0063] Figure 6a This is a microscope image of the semiconductor device structure obtained after removing the hard mask layer 422 in one embodiment of this application. Figure 6b yes Figure 6a A magnified view of the central ellipse.

[0064] The above-mentioned semiconductor device structure fabrication method can also be used to prepare other similar structures, such as Si substrates and silicon dioxide films.

[0065] This application correspondingly provides a semiconductor device structure, which can be formed by the processing method of the semiconductor device structure described in any of the foregoing embodiments. See also Figure 4g A cavity 41 is formed in the substrate 410 of the semiconductor device structure. The bottom of the cavity 41 has an uneven structure composed of trenches 411 and second pillars 414. The depth h of the cavity 41 is not less than 20 micrometers. In one embodiment of this application, the trenches 411 are mesh-like, and the second pillars 414 are cylindrical.

[0066] The aforementioned semiconductor device structure achieves the formation of a small second pillar in a deep trench (i.e., cavity 41) of more than 20 micrometers using the Bosch process, and the top of the second pillar can maintain a good morphology (i.e., the top of the second pillar has a neat structure that tends to be right angle).

[0067] The substrate 410 includes a semiconductor substrate. In one embodiment of this application, the semiconductor substrate material may be undoped single-crystal silicon, doped single-crystal silicon, silicon-on-insulator (SOI), silicon-on-insulator stacked (SSOI), silicon-on-insulator stacked (S-SiGeOI), silicon-on-insulator (SiGeOI), and germanium-on-insulator (GeOI), etc., and may also be at least one of the following materials: Si, Ge, SiGe, SiC, SiGeC, InAs, GaAs, InP, or other III / V compound semiconductors. Figure 4gIn the illustrated embodiment, the substrate is made of monocrystalline silicon. Devices, such as NMOS and / or PMOS transistors, can be formed on the substrate. Correspondingly, conductive components can also be formed in the substrate. These conductive components can be the gate, source, or drain of a transistor, or a metal interconnect structure electrically connected to the transistor, etc. Furthermore, isolation structures such as STI (shallow trench isolation) can be formed on the substrate.

[0068] Figure 5 These are top and cross-sectional views of a semiconductor device structure according to one embodiment of this application. In this embodiment, the second pillar 414 is a cylinder and is arranged in an array. In other embodiments, the second pillar 414 may also be a square pillar or other shaped pillar structure.

[0069] In one embodiment of this application, the height of the second column 414 is 0.5 to 20 micrometers.

[0070] In one embodiment of this application, the ratio of the depth h of the cavity 41 to the height of the second column 414 is not less than 50.

[0071] It should be understood that although the steps in the flowchart of this application are shown sequentially as indicated by the arrows, these steps are not necessarily executed in the order indicated by the arrows. Unless explicitly stated herein, there is no strict order restriction on the execution of these steps, and they can be executed in other orders. Moreover, at least some steps in the flowchart of this application may include multiple steps or multiple stages, which are not necessarily completed at the same time, but may be executed at different times, and the execution order of these steps or stages is not necessarily sequential, but may be performed alternately or in turn with other steps or at least some of the steps or stages of other steps.

[0072] In the description of this specification, references to terms such as "some embodiments," "other embodiments," and "ideal embodiments" indicate that a specific feature, structure, material, or characteristic described in connection with that embodiment or example is included in at least one embodiment or example of the invention. In this specification, the illustrative descriptions of the above terms do not necessarily refer to the same embodiments or examples.

[0073] The technical features of the above embodiments can be combined in any way. For the sake of brevity, not all possible combinations of the technical features of the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0074] The embodiments described above are merely illustrative of several implementation methods of this application, and while the descriptions are relatively specific and detailed, they should not be construed as limiting the scope of the patent application. It should be noted that those skilled in the art can make various modifications and improvements without departing from the concept of this application, and these all fall within the protection scope of this application. Therefore, the protection scope of this patent application should be determined by the appended claims.

Claims

1. A method for fabricating a semiconductor device structure, comprising: A substrate is obtained, wherein a patterned hard mask layer is formed on the first surface of the substrate; A patterned first etch barrier layer is formed on the hard mask layer and the substrate, the first etch barrier layer having a trench window; The substrate is dry-etched to a predetermined depth using the Bosch process to form trenches, and a first pillar is formed on the substrate below the first etching barrier layer adjacent to the trenches. Remove the first etch barrier layer; The substrate is dry-etched using the Bosch process to form a cavity. The first pillar is etched into a second pillar located at the bottom of the cavity. The material removed from the first pillar by etching is the same as the material of the second pillar. The hard mask layer serves as a barrier layer for etching. The depth of the cavity is not less than 20 micrometers.

2. The method for fabricating a semiconductor device structure according to claim 1, characterized in that, The height of the second column is 0.5 to 20 micrometers; and / or the ratio of the depth of the cavity to the height of the second column is not less than 50.

3. The method for fabricating a semiconductor device structure according to claim 1, characterized in that, The step of forming a patterned first etch barrier layer on the hard mask layer and the substrate is to form a patterned photoresist layer by photolithography.

4. The method for fabricating a semiconductor device structure according to claim 3, characterized in that, The step of removing the first etch barrier layer includes removing the photoresist layer using a dry etching process.

5. The method for fabricating a semiconductor device structure according to claim 4, characterized in that, The etching gas used in the step of removing the photoresist layer using a dry etching process includes oxygen.

6. The method for fabricating a semiconductor device structure according to claim 4, characterized in that, The steps of removing the photoresist layer using a dry etching process and the two steps of dry etching the substrate using the Bosch process are performed in the same etching equipment.

7. The method for fabricating a semiconductor device structure according to claim 1, characterized in that, The reactive gases used in both steps of the Bosch process for dry etching the substrate include SF6 and C4F8.

8. The method for fabricating a semiconductor device structure according to claim 1, characterized in that, The material of the hard mask layer includes silicon oxide.

9. The method for fabricating a semiconductor device structure according to claim 1, characterized in that, It also includes the step of removing the hard mask layer.

10. A semiconductor device structure, wherein a cavity and an uneven structure are formed in a substrate of the semiconductor device structure, characterized in that, The semiconductor device structure is formed by the semiconductor device structure processing method as described in any one of claims 1-9, and the concave-convex structure includes the second pillar.

Citation Information

Patent Citations

  • Method for manufacturing shallow trench isolation structure

    CN103515286A

  • Mask blank, method for manufacturing phase shift mask, and method for manufacturing semiconductor device

    US20180299767A1