A cable sheath production method based on a pre-compensation mechanism and a pre-compensation device
By establishing a mapping model to calculate the pre-compensation value and automatically adjusting the position of the die head, the problem of relying on manual adjustment for sheath concentricity in optical cable production was solved, achieving material savings and consistent quality.
Patent Information
- Application Number
- CN202311644913.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-04
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2043-12-04
AI Technical Summary
In current optical cable production, the adjustment of sheath concentricity relies on manual experience, which leads to low efficiency and easily results in sheaths that are too thick or too thin, causing material waste and inconsistent optical cable performance.
By acquiring parameters such as melt index, density, shrinkage rate, and processing temperature of the processed material, a mapping model is established, pre-compensation values are calculated, and the die head position is automatically adjusted to achieve precise control of the sheath concentricity. This is a cable sheath production method and device that adopts a pre-compensation mechanism.
This achieves precise control of sheath concentricity, reduces material waste, improves production efficiency, and ensures consistent optical cable quality.
Smart Images

Figure CN117669080B_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of novel optical cable manufacturing, and more specifically, relates to a sheath concentricity pre-compensation algorithm and device. Background Technology
[0002] In optical cable production, the sheath plays a crucial role in improving the cable's lateral pressure resistance, moisture resistance, and tensile strength. The thickness of the sheath is designed according to different cable types and application environments. An excessively thin sheath will affect the cable's performance and lifespan, while an excessively thick sheath will result in material waste and an increased cable diameter, hindering installation. Optical cable production utilizes a thermoforming process, where the sheath material is extruded through the gap between the core and the cover using an extruder. The distance between the core and the cover determines the cable's concentricity. Only by properly adjusting the cable's concentricity can design standards be met while maximizing material savings.
[0003] Due to the influence of gravity, the distance between the mold core and the mold cover directly above the machine head needs to be slightly larger than that directly below the machine head, requiring pre-compensation during concentricity adjustment. In the current optical cable production process, optical cable concentricity is generally adjusted manually, which is inefficient and requires high skill from operators, easily leading to situations where the sheath is too thick or too thin, causing losses. Summary of the Invention
[0004] To address the aforementioned deficiencies or improvement needs of existing technologies, this invention provides a cable sheath production method and pre-compensation device based on a pre-compensation mechanism. The purpose is to obtain the mapping between processing parameters and pre-compensation values of the processing material during mold assembly, based on multiple sets of processing parameters and corresponding pre-compensation values of the processing material. The optimal installation position of the mold head is calculated through this mapping, and a scanning device is used to solve the technical problem in optical cable sheath production where manual experience is required to adjust the mold position to adjust the sheath concentricity, and the resulting material loss due to inconsistent sheath concentricity.
[0005] To achieve the above objectives, according to one aspect of the present invention, a method for producing cable sheaths based on a pre-compensation mechanism is provided, characterized by comprising the following steps:
[0006] (1) For the die head of the target extruder, obtain the die distance; the distance is half of the difference between the outer diameter of the die core and the inner diameter of the die cover of the target extruder die head;
[0007] (2) Using the target extruder, processing experiments were conducted on the processed material under different production conditions to obtain processing experiment sampling data when the concentricity of the sheath met the design requirements; the processing experiment sampling data included the melt index, density, shrinkage rate, processing temperature and its corresponding pre-compensation value of the processed material;
[0008] The pre-compensation value is the difference between the distance between the upper edge of the outer side of the mold core and the upper edge of the inner side of the mold cover and the fixed distance when the concentricity of the sheath meets the design requirements.
[0009] (3) Based on the processing experiment sampling data obtained in step (2), fit the mapping model of melt index, density, shrinkage rate, processing temperature and fixed distance to pre-compensation value of the processing material:
[0010] X = f(MI,ρ,η,T,Y)
[0011] Where X is the pre-compensation value, MI is the melt index, ρ is the density, η is the shrinkage rate, T is the processing temperature, and Y is the constant distance;
[0012] (4) For actual production conditions, obtain the melt index, density, shrinkage rate and processing temperature parameters of the production material, and calculate the pre-compensation value of the target extruder die head according to the mapping model obtained in step (3);
[0013] (5) Adjust the position of the die core and / or die cover of the target extruder die head so that the distance between the upper edge of the outer side of the die core and the upper edge of the inner side of the die cover is equal to the fixed distance plus the pre-compensation value calculated in step (4). Perform pre-compensation adjustment and use the adjusted target extruder for sheath extrusion processing.
[0014] Preferably, in the cable sheath production method based on the pre-compensation mechanism, the pre-compensation value in the mapping model of step (3) is positively correlated with melt index, density, shrinkage rate and processing temperature.
[0015] Preferably, in the cable sheath production method based on the pre-compensation mechanism, the pre-compensation value and the distance of the mold in step (3) of the mapping model are linearly positively correlated.
[0016] Preferably, in the cable sheath production method based on the pre-compensation mechanism, step (3) uses the following function to fit the data:
[0017] X=(a×MI+b×ρ+c×η+d×T)×Y×f
[0018] Where a, b, c, d, and f are the fitting parameters.
[0019] According to another aspect of the present invention, a pre-compensation device for cable sheath production based on a pre-compensation mechanism is provided, which includes a mapping model acquisition module and a pre-compensation value calculation module.
[0020] The mapping model acquisition module is used to fit the processing experiment sampling data to obtain a mapping model of the melt index, density, shrinkage rate, processing temperature, and distance to the pre-compensation value of the processed material, and submit it to the pre-compensation value calculation module; the distance is half of the difference between the outer diameter of the die core of the target extruder die head and the inner diameter of the die cover.
[0021] The pre-compensation value calculation module is used to obtain the melt index, density, shrinkage rate and processing temperature parameters of the production material and input them into the mapping model to calculate the pre-compensation value of the processed material under actual production conditions.
[0022] Preferably, in the cable sheath production pre-compensation device based on the pre-compensation mechanism, the mapping model of the mapping model acquisition module is obtained through the following steps:
[0023] (S1) Use the processing device to measure and sample production data of the processing material under different production conditions to achieve the design requirements for the concentricity of the sheath. Obtain the melt index, density, shrinkage rate, processing temperature T and its corresponding pre-compensation value of the processing material.
[0024] (S2) Fit the melt index, density, shrinkage rate, processing temperature, and corresponding pre-compensation value data of the preset quantity of products produced by the mold at a preset distance obtained in step (S1) to obtain the mapping of melt index, density, shrinkage rate, processing temperature, and preset distance to the pre-compensation value:
[0025] X = f(MI, ρ, η, T, Y)
[0026] Where X is the pre-compensation value, MI is the melt index, ρ is the density, η is the shrinkage rate, T is the processing temperature, and Y is the constant distance.
[0027] Preferably, in the cable sheath production pre-compensation device based on the pre-compensation mechanism, the pre-compensation value in the pre-compensation value calculation model is positively correlated with melt index, density, shrinkage rate and processing temperature.
[0028] Preferably, in the cable sheath production pre-compensation device based on the pre-compensation mechanism, the pre-compensation value and the distance Y between the mold cover and the mold core are linearly positively correlated in the pre-compensation value calculation model.
[0029] Preferably, the pre-compensation value calculation model of the cable sheath production pre-compensation device based on the pre-compensation mechanism is fitted using the following function:
[0030] X=(a×MI+b×ρ+c×η+d×T)×Y×f
[0031] Where a, b, c, d, and f are the fitting parameters.
[0032] Preferably, the cable sheath production pre-compensation device based on the pre-compensation mechanism further includes a position recognition module and a mold adjustment module; wherein:
[0033] The position recognition module is used to obtain the position information of the mold core and the mold cover, and calculate the distance and submit it to the mapping model acquisition module;
[0034] The mold adjustment module is used to calculate the target position of the mold cover and / or mold core according to the pre-compensation value, so that the distance between the upper edge of the outer side of the mold core and the upper edge of the inner side of the mold cover is equal to the fixed distance plus the pre-compensation value.
[0035] Overall, compared with the prior art, the above-described technical solutions conceived by this invention, when assembling the mold, determine the mapping between processing data and pre-compensation value based on the processing data of different materials, and calculate the pre-compensation value. The concentricity of the cable sheath produced based on the calculated pre-compensation value can reach the preset state. Furthermore, for the same extruder, only one processing experiment is needed to perform pre-compensation for different working conditions, eliminating the need for repeated adjustments that would lead to material waste, thus achieving significant material savings. Attached Figure Description
[0036] Figure 1 This is a schematic diagram of the die head for producing the sheath;
[0037] Figure 2 This is a mapping model fitting result diagram of the cable sheath production method based on pre-compensated matrix provided in Embodiment 1 of the present invention;
[0038] Figure 3 This is a mapping model fitting result diagram of the cable sheath production method based on pre-compensated matrix provided in Embodiment 2 of the present invention.
[0039] In all the accompanying drawings, the same reference numerals are used to denote the same elements or structures, wherein: 1 is the die head, 2 is the flow divider cone, 3 is the mold core, 4 is the mold cover, and 5 is the die head nut. Detailed Implementation
[0040] To make the objectives, technical solutions, and advantages of this invention clearer, the invention will be further described in detail below with reference to embodiments. It should be understood that the specific embodiments described herein are merely illustrative and not intended to limit the invention. Furthermore, the technical features involved in the various embodiments of this invention described below can be combined with each other as long as they do not conflict with each other.
[0041] Optical cable production utilizes a thermoforming process, where the sheath material is extruded from the gap between the core and the cover using an extruder. The spacing between the core and the cover determines the concentricity of the optical cable, and this spacing is easily adjusted to be circumferentially consistent. However, due to the influence of gravity, pre-compensation is required during concentricity adjustment. This means that the spacing between the core and the cover directly above the extruder head needs to be slightly larger than that directly below the extruder head, ensuring that the sheath's concentricity meets product standards upon completion.
[0042] This invention provides a cable sheath production method based on a pre-compensation mechanism. Through repeated practice, it has been confirmed that the main factors affecting the processing performance of the sheath material are its thermodynamic properties, which are closely related to the extrusion and molding processes. These include the melt index, shrinkage rate, density, and processing temperature of the sheath material. Therefore, it is necessary to first obtain the mapping relationship between the pre-compensation value for sheath production and the material processing performance, calculate the pre-compensation value, and pre-compensate the sheath production line based on the pre-compensation value. The specific steps are as follows:
[0043] (1) For the die head of the target extruder, obtain the die distance; the die distance is half of the difference between the outer diameter of the die core and the inner diameter of the die cover of the target extruder die head; that is, the die distance Y = (inner diameter of die cover - outer diameter of die core) / 2;
[0044] (2) Using the target extruder, processing experiments were conducted on the processed material under different production conditions to obtain processing experiment sampling data when the concentricity of the sheath met the design requirements; the processing experiment sampling data included the melt index, density, shrinkage rate, processing temperature and its corresponding pre-compensation value of the processed material;
[0045] Melt index (MI): the weight of a thermoplastic melt passing through a standard capillary tube in ten minutes under certain temperature and pressure, expressed as MI (g / 10min); shrinkage rate is expressed as η; material density is expressed as ρ; processing temperature is T℃.
[0046] (3) Based on the processing experiment sampling data obtained in step (2), fit the mapping model of melt index, density, shrinkage rate, processing temperature and fixed distance to pre-compensation value of the processing material:
[0047] X = f(MI, ρ, η, T, Y)
[0048] Where X is the pre-compensation value, MI is the melt index, ρ is the density, η is the shrinkage rate, T is the processing temperature, and Y is the constant distance;
[0049] Preferably, the pre-compensation value is positively correlated with melt index, density, shrinkage rate, and processing temperature;
[0050] Preferably, under the same melt index, density, shrinkage rate, and processing temperature conditions, using molds with different spacings, the pre-compensation value can be obtained only under the condition of different spacings, and the pre-compensation value and the spacing of the mold can be linearly positively correlated.
[0051] Preferably, since the pre-compensation value melt index, density, shrinkage rate, and processing temperature are positively correlated, and the pre-compensation value and the die's constant distance are linearly positively correlated, the following function is used to fit the data:
[0052] X=(a×MI+b×ρ+c×η+d×T)×Y×f
[0053] Where a, b, c, d, and f are the fitting parameters.
[0054] (4) For actual production conditions, obtain the melt index, density, shrinkage rate and processing temperature parameters of the production material, and calculate the pre-compensation value of the target extruder die head according to the mapping model obtained in step (3);
[0055] (5) Adjust the position of the die core and / or die cover of the target extruder die head so that the distance between the upper edge of the outer side of the die core and the upper edge of the inner side of the die cover is equal to the fixed distance plus the pre-compensation value calculated in step (4). Perform pre-compensation adjustment and use the adjusted target extruder for sheath extrusion processing.
[0056] The cable sheath production pre-compensation device based on the pre-compensation mechanism provided by the present invention completes the function of obtaining the pre-compensation value for specific sheath production equipment, including a mapping model acquisition module and a pre-compensation value calculation module.
[0057] The mapping model acquisition module is used to fit the processing experiment sampling data to obtain a mapping model of the melt index, density, shrinkage rate, processing temperature, and distance to the pre-compensation value of the processed material, and submit it to the pre-compensation value calculation module; the distance is half of the difference between the outer diameter of the die core of the target extruder die head and the inner diameter of the die cover.
[0058] The pre-compensation value calculation module is used to obtain the melt index, density, shrinkage rate and processing temperature parameters of the production material and input them into the mapping model to calculate the pre-compensation value of the processed material under actual production conditions.
[0059] Preferably, the pre-mapping model of the mapping model acquisition module is obtained through the following steps:
[0060] (S1) Use the processing device to measure and sample production data of the processing material under different production conditions to achieve the design requirements for the concentricity of the sheath. Obtain the melt index, density, shrinkage rate, processing temperature T and its corresponding pre-compensation value of the processing material.
[0061] (S1) Use the processing device to measure and sample production data of the processing material under different production conditions to achieve the design requirements for the concentricity of the sheath. Obtain the melt index, density, shrinkage rate, processing temperature T and its corresponding pre-compensation value of the processing material.
[0062] X = f(MI, ρ, η, T, Y)
[0063] Where X is the pre-compensation value, MI is the melt index, ρ is the density, η is the shrinkage rate, T is the processing temperature, and Y is the constant distance.
[0064] Preferably, in the pre-compensation value calculation model, the pre-compensation value and the distance Y between the mold cover and the mold core have a linear positive correlation.
[0065] Preferably, under the same melt index, density, shrinkage rate and processing temperature conditions, using molds with different spacings, the pre-compensation value is obtained only under the condition of different spacings. In the pre-compensation value calculation model, the pre-compensation value and the spacing Y between the mold cover and the mold core are linearly positively correlated.
[0066] Preferably, since the pre-compensation value is positively correlated with melt index, density, shrinkage rate, and processing temperature, and the pre-compensation value is linearly positively correlated with the mold's constant distance, the following function is used to fit the compensation calculation formula:
[0067] X=(a×MI+b×ρ+c×η+d×T)×Y×f
[0068] Where a, b, c, d, and f are the fitting parameters.
[0069] Preferably, a cable sheath production pre-compensation device based on a pre-compensation mechanism further includes a position recognition module, a mold adjustment module, and a production control module.
[0070] The position recognition module is used to obtain the position information of the mold core and mold cover; the mold adjustment module is used to adjust the position of the mold cover and / or mold core; and the production control module is used to realize the pre-compensation function of cable sheath production according to the preset sequence.
[0071] The following is an example:
[0072] Optical cable production utilizes a thermoforming process. The sheath material is extruded through the gap between the core and the cover using an extruder. The spacing between the core and the cover determines the concentricity of the optical cable. This spacing must be consistent throughout 360 degrees. However, due to gravity, the spacing between the core and cover directly above the extruder head needs to be slightly larger than that directly below. Pre-compensation is required during concentricity adjustment. Different sheath materials have different processing properties, resulting in varying pre-compensation values. The optimal die installation position is calculated based on the processing properties of different materials. The die installation position is automatically adjusted using a scanning device and a die head adjustment device, thereby achieving optimal optical cable concentricity and maximizing raw material savings.
[0073] Example 1:
[0074] (1) Install the extruder die head and obtain the die distance as Y. Specifically, Y = (inner diameter of die cover - outer diameter of die core) / 2; Y = 6mm;
[0075] (2) PE material was processed using an extruder at different temperatures T to obtain a sheath that met the design requirements. The melt index (MI), density (ρ), shrinkage rate (η), and pre-compensation value (X) were obtained during processing. The sampled data from the processing experiment are as follows: For MDPE material, the melt index was 0.8 g / 10 min, and the density was 0.948 g / cm³. 3 Shrinkage rate 1.4%, processing temperature 235℃, pre-compensation value 0.175mm;
[0076] (3) The distance Y of the extruder die and the multiple sets of pre-compensation values X, melt index MI, density ρ, shrinkage rate η and processing temperature data T obtained in step (2) are substituted into the following function for fitting:
[0077] X=(a×MI+b×ρ+c×η+d×T)×Y×f
[0078] The formula for calculating the pre-compensation value of PE material is as follows:
[0079] X=(1.6*MI+0.8*ρ+1.2*η+0.9 / 100*T℃)*Y / 200
[0080] The fitting results of the MDPE regression model are as follows Figure 2 As shown, the evaluation R 2 The value is 0.7823, indicating a good fit.
[0081] (4) Calculate the pre-compensation value of PE material for producing sheaths at the production target melt index, density, shrinkage rate and processing temperature according to the pre-compensation calculation model obtained in step (3);
[0082] (5) Adjust the position of the mold cover so that the distance between the upper edge of the mold core and the upper edge of the mold cover is equal to the fixed distance plus the pre-compensation value calculated in step (4). Perform pre-compensation adjustment and use an extruder with a mold that has adjusted the distance between the mold core and the mold cover to process PE material sheaths. The concentricity of the produced sheaths meets the design requirements.
[0083] Example 2:
[0084] (1) Install the extruder die head and obtain the die distance as Y. Specifically, Y = (inner diameter of die cover - outer diameter of die core) / 2; Y = 3mm;
[0085] (2) Nylon 12 material was processed using an extruder at different temperatures T to obtain a sheath that met the design requirements. The melt index (MI), density (ρ), shrinkage rate (small die core), and pre-compensation value (X) were obtained during processing. The sampled data from the processing experiment are as follows: For Nylon 12 material, its melt index is 15.2 g / 10 min, and its density is 1.12 g / cm³. 3 Shrinkage rate 1.16%, processing temperature 220℃, pre-compensation value 0.129mm;
[0086] (3) Substitute the multiple sets of pre-compensation values X, melt index MI, density ρ, shrinkage rate η, and processing temperature T obtained in step (2), along with the distance Y between the mold core and the mold cover, into the following function for fitting:
[0087] The formula for calculating the pre-compensation value of Nylon 12 material, obtained from X=(a×MI+b×ρ+c×η+d×T)×Y×f, is as follows:
[0088] X=(0.3*MI+0.9*ρ+1.1*η+0.8 / 100*T℃)*Y / 200
[0089] The regression model fitting results for Nylon 12 are as follows: Figure 3 As shown, the evaluation R 2 The value is 0.81, indicating a good fit.
[0090] (4) Calculate the pre-compensation value of nylon for producing sheaths at the production target melt index, density, shrinkage rate and processing temperature based on the pre-compensation calculation model obtained in step (3);
[0091] (5) Adjust the position of the mold cover so that the distance between the upper edge of the mold core and the upper edge of the mold cover is equal to the fixed distance plus the pre-compensation value calculated in step (4). Perform pre-compensation adjustment and use an extruder with a mold that has adjusted the distance between the mold core and the mold cover to process the nylon sheath. The concentricity of the produced sheath meets the design requirements.
[0092] Those skilled in the art will readily understand that the above description is merely a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of the present invention should be included within the scope of protection of the present invention.
Claims
1. A method for producing cable sheaths based on a pre-compensation mechanism, characterized in that, Includes the following steps: (1) For the die head of the target extruder, obtain the die distance; the distance is half of the difference between the outer diameter of the die core and the inner diameter of the die cover of the target extruder die head; (2) Using the target extruder, processing experiments were conducted on the processed material under different production conditions to obtain processing experiment sampling data when the concentricity of the sheath met the design requirements; the processing experiment sampling data included the melt index, density, shrinkage rate, processing temperature and its corresponding pre-compensation value of the processed material; The pre-compensation value is the difference between the distance between the upper edge of the outer side of the mold core and the upper edge of the inner side of the mold cover and the fixed distance when the concentricity of the sheath meets the design requirements. (3) Based on the processing experiment sampling data obtained in step (2), fit the mapping model of melt index, density, shrinkage rate, processing temperature and fixed interval to pre-compensation value of the processed material: ; in This is the pre-compensation value. For melt index, For density, Shrinkage rate For processing temperature, For fixed distance; (4) For actual production conditions, obtain the melt index, density, shrinkage rate and processing temperature parameters of the production material, and calculate the pre-compensation value of the target extruder die head according to the mapping model obtained in step (3); (5) Adjust the position of the die core and / or die cover of the target extruder die head so that the distance between the upper edge of the outer side of the die core and the upper edge of the inner side of the die cover is equal to the fixed distance plus the pre-compensation value calculated in step (4). Perform pre-compensation adjustment and use the adjusted target extruder for sheath extrusion processing.
2. The cable sheath production method based on a pre-compensation mechanism as described in claim 1, characterized in that, In step (3), the pre-compensation value in the mapping model is positively correlated with melt index, density, shrinkage rate and processing temperature.
3. The cable sheath production method based on a pre-compensation mechanism as described in claim 1, characterized in that, Step (3) The pre-compensation value and the distance of the mold in the mapping model are linearly positively correlated.
4. The cable sheath production method based on a pre-compensation mechanism as described in claim 1, characterized in that, In step (3), the following function is used to fit the data: ; in, These are the fitting parameters.
5. A pre-compensation device for cable sheath production based on a pre-compensation mechanism, characterized in that, This includes a mapping model acquisition module and a pre-compensation value calculation module; The mapping model acquisition module is used to fit the processing experiment sampling data to obtain a mapping model of the melt index, density, shrinkage rate, processing temperature, and distance to the pre-compensation value of the processed material, and submit it to the pre-compensation value calculation module; the distance is half of the difference between the outer diameter of the die core of the target extruder die head and the inner diameter of the die cover. The pre-compensation value calculation module is used to obtain the melt index, density, shrinkage rate and processing temperature parameters of the production material and input them into the mapping model to calculate the pre-compensation value of the processed material under actual production conditions; the pre-compensation value is: the difference between the distance between the upper edge of the outer side of the mold core and the upper edge of the inner side of the mold cover and the fixed distance when the concentricity of the sheath meets the design requirements. The mapping model of the mapping model acquisition module is obtained through the following steps: (S1) Using a processing device, a preset number of production data samples are taken to measure the concentricity of the sheath under different production conditions to meet the design requirements of the processing material, thereby obtaining the melt index, density, shrinkage rate, and processing temperature of the processing material. and its corresponding pre-compensation value; (S2) Based on the processing experiment sampling data obtained in step (S1), a mapping model for the melt index, density, shrinkage rate, processing temperature, and interval to pre-compensation value of the processed material is fitted: ; in This is the pre-compensation value. For melt index, For density, Shrinkage rate For processing temperature, The pre-compensation value is a fixed distance; in the mapping model of the pre-compensation value, the pre-compensation value is positively correlated with melt index, density, shrinkage rate, and processing temperature; the pre-compensation value and the fixed distance between the mold cover and the mold core are... This is a linear positive correlation.
6. The cable sheath production pre-compensation device based on the pre-compensation mechanism as described in claim 5, characterized in that, The mapping model for the pre-compensation value is fitted using the following function: ; in, These are the fitting parameters.
7. The cable sheath production pre-compensation device based on the pre-compensation mechanism as described in claim 5, characterized in that, It also includes a position recognition module and a mold adjustment module; among which: The position recognition module is used to obtain the position information of the mold core and the mold cover, and calculate the distance and submit it to the mapping model acquisition module; The mold adjustment module is used to calculate the target position of the mold cover and / or mold core according to the pre-compensation value, so that the distance between the upper edge of the outer side of the mold core and the upper edge of the inner side of the mold cover is equal to the fixed distance plus the pre-compensation value.
Citation Information
Patent Citations
Extrusion die easy to adjust concentricity of cable sheath
CN103157687A
Coaxial cable concentricity online compensation control method and system
CN115274218A