Semiconductor device, manufacturing method thereof and electronic device

By designing a field-limited ring structure with gradually increasing gaps in the semiconductor device, the voltage drop at the main junction is allocated to the field-limited ring structure, which solves the problem of avalanche failure of the semiconductor device during the reverse withstand voltage process and improves the reliability of the device. efficiency and reduced costs.

CN117790537BActive Publication Date: 2024-10-25深圳平湖实验室
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202311842844.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-12-28
Publication Date
2024-10-25
Estimated Expiration
2043-12-28

AI Technical Summary

Technical Problem

During the reverse withstand voltage process of semiconductor devices, impact ionization is prone to occur near the main junction, resulting in avalanche failure, which reduces the reliability of the device.

Method used

A semiconductor device is designed, which includes a substrate and a drift layer. The side surface of the drift layer facing away from the substrate is provided with a main junction and a plurality of field-limited ring structures. Any two adjacent field-limited ring structures are in a first direction. With gaps, the gaps between adjacent field-limited ring structures gradually increase along the direction away from the main junction. The depth of the doped region becomes shallower as the distance from the main junction increases, which can reduce the pressure at the main junction. The drop is distributed to each field-limited ring structure, thereby reducing the voltage drop and electric field stress at the main junction.

Benefits of technology

By distributing the voltage drop and reducing the electric field stress, the reliability of the semiconductor device is improved, the reverse bias current and shutdown power consumption are reduced, the manufacturing process is simplified, and the cost is reduced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117790537B_ABST
    Figure CN117790537B_ABST
Patent Text Reader

Abstract

The present invention discloses a semiconductor device, a manufacturing method thereof and an electronic device, comprising a substrate and a drift layer, wherein a main junction and a field limiting ring structure are arranged on a surface of the drift layer facing away from the substrate, and any two adjacent field limiting ring structures have a gap in the first direction, and the gap between adjacent field limiting ring structures gradually increases along the direction away from the main junction. In this way, the depth of the doped region can become shallower and shallower as the distance from the main junction increases, and the voltage drop at the main junction can be distributed to each field limiting ring structure, thereby reducing the voltage drop at the main junction, reducing the electric field stress at the main junction, and improving the reliability of the semiconductor device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a semiconductor device, a manufacturing method thereof and an electronic device. Background Art

[0002] During the reverse withstand voltage test of semiconductor devices, impact ionization is prone to occur near the main junction, especially at the edge of the main junction, leading to avalanche failure of the semiconductor device, which in turn reduces the reliability of the semiconductor device. How to improve the reliability of semiconductor devices has become a technical problem that needs to be solved urgently in this field. Summary of the invention

[0003] The embodiments of the present invention provide a semiconductor device, a manufacturing method thereof and an electronic device, so as to improve the reliability of the semiconductor device.

[0004] In a first aspect, an embodiment of the present invention provides a semiconductor device, comprising: a substrate, and a drift layer disposed on the substrate, wherein a surface of the drift layer on a side away from the substrate is provided with: a main junction and a plurality of field limiting ring structures, each of the field limiting ring structures surrounds the main junction, and any two adjacent field limiting ring structures have a gap in a first direction, wherein the first direction is a direction parallel to the substrate surface and away from the main junction;

[0005] Each of the field limiting ring structures in at least part of the field limiting ring structures comprises: a doping region and a groove arranged in a stacked manner, wherein the groove is arranged on a surface of the doping region on a side away from the substrate;

[0006] Along the first direction, the gaps between adjacent field limiting ring structures gradually increase, and the depths of the grooves gradually decrease.

[0007] In a second aspect, an embodiment of the present invention provides a semiconductor device, comprising: a substrate, and a drift layer disposed on the substrate, wherein a surface of the drift layer facing away from the substrate is provided with: a main junction region and a terminal structure region, and the terminal structure region includes a junction terminal extension structure;

[0008] The main junction region is provided with a boss, and the main junction in the main junction region is provided in the boss;

[0009] The surface of the terminal structure region is an inclined surface, and along a first direction, the distance between the inclined surface and the substrate gradually increases; the first direction is: a direction parallel to the substrate surface and away from the main junction region.

[0010] In a third aspect, an embodiment of the present invention provides a semiconductor device, comprising: a substrate, and a drift layer disposed on the substrate, wherein a surface of the drift layer facing away from the substrate is provided with: a main junction region and a terminal structure region, and the terminal structure region includes a plurality of field limiting rings;

[0011] The main junction region is provided with a boss, and the main junction in the main junction region is provided in the boss;

[0012] The surface of the terminal structure region is an inclined surface, and along a first direction, the distance between the inclined surface and the substrate gradually increases; the first direction is: a direction parallel to the substrate surface and away from the main junction region.

[0013] In a fourth aspect, an embodiment of the present invention provides a method for manufacturing a semiconductor device as described in the first aspect, comprising:

[0014] epitaxially forming a drift layer on the substrate;

[0015] A main junction and a plurality of field limiting ring structures are formed on a surface of the drift layer on a side away from the substrate; wherein each of the field limiting ring structures surrounds the main junction, and any two adjacent field limiting ring structures have a gap in a first direction, and the first direction is: a direction parallel to the substrate surface and away from the main junction; each of the field limiting ring structures in at least some of the field limiting ring structures comprises: a stacked doping region and a groove, and the groove is provided on a surface of the doping region on a side away from the substrate; along the first direction, the gap between adjacent field limiting ring structures gradually increases, and the depth of each groove gradually decreases.

[0016] In a fifth aspect, an embodiment of the present invention provides a method for manufacturing a semiconductor device as described in the second aspect above, comprising:

[0017] epitaxially forming a drift layer on the substrate;

[0018] forming a boss in a main junction region on a surface of the drift layer on a side away from the substrate;

[0019] A main junction is formed within the boss, and a junction terminal extension structure is formed in the terminal structure region, so that the surface of the terminal structure region is an inclined surface, and along a first direction, the distance between the inclined surface and the substrate gradually increases; the first direction is: a direction parallel to the substrate surface and away from the main junction region.

[0020] In a sixth aspect, an embodiment of the present invention provides a method for manufacturing a semiconductor device as described in the third aspect, comprising:

[0021] epitaxially forming a drift layer on the substrate;

[0022] forming a boss in a main junction region on a surface of the drift layer on a side away from the substrate;

[0023] A main junction is formed within the boss, and a plurality of field limiting rings are formed in the terminal structure region, so that the surface of the terminal structure region is an inclined surface, and along a first direction, the distance between the inclined surface and the substrate gradually increases; the first direction is: a direction parallel to the substrate surface and away from the main junction region.

[0024] In a seventh aspect, an embodiment of the present invention provides an electronic device, comprising a semiconductor device as described in the first aspect, the second aspect or the third aspect above.

[0025] The beneficial effects of the present invention are as follows:

[0026] A semiconductor device, a manufacturing method thereof and an electronic device provided by an embodiment of the present invention include a substrate and a drift layer, a main junction and a field limiting ring structure are arranged on a surface of the drift layer facing away from the substrate, any two adjacent field limiting ring structures have a gap in the first direction, and the gap between adjacent field limiting ring structures gradually increases along the direction away from the main junction. In this way, the depth of the doped region can become shallower and shallower as the distance from the main junction increases, and the voltage drop at the main junction can be distributed to each field limiting ring structure, thereby reducing the voltage drop at the main junction, reducing the electric field stress at the main junction, and improving the reliability of the semiconductor device. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] Figure 1 is a cross-sectional view of a semiconductor device provided in an embodiment of the present invention;

[0028] Figure 2 A top view of a terminal structure region of a semiconductor device provided in an embodiment of the present invention;

[0029] Figure 3 for Figure 1 A partial enlarged view of the area shown in Q1;

[0030] Figure 4 is a cross-sectional view of another semiconductor device provided in an embodiment of the present invention;

[0031] Figure 5 is a cross-sectional view of another semiconductor device provided in an embodiment of the present invention;

[0032] Figure 6 is a cross-sectional view of another semiconductor device provided in an embodiment of the present invention;

[0033] Figure 7 is a cross-sectional view of another semiconductor device provided in an embodiment of the present invention;

[0034] Figure 8 This is a simulated data diagram of the electron-hole pair concentration distribution generated by impact ionization;

[0035] Fig. 9A flow chart of a method for manufacturing a semiconductor device provided in an embodiment of the present invention;

[0036] Fig.10 A flow chart of a method for manufacturing a semiconductor device provided in another embodiment of the present invention;

[0037] Fig.11 A flow chart of a method for manufacturing a semiconductor device provided in another embodiment of the present invention;

[0038] Fig.12 A schematic diagram of a manufacturing process of a semiconductor device provided in an embodiment of the present invention;

[0039] Fig.13 It is a simulation data diagram of the horizontal electric field intensity distribution when the semiconductor device 1 withstands reverse voltage;

[0040] Fig.14 It is a simulation data diagram of the horizontal electric field intensity distribution when the semiconductor device 2 withstands reverse voltage;

[0041] Fig.15 It is a simulation data diagram of the horizontal electric field intensity distribution of the semiconductor device 3 when it is reversely withstand voltage;

[0042] Fig.16 It is a simulation data diagram of the vertical electric field intensity distribution of the semiconductor device 3 when it is reversely withstand voltage;

[0043] Fig.17 It is a simulation data diagram of the anode electrode reverse voltage and reverse current density of semiconductor device 1, semiconductor device 2, and semiconductor device 3;

[0044] Fig.18 It is a schematic diagram of the structure of an electronic device provided in an embodiment of the present invention. DETAILED DESCRIPTION

[0045] The following will be combined with the accompanying drawings to describe in detail a semiconductor device, a method for manufacturing the same, and a specific implementation of an electronic device provided by an embodiment of the present invention. It should be noted that the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0046] The embodiment of the present invention provides a first semiconductor device, such as Figure 1 and Figure 2 As shown, it includes: a substrate 102, and a drift layer 103 arranged on the substrate 102, and a surface of the drift layer 103 facing away from the substrate 102 is provided with: a main junction 107 and a plurality of field limiting ring structures 108, wherein: Figure 2It is a top view of the surface of the drift layer 103 facing away from the substrate 102 . Each field limiting ring structure 108 surrounds the main junction 107 . Any two adjacent field limiting ring structures 108 have a gap in the first direction. The first direction is a direction parallel to the surface of the substrate 102 and away from the main junction 107 .

[0047] Each of the field limiting ring structures 108 in at least part of the field limiting ring structures 108 comprises: a stacked doping region 105 and a groove 106, wherein the groove 106 is disposed on a surface of the doping region 105 facing away from the substrate 102, and the doping type of the doping region 105 is opposite to the doping type of the drift layer 103, that is, when the doping type of the drift layer 103 is N-type, the doping type of the doping region 105 is P-type, and when the doping type of the drift layer 103 is P-type, the doping type of the doping region 105 is N-type;

[0048] Along the first direction, the gaps between adjacent field limiting ring structures 108 gradually increase, and the depth of each groove 106 gradually decreases.

[0049] Among them, Figure 3 As shown, Figure 3 for Figure 1 The enlarged view of the area shown in the dotted line frame Q1, the first direction is the direction shown by the arrow F1, the two adjacent field limiting ring structures 108 have a gap in the first direction F1, and the gaps between the adjacent field limiting ring structures 108 are d1, d2, and d3, respectively, d1 is smaller than d2, d2 is smaller than d3, that is, along the first direction F1, the gaps between the adjacent field limiting ring structures 108 gradually increase. In addition, since the grooves 106 and the corresponding doping regions 105 are stacked, when the depth of each groove 106 is gradually reduced, the setting depth of each doping region 105 is also gradually reduced, so that the setting depth of the entire field limiting ring structure 108 is gradually reduced. In addition, the doping region 105 can be understood as a field limiting ring, and the field limiting ring and the doping region have the same meaning below, and the two can be used interchangeably.

[0050] In this way, the depth of each field limiting ring structure becomes shallower as the distance from the main junction increases, and the voltage drop at the main junction can be distributed to each field limiting ring structure, thereby reducing the voltage drop at the main junction, reducing the electric field stress at the main junction, and improving the reliability of the semiconductor device. In addition, the field limiting ring can expand the depletion layer around the main junction, thereby reducing the reverse bias current and reducing the turn-off power consumption of the transistor.

[0051] Alternatively, if Figure 2 As shown, the field limiting ring structures 108 can be arranged concentrically, wherein the shape of the field limiting ring structures 108 is not limited and can be any shape, as long as they are arranged concentrically and surround the main junction 107 .

[0052] Optionally, the number of field limiting ring structures may be, but is not limited to, 2, 3, 4, 5, 6, 7, 8, 9, 10 or more, which may be determined according to actual needs and is not specifically limited here. In this way, when fewer field limiting ring structures are provided, the occupied area of ​​the semiconductor device can be reduced, and when more field limiting ring structures are provided, the electric field strength at the main junction can be significantly reduced, thereby significantly improving the reliability of the semiconductor device.

[0053] Optionally, some grooves in the semiconductor device have the same depth. Figure 4 As shown, two grooves 106 form a group, which can be divided into four groups: 106a, 106b, 106c, and 106d. The two grooves 106 in each group have the same depth, and the grooves 106 with the same depth are adjacent, so that the depth of each groove 106 gradually decreases along the first direction F1. Of course, the number of grooves 106 with the same depth in each group is not limited to two, and can also be one, three, four or more. It is not limited here, as long as the depth of each groove 106 gradually decreases along the first direction F1. It should be understood that Figure 4 Only half of the structure of the semiconductor device is shown, and the other half of the structure is similar, which will not be described here.

[0054] In this way, the depths of some grooves are the same, which reduces the complexity of the process for forming the grooves and reduces the cost of the semiconductor device.

[0055] Of course, the depths of the grooves 106 can be set to be different, such as Figure 3 As shown in , this can meet the design needs of different application scenarios and improve the flexibility of design.

[0056] Alternatively, if Figure 3 As shown, the depth h1 of the groove 106 in the semiconductor device is greater than 0 and not greater than 2 μm. In this way, the difficulty of forming the groove 106 due to the depth h of the groove 106 being too large can be avoided, thereby reducing the manufacturing cost of the semiconductor device.

[0057] Alternatively, if Figure 5 As shown, a main junction region 109 and a terminal structure region 1010 are provided on the surface of the drift layer 103 facing away from the substrate 102, the main junction 107 is located in the main junction region 109, and each field limiting ring structure 108 is located in the terminal structure region 1010; the main junction region 109 has a boss, and the main junction 107 is provided inside the boss. The height of the boss can be set to 0.1 μm to 2 μm, and of course the height of the boss can also be set according to actual needs, which is not limited here.

[0058] Among them, Figure 5As shown, the height of the boss is h2. After the boss is provided, a recessed area is correspondingly formed in the area other than the boss on the surface of the drift layer on one side away from the substrate 102. The field limiting ring structure is provided in the recessed area, thereby increasing the relative depth of the field limiting ring structure 108.

[0059] In this way, by setting the boss, the setting depth of the field limiting ring structure is controlled, the setting depth of the groove is reduced, the manufacturing process of the field limiting ring structure is simpler, and the cost of the semiconductor device is reduced. At the same time, the larger setting depth of the field limiting ring structure can absorb more avalanche breakdown energy, further improving the reliability of the semiconductor device.

[0060] Alternatively, if Figure 5 As shown, the surface M1 of the terminal structure region is parallel to the substrate surface. In this way, the manufacturing process of the boss can be simplified, thereby reducing the manufacturing cost of the semiconductor device.

[0061] Based on the same inventive concept, the embodiment of the present invention also provides a second semiconductor device, such as Figure 6 As shown, it includes: a substrate 102, and a drift layer 103 disposed on the substrate 102, and a surface of the drift layer 103 facing away from the substrate 102 is provided with: a main junction region 109 and a terminal structure region 1010, and the terminal structure region 1010 includes a junction terminal extension structure 1011;

[0062] The main junction region 109 is provided with a boss, and the main junction 107 in the main junction region 109 is provided within the boss;

[0063] The surface of the terminal structure region 1010 is an inclined surface, and along a first direction F1 , the distance between the inclined surface and the substrate 102 gradually increases; the first direction F1 is parallel to the surface of the substrate 102 and away from the main junction region 107 .

[0064] In this way, by setting the inclined surface, the setting depth of the junction terminal extension structure becomes shallower and shallower as the distance from the main junction increases, so that the voltage drop at the main junction can be distributed to the junction terminal extension structure, thereby reducing the voltage drop at the main junction, reducing the electric field stress at the main junction, and improving the reliability of the semiconductor device.

[0065] Based on the same inventive concept, the embodiment of the present invention also provides a third semiconductor device, such as Figure 7 As shown, it includes: a substrate 102, and a drift layer 103 disposed on the substrate 102, and a surface of the drift layer 103 facing away from the substrate 102 is provided with: a main junction region 109 and a terminal structure region 1010, and the terminal structure region 1010 includes a plurality of field limiting rings 1012;

[0066] The main junction region 109 is provided with a boss, and the main junction 107 in the main junction region 109 is provided within the boss;

[0067] The surface of the terminal structure region 1010 is an inclined surface, and along a first direction F1 , the distance between the inclined surface and the substrate 102 gradually increases; the first direction F1 is parallel to the surface of the substrate 102 and away from the main junction region 107 .

[0068] In this way, multiple field limiting rings can expand the depletion layer around the main junction, thereby reducing the reverse bias current and reducing the turn-off power consumption of the transistor. In addition, by setting a boss to control the depth of the field limiting ring, there is no need to form multiple grooves, which can simplify the manufacturing process and reduce the cost of the semiconductor device. It can also distribute the voltage drop at the main junction to each field limiting ring, thereby reducing the voltage drop at the main junction and improving the reliability of the semiconductor device.

[0069] Alternatively, if Figure 6 As shown, in the terminal structure region 1010, the spacing h3 between the side close to the main junction 107 and the side surface of the boss facing away from the substrate 102 is 0.1μm to 2μm, and the spacing h4 between the side away from the main junction 107 and the side surface of the boss facing away from the substrate 102 is 0.1μm to 0.5μm.

[0070] In this way, the surface inclination of the terminal structure area can be controlled to be within an appropriate range, so that the setting depth of the junction terminal extension structure or the field limiting ring becomes shallower and shallower as the distance from the main junction increases, thereby reducing the voltage drop at the main junction and improving the reliability of the semiconductor device; in addition, the doping depth of the junction terminal extension structure or the field limiting ring can be controlled to be within an appropriate range to achieve absorption of avalanche energy, reduce manufacturing difficulty, further improve the reliability of the semiconductor device, and reduce manufacturing costs.

[0071] It should be understood that, for the second type of semiconductor device, when a junction terminal extension structure is formed in the terminal structure region, the doping concentration of the junction terminal extension structure may be lower than the doping concentration of the doping region at the main junction; and for the third type of semiconductor device, when a plurality of field limiting rings are formed in the terminal structure region, the doping concentration of the field limiting rings may be higher than the doping concentration of the doping region at the main junction.

[0072] In addition, the drawings used in the present invention are all PiN diodes, such as Figure 1 As shown, the PiN diode may also include: a main junction doping region 104, a cathode electrode 101, an anode electrode 110, and a passivation layer 111. Of course, the technical solution provided by the present invention may also be used in other transistors, such as but not limited to: metal oxide field effect transistors, Schottky diodes, junction barrier Schottky diodes, triodes, thyristors, insulated gate bipolar transistors, junction field effect transistors, etc.

[0073] Among them, Figure 8As shown in FIG. 1 , since the impact ionization phenomenon of the drift layer 103 below the contact interface between the anode electrode 110 and the passivation layer 111 is more concentrated, and thus avalanche breakdown is more likely to occur, the contact interface between the anode electrode 110 and the passivation layer 111 is arranged above the field limiting ring structure (such as Figure 4 as shown) or above the main knot (as Figure 1 As shown in FIG. 1 , the field limiting ring structure or the main junction can be used to reduce the electric field strength in the region, thereby suppressing the occurrence of avalanche phenomenon and improving the reliability of the semiconductor device. Of course, the same is true for semiconductor devices with junction terminal extension structures or multiple field limiting rings, which will not be described in detail here. It should be noted that in Figure 8 In the embodiment, a doped region is provided below the groove 106. Figure 8 This is a simulation diagram, so the structure of the doped region is Figure 8 It is not very obvious, but this does not mean Figure 8 The semiconductor device in does not include a doped region.

[0074] In addition, when the contact interface between the anode electrode 110 and the passivation layer 111 is disposed on the field limiting ring structure, the corresponding field limiting ring structure contacted by the edge of the anode electrode 110 may not be provided with a groove 106, but of course, a groove 106 may be provided, which is not limited here. Furthermore, when the semiconductor device includes the passivation layer 111, the aspect ratio of the groove 106 may be less than 1:3, so that the passivation layer 111 can fully fill the groove 106.

[0075] Among them, the principle of avalanche breakdown can include: when breakdown occurs, the electric field in the breakdown area is high, and the free carriers generated by impact ionization further excite the free carriers of the next level, the current density in the area increases, and at the same time the local voltage drop decreases, further increasing the current density in the breakdown area. Due to the thermal effect caused by the large local current density, the avalanche breakdown of the semiconductor device is eventually caused.

[0076] Based on the same inventive concept, the embodiment of the present invention provides a first method for manufacturing a semiconductor device, such as Fig. 9 As shown, including:

[0077] S901 , epitaxially forming a drift layer on the substrate.

[0078] Optionally, in step S901, a CVD (Chemical Vapor Deposition) process may be used, using silane and propane as material growth gases and hydrogen as a carrier gas for epitaxial growth to obtain a drift layer. Of course, the drift layer may also be obtained by other methods well known to those skilled in the art, which are not limited here.

[0079] S902. Form a main junction and a plurality of field limiting ring structures on a surface of the drift layer facing away from the substrate; wherein each field limiting ring structure surrounds the main junction, and any two adjacent field limiting ring structures have a gap in a first direction, and the first direction is: a direction parallel to the substrate surface and away from the main junction; each field limiting ring structure in at least some of the field limiting ring structures includes: a stacked doping region and a groove, and the groove is provided on a surface of the doping region facing away from the substrate; along the first direction, the gap between adjacent field limiting ring structures gradually increases, and the depth of each groove gradually decreases.

[0080] In this way, by forming a field limiting ring structure that becomes shallower as the distance from the main junction increases, the voltage drop at the main junction can be distributed to each field limiting ring, thereby reducing the voltage drop at the main junction, reducing the electric field stress at the main junction, and improving the reliability of the semiconductor device. In addition, the field limiting ring can expand the depletion layer around the main junction, thereby reducing the reverse bias current and reducing the turn-off power consumption of the transistor.

[0081] Optionally, the first method for manufacturing a semiconductor device further includes: before forming the main junction and the plurality of field limiting ring structures, etching the drift layer so that a boss is formed on a surface of the drift layer facing away from the substrate;

[0082] The main junction and a plurality of field limiting ring structures are formed, specifically including: forming a main junction within the boss, and forming a plurality of field limiting ring structures in a region other than the boss.

[0083] The etching process may be implemented by a RIE (Reactive Ion Etching) etching process. Of course, the etching process may also be implemented by other methods well known to those skilled in the art, which is not limited here.

[0084] In this way, a boss can be formed through etching, thereby controlling the setting depth of the field limiting ring structure and reducing the setting depth of the groove, making the field limiting ring structure manufacturing process simpler and reducing the cost of semiconductor devices. At the same time, the larger setting depth of the field limiting ring structure can absorb more avalanche breakdown energy, further improving the reliability of the semiconductor device.

[0085] Based on the same inventive concept, the embodiment of the present invention also provides a second method for manufacturing a semiconductor device, such as Fig.10 As shown, including:

[0086] S1001 , epitaxially forming a drift layer on a substrate.

[0087] Optionally, in step S1001, a CVD process may be used, using silane and propane as material growth gases and hydrogen as a carrier gas for epitaxial growth to obtain a drift layer. Of course, the drift layer may also be obtained by other methods well known to those skilled in the art, which are not limited here.

[0088] S1002 , forming a boss in a main junction region on a surface of the drift layer facing away from the substrate.

[0089] Optionally, in step S1001, the boss may be formed by an RIE (Reactive Ion Etching) etching process. Of course, the etching process may also be implemented by other methods well known to those skilled in the art, which is not limited here.

[0090] S1003. A main junction is formed within the boss, and a junction terminal extension structure is formed in the terminal structure area, so that the main junction is arranged within the boss, the surface of the terminal structure area is an inclined surface, and along a first direction, the distance between the inclined surface and the substrate gradually increases; the first direction is: a direction parallel to the substrate surface and away from the main junction area.

[0091] In this way, an inclined surface of the terminal structure region is formed, so that the depth of the junction terminal extension structure becomes shallower as the distance from the main junction increases, and the voltage drop at the main junction can be distributed to the junction terminal extension structure, thereby reducing the voltage drop at the main junction, reducing the electric field stress at the main junction, and improving the reliability of the semiconductor device. The junction terminal extension structure can also expand the depletion layer around the main junction, thereby reducing the reverse bias current and reducing the turn-off power consumption of the transistor.

[0092] Based on the same inventive concept, the embodiment of the present invention also provides a third method for manufacturing a semiconductor device, such as Fig.11 As shown, including:

[0093] S1101 , epitaxially forming a drift layer on the substrate.

[0094] Optionally, in step S1101, a CVD process may be used, using silane and propane as material growth gases and hydrogen as a carrier gas for epitaxial growth to obtain a drift layer. Of course, the drift layer may also be obtained by other methods well known to those skilled in the art, which are not limited here.

[0095] S1102 , forming a boss in a main junction region on a surface of the drift layer facing away from the substrate.

[0096] Optionally, in step S1101, the boss may be formed by an RIE etching process. Of course, the etching process may also be implemented by other methods well known to those skilled in the art, which is not limited here.

[0097] S1103. A main junction is formed inside the boss, and a plurality of field limiting rings are formed in the terminal structure region, so that the main junction is arranged inside the boss, the surface of the terminal structure region is an inclined surface, and along a first direction, the distance between the inclined surface and the substrate gradually increases; the first direction is: a direction parallel to the substrate surface and away from the main junction region.

[0098] In this way, an inclined surface is formed on the surface of the terminal structure area, so that the depth of each field limiting ring becomes shallower as the distance from the main junction increases. Similarly, the voltage drop at the main junction can be distributed to each field limiting ring, thereby reducing the voltage drop at the main junction, reducing the electric field stress at the main junction, and improving the reliability of the semiconductor device. Each field limiting ring can also expand the depletion layer around the main junction, thereby reducing the reverse bias current and reducing the turn-off power consumption of the transistor. In addition, by forming a boss to control the depth of each field limiting ring, there is no need to form multiple grooves, which can simplify the manufacturing process and reduce the cost of the semiconductor device.

[0099] The semiconductor device and the manufacturing method thereof provided by the embodiments of the present invention are explained below in conjunction with specific embodiments.

[0100] Embodiment 1:

[0101] Taking a silicon carbide PiN diode as an example, the manufacturing method and process implementation of the semiconductor device of the first embodiment include the following steps:

[0102] S1, such as Fig.12 As shown in (a), a drift layer is formed on a substrate.

[0103] The specific process may include: using a silicon carbide epitaxial furnace to grow an intrinsic N- epitaxial layer on an N+ heavily doped substrate to obtain a drift layer.

[0104] S2, such as Fig.12 As shown in (b), a groove 106 and a doped region 105 are formed on the surface of the drift layer.

[0105] The specific process may include: using 4:1SPM (i.e., a mixture of sulfuric acid and hydrogen peroxide) and 6:1BOE (Buffered Oxide Etch) to wet clean the surface of the drift layer; then forming a first mask layer with a predetermined pattern on the surface of the drift layer after wet cleaning; then, using the ICP-RIE etching process, etching the area exposed by the first mask layer to form a portion of grooves with the same depth; then, using the ion implantation method, high-energy ions are implanted into the area exposed by the first mask layer, so as to form a doping area corresponding to the groove with a vertical concentration distribution at a specific position; finally, using wet etching to remove the first mask layer and clean it, so as to further make other structures. Afterwards, the same process steps are used to form the remaining grooves and doping areas, and finally, among all the grooves formed, the depth of some grooves is the same, and along the first direction, the depth of each groove gradually decreases.

[0106] Wherein, forming a first mask layer having a predetermined pattern may specifically include:

[0107] Silicon nitride is deposited on the surface of the drift layer as an etching barrier layer; a silicon oxide layer is produced on the surface of the etching barrier layer by a PECVD (Plasma Enhanced Chemical Vapor Deposition) method as a first mask layer; photoresist is spin-coated on the surface of the first mask layer, and the photoresist is patterned to obtain a photoresist with a predetermined pattern; the area exposed by the photoresist is etched to transfer the predetermined pattern to the first mask layer, thereby forming a first mask layer with a predetermined pattern.

[0108] The process parameters of the ICP-RIE etching method can be set as follows: the etching chamber pressure can be 5mTorr to 30mTorr, the ICP power can be 2kW to 4kW, the Bias power can be 0.5kW to 1kW, and the flow rate of SF6 / O2 / Ar can be 8sccm to 40sccm.

[0109] The material to be implanted during ion implantation can be aluminum atoms, the implantation energy can be no greater than 400 keV, and the implantation dose can be 5×10 12 / cm 2 Up to 1×10 14 / cm 2 .

[0110] Furthermore, when removing the first mask layer and performing cleaning, it may specifically include: performing wet etching using hydrofluoric acid to remove the first mask layer and the etching stop layer, and then performing SPM wet cleaning.

[0111] In addition, if Figure 3 As shown, the width d0 of each field limiting ring structure along the first direction F1 can be but not limited to 1.6 μm, and the distance between each field limiting ring structure along the first direction F1 can be but not limited to increase from 1.0 μm with a tolerance of 0.1 μm, that is, d1 is 1.0 μm, d2 is 1.1 μm, and d3 is 1.2 μm.

[0112] S3, such as Fig.12 As shown in (c), a main junction doping region 104 is formed on the surface of the drift layer.

[0113] The specific process of forming the main junction doping region may include: on the surface of the drift layer, using the same process as forming the first mask layer to form a second mask layer with a predetermined pattern; then, using the ion implantation method, high-energy ion implantation is performed into the area exposed by the second mask layer, thereby forming a main junction doping region with a vertical concentration distribution at a specific position; finally, removing the second mask layer and cleaning it to facilitate the production of other structures.

[0114] In addition, after completing step S3, the formed doping region and the main junction doping region are subjected to annealing activation treatment so that the doping region is transformed from amorphous to crystallized, thereby realizing the corresponding function. The activation process includes: using RF-PECVD (Radio Frequency Plasma Enhanced Chemical Vapor Deposition) method or other methods well known to those skilled in the art, which are not limited here. Taking RF-PECVD method as an example, a carbon film with a thickness of about 50nm is deposited on the surface of the structure obtained in the above step, and annealed at 1700°C for 30min. The carbon film can prevent the doping atoms from diffusing outward during the annealing activation process, so that the doping region is transformed from amorphous to crystallized. After the annealing activation treatment, an ashing treatment is performed to remove the carbon film, and the surface of the structure obtained in the above step is subjected to sacrificial oxidation treatment to remove the surface layer, and then a standard RCA (industrial standard wet cleaning process) cleaning is performed.

[0115] S4, such as Fig.12 As shown in (d), a passivation layer, an anode electrode, and a cathode electrode are formed.

[0116] The specific process of forming the passivation layer may include: using PECVD on the surface of the structure obtained in the above steps, and using TEOS (Tetraethyl Orthosilicate) gas source to deposit SiO2 with a thickness greater than 1μm, the preferred thickness may be 1μm to 1.5μm, and ensuring that all grooves are effectively filled, and finally, using a dry etching process to define the main junction area, and forming a passivation layer outside the main junction area.

[0117] The specific process of forming the anode electrode may include: sputtering a layer of metal titanium on the surface of the structure obtained in the above steps using a PVD process, forming an anode ohmic contact between the metal titanium and the main junction doping area, and the thickness of the metal titanium is greater than 1μm, then depositing a layer of metal aluminum with a thickness greater than 2μm, and finally using a lift-off process to remove excess metal outside the main junction area, while retaining metal titanium and metal aluminum in the main junction area.

[0118] The specific process of forming the cathode electrode may include: covering the surface of the structure obtained in the above steps with a blue film, grinding the surface of the substrate facing away from the silicon carbide layer, and then wet cleaning it, and then sputtering metal nickel on the surface of the substrate facing away from the silicon carbide layer by physical vapor deposition. The thickness of the metal nickel can be but is not limited to 1000nm, and using a laser annealing process to form an ohmic contact between the nickel and the substrate.

[0119] It should be understood that the passivation layer, the anode electrode, and the cathode electrode may be made of other materials and structures that are well known to those skilled in the art and can achieve corresponding functions, and are not limited here.

[0120] Thus, the silicon carbide transistor in the first embodiment can be manufactured through the above steps S1 to S4. The effects and principles of the silicon carbide transistor are as follows:

[0121] Note that semiconductor device 1 is a silicon carbide PiN diode in the prior art, and has four field limiting rings but no grooves. When the anode electrode voltage is -600V and the cathode electrode voltage is 0V for simulation, the horizontal electric field at the edge of the main junction is relatively high, with a maximum value of about 2MV / cm, and the vertical electric field at the edge of the main junction is also relatively high, with a maximum value of about 2.1MV / cm; while the absolute values ​​of the electric field strength near the PN junction at the four field limiting rings are similar, about 1.7MV / cm to 1.9MV / cm, that is, the maximum absolute value of the electric field strength is about 1.9MV / cm, which is smaller than the electric field strength at the main junction, indicating that the voltage-dividing effect of the field limiting ring in the prior art is relatively small.

[0122] Semiconductor device 2 is a device manufactured using the above-mentioned embodiment 1, and has four field limiting ring structures. When the same simulation conditions as those of semiconductor device 1 are used, the maximum absolute value of the electric field strength at the edge of the main junction in semiconductor device 2 is about 2.4MV / cm, and the maximum absolute value of the electric field strength near the PN junction at the four field limiting ring structures is also about 2.4MV / cm, which is greater than the absolute value of the electric field strength near the PN junction at the field limiting ring in semiconductor device 1. In this way, semiconductor device 2 can increase the voltage division of the field limiting ring structure, thereby reducing the voltage drop at the main junction and improving the reliability of the semiconductor device.

[0123] like Fig.13 and Fig.14 As shown, Fig.13 is a simulation diagram of the electric field intensity distribution in the horizontal direction of the semiconductor device 1 when it is reverse biased, Fig.14 FIG. 2 is a simulation diagram of the horizontal electric field intensity distribution of the semiconductor device 2 when it is reverse biased. Fig.14 In the semiconductor device 2, the high electric field intensity distribution area in the horizontal direction between the two field limiting ring structures far away from the main junction is Fig.13 The horizontal high electric field strength area at the same position of the semiconductor device 1 has a significantly deeper vertical distribution range, which proves that the overall withstand voltage distribution of the semiconductor device 2 moves toward the field limiting ring structure area outside the main junction, thereby improving the reliability of the semiconductor device 2 during reverse bias, that is, the semiconductor device obtained by the manufacturing method of Example 1 has higher reliability.

[0124] like Fig.15 As shown, semiconductor device 3 is another device manufactured by the above-mentioned embodiment 1, and the difference between semiconductor device 3 and semiconductor device 2 is that: semiconductor device 2 is provided with four field limiting ring structures, and semiconductor device 3 is provided with ten field limiting ring structures; Fig.15The simulation diagram of the horizontal electric field intensity distribution is obtained by using the same simulation conditions as the semiconductor device 1 for the semiconductor device 3. The horizontal electric field intensity in the semiconductor device 3 is approximately uniformly distributed at the PN junction of each field limiting ring structure, that is, the horizontal voltage drop can be evenly distributed to each field limiting ring structure, and the maximum electric field intensity is about 1.6 MV / cm. In this way, the reliability of the semiconductor device can be further improved.

[0125] like Fig.16 As shown, Fig.16 The simulation conditions for semiconductor device 3 are the same as those for semiconductor device 1, and the vertical electric field intensity distribution simulation diagram is obtained. The maximum vertical electric field intensity at the edge of the main junction is about 1.8MV / cm, and the vertical electric field intensity at the PN junction of the field limiting ring structure far away from the main junction is about 1.6MV / cm. In this way, multiple field limiting ring structures fully participate in the withstand voltage of semiconductor device 3, improving the reliability of semiconductor device 3.

[0126] like Fig.17 As shown, Fig.17 It is the reverse current simulation curve of semiconductor device 1, semiconductor device 2, and semiconductor device 3 under the same conditions, wherein the same conditions may include but are not limited to: lattice temperature, reverse voltage, ion implantation concentration and junction depth, initial distance and tolerance between field limiting rings, initial depth and tolerance of trench etching on the surface of field limiting rings, epitaxial thickness and doping concentration, substrate doping concentration, etc.

[0127] from Fig.17 It can be seen that the reverse leakage current of semiconductor device 2 and semiconductor device 3 is significantly reduced compared with that of semiconductor device 1, and the reverse leakage current of semiconductor device 3 is further reduced compared with that of semiconductor device 2. Therefore, the semiconductor device obtained by the manufacturing method of embodiment 1 of the present invention can effectively reduce the reverse leakage current, and more field limiting ring structures can further improve the effect of reducing the leakage current, thereby reducing the reverse energy consumption of the semiconductor device and improving the performance of the semiconductor device.

[0128] Embodiment 2:

[0129] The method for manufacturing the semiconductor device in the second embodiment is substantially similar to the method for manufacturing the semiconductor device in the first embodiment, and the differences include:

[0130] Step S1 in the first embodiment is modified as follows: forming a drift layer on a substrate and forming a boss on the surface of the drift layer. The specific process of forming the boss may be: after forming the drift layer, forming a boss in the main junction region by RIE etching process, and the height of the boss may be 0.1 μm to 2 μm.

[0131] Alternatively, step S2 in the above-mentioned embodiment 1 is modified as follows: forming grooves, doped regions, and bosses on the surface of the drift layer. The specific process of forming the bosses may be: after forming the grooves and doped regions, using RIE etching process to form bosses in the main junction region, the height of the bosses may be 0.1 μm to 2 μm, and in addition, the depth of each groove under this process needs to be increased by 0.1 μm to 2 μm on the original basis.

[0132] Embodiment three:

[0133] The method for manufacturing the semiconductor device in the third embodiment is substantially similar to the method for manufacturing the semiconductor device in the first embodiment, and the differences include:

[0134] Step S1 in the above-mentioned embodiment 1 is modified to: forming a drift layer on the substrate and forming a boss on the surface of the drift layer. The specific process of forming the boss can be: after forming the drift layer, the same process as forming the first mask layer is used to form a third mask layer with a predetermined pattern, and then the third mask layer in the terminal structure area is thinned by dry etching, and then a wet etching process is used to obtain a third mask layer with the same inclination as the surface of the target terminal structure area, and finally an RIE etching process is used and the etching gas is controlled to vertically bombard the surface of the structure obtained in the above steps, and the surface of the drift layer in the terminal structure area is etched into an inclined surface, and along the first direction, the distance between the inclined surface and the substrate gradually increases; the first direction is: a direction parallel to the substrate surface and away from the main junction area. Further, the third mask layer is removed by wet cleaning.

[0135] The step S2 in the above-mentioned first embodiment is modified as follows: forming a plurality of field limiting rings or a junction terminal extension structure in the area other than the boss on the surface of the drift layer.

[0136] Thus, in the second and third embodiments, by setting a boss, the setting depth of the field limiting ring or the junction terminal extension structure is increased, the absorption effect of avalanche energy is improved, the reliability of the semiconductor device is improved, the manufacturing process is simplified, and the manufacturing cost of the semiconductor device is reduced.

[0137] Based on the same inventive concept, an embodiment of the present invention further provides an electronic device, the implementation principle of which is similar to that of the aforementioned semiconductor device. The specific implementation method of the electronic device can refer to the embodiment of the aforementioned semiconductor device, and the repeated parts will not be repeated.

[0138] Specifically, an electronic device provided by an embodiment of the present invention is Fig.18 As shown, it includes: a semiconductor device 1801 as introduced in the above content.

[0139] Among them, electronic devices can be used in but not limited to: power supplies, photovoltaic systems, industrial motors, electric vehicles, etc.

[0140] Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.

Claims

1. A semiconductor device, characterized in that: include: A substrate, and a drift layer disposed on the substrate, wherein a surface of the drift layer facing away from the substrate is provided with: a main junction region and a terminal structure region, and the terminal structure region includes a junction terminal extension structure; The main junction region is provided with a boss, and the main junction in the main junction region is provided in the boss; The surface of the terminal structure region is an inclined surface, and along a first direction, the distance between the inclined surface and the substrate gradually increases; the first direction is: a direction parallel to the substrate surface and away from the main junction region; Along the first direction, a distance between a surface of the junction termination extension structure close to the substrate and the substrate gradually increases.

2. A semiconductor device, characterized in that: include: A substrate, and a drift layer disposed on the substrate, wherein a surface of the drift layer facing away from the substrate is provided with: a main junction region and a terminal structure region, and the terminal structure region includes a plurality of field limiting rings; The main junction region is provided with a boss, and the main junction in the main junction region is provided in the boss; The surface of the terminal structure region is an inclined surface, and along a first direction, the distance between the inclined surface and the substrate gradually increases; the first direction is: a direction parallel to the substrate surface and away from the main junction region; Along the first direction, a distance between a surface of each field limiting ring close to the substrate and the substrate gradually increases.

3. The semiconductor device according to claim 1 or 2, characterized in that In the terminal structure region, the distance between the side close to the main junction and the side surface of the boss facing away from the substrate is 0.1 μm to 2 μm, and the distance between the side away from the main junction and the side surface of the boss facing away from the substrate is 0.1 μm to 0.5 μm.

4. A method for manufacturing a semiconductor device according to claim 1 or 3, characterized in that: include: epitaxially forming a drift layer on the substrate; forming a boss in a main junction region on a surface of the drift layer on a side away from the substrate; A main junction is formed within the boss, and a junction terminal extension structure is formed in the terminal structure region, so that the surface of the terminal structure region is an inclined surface, and along a first direction, the distance between the inclined surface and the substrate gradually increases; the first direction is: a direction parallel to the substrate surface and away from the main junction region.

5. A method for manufacturing a semiconductor device according to claim 2 or 3, characterized in that: include: epitaxially forming a drift layer on the substrate; forming a boss in a main junction region on a surface of the drift layer on a side away from the substrate; A main junction is formed within the boss, and a plurality of field limiting rings are formed in the terminal structure region, so that the surface of the terminal structure region is an inclined surface, and along a first direction, the distance between the inclined surface and the substrate gradually increases; the first direction is: a direction parallel to the substrate surface and away from the main junction region.

6. An electronic device, characterized in that: Comprising the semiconductor device according to any one of claims 1 to 3.