Display panel and display device

By using a composite material layer in the packaging layer of the OLED display panel and using laser irradiation to flow it to fill the cracks and pinholes in the inorganic layer, the crack problem that occurs during the packaging process of the flexible OLED panel is solved and the sealing and stability are improved. .

CN117794325BActive Publication Date: 2024-10-11HKC CORP LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202311837524.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-12-27
Publication Date
2024-10-11
Estimated Expiration
2043-12-27

AI Technical Summary

Technical Problem

Flexible OLED display panels are prone to pinholes or cracks during the packaging process, leading to packaging failure and affecting its stability and lifespan.

Method used

A composite material layer is introduced into the encapsulation layer, and a combination of airgel material and hot melt adhesive material is used to flow the composite material layer through laser irradiation to fill and repair cracks and pinholes in the inorganic layer to improve sealing ability.

Benefits of technology

It effectively improves the sealing performance of the packaging layer and the stability of the display panel, extends the service life of OLED, and improves the display effect.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117794325B_ABST
    Figure CN117794325B_ABST
Patent Text Reader

Abstract

The present application discloses a display panel and a display device, wherein the display panel includes a substrate, a pixel definition layer, a plurality of light-emitting units and an encapsulation layer; the pixel definition layer is arranged on the substrate and has a plurality of pixel openings; a plurality of the light-emitting units are arranged on the substrate; the encapsulation layer covers the plurality of the light-emitting units and is used to seal the light-emitting units; wherein the encapsulation layer includes a first inorganic layer, a composite material layer, an organic layer, and a second inorganic layer, the composite material layer is arranged on the first inorganic layer, the organic layer is arranged on the composite material layer, and the second inorganic layer is arranged on the organic layer; the composite material layer is used to have fluidity under laser irradiation, and part of the composite material layer flows to fill the cracks generated by the first inorganic layer. The present application reduces the possibility of pinholes or cracks in the encapsulation layer by arranging the composite material layer in the encapsulation layer, thereby improving the encapsulation effect of the display panel.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of display technology, and in particular to a display panel and a display device. Background Art

[0002] Organic light emitting diodes (OLEDs) have the advantages of surface light sources, cold light, energy saving, fast response, flexibility, ultra-lightness and low cost, and their mass production technology is becoming increasingly mature. Since OLEDs have poor stability and are extremely sensitive to water, oxygen and heat, packaging technology is particularly critical. The purpose of packaging is mainly to prevent water vapor and oxygen from entering OLEDs. The current mainstream technologies are cover packaging technology and thin film packaging technology. Cover packaging technology is mainly divided into Frit (glass glue packaging), Dam (isolation dam packaging) and Face seal (surface packaging). Especially for flexible and bendable screens, due to multiple bending and deformation, the packaging layer is prone to cracks, and cracks will accelerate the aging rate of OLED organic light-emitting layer devices. Therefore, strict packaging must be performed to extend the life and improve stability.

[0003] The current encapsulation is mainly achieved by laminating an inorganic layer and an organic layer. However, due to the inevitable appearance of protruding small particles in the preparation of the organic light-emitting unit, the inorganic layer in direct contact with the organic light-emitting unit in the encapsulation layer produces pinholes or cracks, resulting in encapsulation failure and other problems. In view of this, those skilled in the art are in urgent need of a technical solution to the above problems. Summary of the invention

[0004] The purpose of the present application is to provide a display panel and a display device, which reduces the possibility of pinholes or cracks in the encapsulation layer by arranging a composite material layer in the encapsulation layer, thereby improving the encapsulation effect of the display panel.

[0005] The present application discloses a display panel, which includes a base substrate, a pixel definition layer, a plurality of light-emitting units and an encapsulation layer; the pixel definition layer is arranged on the base substrate and has a plurality of pixel openings; the plurality of light-emitting units are arranged on the base substrate and are located in the pixel openings; the encapsulation layer covers the plurality of light-emitting units and is used to seal the light-emitting units; wherein the encapsulation layer includes a first inorganic layer, a composite material layer, an organic layer and a second inorganic layer, the composite material layer is arranged on the first inorganic layer, the organic layer is arranged on the composite material layer, and the second inorganic layer is arranged on the organic layer; the composite material layer is used to have fluidity under laser irradiation, and part of the composite material layer flows to fill cracks generated in the first inorganic layer.

[0006] Optionally, the composite material layer includes an aerogel material layer and a hot melt adhesive material layer, the aerogel material layer wraps the hot melt adhesive material layer, the aerogel material layer generates heat when receiving laser irradiation, and the hot melt adhesive material layer fills the cracks generated in the first inorganic layer after receiving the heat and melting.

[0007] Optionally, the thickness of the aerogel material layer is greater than the thickness of the hot melt adhesive material layer; the thickness of the hot melt adhesive material layer is between 0.3um and 0.6um, and the thickness of the aerogel material layer is between 0.5um and 1um.

[0008] Optionally, the composite material layer further includes a metal material or a metal skeleton material, and the metal material or the metal skeleton material is doped in the aerogel material layer to support the aerogel material layer.

[0009] Optionally, the composite material layer includes a plurality of first composite parts, and the plurality of first composite parts are arranged at intervals and respectively correspond to the pixel openings.

[0010] Optionally, the display panel further includes an eaves structure, which is disposed on the pixel definition layer and is used to separate two adjacent light-emitting units; the composite material layer at least covers the eaves structure.

[0011] Optionally, on the orthographic projection of the base substrate, the width of the composite material layer is smaller than the width of the first inorganic layer, and the width of the composite material layer is larger than the width of the organic layer.

[0012] Optionally, the display panel includes a display area and a non-display area, the display panel also includes a blocking structure, the blocking structure is arranged in the non-display area, the light-emitting unit is arranged in the display area, and the blocking structure is arranged around the display area; the blocking structure is used to block the organic layer from extending to the non-display area; on the blocking structure, the composite material layer is arranged between the first inorganic layer and the second inorganic layer.

[0013] Optionally, in the non-display area, on the orthographic projection of the base substrate, the projection of the composite material layer is located within the projection range of the blocking structure.

[0014] The present application also discloses a display device, comprising a driving circuit and the above-mentioned display panel, wherein the driving circuit is used to drive the display panel to display.

[0015] The first inorganic layer in the encapsulation layer is generally formed directly on the light-emitting unit. Since the light-emitting unit has multiple protruding small particles on the light-emitting unit due to the process technology or film particles during the manufacturing process, it is easy to cause pinholes or cracks in the first inorganic layer when forming the first inorganic layer. The present application provides a composite material layer on the first inorganic layer, and uses the fluidity of the composite material layer under laser irradiation to repair cracks or pinholes that may appear on the first inorganic layer. By repairing the first inorganic layer, the sealing ability of the first inorganic layer is improved, thereby improving the encapsulation effect of the display panel and the display effect of the display panel. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] The included drawings are used to provide a further understanding of the embodiments of the present application, which constitute a part of the specification, are used to illustrate the implementation methods of the present application, and together with the text description, explain the principles of the present application. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work. In the drawings:

[0017] Figure 1 is a schematic diagram of a display panel according to a first embodiment of the present application;

[0018] Figure 2 is a schematic diagram of a composite material layer of the present application;

[0019] Figure 3 is a schematic diagram of a display panel according to a second embodiment of the present application;

[0020] Figure 4 is a schematic diagram of a display panel according to a third embodiment of the present application;

[0021] Figure 5 is a schematic diagram of a display device of the present application.

[0022] Among them, 100, display panel; 101, display area; 102, non-display area; 103, base substrate; 110, pixel definition layer; 111, pixel opening; 120, encapsulation layer; 121, first inorganic layer; 122, organic layer; 123, second inorganic layer; 130, composite material layer; 131, aerogel material layer; 132, hot melt adhesive material layer; 133, first composite part; 140, eaves structure; 141, metal layer; 142, inorganic insulating layer; 150, light-emitting unit; 151, bottom electrode; 152, light-emitting layer; 153, top electrode; 160, blocking structure; 200, display device; 210, driving circuit. DETAILED DESCRIPTION

[0023] It should be understood that the terms used herein, the specific structures and functional details disclosed are only for describing specific embodiments and are representative, but the present application can be implemented in many alternative forms and should not be construed as being limited to only the embodiments described herein.

[0024] In the description of the present application, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating relative importance or implicitly indicating the number of technical features indicated. Therefore, unless otherwise specified, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features; "multiple" means two or more. In addition, the terms "upper", "lower", "left", "right", "vertical", "horizontal", etc. indicating orientation or positional relationships are described based on the orientation or relative positional relationships shown in the accompanying drawings, and are only for the convenience of describing the simplified description of the present application, rather than indicating that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present application. For those of ordinary skill in the art, the specific meanings of the above terms in the present application can be understood according to the specific circumstances.

[0025] Figure 1 is a schematic diagram of a display panel of the first embodiment of the present application, see Figure 1 As shown, the present application discloses a display panel 100, which includes a base substrate 103, a pixel definition layer 110, a plurality of light-emitting units 150 and an encapsulation layer 120; the pixel definition layer 110 is arranged on the base substrate 103 and has a plurality of pixel openings 111; the plurality of light-emitting units 150 are arranged on the base substrate 103 and are located in the pixel openings 111; the encapsulation layer 120 covers the plurality of light-emitting units 150 and is used to seal the light-emitting units 150; wherein the encapsulation layer 120 includes a first inorganic layer 121, a composite material layer 130, an organic layer 122 and a second inorganic layer 123, the composite material layer 130 is arranged on the first inorganic layer 121, the organic layer 122 is arranged on the composite material layer 130, and the second inorganic layer 123 is arranged on the organic layer 122; the composite material layer is used to have fluidity under laser irradiation, and part of the composite material layer flows to fill the cracks generated in the first inorganic layer 121.

[0026] The first inorganic layer 121 in the encapsulation layer 120 is generally formed directly on the light-emitting unit 150. Since the light-emitting unit 150 has multiple protruding small particles due to the process technology or film particles during the manufacturing process, when the first inorganic layer 121 is formed, it is easy to cause pinholes or cracks in the first inorganic layer 121. In the present application, a composite material layer 130 is arranged on the first inorganic layer 121. The composite material layer 130 has fluidity under laser irradiation to repair cracks or pinholes that may appear on the first inorganic layer 121. By repairing the first inorganic layer 121, the sealing ability of the first inorganic layer 121 is improved, thereby improving the encapsulation effect of the display panel 100 and the display effect of the display panel 100.

[0027] Figure 2 is a schematic diagram of the composite material layer of the present application, see Figure 2 As shown, the composite material layer 130 includes an aerogel material layer 131 and a hot melt adhesive material layer 132. The aerogel material layer 131 wraps the hot melt adhesive material layer 132. The aerogel material layer 131 generates heat when receiving laser irradiation. The hot melt adhesive material layer 132 melts after receiving the heat and fills the cracks generated on the side of the packaging layer 120 close to the frame glue.

[0028] The composite material of this embodiment is a combination of an aerogel material and a hot-melt adhesive material. The aerogel material generates heat after receiving electromagnetic waves such as lasers. The hot-melt adhesive material melts after absorbing the heat, flows out of the aerogel material, and fills the cracks. Since the hot-melt adhesive material itself is a kind of adhesive, it has the property of bonding the cracks, thereby achieving the repair of the packaging layer 120.

[0029] Aerogel material is currently the most efficient and energy-saving thermal insulation material. Specifically, it is a solid material with a nanoporous network structure and filled with a gaseous dispersion medium in the gaps. It is the world's lowest density solid and is called "solidified smoke". Due to its unique structure, aerogel materials have demonstrated excellent performance in many fields such as thermal, acoustic, optical, electrical and mechanical. Different compounds form a variety of aerogel materials through the preparation process of aerogel, enriching the variety of aerogel materials. The present application mainly utilizes the electromagnetic shielding properties of aerogels for electromagnetic waves. For example, aerogel materials have the ability to convert into thermal energy after absorbing lasers, such as graphene aerogel materials or doped graphene aerogel materials. Doped graphene aerogel materials include GF / PDMS polydimethylsiloxane. The above materials can absorb electromagnetic waves and convert them into thermal energy.

[0030] In this embodiment, the aerogel material includes one or more materials of graphene aerogel material doped with polydimethylsiloxane, one-dimensional carbon nanotubes (CNTs) and multidimensional graphene-based aerogel (NiCo / C / CNT / rGO aerogel) material modified with metal organic framework (MOF) derivatives.

[0031] The hot melt adhesive material layer 132 can be made of hot melt adhesive material made of polyester as the main raw material. Polyester (PES) refers to the general term for polymers containing ester groups (—COO—) in the main chain, which can be divided into two categories: unsaturated polyester and thermoplastic polyester. When polyester is used as a hot melt adhesive matrix, thermoplastic polyester, that is, linear saturated polyester, should be selected as the hot melt adhesive matrix raw material, which is usually formed by condensation of dicarboxylic acid and diol or alkyd. PES hot melt adhesive film is generally milky white or transparent.

[0032] The present application uses a wrapping method to completely wrap the hot melt adhesive material with the outer aerogel material. When the hot melt adhesive material is not needed, the heat insulation properties of the aerogel material are used to prevent the hot melt adhesive material from being affected by the thermal effects of other film layers, causing the emission of partial melting, resulting in the hot melt adhesive material directly liquefying and flowing out into the gap between the film layers of the display panel 100. The present application uses an aerogel wrapping method. On the one hand, the heat insulation properties of the aerogel material are used to prevent the hot melt adhesive material from being disturbed by the outside world when it is not needed. On the other hand, the aerogel material has a certain buffering capacity, which can buffer the impact force transmitted to the packaging layer 120 during the rigid packaging process to prevent the film layer from breaking.

[0033] It is worth mentioning that the aerogel material layer also has excellent heat insulation capabilities. When the aerogel material layer is irradiated with a laser, the aerogel material layer stores most of the heat and converts the absorbed laser into heat energy to be maintained internally. Due to the low thermal conductivity of aerogel, its surrounding film layer will not be affected by heat, while the internal heat energy is absorbed by the hot melt adhesive material layer and flows out from the porous gaps of the aerogel material layer. The melting temperature of the hot melt adhesive material layer can be around 50 degrees Celsius to 80 degrees Celsius. In actual applications, when there is no ultraviolet light irradiation, the aerogel material layer does not absorb visible light and does not generate heat, but the aerogel material layer has a heat insulation effect, so even if the outside is high in temperature, it will not affect the inside. Only after the aerogel material layer itself absorbs heat and generates high temperature can it be transferred to the inside.

[0034] Due to the characteristics of flexible packaging, the display panel 100 of the present application may have film defects on the surface of each film layer of the display panel 100, which may lead to the failure of the packaging of the packaging layer 120. This will be reflected in the display area 101 as regional pixel luminescence display abnormality. By detecting the pixel luminescence current size or light intensity in the pixel circuit, it can be fed back whether there is water vapor entering. When the change value reaches the limit value, it means that there is a possibility of packaging failure around this place. In this regard, the composite material layer 130 can be irradiated with laser in a directional manner. The outer aerogel material layer 131 will absorb the laser and convert the absorbed laser into heat energy to be retained inside. Since the aerogel material layer also has a low thermal conductivity, its surrounding film layer will not be affected by heat. After the internal heat of the aerogel material layer 131 is accumulated, the hot melt adhesive material layer is melted by heat and drips through the gap of the aerogel material layer under the action of gravity. The dripping hot melt adhesive material layer will flow into the position where the crack exists to fill it, and solidify and form after cooling. When there is no crack, the hot melt adhesive will continue to be stored inside the aerogel, and it can continue to be heated and used later. Since the aerogel material layer has good electromagnetic wave absorption ability and thermal insulation properties, the heat utilization rate required for the aerogel material layer to heat the hot melt adhesive material layer is very high, and only a small amount of laser irradiation is required. This heating method is safe and harmless and will not cause any impact or damage to internal devices.

[0035] The thickness of the hot melt adhesive material layer 132 is between 0.3um and 0.6um, and the thickness of the aerogel material layer is between 0.5um and 1um. Since the aerogel material layer is included in the hot melt adhesive material layer, aerogel material layers are respectively provided on the upper and lower sides of the hot melt adhesive, and the thickness of the aerogel material layers is respectively between 0.5um and 1um. That is, the thickness of the composite material is 1.3-2.6um. The aerogel material layer can also support the internal hot melt adhesive by adding a skeleton structure with a certain strength, such as the metal organic framework (MOF) mentioned above.

[0036] Continue to see Figure 1 As shown, the light-emitting unit 150 generally includes a bottom electrode 151, an organic light-emitting layer 152 and a top electrode 153. The organic light-emitting layer 152 is generally formed of an organic light-emitting material, including but not limited to an electron injection layer, an electron parameter layer, a light-emitting layer 152, a hole transport layer and a hole injection layer. The electric field generated by the bottom electrode 151 and the top electrode 153 drives holes and electrons in the light-emitting layer 152 to be excited to emit light, which has the characteristic of self-luminescence. The bottom electrode 151 is generally called an anode, and the top electrode 153 is generally called a cathode.

[0037] In the actual manufacturing process, due to the different materials of the film layers in the organic light-emitting layer 152, the different film layers in the light-emitting area and the gap, and process problems, the organic light-emitting layer 152 in the display area 101 is uneven in actual situations, with some grooves and protrusions, and these grooves and protrusions have a certain randomness and cannot be predicted. The degree of the grooves and protrusions varies, and the maximum step difference can reach the micron level. Therefore, the first inorganic layer 121 above will have ups and downs. The groove position with a large step difference will have the problem of uneven film quality, and the film layer is prone to cracking, which will greatly damage the passivation packaging effect of the first inorganic layer 121.

[0038] At the same time, due to the process of preparing the light-emitting unit 150 device, some unavoidable protruding small particles (Particles) have appeared on the surface of the film layer before the top electrode 153 is plated. Because the cathode metal layer 141 is very thin, these protruding small particles are enough to pierce the ITO and cause pinholes in the ITO in the top electrode 153. Because the film thickness of the first inorganic layer 121 cannot be made thicker, and the sizes of these particles are uneven, some particles may not be completely covered after being encapsulated by the first inorganic layer 121 and are partially exposed. Some small particles will form pinholes after being covered. There will be pinholes and exposed particles on the surface of the film layer of the first inorganic layer 121, and there will be fine cracks in the film layer around these particles. The presence of these pinholes and cracks will also reduce the strength and sealing of the film layer. When the acrylic organic encapsulation layer 120 is cured on top of these film layers, the acrylic will fill the pinholes and cracks, and the water vapor path will directly invade along these interfaces, causing direct failure of the device.

[0039] The aerogel material layer 131 in the composite material layer 130 of the present application is in direct contact with the first inorganic layer 121. Even if there are particles on the first inorganic layer 121, the aerogel material layer 131 has a certain buffering capacity, so that there is no problem of cracks between the first inorganic layer 121 and the organic layer 122 extending to the organic layer 122.

[0040] In a further solution of the present application, the organic layer 122 in the encapsulation layer 120 can be removed, and a thicker aerogel material layer 131 can be used to replace the organic layer 122. The porous structure in the aerogel material layer 131 plays a buffering role, and the porous structure also has a certain ability to store water vapor, which can improve the encapsulation effect between the first inorganic layer 121 and the second inorganic layer 123. Especially for curved screens or folding screens, the aerogel material layer 131 has strong ductility, which can well protect the encapsulation layer 120 from breaking during folding and bending, thereby improving the encapsulation effect of the display panel 100.

[0041] The display panel 100 includes a display area 101 and a non-display area 102. A plurality of light-emitting units 150 are arranged in an array in the display area 101. The encapsulation layer 120 extends from the display area 101 to the non-display area 102. In the display area 101, the encapsulation layer 120 mainly prevents water vapor from invading the light-emitting unit 150 through a three-layer structure of a laminated inorganic material and an organic material. In the non-display area 102, two layers of inorganic materials, i.e., a first inorganic layer 121 and a second inorganic layer 123, are laminated to prevent water vapor from invading from the side.

[0042] Specifically, on the orthographic projection of the base substrate 103, the width of the composite material layer 130 is smaller than the width of the first inorganic layer 121, and the width of the composite material layer 130 is larger than the width of the organic layer 122. The composite material layer 130 also extends to the non-display area 102 and is disposed between the first inorganic layer 121 and the second inorganic layer 123, but the organic layer 122 is at the edge of the display area 101 or slightly exceeds the display area 101 and is blocked by the blocking structure 160.

[0043] In one embodiment, for the composite material layer 130 in the display area 101 , the composite material layer 130 may be configured as a film layer with multiple segments arranged at intervals, specifically including multiple segments of first composite parts 133 , wherein the multiple segments of the first composite parts 133 are arranged at intervals and respectively correspond to the pixel openings 111 .

[0044] In this embodiment, the composite material layer 130 can be arranged in sections, and the first composite part 133 is only arranged at the position of the pixel opening 111 corresponding to the light-emitting unit 150. The first composite part 133 is used to repair the pinholes and cracks of the first inorganic layer 121 on the light-emitting unit 150, thereby achieving accurate repair and saving materials.

[0045] Figure 3 is a schematic diagram of a display panel of the second embodiment of the present application, see Figure 3 As shown, in this embodiment, with respect to the first inorganic layer 121 and the second inorganic layer 123 in the non-display area 102 , a composite material layer 130 may be disposed between the first inorganic layer 121 and the second inorganic layer 123 .

[0046] Specifically, the display panel 100 further includes a blocking structure 160 , which is disposed in the non-display area 102 and surrounds the display area 101 . The main function of the blocking structure 160 is to block the organic layer 122 from flowing toward the non-display area 102 .

[0047] Among them, the first inorganic layer 121 and the second inorganic layer 123 in the encapsulation layer 120 are generally formed by a vapor deposition process, and the process of the organic layer 122 is generally selected to be inkjet printing, and the organic material is combined with a solvent to form an ink to form it on the first inorganic layer 121. Because there is a gap between the print heads in inkjet printing, the organic layer 122 in inkjet printing needs to be statically leveled so that the ink of the organic material is completely spread on the light-emitting unit 150 layer to form a covering package. Since the ink has a certain fluidity, it will flow to the non-display area 102, so a blocking structure 160 is set to prevent the ink of the organic material from flowing to the non-display area 102. Generally speaking, the height of the blocking structure 160 will be higher than the film height of the organic layer 122.

[0048] In this solution, on the blocking structure 160, the composite material layer 130 is disposed between the first inorganic layer 121 and the second inorganic layer 123. By disposing the composite material layer 130 between the first inorganic layer 121 and the second inorganic layer 123, the porous structure in the aerogel material layer in the composite material layer 130 has a certain buffering capacity, which can reduce the stress between the membrane layers.

[0049] Specifically, due to the effect of the barrier structure 160, local stress concentration will occur between the film layers in the encapsulation layer 120, or the film layers will be deformed to varying degrees under the effect of external mechanical forces, which can easily lead to microcracks in the encapsulation layer 120, forming water and oxygen channels, and thus causing the light-emitting unit 150 layer to fail. The important thing about this solution is that a film layer with a porous structure is arranged between the first inorganic layer 121 and the second inorganic layer 123 to disperse the stress generated at the encapsulation barrier layer, prevent unexpected cracks from occurring in the film layers in the encapsulation layer 120, and thus improve the sealing reliability of the encapsulation layer 120. Moreover, the composite material layer 130 has a certain toughness, which can enhance the overall encapsulation strength of the encapsulation area, prevent damage to the encapsulation layer 120 during assembly or subsequent processes, thereby improving the quality and strength of the display panel 100. On the other hand, when the aerogel material layer 131 is subsequently irradiated by electromagnetic waves or lasers, the hot melt adhesive material layer 132 in the composite material layer 130 absorbs the heat generated by the aerogel material layer 131 and melts, thereby sealing the microcracks generated on the first inorganic layer 121 or the second inorganic layer 123, thereby enhancing the packaging effect.

[0050] Furthermore, the cross-sectional view of the barrier structure 160 is a trapezoid, which has four corners. At the four corners, the barrier structure 160 and the adjacent film layer are turned, and have a convex obtuse angle or acute angle. Due to the effect of the obtuse angle and the acute angle, the first inorganic layer 121 covering the barrier structure 160 will have a strong stress. In this regard, the present solution allows the composite material layer 130 to cover at least the four corners of the barrier structure 160.

[0051] Moreover, since the stress at the corner position is strong, especially in a high temperature environment, the film layer will be deformed differently after being heated, which will cause film separation at the corner position. If film separation occurs at the corner position, water vapor will enter through the film separation position. In this solution, an aerogel material layer 131 is provided at the corner position to prevent film separation from occurring at the corner position. Even if film separation occurs, the hot melt adhesive material layer can be used for filling.

[0052] In another embodiment, in the non-display area 102, on the orthographic projection of the base substrate 103, the projection of the composite material layer 130 is located within the projection range of the blocking structure 160. The blocking structure 160 is arranged around the display area 101, and there are multiple blocking structures 160. By covering the composite material layer 130 with multiple blocking structures 160, the film problem of the first inorganic layer 121 and the second inorganic layer 123 at the position of the blocking structure 160 is improved.

[0053] Figure 4 is a schematic diagram of a display panel of the third embodiment of the present application, see Figure 4 As shown, based on the previous embodiment, this embodiment further adds an eaves structure 140, which is arranged on the pixel definition layer 110 to separate two adjacent light-emitting units 150. The purpose of the eaves structure 140 is to realize mask removal evaporation and realize the process of the light-emitting unit 150. Patterning pixels through maskless deposition and photolithography technology can effectively drive the metal mask evaporation process. In order to achieve high resolution and colorization of passive matrix OLEDs and better solve the problems of low cathode template resolution and low device yield, a cathode isolation column structure was introduced in actual research. That is, a metal template is not used in device preparation. Instead, an insulating partition is made on the substrate before evaporating the organic film and the cathode. Ultimately, different pixels of the device are separated to achieve a pixel array. The shape of the isolation column is the key to the isolation effect. The base insulating buffer layer is used to solve the short-circuit problem of the anode between pixels. The PDL layer is used to isolate the anodes between different pixels. At the same time, an inverted trapezoidal isolation column is used to solve the short-circuit problem of the organic light-emitting layer 152 between adjacent pixels. This inverted trapezoidal isolation column is also called an eaves structure 140 or a hanging structure.

[0054] The general preparation process includes forming an anode on the substrate 103, etching the anode to form a required pattern, and then preparing a pixel definition layer 110. The pixel definition layer 110 serves as an insulating base for the overhang structure, and is used to isolate the anodes of adjacent light-emitting units 150. A overhang structure is formed on the pixel definition layer 110. The overhang structure consists of two parts, including a metal layer 141 at the lower layer, which can also be made of metal oxide or transition metal oxide, and an inorganic insulating layer 142 at the upper layer. The inorganic insulating layer 142 has an inverted trapezoidal or mushroom shape, and can be formed of silicon dioxide, silicon nitride, or silicon oxynitride. Different materials have different etching rates to form the above-mentioned mushroom shape. After the overhang structure is completed, the organic light-emitting layer 152 (OLED) material and the cathode are deposited on the substrate by evaporation deposition. The OLED material is arranged on the anode and in direct contact with the anode. Due to the existence of the overhang structure, the organic light-emitting layer 152 and the cathode can be deposited in a faulted manner at the bottom. After a single pixel is formed by a single etching, the single-color OLED material and the cathode are encapsulated and protected by the inorganic encapsulation layer 120 to form an etching protection layer, and then other organic light-emitting layers 152 and cathodes are prepared one by one. After the three-color organic light-emitting layer 152 and the cathode are all patterned, the organic encapsulation layer 120 and the inorganic encapsulation layer 120 are used for overall encapsulation.

[0055] Specifically, the composite material layer 130 is arranged to at least cover the eaves structure 140. In this solution, the composite material layer 130 is formed on the overhang structure, specifically, it is arranged on the first inorganic layer 121 on the overhang structure and directly contacts the first inorganic layer 121. The composite material layer 130 can fully wrap the groove in the pixel opening 111 and the top of the overhang structure, which can greatly improve the stability of the interface overlap between the inorganic layer and the organic layer 122 in the overhang structure. Due to the high elasticity and high ductility of the aerogel, it can also cope with the risk of cracking and failure of the top film layer of the overhang structure when the display screen is deformed such as folding or bending.

[0056] Figure 5 is a schematic diagram of the display device of the present application, see Figure 5 As shown, the present application discloses a display device, wherein the display device 200 includes a display panel 100 and a driving circuit 210 in any of the above embodiments, wherein the driving circuit 210 is used to drive the display panel 100 to display. The display panel 100 in this solution is generally an organic light-emitting display panel 100.

[0057] The first inorganic layer 121 in the encapsulation layer 120 is generally formed directly on the light-emitting unit 150. Since the light-emitting unit 150 has multiple protruding small particles on it due to the process technology or film particles during the manufacturing process, when the first inorganic layer 121 is formed, it is easy to cause pinholes or cracks in the first inorganic layer 121. In the present application, a composite material layer 130 is arranged on the first inorganic layer 121. The composite material layer 130 has fluidity under laser irradiation to repair cracks or pinholes that may appear on the first inorganic layer 121. By repairing the first inorganic layer 121, the sealing ability of the first inorganic layer 121 is improved, thereby improving the encapsulation effect of the display panel 100 and the display effect of the display panel 100.

[0058] It should be noted that the inventive concept of the present application can form a large number of embodiments, but the length of the application document is limited and it is impossible to list them one by one. Therefore, under the premise of no conflict, the embodiments or technical features described above can be arbitrarily combined to form new embodiments. After the embodiments or technical features are combined, the original technical effects will be enhanced.

[0059] The above content is a further detailed description of the present application in combination with specific optional implementation methods, and it cannot be determined that the specific implementation of the present application is limited to these descriptions. For ordinary technicians in the technical field to which the present application belongs, several simple deductions or substitutions can be made without departing from the concept of the present application, which should be deemed to fall within the scope of protection of the present application.

Claims

1. A display panel, characterized in that: The display panel comprises: substrate substrate; A pixel definition layer, disposed on the base substrate, having a plurality of pixel openings; A plurality of light emitting units are disposed on the base substrate and located in the pixel opening; and an encapsulation layer, covering the plurality of light-emitting units and used for sealing the light-emitting units; The encapsulation layer includes a first inorganic layer, a composite material layer, an organic layer, and a second inorganic layer. The composite material layer is disposed on the first inorganic layer, the organic layer is disposed on the composite material layer, and the second inorganic layer is disposed on the organic layer; The composite material layer has fluidity under laser irradiation, and a portion of the composite material layer flows to fill cracks generated in the first inorganic layer; The composite material layer includes an aerogel material layer and a hot melt adhesive material layer, wherein the aerogel material layer wraps the hot melt adhesive material layer, the aerogel material layer generates heat when receiving laser irradiation, and the hot melt adhesive material layer melts after receiving the heat to fill the cracks generated in the first inorganic layer; The composite material layer further includes a metal material, which is doped in the aerogel material layer to support the aerogel material layer.

2. The display panel according to claim 1, characterized in that: The thickness of the aerogel material layer is greater than the thickness of the hot melt adhesive material layer; The thickness of the hot melt adhesive material layer is between 0.3um and 0.6um, and the thickness of the aerogel material layer is between 0.5um and 1um.

3. The display panel according to claim 1, characterized in that: The composite material layer includes a plurality of first composite parts, and the plurality of first composite parts are arranged at intervals and respectively correspond to the pixel openings.

4. The display panel according to claim 1, characterized in that: The display panel further comprises an eaves structure, which is arranged on the pixel definition layer and is used to separate two adjacent light-emitting units; The composite material layer at least covers the eaves structure.

5. The display panel according to claim 1, characterized in that: On the orthographic projection of the base substrate, the width of the composite material layer is smaller than the width of the first inorganic layer, and the width of the composite material layer is larger than the width of the organic layer.

6. The display panel according to claim 5, characterized in that: The display panel includes a display area and a non-display area, and the display panel further includes a blocking structure, the blocking structure is arranged in the non-display area, the light emitting unit is arranged in the display area, and the blocking structure is arranged around the display area; the blocking structure is used to block the organic layer from extending to the non-display area; On the barrier structure, the composite material layer is disposed between the first inorganic layer and the second inorganic layer.

7. The display panel according to claim 6, characterized in that: In the non-display area, on the orthographic projection of the base substrate, the projection of the composite material layer is located within the projection range of the blocking structure.

8. A display device, characterized in that: It comprises a driving circuit and the display panel according to any one of claims 1 to 7, wherein the driving circuit is used to drive the display panel to display.

Citation Information

Patent Citations

  • A display device and a method of making the same

    CN102931210A

  • Organic light emitting display panel and display device

    CN107170777A

  • Display panel and display device

    CN112289954A

  • Display panel and display device

    CN116828920A