Destabilizing agent for softening and removing hardness of concentrated brine and preparation method thereof

By preparing a destabilizing agent for flocculant ion precipitation under alkaline conditions, it combines with calcium, magnesium, and silicate ions in concentrated brine to destroy its stable complex structure, thus solving the problem of poor hardness removal effect and high cost in concentrated brine. problem, achieving the effect of reducing the dosage of chemicals and operating costs.

CN117865365BActive Publication Date: 2024-10-18UNIV OF SCI & TECH BEIJING
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
CN202311754658.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-12-19
Publication Date
2024-10-18
Estimated Expiration
2043-12-19

AI Technical Summary

Technical Problem

The existing technology has poor hardness removal effect in concentrated brine, large dosage, and high cost. Calcium, magnesium, and silicon scaling in the concentrated evaporation and crystallization system leads to reduced heat transfer efficiency and equipment clogging, affecting the economy and stability of the process.

Method used

Under alkaline conditions, flocculant ions form flocculated precipitates on the surface of the loaded sediment to prepare a destabilizing agent, which combines with calcium, magnesium, and silicate ions in concentrated brine through oxygen bridging to destroy its stable complex structure and achieve The settlement and destabilization of the complex reduce the dosage of subsequent double-alkali softening agents.

Benefits of technology

It can effectively change the form of calcium, magnesium and silicate ions in concentrated brine, reduce the dosage of softening and hardening agents in the double alkali method, reduce operating costs, and is suitable for industrial production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117865365B_ABST
    Figure CN117865365B_ABST
Patent Text Reader

Abstract

The present invention relates to the technical field of water treatment, and in particular to a destabilizing agent for softening and removing hardness of concentrated brine and a preparation method thereof. The preparation method comprises: under alkaline conditions, flocculant ions form flocculation precipitation on the surface of a load precipitation to obtain the destabilizing agent; the load precipitation is a precipitation corresponding to the flocculant ions and / or salt ions; the salt ions are one or more of magnesium ions, calcium ions, silicate ions, iron ions, and aluminum ions; the pH value of the alkaline condition is 10-12. The preparation method is simple to operate, has high yield, and low cost. The obtained destabilizing agent can change the form of calcium, magnesium, and silicate ions in concentrated brine after being applied to concentrated brine, realize the destabilization of calcium, magnesium, and silicate ions in a complex environment, reduce the dosage of the subsequent double-alkali method for softening and removing hardness, reduce the operating cost, and is suitable for large-scale industrial production and promotion and application.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of water treatment, and in particular to a destabilizing agent for softening and removing hardness of concentrated brine and a preparation method thereof. Background Art

[0002] As membrane technology becomes more mature and material costs gradually decrease, membrane separation has been widely used in sewage treatment, desalination, industrial separation and other fields. Reverse osmosis technology is a common seawater desalination technology. By applying a pressure greater than the seawater osmotic pressure on the seawater side, water molecules are allowed to pass through the membrane while salt is intercepted, thereby converting seawater into fresh water and concentrated brine. In addition, in recent years, the national environmental policy has become stricter, and zero discharge has become an important development direction for wastewater treatment in various industrial sectors. Wastewater zero discharge technology is to completely reuse the generated wastewater after treatment, ensure that no waste liquid is discharged, maximize the use of water resources, and further reduce the use of new water. The zero discharge process mostly uses the three-stage process of "reverse osmosis membrane concentration + secondary concentration + evaporation crystallization" for harmless treatment of wastewater and resource recovery. However, the total hardness and silicon content in the concentrated brine are high. If they are not effectively removed, not only will scaling occur on the concentrated water side, damaging the membrane service life and equipment performance, but also affecting the subsequent secondary concentration of water recovery rate. At the same time, the calcium-magnesium-silicon scaling formed in the concentrated evaporation crystallization system will lead to reduced heat transfer efficiency, equipment blockage, excessive temperature and other problems, damage system-related equipment, and affect the economy and stability of the overall process. Conventional softening technology mainly uses the double alkali method for softening, but this method has poor hardness removal effect in high-salt systems, large dosage, and high cost; after the concentrated brine is de-hardened, acid needs to be added to adjust it to neutral, and secondary reverse osmosis concentration is performed, which has high operating costs. In addition, the residence time of water body de-hardening is long, the de-hardening process occupies a large area, and the construction cost of the pretreatment softening process is high. Summary of the invention

[0003] In order to solve or partially solve the problems existing in the related art, the present invention provides a destabilizing agent for softening and removing hardness of concentrated brine and a preparation method thereof.

[0004] The present invention provides a method for preparing a destabilizing agent for softening and removing hardness of concentrated brine, which comprises the following steps:

[0005] Under alkaline conditions, flocculant ions form flocculated precipitation on the surface of the loaded precipitation to obtain the destabilizing agent; the loaded precipitation is a precipitation corresponding to the flocculant ions and / or salt ions; the salt ions are one or more of magnesium ions, calcium ions, silicate ions, iron ions, and aluminum ions; the pH value of the alkaline conditions is 10-12.

[0006] Furthermore, the flocculant ions are iron ions and / or aluminum ions.

[0007] Furthermore, the load carrier is one or more of calcium carbonate, aluminum oxide, magnesium oxide, calcium oxide, and magnesium hydroxide.

[0008] Furthermore, the specific operation of flocculant ions forming flocculation precipitation on the surface of the loaded precipitation under alkaline conditions is Scheme I or Scheme II;

[0009] The scheme I is: mixing a first mixed solution containing salt ions and flocculant ions with an alkaline solution to obtain a reaction solution; reacting the reaction solution under heating conditions; during the reaction, synthesizing the load precipitate in situ and forming a flocculated precipitate on the surface of the load precipitate; or,

[0010] The scheme II is as follows: adding the second mixed solution containing flocculant ions and the loaded precipitate into an alkaline solution to obtain a reaction solution; reacting the reaction solution under heating conditions; during the reaction, the flocculant ions form flocculated precipitates on the surface of the loaded precipitate;

[0011] In the schemes I and II, the pH value of the reaction solution is 10-12.

[0012] Furthermore, the alkaline solution includes CO3 2- and OH - .

[0013] Furthermore, the second mixed solution also contains the salt ions.

[0014] Furthermore, the salt ions are from magnesium sulfate, magnesium nitrate, magnesium chloride, calcium chloride or silicate.

[0015] Furthermore, the reaction temperature is 50°C to 200°C, specifically comprising: carrying out a normal pressure reaction under heating conditions, and then heating and pressurizing to carry out a high pressure reaction.

[0016] The present invention also provides a destabilizing agent for softening and removing hardness of concentrated brine, which is prepared according to any one of the methods described above.

[0017] The present invention also provides a method for softening concentrated brine, comprising:

[0018] Add the above destabilizing agent into the reverse osmosis concentrated brine, stir and mix, separate the solid and liquid, and obtain pretreated wastewater;

[0019] The pretreated wastewater is softened by a double alkali method.

[0020] The preparation method of the destabilizing agent for softening and removing hardness of concentrated brine provided by the present invention may have the following beneficial effects:

[0021] The preparation method uses the precipitate corresponding to the flocculant ion and / or the salt ion as a carrier. Under alkaline conditions, the flocculant ion is precipitated to the carrier surface and connected through oxygen bridging. The destabilizer surface prepared in this way has many hydroxyls and can be combined with the complex originally combined with calcium, magnesium and silicate ions in the concentrated brine to destroy the original stable complex structure of calcium and magnesium ions. At the same time, the destabilizer is hydrolyzed and polycondensed by the surface flocculant to exert the flocculation and coagulation effect. Through adsorption bridging and net capture and sweeping, the load carrier in the brine and the complex adsorbed on the surface are aggregated and precipitated together, so that the calcium, magnesium and silicate ions in the solution are destabilized, and the originally complexed calcium, magnesium and silicate ions are released again into the brine system, thereby strengthening the softening and hardness removal effect of the subsequent double-alkali method and reducing the dosage of the double-alkali agent.

[0022] The preparation method provided by the present invention is simple to operate, high in yield and low in cost. The obtained destabilizing agent can change the forms of calcium, magnesium and silicate ions in the concentrated brine after being applied to the concentrated brine, thereby achieving destabilization of the calcium, magnesium and silicate ions in a complex environment, reducing the dosage of the double alkali agent for subsequent softening and dehardening by the double alkali method, reducing the operating cost, and being suitable for large-scale industrial production and promotion and application.

[0023] It is to be understood that the foregoing general description and the following detailed description are exemplary and explanatory only and are not restrictive of the invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] The above and other objects, features and advantages of the present invention will become more apparent through a more detailed description of exemplary embodiments of the present invention in conjunction with the accompanying drawings, wherein like reference numerals generally represent like components throughout the exemplary embodiments of the present invention.

[0025] Figure 1 This is a schematic diagram of the working principle of the destabilizing agent provided by the present invention;

[0026] Figure 2 is a scanning electron microscope image of the destabilizing agent prepared in Example 1 of the present invention;

[0027] Figure 3 is the XRD pattern of the destabilizing agent prepared in Example 1 of the present invention;

[0028] Figure 4 is a scanning electron microscope image of the destabilizing agent prepared in Example 2 of the present invention;

[0029] Figure 5 It is a comparison diagram of the change of calcium ion concentration in reverse osmosis concentrated water after destabilization treatment using the destabilizing agent prepared by the embodiment of the present invention and the dosage of the double alkali method. DETAILED DESCRIPTION

[0030] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0031] The terms used in the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The singular forms "a", "the" and "the" used in the present invention and the appended claims are also intended to include plural forms unless the context clearly indicates other meanings. It should also be understood that the term "and / or" used herein refers to and includes any or all possible combinations of one or more associated listed items.

[0032] It should be understood that although the terms "first", "second", "third", etc. may be used to describe various information in the present invention, such information should not be limited to these terms. These terms are only used to distinguish the same type of information from each other. For example, without departing from the scope of the present invention, the first information may also be referred to as the second information, and similarly, the second information may also be referred to as the first information. Thus, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "multiple" is two or more, unless otherwise clearly and specifically defined.

[0033] The inventor of the present application has found through research that the main reasons for the poor softening and hardness removal effect of the double alkali method and the high double alkali dosage are: the concentrated brine has high salt content, high COD, and complex components, which changes the equilibrium law of complex dissociation and crystal precipitation in the solution, inhibiting the crystal precipitation of calcium, magnesium, and silicate ions, resulting in poor hardness removal effect and high double alkali dosage. Therefore, the present invention considers breaking the stable binding relationship between calcium, magnesium, and silicate and the complex, and releasing the originally complexed calcium, magnesium, and silicate ions back into the brine system, that is, considering destroying the stability of the above-mentioned ion complex, so that the above-mentioned salt ions can be easily removed in the subsequent double alkali softening process. Furthermore, the inventors of the present application considered providing a destabilizing agent, which can be combined with the above-mentioned complex and further form precipitation and sedimentation, thereby separating the complex originally combined with calcium, magnesium and silicate ions from the brine system, thereby changing the complex form of calcium, magnesium and silicate ions in the concentrated brine, destroying the stability of calcium, magnesium and silicate ions in the high salt system, strengthening the subsequent double alkali method for softening and dehardening, and reducing the dosage of the double alkali agent.

[0034] Based on the above inventive concept, an embodiment of the present invention provides a method for preparing a destabilizing agent for softening and removing hardness of concentrated brine, which comprises the following steps:

[0035] Under alkaline conditions, flocculant ions form flocculated precipitation on the surface of the loaded precipitation to obtain the destabilizing agent; the loaded precipitation is a precipitation corresponding to the flocculant ions and / or salt ions; the salt ions are one or more of magnesium ions, calcium ions, silicate ions, iron ions, and aluminum ions; the pH value of the alkaline conditions is 10-12.

[0036] The flocculant ions are precipitated to the carrier surface under alkaline conditions, and the structure of the destabilizer formed is as follows: Figure 1 As shown in Figure A, the destabilizer has many hydroxyl groups on its surface, which can combine with the complexes originally combined with calcium, magnesium and silicate ions in the salt water to destroy the original stable complex structure of calcium and magnesium ions; at the same time, the destabilizer hydrolyzes and polycondenses through the surface flocculant to play a flocculation and coagulation role, and aggregates and settles the load carrier in the salt water and the complex adsorbed on its surface through adsorption bridging and net capture and sweeping, forming a Figure 1 The mechanism shown in A' in the middle destabilizes the calcium, magnesium and silicate ions in the solution at the same time, which is beneficial to the subsequent double alkali method for hardness removal.

[0037] The above-mentioned flocculant ions are preferably iron ions and / or aluminum ions, preferably including iron ions and aluminum ions at the same time, which helps to strengthen the flocculation effect. The iron ions can come from polyferric sulfate or ferric chloride; the aluminum ions can come from aluminum sulfate. The above-mentioned load precipitation is combined with the complex on the one hand, and on the other hand serves as a matrix for the growth of flocculant precipitation. The load precipitation is a precipitation corresponding to the flocculant ions and / or salt ions, which can be one or more of calcium carbonate, aluminum oxide, magnesium oxide, calcium oxide, and magnesium hydroxide. The load carrier is more preferably a precipitation corresponding to the salt ion, because the salt ion precipitation is more easily combined with the complex. The pH value of the above-mentioned alkaline condition is 10-12, that is, a strong alkaline condition, under which it is helpful for the carrier surface hydroxylation and the hydrolysis of iron ions and / or aluminum ions to form polyhydroxy compounds, which are connected by oxygen bridging. The pH value of the alkaline condition is most preferably 10-12.

[0038] The above-mentioned loaded precipitate can be directly added to the alkaline environment in the form of a precipitate, or can also be synthesized in situ. Specifically, the specific operation of the flocculant ions forming a flocculated precipitate on the surface of the loaded precipitate under alkaline conditions can be Scheme I or Scheme II;

[0039] Scheme I is: mixing a first mixed solution containing salt ions and flocculant ions with an alkaline solution to obtain a reaction solution; reacting the reaction solution under heating conditions; during the reaction, synthesizing the load precipitate in situ and forming a flocculated precipitate on the surface of the load precipitate;

[0040] Scheme II is: adding the second mixed solution containing flocculant ions and the load precipitate into an alkaline solution to obtain a reaction solution; reacting the reaction solution under heating conditions; during the reaction, the flocculant ions form flocculated precipitates on the surface of the load precipitate;

[0041] In the schemes I and II, the pH value of the reaction solution is 10-12.

[0042] The above scheme I is a scheme for in-situ synthesis of loaded precipitates, and scheme II is a scheme for direct addition. This embodiment preferably adopts scheme II, and the second mixed solution in this scheme preferably also includes the above salt ions, which helps to form more loaded precipitates through in-situ synthesis during the reaction process. The above salt ions are preferably from magnesium sulfate, magnesium nitrate, magnesium chloride, calcium chloride or silicate. The above alkaline solution includes CO3 2- and OH - , that is, in addition to containing OH - In addition, CO3 2 , it is easier to combine with the above salt ions and flocculant ions to form precipitation, and the water solubility of the formed precipitation is worse, so the alkaline solution contains, which is conducive to forming more loaded precipitation and flocculation precipitation. The molar ratio in the alkaline solution is preferably (1-4):5, more preferably 3:5.

[0043] The temperature of the above reaction is preferably 50°C to 200°C, more preferably 50°C to 105°C, specifically including: carrying out normal pressure reaction under heating conditions, and then heating and pressurizing for high pressure reaction. High pressure reaction is conducive to crystal forming, and the generated crystal form is more regular, which is used to reduce the dosage. A more specific operation can be to heat the reaction solution to 50°C to 60°C for normal pressure reaction; then pour the reaction solution into a high pressure reactor and carry out high pressure reaction at a temperature of 60°C to 105°C. The reaction time of normal pressure reaction is preferably 0.5 to 2h, and the time of high pressure reaction is preferably 4 to 5h. After the reaction, a destabilizing agent can be obtained. Specifically, it can be: after the reaction is completed, it is cooled to room temperature, the mixture obtained after the reaction is centrifuged, filtered, and then cleaned with deionized water, and then dried and ground at a constant temperature in a blast drying oven to obtain a destabilizing agent.

[0044] Another embodiment of the present invention further provides a destabilizing agent for softening and removing hardness of concentrated brine, which is prepared according to any of the methods described above.

[0045] Based on the above-mentioned destabilizing agent, another embodiment of the present invention further provides a method for softening concentrated brine, which comprises:

[0046] Add the above destabilizing agent into the reverse osmosis concentrated brine, stir and mix, separate the solid and liquid, and obtain pretreated wastewater;

[0047] The pretreated wastewater is softened by a double alkali method.

[0048] From the above content, it can be seen that the preparation method of the destabilizing agent for softening and removing hardness of concentrated brine provided by the embodiment of the present invention has the following advantages:

[0049] The preparation method uses the precipitate corresponding to the flocculant ion and / or the salt ion as a carrier. Under alkaline conditions, the flocculant ion is precipitated to the carrier surface and connected through oxygen bridging. The destabilizer surface prepared in this way has many hydroxyls and can be combined with the complex originally combined with calcium, magnesium and silicate ions in the concentrated brine to destroy the original stable complex structure of calcium and magnesium ions. At the same time, the destabilizer is hydrolyzed and polycondensed by the surface flocculant to exert the flocculation and coagulation effect. Through adsorption bridging and net capture and sweeping, the load carrier in the brine and the complex adsorbed on the surface are aggregated and precipitated together, so that the calcium, magnesium and silicate ions in the solution are destabilized, and the originally complexed calcium, magnesium and silicate ions are released again into the brine system, thereby strengthening the softening and hardness removal effect of the subsequent double-alkali method and reducing the dosage of the double-alkali agent.

[0050] The preparation method provided by the present invention is simple to operate, high in yield and low in cost. The obtained destabilizing agent can change the forms of calcium, magnesium and silicate ions in the concentrated brine after being applied to the concentrated brine, thereby achieving destabilization of the calcium, magnesium and silicate ions in a complex environment, reducing the dosage of the double alkali agent for subsequent softening and dehardening by the double alkali method, reducing the operating cost, and being suitable for large-scale industrial production and promotion and application.

[0051] The technical solution of the present invention is further described below in conjunction with specific embodiments:

[0052] Example 1

[0053] (1) Magnesium sulfate and aluminum sulfate were weighed at a Mg / Al molar ratio of 1:1, and fully mixed in 100 mL of deionized water to obtain a mixed solution A. The concentration of magnesium sulfate was 0.08 M, and the concentration of aluminum sulfate was 0.04 M;

[0054] (2) Sodium carbonate and sodium hydroxide are mixed in a molar ratio of n(CO3 2- ) / n(OH - )=0:5, dissolved in deionized water to prepare solution B;

[0055] (3) Pour solution A and solution B into a beaker at the same time and mix thoroughly to ensure that the pH value of the mixed solution is 10. Place the mixed solution in a 50°C water bath and stir continuously for 1 hour, pour it into a high-pressure reactor, and keep it in a 105°C oven for 4 hours until the reaction is completed. After the reaction is completed, cool it to room temperature, centrifuge and filter the material, wash it with deionized water, and then dry it in a blast drying oven at a constant temperature of 55°C for 8 hours and grind it to obtain a destabilizing agent.

[0056] The scanning electron microscope image of the destabilizing agent prepared in this embodiment is as follows Figure 2 As shown, the XRD pattern is Figure 3 shown.

[0057] Example 2

[0058] (1) Magnesium sulfate, aluminum sulfate, and iron sulfate were weighed in a Mg / Al / Fe molar ratio of 2:2:4, and fully mixed in 100 mL of deionized water to obtain a mixed solution A. The concentration of magnesium sulfate was 0.02 M, the concentration of aluminum sulfate was 0.01 M, and the concentration of iron sulfate was 0.02 M;

[0059] (2) Sodium carbonate and sodium hydroxide are mixed in a molar ratio of n(CO3 2- ) / n(OH - )=3:5, dissolved in deionized water to prepare solution B;

[0060] (3) Pour solution A and solution B into a beaker containing 350 mg of CaCO3 and mix them thoroughly. At this time, the molar ratio of Mg / Al / Fe / Ca in the solution is 4:4:8:7, and the pH value of the mixed solution is ensured to be 11. Place the mixed solution in a 50°C water bath and stir it continuously for 1 hour, pour it into a high-pressure reactor, and keep it in a 105°C oven for 4 hours until the reaction is completed. After the reaction is completed, cool it to room temperature, centrifuge the material, filter it, and wash it with deionized water, then dry it in a blast drying oven at a constant temperature of 55°C for 8 hours, grind it, and obtain a destabilizing agent.

[0061] The scanning electron microscope image of the destabilizing agent prepared in this embodiment is as follows Figure 4 shown.

[0062] Example 3

[0063] (1) Magnesium sulfate, aluminum sulfate, and iron sulfate were weighed at a Mg / Al / Fe molar ratio of 5:5:7, and fully mixed in 100 mL of deionized water to obtain a mixed solution A. The concentration of magnesium sulfate was 0.05 M, the concentration of aluminum sulfate was 0.025 M, and the concentration of iron sulfate was 0.035 M;

[0064] (2) Sodium carbonate and sodium hydroxide are mixed in a molar ratio of n(CO3 2- ) / n(OH-)=4:5, dissolved in deionized water to prepare solution B;

[0065] (3) Pour solution A and solution B into a beaker containing 350 mg of CaCO3 and mix them thoroughly. At this time, the molar ratio of Mg / Al / Fe / Ca in the solution is 10:10:14:7, and the pH value of the mixed solution is ensured to be 12. Place the mixed solution in a 50°C water bath and stir it continuously for 1 hour, pour it into a high-pressure reactor, and keep it in a 105°C oven for 4 hours until the reaction is completed. After the reaction is completed, cool it to room temperature, centrifuge the material, filter it, and wash it with deionized water, then dry it in a blast drying oven at a constant temperature of 55°C for 8 hours, grind it, and obtain a destabilizing agent.

[0066]

Double alkali method dosage test

[0067] Application testing:

[0068] The quality of concentrated water containing organic phosphine scale inhibitor used in the experiment is: COD: 600mg / L, ammonia nitrogen: 150mg / L, total phosphorus: 80mg / L, pH: 7.5, conductivity: 154mS / cm.

[0069] The destabilizing agent prepared in Example 1-3 was used to treat the reverse osmosis concentrated water. The specific method was as follows: 250 mg of the destabilizing agent was added to 500 mL of the reverse osmosis concentrated water, and the mixture was stirred at room temperature for 24 h, and then the solid-liquid separation was performed to obtain the treated wastewater. The Ca content of the wastewater was determined by ICP-OES as it changed with pH. 2+ The control group directly used the double alkali method to titrate the reverse osmosis concentrated water used in the laboratory and recorded the double alkali method dosage.

[0070] The results of the test are as follows Figure 5 As shown, Figure 5 (a), (b), (c), and (d) are the changes in calcium ion concentration and the dosage of the double alkali method in the control group, Example 1, Example 2, and Example 3, respectively. As can be seen from the figure, compared with the control group, the dosage of the double alkali can be significantly reduced after the reverse osmosis concentrated water is treated with the destabilizing agent prepared in this embodiment. The destabilizing agent prepared in Example 2 can most efficiently reduce the stability of calcium, magnesium, and silicate ions and reduce the dosage of the double alkali.

[0071] The embodiments of the present invention have been described above, and the above description is exemplary, not exhaustive, and is not limited to the disclosed embodiments. Many modifications and changes will be apparent to those of ordinary skill in the art without departing from the scope and spirit of the described embodiments. The selection of terms used herein is intended to best explain the principles of the embodiments, practical applications, or improvements to the technology in the market, or to enable other persons of ordinary skill in the art to understand the embodiments disclosed herein.

Claims

1. A method for preparing a destabilizing agent for softening and removing hardness of concentrated brine, characterized in that: The steps include: Under alkaline conditions, the flocculant ions form flocculated precipitation on the surface of the loaded precipitation to obtain the destabilizing agent, and the specific operation is scheme I or scheme II; The scheme I is as follows: a first mixed solution containing salt ions and flocculant ions is mixed with an alkaline solution to obtain a reaction solution; the reaction solution is reacted under heating conditions; during the reaction, the load precipitate is synthesized in situ, and a flocculated precipitate is formed on the surface of the load precipitate; or, The scheme II is as follows: adding the second mixed solution containing flocculant ions and the loaded precipitate into an alkaline solution to obtain a reaction solution; reacting the reaction solution under heating conditions; during the reaction, the flocculant ions form flocculated precipitates on the surface of the loaded precipitate; The concentrated brine contains a complex combined with calcium and magnesium ions; The flocculant ions are iron ions and / or aluminum ions; The loaded precipitate is a precipitate corresponding to the flocculant ions and / or the salt ions; the salt ions are one or more of magnesium ions, calcium ions, iron ions, and aluminum ions; The pH value of the alkaline condition is 10-12; The reaction temperature is 50°C to 200°C, and specifically includes: performing a normal pressure reaction under heating conditions, and then heating and pressurizing to perform a high pressure reaction.

2. The preparation method according to claim 1, characterized in that: The loaded precipitate is one or more of calcium carbonate, aluminum oxide and magnesium hydroxide.

3. The preparation method according to claim 1, characterized in that: The alkaline solution includes CO3 2- and OH - .

4. The preparation method according to claim 1, characterized in that: The second mixed solution also contains salt ions, which are derived from magnesium sulfate, magnesium nitrate, magnesium chloride or calcium chloride.

5. A destabilizing agent for softening and removing hardness of concentrated brine, characterized in that: Prepared according to the method according to any one of claims 1 to 4.

6. A method for softening concentrated brine, characterized in that: include: Adding the destabilizing agent described in claim 5 to the reverse osmosis concentrated brine, stirring and mixing, and separating the solid and the liquid to obtain pretreated wastewater; The pretreated wastewater is softened by a double alkali method.

Citation Information

Patent Citations

  • Comprehensive utilization method of concentrated sea water or brackish water

    CN102701476A

  • Preparation method of magnesium hydroxide fire retardant

    CN106882826A

  • Method and device for preventing desulfurization wastewater concentration system from scaling

    CN111908671A

  • Additive for reducing calcium and magnesium ions in primary brine and preparation method thereof

    CN115448331A

  • Flocculation precipitation treatment method of ion-containing drainage

    JP2007275757A