On-chip chiral high-resolution infrared broadband photodetector and preparation method thereof

By using composite chiral metasurfaces and Landau damping mechanisms in infrared circular polarization detectors, the problems of stability, imaging rate and optical path complexity in the existing technology are solved, and high-resolution infrared broadband detection and low-energy infrared detection are achieved. Circular polarization detection, especially effective detection of mid-infrared bands at room temperature.

CN118352412BActive Publication Date: 2024-10-11ZHEJIANG UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410782507.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-06-18
Publication Date
2024-10-11
Estimated Expiration
2044-06-18

AI Technical Summary

Technical Problem

Existing infrared circular polarization detectors have deficiencies in stability, imaging rate, sensitivity and optical path complexity, and cannot achieve hyperspectral imaging analysis and effective detection of infrared bands.

Method used

An on-chip chiral high-resolution infrared broadband photodetector is designed, using bottom silicon and top silicon as the carrier substrate, with gold chiral metasurface, silicon chiral metasurface, boron nitride and graphene, through composite chiral The metasurface and Landau damping mechanism enable high-resolution circular polarization detection and operate at room temperature without external power supply.

Benefits of technology

It achieves high-resolution circularly polarized light infrared broadband detection, improves anti-interference and dehazing imaging capabilities, reduces energy consumption, and operates at room temperature without the need for refrigeration, making a huge breakthrough in the detection of mid-infrared bands.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118352412B_ABST
    Figure CN118352412B_ABST
Patent Text Reader

Abstract

The present invention discloses an on-chip chiral high-resolution infrared broadband photoelectric detector and a preparation method thereof. The bottom silicon oxide and bottom silicon constitute the detector carrier substrate, and the top silicon is provided above the bottom silicon oxide; the top silicon oxide is provided above the top silicon, and two left and right perforated windows with electrodes are provided in the top silicon oxide, the bottom of the gold chiral super surface is in contact with the top of the silicon chiral super surface, and the boron nitride is covered on the gold chiral super surface and the silicon chiral super surface, and the boron nitride, the gold chiral super surface and the silicon chiral super surface are provided in the left perforated window of the top silicon oxide, and the graphene is covered on the boron nitride and the left window electrode; the metal silicide is provided in the right perforated window in the top silicon oxide, and the top of the metal silicide is in contact with the right window electrode. The present invention can be integrated on-chip to realize high-resolution circularly polarized light infrared broadband detection, which is conducive to anti-interference defogging imaging detection, and does not require refrigeration and can work under room temperature conditions.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of photoelectric detection technology, and in particular to an on-chip chiral high-resolution infrared broadband photoelectric detector and a preparation method thereof. Background Art

[0002] Infrared circular polarization detection has important application value in many key areas related to the national economy and people's livelihood, such as molecular chirality detection and space optical communication. First of all, in terms of anti-interference imaging, circular polarization detection has attracted widespread attention due to its special effect of "penetrating clouds and fog". When circularly polarized light propagates in clouds and fog composed of tiny water particles, the randomization rate of the helicity is much smaller than the randomization rate of the propagation direction, so the circular polarization characteristics are maintained. Combining polarization information can help restore the transmittance and depth information of the image, which is beneficial to improving the defogging effect. Therefore, the development of high polarization ratio infrared circular polarization detectors is of great significance.

[0003] At present, the more mature infrared circular polarization detectors are time-separated and space-separated. Time-separated devices need to be equipped with linear polarizers and quarter-wave plates, and circular polarization discrimination is achieved by rotating the linear polarizer or quarter-wave plate. However, this method that relies on mechanical movement has insufficient stability, limited residence time for each polarization state, low imaging rate, and low detection sensitivity. Although the spatial separation type avoids mechanical movement, its optical path is complex, difficult to install, and bulky. In addition, the above methods either obtain full-color polarization information, obtain polarization information of monochromatic light, or obtain polarization information of a few bands, and cannot perform hyperspectral imaging analysis. The focal plane pixel-level separation device that relies on the integration of micro-polarization devices can avoid the main shortcomings of the first two devices and is the future development direction.

[0004] A Chinese patent application with publication number CN117615588A discloses a chiral perovskite circularly polarized light detector and a method for preparing the same. The patent mentions a detector that obtains high circularly polarized light response through a chiral perovskite film, but its detection band is relatively limited and cannot achieve detection in the infrared band. In order to achieve high-resolution detection of the detector, its circular polarization degree of about 67% still needs to be improved.

[0005] A Chinese patent application with publication number CN102879097B discloses a circular polarization hyperspectral imaging detection system. The patent mentions that a dual-channel circular polarization detection system is used to simultaneously acquire spectral image information of the left-handed and right-handed circular polarization components of a target, thereby increasing the ability to acquire differential circular polarization spectral images. However, its composition structure includes a collimation system, a birefringence beam splitting system, an imaging lens, and an image acquisition and processing system. The structure is relatively redundant and bulky, and functional on-chip integration cannot be achieved.

[0006] A Chinese patent application with publication number CN111293188B discloses an integrated high extinction ratio infrared circular polarization detector and design method. The patent mentions that the circular polarization extinction ratio of the device (about 60%) can be improved by combining a chiral mirror metamaterial with a quantum well infrared detector. However, the detector generally has weak absorption of the mid-infrared band as a whole (maximum about 35%), which hinders the overall detection efficiency and sensitivity of the detector. In addition, the infrared circular polarization detector cannot achieve effective circular polarization light detection in the near-infrared band because it has almost no absorption of near-infrared light.

[0007] The reported integrated circular polarization detectors have a single infrared detection range and a generally low polarization ratio. Therefore, it is necessary to provide an on-chip chiral high-resolution infrared broadband photodetector and a preparation method. No circular polarization detectors combining high polarization ratio and infrared broadband detection capabilities have been reported so far. Summary of the invention

[0008] The present invention aims to provide an on-chip chiral high-resolution infrared broadband photodetector and a preparation method thereof in view of the deficiencies in the prior art.

[0009] The object of the present invention is achieved through the following technical solution: an on-chip chiral high-resolution infrared broadband photodetector, the photodetector comprising:

[0010] A bottom silicon with a bottom layer of silicon oxide thereon, which together form a detector carrier substrate;

[0011] The top silicon is arranged above the bottom silicon oxide, and has a top bottom silicon oxide layer with two left and right perforated windows; a left window electrode and a right window electrode connected to form a detector path are respectively arranged around the upper layers of the left and right perforated windows;

[0012] A silicon chiral metasurface, located at the bottom of the left perforated window of the top silicon oxide layer;

[0013] The bottom of the gold chiral metasurface is in contact with the top of the silicon chiral metasurface to form a composite chiral metasurface;

[0014] Boron nitride, coated on top of the composite chiral metasurface;

[0015] Graphene, covering boron nitride and left window electrode;

[0016] The metal silicide is arranged in the right perforated window in the top silicon oxide layer and is in contact with the right window electrode.

[0017] Furthermore, the structural unit graphic design of the gold chiral metasurface is as follows: two centrosymmetrical crescent-shaped holes are outlined in the overall rectangular outer frame, the rectangular corners of the upper left corner and the lower left corner of the rectangular outer frame are removed, and a nano-hole is outlined between the two centrosymmetrical crescent-shaped holes, and the overall structure is an asymmetric chiral structure.

[0018] Furthermore, the silicon chiral metasurface is formed by using a gold chiral metasurface as a mask and then etching the surface of the silicon chiral metasurface using an inductively coupled plasma dry etching system (ICP). 4 F 8 and SF 6 It is produced by etching silicon as a reactive gas.

[0019] Furthermore, the nano-connected strips between the gold chiral metasurfaces are etched by ion beam etching to obtain a composite chiral metasurface in which the silicon chiral metasurfaces are connected by nano-strips, while the gold chiral metasurfaces are not connected. The gold chiral metasurface and the silicon chiral metasurface can flexibly adjust the response wavelength by adjusting different sizes.

[0020] Furthermore, the three-dimensional composite chiral metasurface composed of the gold chiral metasurface and the silicon chiral metasurface realizes light field enhancement and transfers energy to the electronic system through Landau damping, thereby directly exciting the generation of hot carriers and improving the utilization of incident light energy.

[0021] Furthermore, the boron nitride disposed between the graphene and the gold chiral metasurface is used to play a role in blocking the passage of electrons according to the electron energy in the device path, thereby improving the resolution difference of circular polarization detection.

[0022] Furthermore, the circularly polarized infrared broadband detection range of the photodetector involves the near-infrared band and the mid-infrared band;

[0023] Furthermore, the photodetector generates open-circuit voltage and short-circuit current through light without external power supply. The light itself supports the operation of the device and realizes detection of mid-infrared and near-infrared bands at room temperature.

[0024] Furthermore, the metal silicide makes ohmic contact with the top silicon.

[0025] On the other hand, the present invention also provides a method for preparing an on-chip chiral high-resolution circularly polarized infrared broadband low-energy consumption photodetector, the method comprising the following steps:

[0026] (1) Preparation of top silicon oxide: The surface of the N-type doped SOI wafer substrate is cleaned, and it is placed in acetone, isopropanol, and deionized water for ultrasonic cleaning in sequence, and then taken out and blown dry with nitrogen; a top silicon oxide is grown from the surface of the N-type doped SOI wafer using a thermal oxidation process;

[0027] (2) Patterning of the right silicon window: Spin-coat the SOI wafer substrate with the top layer of silicon oxide with photoresist, then use a photolithography machine to photolithography the substrate after photoresist coating and perform development operations. After the photoresist is completely cured, the oxide layer of the window area not protected by the photoresist is etched in a buffered oxide etching solution. The device is removed from the buffered oxide etching solution and cleaned, and then the device is stripped with acetone and isopropanol to complete the patterning of the right silicon window for ohmic contact and form the ohmic contact area of ​​the top silicon.

[0028] (3) Preparation of metal silicide: Ti metal is prepared by magnetron sputtering, and the electrode is formed only in the ohmic contact area through a lift-off process. Then, a rapid annealing process is used to form TiSi in the silicon window area. 2 alloy;

[0029] (4) Patterning of the left window electrode and the right window electrode: perform metal deposition, use acetone solution to peel off the remaining metal except the electrode pattern, and then use isopropyl alcohol to clean the acetone to obtain a complete electrode pattern;

[0030] (5) Patterning of the left silicon window: The left silicon window is patterned on the top silicon oxide surface again by the above-mentioned patterning process of the right silicon window, and then the top silicon oxide in the left silicon window area is etched away in a buffered oxide etch;

[0031] (6) Preparation of gold chiral metasurface and silicon chiral metasurface: The SOI wafer processed in step (1) to step (5) is coated, a design pattern is formed by electron beam lithography, metal is deposited by electron beam evaporation, and then a gold bionic chiral metasurface is obtained by a stripping process; the gold chiral metasurface is used as a mask, and then silicon is etched by an inductively coupled plasma dry etching system ICP to prepare a three-dimensional silicon chiral metasurface; then, the nano-connecting strips between the gold chiral metasurfaces are etched by ion beam etching to obtain a composite chiral metasurface in which the silicon chiral metasurfaces are connected by nano-strips and the gold chiral metasurfaces are not connected;

[0032] (7) Patterning of Boron Nitride: Boron nitride is grown by thermal chemical vapor deposition, and transferred by polymethyl methacrylate-assisted method so that the boron nitride area covers the gold chiral metasurface and the silicon chiral metasurface area. Then, a third photolithography is performed to define the boron nitride covered area. The photoresist is protected in the left silicon window area covered by the boron nitride. Then, the boron nitride area outside the left silicon window area is etched, and finally, the photoresist is removed to achieve patterning of the boron nitride.

[0033] (8) Graphene patterning: Repeat the process of boron nitride patterning in step (7) to achieve graphene patterning, where the graphene covers the boron nitride area and the left window electrode.

[0034] Beneficial effects of the present invention: The present invention can be integrated on-chip to achieve high-resolution circularly polarized infrared broadband detection, which is beneficial to anti-interference defogging imaging detection. It can work at room temperature without refrigeration, which is a huge breakthrough for mid-infrared band detection. Secondly, it can also work without bias voltage, which is expected to bring extremely low energy consumption or even zero energy consumption, and has the advantage of low energy consumption. BRIEF DESCRIPTION OF THE DRAWINGS

[0035] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0036] Figure 1 It is a schematic diagram of the structure of the present invention;

[0037] Figure 2 is a cross-sectional view of the structure of the present invention;

[0038] Figure 3 Schematic diagram of the structure of the gold chiral metasurface;

[0039] Figure 4 Schematic diagram of the structure of the silicon chiral metasurface and a partial enlarged view;

[0040] Figure 5 3D schematic diagram of the combination of gold chiral metasurface and silicon chiral metasurface;

[0041] Figure 6 Process flow chart for fabricating on-chip chiral high-resolution circularly polarized infrared broadband low-energy photodetector;

[0042] Figure 7 The chiral absorption spectra and circular dichroism diagrams of the present invention under different circularly polarized light excitations;

[0043] Figure 8 The principle diagram of the interaction of left / right circularly polarized light at 2300 nm (near infrared band) in the embodiment of the present invention;

[0044] Fig. 9 Schematic diagram of the interaction between left / right circularly polarized light at 4500 nm (mid-infrared band) in the embodiment of the present invention;

[0045] Fig.10This is a photoelectric imaging result diagram measured according to an embodiment of the present invention under left / right circularly polarized light at 2300 nm (near infrared band).

[0046] in:

[0047] 1. Gold chiral metasurface, 2. Silicon chiral metasurface, 3. Graphene, 4. Boron nitride, 5. Left window electrode, 6. Right window electrode, 7. Metal silicide, 8. Top silicon oxide, 9. Bottom silicon oxide, 10. Bottom silicon, 11. Top silicon. DETAILED DESCRIPTION

[0048] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described below in conjunction with the accompanying drawings and implementation examples. It should be understood that the specific implementation examples described herein are only used to explain the present invention and are not used to limit the present invention.

[0049] like Figure 1 and Figure 2 As shown, the present invention provides an on-chip chiral high-resolution infrared broadband photodetector, including a gold chiral metasurface 1, a silicon chiral metasurface 2, graphene 3, boron nitride 4, a left window electrode 5, a right window electrode 6, a metal silicide 7, a top silicon oxide 8, a bottom silicon oxide 9, a bottom silicon 10 and a top silicon 11.

[0050] The bottom silicon oxide 9 and the bottom silicon 10 constitute the detector carrier substrate, and the top silicon 11 is arranged above the bottom silicon oxide 9; the top silicon oxide 8 is arranged above the top silicon 11, and the preparation process of the top silicon oxide 8 can be any one of thermal oxidation growth, PECVD furnace growth, atomic layer deposition (ALD) or electron beam evaporation deposition of silicon oxide; two left and right perforated windows are arranged in the top silicon oxide 8, which can be any one of rectangular grooves, triangular grooves or other polygonal grooves or circular grooves, and the left window electrode 5 and the right window electrode 6 are respectively arranged around the upper layer of the left and right perforated windows, and the left window electrode 5 is connected to the right window electrode 6 to form a detector path; Figure 4 and Figure 5As shown, the bottom of the gold chiral metasurface 1 contacts the top of the silicon chiral metasurface 2 to form a composite chiral metasurface. The metal deposition process of the gold chiral metasurface 1, the left window electrode 5 and the right window electrode 6 can be any one of thermal evaporation, electron beam evaporation or magnetron sputtering. In addition to gold (Au), the material of the gold chiral metasurface 1 can also be replaced by any one of platinum (Pt), palladium (Pd), silver (Ag), copper (Cu), chromium (Cr), titanium (Ti), nickel (Ni) or aluminum (Al). The structural unit graphic design of the gold chiral metasurface 1 is as follows: two centrosymmetrical crescent-shaped slots are outlined in the overall rectangular outer frame, the rectangular corners of the upper left corner and the lower left corner of the rectangular outer frame are removed, and a nano-hole slot is outlined between the two centrosymmetrical crescent-shaped slots. The overall structure is an asymmetric chiral structure, such as Figure 3 The boron nitride 4 covers the gold chiral metasurface 1 and the silicon chiral metasurface 2. The silicon chiral metasurface 2 uses the gold chiral metasurface 1 as a mask and then uses an ICP (inductively coupled plasma dry etching system, using C 4 F 8 and SF 6 Then, the nano-connected strips between the gold chiral metasurfaces 1 are etched by ion beam etching to obtain a composite chiral metasurface in which the silicon chiral metasurfaces 2 are connected by nano-strips, while the gold chiral metasurfaces 1 are not connected. Figure 6 In the process from (a) to (b) of step (8), the composite metasurface greatly improves the detection resolution of left / right circularly polarized light in the present invention. The gold chiral metasurface and the silicon chiral metasurface can flexibly adjust the response wavelength by adjusting different sizes. The size of the composite chiral metasurface in the present invention is one of the examples.

[0051] The boron nitride 4, the gold chiral supersurface 1 and the silicon chiral supersurface 2 are arranged in the left perforated window of the top silicon oxide 8, and the graphene 3 covers the boron nitride 4 and the left window electrode 5. The graphene can also be made of single element silicene, germanene, stanene, borene, black phosphorus, transition metal chalcogenide (such as MoS 2 ,WSe 2 、ReS 2 , PtSe 2 、NbSe 2 ) or main group metal chalcogenides (such as GaS, InSe, SnS, SnS 2), wherein the number of layers can be either a single layer or a multilayer, and the graphene described in the present invention is one of the examples cited. The boron nitride 4 disposed between the graphene 3 and the gold chiral metasurface 1 is used to block the passage of some low-energy electrons in the device path, which helps to improve the resolution difference of circular polarization detection; the boron nitride 4 as a low-energy electron blocking material can also be replaced by either silicon oxide or aluminum oxide. The metal silicide 7 is disposed in the right perforated window in the top silicon oxide 8, and is used to make ohmic contact with the top silicon 11, and can be NiSi, TiSi 2 or CoSi 2 Any one of the above, the top of the metal silicide 7 is in contact with the right window electrode 6;

[0052] Due to the limited absorption rate of graphene to light (only 2.3% for a single layer), the temperature rise of the electronic system is limited, so the number of hot electrons distributed in the high-energy region is small, which is not enough to realize the collection and utilization of long-wavelength light far below the potential barrier, which greatly limits the utilization efficiency of long-wavelength light by the corresponding optoelectronic devices. The gold chiral metasurface and the silicon chiral metasurface in this detector form a three-dimensional composite chiral metasurface, which can realize the localization and enhancement of the light field on the one hand, and can also transfer energy to the electronic system through non-radiative relaxation such as Landau damping on the other hand, thereby directly exciting and generating hot carriers. The results of both of these will improve the utilization of incident light energy and improve the efficiency of photoelectric conversion. A large bandgap boron nitride material (bandgap is about 6 eV) is introduced into the detector of the present invention, and the photogenerated electrons in graphene will face a barrier as high as ~ 4 eV that is difficult to cross. Although the energy of the high-energy electrons at the end of the thermal distribution of hot electrons (hot tail) is higher than that of the directly excited photogenerated electrons due to the intrinsic photogenerated hot carrier effect of graphene, the limited absorptivity of graphene leads to its lower thermalization efficiency (limited hot electron temperature), resulting in less carrier distribution in the high-energy region of this "hot tail".

[0053] like Figure 7 As shown, the circularly polarized infrared broadband detection range of the on-chip chiral high-resolution circularly polarized light infrared broadband low-energy consumption photodetector of the present invention covers the near-infrared band and the mid-infrared band, and different chiral selective absorptions are measured at different wavelengths (1000 nm-6000 nm) and under different circularly polarized light excitations, especially at wavelengths of 1550 nm, 1870 nm, 2300 nm and 4500 nm, it exhibits huge resolution detection of left and right circularly polarized light (circular dichroism value is about 80%), and there have been no reports involving infrared broadband detection and detectors with such a huge circular polarization degree.

[0054] The low energy consumption described in the on-chip chiral high-resolution circularly polarized light infrared broadband low-energy photoelectric detector of the present invention is due to the fact that the present invention can generate open-circuit voltage and short-circuit current through light without external power supply. Light itself can make the device work, and the present invention can realize detection of the mid-infrared band under room temperature conditions, and does not require additional liquid nitrogen refrigeration like traditional mid-infrared detectors. This is a major breakthrough for mid-infrared detectors.

[0055] Take 2300 nm (near infrared band) as an example. Figure 8 As shown in (A), when right circularly polarized light is used as incident light to illuminate the detector, the electrons generated by light in the device path are in a low-energy state due to the weak absorption of the detector to right circularly polarized light. In addition, due to the effect of boron nitride between graphene and the gold chiral metasurface, some low-energy electrons in the device path of the detector are blocked, making the photocurrent intensity of the detector very weak when illuminated by right circularly polarized light. Figure 8 As shown in (B), when left circularly polarized light is used as incident light to illuminate the detector, the electrons generated by light in the device path are in a high-energy state due to the strong absorption of the detector to left circularly polarized light, and the boron nitride in the device does not block the high-energy electrons in the device path, making the photocurrent intensity of the detector very strong when illuminated by left circularly polarized light. The huge difference in the detector's response to the two circularly polarized lights enables high-resolution detection of circularly polarized light in the near-infrared band.

[0056] Take 4500 nm (mid-infrared band) as an example. Fig. 9 As shown in (A), when right circularly polarized light is used as incident light to illuminate the detector, due to the strong absorption of the detector to right circularly polarized light, the electrons generated by light in the device path are in a high-energy state, and the high-energy electrons are not affected by the boron nitride barrier, so when left circularly polarized light is irradiated, the photocurrent intensity of the detector is very strong; Fig. 9 As shown in (B) in the figure, when left circularly polarized light is used as incident light to illuminate the detector, due to the weak absorption of the detector to left circularly polarized light, the electrons generated by light in the device path are in a low energy state, and Figure 7 From the absorption spectrum data measured in the experiment, it can be seen that the half-width of the absorption peak at 4500 nm is wider than that at 2300 nm (near-infrared band), which means that the composite metasurface composed of the gold chiral metasurface and the silicon chiral metasurface has relatively weak light binding at 4500 nm, and there is a certain ohmic loss, so that most of the low-energy electrons generated by left circularly polarized light in the device path of the detector are blocked by boron nitride, and the photocurrent intensity of the detector is extremely low. Therefore, even though the detector's ability to bind light in the mid-infrared band is not as good as that in the near-infrared band, it can also achieve high-resolution detection of circularly polarized light due to the blocking of low-energy electrons.

[0057] like Fig.10As shown in the figure, the detection results of ordinary silicon-based graphene photodetectors are compared in water surface imaging. Fig.10 The high-resolution difference circular polarization photoelectric imaging results measured by the present invention are shown in (A) and Fig.10 In (B), it can be found that the detector can remove the scale light on the water surface and clearly see the underwater situation. Since the scale light, as the reflected light of the external light source (sunlight) on the water surface, has a relatively obvious linear polarization direction, it can be filtered out using a circular polarization detection method with a direction perpendicular to it. In addition, since the composite metasurface composed of the gold chiral metasurface and the silicon chiral metasurface has a huge circular polarization detection ratio, the present invention shows the advantage of high-resolution imaging in water surface imaging.

[0058] On the other hand, the present invention also provides a method for preparing an on-chip chiral circularly polarized infrared broadband photodetector, such as Figure 6 As shown, the method comprises the following steps:

[0059] (1-2) Preparation of top silicon oxide: Use standard SOI wafers (Silicon-On-Insulator), with top silicon thickness of 200 nm-10 um, bottom silicon thickness of 100-500 um, N-type doping, resistivity of 1-10Ω·cm, and crystal orientation of 100. Clean the surface of the N-type doped SOI wafer substrate, and then put it into acetone, isopropanol, and deionized water solution for ultrasonic cleaning, and then take it out and blow dry it with nitrogen; use thermal oxidation process to grow 100-300 nm thick top silicon oxide on the surface of standard 200 nm-10 um thick lightly doped N-type SOI wafer.

[0060] (3) Patterning of the silicon window on the right: Spin-coat the SOI wafer substrate with the top layer of silicon oxide so that the photoresist evenly covers the substrate surface, pre-bake at 105°C for 5 minutes, and then use a photolithography machine to photolithography the substrate after the photolithography is completed. After the photolithography is completed, mix the developer and water in a volume ratio of 1:7 to form a developing solution, perform the developing operation, and post-bake at 120°C for 20 minutes to completely solidify the photoresist, so as to protect the oxide layer under the photoresist in the next wet etching. Then, the oxide layer of the window area not protected by the photoresist is etched in a buffered oxide etch (BOE) solution. The ratio of the BOE solution is: NH 4 F: HF: H 2O = 60 g: 30 ml: 100 ml. The etching rate of BOE solution with this ratio is 100 nm / min. When the thickness of the top silicon oxide layer in the substrate is 100 nm, etching for 1 min is sufficient. After the device is removed from the BOE solution, it is washed in water and then debonded with acetone and isopropanol to complete the patterning of the right silicon window for ohmic contact and form the ohmic contact area of ​​the top silicon.

[0061] (4) Preparation of metal silicide: 40 nm Ti metal is prepared by magnetron sputtering. After the lift-off process, the electrode can be formed only in the ohmic contact area. Then, a rapid annealing process is used, specifically heating at 750℃ for 20 s and 850℃ for 20 s in a nitrogen atmosphere, to form TiSi in the silicon window area. 2 alloy.

[0062] (5) Patterning of the left window electrode and the right window electrode: Continue to repeat the above steps of coating-pre-baking-photolithography-development. The metal deposition operation can be performed using thermal evaporation, electron beam evaporation or magnetron sputtering process. Then, the remaining metal except the electrode pattern is lifted off with acetone solution. The acetone is then cleaned with isopropyl alcohol to obtain the complete left window electrode and right window electrode patterns.

[0063] (6) Patterning of the left silicon window: The left silicon window is patterned on the top silicon oxide surface again using the above-mentioned patterning process for the right silicon window. Subsequently, the top silicon oxide in the left silicon window area is etched away in BOE.

[0064] (7-8) Preparation of gold chiral metasurface and silicon chiral metasurface: The SOI wafer after the above process is coated, the design pattern is lithographically formed by high-resolution electron beam, the metal is deposited by electron beam evaporation, and then the gold bionic chiral metasurface is obtained by the above-mentioned stripping process. The gold chiral metasurface is used as a mask, and then an ICP (inductively coupled plasma dry etching system, using C 4 F 8 and SF 6 As a reaction gas) to etch silicon, a three-dimensional silicon chiral metasurface is prepared. Then, the nano-connected strips between the gold chiral metasurfaces are etched by ion beam etching to obtain a composite chiral metasurface in which the silicon chiral metasurfaces are connected by nano-strips, while the gold chiral metasurfaces are not connected. Figure 6 The process from (a) to (b) in step (8) in .

[0065] (9) Patterning of Boron Nitride: High-quality boron nitride grown by thermal chemical vapor deposition is transferred by polymethyl methacrylate (PMMA)-assisted method. PMMA is spin-coated on the boron nitride as a supporting layer and placed in a copper etching solution. The boron nitride supported by PMMA floating in the etching solution is scooped out and washed in deionized water so that the boron nitride area covers the gold chiral metasurface and the silicon chiral metasurface area. The PMMA on the boron nitride is then removed with dichloromethane. A third photolithography is then performed, and the steps of photoresist coating-pre-baking-photolithography-development are repeated to define the boron nitride covered area. The photoresist is protected in the left silicon window area covered by the boron nitride. The boron nitride area outside the left silicon window area is then etched with an oxygen plasma etching device. Finally, the photoresist is removed to achieve patterning of the boron nitride.

[0066] (10) Graphene patterning: Repeat the above-mentioned boron nitride patterning process to achieve graphene patterning, where the graphene covers the boron nitride area and the left window electrode.

[0067] In summary, the on-chip chiral high-resolution infrared broadband photodetector and preparation method provided by the embodiments of the present invention can be integrated on-chip to achieve high-resolution circularly polarized light infrared broadband detection, which is beneficial to anti-interference defogging imaging detection. And it does not require refrigeration and can work at room temperature, which is a huge breakthrough for detection in the mid-infrared band. Secondly, it can also work without bias voltage, which is expected to bring extremely low energy consumption or even zero energy consumption, and has the advantage of low energy consumption.

[0068] The above embodiments provide an exemplary description of the present invention. Obviously, the specific implementation of the present invention is not limited to the above methods. As long as various improvements are made using the method concept and technical solution of the present invention, or they are directly applied to other occasions without improvement, they are all within the protection scope of the present invention.

Claims

1. An on-chip chiral high-resolution infrared broadband photodetector, characterized in that: The photodetector includes: A bottom silicon with a bottom layer of silicon oxide thereon, which together form a detector carrier substrate; The top silicon is arranged above the bottom silicon oxide, and has a top silicon oxide layer with two left and right perforated windows on the top silicon; a left window electrode and a right window electrode connected to form a detector path are respectively arranged around the upper layers of the left and right perforated windows; A silicon chiral super surface is arranged at the bottom of the left perforated window of the top silicon oxide layer; the silicon chiral super surface is obtained by etching silicon using a gold chiral super surface as a mask; The bottom of the gold chiral supersurface is in contact with the top of the silicon chiral supersurface to form a composite chiral supersurface; the structural unit graphic design of the gold chiral supersurface is as follows: two centrosymmetrical crescent-shaped slots are outlined in the overall rectangular outer frame, the upper left corner and the lower left corner of the rectangular outer frame are removed, and a nano-hole slot is outlined between the two centrosymmetrical crescent-shaped slots, and the overall structure is an asymmetric chiral structure; the nano-connecting strips between the gold chiral supersurfaces are etched by ion beam etching to obtain a composite chiral supersurface in which the silicon chiral supersurfaces are connected by nano-strips, while the gold chiral supersurfaces are not connected; Boron nitride, coated on top of the composite chiral metasurface; Graphene, covered with boron nitride and left window electrode; The metal silicide is arranged in the right perforated window in the top silicon oxide layer and is in contact with the right window electrode.

2. The on-chip chiral high-resolution infrared broadband photodetector according to claim 1, characterized in that: The gold chiral metasurface and the silicon chiral metasurface can achieve flexible regulation of the response wavelength by adjusting different sizes.

3. The on-chip chiral high-resolution infrared broadband photodetector according to claim 1, characterized in that: The three-dimensional composite chiral metasurface composed of gold chiral metasurface and silicon chiral metasurface realizes light field enhancement and transfers energy to the electronic system through Landau damping, thereby directly exciting the generation of hot carriers and improving the utilization of incident light energy.

4. The on-chip chiral high-resolution infrared broadband photodetector according to claim 1, characterized in that: The boron nitride disposed between the graphene and the gold chiral super surface is used to play a role in blocking the passage of electrons according to the electron energy in the device path, thereby improving the resolution difference of circular polarization detection.

5. The on-chip chiral high-resolution infrared broadband photodetector according to claim 1, characterized in that: The circularly polarized infrared broadband detection range of this photodetector covers the near-infrared band and the mid-infrared band.

6. The on-chip chiral high-resolution infrared broadband photodetector according to claim 1, characterized in that: The photodetector generates open-circuit voltage and short-circuit current through illumination without the need for external power supply. The illumination itself supports the operation of the device and enables detection of mid-infrared and near-infrared bands at room temperature.

7. The on-chip chiral high-resolution infrared broadband photodetector according to claim 1, characterized in that: The metal silicide makes ohmic contact with the top silicon.

8. A method for preparing an on-chip chiral high-resolution infrared broadband photodetector according to claim 1, characterized in that: The method comprises the following steps: (1) Preparation of top silicon oxide: The surface of the N-type doped SOI wafer substrate is cleaned, and it is placed in acetone, isopropanol, and deionized water for ultrasonic cleaning in sequence, and then taken out and blown dry with nitrogen; a top silicon oxide is grown from the surface of the N-type doped SOI wafer using a thermal oxidation process; (2) Patterning of the right silicon window: Spin-coat the SOI wafer substrate with the top layer of silicon oxide with photoresist, then use a photolithography machine to photolithography the substrate after photoresist coating and perform development operations. After the photoresist is completely cured, the oxide layer of the window area not protected by the photoresist is etched in a buffered oxide etching solution. The device is removed from the buffered oxide etching solution and cleaned, and then the device is stripped with acetone and isopropanol to complete the patterning of the right silicon window for ohmic contact and form the ohmic contact area of ​​the top silicon. (3) Preparation of metal silicide: Ti metal is prepared by magnetron sputtering, and an electrode is formed only in the ohmic contact area through a lift-off process. Then, a TiSi2 alloy is formed in the silicon window area using a rapid annealing process. (4) Patterning of the left window electrode and the right window electrode: perform metal deposition, use acetone solution to peel off the remaining metal except the electrode pattern, and then use isopropyl alcohol to clean the acetone to obtain a complete electrode pattern; (5) Patterning of the left silicon window: The left silicon window is patterned on the top silicon oxide surface again by the above-mentioned patterning process of the right silicon window, and then the top silicon oxide in the left silicon window area is etched away in a buffered oxide etch; (6) Preparation of gold chiral metasurface and silicon chiral metasurface: The SOI wafer processed in step (1) to step (5) is coated, a design pattern is formed by electron beam lithography, metal is deposited by electron beam evaporation, and then a gold bionic chiral metasurface is obtained by a stripping process; the gold chiral metasurface is used as a mask, and then silicon is etched by an inductively coupled plasma dry etching system ICP to prepare a three-dimensional silicon chiral metasurface; then, the nano-connecting strips between the gold chiral metasurfaces are etched by ion beam etching to obtain a composite chiral metasurface in which the silicon chiral metasurfaces are connected by nano-strips and the gold chiral metasurfaces are not connected; (9) Patterning of Boron Nitride: Boron nitride is grown by thermal chemical vapor deposition, and transferred by polymethyl methacrylate-assisted method so that the boron nitride area covers the gold chiral metasurface and the silicon chiral metasurface area. Then, a third photolithography is performed to define the boron nitride covered area. The photoresist is protected in the left silicon window area covered by the boron nitride. Then, the boron nitride area outside the left silicon window area is etched, and finally, the resist is removed to achieve patterning of the boron nitride. (10) Graphene patterning: Repeat the process of boron nitride patterning in step (9) to achieve graphene patterning, where the graphene covers the boron nitride area and the left window electrode.