A method for controlling end expansion of high-strength C-shaped steel during continuous roll forming

By pre-bending and angle adjustment before the high-strength C-shaped roller forming, combined with the edge minimum strain method, the problem of end flaring control of high-strength C-shaped steel is solved, high-precision roll forming is achieved, and production is improved efficiency.

CN118437813BActive Publication Date: 2024-11-05HEBEI UNIV OF ENG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410906981.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-08
Publication Date
2024-11-05
Estimated Expiration
2044-07-08

AI Technical Summary

Technical Problem

High-strength C-shaped steel often has end flaring defects during roll forming, and existing process optimization methods are difficult to effectively control, resulting in low molding accuracy and low production efficiency.

Method used

Before the profile roll forming, the four forming angles are pre-bending. By adjusting the angle distribution of α and β angles, combined with the minimum strain method of edges, the stress distribution of the profile during the forming process is controlled to avoid the occurrence of end flaring . The specific steps include pre-bending α angle to 18°, β angle to 12°, and adjusting the angle simultaneously during the formation process of fourteen passes, and correcting at the end, and adjusting the α angle and β angle to 90° respectively.

Benefits of technology

It effectively avoids the generation of end flaring of high-strength C-shaped steel, improves molding accuracy, provides a stable high-precision product production method, and solves the problem of controlling the end flaring of continuous roll forming of high-strength C-shaped steel.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118437813B_ABST
    Figure CN118437813B_ABST
Patent Text Reader

Abstract

The present invention provides a method for controlling the end expansion of continuous roll forming of high-strength C-shaped steel, comprising the following steps: before the roll forming of the profile, the four forming angles of the profile are pre-bent to complete the pre-bending of the α angle and the β angle of the profile, and then fourteen passes of forming are performed, the pre-bending angle is changed during the forming, and the angle distribution of the α angle and the β angle is synchronously adjusted in each pass; the order of the α angle is 0°, 0°, 0°, 0°, 0°, 12°, 25°, 37°, 48°, 59°, 70°, 82°, 82° and 92°; the order of the β angle is: 0°, 0°, 30°, 60°, 90°, 0°, 0°, 0°, 0°, 0°, 0°, 0°, 0°, 0° and 0°, and finally the profile is corrected after forming. The present invention enables the high-strength profile to use a reasonable pre-bending angle and forming method during the forming process, that is, the four forming angles of the profile are pre-bent, and a new method is provided for realizing high-precision products of high-strength C-shaped steel in stable batches.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of roll forming, and in particular relates to a method for controlling end expansion of high-strength C-shaped steel by continuous roll forming. Background Art

[0002] Roll forming is a method of continuously rolling metal sheets into desired cross-sections. It is widely used in the fields of automobiles, construction, ships, aerospace, etc. With the development of science and technology, the automation level of the rolling industry has been continuously improved. The materials used have also gradually developed from ordinary steel to high-strength steel. Its characteristics of light weight, high strength, and strong energy absorption are widely used in industries such as construction and automobiles. However, quality control in the rolling process is still a difficult problem. The forming of profiles in the roll forming process is a complex three-dimensional forming with large displacement, which has obvious material nonlinearity, geometric nonlinearity and boundary nonlinearity. Roll forming processing of steel sections is prone to many defects, such as end flaring defects. End flaring is the process of cutting the profile into a certain size by the rolling process. The internal residual stress is released at the shearing mouth, causing the end of the profile to be formed inward or outward. This defect is one of the main reasons for the failure of high-strength steel to meet the forming accuracy standards, and increases the difficulty of installation work, which seriously restricts the development of roll forming technology. In addition, there is no unified forming theory guidance for the design of roll forming process. Engineers mainly rely on experience to continuously trial and error to complete industrial production. The design and commissioning cycle of new products is long, and the production efficiency is low.

[0003] For a long time, in order to improve the end flaring problem, the rolling industry has often used optimized design process design to solve the flaring problem. The end flaring problem of high-strength C-shaped steel is prominent, so it is difficult to control the flaring problem through process optimization. Different sizes of C-shaped steel require different process designs, which undoubtedly takes a lot of time and cost, and cannot guarantee the quality of the product. The initial solution to the end flaring problem was to set a cornering pass in the final rolling unit. The effect was very good for ordinary steel, but high-strength steel has strong performance and it is not easy to solve the end flaring problem of high-strength steel by cornering. Although this method has strong adaptability and increased design challenges, relying solely on process optimization cannot solve the end flaring problem of high-strength steel well, and the accuracy is not high enough.

[0004] Based on this, a method for controlling the end expansion of high-strength C-shaped steel during continuous roll forming was proposed. Summary of the invention

[0005] The technical problem to be solved by the present invention is to provide a method for controlling the end expansion of high-strength C-shaped steel continuous roll forming in view of the deficiencies of the above-mentioned prior art, so as to solve the problems raised in the above-mentioned background technology.

[0006] In order to solve the above technical problems, the technical solution adopted by the present invention is: a method for controlling the end expansion of high-strength C-shaped steel continuous roll forming, comprising the following steps:

[0007] S1. Before the profile is roll-formed, the four forming angles of the profile are pre-bent to complete the pre-bending of the α angle and β angle of the profile;

[0008] S2, perform fourteen passes of forming, change the pre-bending angle during forming, and synchronously adjust the angle distribution of angle α and angle β in each pass;

[0009] S3. Finally, the profile is corrected after forming, with the α angle being 90° and the β angle being 90°.

[0010] As a further illustration of the present invention, the α angle in S1 is pre-bent to 18°, and the β angle is pre-bent to 12°.

[0011] As a further illustration of the present invention, the angle distribution order of angle α in S2 is specifically: 0°, 0°, 0°, 0°, 0°, 12°, 25°, 37°, 48°, 59°, 70°, 82°, 82° and 92°;

[0012] The specific angle allocation order of the β angle is: 0°, 0°, 30°, 60°, 90°, 0°, 0°, 0°, 0°, 0°, 0°, 0°, 0° and 0°.

[0013] Compared with the prior art, the present invention has the following advantages:

[0014] The present invention integrates the end expansion control of high-strength C-shaped steel into the end expansion control method of high-strength C-shaped steel, so that during the forming process of high-strength profile, reasonable pre-bending angles and forming methods are used, that is, the four forming angles of the profile are pre-bent, so that the stress generated by the profile during the forming process is concentrated on the forming angles and integrated with the edge minimum strain method in the downhill forming method, and combined with actual production to achieve high-strength C-shaped steel roller flower optimization design, avoid the generation of end expansion of high-strength C-shaped steel, solve the problem that the end expansion problem of high-strength C-shaped steel continuous roll forming is serious and difficult to control, provide a theoretical basis for avoiding continuous roll forming of high-strength C-shaped steel, and provide a new method for stable batch production of high-precision products of high-strength C-shaped steel. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 is a schematic diagram of a profile after forming in an embodiment of the present invention;

[0016] Figure 2 It is a schematic diagram of some forming passes of the present invention;

[0017] Figure 3 is a schematic diagram of angle distribution during the forming process of the present invention;

[0018] Figure 4 is the main stress vector diagram of the profile in the eighth pass in the embodiment of the present invention;

[0019] Figure 5 is a longitudinal strain curve diagram of a node on the flange of a profile in the eighth pass in an embodiment of the present invention;

[0020] Figure 6 : is the influence diagram of the horizontal forming method, the cross-section center of gravity invariant method and the edge minimum strain method on the end expansion of the profile in the embodiment of the present invention;

[0021] Figure 7 It is a simulated dimensional diagram of the expansion of the cut end of the high-strength C-shaped steel obtained in an embodiment of the present invention. DETAILED DESCRIPTION

[0022] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0023] like Figure 1-3 As shown, the present invention provides a technical solution: a method for controlling the end expansion of high-strength C-shaped steel continuous roll forming, comprising the following steps:

[0024] S1. Before the profile is roll-formed, the four forming angles of the profile are pre-bent. The thickness of the profile is 0.8 mm. The α angle and β angle of the profile are pre-bent to 18° and 12°, as shown in the following example. Figure 2 As shown;

[0025] Most of the residual stress generated by the flange of the profile during the forming process is concentrated in the four forming corners, which reduces the residual stress generated by the profile during the forming process and reduces the expansion of the profile at the cut end, so that the stress generated by the profile in the subsequent forming process is concentrated in the forming corners. The forming method adopts the minimum strain method of the edge in the downhill forming method.

[0026] S2, performing fourteen passes of forming, changing the pre-bending angle during forming, and synchronously adjusting the angle distribution of the α angle and the β angle in each pass; the angle distribution sequence of the α angle is specifically: 0°, 0°, 0°, 0°, 0°, 12°, 25°, 37°, 48°, 59°, 70°, 82°, 82° and 92°;

[0027] The specific order of angle distribution of β angle is: 0°, 0°, 30°, 60°, 90°, 0°, 0°, 0°, 0°, 0°, 0°, 0°, 0° and 0°, as shown in the following figure: Figure 3 shown.

[0028] Figure 4 The figure shows the main stress vector diagram of the profile in the eighth pass. Because the high-strength C-shaped steel product has the flange expanded outward, the eighth pass is the pass with the largest flange forming, so we take the eighth pass as an example.

[0029] from Figure 4 It can be seen from the figure that the rebound release area is where the combined force generated by the transverse bending, longitudinal bending and shear deformation on the profile is completely released, and the profile recovers to a certain extent through its own material elasticity, causing the profile to stretch outward to form a concave curve.

[0030] The plastic deformation zone is the area where the profile moves in the forming direction and contacts the roller. When the profile contacts the roller, the profile is subjected to the transverse bending stress, which bends the profile into the required angle and forms a convex curve. The non-deformation transition zone is the area where the profile is ready to enter the roller but has not been formed. From the three deformation zones, it can be seen that the stress curve of the profile under the force of the roller is concave-convex-concave.

[0031] The change in the stress curve causes the profile to be stretched and sheared in the longitudinal direction. Multiple moments are superimposed and cannot be released. This is also the reason why the internal residual stress continues to increase and is finally released at the cut end, causing the cut end to expand.

[0032] Figure 5 It is the longitudinal strain curve of the node on the flange at the eighth pass.

[0033] Area A is the longitudinal strain of the profile before entering the eighth pass, Area B is the longitudinal strain of the profile during the eighth pass, and Area C is the longitudinal strain of the profile after exiting the eighth pass.

[0034] The strain in area B is the elastic strain plus the plastic strain, and the difference between area C and area A is the accumulation of plastic strain.

[0035] S3, finally, the profile is corrected after forming, the α angle is 90°, the β angle is 90°, as shown in the following figure: Figure 1 shown.

[0036] Figure 6 The effects of three forming methods on the end flaring of profiles are shown.

[0037] A is the horizontal forming method. In the horizontal forming method, the axis of the profile in contact with the roller remains unchanged and remains horizontal. B is the method of keeping the center of gravity of the section unchanged. As the bending part becomes longer, its axis gradually decreases when bending from the flange to better reduce the residual stress.

[0038] C is the minimum strain method of the edge. Starting from the first bending angle, the axis of each pass begins to decrease, adding more bend transition areas to avoid the increase of residual stress from the initial pass. It can be seen that it has the least effect on the expansion of the profile, because it allows more bend transition areas to participate, the fitting height of the profile side is smaller, the residual stress is smaller, and the end expansion is smaller.

[0039] In the prior art, most of the expansion strategies for C-shaped steel products are horizontal forming and setting the bending angle in the last pass.

[0040] The novel C-shaped steel end expansion control method in this embodiment is as follows Figure 6 As shown in B, in the second pass, a strategy combining a reasonable pre-bending angle and the edge minimum strain forming method is used;

[0041] from Figure 6 It can be seen that this method is very effective in improving the end flaring compared with the prior art and meets the forming accuracy.

[0042] Figure 7 is the simulated size of the expansion of the cut end of the high-strength C-shaped steel obtained in this embodiment, Figure 7 It can be seen that the dotted line figure is the profile size of 90° through finite element simulation, and the solid line figure is the designed shape size of 90°. By comparing the simulation results and the design dimensions, it can be proved that a reasonable pre-bending angle and forming method can effectively improve the end flaring defect of high-strength C-shaped steel.

[0043] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.

[0044] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A method for controlling the end expansion of high-strength C-shaped steel continuous roll forming, characterized in that: The following steps are involved: S1. Before the profile is roll-formed, the four forming angles of the profile are pre-bent to complete the pre-bending of the α angle and the β angle of the profile. The α angle is pre-bent to 18°, and the β angle is pre-bent to 12°. The forming method adopts the minimum strain method of the edge in the downhill forming method; S2, performing fourteen passes of forming, changing the pre-bending angle during forming, and synchronously adjusting the angle distribution of the α angle and the β angle in each pass, wherein the angle distribution sequence of the α angle is: 0°, 0°, 0°, 0°, 0°, 12°, 25°, 37°, 48°, 59°, 70°, 82°, 82° and 92°; The specific angle distribution order of the β angle is: 0°, 0°, 30°, 60°, 90°, 0°, 0°, 0°, 0°, 0°, 0°, 0°, 0° and 0°; S3. Finally, the profile is corrected after forming, with the α angle being 90° and the β angle being 90°.