A rapid die-casting equipment for aluminum alloy die-casting parts

By designing rapid die-casting equipment for aluminum alloy die-casting parts, the grouting top block and high-pressure injection mechanism are used to achieve rapid filling and smooth flow of aluminum alloy, which solves the problem of pores in aluminum alloy die-casting parts and improves the die-casting speed and quality.

CN118527628BActive Publication Date: 2024-10-22福建省鼎智新材料科技有限公司
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202411008066.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-26
Publication Date
2024-10-22
Estimated Expiration
2044-07-26

AI Technical Summary

Technical Problem

In the existing aluminum alloy die-casting technology, the aluminum liquid flows quickly during the high-pressure die-casting process, which easily produces pores and oxidation inclusion defects, while the gravity die-casting speed is slow, making it difficult to meet the needs of rapid die-casting.

Method used

A rapid die-casting equipment for aluminum alloy die-casting parts is designed. It adopts a clamping die-casting mechanism and a die-casting mold. The molten metal is divided into four mutually disconnected molding channels through a grouting top block, and a high-pressure injection mechanism is used to achieve rapid filling. , and avoid the generation of air holes through the exhaust mechanism.

Benefits of technology

It achieves smooth linear motion of the molten metal, avoids the generation of pores, improves the forming speed and quality of aluminum alloy die castings, and simultaneously achieves rapid die casting of aluminum alloy die castings.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118527628B_ABST
    Figure CN118527628B_ABST
Patent Text Reader

Abstract

The present invention provides a rapid die-casting device for aluminum alloy die-casting parts, comprising a die-casting mechanism and a die-casting mold, wherein the die-casting mold comprises a concave mold, a convex mold, a grouting top block, a lifting mechanism and a high-pressure injection mechanism, wherein a rectangular cavity is concavely provided on the surface of the concave mold, and a rectangular convex block is provided at the bottom of the convex mold. After the concave mold and the convex mold are closed, a forming mold cavity of a rectangular frame body is formed between the rectangular cavity and the rectangular convex block; the grouting top block divides the forming mold cavity into four mutually unconnected forming flow channels, so that the molten metal entering the forming flow channels can all move smoothly in a straight line along a direction parallel to the forming flow channels, and enter the forming flow channels in a laminar flow manner, so that the molten metal is not easily drawn into the gas, thereby avoiding the generation of pores, and four grouting top blocks simultaneously inject liquid into the four forming flow channels, so that the molten metal can quickly fill the forming flow channels in a short time, thereby improving the forming rate of the rectangular frame.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of aluminum alloy die casting, and in particular to a rapid die casting device for aluminum alloy die castings. Background Art

[0002] refer to Figure 1 , Figure 1 It is a rectangular frame for new energy vehicle batteries. Figure 1 When die-casting aluminum alloy castings, gravity die-casting or high-pressure die-casting is usually used. Gravity die-casting uses lower pressure and slower pouring speed. In the gravity die-casting process, the flow speed of molten metal is relatively slow. This slower flow speed allows the molten metal to enter the cavity in a laminar flow manner, which helps to reduce the gas involved in the molten metal, making the surface of the casting smooth and high-quality, and can avoid the problems of shrinkage holes and pores in the casting; while high-pressure die-casting is to force the molten metal into the cavity of the mold by high pressure, and form the casting by high-speed filling and solidification under pressure. However, in the high-pressure die-casting process, the flow speed of the aluminum liquid is fast, and the aluminum liquid will generate vortices when it flows through the corners of the cavity, which is easy to enclose the air and the cold alloy that enters the cavity first, so that the casting produces a large number of small pores and defects of oxidation inclusions; therefore, it is urgent to provide a fast die-casting equipment for aluminum alloy die-castings that can not only increase the die-casting speed of aluminum alloy die-castings, but also avoid the generation of pores in aluminum alloy die-castings. Summary of the invention

[0003] 1. Technical issues to be resolved

[0004] In order to solve the above problems in the prior art, the present invention provides a rapid die-casting device for aluminum alloy die-castings, which can improve the die-casting speed of aluminum alloy die-castings and avoid the generation of pores in the aluminum alloy die-castings.

[0005] (II) Technical solution

[0006] In order to achieve the above object, the main technical solutions adopted by the present invention include:

[0007] A rapid die-casting device for aluminum alloy die-casting parts, comprising a die-casting mechanism and a die-casting die, wherein the die-casting die comprises a concave die, a convex die, a grouting top block, a lifting mechanism and a high-pressure injection mechanism, wherein a rectangular cavity is concavely provided on the surface of the concave die, and a rectangular convex block is provided at the bottom of the convex die. After the concave die and the convex die are closed, a forming die cavity of a rectangular frame is formed between the rectangular cavity and the rectangular convex block;

[0008] The grouting top blocks are provided with four pieces, which are respectively arranged at the four corners of the molding cavity, and the molding cavity is divided into four mutually unconnected molding flow channels. The top of the grouting top block is provided with a first grouting port, and the side of one side of the grouting top block is provided with a second grouting port. The four grouting top blocks respectively inject the molten metal into the corresponding molding flow channels through the second grouting port.

[0009] A mounting groove corresponding to the grouting top block is provided in the rectangular cavity of the concave mold;

[0010] The lifting mechanism is connected to the grouting top blocks and is used to synchronously control the lifting and lowering movement of the four grouting top blocks in the installation groove;

[0011] The high-pressure injection mechanism is connected to the grouting top block through a pipeline, and is used to apply high pressure to the molten metal and then inject it into the forming flow channel through the grouting top block;

[0012] The die-casting mechanism is connected to the die-casting die and is used to control the die-casting or die-closing between the concave die and the convex die.

[0013] Preferably, the die-casting mold further includes an exhaust mechanism, which includes an upper exhaust block, a lower exhaust block, an L-shaped limit plate, a closing plate, a connecting rod and a spring;

[0014] The upper exhaust block is mounted on the male mold;

[0015] The lower exhaust block is installed on the female mold, and the upper exhaust block and the lower exhaust block are both provided with tooth grooves on one side close to each other. When the female mold and the male mold are closed, the tooth grooves of the upper exhaust block and the lower exhaust block are meshed and matched with each other, and an exhaust gap is formed between the upper exhaust block and the lower exhaust block;

[0016] One end of the horizontal portion of the L-shaped limiting plate is connected to a side of the lower exhaust block away from the concave mold, and a plurality of through holes are formed on the vertical portion of the L-shaped limiting plate;

[0017] The connecting rod is installed in the through hole, and one end of the connecting rod close to the lower exhaust block is connected to the closing plate, and the other end of the connecting rod is provided with a limit block;

[0018] The spring is sleeved on the connecting rod, one end of the spring is connected to the L-shaped limiting plate, and the other end of the spring is connected to the limiting block. Under the action of the spring, the closing plate blocks the air outlet of the exhaust gap.

[0019] Preferably, a rubber sealing strip is provided on one side of the closing plate close to the concave mold, and the rubber sealing strip is used to seal the air outlet of the exhaust gap.

[0020] Preferably, the cross-sections of the upper exhaust block and the lower exhaust block are both T-shaped structures, and the concave mold or the convex mold is provided with a accommodating groove adapted thereto.

[0021] Preferably, the lifting mechanism comprises a first hydraulic cylinder, a lifting plate and a guide rod;

[0022] The bottom of the concave mold is provided with a lifting groove adapted to the lifting plate;

[0023] The guide rod is vertically arranged in the lifting slot;

[0024] The lifting plate is provided with guide holes corresponding to the guide rods, and slurry delivery pipes are fixedly connected to the four corners of the lifting plate, and one end of the top of the slurry delivery pipe is connected to the corresponding grouting top block;

[0025] The piston rod of the first hydraulic cylinder is connected to the lifting plate.

[0026] Preferably, the die-casting mechanism comprises a base, a top seat, a support rod and a second hydraulic cylinder;

[0027] There are four support rods, which are vertically arranged at the four corners of the base surface;

[0028] The top seat is fixed on the top of the support rod;

[0029] The concave die is mounted on the base;

[0030] The second hydraulic cylinder is fixed on the top of the top seat, and the piston rod of the second hydraulic cylinder is connected to the punch, and the punch is slidably installed between the four support rods.

[0031] Preferably, a heating mechanism is further included, wherein the heating mechanism includes a metal heating wire, and the metal heating wire is wound inside the grouting top block to heat the grouting top block.

[0032] Preferably, when the grouting top block moves to the bottom of the inner wall of the installation groove, the heating mechanism is energized to heat the grouting top block.

[0033] (III) Beneficial effects

[0034] The beneficial effects of the present invention are:

[0035] 1. The grouting top block divides the molding cavity into four mutually unconnected molding channels, so that the molten metal entering the molding channels can move smoothly in a straight line along the parallel direction of the molding channels and enter the molding channels in a laminar flow manner. It is not easy for gas to be involved in the molten metal, thus avoiding the generation of pores.

[0036] 2. Four grouting top blocks inject liquid into four molding runners at the same time, so that the molten metal can quickly fill the molding runners in a short time, thereby improving the molding rate;

[0037] 3. The four grouting ejector blocks can be used as ejector rods to eject the rectangular frame in the molding cavity out of the molding cavity to achieve demoulding;

[0038] 4. The exhaust mechanism can realize one-way exhaust, which can prevent external air from entering the molding cavity;

[0039] 5. The heating mechanism can heat the grouting top block, thereby avoiding the coexistence of solid and liquid in the first grouting port and the second grouting port of the grouting top block. BRIEF DESCRIPTION OF THE DRAWINGS

[0040] Figure 1 A schematic diagram of a die casting mentioned in the background technology of the present invention;

[0041] Figure 2 It is a rapid die-casting equipment for aluminum alloy die-casting parts;

[0042] Figure 3 It is a schematic diagram of the connection structure between the concave die and the convex die;

[0043] Figure 4 It is a schematic diagram of the structure of the lifting mechanism;

[0044] Figure 5 It is a schematic diagram of the flow direction of the metal solution in the molding cavity;

[0045] Figure 6 is a schematic diagram of the structure of the exhaust mechanism;

[0046] Figure 7 It is a schematic diagram of the installation structure of the exhaust mechanism;

[0047] Figure 8 It is a structural schematic diagram of the heating mechanism.

[0048] Description of reference numerals:

[0049] 1. Die-casting mechanism;

[0050] 11. Base; 12. Support rod; 13. Top seat; 14. Second hydraulic cylinder;

[0051] 2. Die casting mold;

[0052] 21. male die; 22. female die; 221. forming flow channel; 23. grouting top block; 24. lifting mechanism; 241. guide rod; 242. lifting plate; 243. first hydraulic cylinder;

[0053] 3. Exhaust mechanism;

[0054] 31. Lower exhaust block; 32. Upper exhaust block; 33. L-shaped limit plate; 34. Closing plate; 35. Connecting rod; 36. Limit block; 37. Spring;

[0055] 4. Heating mechanism. DETAILED DESCRIPTION

[0056] In order to better explain the present invention and facilitate understanding, the present invention is described in detail below through specific implementation modes in conjunction with the accompanying drawings.

[0057] Please refer to Figures 2 to 8 The present invention provides a rapid die-casting device for aluminum alloy die-casting parts, including a die-casting mechanism 1 and a die-casting mold 2, wherein the die-casting mold 2 includes a concave mold 22, a convex mold 21, a grouting top block 23, a lifting mechanism 24 and a high-pressure injection mechanism, wherein a rectangular cavity is concavely provided on the surface of the concave mold 22, and a rectangular convex block is provided at the bottom of the convex mold 21. After the concave mold 22 and the convex mold 21 are closed, a rectangular frame forming mold cavity is formed between the rectangular cavity and the rectangular convex block;

[0058] Four grouting top blocks 23 are provided, which are respectively arranged at the four corners of the molding cavity, and the molding cavity is divided into four mutually unconnected molding flow channels 221. A first grouting port is provided at the top of the grouting top block 23, and a second grouting port is provided at one side of the grouting top block 23. The four grouting top blocks 23 respectively inject the molten metal into the corresponding molding flow channels 221 through the second grouting ports.

[0059] A mounting groove corresponding to the grouting top block 23 is provided in the rectangular cavity of the female mold 22;

[0060] The lifting mechanism 24 is connected to the grouting top block 23 and is used to synchronously control the lifting and lowering movement of the four grouting top blocks 23 in the installation groove;

[0061] The high-pressure injection mechanism is connected to the grouting top block 23 through a pipeline, and is used to apply high pressure to the molten metal and then inject it into the molding flow channel 221 through the grouting top block 23;

[0062] The die-casting mechanism 1 is connected to the die-casting die 2 and is used to control the die-casting or die-casting between the female die 22 and the male die 21;

[0063] When in use, the grouting top block 23 is driven by the lifting mechanism 24 to move upward and divide the molding cavity into four mutually unconnected molding flow channels 221. Under the action of the mold closing die-casting mechanism 1, the concave mold 22 and the convex mold 21 are closed, and the high-pressure injection mechanism applies high pressure to the molten metal and injects it into the grouting top block 23. The first grouting port on the top of the grouting top block 23 is blocked by the convex mold 21, so that the molten metal can only flow into the corresponding molding flow channel 221 from the second grouting port. The four grouting top blocks 23 inject liquid into the molding flow channel 221 at the same time, so that the molten metal can quickly fill the molding flow channel 221 in a short time, and flow out from the second grouting port. The molten metal entering the molding runner 221 moves smoothly in a straight line in a direction parallel to the molding runner 221, and enters the molding runner 221 in a laminar flow manner. The molten metal is not easily drawn into the gas, thereby avoiding the generation of pores. After the molding runner 221 is filled with molten metal, all the gas in the molding cavity is discharged, and the lifting mechanism 24 drives the grouting top block 23 back to the installation groove, and the molten metal is replenished into the molding cavity through the first grouting port on the top of the grouting top block 23, so as to fill the area originally occupied by the grouting top block 23 with the molten metal, and realize the mutual connection of the four molding runners 221, so that the rectangular frame in the molding cavity is formed.

[0064] In addition, after the rectangular frame in the molding cavity is formed, the formed rectangular frame can also be pushed out of the molding cavity by the grouting ejector block 23 to achieve demoulding.

[0065] refer to Figure 6 to Figure 7 In this embodiment, the die-casting mold 2 further includes an exhaust mechanism 3, which includes an upper exhaust block 32, a lower exhaust block 31, an L-shaped limit plate 33, a closing plate 34, a connecting rod 35 and a spring 37;

[0066] The upper exhaust block 32 is mounted on the punch 21;

[0067] The lower exhaust block 31 is installed on the die 22. The upper exhaust block 32 and the lower exhaust block 31 are both provided with tooth grooves on one side close to each other. When the die 22 and the punch 21 are closed, the tooth grooves of the upper exhaust block 32 and the lower exhaust block 31 are meshed and matched with each other, and an exhaust gap is formed between the upper exhaust block 32 and the lower exhaust block 31.

[0068] One end of the horizontal portion of the L-shaped limiting plate 33 is connected to the side of the lower exhaust block 31 away from the die 22, and a plurality of through holes are formed on the vertical portion of the L-shaped limiting plate 33;

[0069] The connecting rod 35 is installed in the through hole, and one end of the connecting rod 35 close to the lower exhaust block 31 is connected to the closing plate 34, and the other end of the connecting rod 35 is provided with a limit block 36;

[0070] The spring 37 is sleeved on the connecting rod 35, one end of the spring 37 is connected to the L-shaped limit plate 33, and the other end of the spring 37 is connected to the limit block 36. Under the action of the spring 37, the closing plate 34 blocks the air outlet of the exhaust gap;

[0071] Among them, a rubber sealing strip is provided on one side of the closing plate 34 close to the concave mold 22, and the rubber sealing strip is used to seal the air outlet of the exhaust gap;

[0072] During use, after the molding runner 221 is filled with molten metal, the gas in the molding runner 221 is discharged through the exhaust gap. When the grouting top block 23 returns to the installation groove, a certain degree of negative pressure will be generated in the molding cavity. When the negative pressure acts on the air outlet of the exhaust gap, it will attract the closing plate 34 to block the air outlet of the exhaust gap, so that the exhaust mechanism 3 can only realize one-way exhaust. When the air is inhaled in the reverse direction, it is in a self-sealing state, which can prevent external air from entering the molding cavity.

[0073] In this embodiment, the cross-sections of the upper exhaust block 32 and the lower exhaust block 31 are both T-shaped structures, and the female mold 22 or the male mold 21 is provided with a receiving groove adapted thereto.

[0074] In this embodiment, the lifting mechanism 24 includes a first hydraulic cylinder 243, a lifting plate 242 and a guide rod 241;

[0075] The bottom of the die 22 is provided with a lifting groove adapted to the lifting plate 242;

[0076] The guide rod 241 is vertically arranged in the lifting slot;

[0077] The lifting plate 242 is provided with guide holes corresponding to the guide rods 241. The four corners of the lifting plate 242 are fixedly connected with slurry delivery pipes, and one end of the top of the slurry delivery pipe is connected to the corresponding grouting top block 23.

[0078] The piston rod of the first hydraulic cylinder 243 is connected to the lifting plate 242;

[0079] refer to Figure 4 When in use, the first hydraulic cylinder 243 drives the lifting plate 242 to move up and down, and drives the grouting top block 23 to move up and down through the grouting pipe.

[0080] refer to Figure 2 In this embodiment, the die-casting mechanism 1 includes a base 11, a top seat 13, a support rod 12 and a second hydraulic cylinder 14;

[0081] Four support rods 12 are provided, and are vertically arranged at four corners of the surface of the base 11;

[0082] The top seat 13 is fixed on the top of the support rod 12;

[0083] The die 22 is mounted on the base 11;

[0084] The second hydraulic cylinder 14 is fixed on the top of the top seat 13, and the piston rod of the second hydraulic cylinder 14 is connected to the punch 21, and the punch 21 is slidably installed between the four support rods 12;

[0085] When in use, the second hydraulic cylinder 14 drives the punch 21 to rise and fall, thereby controlling the closing or opening of the die 22 and the punch 21 .

[0086] refer to Figure 8 In this embodiment, a heating mechanism 4 is further included. The heating mechanism 4 includes a metal heating wire. The metal heating wire is wound inside the grouting top block 23 and is used to heat the grouting top block 23. When the grouting top block 23 moves to the bottom of the inner wall of the installation groove, the heating mechanism 4 is energized to heat the grouting top block 23.

[0087] During use, after the grouting top block 23 pushes the formed rectangular frame out of the molding cavity, the residual metal solution in the grouting top block 23 comes into contact with cold air, which may cause the first grouting port and the second grouting port of the grouting top block 23 to coexist with solid and liquid, thereby being blocked. The solidified metal solution at the first grouting port or the second grouting port can be melted by heating with the metal heating wire to avoid being blocked.

[0088] The working principle of the present invention is as follows:

[0089] The grouting top block 23 is driven by the lifting mechanism 24 to move upward and divide the molding cavity into four mutually unconnected molding flow channels 221. Under the action of the mold closing die casting mechanism 1, the concave mold 22 and the punch 21 are closed. The high-pressure injection mechanism applies high pressure to the molten metal and then injects it into the grouting top block 23. The first grouting port on the top of the grouting top block 23 is blocked by the punch 21, so that the molten metal can only flow into the corresponding molding flow channel 221 from the second grouting port. The four grouting top blocks 23 inject liquid into the molding flow channel 221 at the same time, so that the molten metal can quickly fill the molding flow channel 221 in a short time, and the molten metal flowing into the molding flow channel 221 from the second grouting port is parallel to the molding flow channel 221. The molten metal moves smoothly in a straight line in the direction and enters the molding flow channel 221 in a laminar flow manner. The gas is not easily drawn into the molten metal, thereby avoiding the generation of pores. After the molding flow channel 221 is filled with the molten metal, all the gas in the molding cavity is discharged, and the lifting mechanism 24 drives the grouting top block 23 back to the installation groove, and the metal solution is replenished into the molding cavity through the first grouting port on the top of the grouting top block 23, so as to fill the area originally occupied by the grouting top block 23 with the metal solution, and realize the mutual connection of the four molding flow channels 221, so that the rectangular frame in the molding cavity is formed. After the rectangular frame in the molding cavity is formed, the formed rectangular frame can also be pushed out of the molding cavity by the grouting top block 23 to realize demoulding.

[0090] The above are only embodiments of the present invention, and are not intended to limit the patent scope of the present invention. Any equivalent transformations made using the contents of the specification and drawings of the present invention, or directly or indirectly applied in related technical fields, are also included in the patent protection scope of the present invention.

[0091] In addition, it should be understood that although the present specification is described according to implementation modes, not every implementation mode contains only one independent technical solution. This description of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment may also be appropriately combined to form other implementation modes that can be understood by those skilled in the art.

Claims

1. A rapid die-casting equipment for aluminum alloy die-castings, characterized in that: The die-casting device comprises a die-casting mechanism (1) and a die-casting die (2), wherein the die-casting die (2) comprises a concave die (22), a convex die (21), a grouting top block (23), a lifting mechanism (24) and a high-pressure injection mechanism, wherein a rectangular cavity is concavely provided on the surface of the concave die (22), and a rectangular protruding block is provided on the bottom of the convex die (21); after the concave die (22) and the convex die (21) are closed, a rectangular frame forming die cavity is formed between the rectangular cavity and the rectangular protruding block; Four grouting top blocks (23) are provided, which are respectively arranged at the four corners of the molding cavity and divide the molding cavity into four mutually unconnected molding flow channels. A first grouting port is provided at the top of the grouting top block (23), and a second grouting port is provided at one side of the grouting top block (23). The four grouting top blocks (23) respectively inject molten metal into the corresponding molding flow channels through the second grouting ports. A mounting groove corresponding to the grouting top block (23) is provided in the rectangular cavity of the concave mold (22); The lifting mechanism (24) is connected to the grouting top blocks (23) and is used for synchronously controlling the lifting and lowering movement of the four grouting top blocks (23) in the installation groove; The high-pressure injection mechanism is connected to the grouting top block (23) via a pipeline, and is used to apply high pressure to the molten metal and then inject it into the molding flow channel through the grouting top block (23); The die-casting mechanism (1) is connected to the die-casting die (2) and is used to control the die-casting or die-closing between the female die (22) and the male die (21).

2. The rapid die-casting equipment for aluminum alloy die-casting according to claim 1, characterized in that: The die-casting mold (2) further comprises an exhaust mechanism (3), wherein the exhaust mechanism (3) comprises an upper exhaust block (32), a lower exhaust block (31), an L-shaped limiting plate (33), a closing plate (34), a connecting rod (35), and a spring (37); The upper exhaust block (32) is mounted on the male mold (21); The lower exhaust block (31) is mounted on the female die (22), and the upper exhaust block (32) and the lower exhaust block (31) are both provided with tooth grooves on one side close to each other, so that when the female die (22) and the male die (21) are closed, the tooth grooves of the upper exhaust block (32) and the lower exhaust block (31) mesh with each other, and an exhaust gap is formed between the upper exhaust block (32) and the lower exhaust block (31); One end of the horizontal portion of the L-shaped limiting plate (33) is connected to a side of the lower exhaust block (31) away from the die (22), and a plurality of through holes are formed on the vertical portion of the L-shaped limiting plate (33); The connecting rod (35) is installed in the through hole, and one end of the connecting rod (35) close to the lower exhaust block (31) is connected to the closing plate (34), and the other end of the connecting rod (35) is provided with a limiting block (36); The spring (37) is sleeved on the connecting rod (35), one end of the spring (37) is connected to the L-shaped limit plate (33), and the other end of the spring (37) is connected to the limit block (36); under the action of the spring (37), the closing plate (34) blocks the air outlet of the exhaust gap.

3. The rapid die-casting equipment for aluminum alloy die-casting according to claim 2, characterized in that: A rubber sealing strip is provided on one side of the closing plate (34) close to the concave mold (22), and the rubber sealing strip is used to seal the air outlet of the exhaust gap.

4. The rapid die-casting equipment for aluminum alloy die-casting according to claim 2, characterized in that: The cross-sections of the upper exhaust block (32) and the lower exhaust block (31) are both T-shaped structures, and the concave mold (22) or the convex mold (21) is provided with a matching accommodation groove.

5. The rapid die-casting equipment for aluminum alloy die-casting according to claim 1, characterized in that: The lifting mechanism (24) comprises a first hydraulic cylinder (243), a lifting plate (242) and a guide rod (241); The bottom of the concave mold (22) is provided with a lifting groove adapted to the lifting plate (242); The guide rod (241) is vertically arranged in the lifting slot; The lifting plate (242) is provided with guide holes corresponding to the guide rods (241); grouting pipes are fixedly connected to the four corners of the lifting plate (242); and one end of the top of the grouting pipe is connected to the corresponding grouting top block (23); The piston rod of the first hydraulic cylinder (243) is connected to the lifting plate (242).

6. The rapid die-casting equipment for aluminum alloy die-casting according to claim 1, characterized in that: The mold-closing die-casting mechanism (1) comprises a base (11), a top base (13), a support rod (12) and a second hydraulic cylinder (14); Four support rods (12) are provided, and are vertically arranged at four corners of the surface of the base (11); The top seat (13) is fixed on the top of the support rod (12); The concave mold (22) is mounted on the base (11); The second hydraulic cylinder (14) is fixed on the top of the top seat (13), and the piston rod of the second hydraulic cylinder (14) is connected to the punch (21), and the punch (21) is slidably installed between the four support rods (12).

7. The rapid die casting equipment for aluminum alloy die castings according to claim 1, characterized in that: It also comprises a heating mechanism (4), the heating mechanism (4) comprising a metal heating wire, the metal heating wire being wound inside the grouting top block (23) and being used to heat the grouting top block (23).

8. The rapid die-casting equipment for aluminum alloy die-castings according to claim 7, characterized in that: When the grouting top block (23) moves to the bottom of the inner wall of the installation groove, the heating mechanism (4) is energized to heat the grouting top block (23).

Citation Information

Cited By

  • Automatic die-casting mechanism for aluminum alloy accessory preparation

    CN120772494A

  • An automatic die-casting mechanism for preparing aluminum alloy fittings

    CN120772494B