A shale brittleness evaluation method and device based on mechanical failure and heterogeneity
Through mechanical experiments and computer control equipment, the shale core samples were tested and the brittleness index was calculated, which solved the problem of poor accuracy in shale brittleness evaluation in the existing technology, and achieved a comprehensive and accurate evaluation of shale brittleness characteristics.
Patent Information
- Application Number
- CN202410536702.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-29
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2044-04-29
AI Technical Summary
The existing shale brittleness evaluation methods have problems such as limited sample number and low resolution of logging data, resulting in poor evaluation accuracy.
Using a shale brittleness evaluation method based on mechanical failure and heterogeneity, the shale core sample is tested uniaxially through a mechanical experimental device to obtain basic mechanical parameters, and the brittleness index is calculated using computer-controlled equipment, combined with heterogeneity Sex analysis, comprehensively calculate the shale brittleness index.
A comprehensive and accurate evaluation of shale brittleness characteristics has been achieved, the accuracy and efficiency of evaluation have been improved, and a scientific basis for shale gas development has been provided.
Smart Images

Figure CN118533645B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of petroleum geological exploration, and in particular to a shale brittleness evaluation method and equipment based on mechanical failure and heterogeneity. Background Art
[0002] At present, mankind is facing the replacement of old and new energy sources, and unconventional oil and gas resources represented by shale gas are playing an important role. As an important unconventional natural gas resource, the development of shale gas resources has received widespread attention. The efficiency of shale gas development is closely related to the brittleness characteristics of its reservoir. Therefore, the accurate evaluation of shale brittleness is of great significance for the development of shale gas. At present, the commonly used shale brittleness evaluation methods are mainly based on core experiments and logging data, but these methods have certain limitations, such as the limited number of samples in core experiments and the low resolution of logging data. Therefore, it is necessary to study a new shale brittleness evaluation method to improve the accuracy and efficiency of the evaluation. Summary of the invention
[0003] In view of this, the present invention proposes a shale brittleness evaluation method and equipment based on mechanical failure and heterogeneity, integrates and optimizes the current mainstream rock brittleness evaluation method, and designs a set of mechanical experimental equipment and computer control equipment based on this to solve the problem of poor accuracy of shale brittleness evaluation in the prior art.
[0004] The present invention discloses a shale brittleness evaluation method based on mechanical failure and heterogeneity, the method comprising:
[0005] S1. Core sample preparation: select shale core samples, clean, dry and cut them, and prepare them into standard specimens;
[0006] S2. Mechanical parameter test: Perform uniaxial mechanical test on the standard specimen using a mechanical experimental device, and obtain basic mechanical parameters of the standard specimen through preset formulas in a computer-controlled device, wherein the basic mechanical parameters include compressive strength and stress-strain curve;
[0007] S3. Failure morphology analysis: Based on the stress-strain curve, analyze the stress rising rate before the peak value of the curve and the stress falling rate from the peak value to the residual point during the failure process;
[0008] S4. Stress failure brittleness evaluation: Based on the strain characteristics of the pre-peak, post-peak and peak points, the stress failure brittleness index of each standard specimen is calculated using a preset formula;
[0009] S5. Heterogeneity analysis: Calculate the heterogeneity of each standard specimen using a preset formula and statistically analyze the heterogeneity probability distribution;
[0010] S6. Heterogeneity brittleness evaluation: Based on the heterogeneity probability distribution and the preset brittleness evaluation standard, the heterogeneity brittleness index of each standard specimen is calculated using the preset formula;
[0011] S7. Based on shale failure morphology analysis and heterogeneity analysis, the shale brittleness index is comprehensively calculated.
[0012] Optionally, S1 specifically includes: selecting shale core samples, cleaning, drying and cutting them to prepare standard specimens; performing physical property tests on the prepared standard specimens, the physical property tests including density tests, porosity tests and permeability tests; and randomly selecting a number of standard specimens for mechanical parameter tests based on the physical property test results.
[0013] Optionally, in S2, a uniaxial mechanical test is performed on the standard specimen using a mechanical experimental device, and specific operations include: placing the prepared standard specimen in the mechanical experimental device; using a computer control device to control the mechanical experimental device to perform a mechanical experiment on the standard specimen, and describing the experimental mechanical properties, and calculating corresponding mechanical parameters.
[0014] Optionally, the brittleness index calculation formula is:
[0015] BI1=(σ c -σ t ) / σ c ;
[0016] BI2=B i1 ·B i2 ·B i3
[0017] BI=(BI1+BI2) / 2
[0018] Among them, BI1 is the heterogeneous brittleness index, σ c is the compressive strength, σ t is the tensile strength; BI2 is the stress fracture brittleness index, B i1 is the pre-peak brittleness index, B i2 is the post-peak brittleness index, B i3 is the strain control coefficient; BI is the brittleness index.
[0019] Optionally, when the brittleness index BI≥0.5, the shale is brittle; when 0.3≤BI<0.5, the shale is semi-brittle; when BI<0.3, the shale is non-brittle.
[0020] Optionally, the method further includes: modifying the brittleness index BI according to the mineral composition, pore size and number of micro cracks of the shale.
[0021] Optionally, the calculated brittleness index BI is first corrected by the pore size, including:
[0022] Set the pore size of the standard specimen to T, pre-set the first pore size t1, the second pore size t2, the third pore size t3, the fourth pore size t4 and the fifth pore size t5, preset the first brittleness index adjustment coefficient x1, the second first brittleness index adjustment coefficient x2, the third first brittleness index adjustment coefficient x3, the fourth first brittleness index adjustment coefficient x4 and the fifth first brittleness index adjustment coefficient x5, and t1<t2<t3<t4<t5, 0.9<x1<x2<x3<x4<x5<1.1; obtain the calculated brittleness index BI; and determine the first brittleness index adjustment coefficient of the brittleness index BI according to the size relationship between the pore size T of the standard specimen and the pre-set pore sizes ti, i=1, 2, 3, 4, 5, and make a first correction to the brittleness index BI;
[0023] When T≤t1, the first brittleness index adjustment coefficient is determined as the first first brittleness index adjustment coefficient x1, and the brittleness index after the first adjustment is BI*x1;
[0024] When t1<T≤t2, the first brittleness index adjustment coefficient is determined as the second first brittleness index adjustment coefficient x2, and the brittleness index after the first adjustment is BI*x2;
[0025] When t2<T≤t3, the first brittleness index adjustment coefficient is determined as the third first brittleness index adjustment coefficient x3, and the brittleness index after the first adjustment is BI*x3;
[0026] When t3<T≤t4, the first brittleness index adjustment coefficient is determined as the fourth first brittleness index adjustment coefficient x4, and the brittleness index after the first adjustment is BI*x4;
[0027] When t4<T≤t5, the first brittleness index adjustment coefficient is determined as the fifth first brittleness index adjustment coefficient x5, and the brittleness index after the first adjustment is BI*x5.
[0028] Optionally, the calculated brittleness index BI is corrected twice according to the number of micro cracks, including:
[0029] The number of micro cracks of the standard specimen is set as U, the first number of micro cracks u1, the second number of micro cracks u2, the third number of micro cracks u3, the fourth number of micro cracks u4 and the fifth number of micro cracks u5 are preset, the first final brittle index adjustment coefficient y1, the second final brittle index adjustment coefficient y2, the third final brittle index adjustment coefficient y3, the fourth final brittle index adjustment coefficient y4 and the fifth final brittle index adjustment coefficient y5 are preset, and u1<u2<u3<u4<u5, 0.9<y1<y2<y3<y4<y5<1.1; the brittle index BI*xi after the first adjustment is obtained; and according to the relationship between the number of micro cracks U of the standard specimen and the preset number of micro cracks ui, i=1, 2, 3, 4, 5, the final brittle index adjustment coefficient of the brittle index BI is determined, and the brittle index BI is corrected twice;
[0030] When U≤u1, the final brittleness index adjustment coefficient is determined as the first final brittleness index adjustment coefficient y1, and the final adjusted brittleness index is BI*xi*y1;
[0031] When u1<U≤u2, the final brittleness index adjustment coefficient is determined as the second final brittleness index adjustment coefficient y2, and the final adjusted brittleness index is BI*xi*y2;
[0032] When u2<U≤u3, the final brittleness index adjustment coefficient is determined as the third final brittleness index adjustment coefficient y3, and the final adjusted brittleness index is BI*xi*y3;
[0033] When u3<U≤u4, the final brittleness index adjustment coefficient is determined as the fourth final brittleness index adjustment coefficient y4, and the final adjusted brittleness index is BI*xi*y4;
[0034] When u4<U≤u5, the final brittleness index adjustment coefficient is determined as the fifth final brittleness index adjustment coefficient y5, and the final adjusted brittleness index is BI*xi*y5.
[0035] The present invention also discloses a shale brittleness evaluation device based on mechanical failure and heterogeneity, which is used to implement the above-mentioned shale brittleness evaluation method based on mechanical failure and heterogeneity. The device comprises:
[0036] A mechanical experimental device, comprising an experimental mechanical shell, an experimental platform, a specimen holder, a high-strength casing, a pressure column and a stress strain gauge, wherein a cap is fixedly installed inside the experimental mechanical shell, a base is fixedly installed on the top of the cap, the experimental platform is fixedly installed on the base, the specimen holder is installed on the experimental platform, the high-strength casing is installed in the middle of the specimen holder, the specimen holder is used to fix the high-strength casing on the experimental platform, the pressure column is arranged on both sides and the upper side of the high-strength casing, and the stress strain gauge is fixedly installed on both sides of the high-strength casing;
[0037] An experimental auxiliary device, the experimental auxiliary device comprises a gas tank, an oil tank and a liquid tank, the gas tank, the oil tank and the liquid tank are connected to the mechanical experimental device through a connecting pipeline, a peristaltic pump is arranged on the connecting pipeline, and the gas tank, the oil tank and the liquid tank are connected to the connecting pipeline through an inlet steel pipe;
[0038] The control device comprises a computer display, a main switch, an integrated control pipeline and a computer host; the main switch is connected to an oil inlet controller, a liquid inlet controller and an air inlet controller, the computer host comprises a computer memory, a computer CPU and a computer graphics card, the computer host is connected to a stress strain gauge via a connecting pipeline and an integrated control pipeline, and the stress strain gauge is used to transmit basic mechanical parameters to the computer host via the connecting pipeline and the integrated control pipeline.
[0039] Optionally, the pressure column includes a gas, liquid and oil inlet pipe, a primary telescopic pipe, a secondary telescopic pipe, a primary force transmission pipe, a secondary force transmission pipe and a pressure plate;
[0040] The gas, liquid and oil inlet pipe is installed inside the bottom of the pressure column, the secondary telescopic tube is sleeved in the primary telescopic tube, the primary telescopic tube is outerly provided with a pressure rod sleeve, the pressure rod sleeve is connected to the bottom of the pressure column, the primary force transmission tube is outerly provided with a rubber hose sleeve, one side of the rubber hose sleeve is connected to the pressure rod sleeve, and the other side of the rubber hose sleeve is connected to the secondary force transmission tube, and the secondary force transmission tube is connected to the pressure plate through a soft pad.
[0041] Compared with the prior art, the beneficial effect of the present invention is: a shale brittleness evaluation method and equipment based on mechanical failure and heterogeneity, which can comprehensively and accurately evaluate the brittle characteristics of shale. The method first prepares the shale core sample, and then uses the mechanical testing equipment to perform uniaxial mechanical testing on the standard specimen to obtain the basic mechanical parameters of the specimen. Then, according to the preset brittleness index calculation formula, the brittleness index of each specimen is calculated. Then, the brittleness index of each specimen is statistically analyzed to obtain the probability distribution of the brittleness index, thereby analyzing the mechanical heterogeneity of the shale. Finally, according to the probability distribution of the brittleness index, combined with the preset brittleness evaluation standard, the brittleness of the shale is evaluated. BRIEF DESCRIPTION OF THE DRAWINGS
[0042] By reading the detailed description of the preferred embodiment below, various other advantages and benefits will become clear to those of ordinary skill in the art. The accompanying drawings are only used for the purpose of illustrating the preferred embodiment and are not considered to be limitations of the present invention. In addition, the same reference symbols are used to represent the same components throughout the accompanying drawings.
[0043] Figure 1 A schematic flow chart of a shale brittleness evaluation method based on mechanical failure and heterogeneity provided in an embodiment of the present invention;
[0044] Figure 2 A schematic diagram of the structure of a shale brittleness evaluation device based on mechanical failure and heterogeneity provided in an embodiment of the present invention;
[0045] Figure 3 A schematic diagram of the structure of a pressure column provided by an embodiment of the present invention;
[0046] Figure 4 A schematic diagram of a computer display provided by an embodiment of the present invention;
[0047] Figure 5 A schematic diagram for characterizing the pre-peak and post-peak brittleness of shale is provided for an embodiment of the present invention.
[0048] Among them, 1. Experimental mechanical shell; 2. Support platform; 3. Base; 4. Experimental platform; 5. Specimen holder; 6. Pressure column; 61. Pressure column bottom; 62. Gas, liquid and oil inlet pipe; 63. Pressure rod sleeve; 64. Primary telescopic tube; 65. Secondary telescopic tube; 66. Rubber hose sleeve; 67. Primary force transmission tube; 68. Secondary force transmission tube; 69. Soft pad; 610. Pressure plate; 7. Stress strain gauge; 8. High-strength casing; 11. Connecting pipeline; 12. Main switch; 13. Air intake controller; 14. , liquid inlet controller; 15, oil inlet controller; 16, oil tank; 17, liquid tank; 18, gas tank; 19, entering steel pipe; 20, valve; 21, integrated inlet pipe; 22, peristaltic pump; 23, computer graphics card; 24, computer CPU; 25, computer memory; 26, integrated control pipeline; 27, computer display; 271, control panel switch; 272, touch and experimental module; 273, comprehensive brittleness evaluation module; 274, stress failure evaluation module; 275, heterogeneity evaluation module. DETAILED DESCRIPTION
[0049] Exemplary embodiments of the present disclosure will be described in more detail below with reference to the accompanying drawings. Although exemplary embodiments of the present disclosure are shown in the accompanying drawings, it should be understood that the present disclosure can be implemented in various forms and should not be limited by the embodiments described herein. On the contrary, these embodiments are provided in order to enable a more thorough understanding of the present disclosure and to fully convey the scope of the present disclosure to those skilled in the art. It should be noted that, in the absence of conflict, the embodiments of the present invention and the features described in the embodiments can be combined with each other. The present invention will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.
[0050] Please refer to Figure 1-5 The present invention provides a shale brittleness evaluation method based on mechanical failure and heterogeneity, the method comprising:
[0051] S1. Core sample preparation: select shale core samples, clean, dry and cut them, and prepare them into standard specimens.
[0052] S2. Mechanical parameter test: Perform uniaxial mechanical test on the standard specimen using a mechanical experimental device, and obtain basic mechanical parameters of the standard specimen through preset formulas in the computer-controlled equipment. The basic mechanical parameters include compressive strength and stress-strain curve.
[0053] S3. Failure morphology analysis: Based on the stress-strain curve, analyze the stress rise rate before the peak value of the curve and the stress drop rate from the peak value to the residual point during the failure process.
[0054] S4. Stress failure brittleness evaluation: Based on the strain characteristics of the pre-peak, post-peak and peak points, the stress failure brittleness index of each standard specimen is calculated using a preset formula.
[0055] S5. Heterogeneity analysis: Use the preset formula to calculate the heterogeneity of each standard specimen, and statistically analyze the heterogeneity probability distribution.
[0056] S6. Heterogeneous brittleness evaluation: Based on the heterogeneity probability distribution and the preset brittleness evaluation standard, the heterogeneous brittleness index of each standard specimen is calculated using the preset formula.
[0057] S7. Based on shale failure morphology analysis and heterogeneity analysis, the shale brittleness index is comprehensively calculated.
[0058] In some embodiments of the present application, S1 specifically includes: selecting shale core samples, cleaning, drying and cutting them to prepare them into standard specimens; performing physical property tests on the prepared standard specimens, the physical property tests including density tests, porosity tests and permeability tests; based on the physical property test results, randomly selecting a number of standard specimens for mechanical parameter testing.
[0059] In some embodiments of the present application, in S2, a uniaxial mechanical test is performed on the standard specimen using a mechanical experimental device, and specific operations include: placing the prepared standard specimen in the mechanical experimental device; using a computer control device to control the mechanical experimental device to perform a mechanical experiment on the standard specimen, and describing the experimental mechanical properties, and calculating the corresponding mechanical parameters.
[0060] It can be understood that the specific operations include: placing the prepared standard shale core specimen in the high-strength casing 8, and using the specimen holder 5 to stabilize and reinforce the standard specimen; turning on the main switch 12 of the operation panel, turning on the computer control equipment and the peristaltic pump 22; at the same time, starting the air inlet controller 13, the liquid inlet controller 14 and the oil inlet controller 15 to open the valve 20, so as to cause the fluid in the oil tank 16, the liquid tank 17 and the gas tank 18 to enter the mechanical experimental device through the connecting pipeline 11, which is used for lubrication and gas-liquid joint drive pressurization to carry out mechanical testing experiments; during the experiment, the mechanical parameters are transmitted back to the computer memory 25 through the connecting pipeline 11 and the integrated control pipeline 26 through the high-sensitivity micron-level stress and strain gauge 7, and the mechanical parameters and images such as the stress-strain curve are calculated by using the computer CPU 24 using the preset formula in the computer memory 25, and are displayed on the computer display 27 through the computer graphics card 23.
[0061] It can be understood that by cleaning, drying and cutting the shale core samples to prepare standard specimens, the accuracy and repeatability of the test are guaranteed. By using mechanical testing equipment to conduct uniaxial mechanical tests on the standard specimens and obtain the basic mechanical parameters of the specimens, the mechanical properties of shale can be fully understood.
[0062] In some embodiments of the present application, the brittleness index calculation formula is:
[0063] BI1=(σ c -σ t ) / σ c ;
[0064] BI2=B i1 ·B i2 ·B i3
[0065] BI=(BI1+BI2) / 2
[0066] Among them, BI1 is the heterogeneous brittleness index, σ c is the compressive strength, σ t is the tensile strength; BI2 is the stress fracture brittleness index, B i1 is the pre-peak brittleness index, B i2 is the post-peak brittleness index, B i3 is the strain control coefficient; BI is the brittleness index.
[0067] In some embodiments of the present application, when the brittleness index BI≥0.5, the shale is brittle; when 0.3≤BI<0.5, the shale is semi-brittle; when BI<0.3, the shale is non-brittle.
[0068] It is understandable that the brittleness of shale can be objectively evaluated by using the preset brittleness index calculation formula and calculating the brittleness index of each specimen based on the obtained mechanical parameters. The brittleness index of each specimen is statistically analyzed to obtain the probability distribution of the brittleness index, which can analyze the mechanical heterogeneity of shale and provide a scientific basis for the development of shale oil and gas.
[0069] In some embodiments of the present application, the method further includes: modifying the brittleness index BI according to the mineral composition, pore size and number of micro cracks of the shale.
[0070] In some embodiments of the present application, the calculated brittleness index BI is first corrected by the pore size, including: setting the pore size of the standard specimen to T, pre-setting the first pore size t1, the second pore size t2, the third pore size t3, the fourth pore size t4 and the fifth pore size t5, pre-setting the first first brittleness index adjustment coefficient x1, the second first brittleness index adjustment coefficient x2, the third first brittleness index adjustment coefficient x3, the fourth first brittleness index adjustment coefficient x4 and the fifth first brittleness index adjustment coefficient x5, and t1<t2<t3<t4<t5, 0.9<x1<x2<x3<x4<x5<1.1; obtaining the calculated brittleness index BI; and determining the first brittleness index adjustment coefficient of the brittleness index BI according to the size relationship between the pore size T of the standard specimen and the pre-set pore sizes ti, i=1, 2, 3, 4, 5, and performing the first correction on the brittleness index BI.
[0071] When T≤t1, the first brittleness index adjustment coefficient is determined as the first first brittleness index adjustment coefficient x1, and the brittleness index after the first adjustment is BI*x1; when t1<T≤t2, the first brittleness index adjustment coefficient is determined as the second first brittleness index adjustment coefficient x2, and the brittleness index after the first adjustment is BI*x2; when t2<T≤t3, the first brittleness index adjustment coefficient is determined as the third first brittleness index adjustment coefficient x3, and the brittleness index after the first adjustment is BI*x3; when t3<T≤t4, the first brittleness index adjustment coefficient is determined as the fourth first brittleness index adjustment coefficient x4, and the brittleness index after the first adjustment is BI*x4; when t4<T≤t5, the first brittleness index adjustment coefficient is determined as the fifth first brittleness index adjustment coefficient x5, and the brittleness index after the first adjustment is BI*x5.
[0072] It is understandable that the evaluation of shale brittleness based on the probability distribution of the brittleness index and the preset brittleness evaluation standard can guide the fracturing design and construction in actual engineering. Considering factors such as the mineral composition, pore size, and number of microcracks of shale, the calculated brittleness index can be corrected by pore size and number of microcracks to more accurately evaluate the brittleness of shale. The first correction of the brittleness index by pore size can reflect the heterogeneity of the internal structure of shale and improve the accuracy of the evaluation.
[0073] In some embodiments of the present application, the calculated brittleness index BI is corrected secondary by the number of microcracks, including: setting the number of microcracks of the standard specimen to U, pre-setting the first microcrack number u1, the second microcrack number u2, the third microcrack number u3, the fourth microcrack number u4 and the fifth microcrack number u5, pre-setting the first final brittleness index adjustment coefficient y1, the second final brittleness index adjustment coefficient y2, the third final brittleness index adjustment coefficient y3, the fourth final brittleness index adjustment coefficient y4 and the fifth final brittleness index adjustment coefficient y5, and u1<u2<u3<u4<u5, 0.9<y1<y2<y3<y4<y5<1.1; obtaining the brittleness index BI*xi after the first adjustment; and determining the final brittleness index adjustment coefficient of the brittleness index BI according to the relationship between the number of microcracks U of the standard specimen and the pre-set numbers of microcracks ui, i=1, 2, 3, 4, 5, and performing secondary correction on the brittleness index BI.
[0074] When U≤u1, the final brittleness index adjustment coefficient is determined as the first final brittleness index adjustment coefficient y1, and the final adjusted brittleness index is BI*xi*y1; when u1<U≤u2, the final brittleness index adjustment coefficient is determined as the second final brittleness index adjustment coefficient y2, and the final adjusted brittleness index is BI*xi*y2; when u2<U≤u3, the final brittleness index adjustment coefficient is determined as the third final brittleness index adjustment coefficient y3, and the final adjusted brittleness index is BI*xi*y3; when u3<U≤u4, the final brittleness index adjustment coefficient is determined as the fourth final brittleness index adjustment coefficient y4, and the final adjusted brittleness index is BI*xi*y4; when u4<U≤u5, the final brittleness index adjustment coefficient is determined as the fifth final brittleness index adjustment coefficient y5, and the final adjusted brittleness index is BI*xi*y5.
[0075] It can be understood that in this preferred embodiment, the calculation formula of the brittleness index is optimized by considering factors such as the mineral composition, pore size, number of microcracks, mechanical properties and failure characteristics of shale, thereby improving the accuracy and reliability of shale brittleness. First, by correcting the pore size, the brittleness index after the first adjustment is determined according to the pore size of the standard specimen and the preset pore size and the corresponding brittleness index adjustment coefficient. Then, a secondary correction is made by the number of microcracks, considering the influence of the number of microcracks on the brittleness index, and the final adjusted brittleness index is determined. This correction method that comprehensively considers multiple factors can more accurately reflect the brittle characteristics of shale, thereby providing a more reliable basis and guidance for shale exploration and development. In addition, the secondary correction of the brittleness index by the number of microcracks can further consider the distribution of cracks inside the shale, making the evaluation result more reliable. Finally, the brittleness index after the secondary correction is combined with the stress failure brittleness index calculated by the preset formula to calculate the comprehensive brittleness index of shale.
[0076] The present invention also discloses a shale brittleness evaluation device based on mechanical failure and heterogeneity, which is used to implement the above-mentioned shale brittleness evaluation method based on mechanical failure and heterogeneity. The device comprises:
[0077] A mechanical experimental device, the mechanical experimental device includes an experimental mechanical housing 1, an experimental platform 4, a specimen fixture 5, a high-strength casing 8, a pressure column 6 and a stress strain gauge 7. A base 2 is fixedly installed inside the experimental mechanical housing 1, a base 3 is fixedly installed on the top of the base 2, the experimental platform 4 is fixedly installed on the base 3, the specimen fixture 5 is installed on the experimental platform 4, the high-strength casing 8 is installed in the middle of the specimen fixture 5, the specimen fixture 5 is used to fix the high-strength casing 8 on the experimental platform 4, the pressure column 6 is arranged on both sides and the upper side of the high-strength casing 8, and the stress strain gauge 7 is fixedly installed on both sides of the high-strength casing 8.
[0078] An experimental auxiliary device, which includes a gas tank 18, an oil tank 16 and a liquid tank 17. The gas tank 18, the oil tank 16 and the liquid tank 17 are connected to the mechanical experimental device through a connecting pipeline 11. A peristaltic pump 22 is provided on the connecting pipeline 11. The gas tank 18, the oil tank 16 and the liquid tank 17 are connected to the connecting pipeline 11 by entering a steel pipe 19.
[0079] A control device, the control device includes a computer display 27, a main switch 12, an integrated control pipeline 26 and a computer host; the main switch 12 is connected to the oil inlet controller 15, the liquid inlet controller 14 and the air inlet controller 13, the computer host includes a computer memory 25, a computer CPU 24 and a computer graphics card 23, the computer host is connected to the stress strain gauge 7 through the connecting pipeline 11 and the integrated control pipeline 26, and the stress strain gauge 7 is used to transmit basic mechanical parameters to the computer host through the connecting pipeline 11 and the integrated control pipeline 26.
[0080] In some embodiments of the present application, the pressure column 6 includes a gas, liquid and oil inlet pipe 62, a first-level telescopic pipe 64, a second-level telescopic pipe 65, a first-level force transmission pipe 67, a second-level force transmission pipe 68 and a pressure plate 610; the gas, liquid and oil inlet pipe 62 is installed inside the pressure column bottom 61, the second-level telescopic pipe 65 is sleeved in the first-level telescopic pipe 64, the first-level telescopic pipe 64 is outerly provided with a pressure rod sleeve 63, the pressure rod sleeve 63 is connected to the pressure column bottom 61, the first-level force transmission pipe 67 is outerly provided with a rubber hose sleeve 66, one side of the rubber hose sleeve 66 is connected to the pressure rod sleeve 63, and the other side of the rubber hose sleeve 66 is connected to the second-level force transmission pipe 68, and the second-level force transmission pipe 68 is connected to the pressure plate 610 through a soft pad 69.
[0081] In some embodiments of the present application, the computer display 27 includes a control panel switch 271 and a display screen, wherein the control panel switch 271 is used to control the opening and closing of the display screen, and the display screen includes a touch and experimental module 272, a comprehensive brittleness evaluation module 273, a stress failure evaluation module 274 and a heterogeneity evaluation module 275.
[0082] In summary, the present application adopts a shale brittleness evaluation method and equipment based on mechanical failure and heterogeneity, which can comprehensively and accurately evaluate the brittle characteristics of shale. The method first prepares the shale core sample, and then uses the mechanical testing equipment to perform uniaxial compression and uniaxial tension tests on the standard specimen to obtain the basic mechanical parameters of the specimen. Then, according to the preset brittleness index calculation formula, the heterogeneous brittleness index and stress failure brittleness index of each specimen are calculated. Then, the brittleness index of each specimen is statistically analyzed to obtain the probability distribution of the brittleness index, thereby analyzing the mechanical heterogeneity of the shale. Finally, according to the probability distribution of the brittleness index and the preset brittleness evaluation standard, and combined with the stress failure brittleness index, the brittleness of the shale is comprehensively evaluated.
[0083] Those skilled in the art will appreciate that the embodiments of the present application may be provided as methods, systems or computer program products. Therefore, the present application may adopt the form of a complete hardware embodiment, a complete software embodiment, or an embodiment in combination with software and hardware. Moreover, the present application may adopt the form of a computer program product implemented on one or more computer-usable storage media (including but not limited to disk storage, CD-ROM, optical storage, etc.) containing computer-usable program codes.
[0084] The present application is described with reference to flowcharts and / or block diagrams of methods, devices (systems) and computer program products according to embodiments of the present application. It should be understood that each process and / or box in the flowchart and / or block diagram, as well as the combination of processes and / or boxes in the flowchart and / or block diagram, can be implemented by computer program instructions. These computer program instructions can be provided to a processor of a general-purpose computer, a special-purpose computer, an embedded processor or other programmable data processing device to generate a machine, so that the instructions executed by the processor of the computer or other programmable data processing device generate instructions for implementing the processes in the flowchart and / or block diagram. Figure 1 A process or multiple processes and / or boxes Figure 1 A device that provides the functions specified in a block or multiple blocks.
[0085] These computer program instructions may also be stored in a computer-readable memory capable of directing a computer or other programmable data processing device to operate in a specific manner, so that the instructions stored in the computer-readable memory produce an article of manufacture comprising an instruction device, which implements the process Figure 1 A process or multiple processes and / or boxes Figure 1 A function specified in one or more boxes.
[0086] These computer program instructions can also be loaded onto a computer or other programmable data processing device so that a series of operating steps are executed on the computer or other programmable device to produce a computer-implemented process, thereby providing instructions for implementing the process. Figure 1 A process or multiple processes and / or boxes Figure 1 The steps for the functions specified in one or more boxes.
[0087] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the above embodiments, ordinary technicians in the relevant field should understand that the specific implementation methods of the present invention can still be modified or replaced by equivalents. Any modification or equivalent replacement that does not depart from the spirit and scope of the present invention should be covered within the scope of protection of the claims of the present invention.
Claims
1. A shale brittleness evaluation method based on mechanical failure and heterogeneity, characterized in that: The method comprises: S1. Core sample preparation: select shale core samples, clean, dry and cut them, and prepare them into standard specimens; S2. Mechanical parameter test: Perform uniaxial mechanical test on the standard specimen using a mechanical experimental device, and obtain basic mechanical parameters of the standard specimen through preset formulas in a computer-controlled device, wherein the basic mechanical parameters include compressive strength and stress-strain curve; S3. Failure morphology analysis: Based on the stress-strain curve, analyze the stress rising rate before the peak value of the curve and the stress falling rate from the peak value to the residual point during the failure process; S4. Stress failure brittleness evaluation: Based on the strain characteristics of the pre-peak, post-peak and peak points, the stress failure brittleness index of each standard specimen is calculated using a preset formula; S5. Heterogeneity analysis: Calculate the heterogeneity of each standard specimen using a preset formula and statistically analyze the heterogeneity probability distribution; S6. Heterogeneity brittleness evaluation: Based on the heterogeneity probability distribution and the preset brittleness evaluation standard, the heterogeneity brittleness index of each standard specimen is calculated using the preset formula; S7. Based on shale failure morphology analysis and heterogeneity analysis, the shale brittleness index is comprehensively calculated.
2. The shale brittleness evaluation method based on mechanical failure and heterogeneity according to claim 1 is characterized in that: S1 specifically includes: selecting shale core samples, cleaning, drying and cutting them to prepare standard specimens; conducting physical property tests on the prepared standard specimens, including density tests, porosity tests and permeability tests; based on the physical property test results, randomly selecting a number of standard specimens for mechanical parameter tests.
3. The shale brittleness evaluation method based on mechanical failure and heterogeneity according to claim 1 is characterized in that: In S2, a uniaxial mechanical test is performed on the standard specimen using a mechanical experimental device. The specific operations include: placing the prepared standard specimen in the mechanical experimental device; using a computer control device to control the mechanical experimental device to perform a mechanical experiment on the standard specimen, and describing the experimental mechanical properties and calculating the corresponding mechanical parameters.
4. The shale brittleness evaluation method based on mechanical failure and heterogeneity according to claim 1 is characterized in that: The brittleness index calculation formula is: BI1=(σ c -s t ) / s c ; BI2=B i1 ·B i2 ·B i3 BI=(BI1+BI2) / 2 Among them, BI1 is the heterogeneous brittleness index, σ c is the compressive strength, σ t is the tensile strength; BI2 is the stress fracture brittleness index, B i1 is the pre-peak brittleness index, B i2 is the post-peak brittleness index, B i3 is the strain control coefficient; BI is the brittleness index.
5. The shale brittleness evaluation method based on mechanical failure and heterogeneity according to claim 1 is characterized in that: When the brittleness index BI≥0.5, the shale is brittle; when 0.3≤BI<0.5, the shale is semi-brittle; when BI<0.3, the shale is non-brittle.
6. The shale brittleness evaluation method based on mechanical failure and heterogeneity according to claim 4 is characterized in that: The method further comprises: modifying the brittleness index BI according to the mineral composition, pore size and number of micro cracks of the shale.
7. The shale brittleness evaluation method based on mechanical failure and heterogeneity according to claim 6 is characterized in that: The first correction of the calculated brittleness index BI by the pore size includes: Set the pore size of the standard specimen to T, pre-set the first pore size t1, the second pore size t2, the third pore size t3, the fourth pore size t4 and the fifth pore size t5, preset the first brittleness index adjustment coefficient x1, the second first brittleness index adjustment coefficient x2, the third first brittleness index adjustment coefficient x3, the fourth first brittleness index adjustment coefficient x4 and the fifth first brittleness index adjustment coefficient x5, and t1<t2<t3<t4<t5, 0.9<x1<x2<x3<x4<x5<1.1; obtain the calculated brittleness index BI; and determine the first brittleness index adjustment coefficient of the brittleness index BI according to the size relationship between the pore size T of the standard specimen and the pre-set pore sizes ti, i=1, 2, 3, 4, 5, and make a first correction to the brittleness index BI; When T≤t1, the first brittleness index adjustment coefficient is determined as the first first brittleness index adjustment coefficient x1, and the brittleness index after the first adjustment is BI*x1; When t1<T≤t2, the first brittleness index adjustment coefficient is determined as the second first brittleness index adjustment coefficient x2, and the brittleness index after the first adjustment is BI*x2; When t2<T≤t3, the first brittleness index adjustment coefficient is determined as the third first brittleness index adjustment coefficient x3, and the brittleness index after the first adjustment is BI*x3; When t3<T≤t4, the first brittleness index adjustment coefficient is determined as the fourth first brittleness index adjustment coefficient x4, and the brittleness index after the first adjustment is BI*x4; When t4<T≤t5, the first brittleness index adjustment coefficient is determined as the fifth first brittleness index adjustment coefficient x5, and the brittleness index after the first adjustment is BI*x5.
8. The shale brittleness evaluation method based on mechanical failure and heterogeneity according to claim 7 is characterized in that: The calculated brittleness index BI is corrected twice by the number of micro cracks, including: The number of micro cracks of the standard specimen is set as U, the first number of micro cracks u1, the second number of micro cracks u2, the third number of micro cracks u3, the fourth number of micro cracks u4 and the fifth number of micro cracks u5 are preset, the first final brittle index adjustment coefficient y1, the second final brittle index adjustment coefficient y2, the third final brittle index adjustment coefficient y3, the fourth final brittle index adjustment coefficient y4 and the fifth final brittle index adjustment coefficient y5 are preset, and u1<u2<u3<u4<u5, 0.9<y1<y2<y3<y4<y5<1.1; the brittle index BI*xi after the first adjustment is obtained; and according to the relationship between the number of micro cracks U of the standard specimen and the preset number of micro cracks ui, i=1, 2, 3, 4, 5, the final brittle index adjustment coefficient of the brittle index BI is determined, and the brittle index BI is corrected twice; When U≤u1, the final brittleness index adjustment coefficient is determined as the first final brittleness index adjustment coefficient y1, and the final adjusted brittleness index is BI*xi*y1; When u1<U≤u2, the final brittleness index adjustment coefficient is determined as the second final brittleness index adjustment coefficient y2, and the final adjusted brittleness index is BI*xi*y2; When u2<U≤u3, the final brittleness index adjustment coefficient is determined as the third final brittleness index adjustment coefficient y3, and the final adjusted brittleness index is BI*xi*y3; When u3<U≤u4, the final brittleness index adjustment coefficient is determined as the fourth final brittleness index adjustment coefficient y4, and the final adjusted brittleness index is BI*xi*y4; When u4<U≤u5, the final brittleness index adjustment coefficient is determined as the fifth final brittleness index adjustment coefficient y5, and the final adjusted brittleness index is BI*xi*y5.
9. A shale brittleness evaluation device based on mechanical failure and heterogeneity, used to implement the shale brittleness evaluation method based on mechanical failure and heterogeneity as claimed in any one of claims 1 to 8, characterized in that: The device comprises: A mechanical experimental device, comprising an experimental mechanical shell, an experimental platform, a specimen holder, a high-strength casing, a pressure column and a stress strain gauge, wherein a cap is fixedly installed inside the experimental mechanical shell, a base is fixedly installed on the top of the cap, the experimental platform is fixedly installed on the base, the specimen holder is installed on the experimental platform, the high-strength casing is installed in the middle of the specimen holder, the specimen holder is used to fix the high-strength casing on the experimental platform, the pressure column is arranged on both sides and the upper side of the high-strength casing, and the stress strain gauge is fixedly installed on both sides of the high-strength casing; An experimental auxiliary device, the experimental auxiliary device comprises a gas tank, an oil tank and a liquid tank, the gas tank, the oil tank and the liquid tank are connected to the mechanical experimental device through a connecting pipeline, a peristaltic pump is arranged on the connecting pipeline, and the gas tank, the oil tank and the liquid tank are connected to the connecting pipeline through an inlet steel pipe; The control device comprises a computer display, a main switch, an integrated control pipeline and a computer host; the main switch is connected to an oil inlet controller, a liquid inlet controller and an air inlet controller, the computer host comprises a computer memory, a computer CPU and a computer graphics card, the computer host is connected to a stress strain gauge via a connecting pipeline and an integrated control pipeline, and the stress strain gauge is used to transmit basic mechanical parameters to the computer host via the connecting pipeline and the integrated control pipeline.
10. The shale brittleness evaluation device based on mechanical failure and heterogeneity according to claim 9, characterized in that: The pressure column comprises a gas, liquid and oil inlet pipe, a primary telescopic pipe, a secondary telescopic pipe, a primary force transmission pipe, a secondary force transmission pipe and a pressure plate; The gas, liquid and oil inlet pipe is installed inside the bottom of the pressure column, the secondary telescopic tube is sleeved in the primary telescopic tube, the primary telescopic tube is outerly provided with a pressure rod sleeve, the pressure rod sleeve is connected to the bottom of the pressure column, the primary force transmission tube is outerly provided with a rubber hose sleeve, one side of the rubber hose sleeve is connected to the pressure rod sleeve, and the other side of the rubber hose sleeve is connected to the secondary force transmission tube, and the secondary force transmission tube is connected to the pressure plate through a soft pad.