A soil conditioner and preparation method thereof

By combining biodegradable calcium silicate nanocomposites with modified hydroxyl oxides, a soil modification agent that can adsorb heavy metals and fix organic matter is prepared, which solves the problems of reducing nutrient absorption and heavy metal accumulation in acidic soils, and realizes the The soil pH adjustment and continuous improvement effect are achieved, and the service life of the modification agent is extended.

CN118546684BActive Publication Date: 2024-11-01SHANDONG LINRAN AGRI TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411027352.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-30
Publication Date
2024-11-01
Estimated Expiration
2044-07-30

AI Technical Summary

Technical Problem

Acid soil causes plants to absorb nutrients less, accumulate heavy metals and inhibit the growth of harmful substances. The existing modified agents are used in large quantities and need to be frequently applied, making it difficult to stabilize the soil properties in the long term.

Method used

Porous hydrated calcium silicate nanocomposites are combined with modified hydroxyl iron oxide to prepare porous hydrated calcium silicate and magnetic Fe3O4 microspheres through dynamic hydrothermal synthesis, combined with polylactic acid-hydroxyglycolic acid copolymer to form a sustained release Soil Improver, adsorb heavy metals and fixed organic matter.

Benefits of technology

Effectively adjust the soil pH value, reduce heavy metal pollution, extend the improvement effect, prevent the loss of organic matter, improve the crop growth environment, and reduce the need for frequent additions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
Patent Text Reader

Abstract

The present invention belongs to the technical field of soil improvement, and specifically relates to a soil conditioner and a preparation method thereof. The soil conditioner comprises the following components: 40-50 parts of biodegradable calcium silicate nanocomposite material, 30-40 parts of modified ferric hydroxide oxide, 5-10 parts of calcium magnesium phosphate fertilizer, and 10-15 parts of composite bacterial agent. The soil conditioner in the present invention utilizes porous hydrated calcium silicate with high porosity and calcium dissolving and alkali supplying performance, which can neutralize H in the soil. + and provide basic ions Ca to the soil 2+ , the purpose of regulating the pH value of the soil is achieved, and the calcium silicate nanocomposite material is compounded with the polylactic acid-glycolic acid copolymer. The polylactic acid-glycolic acid copolymer material is slowly degraded, and the calcium silicate nanocomposite material is slowly released into the soil, thereby achieving the effect of continuously improving the soil. The improvement effect is better and the continuous action time is longer, and there is no need to frequently add soil conditioners to the soil.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of soil improvement, and in particular relates to a soil improver and a preparation method thereof. Background Art

[0002] In recent years, with the increase in farming intensity and the extensive use of chemical fertilizers, the pH value of cultivated soil has shown an overall downward trend, making the soil acidic. When crops are planted in acidic soil, the permeability of the plasma membrane in some plants will be destroyed, reducing the absorption of elements such as calcium, magnesium, and potassium by crops, and reducing the effectiveness of phosphorus in the soil; at the same time, the activity of harmful heavy metal ions in the soil will increase significantly under acidic conditions, which can easily cause heavy metal accumulation in plants, and aluminum and iron toxicity in the soil will also inhibit crop growth.

[0003] The invention patent with application number CN202210944882.1 discloses an acidic soil conditioner and its preparation method and application, including the following components: slaked lime, biochar, amphoteric indicator particles, montmorillonite powder and water-retaining particles. The above acidic soil conditioner is used in large quantities, and it is necessary to apply the conditioner to the soil repeatedly for a long time to completely modify the soil. Summary of the invention

[0004] The object of the present invention is to provide a soil conditioner and a preparation method thereof to solve the problems raised in the above background technology.

[0005] In order to achieve the above technical objectives, the technical solution of the present invention is:

[0006] A soil conditioner comprises the following components by weight: 40-50 parts of biodegradable calcium silicate nanocomposite material, 30-40 parts of modified ferric oxyhydroxide, 5-10 parts of calcium magnesium phosphate fertilizer and 10-15 parts of composite bacterial agent.

[0007] As an improvement, the composite bacterial agent includes Microbacterium and Bacillus amyloliquefaciens, and the volume ratio of Microbacterium to Bacillus amyloliquefaciens is 1:1.2-1.5.

[0008] The present invention also provides a method for preparing a soil conditioner, comprising the following steps:

[0009] S1. Preparation of calcium silicate nanocomposite materials

[0010] Monodisperse superparamagnetic Fe3O4 microspheres are prepared by a hydrothermal synthesis method, and then the monodisperse superparamagnetic Fe3O4 microspheres, white carbon black, CaO and water are prepared into a mixed slurry, which is added into a reactor after ultrasonic mixing, with a solid-liquid mass ratio of 1:30, and the temperature is raised to 170°C while stirring, and then a hydrothermal synthesis reaction is carried out at a constant temperature and speed of 90r / min for 7h under the condition of 170°C, and after the reaction is completed, the mixture is naturally cooled to room temperature, the slurry is taken out, and magnetic separation is carried out to obtain a suspension, and the suspension is vacuum dried at 70°C to obtain a calcium silicate nanocomposite material;

[0011] S2. Preparation of biodegradable calcium silicate nanocomposite materials

[0012] Weigh 10 g of polylactic acid-glycolic acid copolymer, add it to a beaker containing 30 mL of dichloromethane, seal the beaker with a sealing film, stir for 30 min at 400 r / min using a magnetic stirrer to completely dissolve the polylactic acid-glycolic acid copolymer to form a polylactic acid-glycolic acid copolymer sol, weigh 10 g of the calcium silicate nanocomposite material, slowly add it to the polylactic acid-glycolic acid copolymer sol, mechanically stir for 2 h at 400 r / min, then place the beaker in a vacuum drying oven, and vacuum dry it at 65° C. overnight to obtain a biodegradable calcium silicate nanocomposite material;

[0013] S3. Preparation of modified iron oxyhydroxide

[0014] The ferrous sulfate is rapidly oxidized in hydrogen peroxide to obtain an iron salt precursor, and then the iron salt precursor is dispersed in 100 mL of deionized water in which hexadecyldimethylbenzyl ammonium chloride is pre-dissolved, and fully stirred to be completely dissolved, and then 10 mL of a 5 mol / L sodium hydroxide solution is added, and 20 mL of 30% hydrogen peroxide is added while stirring to produce a precipitate, and then the precipitate is washed three times with deionized water, and the precipitate is freeze-dried to form a modified oxyhydroxy iron;

[0015] S4. Preparation of soil conditioner

[0016] Add biodegradable calcium silicate nanocomposite materials, modified ferric hydroxide oxide and calcium magnesium phosphate fertilizer into a stirring tank, then heat up to 85°C, stir at 85°C for 1 hour, then cool to room temperature, add composite bacterial agent into the stirring tank, and continue stirring for 1 hour to form a soil conditioner.

[0017] As a further improvement, in step S1, the monodisperse superparamagnetic Fe3O4 microspheres are prepared by the following steps:

[0018] S11, 0.72g urea, 2.4g sodium citrate dihydrate, 0.216g ferric chloride hexahydrate, 0.36g ferrous chloride tetrahydrate and 80mL deionized water were added to a reactor, magnetically stirred to completely dissolve them, and then 0.6g sodium polyacrylate was added to the reactor, and stirring was continued to mix the solution completely;

[0019] S12. Heat the reactor to 180°C and react for 4 hours. After the reaction is completed, wash the reaction product three times with deionized water, and then separate the reaction product by magnetic separation to obtain a suspension. Vacuum dry the suspension at 60°C for 24 hours to obtain monodisperse superparamagnetic Fe3O4 microspheres.

[0020] As a further improvement, in step S1, the reactor is heated to 170°C at a heating rate of 2-3°C / min, and the stirring rate during the heating process is 300r / min.

[0021] As a further improvement, in step S1, in the mixed slurry, the molar ratio of monodisperse superparamagnetic Fe3O4 microspheres, white carbon black and CaO is 1:5:11.

[0022] As a further improvement, in step S3, the molar ratio of the iron salt precursor to hexadecyldimethylbenzylammonium chloride is 50:1.

[0023] Due to the adoption of the above technical solution, the beneficial effects of the present invention are:

[0024] The present invention provides a soil conditioner, wherein the biodegradable calcium silicate nanocomposite material is prepared by a dynamic hydrothermal synthesis method to deposit CaO and white carbon black into porous hydrated calcium silicate, and then coated on the surface of Fe3O4. The porous hydrated calcium silicate has a high porosity and calcium dissolving and alkali supplying performance, and can neutralize H in the soil. + and provide basic ions Ca to the soil 2+ , to achieve the purpose of regulating the pH value of the soil.

[0025] However, porous calcium silicate hydrate is prone to cause the risk of heavy metal pollution in the soil when used as an acidic soil conditioner to adjust the soil pH value. The present invention adsorbs heavy metal ions in the soil through the magnetic adsorption effect of Fe3O4 in the biodegradable calcium silicate nanocomposite material, and covers the porous calcium silicate hydrate on the surface of Fe3O4. After the porous calcium silicate hydrate is slowly decomposed in the soil, the internal Fe3O4 is slowly released into the soil to adsorb the heavy metal ions in the soil, so as to prevent the heavy metal pollution of the soil caused by the porous calcium silicate hydrate.

[0026] In the present invention, the prepared calcium silicate nanocomposite material is compounded with a polylactic acid-glycolic acid copolymer. After the soil improver enters the soil, the polylactic acid-glycolic acid copolymer material is slowly degraded within a certain period of time, and the calcium silicate nanocomposite material is slowly released into the soil, so as to achieve the effect of continuously improving the soil, with better improvement effect and longer continuous action time, and it is unnecessary to frequently add the soil improver into the soil.

[0027] In the present invention, the use of porous hydrated calcium silicate will cause the loss of organic matter in the soil, resulting in a low organic matter content in the soil. By adding modified oxyhydroxide iron, the hydroxyl groups in the modified oxyhydroxide iron and the carboxyl groups or hydroxyoxime groups in the organic molecules in the soil undergo a rapid ligand exchange reaction to form a "metal-CO" polar covalent bond, thereby fixing the organic matter in the soil in the soil, preventing the loss of organic matter in the soil, and facilitating the growth of crops. DETAILED DESCRIPTION

[0028] The technical scheme of the present invention will be clearly and completely described below in conjunction with specific embodiments, but it will be appreciated by those skilled in the art that the following described embodiments are part of embodiments of the present invention, rather than all embodiments, and are only used to illustrate the present invention, and should not be considered as limiting the scope of the present invention. Based on the embodiments in the present invention, all other embodiments obtained by those of ordinary skill in the art without making creative work, all belong to the scope of protection of the present invention. If specific conditions are not indicated in the embodiments, they are carried out according to normal conditions or conditions recommended by the manufacturer. If the manufacturer is not indicated in the reagents or instruments used, they are all conventional products that can be purchased commercially. Example 1

[0029] A soil conditioner comprises the following components, measured by weight: 40 parts of biodegradable calcium silicate nanocomposite material, 30 parts of modified ferric oxyhydroxide, 5 parts of calcium magnesium phosphate fertilizer, and 10 parts of composite bacterial agent, wherein the composite bacterial agent contains two microorganisms, namely, Microbacterium and Bacillus amyloliquefaciens, and the volume ratio of Microbacterium to Bacillus amyloliquefaciens is 1:1.2. Example 2

[0030] A soil conditioner comprises the following components by weight: 50 parts of biodegradable calcium silicate nanocomposite material, 40 parts of modified ferric oxyhydroxide, 10 parts of calcium magnesium phosphate fertilizer, and 15 parts of composite bacterial agent, wherein the composite bacterial agent contains two microorganisms, namely, Microbacterium and Bacillus amyloliquefaciens, and the volume ratio of Microbacterium to Bacillus amyloliquefaciens is 1:1.5. Example 3

[0031] A soil conditioner comprises the following components, measured by weight: 45 parts of biodegradable calcium silicate nanocomposite material, 35 parts of modified ferric oxyhydroxide, 8 parts of calcium magnesium phosphate fertilizer, and 12 parts of composite bacterial agent, wherein the composite bacterial agent contains two microorganisms, namely, Microbacterium and Bacillus amyloliquefaciens, and the volume ratio of Microbacterium to Bacillus amyloliquefaciens is 1:1.3. Example 4

[0032] The preparation of biodegradable calcium silicate nanocomposite material comprises the following steps:

[0033] S1. Preparation of monodisperse superparamagnetic Fe3O4 microspheres

[0034] 0.72g urea, 2.4g sodium citrate dihydrate, 0.216g ferric chloride hexahydrate, 0.36g ferrous chloride tetrahydrate and 80mL deionized water were added to a reactor, and magnetic stirring was performed to completely dissolve them. Then, 0.6g sodium polyacrylate was added to the reactor, and stirring was continued to mix the solution completely. Then, the reactor was heated to 180°C and reacted for 4h. After the reaction was completed, the reaction product was washed 3 times with deionized water, and then the reaction product was separated by magnetic separation to obtain a suspension. The suspension was vacuum dried in a vacuum drying oven at 60°C for 24h to obtain monodisperse superparamagnetic Fe3O4 microspheres.

[0035] S2. Preparation of calcium silicate nanocomposite materials

[0036] Monodisperse superparamagnetic Fe3O4 microspheres, white carbon black, CaO and water are prepared into a mixed slurry, and then ultrasonically mixed and added into a reactor, wherein the molar ratio of the monodisperse superparamagnetic Fe3O4 microspheres, white carbon black and CaO is 1:5:11, and the solid-liquid mass ratio is 1:30. The mixture is heated to 170°C at a heating rate of 2-3°C / min at a stirring rate of 300 r / min, and then a hydrothermal synthesis reaction is carried out at a constant temperature and speed of 90 r / min for 7 hours at 170°C. After the reaction is completed, the mixture is naturally cooled to room temperature, the slurry is taken out, and magnetic separation is carried out to obtain a suspension, and the suspension is vacuum dried at 70°C to obtain a calcium silicate nanocomposite material;

[0037] S3. Preparation of biodegradable calcium silicate nanocomposite materials

[0038] Weigh 10 g of polylactic acid-glycolic acid copolymer, add it to a beaker filled with 30 mL of dichloromethane, seal the beaker with a sealing film, and stir it with a magnetic stirrer at 400 r / min for 30 min to completely dissolve the polylactic acid-glycolic acid copolymer to form a polylactic acid-glycolic acid copolymer sol. Weigh 10 g of calcium silicate nanocomposite material, slowly add it to the polylactic acid-glycolic acid copolymer sol, mechanically stir it at 400 r / min for 2 h, and then place the beaker in a vacuum drying oven and vacuum dry it at 65°C overnight to obtain a biodegradable calcium silicate nanocomposite material. Example 5

[0039] The preparation of modified iron oxyhydroxide specifically comprises the following steps:

[0040] Weigh 0.56 kg of ferrous sulfate and add it to 30 mL of 30% hydrogen peroxide for rapid oxidation to obtain an iron salt precursor, and then disperse the iron salt precursor in 100 mL of deionized water in which hexadecyldimethylbenzylammonium chloride has been pre-dissolved, wherein the molar ratio of the iron salt precursor to hexadecyldimethylbenzylammonium chloride is 50:1, stir it thoroughly to make it completely dissolved, and then add 10 ml of 5 mol / L sodium hydroxide solution, and add 20 mL of 30% hydrogen peroxide while stirring to produce a precipitate, and then wash the precipitate with deionized water 3 times, and freeze-dry the precipitate to form modified oxyhydroxy iron. Example 6

[0041] The preparation of soil conditioner comprises the following steps:

[0042] Take 40 parts of biodegradable calcium silicate nanocomposite materials, 30 parts of modified ferric hydroxide oxide and 5 parts of calcium magnesium phosphate fertilizer and add them to a stirring tank, then heat it to 85°C, stir it at 85°C for 1 hour, then cool it to room temperature, add 10 parts of composite bacterial agent to the stirring tank, and continue stirring for 1 hour to form a soil conditioner, wherein the composite bacterial agent contains Microbacterium and Bacillus amyloliquefaciens, and the volume ratio of Microbacterium to Bacillus amyloliquefaciens is 1:1.2. Example 7

[0043] The preparation of soil conditioner comprises the following steps:

[0044] Take 50 parts of biodegradable calcium silicate nanocomposite materials, 40 parts of modified ferric hydroxide oxide and 10 parts of calcium magnesium phosphate fertilizer and add them to a stirring tank, then heat it to 85°C, stir it at 85°C for 1 hour, then cool it to room temperature, add 15 parts of composite bacterial agent to the stirring tank, and continue stirring for 1 hour to form a soil conditioner, wherein the composite bacterial agent contains Microbacterium and Bacillus amyloliquefaciens, and the volume ratio of Microbacterium to Bacillus amyloliquefaciens is 1:1.5. Example 8

[0045] The preparation of soil conditioner comprises the following steps:

[0046] Take 45 parts of biodegradable calcium silicate nanocomposite materials, 35 parts of modified ferric hydroxide oxide and 8 parts of calcium magnesium phosphate fertilizer and add them to a stirring tank, then heat it to 85°C, stir it at 85°C for 1 hour, then cool it to room temperature, add 12 parts of composite bacterial agent to the stirring tank, and continue stirring for 1 hour to form a soil conditioner, wherein the composite bacterial agent contains Microbacterium and Bacillus amyloliquefaciens, and the volume ratio of Microbacterium to Bacillus amyloliquefaciens is 1:1.3. Example 9

[0047] The specific method of soil culture test of soil conditioner is as follows:

[0048] There are three treatment groups, named as group 1, group 2, and group 3, respectively. The three treatment groups respectively add the soil conditioner prepared in Example 6, Example 7, and Example 8 to improve the soil. Each treatment group is repeated 3 times and named as No. 1, No. 2, and No. 3, respectively.

[0049] For each treatment, 6.5 kg of sieved acidic soil was weighed, and different soil conditioners were added to the sieved acidic soil. The conditioners and the sieved acidic soil were fully mixed and placed in plastic pots, wherein 1.5 g of soil conditioner was added to every 1 kg of acidic soil. The plastic pots were filled with farmland irrigation water, and the depth of water in each plastic pot was kept consistent. A light-transmitting film was used to build a shed to cover it, and the pH value of the soil was measured every 15 days. The results are shown in Table 1.

[0050]

[0051] From the results of the above embodiments, it can be seen that the acidic soil conditioner of the embodiments of the present application can effectively increase the pH value of acidic soil, play a role in improving the properties of acidic soil, and the soil conditioner of the embodiments of the present application can make the pH value of the soil reach the optimal value after about 45 days of use. Example 10

[0052] The rice pot test of soil conditioner is as follows:

[0053] Test example: A total of three treatments were set up, named as group 1, group 2, and group 3, respectively. The three treatments were respectively added with the soil conditioners prepared in Example 6, Example 7, and Example 8 for soil improvement. Each treatment was repeated 3 times and named as No. 1, No. 2, and No. 3, respectively.

[0054] For each treatment, 6.5 kg of sieved acidic soil was weighed, and different soil conditioners were added to the sieved acidic soil. The conditioners and the sieved acidic soil were fully mixed and loaded into plastic pots, wherein 1.5 g of soil conditioner was added to every 1 kg of acidic soil. Rice was transplanted in each plastic pot, and farmland was irrigated with water on time according to the growth law of rice. According to the nutrient requirements of potted crops, 1.2 g of urea and 0.9 g of potassium chloride were applied to each plastic pot before rice transplanting. Seven days after rice transplanting, 0.6 g of urea and 0.6 g of potassium chloride were applied to each plastic pot. The fertilizer was applied in liquid form and mixed thoroughly with the soil.

[0055] Control example: 6.5 kg of sieved acidic soil was placed in a plastic pot, and rice was transplanted without using a soil conditioner. The same fertilization method as in the above test example was used as a control example.

[0056] Table 2 shows the data of rice yield, number of filled grains and number of effective panicles in the test example and the control example:

[0057] It can be seen from Table 2 that each treatment in the test example can increase the yield of crops, and there is no significant difference among all treatments.

[0058] The specific implementation of the present invention described above does not constitute a limitation on the protection scope of the present invention. Any other corresponding changes and modifications made based on the technical concept of the present invention should be included in the protection scope of the claims of the present invention.

Claims

1. A method for preparing a soil conditioner, characterized in that: The following steps are involved: S1. Preparation of calcium silicate nanocomposite materials Monodisperse superparamagnetic Fe3O4 microspheres are prepared by a hydrothermal synthesis method, and then the monodisperse superparamagnetic Fe3O4 microspheres, white carbon black, CaO and water are prepared into a mixed slurry, which is added into a reactor after ultrasonic mixing, with a solid-liquid mass ratio of 1:30, and the temperature is raised to 170°C while stirring, and then a hydrothermal synthesis reaction is carried out at a constant temperature and speed of 90r / min for 7h under the condition of 170°C, and after the reaction is completed, the mixture is naturally cooled to room temperature, the slurry is taken out, and magnetic separation is carried out to obtain a suspension, and the suspension is vacuum dried at 70°C to obtain a calcium silicate nanocomposite material; S2. Preparation of biodegradable calcium silicate nanocomposite materials Weigh 10 g of polylactic acid-glycolic acid copolymer, add it to a beaker containing 30 mL of dichloromethane, seal the beaker with a sealing film, stir for 30 min at 400 r / min using a magnetic stirrer to completely dissolve the polylactic acid-glycolic acid copolymer to form a polylactic acid-glycolic acid copolymer sol, weigh 10 g of the calcium silicate nanocomposite material, slowly add it to the polylactic acid-glycolic acid copolymer sol, mechanically stir for 2 h at 400 r / min, then place the beaker in a vacuum drying oven, and vacuum dry it at 65° C. overnight to obtain a biodegradable calcium silicate nanocomposite material; S3. Preparation of modified iron oxyhydroxide The ferrous sulfate is rapidly oxidized in hydrogen peroxide to obtain an iron salt precursor, and then the iron salt precursor is dispersed in 100 mL of deionized water in which hexadecyldimethylbenzyl ammonium chloride is pre-dissolved, and fully stirred to be completely dissolved, and then 10 mL of a 5 mol / L sodium hydroxide solution is added, and 20 mL of 30% hydrogen peroxide is added while stirring to produce a precipitate, and then the precipitate is washed three times with deionized water, and the precipitate is freeze-dried to form a modified oxyhydroxy iron; S4. Preparation of soil conditioner Adding biodegradable calcium silicate nanocomposite, modified ferric hydroxide oxide and calcium magnesium phosphate into a stirring tank, then heating to 85°C, stirring at 85°C for 1 hour, then cooling to room temperature, adding composite bacterial agent into the stirring tank, and continuing stirring for 1 hour to form a soil conditioner; The composite bacterial agent comprises Microbacterium and Bacillus amyloliquefaciens, and the volume ratio of Microbacterium to Bacillus amyloliquefaciens is 1:1.2-1.

5.

2. The method for preparing a soil conditioner according to claim 1, characterized in that: In step S1, the monodisperse superparamagnetic Fe3O4 microspheres are prepared by the following steps: S11, 0.72g urea, 2.4g sodium citrate dihydrate, 0.216g ferric chloride hexahydrate, 0.36g ferrous chloride tetrahydrate and 80mL deionized water were added to a reactor, magnetically stirred to completely dissolve them, and then 0.6g sodium polyacrylate was added to the reactor, and stirring was continued to mix the solution completely; S12. Heat the reactor to 180°C and react for 4 hours. After the reaction is completed, wash the reaction product three times with deionized water, and then separate the reaction product by magnetic separation to obtain a suspension. Vacuum dry the suspension at 60°C for 24 hours to obtain monodisperse superparamagnetic Fe3O4 microspheres.

3. The method for preparing the soil conditioner according to claim 1, characterized in that: In step S1, the reactor is heated to 170°C at a heating rate of 2-3°C / min, and the stirring rate during the heating process is 300r / min.

4. The method for preparing a soil conditioner according to claim 1, characterized in that: In step S1, in the mixed slurry, the molar ratio of monodisperse superparamagnetic Fe3O4 microspheres, white carbon black and CaO is 1:5:

11.

5. The method for preparing the soil conditioner according to claim 1, characterized in that: In step S3, the molar ratio of the iron salt precursor to hexadecyldimethylbenzylammonium chloride is 50:

1.

6. The soil conditioner obtained by the method for preparing the soil conditioner according to any one of claims 1 to 5, characterized in that: The composition comprises the following components by weight: 40-50 parts of biodegradable calcium silicate nanocomposite material, 30-40 parts of modified oxyhydroxide iron, 5-10 parts of calcium magnesium phosphate fertilizer and 10-15 parts of composite bacterial agent.