Methods to improve tire performance
Collect data from vehicle sensors and establish a belt width analysis model. Combined with the constraint range and historical damage information, the belt design is adjusted, which solves the problem of the belt differential design range being too large in the existing technology and significantly improves tire performance. of durability and safety.
Patent Information
- Application Number
- CN202411081295.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-08
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2044-08-08
AI Technical Summary
When the existing technology improves the durability of tires, the differential design range of the belt layer is too large, resulting in uneven stress on the tread, affecting the handling and safety, and there is a lack of targeted design for the end-point damage of different belt layers, resulting in the design Chaos and insufficient durability boost.
Collect tire parameters and historical status information through vehicle sensors, analyze and determine the end point difference and width ratio of each belt layer, establish a belt width analysis model, and adjust the belt width design based on the constraint range and historical damage information to ensure the target Durability and safety.
It significantly improves the durability and damage resistance of the tire, ensures the accuracy and pertinence of the belt design, and extends the service life of the tire.
Smart Images

Figure CN118596749B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of tires, and in particular to a method for improving tire performance. Background Art
[0002] The belt layer is the main load-bearing component of the tire, and its endpoints are the parts of the crown that are most susceptible to fatigue damage. Problems such as shoulder hollows and shoulder cracks and rubber aging are prone to occur, which directly affects the durability of the tire and shortens its service life.
[0003] At present, relevant technologies have proposed that the high temperature resistance of tires can be improved by increasing the range of belt ply differentials. However, the belt ply differential design range of this scheme is too large, which will cause uneven force and stress concentration on the tread when the tire is running at high speed, affecting the handling and safety of the tire. In addition, the tire durability can be improved by increasing the belt ply differential design requirements by limiting the ratio standard of the belt ply to the running surface width. However, since there is no unified design standard for the tire running surface width, the belt ply differential design standard of this method is unclear, which leads to design confusion and cannot effectively improve the tire durability. Summary of the invention
[0004] In view of this, an object of the present invention is to provide a tire performance improvement method, which can significantly improve tire performance.
[0005] In a first aspect, an embodiment of the present invention provides a method for improving tire performance, the method comprising: collecting tire parameter information and tire historical status information of multiple tires through a vehicle sensor set, wherein the tire parameter information comprises: tire section width information and belt width information, and the tire historical status information comprises: belt temperature information, contact area information, average contact pressure information and maximum tire body tension information; performing data analysis and processing on the tire parameter information and tire historical status information to determine the endpoint difference between each belt layer, the width ratio corresponding to each belt layer and the durability time corresponding to each tire; obtaining a standard section width set of the tire The target end point difference range and the target width ratio range of the tires of various standard section widths when the maximum endurance time is reached are determined according to the endurance time, the end point difference range and the width ratio; the standard section width set, and the corresponding target end point difference range and the target width ratio range are input into a preset classifier to perform classification training on the preset classifier to determine a belt width analysis model, wherein the belt width analysis model is used to match the corresponding target width range values of the first belt layer, the second belt layer, the third belt layer and the zeroth belt layer according to the section width of the tire, so as to improve the durability of the tire set according to the target width range value.
[0006] In one embodiment, data analysis and processing are performed on tire parameter information and tire historical status information to determine the endpoint difference between each belt layer, the width ratio corresponding to each belt layer, and the durability time corresponding to each tire, including: determining the endpoint difference between each belt layer based on the belt layer width information, and determining the width ratio corresponding to each belt layer based on the tire section width information and the belt layer width information; and performing durability prediction processing on the tire historical status information through a preset parameter analysis model to determine the durability time corresponding to the tire.
[0007] In one embodiment, the step of determining the endpoint difference between each belt layer based on the belt layer width information includes: determining the difference between half of the width of the first belt layer and half of the width of the zeroth belt layer as the first endpoint difference; and determining the difference between half of the width of the second belt layer and half of the width of the zeroth belt layer as the second endpoint difference.
[0008] In one embodiment, the step of determining the width ratio corresponding to each belt layer according to the tire section width information and the belt layer width information includes: dividing the widths of the first belt layer, the second belt layer, the third belt layer and the zeroth belt layer by the standard section width, respectively, to determine the first width ratio, the second width ratio, the third width ratio and the zeroth width ratio.
[0009] In one embodiment, before the step of determining the target endpoint difference range and target width ratio range for tires of various standard section widths when the maximum endurance time is reached, it also includes: obtaining historical damage information of the tire, wherein the historical damage information includes: the specific damage location of the tire belt layer; matching the corresponding constraint range from a preset database based on the historical damage information, so as to combine the constraint range with the endurance time, the endpoint difference and the width ratio, and determine the target endpoint difference range and the target width ratio range, wherein the constraint range is the endpoint difference constraint range of the first endpoint difference and the second endpoint difference.
[0010] In the second aspect, an embodiment of the present invention further provides a tire, comprising: a tire body and a tire tread, the tire tread comprising: a crown rubber and a belt layer; wherein the crown rubber comprises: a cap rubber and a base rubber, the cap rubber is arranged on the outer surface of the base rubber, the cap rubber is natural rubber or synthetic rubber, and the base rubber is also natural rubber or synthetic rubber; the belt layer is arranged between the tire body and the base rubber, the belt layer is composed of steel wire or nylon combined with rubber, and the belt layer is used to improve the durability and damage resistance of the tire.
[0011] In one embodiment, the belt layer includes: a second belt layer and a third belt layer, and the third belt layer is arranged on the outer surface of the second belt layer; wherein the second belt layer and the third belt layer are working layers for improving the durability and damage resistance of the tire.
[0012] In one embodiment, the belt layer further includes: a first belt layer; wherein the first belt layer is disposed between the tire body and the working layer, and the first belt layer is a transition layer.
[0013] In one embodiment, the belt layer further includes: a zeroth belt layer; wherein the zeroth belt layer is used to be wound along the circumference of the tire by S-type winding to closely fit the first belt layer, the second belt layer, the third belt layer and the tire body.
[0014] The embodiments of the present invention bring the following beneficial effects:
[0015] A tire performance improvement method provided by an embodiment of the present invention can collect tire parameter information and tire historical status information of multiple tires through a vehicle sensor set, and perform data analysis and processing on the tire parameter information and tire historical status information to determine the endpoint difference between each belt layer, the width ratio corresponding to each belt layer and the durability time corresponding to each tire, and then obtain a standard section width set of tires, and determine the target endpoint difference range and target width ratio range of tires of various standard section widths when the maximum durability time is reached based on the durability time, endpoint difference and width ratio, and finally input the standard section width set and the corresponding target endpoint difference range and target width ratio range into a preset classifier to perform classification training on the preset classifier and determine the belt layer width analysis model. The embodiment of the present invention can significantly improve the durability of tires.
[0016] Other features and advantages of the present invention will be described in the following description, and partly become apparent from the description, or understood by practicing the present invention. The purpose and other advantages of the present invention are realized and obtained by the structures particularly pointed out in the description, claims and drawings.
[0017] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, preferred embodiments are given below and described in detail with reference to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] In order to more clearly illustrate the specific implementation methods of the present invention or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0019] Figure 1 A schematic diagram of a process for improving tire performance provided by an embodiment of the present invention;
[0020] Figure 2A schematic structural diagram of a half section of a tire provided by an embodiment of the present invention;
[0021] Figure 3 A schematic diagram of a zero-degree winding structure of a zero-belt layer provided by an embodiment of the present invention;
[0022] Figure 4 A schematic diagram of the structure of an S-shaped winding of a zeroth belt layer provided in an embodiment of the present invention. DETAILED DESCRIPTION
[0023] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution of the present invention will be clearly and completely described in combination with the embodiments below. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0024] At present, the belt layer is the main force-bearing component of the tire, and its end point is the part of the crown that is most susceptible to fatigue damage. It is easy to have problems such as shoulder hollow and shoulder cracking due to rubber aging, which directly affects the durability of the tire and shortens the service life of the tire. Therefore, how to improve the durability of the tire and extend its service life is a problem that has been studied in the field of tire manufacturing technology. The relevant technology proposes that the high temperature resistance of the tire can be improved by increasing the range of the belt layer difference. However, the belt layer difference design range of this scheme is too large, which will cause uneven force and stress concentration on the tread when the tire is running at high speed, and the handling and safety of the tire are affected. In addition, the belt layer difference design requirements can be increased by limiting the ratio standard of the belt layer to the driving surface width, thereby improving the durability of the tire. However, since there is no unified design standard for the driving surface width of the tire, the belt layer difference standard designed by this method is unclear, which leads to design confusion and cannot effectively improve the durability of the tire. In addition, the existing technical scheme is only designed for the cause of the end point damage of a certain belt layer, and there is a lack of targeted design schemes for tire damage caused by the end point damage of different belt layers.
[0025] Based on this, the tire performance improvement method provided by the implementation of the present invention can jointly constrain the belt width through the endpoint difference, width ratio and constraint range, thereby improving the accuracy of the target width range value of the belt layers at each level, and using the belt width analysis model, various causes of belt endpoint damage can be comprehensively considered to obtain the design scheme with the highest tire durability. In addition, the design scheme can also be targetedly adjusted according to the tire's operating conditions, model, purpose and historical damage feedback, etc.
[0026] See also Figure 1The schematic diagram of a process of improving tire performance is shown, and the method mainly includes the following steps S102 to S108:
[0027] Step S102, collecting tire parameter information and tire historical status information of multiple tires through a vehicle sensor set, wherein the tire parameter information includes: tire section width information and belt width information, and the tire historical status information includes: belt temperature information, contact area information, average contact pressure information and maximum tire body tension information.
[0028] Step S104, performing data analysis and processing on the tire parameter information and the tire historical status information to determine the endpoint difference between each belt layer, the width ratio corresponding to each belt layer and the durability time corresponding to each tire. In one embodiment, for tires for special purposes, such as racing tires and other tires that need to withstand high temperatures, the weight of the belt layer temperature can be increased when analyzing the durability time.
[0029] Step S106, obtaining a set of standard section widths of the tire, and determining a target endpoint difference range and a target width ratio range for tires of various standard section widths when the maximum endurance time is reached based on the endurance time, endpoint difference and width ratio. In one embodiment, since the reason why a specific layer in each belt layer is more easily damaged is related to the operating conditions, model and use of the tire, additional weighting coefficients can be set when constructing the belt layer width analysis model based on the operating conditions or specification uses corresponding to the belt layers that are prone to damage as reported in the market, so as to make targeted adjustments to the belt layer width.
[0030] Step S108, input the standard section width set, and the corresponding target endpoint difference range and target width ratio range into a preset classifier to perform classification training on the preset classifier and determine the belt width analysis model, wherein the belt width analysis model is used to match the corresponding target width range values of the first belt layer, the second belt layer, the third belt layer and the zeroth belt layer according to the section width of the tire, so as to improve the durability of the tire set according to the target width range value. In one embodiment, in the tire, there is also a fixed limiting relationship between the first belt layer, the second belt layer, the third belt layer and the zeroth belt layer, that is, the second belt layer width is greater than the first belt layer width, the first belt layer width is greater than the third belt layer width, the third belt layer width is greater than or equal to the zeroth belt layer width, and the belt layer widths are all less than the tire section width, and this limiting relationship is also a basic constraint condition for model training.
[0031] The tire performance improvement method provided by the embodiment of the present invention can significantly improve the durability of the tire.
[0032] The embodiment of the present invention also provides an implementation method for performing data analysis and processing on tire parameter information and tire historical status information to determine the endpoint difference between each belt layer, the width ratio corresponding to each belt layer, and the durability time corresponding to each tire. For details, see (1) to (3) below:
[0033] (1) According to the belt layer width information, the endpoint difference between each belt layer is determined. Specifically, the difference between half the width of the first belt layer and half the width of the zeroth belt layer is determined as the first endpoint difference, and the difference between half the width of the second belt layer and half the width of the zeroth belt layer is determined as the second endpoint difference. In one embodiment, the endpoint difference between belt layer 0 and belt layer 1 is Δ1, the endpoint difference between belt layer 0 and belt layer 2 is Δ2, the endpoint temperature of belt layer 1 is T1, the endpoint temperature of belt layer 2 is T2, and the endpoint temperature of belt layer 0 is T0. When the endpoint difference between belt layer 0 and belt layer 1 Δ1 and the endpoint difference between belt layer 2 Δ2 are designed based on the cross-sectional width w, they can be set to 7mm<Δ1<15mm, and 7mm<Δ2<15mm.
[0034] (2) Determine the width ratio of each belt layer according to the tire section width information and the belt layer width information. Specifically, divide the widths of the first belt layer, the second belt layer, the third belt layer and the zeroth belt layer by the standard section width to determine the first width ratio, the second width ratio, the third width ratio and the zeroth width ratio. In one embodiment, assuming that the width of belt layer 2 is a and the tire section width is w, then the ratio of belt layer 1 to the tire section width w is λ1, the ratio of belt layer 2 to the section width w is λ2, the ratio of belt layer 3 to the section width w is λ3, and the ratio of belt layer 0 to the section width w is λ0. λ can be set to 0.4<λ1<0.7, 0.6<λ2<0.8, 0.2<λ3<0.4, and 0.2<λ0<0.4.
[0035] (3) Through a preset parameter analysis model, durability prediction processing is performed on the tire historical status information to determine the durability time corresponding to the tire. In one embodiment, after determining the endpoint difference between each belt layer, the width ratio corresponding to each belt layer and the durability time corresponding to each tire, the historical damage information of the tire can be obtained, and the corresponding constraint range can be matched from a preset database based on the historical damage information, so that the constraint range is combined with the durability time, the endpoint difference and the width ratio to determine the target endpoint difference range and the target width ratio range, wherein the historical damage information includes: the specific damage position of the tire belt layer, the constraint range is the endpoint difference constraint range of the first endpoint difference and the second endpoint difference, specifically, for tire damage caused by endpoint damage of belt layer 1, the belt layer difference is increased, and for tire damage caused by endpoint damage of belt layer 2, the belt layer difference is reduced by Δ2, and the reduction amount is the preset belt layer difference threshold.
[0036] In practical applications, data analysis and processing are performed on the tire parameter information and tire historical status information in the aforementioned step S102 and step S104 to determine the end point difference between each belt layer, the width ratio corresponding to each belt layer, and the durability time corresponding to each tire, as shown in the following Table 1:
[0037] Table 1: Comparison table of end point difference, width ratio and tire durability time of tires under three embodiments
[0038]
[0039] Referring to Examples 1, 2, and 3 in Table 1 above, in Example 1, Δ1=7.34 mm, Δ2=7.2 mm, λ1=0.61, λ2=0.71, λ3=0.35, λ0=0.30, T1=145.9°C, T2=138.0°C, and T0=157.0°C; in Example 2, Δ1=10.02 mm, Δ2=10.02 mm, λ1=0.57, λ2=0.71, λ3=0.33, and λ0=0.30, T1=143.4℃, T2=139.3℃, T0=155.5℃; in Example 3, Δ1=13.39mm, Δ2=12.82mm, λ1=0.53, λ2=0.71, λ3=0.32, λ0=0.30, T1=141.4℃, T2=141.1℃, T0=154.8℃.
[0040] Compared with Example 1, Δ1 and Δ2 of Example 2 are increased, the ground contact area is increased, the average ground contact pressure is reduced, the rectangular coefficient is reduced, the shoulder carcass tension is increased, the restraint at the end point of belt layer 2 is reduced, the support is weakened, the heat generation caused by strain is higher, the temperature of the end point of belt layer 2 is increased, the temperature of the end point of belt layer 1 is reduced, the temperature of the end point of belt layer 0 is reduced, and the durability performance is improved by 12%.
[0041] Compared with Example 2, Δ1 and Δ2 of Example 3 are increased, the contact area is increased, the average contact pressure is reduced, and the rectangular coefficient is reduced. The shoulder carcass tension is increased, the restraint of the end point of the belt layer 2 is reduced, the support is weakened, the heat generation caused by the strain is high, the temperature of the end point of the belt layer 2 is increased, the temperature of the end point of the belt layer 1 is reduced, the temperature of the end point of the belt layer 0 is reduced, and the durability performance is improved by 10%.
[0042] Based on this, it can be concluded that increasing the belt layer difference increases the contact area, reduces the average contact pressure, and reduces the rectangular coefficient. The increase in shoulder carcass tension is beneficial to improving durability. As the belt layer difference increases, the restraint of the belt layer 2 end point decreases, the support weakens, the heat generated by strain is high, and the temperature of the belt layer 2 end point shows a gradual increase; while the temperature of the wrapping belt layer and the 1# belt layer 0 end point shows a downward trend. Therefore, when making targeted adjustments to the design plan based on the tire's operating conditions, model, purpose, and historical damage feedback, the following strategies (A) to (B) can be adopted:
[0043] (A) For tire damage caused by end point damage of belt layer 1, the belt difference level Δ1 is increased, and the increase amount is the preset belt difference level threshold.
[0044] (B) For tire damage caused by the destruction of the end point of belt layer 2, the belt layer difference level is reduced by Δ2, and the reduction amount is the preset belt layer difference level threshold.
[0045] In order to facilitate understanding of the tire performance improvement method, an embodiment of the present invention provides a schematic diagram of the structure of a tire, see FIG. Figure 2 A structural schematic diagram of a half section of a tire is shown, the tire includes: a tire body and a tire tread, the tire tread includes: a crown rubber and a belt layer; wherein the crown rubber includes: a cap rubber and a base rubber, the cap rubber is arranged on the outer surface of the base rubber, the cap rubber is natural rubber or synthetic rubber, the base rubber is also natural rubber or synthetic rubber, the belt layer is arranged between the tire body and the base rubber, the belt layer is composed of steel wire or nylon combined with rubber, and the belt layer is used to improve the durability and damage resistance of the tire.
[0046] In one embodiment, the belt layer includes: a first belt layer, a second belt layer, a third belt layer and a zeroth belt layer. The second belt layer and the third belt layer are working layers for improving the durability and damage resistance of the tire. The first belt layer is arranged between the tire body and the working layer. The first belt layer is a transition layer. The zeroth belt layer is used to be wound along the circumference of the tire through S-type winding to tightly fit the first belt layer, the second belt layer, the third belt layer and the tire body.
[0047] For further information, see Figure 3 A schematic diagram of a zero-degree winding structure of a zero-belt layer is shown, and Figure 4The structural schematic diagram of the S-type winding of the zeroth belt layer is shown. The zeroth belt layer can be tightly fitted to the first belt layer, the second belt layer, the third belt layer and the tire body by two winding methods: 0° winding and S-type winding. 0° winding means that the zeroth belt layer is fully wound parallel to the carcass with a winding angle of 0°. The S-type winding can optimize the stress of the zeroth belt layer, thereby reducing the risk of zero-degree belt layer cord breakage and increasing the service life of the tire. That is to say, the zeroth belt layer can be wound along the circumference of the tire in the form of S-type winding, or it can be fitted to the outside of the second belt layer (i.e., the outside of the tire circumference) perpendicular to the carcass along the circumference of the tire.
[0048] In summary, the present invention can jointly constrain the belt width through the endpoint difference, width ratio and constraint range, thereby improving the accuracy of the target width range value of each level of the belt, and using the belt width analysis model, it is possible to comprehensively consider various causes of belt endpoint damage and obtain a design scheme with the highest tire durability. In addition, the design scheme can also be adjusted in a targeted manner according to the tire's operating conditions, model, purpose and historical damage feedback.
[0049] Finally, it should be noted that the above-described embodiments are only specific implementations of the present invention, which are used to illustrate the technical solutions of the present invention, rather than to limit them. The protection scope of the present invention is not limited thereto. Although the present invention is described in detail with reference to the above-described embodiments, ordinary technicians in the field should understand that any technician familiar with the technical field can still modify the technical solutions recorded in the above-described embodiments within the technical scope disclosed by the present invention, or can easily think of changes, or make equivalent replacements for some of the technical features therein; and these modifications, changes or replacements do not make the essence of the corresponding technical solutions deviate from the spirit and scope of the technical solutions of the embodiments of the present invention, and should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the protection scope of the claims.
Claims
1. A method for improving tire performance, characterized in that: The method comprises: Collecting tire parameter information and tire historical status information of multiple tires through a vehicle sensor set, wherein the tire parameter information includes: tire section width information and belt width information, and the tire historical status information includes: belt temperature information, contact area information, average contact pressure information and maximum tire body tension information; Performing data analysis and processing on the tire parameter information and the tire historical status information to determine the endpoint difference between each belt layer, the width ratio corresponding to each belt layer, and the durability time corresponding to each tire; Obtaining a set of standard section widths of tires, and determining, according to the endurance time, the end point difference and the width ratio, a target end point difference range and a target width ratio range of the tires of each standard section width when the maximum endurance time is reached; Inputting the standard section width set, the corresponding target endpoint difference range and the target width ratio range into a preset classifier to perform classification training on the preset classifier and determine a belt width analysis model, wherein the belt width analysis model is used to match the corresponding target width range values of the first belt layer, the second belt layer, the third belt layer and the zeroth belt layer according to the section width of the tire, so as to improve the durability of the tire set according to the target width range value; The tire comprises: a tire body and a tire tread, wherein the tire tread comprises: a tire crown rubber and a belt layer; wherein the tire crown rubber comprises: a cap rubber and a base rubber, wherein the cap rubber is arranged on the outer surface of the base rubber, wherein the cap rubber is natural rubber or synthetic rubber, and wherein the base rubber is also natural rubber or synthetic rubber; wherein the belt layer is arranged between the tire body and the base rubber, wherein the belt layer is composed of steel wire or nylon combined with rubber, and wherein the belt layer is used to improve the durability and anti-damage capability of the tire; Wherein, the belt layer comprises: a second belt layer and a third belt layer, and the third belt layer is arranged on the outer surface of the second belt layer; wherein, the second belt layer and the third belt layer are working layers, which are used to improve the durability and damage resistance of the tire; Wherein, the belt layer further comprises: a first belt layer; wherein, the first belt layer is arranged between the tire body and the working layer, and the first belt layer is a transition layer; Wherein, the belt layer further includes: a zeroth belt layer; wherein, the zeroth belt layer is used to be wound along the circumference of the tire through S-type winding to closely fit the first belt layer, the second belt layer, the third belt layer and the tire body.
2. The tire performance improvement method according to claim 1, characterized in that: The step of performing data analysis and processing on the tire parameter information and the tire historical status information to determine the endpoint difference between each belt layer, the width ratio corresponding to each belt layer and the endurance time corresponding to each tire comprises: Determine the end point difference between each belt layer according to the belt layer width information, and determine the width ratio corresponding to each belt layer according to the tire section width information and the belt layer width information; The durability prediction process is performed on the tire historical status information through a preset parameter analysis model to determine the durability time corresponding to the tire.
3. The tire performance improvement method according to claim 2, characterized in that: The step of determining the end point difference between each belt layer according to the belt layer width information comprises: Determine the difference between half of the width of the first belt layer and half of the width of the zeroth belt layer as a first endpoint difference; A difference between half of the width of the second belt layer and half of the width of the zeroth belt layer is determined as a second end point difference.
4. The tire performance improvement method according to claim 2, characterized in that: The step of determining the width ratio corresponding to each belt layer according to the tire section width information and the belt layer width information comprises: The widths of the first belt layer, the second belt layer, the third belt layer and the zeroth belt layer are respectively divided by the standard section width to determine a first width ratio, a second width ratio, a third width ratio and a zeroth width ratio.
5. The tire performance improvement method according to claim 3, characterized in that: After the step of determining the difference between half of the width of the second belt layer and half of the width of the zeroth belt layer as the second endpoint difference, the method further includes: Acquiring historical damage information of the tire, wherein the historical damage information includes: a specific damage location of the tire belt layer; According to the historical damage information, the corresponding constraint range is matched from the preset database, so that the constraint range is combined with the durability time, the endpoint difference and the width ratio to determine the target endpoint difference range and the target width ratio range, wherein the constraint range is the endpoint difference constraint range of the first endpoint difference and the second endpoint difference.