LED chip and preparation method thereof

By providing a first functional layer with a specific opening structure and a metal reflective layer formed by sputtering in the LED chip, and forming an edge of an inclined angle of the slope is solved by forming a metal reflective layer edge with a slope and falling off and The problem of uniform thickness of the transmissive layer improves the brightness uniformity and product yield of the LED chip.

CN118610340BActive Publication Date: 2024-11-19HGC (ZHANGJIAGANG) SEMICON CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411100719.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-12
Publication Date
2024-11-19
Estimated Expiration
2044-08-12

AI Technical Summary

Technical Problem

While improving the problems of gold-bearing and falling off of the metal reflective layer of the LED chip, it is difficult to take into account the thickness uniformity of each area of ​​the induced revelation layer, which affects the brightness uniformity and product yield of the LED chip.

Method used

By providing a first functional layer with a specific opening structure between the revelation layer and the current expansion layer, and forming a metal reflective layer by sputtering, forming an edge of the revelation layer with a slope inclination angle in combination with a wet process, the metal reflective layer is improved by improving the metal reflective layer. The film forming mass and thickness uniformity of the induced retardation layer.

Benefits of technology

It effectively improves the metal edge and fall off problems of the metal reflective layer, while ensuring the thickness uniformity of the transmissive layer, improving the brightness uniformity and product yield of the LED chip, and reducing production and manufacturing costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118610340B_ABST
    Figure CN118610340B_ABST
Patent Text Reader

Abstract

The present application provides an LED chip and a preparation method thereof. The LED chip comprises an epitaxial layer, a current spreading layer, a transmittance-enhancing layer, a first functional layer and a metal reflective layer, wherein the current spreading layer is arranged on one side of the epitaxial layer; the transmittance-enhancing layer is arranged on the side of the current spreading layer away from the epitaxial layer; the first functional layer is arranged on the side of the transmittance-enhancing layer away from the current spreading layer and has a first opening; the metal reflective layer is arranged on the side of the current spreading layer away from the epitaxial layer and is located in the first opening; wherein, in the direction in which the transmittance-enhancing layer is away from the current spreading layer, the diameter of the first opening gradually increases, and the corrosion resistance of the transmittance-enhancing layer to the first solution is greater than the corrosion resistance of the first functional layer to the first solution. The LED chip and the preparation method thereof provided by the present application can improve the edge warping and shedding problems of the silver reflective layer while taking into account the thickness uniformity of each region of the transmittance-enhancing layer, thereby improving the brightness uniformity of the LED chip, improving the product yield, and reducing the production cost.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of semiconductor technology, and in particular to an LED chip and a method for preparing the same. Background Art

[0002] Light Emitting Diode (LED) is an electroluminescent semiconductor light-emitting device. It has been widely used in lighting, display, medical treatment, optical communication and other fields because of its advantages such as low energy consumption, small size, long life, good stability, fast response and stable luminous wavelength.

[0003] LED chips can be divided into normal LED chips, flip-chip LED chips, and vertical LED chips according to their structure. Among them, flip-chip LED chips have the advantages of large current drive, low chip thermal resistance, and high reliability. According to the main reflective layer, flip-chip LED chips can be further divided into silver mirror flip-chip LED chips, distributed Bragg reflector (English full name: Distributed Bragg Reflector, abbreviated: DBR) flip-chip LED chips and omni-directional reflector (English full name: Omni Directional Reflector, abbreviated: ODR) flip-chip LED chips. Among them, silver mirror flip-chip LED chips use silver film as the reflective layer, and have the advantages of high reflectivity and high conductive efficiency at different angles, which are favored by the industry.

[0004] In the related art, during the product development process for a silver mirror reflection structure with a stacked current spreading layer + anti-reflection layer + silver reflective layer having a higher comprehensive reflectivity, the applicant found that by making the anti-reflection layer have a slope with a certain inclination angle, the side plating problem of the metal atoms / metal ions of the subsequently formed silver reflective layer can be improved, thereby improving the edge warping and shedding problems of the silver reflective layer. However, in order to make the anti-reflection layer have a slope with a certain inclination angle, a wet etching process is required, and the uniformity of the wet etching process is difficult to control, which easily causes the thickness difference of each area of ​​the anti-reflection layer to increase, thereby affecting the brightness uniformity of the LED chip and reducing the product yield. Therefore, how to improve the edge warping and shedding problems of the silver reflective layer while taking into account the thickness uniformity of each area of ​​the anti-reflection layer is a technical problem that technicians in this field urgently need to solve. Summary of the invention

[0005] The present application provides an LED chip and a preparation method thereof, which can effectively solve the problem of LED chips in related technologies that it is difficult to improve the edge warping and peeling of the metal reflective layer while taking into account the thickness uniformity of each area of ​​the anti-reflection layer.

[0006] In a first aspect, the present application provides an LED chip, comprising: an epitaxial layer; a current spreading layer, arranged on one side of the epitaxial layer; an anti-reflection layer, arranged on a side of the current spreading layer away from the epitaxial layer; a first functional layer, arranged on a side of the anti-reflection layer away from the current spreading layer, and having a first opening; a metal reflective layer, arranged on a side of the current spreading layer away from the epitaxial layer, and located in the first opening; wherein, in the direction in which the anti-reflection layer is away from the current spreading layer, the diameter of the first opening gradually increases, and the corrosion resistance of the anti-reflection layer to a first solution is greater than the corrosion resistance of the first functional layer to the first solution.

[0007] Optionally, the refractive index of the anti-reflection layer is smaller than the refractive index of the current spreading layer, and the refractive index of the anti-reflection layer is smaller than the refractive index of the first functional layer.

[0008] Optionally, the sidewalls of the anti-reflection layer, the sidewalls of the current spreading layer, and the sidewalls of the epitaxial layer are covered with the first functional layer which is continuously arranged, and the first functional layer is an insulating layer.

[0009] Optionally, the material of the anti-reflection layer includes silicon dioxide, the material of the first functional layer includes aluminum oxide, and the first solution includes an alkaline solution.

[0010] Optionally, an angle between a side wall of the first opening and an orthographic projection of the side wall of the first opening on the anti-reflection layer is a first angle, and a magnitude of the first angle is 10° to 60°.

[0011] Optionally, the material of the metal reflective layer includes silver, and the metal reflective layer is formed in the first opening by sputtering.

[0012] In a second aspect, the present application provides a method for preparing an LED chip, the method for preparing an LED chip comprising the following steps:

[0013] forming an epitaxial layer and a current spreading layer arranged in a stacked manner;

[0014] Performing patterning on the current spreading layer and the epitaxial layer to form a patterned current spreading layer and a patterned epitaxial layer;

[0015] forming a patterned anti-reflection layer on the current spreading layer;

[0016] forming a first functional layer on the anti-reflection layer;

[0017] forming a patterned photoresist layer on the first functional layer;

[0018] Using the photoresist layer as a mask, the first functional layer is corroded by a first solution to form a patterned first functional layer, wherein the first functional layer has a first opening, wherein in a direction in which the anti-reflection layer is away from the current spreading layer, the diameter of the first opening gradually increases, and the corrosion resistance of the anti-reflection layer to the first solution is greater than the corrosion resistance of the first functional layer to the first solution;

[0019] forming a metal reflective layer, wherein the metal reflective layer includes a metal reflective layer covering the photoresist layer and a metal reflective layer located in the first opening;

[0020] The metal reflective layer covering the photoresist layer is stripped off, and the photoresist layer is removed.

[0021] Optionally, the material of the anti-reflection layer includes silicon dioxide, the material of the first functional layer includes aluminum oxide, and the first solution includes an alkaline solution.

[0022] Optionally, in the step of forming the metal reflective layer, the metal reflective layer is formed by sputtering.

[0023] Optionally, in the step of forming a patterned photoresist layer on the first functional layer, the material of the photoresist layer includes negative photoresist, the photoresist layer has a second opening, and the second opening corresponds to the first opening, wherein in the direction of the anti-reflection layer away from the current spreading layer, the diameter of the second opening gradually decreases.

[0024] The present application provides an LED chip and a preparation method thereof, wherein the LED chip comprises an epitaxial layer, a current spreading layer, an anti-reflection layer, a first functional layer and a metal reflective layer, wherein the current spreading layer is arranged on one side of the epitaxial layer; the anti-reflection layer is arranged on the side of the current spreading layer away from the epitaxial layer; the first functional layer is arranged on the side of the anti-reflection layer away from the current spreading layer and has a first opening; the metal reflective layer is arranged on the side of the current spreading layer away from the epitaxial layer and is located in the first opening; wherein, in the direction in which the anti-reflection layer is away from the current spreading layer, the diameter of the first opening gradually increases, and the corrosion resistance of the anti-reflection layer to the first solution is greater than the corrosion resistance of the first functional layer to the first solution. The LED chip and the preparation method thereof provided by the present application can improve the edge warping and shedding problems of the silver reflective layer while taking into account the thickness uniformity of each area of ​​the anti-reflection layer, thereby improving the brightness uniformity of the LED chip, improving the product yield, and reducing the production cost. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] The technical solution and other beneficial effects of the present application will be made apparent by describing in detail the specific implementation methods of the present application in conjunction with the accompanying drawings.

[0026] Figure 1 A schematic cross-sectional view of an LED chip provided in some embodiments of the present application.

[0027] Figure 2 This is a cross-sectional schematic diagram corresponding to step S10 in the method for preparing an LED chip provided in some embodiments of the present application.

[0028] Figure 3 This is a cross-sectional schematic diagram corresponding to step S20 in the method for preparing an LED chip provided in some embodiments of the present application.

[0029] Figure 4 This is a cross-sectional schematic diagram corresponding to step S30 in the method for preparing an LED chip provided in some embodiments of the present application.

[0030] Figure 5 This is a cross-sectional schematic diagram corresponding to step S40 in the method for preparing an LED chip provided in some embodiments of the present application.

[0031] Figure 6 This is a cross-sectional schematic diagram corresponding to step S50 in the method for preparing an LED chip provided in some embodiments of the present application.

[0032] Figure 7 This is a cross-sectional schematic diagram corresponding to step S60 in the method for preparing an LED chip provided in some embodiments of the present application.

[0033] Figure 8 This is a cross-sectional schematic diagram corresponding to step S70 in the method for preparing an LED chip provided in some embodiments of the present application.

[0034] Fig. 9 This is a cross-sectional schematic diagram corresponding to step S80 in the method for preparing an LED chip provided in some embodiments of the present application.

[0035] Fig.10 This is a cross-sectional schematic diagram corresponding to step S90 in the method for preparing an LED chip provided in some embodiments of the present application.

[0036] Description of reference numerals:

[0037] Substrate 100; epitaxial layer 110; first type semiconductor layer 111; light emitting layer 112; second type semiconductor layer 113; current spreading layer 120; anti-reflection layer 130; first functional layer 140; metal reflective layer 150; second functional layer 160; electrode layer 170; first electrode 171; second electrode 172; photoresist layer 180; first opening H1; second opening H2; first through hole H3; second through hole H4; third through hole H5. DETAILED DESCRIPTION

[0038] The technical solutions in the embodiments of the present application will be described clearly and completely below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, rather than all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present application.

[0039] The terms "first" and "second" in this document are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of this application, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.

[0040] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, an electrical connection, or mutual communication; it can be a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0041] The disclosure below provides many different embodiments or examples to realize the different structures of the present application. In order to simplify the disclosure of the present application, the parts and settings of specific examples are described below. Of course, they are only examples, and the purpose is not to limit the present application. In addition, the present application can repeat reference numbers and / or reference letters in different examples, and this repetition is for the purpose of simplification and clarity, which itself does not indicate the relationship between the various embodiments and / or settings discussed.

[0042] In the related art, a metal reflective layer with high reflective efficiency is usually set on the backlight side of the LED chip to increase the total amount of light emitted from the light-emitting side of the LED chip, thereby improving the brightness. The metal reflective layer can be a silver reflective layer with extremely high reflectivity in the white light band, or a gold reflective layer or an aluminum reflective layer with a reflectivity lower than that of silver. However, even the silver reflective layer with extremely high reflectivity in the white light band cannot reach 100%. Therefore, in order to further improve the comprehensive reflectivity, the applicant proposed a structural design of setting an anti-reflection layer between the current spreading layer and the metal reflective layer. At the same time, in order to ensure the chemical stability and high light transmittance of the anti-reflection layer, the anti-reflection layer usually includes silicon oxide and / or nitride, such as silicon dioxide and silicon nitride.

[0043] On this basis, the applicant further discovered that when the metal reflective layer is formed on the anti-reflective film by evaporation, such as when a silver reflective layer is formed on a silicon dioxide anti-reflective layer or a silicon nitride anti-reflective layer, a strong metal migration phenomenon will occur, and the film quality of the formed film is relatively loose, making the metal reflective layer extremely susceptible to corrosion and oxidation, thereby causing device failure and seriously affecting the life and stability of the LED.

[0044] Furthermore, the applicant has further developed a method of forming the metal reflective layer on the anti-reflective layer including silicon oxide and / or nitride by sputtering coating to improve the problems of metal migration, metal corrosion and oxidation. However, the applicant has further discovered that since the film layer formed by the sputtering coating method is very dense and has good coverage, it is easy to cause the edge of the patterned metal reflective layer to peel off when performing the metal stripping process after the subsequent formation of the patterned metal reflective layer, thereby seriously affecting the light output effect.

[0045] Furthermore, the applicant has further developed a method of etching the anti-reflection layer carrying the metal reflective layer through a wet process, so that the edge of the patterned anti-reflection layer forms a slope with a certain inclination angle, so as to improve the film-forming state of the edge of the patterned metal reflective layer and improve the problem of gold warping and shedding at the edge of the patterned metal reflective layer. However, the applicant has further discovered that when the anti-reflection layer carrying the metal reflective layer is corroded through a wet process, the uniformity of the wet etching process is difficult to control, which easily causes the thickness difference of each area of ​​the anti-reflection layer to increase, thereby affecting the brightness uniformity of the LED chip and reducing the product yield.

[0046] On the basis of the above technical background, in order to improve the problem of LED chips in related technologies that it is difficult to improve the edge warping and peeling of the metal reflective layer while taking into account the problem of thickness uniformity in various areas of the anti-reflection layer, the present application provides an LED chip and a preparation method thereof.

[0047] Figure 1 A schematic cross-sectional view of an LED chip provided in some embodiments of the present application. Figure 1As shown, in the first aspect, an embodiment of the present application provides an LED chip, the LED chip comprising an epitaxial layer 110, a current spreading layer 120, an anti-reflection layer 130, a first functional layer 140 and a metal reflective layer 150, wherein the current spreading layer 120 is arranged on one side of the epitaxial layer 110; the anti-reflection layer 130 is arranged on the side of the current spreading layer 120 away from the epitaxial layer 110; the first functional layer 140 is arranged on the side of the anti-reflection layer 130 away from the current spreading layer 120, and has a first opening H1; the metal reflective layer 150 is arranged on the side of the current spreading layer 120 away from the epitaxial layer 110, and is located in the first opening H1; wherein, in the direction in which the anti-reflection layer 130 is away from the current spreading layer 120, the diameter of the first opening H1 gradually increases, and the corrosion resistance of the anti-reflection layer 130 to the first solution is greater than the corrosion resistance of the first functional layer 140 to the first solution.

[0048] In the LED chip provided in the embodiment of the present application, since the anti-reflection layer 130 is disposed between the current spreading layer 120 and the metal reflective layer 150 , the comprehensive reflectivity can be further improved.

[0049] Furthermore, since the first functional layer 140 is provided between the anti-reflection layer 130 and the metal reflective layer 150, the first functional layer 140 can be used as a carrier film layer of the metal reflective layer 150, and by forming a first opening H1 with a side wall having a certain inclined angle in the first functional layer 140, the film forming state of the edge of the patterned metal reflective layer 150 can be improved, thereby improving the problem of gold warping and falling off at the edge of the patterned metal reflective layer 150. Specifically, since the diameter of the first opening H1 gradually increases in the direction in which the anti-reflection layer 130 departs from the current spreading layer 120, the sidewall of the first opening H1 is a slope with a certain inclination angle, so that in the subsequent process of forming the patterned metal reflective layer 150 by using the patterned photoresist layer 180, the slope can be used to reduce the kinetic energy of the metal atoms / metal ions in the metal reflective layer 150, thereby avoiding the metal atoms / metal ions in the metal reflective layer 150 from being deposited at the edge of the pattern in the photoresist layer 180, thereby improving the edge morphology and film formation quality of the patterned metal reflective layer 150, and improving the problem of edge warping and falling off of the metal reflective layer 150.

[0050] In addition, the wet process is more convenient for forming a slope with a certain inclination angle in the first functional layer 140, so the first functional layer 140 can be corroded by the first solution to form the first opening H1. On this basis, since the corrosion resistance of the anti-reflection layer 130 to the first solution is greater than the corrosion resistance of the first functional layer 140 to the first solution, the difference in corrosion resistance between the anti-reflection layer 130 and the first functional layer 140 to the first solution can be utilized, so that when the first opening H1 that can meet the requirements is formed by corrosion, the film morphology of the anti-reflection layer 130 is ensured to be as far as possible not to be destroyed by the first solution, thereby ensuring that each region of the anti-reflection layer 130 has a high thickness uniformity, so that the LED chip can improve the edge gold warping and shedding problems of the silver reflective layer while taking into account the thickness uniformity of each region of the anti-reflection layer 130, thereby improving the brightness uniformity of the LED chip, improving the product yield, and reducing the production cost.

[0051] In some embodiments of the present application, at least a portion of the sidewalls of the first opening H1 are covered with the metal reflective layer 150. In the LED chip provided in the embodiment of the present application, the sidewalls of the first opening H1 can reduce the kinetic energy of the metal atoms / metal ions in the metal reflective layer 150, thereby causing the metal atoms / metal ions to be deposited in the extension direction of the sidewalls. Accordingly, at least a portion of the sidewalls of the first opening H1 are covered with the metal reflective layer 150.

[0052] In some embodiments of the present application, the refractive index of the anti-reflection layer 130 is smaller than the refractive index of the current spreading layer 120 , and the refractive index of the anti-reflection layer 130 is smaller than the refractive index of the first functional layer 140 .

[0053] In the LED chip provided in the embodiment of the present application, since the refractive index of the anti-reflection layer 130 is smaller than the refractive index of the current spreading layer 120 and the first functional layer 140, the light reflected by the side wall of the metal reflective layer 150 can be deflected at the interface between the first functional layer 140 and the anti-reflection layer 130 and form a certain anti-reflection effect. After the anti-reflection effect of the anti-reflection layer 130, the light is emitted from the LED chip through the current spreading layer 120 and the epitaxial layer 110, thereby further improving the brightness and brightness uniformity of the LED chip.

[0054] In some embodiments of the present application, the sidewalls of the anti-reflection layer 130 , the sidewalls of the current spreading layer 120 , and the sidewalls of the epitaxial layer 110 are covered with the first functional layer 140 which is continuously disposed, and the first functional layer 140 is an insulating layer.

[0055] In the LED chip provided in the embodiment of the present application, in the related art, in order to further improve the anti-reflection effect of the anti-reflection layer 130, an optical microstructure is set on the surface of the anti-reflection layer 130. In the related art, the anti-reflection layer 130 will cover the side walls of the current spreading layer 120 and the side walls of the epitaxial layer 110 to ensure the reliability of the LED chip, but when the optical microstructure is set on the surface of the anti-reflection layer 130, the coating effect of the anti-reflection layer 130 on other film layers will be greatly reduced, thereby reducing the reliability of the LED chip. On the basis of setting the first functional layer 140, the present application takes advantage of the fact that the first functional layer 140 is an insulating layer, has high film quality, and has good adhesion effect on the surface of other film layers, and covers the first functional layer 140 that is continuously set on the side walls of the anti-reflection layer 130, the side walls of the current spreading layer 120, and the side walls of the epitaxial layer 110, thereby improving the reliability of the LED chip.

[0056] In some embodiments of the present application, the material of the anti-reflection layer 130 includes silicon dioxide, the material of the first functional layer 140 includes aluminum oxide, and the first solution includes an alkaline solution.

[0057] In the LED chip provided in the embodiment of the present application, the silicon dioxide in the anti-reflection layer 130 has a strong corrosion resistance to alkaline solutions, while the aluminum oxide in the first functional layer 140 is easily corroded by alkaline solutions, such as alkaline developers or ammonia water. Therefore, the difference in corrosion resistance of silicon dioxide and aluminum oxide to alkaline solutions can be utilized to form a first opening H1 of a specific shape in the first functional layer 140 while weakening the influence of the alkaline solution on the anti-reflection layer 130 as much as possible, so that the LED chip can improve the edge warping and shedding problems of the silver reflective layer while taking into account the thickness uniformity of each area of ​​the anti-reflection layer 130, thereby improving the brightness uniformity of the LED chip, improving the product yield, and reducing the production cost.

[0058] Moreover, the refractive index of aluminum oxide is greater than the refractive index of silicon dioxide and the current spreading layer 120, so that the light reflected by the side wall of the metal reflective layer 150 can be deflected at the interface between the first functional layer 140 and the anti-reflection layer 130, and a certain anti-reflection effect is formed. Exemplarily, the material of the current spreading layer 120 includes indium tin oxide. Moreover, aluminum oxide can have a good adhesion effect on the epitaxial layer 110, the current spreading layer 120, and the first functional layer 140, and has good insulation and light transmittance.

[0059] In some embodiments of the present application, an angle between a sidewall of the first opening H1 and an orthographic projection of the sidewall of the first opening H1 on the anti-reflection layer 130 is a first angle, and a magnitude of the first angle is 10° to 60°.

[0060] In the LED chip provided in the embodiment of the present application, the larger the angle of the first angle is, the greater the inclination of the side wall of the first opening H1 is; the smaller the angle of the first angle is, the smaller the inclination of the side wall of the first opening H1 is. The applicant found in the actual design verification of the first angle that the larger the inclination of the side wall of the first opening H1 is, the stronger the ability to resist the climbing of metal atoms / metal ions is. However, since the extension length of the side wall of the first opening H1 in the horizontal direction (the direction parallel to the plane where the substrate 100 is located) also has design requirements, the extension length of the side wall of the first opening H1 in the horizontal direction is related to the chamfer size of the side wall of the opening on the photoresist layer 180. In order to simultaneously meet the design requirements of the extension length of the side wall of the first opening H1 in the horizontal direction and the inclination of the side wall of the first opening H1, and avoid the thickness of the first functional layer 140 being too thick, the present application controls the size of the first angle to be between 10° and 60°. Preferably, the size of the first angle is between 10° and 30°, such as 10°, 15°, 20°, 25°, and 30°.

[0061] In some embodiments of the present application, the material of the metal reflective layer 150 includes silver, and the metal reflective layer 150 is formed in the first opening H1 by sputtering.

[0062] In the LED chip provided in the embodiment of the present application, silver has a higher reflection efficiency in the white light band than other metals. In addition, in order to improve the coverage effect of silver on the anti-reflection layer 130, the present application forms the metal reflective layer 150 in the first opening H1 by sputtering. Of course, the method of forming the metal reflective layer 150 by sputtering also increases the risk of edge warping and falling off of the metal reflective layer 150 during the subsequent peeling process, thereby increasing the necessity of adding the first functional layer 140 and forming the first opening H1 with a preset tilt angle in the first functional layer 140.

[0063] In some embodiments of the present application, the LED chip can be a flip-chip LED chip. The reason is that the metal reflective layer 150 is widely used in flip-chip LED chips, but the present application does not limit the structural type of the LED chip. All LED chips with a current expansion layer and a metal reflective layer can apply the contents disclosed in this application.

[0064] In some embodiments of the present application, the LED chip further comprises a substrate 100, and the material of the substrate 100 may be sapphire or other materials with good light transmittance. Of course, in other embodiments of the present application, the substrate 100 may be omitted to form a thin film LED chip.

[0065] In some embodiments of the present application, the epitaxial layer 110 includes a first-type semiconductor layer 111, a light-emitting layer 112, and a second-type semiconductor layer 113 stacked in sequence. The first-type semiconductor layer 111 may be an N-type semiconductor layer, such as an N-type gallium nitride layer; the light-emitting layer 112 is a multi-quantum well layer; and the second-type semiconductor layer 113 may be a P-type semiconductor layer, such as a P-type gallium nitride layer. The epitaxial layer 110 has a step structure.

[0066] In some embodiments of the present application, the anti-reflection layer 130 has a first through hole H3 , and the metal reflective layer 150 is electrically connected to the current spreading layer 120 through the first through hole H3 .

[0067] In some embodiments of the present application, the LED chip also includes a second functional layer 160 and an electrode layer 170 that are stacked, the material of the second functional layer 160 is the same as the material of the anti-reflection layer 130 or the first functional layer 140, the second functional layer 160 has a second through hole H4, and the electrode layer 170 includes a second electrode 172, and the second electrode 172 is electrically connected to the metal reflective layer 150 through the second through hole H4.

[0068] In some embodiments of the present application, the LED chip also includes a third through hole H5, which passes through the second functional layer 160 and the first functional layer 140, and the electrode layer 170 also includes a first electrode 171, which is electrically connected to the first type semiconductor layer 111 through the third through hole H5.

[0069] In some embodiments of the present application, the LED chip further includes a covering layer (not shown in the figures), and the covering layer covers at least a portion of the non-light-emitting surface of the LED chip to prevent light leakage.

[0070] On the second aspect, the embodiment of the present application provides a method for preparing an LED chip, which is used to prepare an LED chip. The LED chip can improve the edge warping and peeling problems of the silver reflective layer while taking into account the thickness uniformity of each area of ​​the anti-reflection layer 130, thereby improving the brightness uniformity of the LED chip, improving the product yield, and reducing the production cost.

[0071] In some embodiments of the present application, the method for preparing the LED chip includes step S10, step S20, step S30, step S40, step S50, step S60, step S70, step S80, and step S90.

[0072] Figure 2 This is a cross-sectional schematic diagram corresponding to step S10 in the method for preparing an LED chip provided in some embodiments of the present application. Figure 2 As shown, step S10 includes: forming an epitaxial layer 110 and a current spreading layer 120 which are stacked.

[0073] Specifically, step S10 includes: providing a substrate 100, sequentially forming a first type semiconductor layer 111, a light emitting layer 112, and a second type semiconductor layer 113 on the substrate 100, and forming a current spreading layer 120 on the second type semiconductor layer 113. The substrate 100 may be a sapphire substrate 100, the first type semiconductor layer 111 may be an N-type gallium nitride layer, the second type semiconductor layer 113 may be a P-type gallium nitride layer, and the current spreading layer 120 may be an indium tin oxide layer.

[0074] Figure 3 This is a cross-sectional schematic diagram corresponding to step S20 in the method for preparing an LED chip provided in some embodiments of the present application. Figure 3 As shown, step S20 includes: patterning the current spreading layer 120 and the epitaxial layer 110 to form a patterned current spreading layer 120 and a patterned epitaxial layer 110 .

[0075] Specifically, step S20 includes: patterning the current spreading layer 120 to expose the second type semiconductor layer 113 in a local area, and then patterning the second type semiconductor layer 113 and the light emitting layer 112 in a partial area of ​​the local area to form a patterned epitaxial layer 110 with a step structure.

[0076] Figure 4 This is a cross-sectional schematic diagram corresponding to step S30 in the method for preparing an LED chip provided in some embodiments of the present application. Figure 4 As shown, step S30 includes: forming a patterned anti-reflection layer 130 on the current spreading layer 120 .

[0077] Specifically, step S30 includes: forming an anti-reflection layer 130 on the current spreading layer 120, and then performing photolithography, etching and stripping to form a patterned anti-reflection layer 130 having a first through hole H3. Optionally, the anti-reflection layer 130 is made of silicon dioxide.

[0078] Figure 5This is a cross-sectional schematic diagram corresponding to step S40 in the method for preparing an LED chip provided in some embodiments of the present application. Figure 5 As shown, step S40 includes: forming a first functional layer 140 on the anti-reflection layer 130 .

[0079] Specifically, step S40 includes: forming a first functional layer 140 on the anti-reflection layer 130 by electron beam evaporation, wherein the thickness of the first functional layer 140 is controlled to be between 1000 angstroms and 5000 angstroms. Optionally, the material of the first functional layer 140 includes aluminum oxide.

[0080] Figure 6 This is a cross-sectional schematic diagram corresponding to step S50 in the method for preparing an LED chip provided in some embodiments of the present application. Figure 6 As shown, step S50 includes: forming a patterned photoresist layer 180 on the first functional layer 140 .

[0081] Specifically, step S50 includes: forming a photoresist layer 180 on the first functional layer 140, irradiating the photoresist layer 180 with an ultraviolet light source arranged on a side of the photoresist layer 180 away from the first functional layer 140, and developing to form a patterned photoresist layer 180, wherein the patterned photoresist layer 180 has a second opening H2, and the second opening H2 has a chamfer, wherein in the direction in which the anti-reflection layer 130 is away from the current spreading layer 120, the diameter of the second opening H2 gradually decreases. It should be noted that the reason why the patterned photoresist layer 180 can form the second opening H2 with a chamfered structure is that the material of the photoresist layer 180 includes negative photoresist. In the process of irradiating the photoresist layer 180 with the ultraviolet light source, the irradiation pattern of the ultraviolet light source on the photoresist layer 180 also has a certain pattern shape, but the light attenuation at the edge of the irradiation pattern will be more serious, which will cause the photoresist at the bottom of the irradiation pattern to be unable to be fully exposed, and then after the development process, the second opening H2 with a chamfered structure will be formed on the patterned photoresist layer 180.

[0082] Figure 7 This is a cross-sectional schematic diagram corresponding to step S60 in the method for preparing an LED chip provided in some embodiments of the present application. Figure 7As shown, step S60 includes: using the photoresist layer 180 as a mask, using a first solution to etch the first functional layer 140 to form a patterned first functional layer 140, wherein the first functional layer 140 has a first opening H1, wherein the diameter of the first opening H1 gradually increases in the direction in which the anti-reflection layer 130 is away from the current spreading layer 120, and the corrosion resistance of the anti-reflection layer 130 to the first solution is greater than the corrosion resistance of the first functional layer 140 to the first solution. Specifically, the first solution is an alkaline solution, such as an alkaline developer or ammonia water.

[0083] Specifically, the second opening H2 is arranged corresponding to the first opening H1, and the edge of the second opening H2 is flush with the edge of the first opening H1. The edge size of the first opening H1 can be controlled by means of an etching process for the first functional layer 140, so that the edge of the second opening H2 is flush with the edge of the first opening H1, so that the combined structure can be used to avoid the subsequent contact between the metal reflective layer 150 in the first opening H1 and the side wall of the second opening H2 as much as possible.

[0084] Figure 8 This is a cross-sectional schematic diagram corresponding to step S70 in the method for preparing an LED chip provided in some embodiments of the present application. Figure 8 As shown, step S70 includes: forming a metal reflective layer 150 , wherein the metal reflective layer 150 includes the metal reflective layer 150 covering the photoresist layer 180 and the metal reflective layer 150 located in the first opening H1 .

[0085] Specifically, step S70 includes: forming the metal reflective layer 150 by sputtering to improve the film quality of the metal reflective layer 150 on the anti-reflection layer 130, improve the problems of metal migration and metal corrosion and oxidation, and improve the film density of the metal reflective layer 150. Optionally, the metal reflective layer 150 is a silver reflective layer.

[0086] Fig. 9 This is a cross-sectional schematic diagram corresponding to step S80 in the method for preparing an LED chip provided in some embodiments of the present application. Fig. 9 As shown, step S80 includes: stripping off the metal reflective layer 150 covering the photoresist layer 180 , and removing the photoresist layer 180 .

[0087] In the method for preparing the LED chip provided in the embodiment of the present application, since in the process of sputtering to form the metal reflective layer 150, compared with other film forming methods, the kinetic energy of the metal atoms / metal ions is larger and more dense, the metal atoms / metal ions attached to the surface of the carrier film layer (anti-reflection layer 130) are prone to lateral expansion. As mentioned above, since the second opening H2 has a chamfer, in the process of sputtering coating, if the kinetic energy of the metal atoms / metal ions with larger kinetic energy is not reduced, the metal atoms / metal ions will lateral expand along the side wall of the second opening H2 of the photoresist layer 180, and metal deposition will be generated along the side wall of the second opening H2. When the metal reflective layer 150 deposited on the side wall of the second opening H2 contacts and adheres to the metal reflective layer 150 on the surface of the carrier film layer, problems of metal warping and falling off will occur in the subsequent metal stripping process.

[0088] However, since the diameter of the first opening H1 gradually increases in the direction in which the anti-reflection layer 130 moves away from the current spreading layer 120, the slope of the side wall of the first opening H1 can be used to reduce the kinetic energy of the metal atoms / metal ions formed on the supporting film layer (anti-reflection layer 130) during the process of sputtering to form the metal reflective layer 150, thereby preventing the metal reflective layer 150 from being deposited and further accumulated on the side wall of the second opening H2, thereby improving the problem of metal warping and falling off.

[0089] In addition, since the corrosion resistance of the anti-reflection layer 130 to the first solution is greater than the corrosion resistance of the first functional layer 140 to the first solution, the difference in corrosion resistance between the anti-reflection layer 130 and the first functional layer 140 to the first solution can be utilized, so that while the first opening H1 that can meet the requirements is formed by corrosion, the film morphology of the anti-reflection layer 130 is ensured to be as far as possible not to be destroyed by the first solution, thereby ensuring that each region of the anti-reflection layer 130 has a high thickness uniformity, so that the LED chip can improve the edge warping and shedding problems of the silver reflective layer while taking into account the thickness uniformity of each region of the anti-reflection layer 130, thereby improving the brightness uniformity of the LED chip, improving the product yield, and reducing the production cost.

[0090] Fig.10 This is a cross-sectional schematic diagram corresponding to step S90 in the method for preparing an LED chip provided in some embodiments of the present application. Fig.10 As shown, step S90 includes: sequentially forming a patterned second functional layer 160 and a patterned electrode layer 170 on the metal reflective layer 150 .

[0091] Specifically, step S90 includes: forming a second functional layer 160 on the metal reflective layer 150, and patterning the second functional layer 160 to form a second through hole H4 penetrating the second functional layer 160 and a third through hole H5 penetrating the second functional layer 160 and the first functional layer 140. To facilitate the formation of the third through hole H5, the material of the second functional layer 160 can be the same as that of the first functional layer 140.

[0092] Specifically, step S90 also includes forming a patterned electrode layer 170 on the patterned second functional layer 160, the electrode layer 170 includes a first electrode 171 and a second electrode 172, the first electrode 171 is electrically connected to the first type semiconductor layer 111 through the third through hole H5; the second electrode 172 is electrically connected to the metal reflective layer 150 through the second through hole H4, and then electrically connected to the second type semiconductor layer 113 through the current spreading layer 120.

[0093] In some embodiments of the present application, after step S80 and before step S90, the following step is further included: forming a covering layer, wherein the covering layer covers at least a portion of the non-light-emitting surface of the LED chip to prevent light leakage.

[0094] In summary, the present application provides an LED chip and a preparation method thereof, wherein the LED chip comprises an epitaxial layer, a current spreading layer, an anti-reflection layer, a first functional layer and a metal reflective layer, wherein the current spreading layer is arranged on one side of the epitaxial layer; the anti-reflection layer is arranged on the side of the current spreading layer away from the epitaxial layer; the first functional layer is arranged on the side of the anti-reflection layer away from the current spreading layer and has a first opening; the metal reflective layer is arranged on the side of the current spreading layer away from the epitaxial layer and is located in the first opening; wherein, in the direction in which the anti-reflection layer is away from the current spreading layer, the diameter of the first opening gradually increases, and the corrosion resistance of the anti-reflection layer to the first solution is greater than the corrosion resistance of the first functional layer to the first solution. The LED chip and the preparation method thereof provided by the present application can improve the edge warping and shedding problems of the silver reflective layer while taking into account the thickness uniformity of each area of ​​the anti-reflection layer, thereby improving the brightness uniformity of the LED chip, improving the product yield, and reducing the production cost.

[0095] The above is a detailed introduction to an LED chip and a preparation method thereof provided in an embodiment of the present application. Specific examples are used herein to illustrate the principles and implementation methods of the present application. The description of the above embodiments is only used to help understand the method of the present application and its core idea. At the same time, for technicians in this field, according to the idea of ​​the present application, there will be changes in the specific implementation method and application scope. In summary, the content of this specification should not be understood as a limitation on the present application.

Claims

1. A method for preparing an LED chip, characterized in that: The method for preparing the LED chip comprises the following steps: forming an epitaxial layer and a current spreading layer arranged in a stacked manner; Performing patterning on the current spreading layer and the epitaxial layer to form a patterned current spreading layer and a patterned epitaxial layer; forming a patterned anti-reflection layer on the current spreading layer; forming a first functional layer on the anti-reflection layer; forming a patterned photoresist layer on the first functional layer; Using the photoresist layer as a mask, the first functional layer is corroded by a first solution to form a patterned first functional layer, wherein the first functional layer has a first opening, wherein in a direction in which the anti-reflection layer is away from the current spreading layer, the diameter of the first opening gradually increases, and the corrosion resistance of the anti-reflection layer to the first solution is greater than the corrosion resistance of the first functional layer to the first solution; forming a metal reflective layer, wherein the metal reflective layer includes a metal reflective layer covering the photoresist layer and a metal reflective layer located in the first opening; The metal reflective layer covering the photoresist layer is stripped off, and the photoresist layer is removed.

2. The method for preparing an LED chip according to claim 1, characterized in that: The material of the anti-reflection layer includes silicon dioxide, the material of the first functional layer includes aluminum oxide, and the first solution includes an alkaline solution.

3. The method for preparing an LED chip according to claim 1, characterized in that: In the step of forming the metal reflective layer, the metal reflective layer is formed by sputtering.

4. The method for preparing an LED chip according to claim 1, characterized in that: In the step of forming a patterned photoresist layer on the first functional layer, the material of the photoresist layer includes negative photoresist, and the photoresist layer has a second opening, which corresponds to the first opening, wherein the diameter of the second opening gradually decreases in the direction in which the transmittance enhancement layer departs from the current spreading layer.

5. An LED chip, characterized in that: The LED chip is prepared by the method for preparing an LED chip according to any one of claims 1 to 4, and the LED chip comprises: Epitaxial layer; A current spreading layer, arranged on one side of the epitaxial layer; An anti-reflection layer, arranged on a side of the current spreading layer away from the epitaxial layer; A first functional layer is disposed on a side of the anti-reflection layer away from the current spreading layer and has a first opening; A metal reflective layer, disposed on a side of the current spreading layer away from the epitaxial layer and located in the first opening; Wherein, in the direction in which the transmittance-enhancing layer departs from the current spreading layer, the diameter of the first opening gradually increases, and the corrosion resistance of the transmittance-enhancing layer to the first solution is greater than the corrosion resistance of the first functional layer to the first solution.

6. The LED chip according to claim 5, characterized in that: The refractive index of the anti-reflection layer is smaller than the refractive index of the current spreading layer, and the refractive index of the anti-reflection layer is smaller than the refractive index of the first functional layer.

7. The LED chip according to claim 6, characterized in that: The sidewalls of the anti-reflection layer, the sidewalls of the current spreading layer, and the sidewalls of the epitaxial layer are covered with the first functional layer which is continuously arranged, and the first functional layer is an insulating layer.

8. The LED chip according to claim 7, characterized in that: The material of the anti-reflection layer includes silicon dioxide, the material of the first functional layer includes aluminum oxide, and the first solution includes an alkaline solution.

9. The LED chip according to claim 5, characterized in that: An angle between a side wall of the first opening and an orthographic projection of the side wall of the first opening on the anti-reflection layer is a first angle, and a magnitude of the first angle is 10° to 60°.

10. The LED chip according to claim 5, characterized in that: The material of the metal reflective layer includes silver, and the metal reflective layer is formed in the first opening by sputtering.