A comprehensive treatment method for hazardous waste from aluminum plants

Through the classification and treatment of hazardous waste in aluminum plants, including multi-stage treatment of lithium-containing hazardous waste and lithium-free hazardous waste, resource regeneration and pollution reduction are achieved, and the problems of high cost and low recovery rate of hazardous waste treatment in aluminum plants are solved. , improving economic and environmental benefits.

CN118616457BActive Publication Date: 2024-10-18王绘超
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202411080343.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-08
Publication Date
2024-10-18
Estimated Expiration
2044-08-08

AI Technical Summary

Technical Problem

The production cost of hazardous waste in aluminum plants is high, the recovery rate is low, the economic benefits are poor, and there are pollution problems. It is difficult to effectively process and utilize these hazardous waste materials with existing technology.

Method used

By classifying hazardous wastes from aluminum plants, including the specific steps for lithium-containing hazardous wastes and lithium-free hazardous wastes: the stages of batching and grinding of lithium-containing hazardous wastes, flotation carbon separation, leaching, purification, lithium precipitation and concentration, etc. Utilize recycling and recovery processing; denitrification and sulfuric acid leaching and filtration of lithium-free hazardous waste to generate aluminum sulfate solution, which can be used in subsequent steps to achieve resource regeneration and pollution reduction.

Benefits of technology

It realizes the extraction of various regeneration products such as refined carbon, lithium carbonate, sodium sulfate, etc., reduces wastewater discharge, has low treatment costs, improves economic and environmental benefits, has high resource utilization rate, effectively eliminates harmful substances, and reduces pollution.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118616457B_ABST
    Figure CN118616457B_ABST
Patent Text Reader

Abstract

The present invention relates to hazardous waste treatment technology, and in particular to a comprehensive treatment method for hazardous waste in an aluminum plant, the method comprising the following steps: step A: classifying hazardous waste to obtain lithium-containing hazardous waste and lithium-free hazardous waste; step B: the specific treatment steps for lithium-containing hazardous waste include six stages of batching and grinding, flotation carbon separation, leaching, purification, lithium precipitation and concentrated nitration; wherein the output materials between the leaching, purification, lithium precipitation and concentrated nitration are subjected to circulation / recycling treatment; step C: denitrifying the lithium-free hazardous waste to obtain denitrified lithium-free hazardous waste, acid-leaching the denitrified lithium-free hazardous waste and filtering it to obtain aluminum sulfate solution and leached slag. The present invention comprehensively treats hazardous waste in aluminum plants, reduces pollution, improves energy utilization, and thus improves economic benefits.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to hazardous waste treatment technology, and in particular to a comprehensive treatment method for hazardous waste from aluminum plants. Background Art

[0002] Aluminum is a very important basic raw material and has very important applications in all walks of life. However, aluminum smelting is a highly polluting and energy-intensive industry. Its production will produce many hazardous wastes, such as overhaul slag, cathode carbon, aluminum ash, etc., which contain not only useful substances such as lithium, carbon, cryolite, aluminum, silicon, but also fluorides, cyanides, heavy metals, and other harmful substances. They are listed as hazardous wastes by the state. The state has relevant laws and regulations on the storage and utilization of hazardous wastes, and strictly controls them. Many units and individuals in China have carried out experimental research on the comprehensive utilization of hazardous wastes from aluminum plants to varying degrees, and have achieved some results, but their production costs are high, the recovery rate is low, the economic benefits are poor, and they even result in losses.

[0003] The present application provides a comprehensive treatment method for hazardous waste from an aluminum plant, which comprehensively treats hazardous waste from the aluminum plant, improves energy utilization, and further improves economic benefits. Summary of the invention

[0004] The present application provides a comprehensive treatment method for hazardous waste from an aluminum plant, which comprehensively treats hazardous waste from the aluminum plant, improves energy utilization, and thus improves economic benefits. Another purpose of the present invention is to reduce pollution during the recycling and treatment of hazardous waste.

[0005] The present invention is achieved through the following technical solutions:

[0006] A comprehensive treatment method for hazardous waste from an aluminum plant, specifically comprising the following steps:

[0007] Step A: Classify hazardous waste to obtain lithium-containing hazardous waste and lithium-free hazardous waste, and store them separately;

[0008] Step B: The specific treatment steps for lithium-containing hazardous waste include six stages: batching and grinding, flotation and carbon separation, leaching, purification, lithium precipitation and concentrated nitrate separation; wherein the output materials between the leaching, purification, lithium precipitation and concentrated nitrate separation are subjected to circulation / recycling treatment;

[0009] Step C: The specific treatment steps for non-lithium hazardous waste are as follows:

[0010] Step C1: denitrifying the lithium-free hazardous waste to obtain denitrified lithium-free hazardous waste;

[0011] Step C2: leaching the denitrified lithium-free hazardous waste with sulfuric acid and filtering it to obtain an aluminum sulfate solution and leached residue;

[0012] Wherein, the aluminum sulfate solution in step C2 is applied to the leaching stage of step B.

[0013] Furthermore, in the step B, lithium-containing hazardous waste is ground into lithium-containing hazardous waste powder; the carbon content of the lithium-containing hazardous waste powder is 35wt%±1wt%, and the particle size is ≤74μm.

[0014] Furthermore, the lithium-containing hazardous waste powder is subjected to flotation separation to obtain floating carbon and floating tailings; the grade of the floating carbon is ≥80%.

[0015] Furthermore, the floating carbon is leached to obtain lithium precious liquid and refined carbon.

[0016] Furthermore, the lithium precious solution 1 is used as a leaching solution for the floating tail to leach the floating tail to obtain lithium precious solution 2 and leaching residue.

[0017] Furthermore, the leaching includes pulping pre-leaching, reactor leaching, filter pressing and countercurrent multi-gradient washing; the washing liquid of the countercurrent multi-gradient washing is circulated for pulping pre-leaching and reactor leaching; wherein the temperature of the reactor leaching is 50°C-95°C.

[0018] Furthermore, the lithium precious liquid II is purified to obtain purified slag and purified liquid, and the purified slag is mixed with the floating tail and re-leached; wherein, in the purification step, sodium hydroxide and sodium carbonate are used as a combined purifier in a mass ratio of 1:1, the temperature is 50°C-95°C, and the pH value is 7-10.

[0019] Furthermore, in the lithium precious solution 2, the concentration of lithium is greater than or equal to 8 g / L.

[0020] Furthermore, sodium carbonate is added in batches according to 7-10 times of the total amount of lithium in the purified solution to precipitate lithium to obtain lithium carbonate and lean solution; during the lithium precipitation process, the temperature is 50° C.-95° C. and the reaction time is 1-3 hours.

[0021] Furthermore, the treatment steps of the lean liquid are: first evaporate and concentrate about 50% of the water, cool to below 10°C, remove about 70% of the sodium and sulfur, and filter to obtain sodium sulfate; wherein the denitrified water after denitrification is returned to the lithium precipitation system for recycling.

[0022] The present invention has the following beneficial effects:

[0023] 1. The present invention extracts various regenerated products such as refined carbon, lithium carbonate, sodium sulfate, aluminum sulfate, etc. from hazardous waste materials in aluminum smelting, and the water in the leachate and filtrate in the overall production process can be basically recycled, and less wastewater is discharged.

[0024] 2. The present invention uses less treatment liquid, has low treatment cost, and has a simple and easy-to-implement production process. According to preliminary calculations, the products produced are used for lithium carbonate, sodium sulfate, cryolite and their metallurgical auxiliary materials and refractory ingredients. Each ton of raw materials can produce products worth about 8,000 yuan, with huge economic, environmental and social benefits.

[0025] 3. The present invention eliminates harmful substances in various reactions, thereby achieving the goals of resource utilization and pollution elimination. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 This is the comprehensive treatment process of hazardous waste from aluminum plants of the present invention. DETAILED DESCRIPTION

[0027] The following will be combined with the drawings in the embodiments of the invention to clearly and completely describe the technical solutions in the embodiments of the invention. Obviously, the described embodiments are only part of the embodiments of the invention, not all of the embodiments. Based on the embodiments of the invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the invention.

[0028] like Figure 1 As shown, a comprehensive treatment method for hazardous waste from an aluminum plant comprises the following steps:

[0029] Hazardous waste is classified into lithium-containing hazardous waste and lithium-free hazardous waste, which are stored separately. Specifically, aluminum electrolytic cell overhaul slag, waste cathode, and waste electrolyte are classified as lithium-containing hazardous waste, which contains 0.2% to 1.5% lithium. Other components are mainly carbon, silicon dioxide, aluminum oxide, cryolite and other fluorine-containing substances, and cyanide compounds. Aluminum ash and aluminum slag are classified as lithium-free hazardous waste, whose main components are elemental aluminum, aluminum oxide, ammonia nitrogen, etc. These two types of hazardous waste can cover more than 90% of the hazardous waste with recycling value in aluminum plants. Pollution can be reduced and economic benefits can be improved through recycling and treatment. In order to ensure the treatment effect and obtain high-purity products, lithium-containing hazardous waste and lithium-free hazardous waste are treated separately.

[0030] Among them, the steps for treating lithium-containing hazardous waste are as follows:

[0031] First, batching and crushing lithium-containing hazardous waste to obtain lithium-containing hazardous waste crushed material. In this step, batching is to mix lithium-containing hazardous waste crushed materials with different carbon contents in proportion to obtain a homogenized material with a carbon content of 35wt%±1%. The homogenized material is crushed to a particle size of less than 10mm to obtain lithium-containing hazardous waste crushed material, thereby increasing the bulk density and providing a basis for subsequent grinding steps; so that the flotation carbon separation after closed-circuit grinding can achieve better flotation effect. Under normal circumstances, the carbon content of overhaul slag and waste furnace materials is about 20%, and the carbon content of cathode carbon, electrode blocks, etc. is generally about 50%, which are tested before batching.

[0032] Second, the lithium-containing hazardous waste crushed materials are ground to obtain lithium-containing hazardous waste powder. In this step, closed-circuit grinding is performed by a wet grid ball mill to grind the lithium-containing hazardous waste crushed materials to 200 mesh. The MQG grid ball mill and the FG spiral distributor constitute a closed-circuit grinding system. The qualified grinding products enter the flotation system after classification overflow, and the coarse sand returns to the ball mill for re-grinding. The grinding concentration is 50% to 60%, the classification overflow concentration is about 10% to 40%, and the classification overflow fineness is 20% to 70% of 200 mesh, which meets the optimal conditions required by the flotation system. While grinding, an environmentally friendly cyanide removal device is added, and bleaching powder or hydrogen peroxide is added as required to eliminate the harmful effects of cyanide.

[0033] Third, the lithium-containing hazardous waste powder is subjected to flotation separation to obtain floating carbon and floating tailings. In this step, the flotation includes the steps of dosing, roughing, scavenging and concentrating, wherein the dosing is the addition of a mixed collector Hs+ys in an amount of 60-500 g / ton, and the addition of a frother HP in an amount of 20-160 g / ton. After roughing, scavenging and multiple concentrating by an SF type flotation machine, slag carbon separation is achieved, and the flotation water is recycled.

[0034] Fourth, the floating carbon is leached and then dehydrated to obtain lithium precious solution 1 and refined carbon, and the floating tail is leached and then dehydrated to obtain lithium precious solution 2 and leached residue, wherein the leaching of the floating carbon includes the following steps:

[0035] Ⅰ, pulping, the leachate is an aqueous solution of aluminum sulfate 18hydrate, the standard of the aqueous solution of aluminum sulfate 18hydrate can be expressed by the alumina content in the solution as equivalent, according to the changes of lithium, sodium, potassium, aluminum, fluorine, silicon, and other components in the raw materials, the alumina equivalent in the leachate is 0.2% to 8%, the floating carbon is mixed with the leachate to make pulp, and a premixed slurry is obtained; Ⅱ, pre-impregnation, the premixed slurry is put into a reactor, stirring is started for pre-impregnation, and the pre-impregnation time is 60 minutes; Ⅲ, reactor leaching, the reactor temperature is controlled to be 50-95°C, the reaction time is 1-5 hours, and the reaction end point is reached when the components in the liquid phase no longer change after detection;

[0036] Leaching the floating tail includes the following steps:

[0037] ①, pulping, lithium precious liquid 1 is supplemented with an aqueous solution of aluminum sulfate 18hydrate as a leachate, the floating tail is mixed with the leachate to prepare pulp, and a premixed slurry 2 is obtained; ②, pre-impregnation, the premixed slurry 2 is put into a reactor, stirring is started for pre-impregnation, and the pre-impregnation time is 60 minutes; ③, reactor leaching, the reaction time is 1-5 hours, and the reaction end point is reached when the components in the liquid phase no longer change after detection, and the leached residue is washed and then enters the cryolite production system.

[0038] Fifth, purify the lithium precious liquid II by using sodium hydroxide and sodium carbonate in a mass ratio of 1:1 as a combined purifier, adjusting the pH value to 7-10 at a temperature of 50-95°C, so that the metal impurity ions in the precious liquid are precipitated as hydroxides or carbonates and basic carbonates. The comprehensive purification rate of harmful impurities reaches 99%, and purified slag and purified liquid are obtained. The lithium concentration in the purified liquid is greater than 8g / L. The purified slag is returned to the leaching process of floating carbon and floating tailings, and the purified liquid enters the next step.

[0039] Sixth, lithium is precipitated in the purified liquid. Industrial pure sodium carbonate is added in batches at a ratio of 1:7-10 according to the total weight of lithium in the purified liquid. The reaction is carried out at 50-95°C for 1-3 hours. Lithium carbonate and lean solution are obtained after filtration. The lithium carbonate is dried and stored, and the lean solution enters the next step.

[0040] Seventh, evaporate and concentrate the lean liquid, then cool it to 10°C, cool it to separate out the nitrate, remove about 70% of the sodium and sulfur and about 50% of the water, filter it to get sodium sulfate, store it, and return the filtrate to the lithium precipitation step.

[0041] The steps for lithium-free hazardous waste treatment are as follows:

[0042] A. Denitrification of lithium-free hazardous waste to obtain denitrified lithium-free hazardous waste; wherein the denitrification is a conventional water washing (immersion) method, and the nitrogen-containing lithium-free hazardous waste is mainly aluminum ash, and the main nitrogen-containing substance is aluminum nitride, which reacts with water to generate aluminum hydroxide and ammonia;

[0043] B. The denitrification lithium-free hazardous waste is leached with sulfuric acid and then filtered to obtain an aluminum sulfate solution (an aqueous solution of aluminum sulfate 18hydrate) and leached residue. The aluminum sulfate solution is used for leaching and washing floating carbon.

[0044] The experimental technical indicators of this embodiment are as follows:

[0045]

[0046] The homogenized material contains a variety of materials, such as aluminum electrolytic cell overhaul slag, waste cathode, waste electrolyte, electrode blocks, etc., and the table of the present invention only shows two of them that account for a larger proportion (i.e., overhaul slag and cathode carbon); after the treatment of the present invention, the refined carbon yield is 90.5% and the lithium recovery rate is 97.2%.

[0047] Finally, it should be noted that the above is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A comprehensive treatment method for hazardous waste from aluminum plants, It is characterized in that The specific steps include: Step A: Classify hazardous waste to obtain lithium-containing hazardous waste and lithium-free hazardous waste, and store them separately; Step B: The specific treatment steps for lithium-containing hazardous waste include six stages: batching and grinding, flotation and carbon separation, leaching, purification, lithium precipitation and concentrated nitrate separation; wherein the output materials between the leaching, purification, lithium precipitation and concentrated nitrate separation are subjected to circulation / recycling treatment; Step C: The specific treatment steps for non-lithium hazardous waste are as follows: Step C1: denitrifying the lithium-free hazardous waste to obtain denitrified lithium-free hazardous waste; Step C2: leaching the denitrified lithium-free hazardous waste with sulfuric acid and filtering it to obtain an aluminum sulfate solution and leached residue; Wherein, the aluminum sulfate solution in step C2 is applied to the leaching stage of step B; Lithium-containing hazardous waste powder is subjected to flotation separation to obtain floating carbon and floating tail; the grade of the floating carbon is ≥80%; The floating carbon is leached to obtain lithium precious liquid and refined carbon; The lithium precious solution 1 is used as the leaching solution of the floating tail to leach the floating tail to obtain lithium precious solution 2 and leaching residue; The leaching includes pulping pre-leaching, reactor leaching, filter pressing and countercurrent multi-gradient washing; the washing liquid of the countercurrent multi-gradient washing is circulated for pulping pre-leaching and reactor leaching; wherein the reactor leaching temperature is 50°C-95°C; The lithium precious liquid II is purified to obtain purified slag and purified liquid, and the purified slag is mixed with the floating tail and re-leached; wherein, in the purification step, sodium hydroxide and sodium carbonate are used as a combined purifier in a mass ratio of 1:1, the temperature is 50°C-95°C, and the pH value is 7-10; Sodium carbonate is added in batches according to 7-10 times the total amount of lithium in the purified solution to precipitate lithium to obtain lithium carbonate and lean solution; during the lithium precipitation process, the temperature is 50° C.-95° C. and the reaction time is 1-3 hours; The treatment steps of the barren liquid are: first evaporate and concentrate about 50% of the water, cool to below 10°C, remove about 70% of the sodium and sulfur, and filter to obtain sodium sulfate; wherein the denitrified water after denitrification is returned to the lithium precipitation system for recycling.

2. The comprehensive treatment method for hazardous waste from aluminum plants according to claim 1, It is characterized in that In the step B, lithium-containing hazardous waste is ground into lithium-containing hazardous waste powder; the lithium-containing hazardous waste powder has a carbon content of 35wt%±1wt% and a particle size of ≤74μm.

3. The comprehensive treatment method for hazardous waste from aluminum plants according to claim 1, It is characterized in that In the lithium precious solution 2, the concentration of lithium is greater than or equal to 8 g / L.

Citation Information

Patent Citations

  • Regeneration recycling method of electrolytic aluminum overhaul slag and overhaul slag leachate and application method of recycled material

    CN113426796A

  • Aluminum electrolysis dangerous waste residue combined treatment and resource comprehensive utilization method

    CN113426807A