A tear resistance testing device for functional fabric production
By simulating different tearing scenarios and conditions in the fabric detection device, the problem of inconsistency between the detection results and the actual use process in the existing technology is solved, a more accurate and reliable assessment of the fabric's tear resistance performance is achieved, and product quality and users are improved. experience.
Patent Information
- Application Number
- CN202411119089.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-15
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2044-08-15
AI Technical Summary
Existing fabric tear resistance detection devices cannot simulate the different tearing conditions of fabrics during actual use, resulting in errors between the detection results and the actual use process, affecting product quality.
A tear resistance performance testing device for functional fabric production is designed, including a test bench, a first drive component, a clamping block, a rotating component, an extrusion block and an extrusion component. It simulates different tears by changing the shape and position of the crack. Scenarios use extrusion blocks and motors to simulate the tearing of fabrics by different objects to improve the authenticity and accuracy of the test.
By simulating different tearing scenarios and conditions, the reliability and accuracy of test results are improved, helping designers optimize fabric formulas and production processes, and improve product quality and user experience.
Smart Images

Figure CN118654996B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of fabric performance testing devices, and in particular to a tear resistance testing device for functional fabric production. Background Art
[0002] In order to evaluate the durability and quality of fabrics under external forces, it is usually necessary to conduct a tear resistance test on the fabrics. When conducting a tear resistance test on the fabrics, a regular tear is usually cut on the fabric first, and then the test tool is inserted into the tear of the fabric, and the test tool is moved toward both ends to pull and tear the tear on the fabric until the fabric breaks. The tear resistance of the fabric is evaluated through the peak value when the fabric breaks, thereby realizing the tear resistance test of the fabric. However, for clothing, in most cases, when a tear occurs on the clothing and is pulled, the force is usually at both ends of the tear, rather than pulling outward from the inside of the tear, which leads to errors between the test results and the actual use process.
[0003] At the same time, different garments may encounter different tearing situations during actual use, so the cracks on the fabric should be diverse and more realistic. The existing testing method cuts a fixed-shaped crack on the fabric for testing, which makes the test results single and unrepresentative, and cannot simulate the performance of the product in a real environment. Summary of the invention
[0004] In order to overcome the shortcomings of existing detection devices that cannot simulate the tearing of fabrics during actual use, resulting in errors between test results and products during actual use, affecting product quality, the present invention provides a tear resistance detection device for functional fabric production.
[0005] The technical solution of the present invention is: a tear resistance performance detection device for functional fabric production, including a test bench; also including a first drive component, a clamping block, a second drive component, a rotating component, an extrusion block and an extrusion component; the first drive component is installed on the test bench; a plurality of clamping blocks are arranged on the first drive component, and the first drive component is used to drive the clamping block to move left and right; the second drive component is installed on the test bench; a rotating component is installed on the second drive component, and the second drive component is used to drive the rotating component to move left and right; a plurality of extrusion blocks are arranged on the rotating component; each extrusion block is provided with a plurality of contact surfaces for simulating different objects tearing the fabric, and the rotating component is used to drive the extrusion block to rotate to change the contact surface between the extrusion block and the fabric crack; each extrusion block is provided with a smooth portion; each extrusion block is provided with a plurality of hooks; each extrusion block is provided with a tip; each extrusion block is provided with a plurality of curved arc strips; the second drive component is installed with an extrusion component for extruding the fabric.
[0006] Optionally, each extrusion block is configured to be in the shape of an elliptical cylinder.
[0007] Optionally, each clamping block is composed of two mounting blocks that rotate to open and close; and a plurality of rubber strips for increasing friction are arranged on the lower surface of the mounting block above each clamping block.
[0008] Optionally, the shape of the slit cut on the fabric is set to be circular, oval or scratch-shaped.
[0009] Optionally, a heating device is installed inside each extrusion block; each extrusion block is provided with a heating part for burning the crack, the heating part is made of heat-conducting material and is connected to the heating device.
[0010] Optionally, the rotating assembly includes a first motor and a bearing plate; a plurality of first motors are arranged on the movable part of the second driving assembly; the output end of each first motor is fixedly connected to the bearing plate, and each extrusion block is fixedly connected to an adjacent bearing plate.
[0011] Optionally, the extrusion assembly includes a first driving member and a connecting plate; a plurality of first driving members are arranged on the movable part of the second driving assembly, and the first driving member is an electric push rod; the telescopic end of each first driving member is fixedly connected to a connecting plate; and each first motor is fixedly connected to an adjacent connecting plate.
[0012] Optionally, it includes a mounting plate, a second driving member and a partition; a plurality of mounting plates are fixedly connected to each supporting plate; a second driving member is fixedly connected to each mounting plate, and the second driving member is an electric push rod; the telescopic ends of two adjacent second driving members are commonly fixedly connected to a partition for cleaning lines, and each partition is fitted with a side of the extrusion block provided with a hook; a plurality of limiting holes are provided on each partition, and each limiting hole corresponds to the position of an adjacent hook.
[0013] Optionally, a pressing system is also included; the pressing system includes a connecting shaft, an extrusion hook, a second motor, a third drive assembly and an extrusion ring; each clamp block is provided with a first limiting groove on the side close to the extrusion block; a connecting shaft is rotatably connected in each first limiting groove; a number of extrusion hooks are slidably connected to each connecting shaft, and adjacent extrusion hooks are movably connected by springs; a second motor is fixedly connected in each first limiting groove, and the connecting shaft is fixedly connected to the output end of the second motor; a second limiting groove is provided on each clamp block; a third drive assembly is installed in each second limiting groove; and a number of extrusion rings are provided on the third drive assembly.
[0014] Optionally, each extrusion hook end is provided with a protrusion to prevent piercing the fabric.
[0015] The beneficial effects of the present invention are as follows: the present invention realizes that by comparing the test results under different tear shapes, the designer can optimize the formula or production process of the fabric and improve the product quality; by changing the position of the tear on the fabric, the different parts of the clothing that are torn during actual use are simulated, thereby improving the authenticity of the test, and at the same time, it is convenient for the designer to check the uniformity of the entire fabric and make improvements in subsequent product iterations;
[0016] The extrusion block simulates an object piercing the clothing, and the scene simulation of artificially driving the fabric to pull and tear the extrusion block is realized, thereby simulating the tearing of the fabric in different scenarios and improving the reliability of the test results;
[0017] The first motor drives the extrusion block to rotate, thereby changing the contact surface between the extrusion block and the fabric tear, thereby testing the tear resistance of the fabric under different conditions, and obtaining a more comprehensive material performance evaluation;
[0018] By setting the extrusion block in an elliptical column shape, the size of the contact surface between the extrusion block and the fabric tear is changed, thereby assisting in manually determining the true tear strength of the fabric and improving the accuracy of the test;
[0019] The heating part of the extrusion block is used to squeeze the area around the tear in the fabric, thereby simulating the tearing of the elbows or knees of people's clothes after falling during exercise, further improving the authenticity of the test data. At the same time, targeted tear resistance tests are carried out on some parts of the fabric to improve the overall quality of the clothing and user experience. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 This is a schematic diagram of the three-dimensional structure of the tear resistance testing device for functional fabric production of the present invention;
[0021] Figure 2 It is a schematic diagram of the combined three-dimensional structure of the clamping block and the extrusion block of the present invention;
[0022] Figure 3 It is a schematic diagram of the three-dimensional structure of the first driving assembly, the clamping block and the extrusion block of the present invention;
[0023] Figure 4 It is a schematic diagram of the three-dimensional structure of the clamping block of the present invention;
[0024] Figure 5 It is a schematic diagram of the combined three-dimensional structure of the extrusion block and the rotating assembly of the present invention;
[0025] Figure 6 It is a schematic diagram of the three-dimensional structure of the extrusion block of the present invention;
[0026] Figure 7 It is a schematic diagram of the combined three-dimensional structure of the extrusion block, the mounting plate and the partition plate of the present invention;
[0027] Figure 8 It is a schematic diagram of the three-dimensional structure of the pressing system of the present invention;
[0028] Fig. 9 It is a schematic diagram of the three-dimensional structure of the extrusion hook and extrusion ring combination of the present invention.
[0029] Markings in the accompanying drawings: 1-test bench, 2-clamping block, 2001-rubber strip, 2002-first limiting groove, 2003-second limiting groove, 3-extrusion block, 3001-smooth part, 3002-bending hook, 3003-tip, 3004-bending strip, 3005-heating part, 4-fabric, 101-first slide rail, 102-first electric slider, 201-second slide rail, 202-second electric slider, 203-connecting block, 204-fixing plate, 205-first motor, 206-carrying plate, 301-first driving member, 302-connecting plate, 401-mounting plate, 402-second driving member, 403-partition, 501-connecting shaft, 502-extrusion hook, 50201-convex part, 503-second motor, 504-third slide rail, 505-third electric slider, 506-extrusion ring. DETAILED DESCRIPTION
[0030] The following descriptions are merely preferred embodiments of the present invention and are not intended to limit the protection scope of the present invention.
[0031] Example 1
[0032] A tear resistance testing device for the production of functional fabrics 4, such as Figure 1-Figure 6 As shown, a test bench 1 is included;
[0033] It also includes a first driving component, a clamping block 2, a second driving component, a rotating component, an extrusion block 3 and an extrusion component; the first driving component is installed on the test bench 1; two left-right symmetrical clamping blocks 2 are arranged on the first driving component; the second driving component is installed on the test bench 1; the rotating component is installed on the second driving component; two extrusion blocks 3 are arranged on the rotating component; each extrusion block 3 is provided with a plurality of contact surfaces; each extrusion block 3 is provided with a smooth portion 3001; each extrusion block 3 is provided with a plurality of hooks 3002; each extrusion block 3 is provided with a tip 3003; each extrusion block 3 is provided with a plurality of curved arc bars 3004; the extrusion component is installed on the second driving component.
[0034] Each extrusion block 3 is configured to be in the shape of an elliptical column.
[0035] Each clamping block 2 is composed of two mounting blocks that rotate to open and close; a plurality of rubber strips 2001 are provided on the lower surface of the mounting block above each clamping block 2 .
[0036] The shape of the slit cut on the fabric 4 is set to be circular, oval or scratched. A heating device is installed inside each extrusion block 3; each extrusion block 3 is provided with a heating part 3005, which is made of heat-conducting material and connected to the heating device.
[0037] The first driving assembly includes a first slide rail 101 and a first electric slider 102 ; the first slide rail 101 is fixedly connected to the test bench 1 ; each first slide rail 101 is slidably connected to two first electric sliders 102 , and each clamping block 2 is fixedly connected to an adjacent first electric slider 102 .
[0038] The second driving assembly includes a second slide rail 201, a second electric slider 202, a connecting block 203 and a fixed plate 204; the second slide rail 201 is fixedly connected to the test bench 1; two second electric sliders 202 are slidably connected to the second slide rail 201; each second electric slider 202 is fixedly connected to a connecting block 203; each connecting block 203 is fixedly connected to a fixed plate 204, and each fixed plate 204 is connected to a corresponding rotating assembly.
[0039] The rotating assembly includes a first motor 205 and a supporting plate 206; each fixed plate 204 is connected to a first motor 205; the output end of each first motor 205 is fixedly connected to the supporting plate 206, and each extrusion block 3 is fixedly connected to the adjacent supporting plate 206, and the first motor 205 drives the supporting plate 206 and the extrusion block 3 to rotate.
[0040] The extrusion assembly includes a first driving member 301 and a connecting plate 302; each connecting block 203 is fixedly connected to a first driving member 301, and the first driving member 301 is an electric push rod; the telescopic end of each first driving member 301 is fixedly connected to a connecting plate 302; each first motor 205 is fixedly connected to an adjacent connecting plate 302, and each first motor 205 is slidably connected to an adjacent fixed plate 204, and the first motor 205 and the connecting plate 302 are driven to move up and down by the first driving member 301.
[0041] The working steps of this embodiment are:
[0042] In the first step, the fabrics 4 to be tested are manually cut to size, and then rips are cut on the fabrics 4 according to the test requirements. In order to simulate different tearing conditions of clothing during actual use, the rips are cut into circular or elliptical shapes. Such rips simulate small holes in the clothing or local damage caused by wear and tear. Or the rips are cut into irregular shapes, such as sharp angles, curves or jagged edges, so as to more realistically simulate the scene when the clothing is accidentally torn or worn. At the same time, the position of the rips on the fabric 4 is changed, so that the test results are more in line with reality and the reliability of the test data is improved.
[0043] In the second step, the clamp blocks 2 are controlled to open, and the two ends of the fabric 4 are placed on adjacent clamp blocks 2 respectively. Then the clamp blocks 2 are controlled to close so that the clamp blocks 2 clamp and fix the two ends of the fabric 4. At this time, the fabric 4 between the two clamp blocks 2 is in a relaxed state.
[0044] In the third step, after the fabric 4 is fixed, there are two testing methods. The first method is to pull the fabric 4 from both ends. The second method is to pull the fabric 4 from the cracks on the fabric 4 to both ends.
[0045] The following is the first test method: first, control the first electric slider 102 to drive the adjacent clamping blocks 2 to move to the left and right respectively, so that the two clamping blocks 2 pull and tear the fabric 4, and the test bench 1 records the data until the fabric 4 breaks and the test is completed, control the first electric slider 102 to drive the adjacent clamping blocks 2 back to the original position, then remove the broken fabric 4 from the clamping block 2, and fix the next fabric 4 to be tested on the clamping block 2, and then repeat the above test steps; increase the friction between the fabric 4 and the clamping block 2 through the rubber strip 2001 on the clamping block 2, thereby preventing the fabric 4 from being separated from the clamping block 2 during the pulling and tearing of the fabric 4 by the clamping block 2, thereby affecting the test results.
[0046] When the two clamps 2 pull and tear the fabric 4, according to the situation in the first step, firstly, multiple tests are carried out according to the different crack shapes. By comparing the test results under different crack shapes, it is convenient for designers to optimize the formula or production process of the fabric 4 and improve product quality; then different positions of the same crack shape are tested respectively, and multiple situations are discussed at this time. The first situation is: the crack is located in the middle of the two clamps 2; the second situation is: the crack position is closer to the left clamp 2; the third situation is: the crack position is closer to the right clamp 2;
[0047] By changing the position of the tear on the fabric 4 to simulate different parts of the clothing being torn during actual use, the authenticity of the test is improved, and it is convenient for designers to check the uniformity of the entire fabric 4 and make improvements in subsequent product iterations.
[0048] The fourth step is that when people are engaged in outdoor activities, such as climbing, and their clothes are pierced by objects and cracks are created, they usually first move the clothes manually, so that the clothes drive the objects that penetrate into the cracks in the clothes to move. At this time, the object is in a passive state and pulls the cracks in the clothes. In order to make the tear resistance test results of the fabric 4 more in line with reality, the second electric slider 202 is controlled to drive the extrusion block 3, the connecting block 203 and the fixing plate 204 to move into the crack of the fabric 4, and then the first electric slider 102 is controlled to drive the clamping block 2 and the fabric 4 to move to the left or right together, so that the fabric 4 squeezes the adjacent extrusion block 3, and the extrusion block 3 simulates the object that pierces the clothes, so as to realize the scene simulation of artificially driving the fabric 4 to pull and tear the extrusion block 3, thereby simulating the tearing of the fabric 4 in different scenes and improving the reliability of the test results.
[0049] Step 5. The following is the second test method, that is, pulling from the crack on the fabric 4 to both ends: the initial position of the extrusion block 3 and the second electric slider 202 is located at the left end or the right end of the second slide rail 201. When the fabric 4 is fixed, the second electric slider 202 is controlled to drive the extrusion block 3, the connecting block 203 and the fixing plate 204 to move into the crack of the fabric 4. Then, the two second electric sliders 202 are controlled to drive the corresponding extrusion blocks 3 to move in opposite directions, and the crack on the fabric 4 is pulled and torn. The test data is recorded through the test bench 1. After the fabric 4 breaks, the test is completed, and the second electric slider 202 is controlled to drive the extrusion block 3, the connecting block 203 and the fixing plate 204 to move to the initial position, and the broken fabric 4 is removed, and a new fabric 4 is replaced on the clamping block 2. Then, the above steps are repeated to start the test.
[0050] When the extrusion block 3 pulls and tears the crack on the fabric 4, in order to simulate the tearing of the crack by different objects, the first motor 205 is first controlled to rotate, and the extrusion block 3 and the carrier plate 206 are driven to rotate together, so that the contact surface on the extrusion block 3 contacts the crack of the fabric 4 respectively, and the fabric 4 is pulled and torn. At this time, there are multiple situations for discussion. The first situation is: the smooth part 3001 of the extrusion block 3 contacts the crack of the fabric 4, so as to simulate the tearing of the crack of the fabric 4 by an object with a smooth surface;
[0051] The second situation is: the side of the extrusion block 3 provided with the hook 3002 is in contact with the tear of the fabric 4, so as to simulate the tearing situation of the tear of the fabric 4 pulled by a sharp object such as a thorn;
[0052] The third situation is: the tip 3003 of the squeezing block 3, which is arranged in the shape of a table corner, is in contact with the tear of the fabric 4, so as to simulate the tearing of the clothes caused by the squeezing and pulling of the table corner when people are wearing clothes and walking;
[0053] The fourth situation is: the curved strip 3004 of the extrusion block 3 is brought into contact with the tear of the fabric 4, thereby simulating the tearing of the fabric 4 by an object with a rough surface penetrating into the tear of the clothing;
[0054] Before the fabric 4 contacts the extrusion block 3, the extrusion block 3 is driven to rotate by the first motor 205 to change the contact surface between the extrusion block 3 and the crack of the fabric 4, thereby testing the tear resistance of the fabric 4 under different conditions and obtaining a more comprehensive material performance evaluation. At the same time, since some specific types of fabrics 4 react differently to contact surfaces of different sizes, the extrusion block 3 is set in an elliptical column shape to change the size of the contact surface between the extrusion block 3 and the crack of the fabric 4, thereby assisting in manually determining the true tear strength of the fabric 4 and improving the accuracy of the test.
[0055] Step 6. Secondly, for some fabrics 4 that are more sensitive to temperature, in order to make the cracks on the fabrics 4 more realistic, after the fabrics 4 are fixed, the second electric slider 202 is controlled to drive the extrusion block 3, the connecting block 203 and the fixing plate 204 to move into the crack of the fabric 4, and the first driving member 301 is controlled to drive the first motor 205 and the connecting plate 302 to move downward, so that the heating part 3005 of the extrusion block 3 and the crack of the fabric 4 are located at the same height, and then the heating device is started to transfer heat to the heating part 3005, so that the part of the fabric 4 that contacts the heating part 3005 is melted and a small hard lump is generated, and then the heating device is turned off, and then the tear resistance test is completed according to the above steps to simulate the reaction of people's clothes when encountering high temperature during cooking, and then the crack of the fabric 4 is pulled and torn, so as to detect whether the fabric 4 can maintain sufficient strength after the burning treatment, and whether it can resist tearing when subjected to external force, so that the designer can optimize the material of the fabric 4.
[0056] Step 7. When people fall during exercise, the clothes at the elbows and knees usually rub against the ground and become damaged. When people fall, their elbows and knees are usually bent, so the clothes will not only be pulled, but also squeezed by the elbow and knee joints. Therefore, when performing tear resistance test on fabric 4, in order to ensure the durability and safety of the clothes, it is necessary to focus on testing the elbows and knees of the clothes.
[0057] In the third step of the above process: when the two clamping blocks 2 pull and tear the fabric 4, the first driving member 301 is controlled to drive the first motor 205 and the extrusion block 3 to move upward until the heating part 3005 of the extrusion block 3 squeezes the upper fabric 4, and at the same time, the second electric slider 202 is controlled to drive the extrusion block 3 to move around the tear in the fabric 4, so that the heating part 3005 of the extrusion block 3 squeezes the fabric 4 around the tear, thereby simulating the tearing of the elbows or knees of people's clothes after they fall during exercise, further improving the authenticity of the test data, and at the same time, by conducting targeted tear resistance tests on some parts of the fabric 4, the overall quality of the clothing and user experience are improved.
[0058] Example 2
[0059] On the basis of Example 1, Figure 1 , Figure 2 and Figure 7-Figure 9 As shown, it includes a mounting plate 401, a second driving member 402 and a partition 403; each supporting plate 206 is fixedly connected to two left-right symmetrical mounting plates 401; each mounting plate 401 is fixedly connected to a second driving member 402, and the second driving member 402 is an electric push rod; the telescopic ends of two adjacent second driving members 402 are commonly fixedly connected to a partition 403, and each partition 403 is fitted with a side of the extrusion block 3 on which a hook 3002 is provided; each partition 403 is provided with a plurality of limiting holes, and each limiting hole corresponds to the position of an adjacent hook 3002.
[0060] It also includes a pressing system; the pressing system includes a connecting shaft 501, an extrusion hook 502, a second motor 503, a third drive assembly and an extrusion ring 506; each clamping block 2 is provided with a first limiting groove 2002 on the side close to the extrusion block 3; each first limiting groove 2002 is rotatably connected with a connecting shaft 501; each connecting shaft 501 is slidably connected with five extrusion hooks 502, and adjacent extrusion hooks 502 are movably connected by springs; each first limiting groove 2002 is fixedly connected with a second motor 503, and the connecting shaft 501 is fixedly connected to the output end of the second motor 503; each clamping block 2 is provided with a second limiting groove 2003; each second limiting groove 2003 is installed with a third drive assembly; four extrusion rings 506 are provided on the third drive assembly.
[0061] The third driving assembly includes a third slide rail 504 and a third electric slider 505; a third slide rail 504 is fixedly connected to the second limiting groove 2003 of each clamping block 2; two third electric sliders 505 are slidably connected to each third slide rail 504, and each extrusion ring 506 is fixedly connected to the adjacent third electric slider 505.
[0062] Each extrusion hook 502 is provided with a protrusion 50201 at the end thereof.
[0063] The working principle of this embodiment is:
[0064] In the fifth step of Example 1: when one side of the extrusion block 3 provided with the hook 3002 contacts the crack of the fabric 4 and pulls the crack of the fabric 4 to the left and right, some fibers on the fabric 4 will be entangled on the hook 3002. Over time, as the fibers accumulate on the hook 3002, the tearing effect of the hook 3002 on the fabric 4 will be affected. To avoid the above situation, after the test is completed, the fabric 4 is removed from the clamping block 2, and the second driving member 402 is controlled to drive the adjacent partition plate 403 to move away from the extrusion block 3, and the fibers entangled on the hook 3002 are scraped and cleaned by the partition plate 403, thereby preventing the fibers from accumulating for a long time and affecting the tearing effect of the hook 3002 of the extrusion block 3 on the fabric 4.
[0065] In the third step of Example 1: Clothes usually develop wrinkles due to body movements during wearing, but the existing fabric 4 tear resistance detection device usually tests the fabric 4 in an unfolded state, which cannot match the actual usage situation, resulting in a lack of authenticity in the test data.
[0066] In order to solve the above-mentioned problem and increase the authenticity of the test, according to the test requirements, the second motor 503 is controlled to drive the extrusion hook 502 to rotate toward the side of the fabric 4, so that the extrusion hook 502 squeezes the fabric 4 below, thereby making the squeezed part of the fabric 4 concave downward, and then the third electric slider 505 is controlled to drive the adjacent extrusion rings 506 to move toward the middle of the clamping block 2, so that the extrusion rings 506 squeeze the adjacent extrusion hooks 502. Since the adjacent extrusion hooks 502 are connected by springs, the adjacent extrusion hooks 502 will gradually move closer to the middle.
[0067] At the same time, the downwardly concave parts of the fabric 4 will be brought closer together to form wrinkles on the fabric 4, and then the first electric slider 102 will be controlled to drive the adjacent clamping blocks 2 to move to the left and right respectively, so that the two clamping blocks 2 will pull and tear the wrinkled fabric 4, and record the test data until the fabric 4 breaks and the test ends.
[0068] Then, the third electric slider 505 is controlled to drive the squeezing ring 506 to move to the original position. At this time, the adjacent squeezing hooks 502 are reset to the initial position through the rebound of the spring, and then the broken fabric 4 is removed and the next fabric 4 is tested; the squeezing hook 502 is driven to rotate by the second motor 503, so that the squeezing hook 502 squeezes the fabric 4 to make it concave downward, and then the squeezing ring 506 is driven by the third electric slider 505 to squeeze the adjacent squeezing hooks 502, so that the adjacent squeezing hooks 502 are brought closer to each other, so that the fabric 4 forms a wrinkle, thereby simulating the tearing of clothes after being pulled during actual wearing, and further improving the reliability of the test results. At the same time, when wrinkles are formed on the fabric 4, the weak strength of certain areas of the fabric 4 will be exposed. Discovering these potential tearing points by pulling will help the manufacturer of the fabric 4 to optimize the material or process.
[0069] When the extrusion hook 502 squeezes the fabric 4, the convex portion 50201 reduces the extrusion force of the extrusion hook 502 on the fabric 4 to prevent the extrusion hook 502 from piercing the fabric 4, resulting in additional tearing force on the fabric 4 when the clamp 2 subsequently pulls the fabric 4, thereby avoiding affecting the accuracy of the test results.
[0070] The above is only a specific embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Any person skilled in the art can easily think of changes or substitutions within the technical scope disclosed by the present invention, which should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention should be based on the protection scope of the claims.
Claims
1. A tear resistance testing device for functional fabric production, comprising a test bench (1); characterized in that: The test bench (1) also includes a first drive assembly, a clamping block (2), a second drive assembly, a rotating assembly, an extrusion block (3) and an extrusion assembly; the first drive assembly is mounted on the test bench (1); a plurality of clamping blocks (2) are arranged on the first drive assembly, and the first drive assembly is used to drive the clamping block (2) to move left and right; the second drive assembly is mounted on the test bench (1); a rotating assembly is mounted on the second drive assembly, and the second drive assembly is used to drive the rotating assembly to move left and right; a plurality of extrusion blocks (3) are arranged on the rotating assembly; each extrusion block (3) is provided with a plurality of The plurality of extrusion blocks (3001) are used to simulate the contact surfaces of different objects tearing the fabric (4); the rotating assembly is used to drive the extrusion block (3) to rotate so as to change the contact surface between the extrusion block (3) and the tear of the fabric (4); each extrusion block (3) is provided with a smooth portion (3001); each extrusion block (3) is provided with a plurality of hooks (3002); each extrusion block (3) is provided with a tip (3003); each extrusion block (3) is provided with a plurality of curved arc strips (3004); and an extrusion assembly for extruding the fabric (4) is installed on the second driving assembly; The rotating assembly comprises a first motor (205) and a bearing plate (206); a plurality of first motors (205) are arranged on the movable part of the second driving assembly; the output end of each first motor (205) is fixedly connected to the bearing plate (206), and each extrusion block (3) is fixedly connected to an adjacent bearing plate (206); The extrusion assembly comprises a first driving member (301) and a connecting plate (302); a plurality of first driving members (301) are arranged on the movable part of the second driving assembly, and the first driving members (301) are electric push rods; the telescopic end of each first driving member (301) is fixedly connected to the connecting plate (302); each first motor (205) is fixedly connected to an adjacent connecting plate (302); It also includes a mounting plate (401), a second driving member (402) and a partition (403); each bearing plate (206) is fixedly connected to a plurality of mounting plates (401); each mounting plate (401) is fixedly connected to a second driving member (402), and the second driving member (402) is an electric push rod; the telescopic ends of two adjacent second driving members (402) are commonly fixedly connected to a partition (403) for cleaning lines, and each partition (403) is in contact with a side of the extrusion block (3) on which a hook (3002) is provided; each partition (403) is provided with a plurality of limiting holes, and each limiting hole corresponds to the position of an adjacent hook (3002); The pressing system also includes a pressing system, which includes a connecting shaft (501), an extrusion hook (502), a second motor (503), a third driving component and an extrusion ring (506); each clamping block (2) is provided with a first limiting groove (2002) on the side close to the extrusion block (3); each first limiting groove (2002) is rotatably connected with a connecting shaft (501); each connecting shaft (501) is slidably connected with a plurality of extrusion hooks (502), and adjacent extrusion hooks (502) are movably connected via springs; each first limiting groove (2002) is fixedly connected with a second motor (503), and the connecting shaft (501) is fixedly connected to the output end of the second motor (503); each clamping block (2) is provided with a second limiting groove (2003); each second limiting groove (2003) is installed with a third driving component; and the third driving component is provided with a plurality of extrusion rings (506).
2. The tear resistance testing device for functional fabric production according to claim 1, characterized in that: Each extrusion block (3) is configured in the shape of an elliptical column.
3. The tear resistance testing device for functional fabric production according to claim 1, characterized in that: Each clamping block (2) is composed of two mounting blocks that rotate to open and close; a plurality of rubber strips (2001) for increasing friction are arranged on the lower surface of the mounting block above each clamping block (2).
4. The tear resistance testing device for functional fabric production according to claim 1, characterized in that: The shape of the slit cut on the fabric (4) is set to be circular, elliptical or scratched.
5. The tear resistance testing device for functional fabric production according to claim 1, characterized in that: A heating device is installed inside each extrusion block (3); a heating portion (3005) for burning the crack is provided on each extrusion block (3); the heating portion (3005) is made of a heat-conducting material and is connected to the heating device.
6. The tear resistance testing device for functional fabric production according to claim 1, characterized in that: Each extrusion hook (502) is provided at the end with a convex portion (50201) for preventing the fabric (4) from being pierced.