Substrate wiring structure and preparation method thereof

By adding metal layers on the circumference of the pad and setting grooves and metal columns on the dielectric layer, the problems of structural fracture caused by insufficient pad thickness and wiring trace cracking caused by excessive thickness are solved, and the reliability of the pad is improved. The bonding force prevents structural stratification and cracking.

CN118676110BActive Publication Date: 2024-11-01FOREHOPE SEMICONDUCTOR (NINGBO) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411162762.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-23
Publication Date
2024-11-01
Estimated Expiration
2044-08-23

AI Technical Summary

Technical Problem

In the 2.5D packaging structure, insufficient pad thickness can easily lead to structural fracture, and excessive thickness will cause large morphology of the dielectric layer to cause cracking of wiring traces.

Method used

A substrate wiring structure is designed, by adding a first metal layer and a second metal layer to the circumference of the pad, and providing grooves and metal columns on the dielectric layer, the thickness and bonding force of the pad are improved, and the structure is prevented from being divided. layer and cracking.

Benefits of technology

Improve the reliability of the pad, reduce the risk of breakdown or breaking during reliability tests, enhance the bonding force between the pad and the dielectric layer, and prevent cracking problems caused by the surface undulation of the wiring layer.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118676110B_ABST
    Figure CN118676110B_ABST
Patent Text Reader

Abstract

The present application provides a substrate wiring structure and a preparation method thereof, and relates to the field of semiconductor technology. The substrate wiring structure includes a pad, a dielectric layer, a wiring layer, a bump, a first metal layer, and a second metal layer. The pad has a first surface and a second surface arranged opposite to each other, and a peripheral side surface connecting the first surface and the second surface. The pad is arranged in the dielectric layer; the dielectric layer is provided with a first groove exposing a portion of the first surface, and a second groove exposing a portion of the second surface. The wiring layer is arranged in the first groove and extends to the surface of the dielectric layer; the wiring layer and the pad are electrically connected. The bump is arranged in the second groove and exposes the surface of the dielectric layer away from the wiring layer; the bump and the pad are electrically connected. The first metal layer covers a portion of the peripheral side surface and a portion of the first surface, and the first metal layer is electrically connected to the wiring layer. The second metal layer covers a portion of the peripheral side surface and a portion of the second surface, and the second metal layer is electrically connected to the bump. Improve the reliability of the substrate structure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a substrate wiring structure and a preparation method thereof. Background Art

[0002] There are a large number of integrated chips in the 2.5D packaging structure, and organic materials are usually used as substrates for chip mounting. In the substrate process, the circuit layer is redistributed on the seed layer on the surface of the pad to change the original chip circuit contact position (input / output solder joint position). If the pad thickness is too thin, it is easy to continuously form intermetallic compounds IMC (Intermetallic Compound) during the reliability test, resulting in structural fracture. If the pad thickness is large, when a thicker copper layer is used to expose and develop the dielectric layer, the morphology of the dielectric layer surface fluctuates greatly, which will cause the wiring traces in the redistribution structure of the dielectric layer to crack easily due to large morphology fluctuations. Summary of the invention

[0003] The objects of the present invention include, for example, providing a substrate wiring structure and a method for preparing the same, which can prevent the pads from breaking through or breaking during reliability testing, and can also avoid delamination or cracking of rewiring wiring traces.

[0004] The embodiments of the present invention can be implemented as follows:

[0005] In a first aspect, the present invention provides a substrate wiring structure, comprising:

[0006] A pad having a first surface and a second surface arranged opposite to each other, and a peripheral side surface connecting the first surface and the second surface;

[0007] A dielectric layer, wherein the pad is disposed in the dielectric layer; the dielectric layer is provided with a first groove exposing a portion of the first surface, and a second groove exposing a portion of the second surface;

[0008] A wiring layer, the wiring layer is arranged in the first groove and extends to the surface of the dielectric layer; the wiring layer is electrically connected to the pad;

[0009] A bump, the bump being arranged in the second groove and exposing a surface of the dielectric layer away from the wiring layer; the bump being electrically connected to the pad;

[0010] a first metal layer, the first metal layer covering a portion of the peripheral side surface and a portion of the first surface, the first metal layer being electrically connected to the wiring layer;

[0011] A second metal layer covers a portion of the peripheral side surface and a portion of the second surface, and the second metal layer is electrically connected to the bump.

[0012] In an optional embodiment, a first seed layer is further included; the groove wall of the first groove includes a first side surface, a step surface and a second side surface connected in sequence; the first side surface is connected to the first surface;

[0013] The first seed layer is arranged along the groove wall of the first groove, the first seed layer covers the first side surface, the step surface and a part of the second side surface, and the first seed layer is lower than the notch of the first groove;

[0014] The first metal layer is electrically connected to a first seed layer covering the first side surface, and the first metal layer and the first seed layer covering the step surface are spaced apart.

[0015] In an optional embodiment, the first metal layer and the second metal layer are symmetrically arranged about the pad;

[0016] And / or, the first groove and the second groove are symmetrically arranged with respect to the pad;

[0017] And / or, a second seed layer is disposed in the second groove, and the first seed layer and the second seed layer are symmetrically arranged with respect to the pad.

[0018] In an optional embodiment, it further includes a first metal column disposed in the first groove, the first metal column is connected to the first surface and is spaced apart from the first seed layer;

[0019] And / or, it also includes a second metal column disposed in the second groove, the second metal column is connected to the second surface and is spaced apart from the second seed layer.

[0020] In an optional embodiment, the first surface is provided with a plurality of spaced-apart first metal pillars, and the plurality of first metal pillars have different heights;

[0021] And / or, a side of the first metal column away from the first surface is lower than a side of the first seed layer away from the first surface.

[0022] In an optional embodiment, a roughening groove is provided on a side of the wiring layer away from the pad surface.

[0023] In an optional embodiment, the first metal layer and the second metal layer are in contact on the peripheral side surface;

[0024] And / or, one end of the first metal layer away from the peripheral side surface is an inclined surface, and the cross-sectional area of ​​the first metal layer gradually increases from one end close to the second metal layer to one end away from the second metal layer.

[0025] In an optional embodiment, a third seed layer is provided between the second surface and the bump.

[0026] In an optional embodiment, the bump includes a connecting portion and a ball portion, the connecting portion is electrically connected to the pad, the ball portion is connected to the connecting portion, and a roughened portion is provided on a side of the connecting portion close to the ball portion.

[0027] In a second aspect, the present invention provides a preparation method for preparing a substrate wiring structure as described in any one of the aforementioned embodiments.

[0028] The beneficial effects of the embodiments of the present invention include, for example:

[0029] The substrate wiring structure provided by the embodiment of the present invention has a first metal layer and a second metal layer added to the peripheral side of the pad, and the first metal layer covers part of the first surface of the pad, and the second metal layer covers part of the second surface of the pad. This not only increases the thickness of the pad, improves the reliability of the pad structure, and reduces the risk of breakdown or fracture in reliability testing. At the same time, it improves the bonding force between the pad and the dielectric layer, prevents structural delamination, and can also prevent the wiring layer from cracking due to the large surface fluctuations of the dielectric layer.

[0030] The method for preparing a substrate wiring structure provided by an embodiment of the present invention is used to prepare the above-mentioned substrate wiring structure, which can improve the reliability of the pad, improve the bonding strength between the pad and the dielectric layer, and prevent the wiring layer from cracking due to large undulations on the surface of the dielectric layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for use in the embodiments are briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present invention and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work.

[0032] Figure 1 A schematic diagram of a first structural example of a substrate wiring structure provided by an embodiment of the present invention;

[0033] Figure 2 A schematic structural diagram of a first groove of a dielectric layer in a substrate wiring structure provided by an embodiment of the present invention;

[0034] Figure 3 A second structural schematic diagram of a substrate wiring structure provided by an embodiment of the present invention;

[0035] Figure 4 A third structural schematic diagram of a substrate wiring structure provided by an embodiment of the present invention;

[0036] Figure 5 A fourth structural schematic diagram of a substrate wiring structure provided by an embodiment of the present invention;

[0037] Figure 6 A fifth structural schematic diagram of a substrate wiring structure provided by an embodiment of the present invention;

[0038] Figure 7 A sixth structural schematic diagram of a substrate wiring structure provided by an embodiment of the present invention;

[0039] Figure 8 A seventh structural schematic diagram of a substrate wiring structure provided by an embodiment of the present invention;

[0040] Fig. 9 A schematic diagram of the structure of a substrate wiring structure provided by an embodiment of the present invention for mounting a chip;

[0041] Figures 10 to 15 A schematic diagram of a process for manufacturing a substrate wiring structure provided by an embodiment of the present invention;

[0042] Fig.16 A schematic diagram of the manufacturing process of the welding pad of the substrate wiring structure provided by an embodiment of the present invention.

[0043] Icons: 100-substrate wiring structure; 110-pad; 111-first surface; 112-second surface; 113-side surface; 120-dielectric layer; 130-first groove; 131-first side surface; 132-step surface; 133-second side surface; 140-second groove; 150-wiring layer; 151-roughened groove; 152-pad; 160-bump; 161-connecting part; 162-ball part; 163-roughened part; 101-first metal layer; 102-second metal layer; 10 3-first seed layer; 104-second seed layer; 105-first metal pillar; 106-second metal pillar; 107-third seed layer; 210-chip; 220-solder point; 201-carrier; 202-glue layer; 203-aluminum layer; 121-first dielectric layer; 1211-first annular groove; 1212-dielectric platform; 122-second dielectric layer; 123-third dielectric layer; 124-fourth dielectric layer; 1241-second annular groove; 125-fifth dielectric layer; 126-sixth dielectric layer. DETAILED DESCRIPTION

[0044] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Generally, the components of the embodiments of the present invention described and shown in the drawings here can be arranged and designed in various different configurations.

[0045] Therefore, the following detailed description of the embodiments of the present invention provided in the accompanying drawings is not intended to limit the scope of the invention claimed for protection, but merely represents selected embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0046] It should be noted that similar reference numerals and letters denote similar items in the following drawings, and therefore, once an item is defined in one drawing, further definition and explanation thereof is not required in subsequent drawings.

[0047] In the description of the present invention, it should be noted that if the terms "upper", "lower", "inside", "outside", etc. appear to indicate an orientation or position relationship, they are based on the orientation or position relationship shown in the accompanying drawings, or are the orientation or position relationship in which the product of the invention is usually placed when used. They are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.

[0048] In addition, the terms “first”, “second”, etc., if used, are merely used to distinguish between the descriptions and should not be understood as indicating or implying relative importance.

[0049] It should be noted that, in the absence of conflict, the features in the embodiments of the present invention may be combined with each other.

[0050] Please refer to Figure 1, this embodiment provides a substrate wiring structure 100, including a pad 110, a dielectric layer 120, a wiring layer 150, a bump 160, a first metal layer 101 and a second metal layer 102. The pad 110 has a first surface 111 and a second surface 112 arranged opposite to each other, and a peripheral side surface 113 connecting the first surface 111 and the second surface 112. The pad 110 is arranged in the dielectric layer 120; the dielectric layer 120 is provided with a first groove 130 exposing a portion of the first surface 111 and a second groove 140 exposing a portion of the second surface 112. The wiring layer 150 is arranged in the first groove 130 and extends to the surface of the dielectric layer 120. In this embodiment, the wiring layer 150 protrudes from the surface of the dielectric layer 120. The wiring layer 150 and the pad 110 are electrically connected. The bump 160 is arranged in the second groove 140 and exposes the surface of the dielectric layer 120 away from the wiring layer 150. The bump 160 and the pad 110 are electrically connected. The first metal layer 101 covers part of the peripheral side surface 113 and part of the first surface 111, and the first metal layer 101 is electrically connected to the wiring layer 150. The second metal layer 102 covers part of the peripheral side surface 113 and part of the second surface 112, and the second metal layer 102 is electrically connected to the bump 160. This arrangement not only increases the thickness of the pad 110, improves the structural reliability of the pad 110, and reduces the risk of breakdown or fracture in reliability testing. At the same time, it improves the bonding force between the pad 110 and the dielectric layer 120, prevents structural delamination, and can also prevent the wiring layer 150 from cracking due to the large surface undulations of the dielectric layer 120.

[0051] It can be understood that if the thickness of the pad 110 is relatively thin, the pad 110 is easily broken down during the reliability test, resulting in a short circuit in the circuit and inability to perform electrical testing. Also, during the welding process between the pad 110 and the solder ball, intermetallic compounds are continuously formed and part of the pad 110 is consumed, resulting in welding delamination and leakage current. In this embodiment, a first metal layer 101 and a second metal layer 102 are provided to increase the thickness of the pad 110, improve the structural reliability, and prevent the pad 110 from being broken down and short-circuited during electrical testing. It is also beneficial to improve the bonding force between the pad 110 and the dielectric layer 120 and between the pad 110 and the wiring layer 150.

[0052] The first metal layer 101 and the second metal layer 102 are conducive to increasing the current and voltage transmission area of ​​the pad 110 for electrical transmission, thereby improving the electrical performance of the pad 110, and the first metal layer 101 and the second metal layer 102 wrap the pad 110 from the peripheral side surface 113 of the pad 110, which effectively protects the pad 110. In addition, the first metal layer 101 and the second metal layer 102 are respectively arranged on the upper and lower sides of the pad 110, which is conducive to balancing the stress on both sides of the pad 110, and the structure is reliable, reducing structural stress, and preventing delamination. Optionally, the cross-sections of the first metal layer 101 and the second metal layer 102 are respectively trapezoidal.

[0053] Combination Figure 2 The dielectric layer 120 includes a first dielectric layer 121 and a second dielectric layer 122. The first dielectric layer 121 covers the pad 110, and the thickness of the first dielectric layer 121 is greater than the thickness of the pad 110. The first dielectric layer 121 is provided with a first annular groove 1211 (see Fig.10 ), the bottom of the first annular groove 1211 exposes part of the peripheral side surface 113 and part of the first surface 111 of the pad 110. The depth of the first annular groove 1211 is less than the thickness of the first dielectric layer 121. The groove wall of the first annular groove 1211 is inclined so that the groove gradually widens. The first metal layer 101 fills the first annular groove 1211.

[0054] Optionally, the substrate wiring structure 100 further includes a first seed layer 103 and a second seed layer 104. Of course, the first seed layer 103 and the second seed layer 104 can be set selectively or simultaneously, which is not specifically limited here. The second dielectric layer 122 covers the first dielectric layer 121. The first groove 130 penetrates the second dielectric layer 122 and a portion of the first dielectric layer 121 to expose the first surface 111 of the pad 110. It can be understood that the first surface 111 of the pad 110 exposed by the first groove 130 is the remaining first surface 111 except for the first metal layer 101.

[0055] The groove wall of the first groove 130 includes a first side surface 131, a step surface 132, and a second side surface 133 connected in sequence. The first side surface 131 is connected to the first surface 111 of the pad 110. The first side surface 131 is inclined so that the notch of the first groove 130 gradually increases. The step surface 132 is approximately horizontally arranged, connected to one end of the first side surface 131 away from the first surface 111, and extends to the outside of the notch. The second side surface 133 is connected to the side of the step surface 132 away from the first side surface 131. The second side surface 133 is arranged roughly in the vertical direction. In this embodiment, the first groove 130 and the second groove 140 are Damascus grooves, respectively.

[0056] The first seed layer 103 is arranged along the groove wall of the first groove 130, and the first seed layer 103 covers the first side surface 131, the step surface 132 and part of the second side surface 133, and the first seed layer 103 is lower than the notch of the first groove 130. It can be understood that the groove bottom area of ​​the first groove 130 is smaller than the area of ​​the first surface 111. The first seed layer 103 completely covers the first side surface 131 and the step surface 132, partially covers the groove bottom of the first groove 130, and reserves the middle part of the groove bottom of the first groove 130 for growing the first metal column 105. The first seed layer 103 partially covers the second side surface 133 and is lower than the notch of the first groove 130. This arrangement can improve the bonding force between the wiring layer 150 and the pad 110. Optionally, the distance between the first seed layer 103 and the notch of the first groove 130 is half the height of the second side surface 133 in the vertical direction. The bonding force between the wiring layer 150 and the second dielectric layer 122 can be improved, and the second side surface 133 can protect the wiring layer 150 to a certain extent to prevent delamination and cracking.

[0057] The first metal column 105 is arranged in the first groove 130, the first metal column 105 is connected to the first surface 111, and is spaced apart from the first seed layer 103. The number of the first metal column 105 is not limited, and it can be one or more. Its shape is also not limited, and the cross-sectional shape can be circular, elliptical, T-shaped, U-shaped, V-shaped, triangular, semicircular, crescent, quadrilateral, pentagon, hexagon, octagon or other arbitrary shapes. The setting of the first metal column 105 can further improve the bonding force between the pad 110 and the wiring layer 150, and increase the thickness of the pad 110 to prevent the pad 110 from being punctured. At the same time, the heat dissipation performance can also be improved. The height of the first metal column 105 is lower than or flush with the surface of the first seed layer 103. Of course, in some embodiments, the height of the first metal column 105 can also be higher than the surface of the first seed layer 103, which is not specifically limited here.

[0058] Optional, combined Figure 3 The heights of the plurality of first metal pillars 105 may be different. Designing different heights can, on the one hand, enhance the bonding force between the wiring layer 150 and the pad 110. On the other hand, the conductivity of the pad 110 can be controlled by designing different heights.

[0059] It can be understood that the first metal pillar 105 grows directly on the first surface 111 of the pad 110, and the first metal pillar 105 can be regarded as a part of the pad 110. According to the calculation formula of the conductor resistance: R=ρL / A, where R is the resistance of the conductor; ρ is the resistivity of the conductor material; for the same material, the resistivity is a constant; L is the length of the conductor; A is the cross-sectional area of ​​the conductor. For this embodiment, the bottom size of the first groove 130 is fixed, then the length of the pad 110 used to transmit current to the wiring layer 150 is constant; the material resistivity is constant; the resistance and the cross-sectional area are inversely proportional. After the first metal pillar 105 is set, the cross-sectional area of ​​the pad 110 can be increased, thereby reducing the resistance. According to Ohm's law, U=IR; U is voltage, I is current; R is resistance. When the transmission voltage remains unchanged, the resistance and current are inversely proportional. The reduction of the resistance of the pad 110 will increase the transmission current accordingly, thereby increasing the conductivity of the pad 110 and improving the transmission performance.

[0060] In addition, according to the conductivity calculation formula, A=ρG; A is the cross-sectional area of ​​the conductor; ρ is the resistivity of the conductor material; G is the conductivity, which indicates the conductivity of the conductor. It can be seen that the cross-sectional area and the conductivity of the conductor are proportional. When the first metal column 105 is provided, the cross-sectional area of ​​the pad 110 increases, and the conductivity, that is, the conductivity of the pad 110 can be increased accordingly.

[0061] The first metal layer 101 is electrically connected to the first seed layer 103 covering the first side surface 131, and the first metal layer 101 and the first seed layer 103 covering the step surface 132 are arranged at intervals. In this embodiment, the first metal layer 101 and the first seed layer 103 covering the first side surface 131 are in direct contact. The end of the first metal layer 101 away from the peripheral side surface 113 is inclined, and the cross-sectional area of ​​the first metal layer 101 gradually increases from the end close to the second metal layer 102 to the end away from the second metal layer 102. In this embodiment, the cross-section of the first metal layer 101 is roughly trapezoidal, and the first groove 130 is located in the middle of the upper plane of the trapezoid. The trapezoidal design can increase the contact area between the first metal layer 101 and the dielectric layer 120 and enhance the bonding force. The thickness and width of the pad 110 can also be increased, and the structure is reliable and the reliability is better.

[0062] Optionally, the first metal layer 101 and the second metal layer 102 are symmetrically arranged about the pad 110, which can effectively balance the structural stress on both sides. Alternatively, the first groove 130 and the second groove 140 are symmetrically arranged about the pad 110. Alternatively, a second seed layer 104 is provided in the second groove 140, and the first seed layer 103 and the second seed layer 104 are symmetrically arranged about the pad 110. In this embodiment, the first metal layer 101 and the second metal layer 102 are symmetrically arranged about the pad 110. The first groove 130 and the second groove 140 are symmetrically arranged about the pad 110. The first seed layer 103 and the second seed layer 104 are symmetrically arranged about the pad 110. Of course, one or two of the above three groups of features may also be symmetrically arranged, which is not specifically limited here.

[0063] Optionally, the structure of the second seed layer 104 is similar to that of the first seed layer 103, which improves the bonding force between the pad 110 and the bump 160, and improves the bonding force between the bump 160 and the dielectric layer 120. A second metal column 106 is provided in the second groove 140, and the second metal column 106 is connected to the second surface 112 and is spaced apart from the second seed layer 104. The first metal column 105 and the second metal column 106 can be provided one by one or at the same time. The first metal column 105 and the second metal column 106 can be provided symmetrically or asymmetrically. Optionally, the second metal column 106 is provided in the second groove 140, and the second metal column 106 is provided in the second groove 140, and the second metal column 106 is provided in a spaced apart manner. Figure 3 The second metal pillar 106 is a plurality of metal pillars of different heights, which are arranged in a staggered manner, can improve the bonding force and facilitate the control of the transmission current and conductivity of the pad 110, and can also improve the heat dissipation performance of the bump 160.

[0064] Optionally, the side of the first metal column 105 away from the first surface 111 is not higher than the side of the first seed layer 103 away from the first surface 111. The side of the second metal column 106 away from the second surface 112 is not higher than the side of the second seed layer 104 away from the second surface 112. The first metal column 105 may be one or more, and the second metal column 106 may be one or more. Figure 1 As shown, there are two first metal pillars 105 and two second metal pillars 106. Figure 4 As shown, the first metal column 105 and the second metal column 106 are each one. Figure 5 As shown, there is one first metal pillar 105 and two second metal pillars 106 .

[0065] Optionally, the dielectric layer 120 includes a third dielectric layer 123. The surface of the wiring layer 150 protrudes from the surface of the second dielectric layer 122. The third dielectric layer 123 covers the wiring layer 150 and the second dielectric layer 122, and protects the wiring layer 150.

[0066] Combination Figure 6 , Fig. 9A window is provided on the third dielectric layer 123, and the window exposes the output end of the wiring layer 150. The window is electroplated with metal to form a pad 152, and the pad 152 is electrically connected to the wiring layer 150. The pad 152 protrudes from the surface of the third dielectric layer 123, so as to facilitate electrical connection with the chip 210 or other components, modules, etc.

[0067] The wiring layer 150 is provided with a roughened groove 151 on one side away from the surface of the pad 110. This can improve the bonding strength between the wiring layer 150 and the dielectric layer 120, or, in the case where the pad 152 is provided, can also improve the bonding strength between the wiring layer 150 and the pad 152. Alternatively, when applied to a stacked structure, the roughened groove 151 on the wiring layer 150 can improve the bonding strength between the wiring layer 150 and the solder joint 220 of the chip 210 (see FIG. Figure 8 The roughening groove 151 may be a tiny protrusion or groove structure, and in this embodiment, it is a beehive-shaped groove structure.

[0068] The dielectric layer 120 further includes a fourth dielectric layer 124 and a fifth dielectric layer 125 which are sequentially disposed on one side of the second surface 112 of the pad 110. The fourth dielectric layer 124 is provided with a second annular groove 1241 (see Fig.13 ). The depth of the second annular groove 1241 is greater than the thickness of the fourth dielectric layer 124. That is, the second annular groove 1241 penetrates the fourth dielectric layer 124 and a portion of the first dielectric layer 121 to expose a portion of the peripheral side surface 113 and a portion of the second surface 112 of the pad 110. The groove wall of the second annular groove 1241 is inclined so that the groove gradually widens. The second metal layer 102 fills the second annular groove 1241.

[0069] Optionally, the first metal layer 101 and the second metal layer 102 are in contact on the peripheral side surface 113. That is, a portion of the peripheral side surface 113 of the pad 110 is covered and wrapped by the first metal layer 101, and another portion is covered and wrapped by the second metal layer 102. In this way, the structure of the pad 110 can be enhanced, the cross-sectional area of ​​the pad 110 can be increased, the transmission current can be increased, and the conductivity and heat dissipation can be improved. In this embodiment, the second metal layer 102 and the first metal layer 101 are symmetrically designed, that is, the cross-section of the second metal layer 102 is also trapezoidal.

[0070] Combination Figure 7Optionally, a third seed layer 107 is provided between the second surface 112 and the bump 160. The third seed layer 107 can further increase the thickness of the pad 110, improve the reliability of the pad 110, and improve the bonding force between the bump 160 and the pad 110. It should be understood that due to the provision of the third seed layer 107, a sixth dielectric layer 126 will be added in the process technology to protect the third seed layer 107, and the thickness of the sixth dielectric layer 126 and the third seed layer 107 are equal. The sixth dielectric layer 126 is located between the first dielectric layer 121 and the fourth dielectric layer 124. Therefore, the overall thickness of the dielectric layer 120 is also increased, the insulation performance is better, and the gap between the wiring layer 150 and the bump 160 is increased, which is conducive to reducing parasitic current and capacitance effects.

[0071] In this embodiment, the surface of the second seed layer 104 is lower than the notch of the second groove 140. In this way, when the bump 160 is formed, the bump 160 can be grown from the second seed layer 104 in the second groove 140 and extend out of the surface of the fifth dielectric layer 125. That is, the end of the bump 160 close to the pad 110 is located in the second groove 140, which can improve the reliability of the bump 160 and improve the bonding force between the bump 160 and the fifth dielectric layer 125. The side wall of the second groove 140 plays a certain protective role on the bump 160, preventing the bump 160 from cracking or delamination at the junction with the surface of the fifth dielectric layer 125.

[0072] Combination Figure 8 Optionally, the bump 160 includes a connecting portion 161 and a ball portion 162, the connecting portion 161 is electrically connected to the pad 110, the ball portion 162 is connected to the connecting portion 161, and a roughened portion 163 is provided on one side of the connecting portion 161 close to the ball portion 162. The connecting portion 161 is located in the second groove 140, and the ball portion 162 protrudes from the surface of the dielectric layer 120. In this embodiment, the connecting portion 161 is lower than the notch of the second groove 140. The groove wall of the second groove 140 can play a certain protective role on the ball portion 162. Prevent cracking or delamination at the junction of the ball portion 162 and the surface of the fifth dielectric layer 125. The provision of the roughened portion 163 can improve the bonding force between the connecting portion 161 and the ball portion 162, as well as improve the bonding force between the bump 160 and the fifth dielectric layer 125. The roughened portion 163 is similar in structure to the roughened groove 151 on the wiring layer 150.

[0073] The material of the dielectric layer 120 in this embodiment can be at least one of silicon nitride, silicon oxynitride, polyimide, benzocyclobutene, etc. The first metal pillar 105 and the second metal pillar 106 can be made of copper.

[0074] When the substrate wiring structure 100 is used in a stacked structure, electronic components such as a chip 210 are mounted in the substrate structure, and the solder joints 220 of the chip 210 are electrically connected to the wiring layer 150. At this time, the output end of the wiring layer 150 is exposed on the surface of the dielectric layer 120. Multiple chips 210 can be mounted in each substrate structure, such as Fig. 9 It can be understood that if the substrate wiring structure 100 is not used in a stacked structure, a dielectric layer 120 will be added to the surface of the wiring layer 150 for protection. Figure 1 , Figures 3 to 6 shown.

[0075] Combination Figures 10 to 15 The embodiment of the present invention provides a preparation method for preparing the substrate wiring structure 100 as in any one of the above-mentioned embodiments. The preparation method is roughly as follows:

[0076] Step S1: Provide a carrier 201, and apply a debonding adhesive layer 202 on the surface of the carrier 201. The adhesive layer 202 can be separated by irradiating UV ultraviolet light. Use sputtering, chemical plating, electroplating, physical vapor deposition, chemical vapor deposition, metal organic chemical vapor deposition, atomic layer deposition, low pressure chemical vapor deposition or plasma enhanced chemical vapor deposition to form a metal aluminum layer 203 and a copper column in sequence, and the aluminum layer 203 serves as a barrier layer to protect the bottom debonding adhesive layer 202. The copper column is located on the aluminum layer 203, and the copper column serves as a pad 110. Use any process of spin coating, spraying, printing, physical vapor deposition, chemical vapor deposition, metal organic chemical vapor deposition, atomic layer deposition, low pressure chemical vapor deposition or plasma enhanced chemical vapor deposition to form a first dielectric layer 121. The material of the first dielectric layer 121 can be at least one of silicon nitride, silicon oxynitride, polyimide and benzocyclobutene.

[0077] Step S2: Using dry etching or chemical etching, a first annular groove 1211 is formed in the dielectric layer 120, and the cross section is roughly trapezoidal. The notch size of the first annular groove 1211 is larger than the groove bottom size. The groove bottom of the first annular groove 1211 is located at a position half of the thickness of the pad 110 in the vertical direction. The middle part of the first annular groove 1211 has a dielectric platform 1212 located on the first surface 111 of the pad 110.

[0078] The residue after etching in the first annular groove 1211 is removed by chemical cleaning or plasma cleaning. The metal layer is electroplated in the first annular groove 1211 by electroplating to form a trapezoidal first metal layer 101. The first metal layer 101 fills the first annular groove 1211. The dielectric platform 1212 of the first surface 111 is removed by dry etching or chemical etching again to expose the pad 110. The residue after etching on the first surface 111 is removed by chemical cleaning or plasma cleaning.

[0079] The second dielectric layer 122 is formed by any process including spin coating, spray coating, printing, physical vapor deposition, chemical vapor deposition, metal organic chemical vapor deposition, atomic layer deposition, low pressure chemical vapor deposition or plasma enhanced chemical vapor deposition. The material of the second dielectric layer 122 can be at least one of silicon nitride, silicon oxynitride, polyimide and benzocyclobutene.

[0080] Step S3: A first groove 130 is formed on the second dielectric layer 122, and the first groove 130 is a Damascus groove. The first groove 130 is formed from the second dielectric layer 122 to the first surface 111 of the pad 110. Optionally, a photomask (pattern layer) is covered on the second dielectric layer 122, and an opening layer (Damask groove) of the pattern layer is formed by an exposure and development process.

[0081] The first seed layer 103 is formed in the first groove 130 by using processes such as sputtering, chemical plating, electroplating, physical vapor deposition, chemical vapor deposition, metal organic chemical vapor deposition, atomic layer deposition, low pressure chemical vapor deposition or plasma enhanced chemical vapor deposition. The first seed layer 103 is lower than the surface of the second dielectric layer 122 to enhance the bonding force of the sidewall wiring layer 150.

[0082] The first metal column 105 is formed in the first groove 130 by electroplating process, and the first metal column 105 can be a copper column. The first metal column 105 is connected to the first surface 111 of the pad 110 and is spaced apart from the first seed layer 103. After the first metal column 105 is formed, a metal wiring layer 150 is formed in the first groove 130 by sputtering, chemical plating, electroplating, physical vapor deposition, chemical vapor deposition, metal organic chemical vapor deposition, atomic layer deposition, low pressure chemical vapor deposition or plasma enhanced chemical vapor deposition. The wiring layer 150 fills the entire first groove 130 and protrudes from the upper surface of the second dielectric layer 122. It can be understood that the wiring layer 150 is respectively connected to the first seed layer 103, the first metal column 105 and the first surface 111 of the pad 110 to achieve electrical connection. And the arrangement of the first seed layer 103 and the first metal column 105 can enhance the bonding force between the wiring layer 150 and the pad 110 and the dielectric layer 120 respectively.

[0083] Optionally, the surface of the wiring layer 150 away from the pad 110 is etched by micro-etching to form a micro honeycomb structure, that is, a roughened groove 151 is formed. Then, a third dielectric layer 123 is formed on the wiring layer 150 by a coating process. The third dielectric layer 123 is used to protect the wiring layer 150, and the upper part of the substrate wiring structure 100 is completed. It can be understood that the roughened groove 151 can further enhance the bonding force between the wiring layer 150 and the third dielectric layer 123.

[0084] Step S4: Separating the carrier 201. The carrier 201 is separated from the aluminum layer 203 by UV light irradiation or laser debonding.

[0085] The aluminum layer 203 is removed by etching or grinding to expose the second surface 112 of the pad 110 .

[0086] A fourth dielectric layer 124 is formed on the second surface 112 by a coating process. A second annular groove 1241 with a trapezoidal cross section is formed on the fourth dielectric layer 124 by dry etching. The structure of the second annular groove 1241 is similar to that of the first annular groove 1211. The notch size of the second annular groove 1241 is larger than the size of the groove bottom. The groove bottom of the second annular groove 1241 is located at a position half the thickness of the pad 110 in the vertical direction. The middle portion of the second annular groove 1241 has a dielectric platform 1212 located on the second surface 112 of the pad 110.

[0087] The residue after etching in the second annular groove 1241 is removed by chemical cleaning or plasma cleaning. The metal layer is electroplated in the second annular groove 1241 by electroplating to form a trapezoidal second metal layer 102. The second metal layer 102 fills the first annular groove 1211. The dielectric platform 1212 of the second surface 112 is removed by dry etching or chemical etching again, and the second surface 112 of the pad 110 is exposed. The residue after etching of the second surface 112 is removed by chemical cleaning or plasma cleaning.

[0088] The fifth dielectric layer 125 covering the second metal layer 102 is formed by any process such as spin coating, spray coating, printing, physical vapor deposition, chemical vapor deposition, metal organic chemical vapor deposition, atomic layer deposition, low pressure chemical vapor deposition or plasma enhanced chemical vapor deposition. A second groove 140 is opened on the fifth dielectric layer 125, and the second groove 140 is a Damascus groove. The second groove 140 is opened from the fifth dielectric layer 125 to the second surface 112 of the pad 110. The second seed layer 104 and the second metal column 106 are sequentially formed in the second groove 140. The formation method of the second groove 140, the second seed layer 104 and the second metal column 106 can refer to the formation method of the first groove 130, the first seed layer 103 and the first metal column 105 mentioned above.

[0089] The electroplating process is used to electroplate the metal layer to form the connection part 161, and then the hemisphere of the bump 160 is formed by formic acid reflow. The connection part 161 can be made of nickel, and the hemisphere part 162 can be made of SnAg, SnAgCu or Sn-Bi, etc., to improve the bonding strength. At this point, the substrate wiring structure 100 is completed.

[0090] The materials of the first dielectric layer 121 , the second dielectric layer 122 , the third dielectric layer 123 , the fourth dielectric layer 124 , the fifth dielectric layer 125 and the sixth dielectric layer 126 are consistent.

[0091] It should be noted that in the existing process, when the aluminum layer 203 is removed by grinding, part of the pad 110 may be removed, resulting in thinning of the back of the pad 110, thereby affecting the conductive performance of the pad 110. In this embodiment, the second metal layer 102, the third seed layer 107 and the second metal column 106 can increase the thickness of the pad 110, thereby improving the reliability and conductive performance of the pad 110.

[0092] Optional, combined Fig.16 If it is necessary to set a pad 152 on the wiring layer 150 , a window can be opened on the third dielectric layer 123 , and then metal is electroplated to form the pad 152 .

[0093] In summary, the substrate wiring structure 100 and the preparation method thereof provided in the embodiment of the present invention are conducive to increasing the thickness of the pad 110, improving the reliability and conductivity of the pad 110, preventing short circuits in electrical testing, and improving the bonding force between the pad 110 and the wiring layer 150 and between the pad 110 and the dielectric layer 120.

[0094] The above is only a specific embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Any changes or substitutions that can be easily thought of by a person skilled in the art within the technical scope disclosed by the present invention should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention should be based on the protection scope of the claims.

Claims

1. A substrate wiring structure, It is characterized in that include: A pad having a first surface and a second surface arranged opposite to each other, and a peripheral side surface connecting the first surface and the second surface; A dielectric layer, wherein the pad is disposed in the dielectric layer; the dielectric layer is provided with a first groove exposing a portion of the first surface, and a second groove exposing a portion of the second surface; A wiring layer, the wiring layer is arranged in the first groove and extends to the surface of the dielectric layer; the wiring layer is electrically connected to the pad; A bump, the bump being arranged in the second groove and exposing a surface of the dielectric layer away from the wiring layer; the bump being electrically connected to the pad; a first metal layer, the first metal layer covering a portion of the peripheral side surface and a portion of the first surface, the first metal layer being electrically connected to the wiring layer; A second metal layer, wherein the second metal layer covers a portion of the peripheral side surface and a portion of the second surface, and the second metal layer is electrically connected to the bump.

2. The substrate wiring structure according to claim 1, It is characterized in that It also includes a first seed layer; the groove wall of the first groove includes a first side surface, a step surface and a second side surface connected in sequence; the first side surface is connected to the first surface; The first seed layer is arranged along the groove wall of the first groove, the first seed layer covers the first side surface, the step surface and a part of the second side surface, and the first seed layer is lower than the notch of the first groove; The first metal layer is electrically connected to a first seed layer covering the first side surface, and the first metal layer and the first seed layer covering the step surface are spaced apart.

3. The substrate wiring structure according to claim 2, It is characterized in that The first metal layer and the second metal layer are symmetrically arranged about the pad; And / or, the first groove and the second groove are symmetrically arranged with respect to the pad; And / or, a second seed layer is disposed in the second groove, and the first seed layer and the second seed layer are symmetrically arranged with respect to the pad.

4. The substrate wiring structure according to claim 3, It is characterized in that Also includes a first metal column disposed in the first groove, the first metal column is connected to the first surface and is spaced apart from the first seed layer; And / or, it also includes a second metal column disposed in the second groove, the second metal column is connected to the second surface and is spaced apart from the second seed layer.

5. The substrate wiring structure according to claim 4, It is characterized in that The first surface is provided with a plurality of spaced-apart first metal pillars, and the plurality of first metal pillars have different heights; And / or, a side of the first metal column away from the first surface is not higher than a side of the first seed layer away from the first surface.

6. The substrate wiring structure according to claim 1, It is characterized in that A roughening groove is provided on one side of the wiring layer away from the pad surface.

7. The substrate wiring structure according to claim 1, It is characterized in that The first metal layer and the second metal layer are in contact with each other on the peripheral side surface; And / or, one end of the first metal layer away from the peripheral side surface is an inclined surface, and the cross-sectional area of ​​the first metal layer gradually increases from one end close to the second metal layer to one end away from the second metal layer.

8. The substrate wiring structure according to claim 1, It is characterized in that A third seed layer is disposed between the second surface and the bump.

9. The substrate wiring structure according to any one of claims 1 to 8, It is characterized in that The bump includes a connecting portion and a ball portion, the connecting portion is electrically connected to the pad, the ball portion is connected to the connecting portion, and a roughened portion is provided on a side of the connecting portion close to the ball portion.

10. A preparation method, It is characterized in that Used for preparing a substrate wiring structure as claimed in any one of claims 1 to 9.