Bi2Te3-based double i-type heterojunction infrared detector and its manufacturing method

By using Bi2Te3's dual-i-type heterojunction structure in the infrared detector, the MoSe2, Bi2Te3 and WS2 material layers are stacked to form a single-sided depletion zone, which solves the problem of interface capture effect and low efficiency of traditional infrared detectors, and realizes the Higher photoelectric conversion efficiency and response speed.

CN118676239BActive Publication Date: 2024-11-05GUANGZHOU NANSHA DISTRICT BEIKE PHOTON SENSING TECH RES INST +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411147335.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-21
Publication Date
2024-11-05
Estimated Expiration
2044-08-21

AI Technical Summary

Technical Problem

Traditional infrared detectors based on two-dimensional semiconductors have slow response speed due to interface capture effect and low photoelectric conversion efficiency, and carriers are tunneled and reorganized on the interface, limiting the performance of the device.

Method used

Using Bi2Te3-based bii-type heterojunction structure, MoSe2-Bi2Te3-WS2 bii-type heterojunction is constructed by stacking MoSe2, Bi2Te3, and WS2 material layers in turn to form a one-sided depletion region to suppress interface capture effect and photogenesis of electrons. -Hole recombination to improve photoelectric conversion efficiency and response speed.

Benefits of technology

The photoelectric conversion efficiency and response speed of infrared detectors are significantly improved. Through the interface effect of fast carrier transport of Bi2Te3 and the i-band alignment, the problems of low efficiency and slow speed of traditional infrared detectors are solved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118676239B_ABST
    Figure CN118676239B_ABST
Patent Text Reader

Abstract

The present invention relates to the field of infrared detector technology, and provides a Bi2Te3-based double i-type heterojunction infrared detector and a manufacturing method thereof, comprising a substrate, a MoSe2 material layer, a Bi2Te3 material layer, a WS2 material layer, a source electrode and a drain electrode; the MoSe2 material layer is arranged on the substrate surface; the Bi2Te3 material layer is arranged on the substrate surface and one end of the Bi2Te3 material layer contacts the surface of the MoSe2 material layer, forming an i-type heterojunction with the MoSe2 material layer; the WS2 material layer is arranged on the substrate surface and one end of the WS2 material layer contacts the surface of the Bi2Te3 material layer, forming an i-type heterojunction with the Bi2Te3 material layer; the source electrode is arranged on the substrate surface and contacts the MoSe2 material layer, the drain electrode is arranged on the substrate surface and contacts the WS2 material layer, and the Bi2Te3 material layer does not contact the source electrode and the drain electrode. The present invention effectively suppresses the interlayer recombination and interface capture effect of photogenerated electron-hole pairs, thereby improving the photoelectric conversion efficiency and response speed of the infrared detector.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of infrared detectors, and in particular to a Bi2Te3-based double i-type heterojunction infrared detector and a manufacturing method thereof. Background Art

[0002] Infrared detectors are widely used in military defense, imaging, optical communications and other fields. Low-dimensional van der Waals semiconductors (vdWs), such as transition metal dichalcogenides, black phosphorus, graphene, etc., show great development potential in the next generation of electronic and optoelectronic devices due to their unique properties, including atomic-scale size, strong light-matter interaction and layer-dependent band structure. In the past few decades, photodetectors based on these materials have achieved high performance such as high responsiveness, wide detection range, and high detection rate. Moreover, combining different low-dimensional vdWs materials into vdWs heterojunctions can integrate the advantages of single materials and further improve the performance of infrared detectors.

[0003] Unlike traditional chemical bond heterostructures, the interface of vdWs heterojunction has no dangling bonds, which enables it to achieve different energy band arrangements regardless of lattice adaptation. So far, various vdws heterojunctions based on two-dimensional semiconductors have been reported, such as MoTe2 / MoS2, GaTe / MoS2, GaTe / InSe, BP / MoS2 and MoS2 / WSe2, etc., and these structures are all typical type-ii band alignment, forming a staggered gap between the two semiconductors and leaving a bilateral depletion region at the interface. However, this usually causes most carriers to undergo a certain degree of tunneling recombination at the interface, limiting the photoelectric conversion efficiency. In addition, since both electrons and holes need to cross the interface, an interface capture effect will inevitably occur, significantly reducing the response speed of the device. In order to solve these problems, an i-type band-aligned heterostructure is proposed, which forms a unilateral depletion region at the interface, and only one type of photogenerated carrier passes through the heterointerface and quickly recombine with the carriers at the opposite position in the accumulation region. In this way, the interlayer recombination and interface capture effects of photogenerated electron-hole pairs will be suppressed, thereby improving the device efficiency and response speed. Summary of the invention

[0004] In view of the above problems, the present invention is proposed to provide a Bi2Te3-based double i-type heterojunction infrared detector and a method for manufacturing the same that overcomes the above problems or at least partially solves the above problems.

[0005] In one aspect of the present invention, a double i-type heterojunction infrared detector based on Bi2Te3 is provided, comprising a substrate, a MoSe2 material layer, a Bi2Te3 material layer, a WS2 material layer, a source electrode and a drain electrode;

[0006] A MoSe2 material layer is arranged on the surface of the substrate;

[0007] A Bi2Te3 material layer is disposed on the surface of the substrate, and one end of the Bi2Te3 material layer contacts the surface of the MoSe2 material layer to form an i-type heterojunction with the MoSe2 material layer;

[0008] A WS2 material layer is disposed on the surface of the substrate, and one end of the WS2 material layer contacts the surface of the Bi2Te3 material layer to form an i-type heterojunction with the Bi2Te3 material layer;

[0009] The source electrode is arranged on the surface of the substrate and contacts the MoSe2 material layer, the drain electrode is arranged on the surface of the substrate and contacts the WS2 material layer, and the Bi2Te3 material layer does not contact the source electrode or the drain electrode.

[0010] Among them, the thickness of the Bi2Te3 material layer is greater than the thickness of the MoSe2 material layer, and the thickness of the MoSe2 material layer is greater than the thickness of the WS2 material layer.

[0011] Among them, the thickness of the MoSe2 material layer is 25 nm ~35 nm, the thickness of the Bi2Te3 material layer is 45 nm ~55 nm, and the thickness of the WS2 material layer is 15 nm ~25 nm.

[0012] Wherein, the junction area of ​​the i-type heterojunction is 150-200 μm 2 .

[0013] Wherein, the substrate is a SiO2 / Si substrate.

[0014] Another aspect of the present invention further provides a method for manufacturing the Bi2Te3-based double i-type heterojunction infrared detector as described above, the method comprising:

[0015] Making a substrate;

[0016] Forming a MoSe2 material layer on the surface of the substrate;

[0017] Forming a Bi2Te3 material layer on the surface of the substrate, wherein one end of the Bi2Te3 material layer contacts the surface of the MoSe2 material layer to form an i-type heterojunction with the MoSe2 material layer;

[0018] Forming a WS2 material layer on the surface of the substrate, wherein one end of the WS2 material layer contacts the surface of the Bi2Te3 material layer to form an i-type heterojunction with the Bi2Te3 material layer;

[0019] A source electrode and a drain electrode are formed on the surface of the substrate, the source electrode is in contact with the MoSe2 material layer, and the drain electrode is in contact with the WS2 material layer.

[0020] Wherein, the manufacturing substrate comprises:

[0021] Cutting the P-type SiO2 / Si material into a rectangular substrate of a preset size;

[0022] The cut substrates are sequentially placed in an acetone solution and an isopropanol solution for ultrasonic cleaning for a preset time period;

[0023] The ultrasonically cleaned substrate is rinsed with deionized water;

[0024] The rinsed substrate is dried.

[0025] Wherein, forming a MoSe2 material layer on the surface of the substrate comprises:

[0026] MoSe2 material layers of different thicknesses were obtained by mechanical stripping, and the MoSe2 material layers were transferred to the substrate surface using PDMS;

[0027] Further, a Bi2Te3 material layer is formed on the surface of the substrate, one end of the Bi2Te3 material layer contacts the surface of the MoSe2 material layer, and forms an i-type heterojunction with the MoSe2 material layer, including:

[0028] Obtain Bi2Te3 material layers of different thicknesses by mechanical stripping, transfer the Bi2Te3 material layers to the substrate surface by using PDMS, and stack one end of the Bi2Te3 material layer on the MoSe2 material layer to form an i-type heterojunction with the MoSe2 material layer;

[0029] Further, a WS2 material layer is formed on the surface of the substrate, one end of the WS2 material layer contacts the surface of the Bi2Te3 material layer, and forms an i-type heterojunction with the Bi2Te3 material layer, including:

[0030] WS2 material layers of different thicknesses were obtained by mechanical stripping, and the WS2 material layers were transferred to the substrate surface using PDMS. One end of the WS2 material layer was stacked on the side of the Bi2Te3 material layer that was not in contact with the MoSe2 material layer to form an i-type heterojunction with the Bi2Te3 material layer.

[0031] Wherein, forming a source electrode and a drain electrode on the surface of the substrate comprises:

[0032] Through electron beam exposure technology and development, an electrode pattern mask is made on a substrate formed with a MoSe2 material layer, a Bi2Te3 material layer and a WS2 material layer. A 15nm thick Cr layer and a 45nm thick Au layer are sequentially evaporated using an electron beam evaporator, and then acetone is used for soaking to remove the photoresist and the metal layer outside the electrode area. After that, it is washed with deionized water and blown dry with a nitrogen gun to obtain a source electrode and a drain electrode.

[0033] The Bi2Te3-based double i-type heterojunction infrared detector and its manufacturing method provided in the embodiment of the present invention construct a MoSe2-Bi2Te3-WS2 double i-type heterojunction by stacking MoSe2, Bi2Te3, and WS2 material layers in sequence on a substrate, giving full play to the advantages of Bi2Te3's fast carrier transport and i-type band alignment interface effect and low recombination efficiency of photogenerated electron-hole pairs, solving the problems of low photoelectric conversion efficiency and slow response speed of traditional infrared detectors based on two-dimensional materials, thereby improving the photoelectric conversion efficiency and response speed of the device.

[0034] The above description is only an overview of the technical solution of the present invention. In order to more clearly understand the technical means of the present invention, it can be implemented according to the contents of the specification. In order to make the above and other purposes, features and advantages of the present invention more obvious and easy to understand, the specific implementation methods of the present invention are listed below. BRIEF DESCRIPTION OF THE DRAWINGS

[0035] Various other advantages and benefits will become apparent to those of ordinary skill in the art by reading the detailed description of the preferred embodiments below. The accompanying drawings are only for the purpose of illustrating the preferred embodiments and are not to be considered as limiting the present invention. Moreover, the same reference symbols are used throughout the accompanying drawings to represent the same components. In the accompanying drawings:

[0036] Figure 1 A schematic diagram of the structure of a double i-type heterojunction infrared detector based on Bi2Te3 provided in an embodiment of the present invention;

[0037] Figure 2 Schematic diagram of the energy band structure of the MoSe2-Bi2Te3-WS2 double i-type heterojunction provided in an embodiment of the present invention;

[0038] Figure 3 A flow chart of a method for manufacturing a Bi2Te3-based double i-type heterojunction infrared detector provided in an embodiment of the present invention;

[0039] Figure 4 A sample schematic diagram of the manufacturing process of a Bi2Te3-based double i-type heterojunction infrared detector provided in an embodiment of the present invention;

[0040] Figure 5The double i-type heterojunction infrared detector based on Bi2Te3 provided in the embodiment of the present invention has a light power density of "44.5~80.6 mW / cm" under 976 nm laser excitation without gate voltage. 2 " I ds - V ds Schematic diagram of the curve. DETAILED DESCRIPTION

[0041] The exemplary embodiments of the present disclosure will be described in more detail below with reference to the accompanying drawings. Although the exemplary embodiments of the present disclosure are shown in the accompanying drawings, it should be understood that the present disclosure can be implemented in various forms and should not be limited by the embodiments set forth herein. On the contrary, these embodiments are provided to enable a more thorough understanding of the present disclosure and to fully convey the scope of the present disclosure to those skilled in the art.

[0042] Those skilled in the art will appreciate that, unless otherwise stated, the singular forms "a", "an", "said" and "the" used herein may also include plural forms. It should be further understood that the term "comprising" used in the specification of the present invention refers to the presence of the features, integers, steps, operations, elements and / or components, but does not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components and / or groups thereof.

[0043] Those skilled in the art will understand that, unless otherwise defined, all terms (including technical and scientific terms) used herein have the same meaning as generally understood by those skilled in the art in the art to which the present invention belongs. It should also be understood that terms such as those defined in general dictionaries should be understood to have meanings consistent with the meanings in the context of the prior art, and will not be interpreted with idealized or overly formal meanings unless specifically defined.

[0044] Van der Waals (vdWs) heterostructures based on low-dimensional semiconductor materials provide great opportunities for the study of next-generation electronic and optoelectronic devices. Careful design of band alignment engineering for different crystal structure combinations is essential to achieve excellent performance of the detector. In response to the needs of high-efficiency photoelectric conversion efficiency and fast response for infrared detection, the present invention proposes a double i-type heterojunction infrared detector based on Bi2Te3. By stacking MoSe2, Bi2Te3, and WS2 materials in sequence to construct a MoSe2-Bi2Te3-WS2 double i-type heterojunction, a single-sided depletion region is formed on the MoSe2 and WS2 sides, and the interlayer recombination and interface capture effects of photogenerated electron-hole pairs will be effectively suppressed, thereby improving the photoelectric conversion efficiency and response speed of the device. The present invention reveals the potential applications of mixed-dimensional vdWs heterostructures and provides new ideas for exploring high-performance photodetectors with advanced functions.

[0045] Figure 1 The schematic diagram of the structure of the double i-type heterojunction infrared detector based on Bi2Te3 proposed by the present invention is shown. Figure 1 The Bi2Te3-based double i-type heterojunction infrared detector provided by the present invention includes a substrate 101, a MoSe2 material layer 102, a Bi2Te3 material layer 103, a WS2 material layer 104, a source electrode 105 and a drain electrode 106;

[0046] The MoSe2 material layer 102 is arranged on the surface of the substrate 101;

[0047] A Bi2Te3 material layer 103 is disposed on the surface of the substrate 101 and one end of the Bi2Te3 material layer 103 contacts the surface of the MoSe2 material layer 102 to form an i-type heterojunction with the MoSe2 material layer 102;

[0048] The WS2 material layer 104 is disposed on the surface of the substrate 101 and one end of the WS2 material layer 104 contacts the surface of the Bi2Te3 material layer 103 to form an i-type heterojunction with the Bi2Te3 material layer 103;

[0049] The source electrode 105 is disposed on the surface of the substrate 101 and in contact with the MoSe 2 material layer 102 . The drain electrode 106 is disposed on the surface of the substrate 101 and in contact with the WS 2 material layer 104 . The Bi 2 Te 3 material layer 103 is not in contact with the source electrode 105 or the drain electrode 106 .

[0050] When the voltage between the source electrode and the drain electrode is 0 V, the electrons in the MoSe2 material layer and the WS2 material layer are transferred to the Bi2Te3 material layer, forming a depletion region on the MoSe2 side and the WS2 side, and an accumulation region on the Bi2Te3 side; when a bias voltage is applied between the source electrode and the drain electrode, the heterojunction barrier and the Schottky barrier become smaller, and electrons are injected into the MoSe2 side and the WS2 side, and flow to the Bi2Te3 material layer through the heterojunction barrier, generating an electron-dominated current.

[0051] As a two-dimensional topological insulator composed of a single Dirac cone, Bi2Te3 has an insulating body state and a conductive gapless surface state. Its ultrahigh carrier mobility and strong light absorption behavior make it a suitable candidate for infrared light detection at room temperature. In addition, the metallic Dirac surface state of Bi2Te3 protected by time-reversal symmetry can not only effectively suppress electron backscattering, but also provide topological protection for itself, enabling it to maintain fast carrier transport capability and long-term chemical stability in an air environment. In addition, the surface of Bi2Te3 without dangling bonds is conducive to reducing carrier generation-recombination noise. Therefore, constructing an i-type band-aligned heterostructure of Bi2Te3 will greatly improve the photoelectric conversion efficiency and response speed of infrared detectors. The present invention proposes a double i-type heterojunction infrared detector based on Bi2Te3, and constructs a MoSe2-Bi2Te3-WS2 double i-type heterojunction by stacking MoSe2, Bi2Te3, and WS2 material layers in sequence, giving full play to the advantages of Bi2Te3's fast carrier transport and i-type band alignment interface effect and low recombination efficiency of photogenerated electron-hole pairs, thereby solving the problems of low photoelectric conversion efficiency and slow response speed of traditional infrared detectors based on two-dimensional materials.

[0052] In an optional embodiment, the thickness of the Bi2Te3 material layer is greater than the thickness of the MoSe2 material layer, and the thickness of the MoSe2 material layer is greater than the thickness of the WS2 material layer. In an optional embodiment, the thickness of the MoSe2 material layer is 25 nm to 35 nm, the thickness of the Bi2Te3 material layer is 45 nm to 55 nm, and the thickness of the WS2 material layer is 15 nm to 25 nm.

[0053] The junction area of ​​the i-type heterojunction is 150 μm 2 ~200 μm 2 .

[0054] Wherein, the substrate is a SiO2 / Si substrate.

[0055] In this embodiment, the schematic diagram of the MoSe2-Bi2Te3-WS2 double i-type heterojunction energy band structure is as follows: Figure 2The MoSe2, Bi2Te3, and WS2 material layers are obtained by mechanical stripping, with thicknesses of 30 nm, 50 nm, and 20 nm, respectively, and are stacked horizontally as the bottom, middle, and top layers, respectively, with a junction area of ​​190 μm 2 . The source electrode and drain electrode are connected to MoSe2 and WS2 respectively, and the middle Bi2Te3 layer is not in contact with the source electrode and the drain electrode. The band alignment analysis of the heterojunction under different bias conditions is as follows: In the equilibrium state with a voltage of 0 V, the electrons in MoSe2 and WS2 will be transferred to Bi2Te3, forming a depletion region on the MoSe2 side and the WS2 side, and an accumulation region on the Bi2Te3 side. When the bias voltage is applied, the heterojunction barrier and the Schottky barrier become smaller, and electrons are easily injected into MoSe2 and WS2, pass through the heterojunction barrier, and then flow to Bi2Te3, generating a large electron-dominated current.

[0056] Another embodiment of the present invention further provides a method for manufacturing the Bi2Te3-based double i-type heterojunction infrared detector as described above, such as Figure 3 As shown, the method for manufacturing a double i-type heterojunction infrared detector based on Bi2Te3 provided in an embodiment of the present invention includes the following specific processing flow:

[0057] S11, preparing a substrate;

[0058] S12, forming a MoSe2 material layer on the surface of the substrate;

[0059] S13, forming a Bi2Te3 material layer on the surface of the substrate, wherein one end of the Bi2Te3 material layer contacts the surface of the MoSe2 material layer to form an i-type heterojunction with the MoSe2 material layer;

[0060] S14, forming a WS2 material layer on the surface of the substrate, wherein one end of the WS2 material layer contacts the surface of the Bi2Te3 material layer to form an i-type heterojunction with the Bi2Te3 material layer;

[0061] S15. Forming a source electrode and a drain electrode on the surface of the substrate, wherein the source electrode is in contact with the MoSe2 material layer, and the drain electrode is in contact with the WS2 material layer.

[0062] In an embodiment of the present invention, manufacturing a substrate specifically includes: cutting a P-type SiO2 / Si material into a rectangular substrate of a preset size; placing the cut substrates in an acetone solution and an isopropanol solution in turn for ultrasonic cleaning for a preset time; rinsing the ultrasonically cleaned substrates with deionized water; and drying the rinsed substrates.

[0063] Specifically, when making the substrate, the P-type SiO2 / Si material can be cut into a 10mm×10mm rectangle, such as a square, and ultrasonically cleaned in an acetone solution for 20 minutes, and then ultrasonically cleaned in an isopropanol solution for 20 minutes, and then rinsed with clean deionized water and dried with a nitrogen gun. Furthermore, in order to remove water vapor, the cleaned substrate can be placed on a heating table for heating.

[0064] In the embodiment of the present invention, forming the MoSe2 material layer on the substrate surface specifically includes: obtaining MoSe2 material layers of different thicknesses by a mechanical stripping method, and transferring the MoSe2 material layer to the substrate surface by using PDMS.

[0065] Furthermore, a Bi2Te3 material layer is formed on the surface of the substrate, one end of the Bi2Te3 material layer contacts the surface of the MoSe2 material layer, and forms an i-type heterojunction with the MoSe2 material layer, specifically including: obtaining Bi2Te3 material layers of different thicknesses by a mechanical stripping method, transferring the Bi2Te3 material layer to the surface of the substrate by using PDMS, and stacking one end of the Bi2Te3 material layer on the MoSe2 material layer to form an i-type heterojunction with the MoSe2 material layer.

[0066] Furthermore, a WS2 material layer is formed on the surface of the substrate, one end of the WS2 material layer contacts the surface of the Bi2Te3 material layer, and forms an i-type heterojunction with the Bi2Te3 material layer, specifically comprising: obtaining WS2 material layers of different thicknesses by a mechanical stripping method, transferring the WS2 material layer to the surface of the substrate by using PDMS, and stacking one end of the WS2 material layer on a side of the Bi2Te3 material layer that is not in contact with the MoSe2 material layer, and forming an i-type heterojunction with the Bi2Te3 material layer.

[0067] Specifically, the prepared substrate is placed on a dry transfer platform, and the few layers of MoSe2 are first transferred to the substrate by mechanical stripping by high temperature heating. The specific method is to tear off MoSe2 films of different thicknesses with blue film tape, cut the PDMS film into rectangles, and paste it on the surface of the slide. Then, the MoSe2 material on the blue film tape is transferred to PDMS, and the MoSe2 film of suitable thickness and size is found under a microscope and transferred to the prepared substrate. Then, Bi2Te3 and WS2 are transferred in the same way to construct a MoSe2-Bi2Te3-WS2 heterojunction.

[0068] In an embodiment of the present invention, forming a source electrode and a drain electrode on the surface of the substrate includes: making an electrode pattern mask on a substrate having a MoSe2 material layer, a Bi2Te3 material layer and a WS2 material layer through electron beam exposure technology and development, sequentially vapor-depositing a Cr layer with a thickness of 15 nm and an Au layer with a thickness of 45 nm using an electron beam evaporator, and then washing with acetone to remove the photoresist and the metal layer outside the electrode area, and then washing with deionized water and drying with a nitrogen gun to obtain a source electrode and a drain electrode.

[0069] Specifically, in order to prepare the metal electrode, a layer of photoresist is first evenly coated on the sample, and the electrode pattern is engraved on the sample by electron beam exposure and developed. Then, Cr / Au (15 / 45 nm) electrode evaporation is performed in an electron beam evaporation chamber. After completion, the sample is immersed in a degumming solution to remove excess metal, then washed with deionized water and dried with a nitrogen gun for subsequent testing.

[0070] Figure 4 This is a sample schematic diagram of the manufacturing process of a double i-type heterojunction infrared detector based on Bi2Te3. Figure 4 (a), (b), and (c) correspond to sample examples after substrate processing, material transfer, and electrode evaporation, respectively.

[0071] In order to verify the technical solution of the present invention, the present invention tests the light response of the double i-type heterojunction infrared detector based on Bi2Te3 at an excitation wavelength of 976 nm. In this embodiment, when the double i-type heterojunction infrared detector based on Bi2Te3 is implemented, the thickness of the MoSe2 material layer is 30 nm, the thickness of the Bi2Te3 material layer is 50 nm, and the thickness of the WS2 material layer is 20 nm. Among them, the junction area of ​​the i-type heterojunction is 190 μm 2 . Figure 5 It shows that the optical power density is between 44.5 and 80.6 mW / cm without gate voltage. 2 " I ds - V ds It can be seen that Ids increases with the increase of optical power density under both positive bias and negative bias, and the photocurrent changes more under positive bias.

[0072] When V ds When V > 0 V, the larger band bending at the edge of WS2 / Bi2Te3 is conducive to the photogenerated carriers to cross WS2 / Bi2Te3, while the built-in electric field of MoSe2 / Bi2Te3 is weakened. The photogenerated electrons from MoSe2 can be transferred to Bi2Te3 via hot ions, resulting in a larger photocurrent. ds<0 V, the band bending at the WS2 / Bi2Te3 interface is weakened, while the band bending at the MoSe2 / Bi2Te3 interface is enhanced, resulting in an increase in the potential barrier and greatly reducing the efficiency of electron transfer. At the same time, this band bending in the i-type band alignment leads to the accumulation of photogenerated electrons in Bi2Te3 and holes in MoSe2 at their interface. Therefore, significant interlayer recombination is likely to occur, resulting in a small photocurrent.

[0073] The Bi2Te3-based double i-type heterojunction infrared detector and its manufacturing method provided in the embodiment of the present invention construct a MoSe2-Bi2Te3-WS2 double i-type heterojunction by stacking MoSe2, Bi2Te3, and WS2 material layers in sequence on a substrate, giving full play to the advantages of Bi2Te3's fast carrier transport and i-type band alignment interface effect and low recombination efficiency of photogenerated electron-hole pairs, solving the problems of low photoelectric conversion efficiency and slow response speed of traditional infrared detectors based on two-dimensional materials, thereby improving the photoelectric conversion efficiency and response speed of the device.

[0074] Those skilled in the art will appreciate that, although some embodiments herein include certain features included in other embodiments but not other features, the combination of features of different embodiments is meant to be within the scope of the present invention and form different embodiments. For example, any one of the claimed embodiments may be used in any combination.

[0075] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A double i-type heterojunction infrared detector based on Bi2Te3, characterized in that: It includes a substrate, a MoSe2 material layer, a Bi2Te3 material layer, a WS2 material layer, a source electrode and a drain electrode; The MoSe2 material layer is arranged on the surface of the substrate; A Bi2Te3 material layer is disposed on the surface of the substrate, and one end of the Bi2Te3 material layer contacts the surface of the MoSe2 material layer to form an i-type heterojunction with the MoSe2 material layer; A WS2 material layer is disposed on the surface of the substrate, and one end of the WS2 material layer contacts the surface of the Bi2Te3 material layer to form an i-type heterojunction with the Bi2Te3 material layer; The source electrode is arranged on the surface of the substrate and contacts the MoSe2 material layer, the drain electrode is arranged on the surface of the substrate and contacts the WS2 material layer, and the Bi2Te3 material layer does not contact the source electrode or the drain electrode; Among them, the surfaces of the MoSe2 material layer and the WS2 material layer are not in contact.

2. The Bi2Te3-based double i-type heterojunction infrared detector according to claim 1, characterized in that: The thickness of the Bi2Te3 material layer is greater than that of the MoSe2 material layer, and the thickness of the MoSe2 material layer is greater than that of the WS2 material layer.

3. The double i-type heterojunction infrared detector based on Bi2Te3 according to claim 1, characterized in that: The thickness of the MoSe2 material layer is 25 nm ~35 nm, the thickness of the Bi2Te3 material layer is 45 nm ~55 nm, and the thickness of the WS2 material layer is 15nm ~25 nm.

4. The double i-type heterojunction infrared detector based on Bi2Te3 according to claim 1, characterized in that: The junction area of ​​the i-type heterojunction is 150-200 μm 2 .

5. The Bi2Te3-based double i-type heterojunction infrared detector according to claim 1, characterized in that: The substrate is a SiO2 / Si substrate.

6. A method for manufacturing a Bi2Te3-based double i-type heterojunction infrared detector according to any one of claims 1 to 5, characterized in that: The method comprises: Making a substrate; Forming a MoSe2 material layer on the surface of the substrate; Forming a Bi2Te3 material layer on the surface of the substrate, wherein one end of the Bi2Te3 material layer contacts the surface of the MoSe2 material layer to form an i-type heterojunction with the MoSe2 material layer; Forming a WS2 material layer on the surface of the substrate, wherein one end of the WS2 material layer contacts the surface of the Bi2Te3 material layer to form an i-type heterojunction with the Bi2Te3 material layer; A source electrode and a drain electrode are formed on the surface of the substrate, the source electrode is in contact with the MoSe2 material layer, and the drain electrode is in contact with the WS2 material layer.

7. The method for manufacturing a Bi2Te3-based double i-type heterojunction infrared detector according to claim 6, characterized in that: The manufacturing substrate comprises: Cutting the P-type SiO2 / Si material into a rectangular substrate of a preset size; The cut substrates are sequentially placed in an acetone solution and an isopropanol solution for ultrasonic cleaning for a preset time period; The ultrasonically cleaned substrate is rinsed with deionized water; The rinsed substrate is dried.

8. The method for manufacturing a Bi2Te3-based double i-type heterojunction infrared detector according to claim 6, characterized in that: Forming a MoSe2 material layer on the substrate surface includes: MoSe2 material layers of different thicknesses were obtained by mechanical stripping, and the MoSe2 material layers were transferred to the substrate surface using PDMS; Forming a Bi2Te3 material layer on the surface of the substrate, wherein one end of the Bi2Te3 material layer contacts the surface of the MoSe2 material layer and forms an i-type heterojunction with the MoSe2 material layer, including: Obtain Bi2Te3 material layers of different thicknesses by mechanical stripping, transfer the Bi2Te3 material layers to the substrate surface by using PDMS, and stack one end of the Bi2Te3 material layer on the MoSe2 material layer to form an i-type heterojunction with the MoSe2 material layer; A WS2 material layer is formed on the surface of the substrate, one end of the WS2 material layer contacts the surface of the Bi2Te3 material layer, and forms an i-type heterojunction with the Bi2Te3 material layer, including: WS2 material layers of different thicknesses were obtained by mechanical stripping, and the WS2 material layers were transferred to the substrate surface using PDMS. One end of the WS2 material layer was stacked on the side of the Bi2Te3 material layer that was not in contact with the MoSe2 material layer to form an i-type heterojunction with the Bi2Te3 material layer.

9. The method for manufacturing a Bi2Te3-based double i-type heterojunction infrared detector according to claim 8, characterized in that: Forming a source electrode and a drain electrode on the surface of the substrate includes: Through electron beam exposure technology and development, an electrode pattern mask is made on a substrate formed with a MoSe2 material layer, a Bi2Te3 material layer and a WS2 material layer. A 15nm thick Cr layer and a 45nm thick Au layer are sequentially evaporated using an electron beam evaporator, and then acetone is used for soaking to remove the photoresist and the metal layer outside the electrode area. After that, it is washed with deionized water and blown dry with a nitrogen gun to obtain a source electrode and a drain electrode.