Anode bonding method for wafer-level SOI (Silicon On Insulator) silicon wafer
By removing the oxide layer of the SOI silicon wafer and sputtering a metal layer on its conductive channel, the problem of insufficient conductivity of the SOI silicon wafer is solved, and precise alignment and high-strength bonding with the glass wafer are achieved, which is suitable for a variety of applications. scene.
Patent Information
- Application Number
- CN202410885735.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-03
- Publication Date
- 2024-10-01
AI Technical Summary
SOI silicon wafers lack conductivity due to the buried oxide layer in the middle, resulting in insufficient anode bonding strength. Existing methods require misalignment and are not suitable for mass production.
The top oxide layer of the SOI silicon wafer is removed by wet or dry methods to prepare a conductive channel, and a metal layer is sputtered or evaporated between the top silicon and the substrate silicon. The conductive channel is formed and then accurately aligned and bonded with the glass wafer. .
It achieves precise alignment and high-strength bonding of SOI silicon wafers and glass wafers, is suitable for most application scenarios, and is compatible with conventional bonding equipment.
Smart Images

Figure CN118723918A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of microsystems (MEMS) and wafer-level packaging, and in particular to a wafer-level SOI silicon wafer anode bonding method. Background Art
[0002] At present, in the field of microsystems (MEMS) and wafer-level packaging, anodic bonding based on SOI silicon wafers can be applied to devices isolated from the external environment. Compared with BCB bonding and silicon-silicon bonding, it has the advantages of low cost and easy processing, and can be widely used in pressure sensors, inertial gyroscopes, and accelerometers. Generally, anodic bonding uses single-polished silicon wafers or double-polished silicon wafers to bond with glass wafers. During the processing, the silicon wafer and glass wafer need to be heated to 200℃~400℃, and then a DC voltage of 500~1000V is applied to realize the transfer of charge, thereby forming a stable structural layer on the bonding surface. Therefore, during the processing, the silicon wafer needs to have a certain conductivity, but because the SOI silicon wafer has an intermediate buried oxide layer, the SOI silicon wafer does not have good conductivity and cannot form sufficient bonding strength.
[0003] After searching existing patents, the Chinese patent "A wafer-level bonding method for SOI silicon wafers and glass" (patent number CN202211341952.0) uses a certain misalignment between the SOI wafer and the glass wafer, and then the positive and negative electrodes are contacted with the exposed silicon and glass wafer of the SOI wafer respectively, thereby completing the charge transfer and forming a good bonding strength. Since this method requires a certain misalignment between the two wafers, it is impossible to accurately align the patterns on the two wafers, and the bonding equipment needs to have special electrodes, which cannot be adapted to most usage scenarios. Summary of the invention
[0004] The object of the present invention is to provide a wafer-level SOI silicon wafer anodic bonding method, which can accurately align the SOI silicon wafer and the glass wafer and has good bonding strength.
[0005] The technical solution adopted by the present invention to solve its technical problem is: A wafer-level SOI silicon wafer anodic bonding method comprises the following steps: S1. Take the SOI silicon wafer, and use wet etching or dry etching to remove the exposed buried oxide layer between the top silicon and the substrate silicon of the SOI silicon wafer, and keep the middle top silicon part; S2, using a sputtering or evaporation process to form a layer of metal on the top silicon surface and the exposed substrate silicon surface; S3, using photolithography and corrosion or etching process to remove part of the metal of the top silicon layer, leaving only the metal connection between the top silicon layer and the substrate silicon layer, thereby forming a conductive channel between the top silicon layer and the substrate silicon layer; S4. Align the SOI silicon wafer and the glass wafer and perform anodic bonding.
[0006] The beneficial effect of the present invention is that a conductive channel is formed between the top silicon and substrate silicon of the SOI silicon wafer, and then accurately aligned and bonded with the glass sheet, forming a wafer-level SOI silicon wafer anodic bonding method suitable for most application scenarios. BRIEF DESCRIPTION OF THE DRAWINGS
[0007] Figure 1 It is a cross-sectional view of the initial SOI silicon wafer; Figure 2 It is the SOI wafer after removing the exposed buried oxide layer; Figure 3 It is the SOI wafer after the metal layer is made; Figure 4 SOI wafer after removing most of the metal from the top silicon Figure 5 It is a schematic diagram of anodic bonding between a processed SOI wafer and a glass sheet; Figure 6 is an overall effect diagram of the wafer after processing of the present invention (top view); Figure 7 This is the overall effect of the wafer after processing using the existing method (top view). DETAILED DESCRIPTION
[0008] Select a SOI wafer with a thickness of (400-1-25) um, such as Figure 1 , Figure 2 : Since the top silicon surface of the SOI wafer is generally smaller in diameter than the substrate silicon surface, the BOE solution is used to etch for 5 minutes to remove the buried oxide layer of the SOI wafer; like Figure 3 As shown, a magnetron sputtering machine is then used to sputter a 3000Å thick metal aluminum on the top silicon surface of the processed SOI wafer; like Figure 4 As shown, a photoresist with a thickness of 1 um is applied to the aluminum-sputtered side of the wafer, and then a contact photolithography machine and a customized mask are used to expose the photoresist covering the top silicon layer for 300 ms, followed by development for 2 minutes to remove the exposed photoresist, and then the wafer is immersed in aluminum etching solution for 3 minutes to cleanly etch the metal aluminum covering the top silicon layer, and then the photoresist is removed by soaking in an organic solution for 1 hour; like Figure 5 As shown, using anodic bonding equipment, the SOI silicon wafer and the glass wafer are heated to 300~400℃, and then a DC voltage of 600~1000V is applied to bond the glass wafer to the top silicon surface.
[0009] The effect of the anodic bonding of the present invention is as follows Figure 6As shown, the direction of the glass is consistent with the flat edge of the wafer. During the bonding alignment process, conventional bonding alignment marks can be used for identification and alignment. Figure 7 In order to ensure the bonding strength, the prior art shown requires that the flat edges of the glass sheet and the wafer be offset by 90° and a special fixture be used to apply DC voltage to the glass sheet and the wafer respectively. Therefore, conventional bonding alignment marks cannot be used for identification and alignment, resulting in extremely difficult and low alignment accuracy for the glass sheet and the wafer, and is not suitable for large-scale production.
Claims
1. A wafer-level SOI silicon wafer anodic bonding method, Features The following steps are involved: S1. Take the SOI silicon wafer, and use wet etching or dry etching to remove the exposed buried oxide layer between the top silicon and the substrate silicon of the SOI silicon wafer, and keep the middle top silicon part; S2, using a sputtering or evaporation process to form a layer of metal on the top silicon surface and the exposed substrate silicon surface; S3, using photolithography and corrosion or etching process to remove part of the metal of the top silicon layer, leaving only the metal connection between the top silicon layer and the substrate silicon layer, thereby forming a conductive channel between the top silicon layer and the substrate silicon layer; S4. Align the SOI silicon wafer and the glass wafer and perform anodic bonding.