Silicon carbide device and forming method thereof

By forming a multi-layer structure and a doped layer on a silicon carbide substrate, the problem of forming a super-junction structure in silicon carbide devices is solved, and efficient silicon carbide device manufacturing is achieved.

CN118737831APending Publication Date: 2024-10-01ALPHA POWER SOLUTIONS SHANGHAI LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410758444.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-12
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

In the prior art, the application of super junction structures of silicon carbide devices has not appeared, and there is a lack of effective formation methods.

Method used

By forming first and second silicon carbide epitaxial layers on a silicon carbide substrate, filling the doped layer on the bottom and sidewalls of the trench, and removing part of the doped layer higher than the top surface of the second silicon carbide epitaxial layer, a formation Transistor structure to achieve the formation of super junction structure.

Benefits of technology

Successfully achieved the formation of super junction structure in silicon carbide devices, improving the reliability and efficiency of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118737831A_ABST
    Figure CN118737831A_ABST
Patent Text Reader

Abstract

The invention provides a silicon carbide device and a forming method thereof, and the silicon carbide device comprises a silicon carbide substrate, a first silicon carbide epitaxial layer is formed on the surface of the silicon carbide substrate, and a groove is formed in the first silicon carbide epitaxial layer; the second silicon carbide epitaxial layer is located at the bottom and the side wall of the groove and on the surface of the first silicon carbide epitaxial layer; the doping layer is located on a part of the surface of the second silicon carbide epitaxial layer and fills the groove, and the top surface of the doping layer is not higher than the top surface of the second silicon carbide epitaxial layer; and the transistor structure is positioned on the second silicon carbide epitaxial layer. The invention provides a silicon carbide device and a forming method thereof. A super junction structure can be formed in the silicon carbide device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of semiconductor technology, and in particular to a silicon carbide device and a method for forming the same. Background Art

[0002] Silicon carbide devices (SiC MOSFET) are semiconductor devices that are different from traditional silicon substrates and horizontal channels. However, there are still defects in the formation process of silicon carbide devices. For example, the application of super junction structure in silicon carbide devices has not yet appeared and developed.

[0003] Therefore, it is necessary to provide a more effective and reliable technical solution to achieve the formation of a super junction structure in silicon carbide devices. Summary of the invention

[0004] The present application provides a silicon carbide device and a method for forming the same, which can realize the formation of a super junction structure in the silicon carbide device.

[0005] One aspect of the present application provides a method for forming a silicon carbide device, comprising: providing a silicon carbide substrate, a first silicon carbide epitaxial layer formed on the surface of the silicon carbide substrate, a groove formed in the first silicon carbide epitaxial layer; forming a second silicon carbide epitaxial layer at the bottom and sidewalls of the groove and on the surface of the first silicon carbide epitaxial layer; forming a doped layer filling the groove on the surface of the second silicon carbide epitaxial layer; removing a portion of the doped layer higher than the top surface of the second silicon carbide epitaxial layer; and forming a transistor structure on the second silicon carbide epitaxial layer.

[0006] In some embodiments of the present application, both the first silicon carbide epitaxial layer and the second silicon carbide epitaxial layer are doped, and the doping types of the first silicon carbide epitaxial layer and the second silicon carbide epitaxial layer are opposite.

[0007] In some embodiments of the present application, the doping type of the doping layer and the second silicon carbide epitaxial layer is the same.

[0008] In some embodiments of the present application, the thickness of the second silicon carbide epitaxial layer is 0.05 to 0.3 microns.

[0009] In some embodiments of the present application, after removing a portion of the doped layer that is higher than the top surface of the second silicon carbide epitaxial layer, the method for forming the silicon carbide device further includes: etching the doped layer so that the top surface of the doped layer is lower than the top surface of the second silicon carbide epitaxial layer.

[0010] Another aspect of the present application also provides a silicon carbide device, including: a silicon carbide substrate, a first silicon carbide epitaxial layer is formed on the surface of the silicon carbide substrate, and a groove is formed in the first silicon carbide epitaxial layer; a second silicon carbide epitaxial layer is located at the bottom and sidewalls of the groove and the surface of the first silicon carbide epitaxial layer; a doping layer is located on a portion of the surface of the second silicon carbide epitaxial layer and fills the groove, and the top surface of the doping layer is not higher than the top surface of the second silicon carbide epitaxial layer; a transistor structure is located on the second silicon carbide epitaxial layer.

[0011] In some embodiments of the present application, both the first silicon carbide epitaxial layer and the second silicon carbide epitaxial layer are doped, and the doping types of the first silicon carbide epitaxial layer and the second silicon carbide epitaxial layer are opposite.

[0012] In some embodiments of the present application, the doping type of the doping layer and the second silicon carbide epitaxial layer is the same.

[0013] In some embodiments of the present application, the thickness of the second silicon carbide epitaxial layer is 0.05 to 0.3 microns.

[0014] In some embodiments of the present application, a top surface of the doping layer is lower than a top surface of the second silicon carbide epitaxial layer.

[0015] The present application provides a silicon carbide device and a method for forming the same, which can realize the formation of a super junction structure in the silicon carbide device. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] The following figures describe in detail the exemplary embodiments disclosed in this application. The same reference numerals represent similar structures in several views of the drawings. Those skilled in the art will understand that these embodiments are non-limiting, exemplary embodiments, and the drawings are only for the purpose of illustration and description, and are not intended to limit the scope of this application. Other embodiments may also accomplish the inventive intent in this application. It should be understood that the drawings are not drawn to scale.

[0017] in:

[0018] Figures 1 to 5 This is a schematic diagram of the structure of each step in the method for forming a silicon carbide device described in an embodiment of the present application. DETAILED DESCRIPTION

[0019] The following description provides specific application scenarios and requirements of the present application, with the purpose of enabling those skilled in the art to make and use the content in the present application. It will be apparent to those skilled in the art that various local modifications to the disclosed embodiments are apparent, and the general principles defined herein may be applied to other embodiments and applications without departing from the spirit and scope of the present application. Therefore, the present application is not limited to the embodiments shown, but to the widest scope consistent with the claims.

[0020] The technical solution of the present invention is described in detail below in conjunction with the embodiments and drawings.

[0021] Figures 1 to 5 The following is a structural schematic diagram of each step in the method for forming a silicon carbide device according to an embodiment of the present application. The method for forming a silicon carbide device according to an embodiment of the present application is described in detail in conjunction with the accompanying drawings.

[0022] refer to Figure 1 As shown, a silicon carbide substrate 100 is provided, a first silicon carbide epitaxial layer 110 is formed on the surface of the silicon carbide substrate 100 , and a trench 120 is formed in the first silicon carbide epitaxial layer 110 .

[0023] The semiconductor structure described in the embodiment of the present application is a silicon carbide device MOSFET with a super junction structure. The material of the silicon carbide substrate 100 is silicon carbide material, and the material of the first silicon carbide epitaxial layer 110 is also silicon carbide material. In some embodiments of the present application, the silicon carbide substrate 100 and the first silicon carbide epitaxial layer 110 may have doping ions, such as N-type doping ions.

[0024] In some embodiments of the present application, the material of the first silicon carbide epitaxial layer 110 is 4H-SiC, and the surface of the first silicon carbide epitaxial layer 110 is the silicon face or carbon face of the 4H-SiC. There are various polycrystalline types of silicon carbide, the most common of which are 3C-SiC with a cubic crystal structure, 4H-SiC and 6H-SiC with a hexagonal crystal structure, etc. The first silicon carbide epitaxial layer 110 of the present application uses 4H-SiC. 4H-SiC can be oriented and polished to present a main crystal plane as its surface, such as the (0001) plane, that is, the silicon plane, with silicon as the surface. Other planes perpendicular to the silicon plane also include A plane or M plane, and the opposite side of the silicon plane is the carbon plane.

[0025] In some embodiments of the present application, the width of the groove 120 is 0.5 to 2.5 microns.

[0026] refer to Figure 2 As shown, a second silicon carbide epitaxial layer 130 is formed on the bottom and sidewalls of the trench 120 and on the surface of the first silicon carbide epitaxial layer 110 .

[0027] In some embodiments of the present application, the material of the second silicon carbide epitaxial layer 130 is silicon carbide material. The second silicon carbide epitaxial layer 130 may be doped. The doping type of the second silicon carbide epitaxial layer 130 is opposite to that of the first silicon carbide epitaxial layer 110. The doping type of the second silicon carbide epitaxial layer 130 is, for example, P-type. The method for forming the second silicon carbide epitaxial layer 130 includes an in-situ doping epitaxial growth process.

[0028] In some embodiments of the present application, the thickness of the second silicon carbide epitaxial layer 130 is 0.05 to 0.3 microns.

[0029] In some embodiments of the present application, the thickness of the portion of the second silicon carbide epitaxial layer 130 located on the top surface of the first silicon carbide epitaxial layer 110 is greater than the thickness of the portion of the second silicon carbide epitaxial layer 130 located at the bottom and sidewall of the trench 120. This is because a MOS transistor is to be formed on the portion of the second silicon carbide epitaxial layer 130 located on the top surface of the first silicon carbide epitaxial layer 110 later.

[0030] refer to Figure 3 As shown, a doping layer 140 filling the trench 120 is formed on the surface of the second silicon carbide epitaxial layer 130 .

[0031] In some embodiments of the present application, the material of the doping layer 140 includes doped polysilicon. The doping type of the doping layer 140 and the second silicon carbide epitaxial layer 130 is the same, for example, P-type. The method of forming the doping layer 140 includes an in-situ doped chemical vapor deposition process or an in-situ doped epitaxial growth process.

[0032] refer to Figure 4 As shown, a portion of the doped layer 140 that is higher than the top surface of the second silicon carbide epitaxial layer 130 is removed, and the doped layer 140 is etched back so that the top surface of the doped layer 140 is lower than the top surface of the second silicon carbide epitaxial layer 130. The top surface of the doped layer 140 is lower than the top surface of the second silicon carbide epitaxial layer 130, which can increase the exposed area of ​​the second silicon carbide epitaxial layer 130 and increase the contact area between the subsequent second silicon carbide epitaxial layer 130 and the metal layer.

[0033] In some embodiments of the present application, a top surface of the doping layer 140 is not higher than a top surface of the second silicon carbide epitaxial layer 130 , and is not lower than a top surface of the first silicon carbide epitaxial layer 110 .

[0034] refer to Figure 5 As shown, a transistor structure 150 is formed on a portion of the second silicon carbide epitaxial layer 130 located on the top surface of the first silicon carbide epitaxial layer 110. The transistor structure 150 is, for example, a MOS transistor.

[0035] In some embodiments of the present application, the transistor structure 150 includes a gate structure 152 located on the top surface of the second silicon carbide epitaxial layer 130 and a source region 151 in the second silicon carbide epitaxial layer 130 located on both sides of the gate structure 152. The gate structure 152 may include a gate located on the top surface of the second silicon carbide epitaxial layer 130 and an insulating layer covering the sidewall and top surface of the gate, wherein the insulating layer is used to insulate and isolate the gate from a subsequent metal layer, so that the metal layer can be electrically connected to the source region 151, but not electrically connected to the gate.

[0036] In some embodiments of the present application, the method for forming the silicon carbide device further includes: forming a metal layer covering the second silicon carbide epitaxial layer 130, the transistor structure 150, and the doping layer 140 on the second silicon carbide epitaxial layer 130. The material of the metal layer includes any one or more of titanium nitride, tungsten, or titanium metal silicide.

[0037] In some embodiments of the present application, the metal layer serves as a source metal electrically connected to the source region 151 , but is not electrically connected to the gate in the gate structure 152 .

[0038] The present application provides a method for forming a silicon carbide device, which can realize the formation of a super junction structure in the silicon carbide device.

[0039] The embodiment of the present application also provides a silicon carbide device, referring to Figure 5 As shown, it includes: a silicon carbide substrate 100, a first silicon carbide epitaxial layer 110 is formed on the surface of the silicon carbide substrate 100, and a groove 120 is formed in the first silicon carbide epitaxial layer 110; a second silicon carbide epitaxial layer 130, located at the bottom and sidewalls of the groove 120 and the surface of the first silicon carbide epitaxial layer 110; a doping layer 140, located on a portion of the surface of the second silicon carbide epitaxial layer 130 and filling the groove 120, and the top surface of the doping layer 140 is not higher than the top surface of the second silicon carbide epitaxial layer 130; a transistor structure 150, located on the second silicon carbide epitaxial layer 130.

[0040] The semiconductor structure described in the embodiment of the present application is a silicon carbide device MOSFET with a super junction structure. The material of the silicon carbide substrate 100 is silicon carbide material, and the material of the first silicon carbide epitaxial layer 110 is also silicon carbide material. In some embodiments of the present application, the silicon carbide substrate 100 and the first silicon carbide epitaxial layer 110 may have doping ions, such as N-type doping ions.

[0041] In some embodiments of the present application, the material of the first silicon carbide epitaxial layer 110 is 4H-SiC, and the surface of the first silicon carbide epitaxial layer 110 is the silicon face or carbon face of the 4H-SiC. There are various polycrystalline types of silicon carbide, the most common of which are 3C-SiC with a cubic crystal structure, 4H-SiC and 6H-SiC with a hexagonal crystal structure, etc. The first silicon carbide epitaxial layer 110 of the present application uses 4H-SiC. 4H-SiC can be oriented and polished to present a main crystal plane as its surface, such as the (0001) plane, that is, the silicon plane, with silicon as the surface. Other planes perpendicular to the silicon plane also include A plane or M plane, and the opposite side of the silicon plane is the carbon plane.

[0042] In some embodiments of the present application, the width of the groove 120 is 0.5 to 2.5 microns.

[0043] In some embodiments of the present application, the material of the second silicon carbide epitaxial layer 130 is silicon carbide material. The second silicon carbide epitaxial layer 130 may be doped. The doping type of the second silicon carbide epitaxial layer 130 is opposite to that of the first silicon carbide epitaxial layer 110. The doping type of the second silicon carbide epitaxial layer 130 is, for example, P-type.

[0044] In some embodiments of the present application, the thickness of the second silicon carbide epitaxial layer 130 is 0.05 to 0.3 microns.

[0045] In some embodiments of the present application, the thickness of the portion of the second silicon carbide epitaxial layer 130 located on the top surface of the first silicon carbide epitaxial layer 110 is greater than the thickness of the portion of the second silicon carbide epitaxial layer 130 located at the bottom and sidewall of the trench 120 .

[0046] In some embodiments of the present application, the material of the doping layer 140 includes doped polysilicon. The doping type of the doping layer 140 and the second silicon carbide epitaxial layer 130 is the same, for example, P type.

[0047] In some embodiments of the present application, the top surface of the doped layer 140 is not higher than the top surface of the second silicon carbide epitaxial layer 130, and is not lower than the top surface of the first silicon carbide epitaxial layer 110. Preferably, the top surface of the doped layer 140 is lower than the top surface of the second silicon carbide epitaxial layer 130. The top surface of the doped layer 140 being lower than the top surface of the second silicon carbide epitaxial layer 130 can increase the exposed area of ​​the second silicon carbide epitaxial layer 130, and increase the contact area between the subsequent second silicon carbide epitaxial layer 130 and the metal layer.

[0048] In some embodiments of the present application, the transistor structure 150 is, for example, a MOS transistor.

[0049] In some embodiments of the present application, the transistor structure 150 includes a gate structure 152 located on the top surface of the second silicon carbide epitaxial layer 130 and a source region 151 in the second silicon carbide epitaxial layer 130 located on both sides of the gate structure 152. The gate structure 152 may include a gate located on the top surface of the second silicon carbide epitaxial layer 130 and an insulating layer covering the sidewall and top surface of the gate, wherein the insulating layer is used to insulate and isolate the gate from a subsequent metal layer, so that the metal layer can be electrically connected to the source region 151, but not electrically connected to the gate.

[0050] In some embodiments of the present application, the silicon carbide device further includes: a metal layer located on the second silicon carbide epitaxial layer 130 and covering the second silicon carbide epitaxial layer 130, the transistor structure 150, and the doping layer 140. The material of the metal layer includes any one or more of titanium nitride, tungsten, or titanium metal silicide.

[0051] In some embodiments of the present application, the metal layer serves as a source metal electrically connected to the source region 151 , but is not electrically connected to the gate in the gate structure 152 .

[0052] The present application provides a silicon carbide device and a method for forming the same, which can realize the formation of a super junction structure in the silicon carbide device.

[0053] In summary, after reading the contents of this application, those skilled in the art will appreciate that the aforementioned application contents may be presented only in an exemplary manner and may not be restrictive. Although not explicitly stated herein, those skilled in the art will appreciate that this application is intended to encompass various reasonable changes, improvements and modifications to the embodiments. These changes, improvements and modifications are within the spirit and scope of the exemplary embodiments of this application.

[0054] It should be understood that the term "and / or" used in this embodiment includes any or all combinations of one or more of the associated listed items. It should be understood that when an element is referred to as being "connected" or "coupled" to another element, it can be directly connected or coupled to another element, or there can also be intermediate elements.

[0055] Similarly, it should be understood that when an element such as a layer, region, or substrate is referred to as being "on" another element, it can be directly on the other element or there can be intervening elements. In contrast, the term "directly" means that there are no intervening elements. It should also be understood that the terms "comprising," "containing," "including," or "comprising," when used in this application document, indicate the presence of the recited features, wholes, steps, operations, elements, and / or components, but do not exclude the presence or addition of one or more other features, wholes, steps, operations, elements, components, and / or groups thereof.

[0056] It should also be understood that although the terms first, second, third, etc. can be used to describe various elements, these elements should not be limited by these terms. These terms are only used to distinguish one element from another element. Therefore, without departing from the teachings of the present application, the first element in some embodiments can be referred to as the second element in other embodiments. The same reference numerals or the same reference signs represent the same elements throughout the specification.

[0057] In addition, the present specification describes exemplary embodiments by reference to idealized exemplary cross-sectional views and / or plan views and / or stereograms. Therefore, differences from the illustrated shapes due to, for example, manufacturing techniques and / or tolerances are foreseeable. Therefore, the exemplary embodiments should not be interpreted as being limited to the shapes of the regions shown herein, but should include deviations in shapes caused by, for example, manufacturing. For example, an etched region shown as a rectangle will typically have circular or curved features. Therefore, the region shown in the figure is schematic in nature, and its shape is not intended to illustrate the actual shape of the region of the device nor to limit the scope of the exemplary embodiments.

Claims

1. A method for forming a silicon carbide device, characterized in that: include: Providing a silicon carbide substrate, wherein a first silicon carbide epitaxial layer is formed on a surface of the silicon carbide substrate, and a groove is formed in the first silicon carbide epitaxial layer; forming a second silicon carbide epitaxial layer at the bottom and sidewalls of the trench and on the surface of the first silicon carbide epitaxial layer; forming a doping layer filling the groove on a surface of the second silicon carbide epitaxial layer; removing a portion of the doped layer above a top surface of the second silicon carbide epitaxial layer; A transistor structure is formed on the second silicon carbide epitaxial layer.

2. The method for forming a silicon carbide device according to claim 1, wherein: The first silicon carbide epitaxial layer and the second silicon carbide epitaxial layer are both doped, and the doping types of the first silicon carbide epitaxial layer and the second silicon carbide epitaxial layer are opposite.

3. The method for forming a silicon carbide device according to claim 2, wherein: The doping type of the doping layer and the second silicon carbide epitaxial layer is the same.

4. The method for forming a silicon carbide device according to claim 1, wherein: The thickness of the second silicon carbide epitaxial layer is 0.05 to 0.3 microns.

5. The method for forming a silicon carbide device according to claim 1, wherein: After removing the portion of the doped layer that is higher than the top surface of the second silicon carbide epitaxial layer, the method further includes: etching the doped layer so that the top surface of the doped layer is lower than the top surface of the second silicon carbide epitaxial layer.

6. A silicon carbide device, characterized in that: include: A silicon carbide substrate, wherein a first silicon carbide epitaxial layer is formed on a surface of the silicon carbide substrate, and a groove is formed in the first silicon carbide epitaxial layer; A second silicon carbide epitaxial layer, located at the bottom and sidewalls of the trench and on the surface of the first silicon carbide epitaxial layer; a doping layer, located on a portion of the surface of the second silicon carbide epitaxial layer and filling the groove, wherein a top surface of the doping layer is not higher than a top surface of the second silicon carbide epitaxial layer; The transistor structure is located on the second silicon carbide epitaxial layer.

7. The silicon carbide device according to claim 6, characterized in that: The first silicon carbide epitaxial layer and the second silicon carbide epitaxial layer are both doped, and the doping types of the first silicon carbide epitaxial layer and the second silicon carbide epitaxial layer are opposite.

8. The silicon carbide device according to claim 7, characterized in that: The doping type of the doping layer and the second silicon carbide epitaxial layer is the same.

9. The silicon carbide device according to claim 6, characterized in that: The thickness of the second silicon carbide epitaxial layer is 0.05 to 0.3 microns.

10. The silicon carbide device according to claim 6, characterized in that: A top surface of the doping layer is lower than a top surface of the second silicon carbide epitaxial layer.