METHOD FOR MANUFACTURING A SILICON CARBIDE-BASED SEMICONDUCTIVE STRUCTURE AND AN INTERMEDIATE COMPOSITE STRUCTURE
Patent Information
- Application Number
- FR2021002306
- Authority / Receiving Office
- FR · FR
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-03-09
- Publication Date
- 2024-10-04
- Estimated Expiration
- 2041-03-09
Smart Images

Figure 00000019_0000 
Figure 00000019_0001 
Figure 00000019_0002
Abstract
Description
Title of the invention: METHOD FOR MANUFACTURING A SEMICONDUCTOR STRUCTURE BASED ON CARBIDE SILICON AND INTERMEDIATE COMPOSITE STRUCTURE FIELD OF THE INVENTION
[0001] The present invention relates to the field of semiconductor materials for microelectronic components. It relates in particular to a method for manufacturing a semiconductor structure comprising an active layer of high-quality monocrystalline silicon carbide comprising or intended to accommodate electronic components, said active layer being arranged on a support layer of polycrystalline silicon carbide. The invention also relates to an intermediate composite structure obtained during said method. TECHNOLOGICAL BACKGROUND OF THE INVENTION
[0002] Interest in silicon carbide (SiC) has increased significantly in recent years because this semiconductor material can increase power handling capacity. SiC is increasingly widely used for the manufacture of innovative power devices to meet the needs of emerging fields of electronics, such as electric vehicles.
[0003] Power devices and integrated power systems based on monocrystalline silicon carbide can handle much higher power density compared to their traditional silicon counterparts, and with smaller active area dimensions. To further limit the dimensions of power devices on SiC, it is advantageous to manufacture vertical rather than lateral components. For this, vertical electrical conduction, between an electrode arranged on the front face of the assembly of components and an electrode arranged on the rear face, must be allowed by said assembly.
[0004] Massive monocrystalline SiC substrates intended for the microelectronics industry nevertheless remain expensive and difficult to supply in large sizes. In addition, when produced on a massive substrate, the set of electronic components often requires the substrate to be thinned on the rear face, typically around 100 microns, to reduce the vertical electrical resistivity and / or to meet size and miniaturization specifications.
[0005] It is therefore advantageous to use thin film transfer solutions to develop composite structures typically comprising a thin film of monocrystalline SiC on a lower cost support substrate, the thin film being used to form the electronic components. A thin film transfer solution A well-known method is the Smart Cut™ process, based on light ion implantation and direct bonding. Such a process makes it possible, for example, to manufacture a composite structure comprising a thin layer of monocrystalline SiC (c-SiC), taken from a c-SiC donor substrate, in direct contact with a polycrystalline SiC (p-SiC) support substrate, and allowing vertical electrical conduction. The support substrate, which must be of sufficient thickness to be compatible with the formation of the components, is finally thinned to obtain the set of electronic components ready for integration. Even if said support substrate is of lower quality, the thinning steps and the loss of material remain cost contributors that one would like to eliminate.
[0006] Also known is document US8436363, which describes a method for manufacturing a composite structure comprising a thin layer of c-SiC arranged on a metal support substrate whose coefficient of thermal expansion is matched with that of the thin layer. This manufacturing method comprises the following steps:
[0007] - the formation of a fragile plane buried in a c-SiC donor substrate, delimiting a thin layer between said buried fragile plane and a front surface of the donor substrate,
[0008] - the deposition of a metallic layer, for example tungsten or molybdenum, on the front surface of the donor substrate to form the support substrate of sufficient thickness to fulfill the role of stiffener,
[0009] - the separation along the buried fragile plane, to form on the one hand, the structure composite comprising the metal support substrate and the thin c-SiC layer, and on the other hand, the rest of the donor substrate in c-SiC.
[0010] The disadvantage of this approach is that a metal support substrate is not always compatible with electronic component manufacturing lines. It may also be necessary to thin the support substrate, depending on the applications. SUBJECT OF THE INVENTION
[0011] The present invention relates to an alternative solution to those of the state of the art, and aims to overcome all or part of the aforementioned drawbacks. It relates in particular to a method for manufacturing a semiconductor structure for electronic components, advantageously vertical, produced on and / or in an active layer of high-quality monocrystalline silicon carbide, which is arranged on a support layer of polycrystalline silicon carbide. The invention also relates to a composite structure obtained at an intermediate stage of said manufacturing method. BRIEF DESCRIPTION OF THE INVENTION
[0012] The invention relates to a method of manufacturing a semiconductor structure, including:
[0013] a) a step of providing a temporary graphite substrate having a grain size of between 4 microns and 35 microns, a porosity of between 6 and 17%, and a coefficient of thermal expansion of between 4.10-6 / °C and 5.10-6 / °C;
[0014] b) a step of depositing, on a front face of the temporary substrate, a support layer of polycrystalline silicon carbide having a thickness of between 10 microns and 200 microns,
[0015] c) a step of transferring a useful layer of monocrystalline silicon carbide onto the support layer, directly or via an intermediate layer, to form a composite structure, said transfer implementing bonding by molecular adhesion,
[0016] d) a step of forming an active layer on the useful layer,
[0017] e) a step of removing the temporary substrate to form the semi-structure conductive, said structure including the active layer, the useful layer and the support layer.
[0018] According to other advantageous and non-limiting characteristics of the invention, taken alone or in any technically feasible combination:
[0019] • the deposition of step b) is also carried out on a rear face of the temporary substrate to form a second support layer, and / or on a peripheral edge of said substrate; • step c) of transfer includes: • the introduction of light species into a monocrystalline silicon carbide donor substrate, to form a buried fragile plane defining with a front face of the donor substrate, the useful layer, • assembly of the front face of the donor substrate on the support layer, directly or via an intermediate layer, by molecular adhesion bonding, • separation along the buried fragile plane to transfer the useful layer onto the support layer; • the intermediate layer is formed of tungsten, silicon, silicon carbide or other conductive or semiconductive materials; • separation takes place during heat treatment at a temperature between 800°C and 1200°C; • step d) comprises epitaxial growth of at least one additional layer of doped monocrystalline silicon carbide, on the useful layer, said additional layer forming all or part of the active layer; • the manufacturing method comprises a step of) producing all or part of electronic components on and / or in the active layer, the step of) being inserted between step d) and step e); • step e) comprises mechanical disassembly by propagation of a crack in the temporary substrate following the application of a mechanical stress, the crack extending substantially parallel to the plane of the interface between the temporary substrate and the support layer; • step e) comprises chemical disassembly between the support layer and the temporary substrate by lateral chemical etching; • step e) comprises chemical etching of all or part of the temporary substrate; • step e) comprises disassembly by thermal damage of the graphite from the temporary substrate; • step c) comprises the transfer of a second useful layer of monocrystalline silicon carbide onto the second support layer, directly or via a second intermediate layer, said transfer implementing bonding by molecular adhesion; • step d) comprises the formation of a second active layer on the second useful layer; • step e) makes it possible to form a second semiconductor structure, said structure including the second active layer, the second useful layer and the second support layer; the temporary substrate, provided in step a), has a circular wafer shape and a diameter 5% to 10% larger than a diameter targeted for the semiconductor structure; • the temporary substrate, provided in step a), has a circular wafer shape and a diameter slightly smaller than a diameter targeted for the semiconductor structure, so that the deposition of step b), also carried out on a peripheral edge of the temporary substrate, makes it possible to achieve said targeted diameter.
[0020] The invention also relates to a composite structure comprising:
[0021] - a temporary graphite substrate having a grain size of between 4 microns and 35 microns, a porosity between 6 and 17%, and a coefficient of thermal expansion between 4.10-6 / °C and 5.10-6 / °C,
[0022] - a support layer of polycrystalline silicon carbide having a thickness between 10 microns and 200 microns, at least arranged on one front face of the temporary substrate,
[0023] - a useful layer of monocrystalline silicon carbide, arranged on the layer support.
[0024] According to advantageous and non-limiting characteristics of the invention, taken alone or in any technically feasible combination:
[0025] • the useful layer has a thickness of between 100 nm and 1500 nm; • the temporary substrate has a thickness between 100 microns and 2000 microns; • the temporary substrate has a thermal conductivity of between 70 Wm '.K 1 and 130 Wm '.K '. BRIEF DESCRIPTION OF THE FIGURES
[0026] Other characteristics and advantages of the invention will emerge from the detailed description of the invention which follows with reference to the appended figures in which:
[0027] [fig. 1] [fig.l] shows a semiconductor structure developed using a process of manufacture in accordance with the invention;
[0028] [fig.2a]
[0029] [fig.2b]
[0030] [fig.2c]
[0031] [fig.2d]
[0032] [fig.2d']
[0033] [fig.2e] Figures 2a, 2b, 2c, 2d, 2d' and 2e show steps of a manufacturing method according to the invention;
[0034] [fig.3a]
[0035] [fig.3b] Figures 3a and 3b show steps of an embodiment by particular of the manufacturing process in accordance with the invention;
[0036] [fig.4a]
[0037] [fig.4b]
[0038] [fig.4c] Figures 4a to 4c show a step c) of transfer of the manufacturing method according to the invention.
[0039] The same references in the figures may be used for elements of the same type.
[0040] The figures are schematic representations which, for the sake of readability, are not to scale. In particular, the thicknesses of the layers along the z axis are not to scale with respect to the lateral dimensions along the x and y axes; and the relative thicknesses of the layers to each other are not necessarily respected in the figures. DETAILED DESCRIPTION OF THE INVENTION
[0041] The present invention relates to a method for manufacturing a semiconductor structure 100 ([fig.l]). By semiconductor structure 100, we mean at least a stack of layers 4,3,2 intended to accommodate a plurality of microelectronic components; we also mean the stack of layers 4,3,2 with said electronic components 40, resulting from a collective manufacturing on and / or in the active layer 4 held in the form of a wafer by a support layer 2, and ready to undergo the singulation steps prior to packaging.
[0042] The manufacturing method advantageously applies to vertical microelectronic components, which require vertical electrical conduction through the support layer 2, which forms the mechanical support of said components 40.
[0043] The manufacturing method firstly comprises a step a) of providing a temporary graphite substrate 1 having a front face 1a, a rear face 1b and a peripheral edge 1c ([fig.2a]). The graphite of the temporary substrate 1 has a grain size of between 4 microns and 35 microns, a porosity of between 6 and 17%, and a coefficient of thermal expansion of between 4.10-6 / °C and 5.10-6 / °C. These characteristics are notably chosen to provide an excellent seed for the deposition of a layer of polycrystalline silicon carbide (p-SiC), called support layer 2 hereinafter, and which will be described with reference to step b) of the method.
[0044] In particular, the grain size range is defined so that it is of the same order of magnitude as the expected grain size for the support layer 2, in the plane of the faces 1a, 1b. The thermal conductivity of the support layer 2 is thus ensured, because the grains of said layer will not be too small; moreover, even if the grain size is caused to increase during the deposition of the support layer 2, it remains within a controlled size range, due to the defined range of grain sizes of the graphite, which limits the roughness at the free surface of the deposited support layer 2. The porosity range is also restricted so as to control the surface roughness of the support layer 2 after its deposition (subsequent step b). Typically, it will thus be possible to limit the surface roughness to less than 1 micron RMS, or even to less than 10m RMS, so as to reduce the smoothing treatments after the deposition of the support layer 2.Finally, the coefficient of thermal expansion is defined to match the coefficient of thermal expansion of silicon carbide, to limit mechanical stresses in the structure during treatments (described later in the process) involving high temperatures.
[0045] The temporary substrate 1 is compatible with temperatures up to 1400°C when the atmosphere is controlled, i.e. without oxygen; because if exposed to air, graphite begins to burn in a low temperature range, typically 400°C - 600°C. Protected by a protective layer completely encapsulating it, the temporary graphite substrate 1 is compatible with very high temperatures, even above 1400°C.
[0046] The manufacturing method then comprises a step b) of depositing, on the front face 1a of the temporary substrate 1, a support layer 2 made of polycrystalline silicon carbide (p-SiC) ([fig.2b]).
[0047] The deposition can be carried out by any known technique, in particular by chemical deposition. in vapor phase (CVD), at a temperature of the order of 1100°C to 1400°C. For example, a thermal CVD technique such as atmospheric pressure deposition (APCVD for "atmospheric pressure CVD) or low pressure deposition (LPCVD for "low pressure CVD") can be mentioned, the precursors being able to be chosen from methylsilane, dimethyldichlorosilane or even dichlorosilane + i-butane. A plasma-assisted CVD technique (PECVD for "plasma enhanced CVD") can also be used, with for example silicon tetrachloride and methane as precursors; preferably, the frequency of the source used to generate the electrical discharge creating the plasma is of the order of 3.3 MHz, and more generally between 10 kHz and 100 GHz.
[0048] Prior to deposition, conventional cleaning sequences may be applied to the temporary substrate 1 to eliminate all or part of the particulate, metallic or organic contaminants potentially present on its free faces 1a, 1b.
[0049] The support layer 2 made of p-SiC has a thickness of between 10 microns and 200 microns. This thickness is chosen according to the thickness specifications expected for the semiconductor structure 100. The support layer 2 will, in this structure 100, have the role of mechanical substrate and will potentially have to ensure vertical electrical conduction. To guarantee this latter electrical conduction property (low resistivity), the support layer 2 is advantageously doped with n or p type as required.
[0050] According to an advantageous embodiment, the deposition of step b) is also carried out on the rear face 1b of the temporary substrate 1 to form a second support layer 2', and / or on the peripheral edge 1c of said substrate 1.
[0051] The role of the second support layer 2' (and of the p-SiC deposited on the peripheral edge 1c) can essentially be to protect the temporary graphite substrate 1 during the very high temperature heat treatments which will follow in the process; the thickness of the second support layer 2' and of the p-SiC deposited on the peripheral edge 1c (also called the protective layer hereinafter) will then be limited, of the order of a micron or a few microns.
[0052] The second support layer 2' can alternatively be deposited on the rear face 1b of the temporary substrate 1 in order to carry out the following steps of the method at the two faces 1a, 1b of said substrate 1 ([fig.3a]). The second support layer 2' then has a thickness of the same order of magnitude as the first support layer 2 arranged on the side of the front face 1a of the temporary substrate 1.
[0053] In general, after deposition of the support layer 2 (and potentially of the second support layer 2'), a surface treatment is carried out, to improve the surface roughness of the support layer 2 and / or the quality of the edges of the structure, with a view to the following step of transferring the useful layer 3.
[0054] Conventional techniques of chemical etching (wet or dry) and / or mechanical grinding and / or chemical-mechanical polishing can be implemented to achieve a surface roughness of the p-SiC of the order of 0.5 nm RMS, preferably less than 0.3 nm RMS (roughness measurement by atomic force microscopy - AFM, on a scan of 20 microns x 20 microns for example). The aforementioned characteristics of the graphite forming the temporary substrate 1 nevertheless make it possible to limit the surface treatments to be applied.
[0055] According to a first variant, the temporary substrate 1, provided in step a), which typically has a circular wafer shape, has a diameter 5% to 10% larger than the diameter targeted for the final semiconductor structure 100. This can make it possible to limit edge problems during the deposition of step b) and to maximize the surface area occupied by the future components 40 on the semiconductor structure 100.
[0056] According to a second variant, the temporary substrate 1, provided in step a), has a diameter slightly smaller than the diameter targeted for the final semiconductor structure 100 (typically less than 5% smaller), so that the deposition of step b), carried out in this case on the peripheral edge of the temporary substrate 1, makes it possible to achieve said targeted diameter.
[0057] The manufacturing method according to the invention then comprises a step c) of transferring a useful layer 3 made of monocrystalline silicon carbide (c-SiC) directly onto the support layer 2 or via an intermediate layer, to form a composite structure 10 ([fig.2c]). The transfer implements bonding by molecular adhesion, and consequently a bonding interface 5. The intermediate layer can be formed on the side of the useful layer 3 and / or on the side of the support layer 2, to promote said bonding.
[0058] Advantageously, and as is known with reference to the Smart Cut™ process, transfer step c) successively comprises:
[0059] - the introduction of light species into a donor substrate 30 made of silicon carbide monocrystalline, to form a buried fragile plane 31, defining with the front face 30a of the donor substrate 30, the useful layer 3 ([fig.4a]),
[0060] - the assembly of the front face 30a of the donor substrate 30 on the support layer 2, directly or via an intermediate layer, by molecular adhesion bonding, along a bonding interface 5 ([fig.4b]),
[0061] - separation along the buried fragile plane 31 to transfer the useful layer 3 onto support layer 2 ([fig.4c]).
[0062] The light species are preferably hydrogen, helium or a co-implantation of these two species, and are implanted at a determined depth in the donor substrate 30, consistent with the thickness of the targeted useful layer 3 ([fig.4a]). These light species will form, around the determined depth, microcavities distributed in a thin layer parallel to the free surface 30a of the donor substrate 30, i.e. parallel to the plane (x,y) in the figures. This thin layer is called the buried fragile plane 31, for the sake of simplification.
[0063] The implantation energy of the light species is chosen so as to reach the determined depth. For example, hydrogen ions will be implanted at an energy between 10 keV and 250 keV, and at a dose between 5E16 / cm2 and Ie 17 / cm2, to delimit a useful layer 3 having a thickness of the order of 100 to 1500 nm. Note that an additional layer may be deposited on the front face 30a of the donor substrate 30, prior to the ion implantation step. This additional layer may be composed of a material such as silicon oxide or silicon nitride for example. It may be kept for the following step (and form all or part of the aforementioned intermediate layer), or it may be removed.
[0064] The assembly of the donor substrate 30 on the support layer 2 takes place at their respective front faces and forms a bonded assembly, along the bonding interface 5 ([fig.4b]). As is well known per se, bonding by molecular adhesion does not require an adhesive material, bonds being established at the atomic scale between the assembled surfaces. Several types of bonding by molecular adhesion exist, which differ in particular by the conditions of temperature, pressure, atmosphere or treatments prior to bringing the surfaces into contact. We can cite bonding at room temperature with or without prior plasma activation of the surfaces to be assembled, bonding by atomic diffusion ("Atomic diffusion bonding" or ADB according to the English terminology), bonding with surface activation ("Surface-activated bonding" or SAB), etc.
[0065] The assembly step may comprise, prior to bringing the faces to be assembled into contact, conventional cleaning sequences, surface activation or other surface preparations, capable of promoting the quality of the bonding interface 5 (low defectivity, high adhesion energy).
[0066] As already mentioned, the front face 30a of the donor substrate 30 and / or the free face of the support layer 2 may possibly comprise an intermediate layer, for example metallic (tungsten, etc.) or doped semiconducting (silicon, etc.) to promote vertical electrical conduction, or insulating (silicon oxide, silicon nitride, etc.) for applications not requiring vertical electrical conduction. The intermediate layer is capable of promoting bonding by molecular adhesion, in particular by erasing residual roughness or surface defects present on the faces to be assembled. It may undergo planarization or smoothing treatments, to achieve a roughness lower than 1 nm RMS, or even lower than 0.5 nm RMS, favorable to bonding.
[0067] The separation along the buried fragile plane 31 usually takes place by the application of a heat treatment at a temperature between 800°C and 1200°C ([fig.4c]). Such a heat treatment induces the development of cavities and microcracks in the buried fragile plane 31, and their pressurization by the light species present in gaseous form, until the propagation of a fracture along said fragile plane 31. Alternatively or jointly, a mechanical stress can be applied to the bonded assembly and in particular at the level of the buried fragile plane 31, so as to propagate or help to mechanically propagate the fracture leading to separation. At the end of this separation, on the one hand the composite structure 10 is obtained comprising the temporary substrate 1 made of graphite, the support layer 2 made of p-SiC and the useful layer 3 transferred in c-SiC, and on the other hand, the remainder 30' of the donor substrate. The useful layer 3 typically has a thickness between 100nm and 1500nm.The level and type of doping of the useful layer 3 is defined by the choice of the properties of the donor substrate 30 or can be adjusted subsequently via known techniques for doping semiconductor layers.
[0068] The free surface of the useful layer 3 is usually rough after separation: for example, it has a roughness of between 5nm and 100nm RMS (AFM, 20 micron x 20 micron scan). Cleaning and / or smoothing steps can be applied to restore a good surface condition (typically, a roughness of less than a few angstroms RMS on a 20 micron x 20 micron scan by AFM).
[0069] Alternatively, the free surface of the useful layer 3 may remain rough, as separated, when the following step of the method tolerates this roughness.
[0070] If the edges 1c and the rear face 1b of the temporary substrate 1 are not covered by a protective layer, the separation heat treatment is carried out in a controlled atmosphere free of oxygen.
[0071] Advantageously, a protective layer is deposited before this heat treatment, to relax the atmospheric conditions of said treatment. The protective layer may be formed in p-SiC as indicated with reference to the particular embodiment involving the second support layer 2', or in amorphous SiC.
[0072] In the particular embodiment implementing a second support layer 2', step c) may also comprise the transfer of a second useful layer 3' in c-SiC onto the second support layer 2', directly or via a second intermediate layer, involving a second bonding interface 5' ([fig.3b]).
[0073] The manufacturing method according to the invention then comprises a step d) of forming an active layer 4 on the useful layer 3 ([fig.2d]).
[0074] Advantageously, the active layer 4 is produced by epitaxial growth of at least one additional layer of doped monocrystalline silicon carbide, on the useful layer 3. This epitaxial growth is carried out in the conventional temperature range, namely between 1500°C and 1900°C and forms a layer with a thickness of the order of 1 micron to a few tens of microns, depending on the electronic components targeted.
[0075] The presence of a protective layer on the edges 1c and the rear face 1b of the temporary graphite substrate 1, in the composite structure 10 is required so that the aforementioned very high temperature treatments do not damage the graphite. As mentioned previously, this protective layer may for example consist of a layer of polycrystalline silicon carbide (second support layer 2') or amorphous silicon carbide.
[0076] The manufacturing method according to the invention may further comprise a step of producing all or part of the electronic components 40 on and / or in the active layer 4 ([fig.2d]'). The electronic components 40 may for example consist of transistors or other high voltage and / or high frequency components.
[0077] For their manufacture on and / or in the active layer 4, conventional steps of cleaning, deposition, lithography, implantation, etching, planarization and heat treatment are carried out. In particular, among the heat treatments mentioned, some aim to activate dopants introduced locally into the active layer 4 (or the useful layer 3), and are typically carried out at a temperature greater than or equal to 1600°C.
[0078] Note that in the particular embodiment implementing a second support layer 2' on the rear face of the temporary substrate 1, step d) may also comprise the formation of a second active layer on the second useful layer 3'; and step d') may comprise the development of all or part of second electronic components on and / or in said second active layer.
[0079] Finally, the manufacturing method according to the invention comprises a step e) of removing the temporary substrate 1 to form the semiconductor structure 100, said structure including the active layer 4, the useful layer 3 and the support layer 2 (figure 2e(i)), and potentially the electronic components 40 (figure 2e(ii)), if a step d has been carried out.
[0080] Several variants can be implemented for this step: certain variants (first and second variants described below) are based on the dismantling of said substrate 1 and therefore can potentially include its recycling for a new use; other variants (third and fourth variants) involve the partial or total elimination of the temporary substrate 1.
[0081] According to a first variant, step e) comprises mechanical disassembly by propagation of a crack in the temporary substrate 1 following the application of a mechanical stress, the crack extending substantially parallel to the plane of the interface between the temporary substrate 1 and the support layer 2, 2'. For example, the insertion of a beveled tool opposite or close to said interface allows to initiate and propagate an opening at this interface or in the graphite of the temporary substrate 1, until the complete separation between the semiconductor structure 100 and the temporary substrate 1. Advantageously, the protective layer present on the edges 1c of the temporary substrate 1 is removed, to promote the initiation of the crack in the graphite.
[0082] According to a second variant, step e) comprises a chemical disassembly between the support layer 2, 2' and the temporary substrate 1 by lateral chemical etching. The protective layer located on the edges 1c of the temporary substrate 1 in the composite structure 10 must be removed chemically or mechanically, to allow access to the graphite. The lateral chemical etching may in particular use a solution based on nitric acid and / or sulfuric acid, for example a solution of concentrated sulfuric acid and potassium dichromate or a solution of sulfuric acid, nitric acid and potassium chlorate. A chemical etching using an alkaline solution (of the potassium hydroxide (KOH) or sodium hydroxide (NaOH) type) may also be applied.
[0083] Of course, care will be taken to protect the free face and the edges of the active layer 4 and the electronic components 40 if they are present, and / or to limit the time of contact with the etching solution, to avoid damaging them during this chemical disassembly.
[0084] According to a third variant, step e) comprises a chemical etching of all or part of the temporary substrate 1. As mentioned previously, the protective layer on the edges 1c and on the rear face 1b (second support layer 2') of the temporary substrate 1 of the composite structure 10 will have to be removed to give access to the graphite. It will typically be possible to carry out a mechanical removal, for example by lapping the edges and the rear face ("edge grinding" or "grinding" according to the English terminology), or a chemical removal, depending on the nature of the protective layer. The chemical etching of the temporary substrate 1 may for example implement one of the solutions stated above for the second variant, taking care to protect the active layer 4 and potentially the components 40.
[0085] According to a fourth variant, step e) comprises disassembly by thermal damage of the graphite making up the temporary substrate 1. Here again, it is required to remove the protective layer present at least on the edges of the temporary substrate 1. When there is no second useful layer 3' on the rear face of the composite structure 10, the protective layer can also be removed from this face.
[0086] Disassembly by thermal damage can be carried out at a temperature between 600°C and 1000°C, in the presence of oxygen: the graphite of the temporary substrate 1 is then burnt and crumbles to leave only the semi-structure intact. driver 100.
[0087] Of course, in the case where the electronic components 40 have been produced during step d', this disassembly variant can only be applied if said components 40 are compatible with the temperature applied.
[0088] Note that the aforementioned variants may possibly be combined with each other, according to any technically feasible combination.
[0089] Regardless of the variant implemented, the removal of the temporary substrate 1 may leave residues on the rear face 2b of the support layer 2. These residues are then removed by lapping or mechanical grinding, by chemical-mechanical polishing, by chemical etching and / or by thermal damage. The chemical-mechanical polishing or chemical etching techniques may also be implemented to reduce the roughness of the rear face 2b of the support layer 2, if necessary.
[0090] In the particular embodiment mentioned above, for which a second support layer 2', a second useful layer 3' and a second active layer are arranged on the rear face 1b of the temporary substrate 1, step e) of removing the temporary substrate 1 also makes it possible to form a second semiconductor structure, said structure including the second active layer (and potentially electronic components), the second useful layer 3' and the second support layer 2'.
[0091] If the semiconductor structure 100 must be handled during and after the removal of the temporary substrate 1, and its total thickness is insufficient for its mechanical maintenance during this handling, it is possible to use a removable handle: the latter is arranged on the active layer 4 and temporarily secured to it, to carry out the handling up to the singulation step for example.
[0092] The semiconductor structure 100 obtained at the end of the manufacturing method according to the invention comprises an active layer 4 finalized with potentially electronic components 40, and arranged on a support layer 2 having the thickness targeted for the application. No mechanical thinning involving a significant loss of material is required. The support layer 2 is made of good quality p-SiC (because it is deposited at relatively high temperatures) but at low cost compared to a solid substrate of monocrystalline or polycrystalline SiC which would have had to be significantly thinned before singulating the components. The temporary graphite substrate 1 is advantageously recovered for recycling. If it is not reused, since graphite constitutes a low-cost material, the manufacturing method according to the invention remains economically advantageous compared to a solution with a solid SiC substrate.The choice of physical characteristics of the temporary graphite substrate 1 (grain size, porosity, coefficient of thermal expansion) ensures the . formation of a support layer 2 allowing the obtaining of a robust and high-quality composite structure 10, and allowing the obtaining of a reliable and high-performance semiconductor structure 100. The performance of the components 40 comes in particular from the fact that the composite structure 10 allows treatments at very high temperatures for the formation of the active layer 4.
[0093] The invention also relates to a composite structure 10, described previously with reference to the manufacturing method, and corresponding to an intermediate structure obtained during said method (figures 2c, 2d, 3b).
[0094] The composite structure 10 comprises: - a temporary graphite substrate 1 having a grain size of between 4 microns and 35 microns, a porosity of between 6 and 17%, and a coefficient of thermal expansion of between 4.10 6 / °C and 5.106 / °C,
[0095] - a support layer 2 made of polycrystalline silicon carbide having a thickness between 10 microns and 200 microns, at least arranged on one front face of the temporary substrate 1, - a useful layer 3 of monocrystalline silicon carbide, placed directly on the support layer 2 or via an intermediate layer.
[0096] Preferably, the useful layer 3 has a thickness of between 100 nm and 1500 nm. The temporary substrate 1 has a thickness of between 100 microns and 2000 microns.
[0097] For applications for vertical microelectronic components, the support layer 2 advantageously has good electrical conductivity, i.e. between 0.015 and 0.03 ohm.cm, high thermal conductivity, i.e. greater than or equal to 200 Wm '.K1 and a thermal expansion coefficient similar to that of the useful layer 3, i.e. typically between 3.8.10 6 / °C and 4.2.10 6 / °C at room temperature.
[0098] The temporary substrate 1 may advantageously have a thermal conductivity of between 70W.m '.K 1 and 130W.ni1.K *, so as to ensure a uniform temperature on the temporary substrate 1 during the very high temperature heat treatment steps of the manufacturing process. This improves in particular the uniformity of the deposited layers and the reproducibility of the physical properties of the layers and components produced.
[0099] Finally, as has been described with reference to the manufacturing method according to the invention, the composite structure 10 may be “double-sided”, that is to say comprise:
[0100] - a second support layer 2' made of polycrystalline silicon carbide having a thickness of between 10 microns and 200 microns, placed on the temporary substrate 1,
[0101] - a second useful layer 3' of monocrystalline silicon carbide, arranged on the second support layer 2' ([fig.3b]).
[0102] Such a composite structure 10 allows the formation of two active layers 4, respectively on the first 3 and the second 3' useful layer, and, at the end of the manufacturing method according to the invention, the obtaining of two semiconductor structures 100, from a single temporary substrate 1.
[0103] Of course, the invention is not limited to the embodiments and examples described, and variant embodiments may be made without departing from the scope of the invention as defined by the claims.
Claims
Claims
1. A method of manufacturing a semiconductor structure (100), comprising: a) a step of providing a temporary graphite substrate (1) having a grain size of between 4 microns and 35 microns, a porosity of between 6 and 17%, and a coefficient of thermal expansion of between 4.10 6 / °C and 5.10 6 / °C; b) a step of depositing, on a front face (la) of the temporary substrate (1), a support layer (2) of polycrystalline silicon carbide having a thickness of between 10 microns and 200 microns, c) a step of transferring a useful layer (3) of monocrystalline silicon carbide onto the support layer (2), directly or via an intermediate layer, to form a composite structure (10), said transfer implementing bonding by molecular adhesion, d) a step of forming an active layer (4) on the useful layer (3), e) a step of removing the temporary substrate (1) to form the semiconductor structure (100), said structure including the active layer (4), the useful layer (3) and the support layer (2).
2. Manufacturing method according to the preceding claim, in which the deposition of step b) is also carried out: - on a rear face (1b) of the temporary substrate (1) to form a second support layer (2'), and / or - on a peripheral edge (le) of said substrate (1).
3. Manufacturing method according to one of the preceding claims, in which the transfer step c) comprises: - the introduction of light species into a donor substrate (30) made of monocrystalline silicon carbide, to form a buried fragile plane (31) defining with a front face (30a) of the donor substrate (30), the useful layer (3), - the assembly of the front face (30a) of the donor substrate (30) on the support layer (2), directly or via an intermediate layer, by bonding by molecular adhesion, - the separation along the buried fragile plane (31) to transfer the useful layer (3) onto the support layer (2).
4. A manufacturing method according to the preceding claim, wherein the intermediate layer is formed from tungsten, silicon, carbide, silicon or other conductive or semiconducting materials.
5. Manufacturing method according to one of the preceding claims, in which step d) comprises epitaxial growth of at least one additional layer of doped monocrystalline silicon carbide, on the useful layer (3), said additional layer forming all or part of the active layer (4).
6. Manufacturing method according to one of the preceding claims, comprising a step d) of producing all or part of the electronic components (40) on and / or in the active layer (4), step d) being interposed between step d) and step e).
7. Manufacturing method according to one of the preceding claims, wherein: - step e) comprises mechanical disassembly by propagation of a crack in the temporary substrate (1) following the application of a mechanical stress, the crack extending substantially parallel to the plane of the interface between the temporary substrate (1) and the support layer (2), and / or - step e) comprises chemical disassembly between the support layer (2) and the temporary substrate (1) by lateral chemical etching, and / or - step e) comprises chemical etching of all or part of the temporary substrate (1), and / or - step e) comprises disassembly by thermal damage to the graphite of the temporary substrate (1).
8. Manufacturing method according to claim 2, wherein: - step c) comprises the transfer of a second useful layer (3') of monocrystalline silicon carbide onto the second support layer (2'), directly or via a second intermediate layer, said transfer implementing bonding by molecular adhesion, - step d) comprises the formation of a second active layer on the second useful layer (3'), - step e) makes it possible to form a second semiconductor structure (100), said structure including the second active layer, the second useful layer (3') and the second support layer (2').
9. Manufacturing method according to one of the preceding claims, wherein the temporary substrate (1), provided in step a), has a circular wafer shape and a diameter 5% to 10% larger than a diameter targeted for the semiconductor structure (100).
10. Manufacturing method according to one of claims 1 to 8, in which the temporary substrate (1), provided in step a), has a circular wafer shape and a diameter slightly smaller than a diameter targeted for the semiconductor structure (100), so that the deposition of step b), also carried out on a peripheral edge (le) of the temporary substrate (1), makes it possible to achieve said targeted diameter.
11. Composite structure (10) comprising: - a temporary substrate (1) made of graphite having a grain size of between 4 microns and 35 microns, a porosity of between 6 and 17%, and a coefficient of thermal expansion of between 4.10 6 / °C and 5.106 / °C, - a support layer (2) made of polycrystalline silicon carbide having a thickness of between 10 microns and 200 microns, at least arranged on a front face of the temporary substrate (1), - a useful layer (3) made of monocrystalline silicon carbide, arranged on the support layer (2).
12. Composite structure according to the preceding claim, in which the useful layer (3) has a thickness of between 100 nm and 1500
13. llili. Composite structure according to one of the two preceding claims, in which the temporary substrate (1) has a thickness of between 100 microns and 2000 microns.
14. Composite structure according to one of the three preceding claims, in which the temporary substrate (1) has a thermal conductivity of between 70 Wm *.K1 and 130 Wm *.K '.
Citation Information
Cited By
METHOD FOR MANUFACTURING A MULTILAYER STRUCTURE AND AN INTERMEDIATE MULTILAYER STRUCTURE
FR3169057A1
METHOD FOR MANUFACTURING A BEARING SUBSTRATE AND BEARING SUBSTRATE
FR3170209A1
METHOD FOR MANUFACTURING A MULTILAYER STRUCTURE AND MULTILAYER STRUCTURE
FR3173772A1
Method for producing a multilayer structure and intermediate multilayer structure
WO2026109745A1
Method for manufacturing a carrier substrate, and carrier substrate
WO2026131596A1