Method of manufacturing semiconductor device using isolation structure
By forming an isolation structure inside and outside the stack and performing chemical mechanical polishing during the semiconductor device manufacturing process, the physical stress and process risks caused by the different hardness of the materials in the semiconductor device manufacturing are solved, and the manufacturing efficiency and quality are improved.
Patent Information
- Application Number
- CN202311390667.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-03-29
- Filing Date
- 2023-10-25
- Publication Date
- 2024-10-01
AI Technical Summary
In the manufacturing process of semiconductor devices, as the width of two-dimensional planar metal lines decreases, manufacturing equipment and investment costs increase, the development cycle is extended, and there are physical stresses and process risks caused by different hardnesses of materials in the planarization process, such as film peeling. Phenomenon.
By forming openings in and on the stack, depositing storage layers and conductive layers, and forming isolation structures on the conductive and storage layers, planarization using a chemical mechanical polishing process until the stack is exposed reduces physical stress and process risks.
It effectively reduces the physical stress in the planarization process, reduces process risks such as film peeling, and improves the manufacturing efficiency and quality of semiconductor devices.
Smart Images

Figure CN118742045A_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims priority to Korean Patent Application No. 10-2023-0041145 filed on Mar. 29, 2023, which is hereby incorporated by reference in its entirety. Technical Field
[0003] Embodiments relate to a planarization process method, and more particularly, to a method of manufacturing a semiconductor device using an isolation structure in a planarization process. Background Art
[0004] Recently, as electronic devices are reduced in size, have low power consumption and high performance, and are diversified, various electronic devices such as computers and portable communication devices require semiconductor devices capable of storing information. Accordingly, semiconductor devices capable of storing data by utilizing the characteristic of switching different resistance states according to a voltage or current applied to the semiconductor device are studied. Such semiconductor devices include resistive random access memory (RRAM), phase change random access memory (PRAM), ferroelectric random access memory (FRAM), magnetic random access memory (MRAM), and electric fuses.
[0005] In order to reduce the size of a semiconductor device and increase the data storage capacity of the semiconductor device, a semiconductor device has been developed such that many memory cells are integrated in the same area by reducing a metal line width in a two-dimensional plane.
[0006] Due to problems associated with manufacturing equipment, investment costs, and development cycles as the width of metal lines in a two-dimensional plane decreases, methods of manufacturing semiconductor devices as three-dimensional structures are being studied and developed. Summary of the invention
[0007] In an embodiment, a manufacturing method may include: forming an opening in a stack, forming a variable resistance layer in the opening and on the stack, forming a conductive layer on the variable resistance layer, forming a conductive pattern by etching the conductive layer, the conductive pattern including a first portion in the opening and a second portion on the stack, forming a variable resistance pattern by etching the variable resistance layer, the variable resistance pattern including a first portion in the opening and a second portion on the stack, and planarizing the conductive pattern and the variable resistance pattern until the stack is exposed.
[0008] In an embodiment, a method for manufacturing a semiconductor device may include: forming a stack, the stack including a first material layer and a second material layer alternately stacked, forming an opening in the stack, forming a storage layer in the opening and on the stack, forming a first conductive layer on the storage layer, forming an isolation structure in the storage layer and the first conductive layer, and planarizing the first conductive layer, the storage layer, and the isolation structure until the stack is exposed.
[0009] In an embodiment, a method for manufacturing a semiconductor device may include: forming a stack, forming an opening in the stack, forming a storage layer in the opening and on the stack, forming a conductive layer on the storage layer, forming conductive patterns and grooves separating the conductive patterns from each other by etching the conductive layer, each of the conductive patterns including a first portion in the opening and a second portion connected to the first portion and disposed on the stack; and forming an isolation structure in the groove. BRIEF DESCRIPTION OF THE DRAWINGS
[0010] Figure 1A , Figure 2A , Figure 3A , Figure 4A , Figure 5A , Fig. 6A as well as Fig. 7A is a cross-sectional view for describing a manufacturing method according to an embodiment of the present disclosure.
[0011] Figure 1B , Figure 2B , Figure 3B , Figure 4B , Figure 5B , Figure 6B as well as Figure 7B is a plan view for describing a manufacturing method according to an embodiment of the present disclosure.
[0012] Fig. 8A and Figure 8B is a view for describing a planarization process according to an embodiment of the present disclosure.
[0013] Fig.9A and Fig. 9B is a plan view of an isolation structure according to an embodiment of the present disclosure.
[0014] Fig. 10A and Fig. 10B 2 is a view for describing a semiconductor device according to an embodiment of the present disclosure.
[0015] Fig.11A , Fig. 11B , Fig. 11C , Fig.11D , Fig.11E , Fig.11F , Fig.11G as well as Fig.11His a view for describing a method of manufacturing a semiconductor device according to an embodiment of the present disclosure. DETAILED DESCRIPTION
[0016] Hereinafter, embodiments according to the technical spirit of the present disclosure are described with reference to the accompanying drawings.
[0017] Embodiments of the present disclosure provide a manufacturing method for reducing the risk of a planarization process of materials having different hardness values, and a method of manufacturing a semiconductor device using the manufacturing method.
[0018] The risk of a planarization process for materials having different hardnesses (eg, film peeling) can be reduced.
[0019] Figure 1A , Figure 2A , Figure 3A , Figure 4A , Figure 5A , Fig. 6A as well as Fig. 7A is a cross-sectional view for describing a manufacturing method according to an embodiment of the present disclosure. In this article, Figure 1A , Figure 2A , Figure 3A , Figure 4A , Figure 5A , Fig. 6A as well as Fig. 7A A cross-sectional view of the semiconductor device according to planes defined in a first direction I and a third direction III may be illustrated.
[0020] Figure 1B , Figure 2B , Figure 3B , Figure 4B , Figure 5B , Figure 6B as well as Figure 7B is a plan view of a semiconductor device for describing a manufacturing method according to an embodiment of the present disclosure. In this case, Figure 1B , Figure 2B , Figure 3B , Figure 4B , Figure 5B , Figure 6B as well as Figure 7B It can be a plan view of a semiconductor device. Figure 1A , Figure 2A , Figure 3A , Figure 4A , Figure 5A , Fig. 6A as well as Fig. 7A Can be respectively along Figure 1B , Figure 2B , Figure 3B , Figure 4B , Figure 5B , Figure 6Band a cross-sectional view taken along line AA' in 7B.
[0021] refer to Figure 1A and 1B , a stack 10 may be formed. The stack 10 may include an insulating layer or may include a conductive layer. As an embodiment, the stack 10 may include a first material layer and a second material layer that have been alternately stacked. An opening OP may be formed in the stack 10. As an embodiment, a plurality of openings OP may be arranged along a first direction I and a second direction II intersecting the first direction I. The opening OP may extend along a third direction III in the stack 10. In this case, the third direction III may be a direction orthogonal to a plane defined by the first direction I and the second direction II.
[0022] refer to Figure 2A and Figure 2B , a storage layer 20 may be formed. In this case, the storage layer 20 may include a floating gate, polysilicon, a charge trapping material, a nitride, a variable resistance material, or a phase change material. In an embodiment, a storage layer (e.g., a variable resistance layer) 20 may be formed on the stack 10. When the present disclosure describes the first layer as being "on" or "above" the second layer, it not only indicates that the first layer is directly on or above the second layer without any intermediate layer therebetween, but also indicates that the first layer is on or above the second layer and there are one or more intermediate layers between the first layer and the second layer. The storage layer 20 may be formed along the outline of the stack 10. As an embodiment, the storage layer 20 may be deposited along the inner side of the opening OP and the upper surface of the stack 10. Figure 2B There may be a view showing the memory layer 20 - 1 disposed along the inner side of the opening OP and the memory layer 20 - 2 disposed along the upper surface of the stack 10 .
[0023] refer to Figure 3A and Figure 3B , a conductive layer 30 may be formed. In this case, the conductive layer 30 may be suitable for forming a gate line, such as a word line or a bit line. The conductive layer 30 may include a conductive material such as polysilicon or a metal. The conductive layer 30 may be formed on the storage layer 20. The conductive layer 30 may be deposited along the contour of the storage layer 20. The conductive layer 30 may be formed within the opening OP and on the stack 10. The storage layer 20 and the conductive layer 30 may have different hardness values. As an embodiment, the hardness of the storage layer 20 may be less than the hardness of the conductive layer 30.
[0024] refer to Figure 4A and Figure 4B, a mask pattern M may be formed. As an embodiment, after forming a mask layer on the conductive layer 30, the mask pattern M may be formed by patterning the mask layer. The mask pattern M may have a form in which the mask pattern covers the opening OP and at least partially exposes the area between the openings OP. As an embodiment, the mask pattern M may include a line pattern extending along the second direction II, and may expose a portion of the conductive layer 30 located between the line patterns.
[0025] refer to Figure 5A and Figure 5B , a trench T may be formed by etching the conductive layer 30 and the storage layer 20 using the mask pattern M as an etching barrier. Accordingly, a conductive pattern 30A may be formed, the conductive pattern including a first portion 30_P1 located within the opening OP and a second portion 30_P2 connected to the first portion 30_P1 and disposed above the stack 10. In a cross section defined along the first direction I and the third direction III, the conductive pattern 30A may have a T shape. A storage pattern 20A may be formed, the storage pattern including a first portion 20_P1 located within the opening OP and a second portion 20_P2 connected to the first portion 20_P1 and disposed above the stack 10. The conductive patterns 30A may be separated from each other by the trench T. The storage patterns 20A may be separated from each other by the trench T. Next, the mask pattern M may be removed.
[0026] refer to Fig. 6A and Figure 6B , an isolation structure 40 may be formed in the trench T. Specifically, the isolation structure 40 may be formed in the trench T corresponding to the space where the conductive layer 30 and the memory layer 20 have been etched using the mask pattern M. For example, the isolation structure 40 may be formed between a pair of adjacent second portions 30_P2 of the conductive pattern 30A disposed on the stack 10, and between a pair of adjacent second portions 20_P2 of the memory pattern 20A disposed on the stack 10. The isolation structure 40 may include a material having a greater hardness than the memory pattern 20A. As an embodiment, the isolation structure 40 may include an insulating material such as an oxide or a nitride.
[0027] refer to Fig. 7A and Figure 7B , the conductive pattern 30A and the storage pattern 20A may be planarized until the stack 10 is exposed. The planarization process may be performed by using a chemical mechanical polishing (CMP) process. Accordingly, the conductive pattern 30B and the storage pattern 20B may be formed within the opening OP. In this case, the conductive pattern 30B may be a bit line.
[0028] Fig. 8A and Figure 8Bis a view for describing a planarization process according to an embodiment of the present disclosure.
[0029] Fig. 8A It may be shown that the amount of stress applied to the memory layer 20 when the planarization process is performed without forming the isolation structure 40. Since the planarization process is performed until the stack 10 is exposed, a mechanical stress S having an amount corresponding to a region of the memory layer 20 formed on the stack 10 may be transferred to the memory layer 20.
[0030] Figure 8B It may be shown that the amount of stress applied to the memory pattern 20A when the planarization process is performed after forming the isolation structure 40. Since the planarization process is performed until the stack 10 is exposed, a mechanical stress S having an amount corresponding to the region of the memory pattern 20A formed on the stack 10 may be transferred to the memory pattern 20A.
[0031] That is, with Fig. 8A Compared with the area of the storage layer 20 in FIG. 1 , the area of the storage layer 20 in FIG. 1 has been reduced by forming the isolation structure 40. Figure 8B Accordingly, compared with the manufacturing method in which the planarization process is performed without forming the isolation structure 40, according to Figure 8B The manufacturing method of performing a planarization process of an embodiment can reduce the physical stress applied to the memory pattern 20A. In addition, without wishing to be limited by theory, the isolation structure 40 may include a material having an elastic modulus greater than that of the memory pattern 20A. As a result, when the planarization process is performed, the isolation structure 40 can support a relatively large amount of force applied thereto, thereby reducing the amount of stress applied to the memory pattern 20A. In addition, the isolation structure 40 including a material having a greater hardness than the memory pattern 20A can also play a role in dispersing the physical stress applied to the memory pattern 20A.
[0032] As a result, since the planarization process is performed after forming the isolation structure, the manufacturing method according to the embodiment of the present disclosure can reduce the physical stress occurring in the planarization process. In addition, the manufacturing method can reduce process risks such as film peeling by reducing the physical stress occurring in the planarization process.
[0033] Fig.9A and Fig. 9B is a plan view of an isolation structure according to another embodiment of the present disclosure.
[0034] refer to Fig.9A, the isolation structure 40 may include an opening form having the same size and shape as the opening OP. Therefore, the area between the openings OP, that is, the conductive layer 30 and the memory layer 20 formed on the stack 10 may be removed by the isolation structure 40. In addition, the memory layers 20 respectively formed in the openings OP may be separated from each other by the isolation structure 40.
[0035] refer to Fig. 9B , the isolation structure 40 may have a polygonal (e.g., quadrilateral) form surrounding the opening OP. Therefore, the isolation structure 40 may remove the region between the openings OP, that is, the portion of the conductive layer 30 and the memory layer 20 formed on the stack 10. Accordingly, the conductive layer 30 and the memory layer 20 formed within the polygon may be separated from each other by the isolation structure 40.
[0036] As in Figure 6B , Fig.9A and Fig. 9B In the embodiment, the isolation structure 40 may be used to remove part or all of the conductive layer 30 and the memory layer 20 formed on the stack 10, and may be implemented in various forms.
[0037] Fig. 10A and Fig. 10B 1 is a view for describing a semiconductor device according to an embodiment of the present disclosure. Hereinafter, for the sake of brevity, contents repeated with the foregoing contents may be omitted.
[0038] refer to Fig. 10A , a semiconductor device according to an embodiment of the present disclosure may include a substrate 100 , a first insulating layer 110 , a second insulating layer 120 , a first conductive layer 131 , a second conductive layer 132 , and a memory layer 140 .
[0039] The first insulating layer 110 and the second insulating layer 120 may be alternately stacked on the substrate 100. The first conductive layers 131 may be each disposed between the second insulating layer 120 and each second conductive layer 132. In this case, the first conductive layers 131 may each be a word line. As an embodiment, the first conductive layer 131 may include a conductive material such as polysilicon or a metal. The first insulating layer 110 may be suitable for insulating the already stacked first conductive layers 131 from each other. The second insulating layer 120 may be used to insulate the first conductive layers 131 adjacent to each other in the first direction I from each other. As an embodiment, the first insulating layer 110 and the second insulating layer 120 may each include an insulating material such as an oxide, a nitride, or an air gap.
[0040] The second conductive layer 132 and the memory layer 140 may penetrate the first insulating layer 110 and the first conductive layer 131 and may extend in the third direction III. The second conductive layer 132 may be a bit line.
[0041] The memory cell MC may be disposed at a region where the first conductive layer 131 and the second conductive layer 132 cross each other. The memory cell MC may include the first conductive layer 131 , the second conductive layer 132 , and a memory layer 140 .
[0042] The storage layer 140 may include a floating gate, polysilicon, a charge trapping material, a nitride, a variable resistance material, or a phase change material. As an embodiment, the storage layer 140 may include a chalcogenide material. The storage layer 140 may have two states according to the electrical signal provided by the word line and the bit line. For example, the state of the storage layer 140 may be changed to a reset state or a set state by a programming operation. The reset state and the set state may be states with different resistance levels. For example, the reset state and the set state may be states with different phases.
[0043] refer to Fig. 10B , the semiconductor device according to the embodiment of the present disclosure may further include an isolation structure IS formed on the first insulating layer 110. The second conductive pattern 132A may have a T-shaped cross-section and may include a first portion located within the stack ST and a second portion located above the stack ST. The storage pattern 140A may include a first portion located within the stack ST and a second portion located above the stack ST. The wiring 150 may be connected to the isolation structure IS and the second conductive pattern 132A. The wiring 150 may be electrically connected to the second conductive pattern 132A, i.e., a bit line. The bit line and the peripheral circuit may be electrically connected through the wiring 150.
[0044] Fig.11A , Fig. 11B , Fig. 11C , Fig.11D , Fig.11E , Fig.11F , Fig.11G , Fig.11H is a view for describing a method of manufacturing a semiconductor device according to an embodiment of the present disclosure.
[0045] refer to Fig.11A , a stacked ST may be formed. The stacked ST may be formed by alternately stacking first material layers 110 and second material layers 120 on the semiconductor substrate 100. As an embodiment, the first material layers 110 may each include a material having a higher etching selectivity ratio than the second material layers 120. The first material layers 110 may each include an oxide, and the second material layers 120 may each include a nitride. The first material layers 110 may each include a nitride, and the second material layers 120 may each include an oxide.
[0046] refer to Fig. 11B, an opening OP may be formed in the stack ST. As an embodiment, a plurality of openings OP may be arranged in a first direction I and a second direction II intersecting the first direction I. The opening OP may extend along a third direction III in the stack ST. In this case, the third direction III may be a direction orthogonal to a plane defined by the first direction I and the second direction II.
[0047] refer to Fig. 11C , a space (eg, a recess) R in which a word line is to be disposed may be formed within the opening OP. As an embodiment, the recess R may be formed by selectively etching the second material layer 120 within the opening OP.
[0048] refer to Fig.11D , a first conductive layer 131 may be formed in each recess R. In this case, the first conductive layer 131 may be a word line WL. The first conductive layer 131 may include a conductive material such as polysilicon or metal.
[0049] refer to Fig.11E , a storage layer (or initial storage layer) 140 may be formed. The storage layer 140 may include a floating gate, polysilicon, a charge trapping material, a nitride, a variable resistance material, or a phase change material. As an embodiment, the storage layer 140 may be formed in the opening OP and on the stack ST. For example, the storage layer 140 may be deposited along the inner side of the opening OP and the upper surface of the stack ST.
[0050] Next, a second conductive layer (or initial second conductive layer) 132 may be formed. The second conductive layer 132 may be used to form a bit line. The second conductive layer 132 may include a conductive material such as polysilicon or a metal. As an embodiment, the second conductive layer 132 may be formed on the storage layer 140. The second conductive layer 132 may be deposited along the contour of the storage layer 140. The second conductive layer 132 may be formed within the opening OP and on the stack ST. The storage layer 140 and the second conductive layer 132 may have different hardness values. As an embodiment, the hardness of the storage layer 140 may be less than the hardness of the second conductive layer 132.
[0051] refer to Fig.11F, a mask pattern M may be formed. As an embodiment, after forming a mask layer on the second conductive layer 132, the mask pattern M may be formed by patterning the mask layer. The mask pattern M may cover the storage layer 140 and the second conductive layer 132 formed within each opening OP, and may have a form in which the mask pattern at least partially exposes a region of the second conductive layer 132 formed on the stack ST. The mask pattern M may include one or more line patterns each extending in the second direction II, and may expose the second conductive layer 132 between the line patterns. For example, the mask pattern M may expose one or more portions of the second conductive layer 132 formed on the stack ST, such that each of these portions is located between pairs of adjacent line patterns of the mask pattern M.
[0052] Next, the trench T may be formed by etching the second conductive layer 132 and the memory layer 140 using the mask pattern M as an etching barrier. Portions of the second conductive layer 132 and the memory layer 140 formed on the stack ST may be removed through the trench T so that a second conductive pattern 132A and a memory pattern 140A may be formed. Next, the mask pattern M may be removed. The second conductive pattern 132A may have a T-shaped cross section and may include a first portion located within the opening OP and a second portion connected to the first portion and disposed on the stack ST. The memory pattern 140A may include a first portion within the opening OP and a second portion connected to the first portion and disposed on the stack ST.
[0053] refer to Fig.11G , an isolation structure IS may be formed within the trench T. For example, the isolation structure IS may be formed between the second portions of the adjacent pairs of second conductive patterns 132A and between the second portions of the adjacent pairs of memory patterns 140A. The isolation structure IS may include a material having a greater hardness than the memory layer 140. As an embodiment, the isolation structure IS may include an insulating material such as oxide or nitride.
[0054] refer to Fig.11H, the second conductive pattern 132A and the storage pattern 140A may be planarized until the stack ST is exposed. For example, the second conductive pattern 132A, the isolation structure IS, and the storage pattern 140A may be planarized until the stack ST is exposed to retain a first portion of the second conductive pattern 132A within the opening OP and a first portion of the storage pattern 140A within the opening OP. A chemical mechanical polishing (CMP) process may be used as a planarization process. Next, a metal process may be performed to connect the wiring 150 to the second conductive layer 132B located within the opening OP. For example, the wiring 150 may be connected to the first portion of the second conductive pattern 132A that remains within the opening OP. In this case, the wiring 150 may connect a bit line (e.g., Fig. 10A The second conductive layer 132 in the body) and the peripheral circuits.
[0055] For reference, the planarization process may be omitted. As an embodiment, after forming the isolation structure IS, a wiring may be formed so that the wiring is connected to the second conductive pattern 132A having a T shape. Accordingly, the reference structure may be manufactured. Fig. 10B A semiconductor device is described.
[0056] Since the planarization process is performed in a state where the isolation structure IS is already formed until the stack ST is exposed, the method of manufacturing a semiconductor device according to an embodiment of the present disclosure can reduce the physical stress applied to the memory pattern 140A due to the planarization process. In addition, the method can reduce the process risk by preventing the film peeling phenomenon of the memory layer 140 caused by the planarization process.
[0057] The method of manufacturing a semiconductor device according to an embodiment of the present disclosure is not limited to a method of forming a word line (i.e., the first conductive layer 131), a memory cell (i.e., a memory cell MC including a memory layer 140 disposed between the first conductive layer 131 and the second conductive layer 132), and a bit line (i.e., the second conductive layer 132), and can be applied to a manufacturing method for planarizing a plurality of other layers having different hardnesses at the same time. Accordingly, the risk of a layer having a relatively low hardness being damaged in a planarization process can be significantly reduced.
[0058] Accordingly, the manufacturing method according to the present disclosure can also be applied to the technology of forming word lines, memory cells, and bit lines by using a manufacturing method different from the method of manufacturing a semiconductor device according to the embodiment of the present disclosure. More specifically, although different methods are used to manufacture word lines, memory cells, and bit lines, those skilled in the art can practice the manufacturing method of forming an isolation structure according to the embodiment of the present disclosure to remove the storage layer and the conductive layer formed on the stack for forming the storage layer and the conductive layer in the opening in the stack.
[0059] Although the embodiments according to the technical spirit of the present disclosure have been described above with reference to the accompanying drawings, the embodiments are provided only to describe specific embodiments according to the concept of the present disclosure, and the embodiments of the present disclosure are not limited to these embodiments. A person of ordinary skill in the art to which the present disclosure belongs may replace, modify and change the embodiments in various ways without departing from the technical spirit of the present disclosure written in the claims. These replacements, modifications and changes may fall within the scope of the present disclosure.
Claims
1. A manufacturing method comprising: forming an opening in the stack; forming a variable resistance layer in the opening and on the stack; forming a conductive layer on the variable resistance layer; forming a conductive pattern by etching the conductive layer, the conductive pattern comprising a first portion located in the opening and a second portion located on the stack; forming a variable resistance pattern by etching the variable resistance layer, the variable resistance pattern comprising a first portion located in the opening and a second portion located on the stack; as well as The conductive pattern and the variable resistance pattern are planarized until the stack is exposed.
2. The manufacturing method according to claim 1, further comprising: An isolation structure is formed in a space where the conductive layer and the variable resistance layer have been etched, the isolation structure having a greater hardness than the variable resistance layer.
3. The manufacturing method according to claim 2, wherein: The step of forming the isolation structure comprises: forming a mask pattern that covers the opening and exposes a portion of the conductive layer; forming a trench by etching the conductive layer and the variable resistance layer using the mask pattern as an etch barrier; and The isolation structure is formed in the trench.
4. The manufacturing method according to claim 3, wherein: The step of forming a mask pattern comprises: forming a mask layer on the conductive layer; and The mask layer is patterned to form the mask pattern covering the opening and exposing a portion of the conductive layer.
5. A method for manufacturing a semiconductor device, comprising: forming a stack comprising alternatingly stacked layers of a first material and layers of a second material; forming an opening in the stack; forming a storage layer within the opening and on the stack; forming a first conductive layer on the storage layer; forming an isolation structure in the storage layer and the first conductive layer; as well as The first conductive layer, the storage layer, and the isolation structure are planarized until the stack is exposed.
6. The method of claim 5, wherein: The memory layer includes a variable resistance material.
7. The method of claim 5, wherein: The isolation structure includes a material having a greater hardness than the memory layer.
8. The method of claim 5, wherein: The step of forming the isolation structure comprises: forming a mask pattern on the first conductive layer; forming a trench by etching the first conductive layer and the memory layer using the mask pattern as an etch barrier; and The isolation structure is formed in the trench.
9. The method of claim 8, wherein: The mask pattern covers the opening and exposes a portion of the first conductive layer formed over the stack.
10. The method of claim 5, further comprising: selectively etching the first material layer; as well as A second conductive layer is formed in the selectively etched space.
11. A method for manufacturing a semiconductor device, comprising: Form a stack; forming an opening in the stack; forming a storage layer within the opening and on the stack; forming a conductive layer on the storage layer; forming conductive patterns and grooves separating the conductive patterns from each other by etching the conductive layer, each of the conductive patterns including a first portion located within the opening and a second portion connected to the first portion and disposed on the stack; as well as An isolation structure is formed in the trench.
12. The method of claim 11, wherein: The isolation structure has a greater hardness than the storage layer.
13. The method of claim 11, wherein: The steps of forming the groove include: forming a mask pattern that covers the opening and exposes a portion of the conductive pattern disposed over the stack; and A trench is formed by etching the second portion and a portion of the memory layer using the mask pattern as an etch barrier.
14. The method of claim 11, wherein: A wiring is connected to a first portion of each of the conductive patterns.
15. The method of claim 14, further comprising: forming storage patterns by etching the storage layer, each of the storage patterns comprising a first portion located within the opening and a second portion connected to the first portion and disposed on the stack; as well as The grooves separate the storage patterns from each other.
16. The method of claim 15, wherein: The isolation structure is formed between the second portions of the adjacent pairs of the conductive patterns and between the second portions of the adjacent pairs of the storage patterns.
17. The method of claim 11, wherein: Wiring is connected to the isolation structure and the conductive pattern.
18. The method of claim 17, wherein: The wiring is electrically connected to the conductive pattern and the peripheral circuit.