Phase change memory cell with dual active volumes
By adopting a physically symmetrical mushroom-shaped unit device structure in the phase change memory unit and utilizing the symmetrical thermal constraints of the internal electrodes and filament layers, the polarity dependence of the phase change memory unit in neuromorphic computing in the prior art is solved. The problem of high programming current and high power consumption is achieved, and more efficient computing speed and energy efficiency are achieved.
Patent Information
- Application Number
- CN202380022859.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-03-02
- Filing Date
- 2023-02-21
- Publication Date
- 2024-10-01
AI Technical Summary
Existing phase-change memory cells suffer from polarity dependence, large programming current, and high power consumption in neuromorphic computing, especially in analog computing, which limits their speed and accuracy.
Adopting a physically symmetrical mushroom-shaped unit device structure, by forming internal electrodes and filament layers in the phase change material layer, it provides symmetrical thermal confinement, reduces programming current, and reduces power consumption during simulation calculations.
The symmetric read operation is realized, which reduces the read time and power consumption, improves the calculation speed and energy efficiency, and reduces the unit's programming current and power consumption.
Smart Images

Figure CN118743333A_ABST
Abstract
Description
Background Art
[0001] The present invention generally relates to a phase change memory cell, and more particularly to a phase change memory cell with dual active volumes.
[0002] Phase change memory cells can be used for data storage. Phase change memory cells are non-volatile random access memories. A typical configuration of a phase change memory cell may include a phase change material arranged between and coupled to at least two electrodes. When using a phase change memory cell, the phase change material can be operated in one of at least two reversibly transformable phases, namely an amorphous phase and a crystalline phase. The amorphous phase and the crystalline phase are different from each other. In the amorphous phase, the phase change material has a significantly higher resistance than the crystalline phase. In order to promote the phase transition, energy is provided to the phase change material, such as electrical energy, thermal energy, any other suitable form of energy, or a combination thereof, which can achieve the desired phase transition. Summary of the invention
[0003] According to an embodiment of the present invention, a structure is provided. The structure may include: a first phase-change material layer vertically aligned above a bottom electrode; a dielectric layer vertically aligned above the first phase-change material layer; a second phase-change material layer vertically aligned above the dielectric layer; an inner electrode physically and electrically connected to the first phase-change material layer and the second phase-change material layer, the inner electrode being surrounded by the dielectric layer; and a top electrode vertically aligned above the second phase-change material layer.
[0004] In another embodiment, the lateral diameter of the inner electrode is less than the lateral diameter of the bottom electrode. Embodiments also include a first raised pad vertically aligned between the first phase change material layer and the dielectric layer and a second raised pad vertically aligned between the second phase change material layer and the dielectric layer. Embodiments also include a first thermal barrier layer vertically aligned between the first phase change material layer and the dielectric layer and a first thermal barrier layer vertically aligned between the second phase change material layer and the dielectric layer. Embodiments also include a first adhesion layer vertically aligned between the first phase change material layer and the dielectric layer and a first adhesion layer vertically aligned between the second phase change material layer and the dielectric layer.
[0005] According to an embodiment of the present invention, a structure is provided. The structure includes: a first phase change material layer aligned over a first portion of an internal electrode; a first external electrode vertically aligned over the first phase change material layer; a second phase change material layer aligned over a second portion of the internal electrode; a second external electrode vertically aligned over the second phase change material layer; and a dielectric layer vertically physically and electrically separating the first phase change material layer and the first external electrode from the second phase change material layer and the second external electrode.
[0006] According to an embodiment of the present invention, a structure is provided. The structure includes: a first phase change material layer aligned above a first external electrode; an internal electrode physically and electrically connected between the first phase change material layer and a second phase change material layer; a second external electrode vertically aligned above the second phase change material layer; and a dielectric layer vertically physically and electrically separating the first phase change material layer and the first external electrode from the second phase change material layer and the second external electrode.
[0007] According to an embodiment of the present invention, a structure is provided. The structure includes: a first phase change material layer vertically aligned above a bottom electrode; a filament layer vertically aligned above the first phase change material layer; a second phase change material layer vertically aligned above the filament layer; an internal break in the filament layer connecting the first phase change material layer and the second phase change material layer; and a top electrode vertically aligned above the second phase change material layer.
[0008] In another embodiment, the filament layer comprises a high-k dielectric. In one embodiment, the filament layer comprises a mixed ion-electronic conductive filament. The embodiment further comprises a first pad vertically aligned between the first phase change material layer and the filament layer and a second pad vertically aligned between the second phase change material layer and the filament layer. In one embodiment, the first pad and the second pad are each a raised layer. In one embodiment, the first pad and the second pad are each a thermal barrier layer. In one embodiment, the first pad and the second pad are each an adhesion layer. The embodiment further comprises a first pad vertically aligned between the first phase change material layer and the bottom electrode and a second pad vertically aligned between the second phase change material layer and the top electrode. In one embodiment, the first pad and the second pad are each a raised layer. In one embodiment, the first pad and the second pad are each a thermal barrier layer. In one embodiment, the first pad and the second pad are each an adhesion layer.
[0009] According to an embodiment of the present invention, a method is provided. The method may include: forming a first phase-change material layer above a bottom electrode; forming a dielectric layer above the first phase-change material layer; forming an internal electrode in the dielectric layer; forming a second phase-change material layer above the dielectric layer, wherein the internal electrode is physically and electrically connected to both the first phase-change material layer and the second phase-change material layer; and forming a top electrode above the second phase-change material layer.
[0010] Another embodiment includes providing a high voltage pulse to a dielectric layer to form an internal electrode, wherein the dielectric layer includes a dielectric constant greater than or equal to 5.0. One embodiment includes resetting the structure to an amorphous stage by applying a current to the internal electrode. One embodiment includes reading a memory state of the structure by applying a voltage between the bottom electrode and the top electrode. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] The following detailed description, which is given by way of example and is not intended to limit the invention thereto, will be best understood in conjunction with the accompanying drawings, in which:
[0012] Figure 1 illustrates a cross-sectional view of a semiconductor structure at an intermediate manufacturing stage according to an exemplary embodiment;
[0013] Figure 2 A cross-sectional view of a semiconductor structure according to an exemplary embodiment is shown, which illustrates depositing a first external electrode and forming a first phase change material layer;
[0014] Figure 3 A cross-sectional view of a semiconductor structure showing patterning of internal electrodes according to an exemplary embodiment is shown;
[0015] Figure 4 shows a cross-sectional view of a semiconductor structure according to an exemplary embodiment, showing forming a second phase change material layer and forming a second external electrode;
[0016] Figure 5 A cross-sectional view of a semiconductor structure is shown showing selective removal of portions of the semiconductor structure according to an exemplary embodiment; and
[0017] Figure 6 A cross-sectional view of a semiconductor structure showing deposited dielectric and top contact is shown according to an exemplary embodiment;
[0018] Figure 7 According to an exemplary embodiment, Figure 6 A cross-sectional view of a semiconductor structure of FIG. 1 and showing a symmetrical amorphous configuration;
[0019] Figure 8 illustrates a cross-sectional view of a second semiconductor structure at an intermediate manufacturing stage according to an exemplary embodiment;
[0020] Fig. 9 shows a cross-sectional view of a second semiconductor structure according to an exemplary embodiment, showing forming a liner, forming a second phase change material layer, and forming a second external electrode;
[0021] Fig.10 illustrates a cross-sectional view of a second semiconductor structure showing selective removal of portions of the semiconductor structure according to an exemplary embodiment; and
[0022] Fig.11 illustrates a cross-sectional view of a second semiconductor structure showing deposited dielectric and top contact according to an exemplary embodiment;
[0023] Fig.12 According to an exemplary embodiment, Fig.11a cross-sectional view of a second semiconductor structure of FIG. 1 and illustrating a symmetrical amorphous configuration;
[0024] Fig.13 shows a cross-sectional view of a third semiconductor structure according to an embodiment;
[0025] Fig.14 shows a cross-sectional view of a fourth semiconductor structure according to an embodiment;
[0026] Fig.15 shows a cross-sectional view of a fifth semiconductor structure according to an embodiment;
[0027] Fig.16 shows a cross-sectional view of a sixth semiconductor structure according to an embodiment; and
[0028] Fig.17 A cross-sectional view of a seventh semiconductor structure in accordance with an embodiment is shown.
[0029] The drawings are not necessarily to scale. The drawings are merely schematic representations and are not intended to depict specific parameters of the invention. The drawings are intended to depict only typical embodiments of the invention. In the drawings, the same reference numerals represent the same elements. DETAILED DESCRIPTION
[0030] Detailed embodiments of the claimed structures and methods are disclosed herein; however, it is understood that the disclosed embodiments are merely illustrative of the claimed structures and methods that may be implemented in various forms. However, the present invention may be implemented in many different forms and should not be construed as limited to the exemplary embodiments set forth herein. Rather, these exemplary embodiments are provided to make this disclosure thorough and complete and to fully convey the scope of the invention to those skilled in the art. In the description, details of well-known features and techniques may be omitted to avoid unnecessarily obscuring the presented embodiments.
[0031] For purposes of the following description, the terms "upper", "lower", "right", "left", "vertical", "horizontal", "top", "bottom" and their derivatives shall refer to the disclosed structures and methods as oriented in the accompanying drawings. The terms "overlying", "on top", "on top of", "over", or "on top of" indicate that a first element, e.g., a first structure, is present on a second element, e.g., a second structure, wherein an intermediate element, e.g., an interface structure, may be present between the first element and the second element. The term "direct contact" means that a first element, e.g., a first structure, and a second element, e.g., a second structure, are connected without any intermediate conductive, insulating, or semiconducting layer at the interface of the two elements.
[0032] In order not to obscure the presentation of embodiments of the present invention, in the following detailed description, some processing steps or operations known in the art may be combined together for presentation and for illustration purposes, and may not be described in detail in some instances. In other instances, some processing steps or operations known in the art may not be described at all. It should be understood that the following description is more focused on the distinguishing features or elements of various embodiments of the present invention.
[0033] Embodiments of the present invention relate generally to phase change memory cells and, more particularly, to phase change memory cells having dual active volumes.
[0034] As described above, a typical configuration of a phase change memory cell may include a phase change material arranged between and coupled to at least two electrodes. The bottom contact and the top contact may each be connected to one of the two electrodes. The phase change material may be used as a phase change memory to store data by controlling the resistance state of the phase change material. The low resistance state causes the phase change material to be fully crystallized. The high resistance state has an amorphized phase change material. The phase change material may be amorphized by providing energy to the phase change material, such as electrical energy, thermal energy, any other suitable form of energy that can achieve the desired phase transformation, or a combination thereof. For example, a current pulse may be applied to either of the two electrodes from a top or bottom contact, which may be referred to as a heater electrode. For more than two memory states, for example for analog computing, the amount of amorphous volume may be controlled for a continuous region of programmable resistance states.
[0035] When the phase change material has an energy supply to change to an amorphized state, the portion of the phase change material that becomes amorphized typically becomes amorphized starting from where the current pulse is applied and spreads out in a "mushroom shape". This results in a semicircular or mushroom-shaped portion of the amorphized phase change material and the remainder of the crystalline phase change material. The memory cell may be referred to as a mushroom-shaped cell. The mushroom-shaped cell exhibits read bias polarity asymmetry. Measuring the resistance of the mushroom-shaped cell varies depending on the polarity of the applied read voltage, resulting in different values. The polarity dependence of the mushroom-shaped cell limits the speed, power efficiency, and accuracy of neuromorphic computing using phase change memory cells. Neuromorphic computing or neuromorphic engineering is used for artificial intelligence.
[0036] Additionally, the bottom electrode or heater of the phase change material needs to be made as small as possible with good reproducibility to allow high current flux and minimize the total programming current required to reset the phase change material to the high resistance amorphized state.
[0037] A physically symmetric mushroom-shaped cell device is proposed to address these issues. The physically symmetric mushroom-shaped cell device has little to no polarity dependence due to its symmetrical amorphous configuration, reduced programming current due to improved thermal confinement from the phase change material above and below the heater electrode, and lower power consumption during analog calculations due to higher SET / RESET resistances of the structure changing to and from the amorphous and crystalline states. The SET and RESET resistances can be up to twice that of a single active area device. These resistances can be tuned by modifying the thickness of the phase change material layer.
[0038] In the present invention, a first phase change material layer can be formed, a dielectric layer having an internal electrode can be formed, and a second phase change material layer can be formed. The internal electrode and the additional layer of the second phase change material layer provide a physically symmetrical mushroom-shaped cell device having a reduced programming current and lower power consumption during analog computing due to improved thermal confinement of the phase change material above and below the internal electrode. The internal electrode can be referred to as a heater electrode. The physically symmetrical mushroom-shaped cell device will allow a bidirectional read operation so that individual cells can be read in either direction, thereby saving time and power to read the device.
[0039] In an embodiment, a first liner is formed between the first phase change material layer and the dielectric layer and the internal electrode layer, and a second liner is formed between the dielectric layer and the internal electrode layer and the second phase change material layer.
[0040] In one embodiment, a filament layer may be formed between the first phase change material layer and the second phase change material layer. A portion of the filament layer may be destroyed to form a contact similar to an internal electrode between the first phase change material layer and the second phase change material layer.
[0041] In one embodiment, a first liner is formed between the first phase change material layer and the filament layer, and a second liner is formed between the filament layer and the second phase change material layer.
[0042] In one embodiment, a first pad is formed between the first phase-change material layer and the first external electrode, and a second pad is formed between the second external electrode and the second phase-change material layer.
[0043] The liner may include one or more layers and may include a thermal barrier layer, an adhesion layer, and a raised liner to reduce programming current and drift.
[0044] The internal electrodes and filament layers can each be considered as atomically thin heaters that help reduce the programming current of a single cell. The integration of the internal electrodes or filament layers helps provide symmetrical reading of a single cell that is independent of the read polarity. In artificial intelligence applications, the resistance of the device corresponds to a weight that can be positive or negative. The positive component of the weight on the device can be labeled G+, and the negative component of the weight on the device can be labeled G-. If there is no asymmetry in the devices, both devices can be read simultaneously by applying a positive voltage to one device, a negative voltage to the other, and allowing the currents to cancel. This can increase the speed and energy efficiency of the architecture.
[0045] The internal electrode and filament layer can provide simpler integration, which avoids unusual heater masks by using filaments instead of patterned heaters. When the heater vias are typically patterned in the dielectric, there is some gouging in the underlying material. In such a structure, this can damage the bottom PCM layer. If, instead of patterning the heater, the dielectric is subjected to a large electric field, this can cause dielectric breakdown and form a conductive filament through the dielectric. This effectively creates a very narrow heater without the need to explicitly pattern the vias.
[0046] When forming these layers, the internal electrodes and filament layers each provide self-alignment features, making it easy to perform these manufacturing steps.
[0047] The following is referenced Figure 1-17 The accompanying drawings in detail describe a method of forming a phase change memory cell having dual active volumes according to illustrative embodiments.
[0048] Reference now Figure 1 , a semiconductor structure (hereinafter "structure") 100 is shown at an intermediate step of fabrication according to an embodiment. The structure 100 may include a stack of layers formed on top of a substrate 102 and subsequently patterned into individual units. The structure 100 includes, for example, a substrate 102, a dielectric layer 104, and a bottom contact 106.
[0049] The substrate 102 may be a silicon substrate on which connections and structures such as transistors and isolation are built. The substrate 102 may be, for example, a bulk substrate, which may be made of any of several known semiconductor materials, such as silicon, germanium, silicon-germanium alloys, and compound (e.g., III-V and II-VI) semiconductor materials. Non-limiting examples of compound semiconductor materials include gallium arsenide, indium arsenide, and indium phosphide, or indium gallium arsenide. Typically, the substrate 102 may be about, but not limited to, several hundred microns thick.
[0050] A dielectric layer 104 may be deposited across the top of structure 100 in an overlying layer using any known deposition technique (e.g., chemical vapor deposition, atomic layer deposition, physical layer deposition, or some combination thereof). Dielectric layer 104 may include materials such as oxides, nitrides, or some combination thereof. In one embodiment, dielectric layer 104 may include an oxide, such as silicon oxide. In an alternative embodiment, dielectric layer 104 may include a nitride, such as silicon nitride. Chemical mechanical planarization techniques may optionally be used to polish dielectric layer 104 and provide a substantially smooth and uniform surface in preparation for subsequent processing techniques.
[0051] The conductive material layer of the bottom contact 106 is deposited in a trench (not shown) formed in the dielectric layer 104. The bottom contact 106 can be formed of a conductive material layer (e.g., copper, tungsten, cobalt, or aluminum). The conductive material layer can be deposited using typical deposition techniques, such as atomic layer deposition, molecular layer deposition, and chemical vapor deposition. In one embodiment, the bottom contact 106 can have a thickness ranging from about 10 nm to about 100 nm, although thicknesses less than 10 nm and greater than 100 nm are also acceptable. Chemical mechanical polishing (CMP) techniques can be used to remove excess material and polish the upper surface of the structure 100 to provide a uniform, level surface.
[0052] Reference now Figure 2 , showing a structure 100 according to an embodiment. A first external electrode 110 and a first phase change material layer 112 may be formed.
[0053] The conductive material layer of the first external electrode 110 may be blanket deposited on the structure 100, on the bottom contact 106, and on the dielectric layer 104. The first external electrode 110 may be formed as described for the bottom contact 106. The first external electrode 110 may alternatively be deposited in a trench on the structure 100.
[0054] The first phase change material layer 112 may be deposited uniformly on the structure 100 and directly on the top surface of the conductive material layer of the first external electrode 110. The first phase change material layer 112 may be deposited on the first external electrode 110 using conventional deposition processes (e.g., electroplating, electroless plating, chemical vapor deposition, physical vapor deposition, or a combination of these methods). According to an embodiment of the present invention, the first phase change material layer 112 may be formed of a mixture of gallium (Ga) and antimony (Sb) with at least one of tellurium (Te), silicon (Si), germanium (Ge), arsenic (As), selenium (Se), indium (In), tin (Sn), bismuth (Bi), silver (Ag), gold (Au), and antimony (Sb). It should be understood that the foregoing list is merely illustrative, and therefore, other elements may also be used to form the first phase change material layer 112 while maintaining the spirit of the inventive principles disclosed herein. In one embodiment, the first phase change material layer 112 may be made of a chalcogenide alloy such as germanium-antimony-tellurium (GST). According to another embodiment, the first phase change material layer 112 may also be made of a transition metal oxide having multiple resistance states. For example, the first phase change material layer 112 may be made of at least one material selected from the group consisting of NiO, TiO2, HfO, Nb2O5, ZnO, WO3, and CoO or GST (Ge2Sb2Te5) or PCMO (PrxCa1-xMnO3). In another embodiment, the first phase change material layer 112 may be a compound including one or more elements selected from the group consisting of sulfur (S), selenium (Se), tellurium (Te), arsenic (As), antimony (Sb), germanium (Ge), tin (Sn), indium (In) and silver (Ag). In one embodiment, the first phase change material layer 112 may have a thickness in the range of about 10nm to about 100nm, but a thickness less than 10nm and greater than 100nm is also acceptable.
[0055] Chemical mechanical polishing (CMP) techniques may be used to remove excess material and polish the upper surface of structure 100 to provide a uniform, level surface.
[0056] Reference now Figure 3 , showing a structure 100 according to an embodiment. A dielectric layer 120 and an internal electrode 122 may be formed.
[0057] The dielectric layer 120 may be formed on the first phase change material layer 112 and formed as described for the dielectric layer 104. An opening (not shown) may be formed in the dielectric layer 120 to expose a portion of the upper surface of the first phase change material layer 112. The opening may be formed by methods known in the art. An internal electrode 122 may be formed in the opening (not shown). The internal electrode 122 may be formed as described for the first external electrode 110. The internal electrode 122 may be referred to as a heater element.
[0058] Chemical mechanical polishing (CMP) techniques may be used to remove excess material and polish the upper surface of structure 100 to provide a uniform level surface for internal electrodes 122 and dielectric layer 120 .
[0059] Reference now Figure 4 , showing a structure 100 according to an embodiment. A second phase change material layer 130 and a second external electrode 110 may be formed.
[0060] The second phase change material layer 130 may be formed on the internal electrode 122 and the dielectric layer 120 as described for the first phase change material layer 112. The second external electrode 132 may be formed on the second phase change material layer 130 and formed as described for the first external electrode 110.
[0061] Chemical mechanical polishing (CMP) techniques may be used to remove excess material and polish the upper surface of the structure 100 to provide a uniform level surface of the second external electrode 132 .
[0062] Reference now Figure 5 , shows a structure 100 according to an embodiment. The structure 100 may be patterned as a single unit.
[0063] After forming or depositing the above-mentioned layers and materials, they are patterned into a single unit, as depicted. Patterning techniques known in the art can be used to form a single unit. More specifically, anisotropic etching techniques (e.g., reactive ion etching) can be used to selectively remove the second external electrode 132, the second phase-change material layer 130, the dielectric layer 120, the first phase-change material layer 112, and the first external electrode 110. The unit may include a vertically aligned portion of the second external electrode 132, the second phase-change material layer 130, the dielectric layer 120, the first phase-change material layer 112, and the first external electrode 110. Preferably, as a result of patterning the above-mentioned layers, the upper surface of the dielectric layer 104 is exposed. Typically, the footprint of each unit will mimic an existing phase-change memory column unit and is similarly limited based on the function of the phase-change memory column unit. For example, a typical phase-change memory column unit may have a lateral width or diameter ranging from about 10nm to about 200nm.
[0064] The width or diameter Wa of the inner electrode 122 is substantially smaller than the width or diameter Wb of the first and second outer electrodes 110, 132. In one embodiment, Wa is 5 times smaller than Wb. In one embodiment, Wa may be between 5 and 50 times smaller than Wb. In one embodiment, Wa is smaller than Wb of each of the first and second outer electrodes 110, 132. In one embodiment, the first and second outer electrodes 110, 132 may each have a smaller width or diameter than the other.
[0065] Reference now Figure 6 and 7 , shows a structure 100 according to one embodiment. A dielectric layer 140 and a top contact 142 may be formed.
[0066] The dielectric layer 140 may be formed as described for the dielectric layer 104. A second opening (not shown) may be formed in the dielectric layer 140, exposing a portion of the upper surface of the second external electrode 132. The second opening may be formed by methods known in the art. A top contact 142 may be formed in the second opening (not shown). The top contact 142 may be formed as described for the bottom contact 106.
[0067] Chemical mechanical polishing (CMP) techniques may be used to remove excess material and polish the upper surface of structure 100 to provide a uniform level surface for dielectric layer 140 and top contact 142 .
[0068] like Figure 7 As shown in FIG. 1 , a portion of each of the first phase change material layer 112 and the second phase change material layer 130 is shown as a dashed line. The dashed line portion represents a mushroom-shaped portion that may first be amorphized when current may be applied to the internal electrode 122 (which may be referred to as a heater electrode).
[0069] A conventional phase change memory cell may include a bottom contact 106, a first external electrode 110 (which may be referred to as a bottom electrode), a first phase change material layer 112, a top electrode directly above the phase change material layer 112, and a top contact on the top electrode. In the present invention, an internal electrode 122 and a second phase change material layer 130 are added between the first phase change material layer 112 and the first external electrode 110 (which may be referred to as a top electrode).
[0070] The internal electrode 122 and the additional layer of second phase change material layer 130 provide a physically symmetrical mushroom shaped cell device with reduced programming current due to improved thermal confinement from the phase change material above and below the heater electrode and lower power consumption during analog computations.
[0071] Although only a single cell is shown, it should be noted that structure 100 typically includes an array of thousands of cells, all formed according to the methods disclosed herein.
[0072] Reference now Figures 8 to 12 , an alternative embodiment is shown.
[0073] Reference now Figure 8, a semiconductor structure (hereinafter "structure") 200 is shown at an intermediate manufacturing step according to an embodiment. The structure 200 may include a stack of layers formed on top of a substrate 202 and then patterned into a single unit. The structure 200 includes, for example, a dielectric layer 204, a bottom contact 206, a first external electrode 210, a first phase change material layer 212, a first liner 218, a dielectric layer 220, and an internal electrode 222.
[0074] Similar named portions are formed as described above, including substrate 202, dielectric layer 204, bottom contact 206, first external electrode 210 and first phase change material layer 212, dielectric layer 220, and internal electrode 222.
[0075] The first liner 218 may be deposited on top of the first phase change material layer 212. The first liner 218 may include any suitable barrier material known in the art, such as titanium nitride (TiN), tantalum nitride (TaN), cobalt, ruthenium, carbon (C), amorphous carbon, titanium carbide (TiC), tantalum carbide (TaC), titanium aluminum nitride (TiAlN), tantalum aluminum nitride (TaAlN), titanium aluminum carbide (TiAlC), tantalum aluminum carbon (TaAlC), hafnium nitride (HfN) or tungsten nitride (WN), which may be alone or in combination with other suitable barrier materials. Since the etching for creating the opening for the internal electrode 222e may stop when it reaches the first liner 218 when patterning the via for the internal electrode 222e, the first liner 218 may also be referred to as an etch stop. Therefore, even if the first liner 218 has an electrical purpose for conductivity, it may facilitate processing by acting as an etch stop.
[0076] The first liner 218 may include one or more layers and may include a thermal barrier layer, an adhesion layer, and a raised liner to reduce programming current and drift.
[0077] Dielectric layer 220 may be formed on first liner 218 and formed as described for dielectric layer 104. Internal electrode 222 may be formed in a third opening (not shown) in dielectric layer 220 and formed as described for internal electrode 122. Chemical mechanical polishing (CMP) techniques may be used to remove excess material and polish the upper surface of structure 200 to provide a uniform, level surface.
[0078] Reference now Fig. 9 , showing a structure 200 according to an embodiment. A second liner 224, a second phase change material layer 230, and a second external electrode 210 may be formed.
[0079] The second liner 224 may be formed on the dielectric layer 220 and the internal electrode 222. The second liner 224 may be formed as described for the first liner 218. The second external electrode 210 may be formed on the second liner 224 as described for the first external electrode 110.
[0080] According to the present embodiment, the first liner 218 serves as a barrier to physically separate the first phase change material layer 212 from subsequent layers formed thereon. The second liner 224 serves as a barrier to physically separate the second phase change material layer 230 from the dielectric layer 220 and the internal electrode 222. In an embodiment, the first liner 218 and the second liner 224 may each have a thickness ranging from about 1 nm to about 30 nm, although thicknesses less than 1 nm and greater than 30 nm may be acceptable.
[0081] Reference now Fig.10 , shows a structure 200 according to one embodiment. The structure 200 may be patterned as a single unit.
[0082] After forming or depositing the above-mentioned layers and materials, they are patterned into a single unit, as depicted. Patterning techniques known in the art can be used to form a single unit. More specifically, anisotropic etching techniques (e.g., reactive ion etching) can be used to selectively remove the second external electrode 232, the second phase-change material layer 230, the second liner 224, the dielectric layer 220, the first liner 218, the first phase-change material layer 212, and the first external electrode 210. The unit may include a second external electrode 232, a second phase-change material layer 230, a second liner 224, a dielectric layer 220, a first liner 218, a first phase-change material layer 212, and a vertically aligned portion of the first external electrode 210. Preferably, as a result of patterning the above-mentioned layers, the upper surface of the dielectric layer 204 is exposed. Typically, the footprint of each unit will mimic an existing phase-change memory pillar unit and is similarly limited based on the function of the phase-change memory pillar unit. For example, a typical phase change memory pillar cell may have a lateral width or diameter ranging from about 10 nm to about 200 nm.
[0083] Reference now Fig.11 and 12 , shows a structure 200 according to one embodiment. A dielectric layer 240 and a top contact 242 may be formed.
[0084] The dielectric layer 240 may be formed as described for the dielectric layer 104. A fourth opening (not shown) may be formed in the dielectric layer 240, exposing a portion of the upper surface of the second external electrode 232. The fourth opening may be formed by methods known in the art. A top contact 242 may be formed in the fourth opening (not shown). The top contact 242 may be formed as described for the bottom contact 106.
[0085] Chemical mechanical polishing (CMP) techniques may be used to remove excess material and polish the upper surface of structure 200 , providing a uniform level surface for dielectric layer 240 and top contact 242 .
[0086] like Fig.12 As shown in FIG. 1 , a portion of each of the first phase change material layer 212 and the second phase change material layer 230 is shown as a dashed line. The dashed line portion indicates a mushroom-shaped portion that may first be amorphized when current may be applied to the inner electrode 222 (which may be referred to as a heater electrode).
[0087] The additional layer of internal electrode 222 and second phase change material layer 230 provides a physically symmetrical mushroom shaped cell device with reduced programming current due to improved thermal confinement from the phase change material above and below the heater electrode and lower power consumption during analog computations.
[0088] Compare Figure 7 and 8 The structure of 100 Fig.11 and 12 In the structure 200, the second liner 224 and the first liner 218 are additional layers of the structure 200. The first liner 218 and the second liner 224 each serve as a barrier to physically separate the first and second phase change material layers 212 and 230 from the dielectric layer 220 and the internal electrode 222.
[0089] Although only a single cell is shown, it should be noted that structure 200 typically includes an array of thousands of cells, all formed according to the methods disclosed herein.
[0090] Reference now Fig.13 , an alternative embodiment is shown.
[0091] Reference now Fig.13 , a semiconductor structure (hereinafter “structure”) 300 is shown at an intermediate manufacturing step according to one embodiment. The structure 300 may include a stack of layers formed on top of a substrate 302 and then patterned into a single unit. The structure 300 includes, for example, a dielectric layer 304, a first external electrode 310, a first phase change material layer 312, a dielectric layer 340, a second phase change material layer 330, a second external electrode 342, and an internal electrode 322.
[0092] Similar named portions are formed as described above, including substrate 302 , dielectric layer 304 , first external electrode 310 , first phase change material layer 312 , dielectric layer 340 , second phase change material layer 330 , second external electrode 342 , and internal electrode 322 .
[0093] The internal electrode 322 may be formed in the dielectric layer 304, wherein a portion of the internal electrode 322 is buried in the dielectric layer 304 and two separate portions extend to an upper surface coplanar with an upper surface of the dielectric layer 304. A phase-change material layer (not shown) may be formed on the dielectric layer 304 and the internal electrode 322. An electrode layer (not shown) may be formed on the phase-change material layer (not shown). The phase-change material layer (not shown) and the electrode layer (not shown) may be patterned into a vertically aligned first external electrode 310 and a first phase-change material layer 312 and a separate vertically aligned second external electrode 332 and a second phase-change material layer 330. A dielectric layer 340 may be formed around the vertically aligned first external electrode 310 and the first phase-change material layer 312 and the separate vertically aligned second external electrode 332 and the second phase-change material layer 330. A contact (not shown) may be formed to each of the first external electrode 310 and the second external electrode 342. The vertically aligned first external electrode 310 and the first phase change material layer 312 may be aligned over a first portion of the inner electrode coplanar with the upper surface of the dielectric layer 304. The vertically aligned second external electrode 332 and the second phase change material layer 330 may be aligned over a second portion of the inner electrode coplanar with the upper surface of the dielectric layer 304.
[0094] Structure 300 may be a single unit cell. Although only one single unit cell is shown, it should be noted that structure 300 typically includes an array of thousands of units, all formed according to the methods disclosed herein.
[0095] Structure 300 provides a physically symmetrical mushroom-shaped cell device with reduced programming current due to improved thermal confinement from the phase change material above and below the heater electrode, and lower power consumption during analog computations.
[0096] Compare Figure 7 and 8 The structure of 100 and Fig.13 The structure 300 may be easier to manufacture, however, the structure 300 may consume more surface area for wiring.
[0097] Reference now Fig.14, according to one embodiment, a semiconductor structure (hereinafter "structure") 400 is shown at an intermediate manufacturing step. The structure 400 may include a layer stack formed on top of a substrate 402 and then patterned into a single unit. The structure 400 includes, for example, a dielectric layer 404, a first external electrode 410, a dielectric layer 420, a first phase change material layer 412, a second phase change material layer 430, a dielectric layer 440, a second external electrode 432, and an internal electrode 422.
[0098] Similar named portions are formed as described above, including substrate 402 , dielectric layer 404 , first external electrode 410 , dielectric layer 420 , first phase change material layer 412 , dielectric layer 440 , second phase change material layer 430 , second external electrode 432 , and internal electrode 422 .
[0099] The first external electrode 410 may be formed in the dielectric layer 404. A phase-change material layer (not shown) may be formed on the dielectric layer 404 and the internal electrode 422. The phase-change material layer (not shown) may be patterned into a first phase-change material layer 412 and a second phase-change material layer 430, wherein the first phase-change material layer 412 is aligned above and connected to the first external electrode 410. An internal spacer 442 connecting the first phase-change material layer 412 and the second phase-change material layer 430 may be formed on the dielectric layer 404. The dielectric layer 420 may be formed around the first phase-change material layer 412, the internal electrode 422, and the second phase-change material layer 430. A dielectric layer 440 may be formed. A fifth opening (not shown) may be formed in the dielectric layer 440 to expose a portion of the upper surface of the second phase-change material layer 430. The second external electrode 432 may be formed in the fifth opening (not shown) to align with and physically connect to the second phase-change material layer 430. A contact (not shown) may be formed to each of the first external electrode 410 and the second external electrode 432 .
[0100] Structure 400 may be a single unit cell. Although only one single unit cell is shown, it should be noted that structure 400 typically includes an array of thousands of units, all formed according to the methods disclosed herein.
[0101] Structure 400 provides a physically symmetrical mushroom-shaped cell device with reduced programming current due to improved thermal confinement from the phase change material above and below the heater electrode, and lower power consumption during analog computations.
[0102] Compare Figure 7 and 8 Structure 100, Fig.13 The structure of 300 and Fig.14 The structure 400 is easier to manufacture, while the structure 300 consumes more surface area for wiring.
[0103] Reference now Figure 15-17 , an alternative embodiment using a conductive filament instead of an internal electrode between two phase change material layers is shown and described. There are two embodiments to form the conductive filament. The conductive filament can be formed by using a high-k dielectric layer that breaks down to form the conductive filament. Alternatively, a hybrid ionic electronic conductive filament device can be used.
[0104] Reference now Fig.15 , a semiconductor structure (hereinafter “structure”) 500 is shown at an intermediate manufacturing step according to one embodiment. The structure 500 may include a stack of layers formed on top of a substrate 502 and then patterned into a single unit. The structure 500 includes, for example, a dielectric layer 504, a bottom contact 506, a first external electrode 510, a first phase change material layer 512, a second phase change material layer 530, a dielectric layer 540, a second external electrode 532, and a top contact 542.
[0105] The structure 500 also includes, for example, a filament layer 550 and a filament layer break 552. The filament layer 550 and the filament layer break 552 were not present in the previous embodiment.
[0106] Similar named portions are formed as described above, including substrate 502, dielectric layer 504, bottom contact 506, first external electrode 510, first phase change material layer 512, second phase change material layer 530, dielectric layer 540, second external electrode 532, and top contact 542.
[0107] The filament layer 550 may be conformally formed on the first phase change material layer 512. The filament layer 550 may include a high-k dielectric layer, for example, a MOX (metal oxide semiconductor), such as tantalum oxide (Ta2O5) and hafnium oxide (HfO2). The filament layer 550 may include one or more layers consisting of one or more materials. The filament layer 550 may be formed by PVD (physical vapor deposition). The thickness of the filament layer 550 may be between 1 nm and 50 nm, although the thickness may be less than 1 nm or greater than 50 nm. The filament layer 550 may include one or more layers consisting of one or more materials. In one embodiment, the filament layer 550 includes a material having a dielectric constant equal to or greater than 3.9.
[0108] In one embodiment, dielectric layer 504 and dielectric layer 540 may include a material having a dielectric constant less than or equal to 3.9. In one embodiment, dielectric layer 504 and dielectric layer 540 may each have a dielectric constant less than that of filament layer 550 .
[0109] In one embodiment, the filament layer 550 may include mixed ion conductive (MIEC) filaments, such as silicon (Si) or silver (Ag) with an ion barrier. An ion barrier is an energy barrier for ions to move in physical space. The ions stay in place until sufficient energy (e.g., an electric field) overcomes the barrier.
[0110] The second phase change material layer 530 may be conformally formed on the filament layer 550. The structure 500 may be patterned into a single unit as described above.
[0111] A portion of the filament layer 550 may be transformed into a filament layer break 552 by a high voltage pulse or by applying a sufficiently large electric field to induce dielectric breakdown in the filament layer 550, thereby forming a conductive bridge.
[0112] The filament layer break 552 is a conductive path between the first phase change material layer 512 and the second phase change material layer 530 .
[0113] Structure 500 may be a single unit cell. Although only a single unit cell is shown, it should be noted that structure 500 typically includes an array of thousands of units, all formed according to the methods disclosed herein.
[0114] Structure 500 provides a physically symmetrical mushroom-shaped cell device with reduced programming current due to improved thermal confinement from the phase change material above and below the filament layer break 552, and lower power consumption during analog computations.
[0115] like Fig.15 As shown in FIG. 5 , a portion of each of the first phase change material layer 512 and the second phase change material layer 530 is shown as a dotted line. The dotted line portion indicates a mushroom-shaped portion that will first be amorphized when current is applied to the filament layer break 552 (which may be referred to as a heater electrode).
[0116] Reference now Fig.16 , a semiconductor structure (hereinafter "structure") 600 is shown at an intermediate manufacturing step according to one embodiment. The structure 600 may include a stack of layers formed on top of a substrate 602 and subsequently patterned into a single unit. The structure 600 includes, for example, a dielectric layer 604, a bottom contact 606, a first external electrode 610, a first phase change material layer 612, a second phase change material layer 630, a dielectric layer 640, a second external electrode 632, and a top contact 642. The structure 600 also includes, for example, a filament layer 650, a filament layer break 652, a first pad 648, and a second pad 654.
[0117] Similar named portions are formed as described above, including substrate 602, dielectric layer 604, bottom contact 606, first external electrode 610. First phase change material layer 612, second phase change material layer 630, dielectric layer 640, second external electrode 632, top contact 642, filament layer 650, and filament layer break 652.
[0118] A first liner 648 may be formed on the first phase change material layer 612. The first liner 648 may be formed as described for the first liner 218. A filament layer 650 may be conformally formed on the first liner 648. A second liner 654 may be formed on the filament layer 650. The second liner 654 may be formed as described for the first liner 218. A second phase change material layer 630 may be conformally formed on the filament layer 650.
[0119] The structure 600 may be patterned into a single unit as described above. The dielectric layer 640 and the top contact 642 may be formed as described above.
[0120] A portion of the filament layer 650 may become a filament layer break 652 as described for the filament break 552. The filament layer break 652 is a conductive path between the first phase change material layer 612 and the second phase change material layer 630.
[0121] Structure 600 may be a single unit cell. Although only a single unit cell is shown, it should be noted that structure 600 typically includes an array of thousands of units, all formed according to the methods disclosed herein.
[0122] Structure 600 provides a physically symmetrical mushroom-shaped cell device with reduced programming current due to improved thermal confinement from the phase change material above and below the filament layer break 652, and lower power consumption during analog computations.
[0123] According to the present embodiment, the first liner 648 acts as a barrier to physically separate the first phase change material layer 612 from subsequent layers formed thereon. The second liner 654 acts as a barrier to physically separate the second phase change material layer 630 from the filament layer 650 and the filament layer break 652. In one embodiment, the first liner 648 and the second liner 654 may each have a thickness ranging from about 1 nm to about 30 nm, although thicknesses less than 1 nm and greater than 30 nm may be acceptable.
[0124] Structure 600 provides a physically symmetrical mushroom-shaped cell device with reduced programming current due to improved thermal confinement from the phase change material above and below the filament layer break 652, and lower power consumption during analog computations.
[0125] like Fig.16As shown in FIG. 6 , a portion of each of the first phase change material layer 612 and the second phase change material layer 630 is shown as a dotted line. The dotted line portion represents a mushroom-shaped portion that is first amorphized when current is applied to the filament layer break 652 (which may be referred to as a heater electrode).
[0126] Reference now Fig.17 , according to an embodiment, a semiconductor structure (hereinafter "structure") 700 is shown at an intermediate manufacturing step. The structure 700 may include a stack of layers formed on top of a substrate 702 and then patterned into a single unit. The structure 700 includes, for example, a dielectric layer 704, a bottom contact 706, a first external electrode 710, a first phase change material layer 712, a second phase change material layer 730, a dielectric layer 740, a second external electrode 732, and a top contact 742. The structure 700 also includes, for example, a filament layer 750, a filament layer break 752, a first pad 748, and a second pad 754.
[0127] Portions with similar naming are formed as described above, including a substrate 702, a dielectric layer 704, a bottom contact 706 and a first external electrode 710, a first phase change material layer 712, a second phase change material layer 730, a dielectric layer 740, a second external electrode 732, a top contact 742, a filament layer 750, a filament layer break 752, a first pad 748 and a second pad 754.
[0128] The first pad 748 may be formed on the first external electrode 710. The first phase-change material layer 712 may be formed on the first pad 748. The filament layer 750 may be conformally formed on the first phase-change material layer 712. The second pad 754 may be on the filament layer 750.
[0129] The structure 700 may be patterned into a single unit as described above. A dielectric layer 740 and a top contact 742 may be formed.
[0130] A portion of the filament layer 750 may become a filament layer break 752. The filament layer break 752 is a conductive path between the first phase change material layer 712 and the second phase change material layer 730.
[0131] Structure 700 may be a single unit cell. Although only a single unit cell is shown, it should be noted that structure 700 typically includes an array of thousands of units, all formed according to the methods disclosed herein.
[0132] Structure 700 provides a physically symmetrical mushroom-shaped cell device with reduced programming current due to improved thermal confinement from the phase change material above and below the filament layer break 752, and lower power consumption during analog computations.
[0133] According to the present embodiment, the first liner 748 serves as a barrier to physically separate the first phase-change material layer 712 from the first external electrode 710. The second liner 754 serves as a barrier to physically separate the second phase-change material layer 730 from the second external electrode 732.
[0134] Structure 7600 provides a physically symmetrical mushroom-shaped cell device with reduced programming current due to improved thermal confinement from the phase change material above and below the filament layer break 752, and lower power consumption during analog computations.
[0135] like Fig.17 As shown in FIG. 1 , a portion of each of the first phase change material layer 712 and the second phase change material layer 730 is shown as a dotted line. The dotted line portion indicates a mushroom-shaped portion that may be first amorphized when current is applied to the filament layer break 752 (which may be referred to as a heater electrode).
[0136] The description of various embodiments of the present invention has been given for the purpose of illustration, but it is not intended to be exhaustive or limited to the disclosed embodiments. Many modifications and variations will be apparent to those of ordinary skill in the art without departing from the scope and spirit of the described embodiments. The terms used herein are selected to best explain the principles of the embodiments, practical applications, or technical improvements existing in the market, or to enable other persons of ordinary skill in the art to understand the embodiments disclosed herein.
Claims
1. A structure, include: a first phase change material layer vertically aligned over the bottom electrode; a dielectric layer vertically aligned over the first phase change material layer; a second phase change material layer vertically aligned over the dielectric layer; an internal electrode physically and electrically connected to the first phase change material layer and the second phase change material layer, the internal electrode being surrounded by the dielectric layer; as well as A top electrode is vertically aligned over the second phase change material layer.
2. The structure of claim 1, wherein a lateral diameter of the inner electrode is smaller than a lateral diameter of the bottom electrode.
3. The structure according to claim 1, further comprising: include: a first raised pad vertically aligned between the first phase change material layer and the dielectric layer; as well as A second raised pad is vertically aligned between the second phase change material layer and the dielectric layer.
4. The structure according to claim 1, further comprising: include: a first thermal barrier layer vertically aligned between the first phase change material layer and the dielectric layer; as well as A first thermal barrier layer is vertically aligned between the second phase change material layer and the dielectric layer.
5. The structure according to claim 1, further comprising: include: a first adhesion layer vertically aligned between the first phase change material layer and the dielectric layer; as well as A first adhesion layer is vertically aligned between the second phase change material layer and the dielectric layer.
6. A structure, include: a first phase change material layer aligned over a first portion of an internal electrode; a first external electrode vertically aligned over the first phase change material layer; a second phase change material layer aligned over a second portion of the internal electrode; a second external electrode vertically aligned over the second phase change material layer; as well as A dielectric layer vertically physically and electrically separates the first phase-change material layer and the first external electrode from the second phase-change material layer and the second external electrode.
7. A structure, include: a first phase change material layer aligned over the first external electrode; an internal electrode physically and electrically connected between the first phase change material layer and the second phase change material layer; a second external electrode vertically aligned over the second phase change material layer; as well as A dielectric layer vertically physically and electrically separates the first phase-change material layer and the first external electrode from the second phase-change material layer and the second external electrode.
8. A structure, include: a first phase change material layer vertically aligned over the bottom electrode; a layer of filaments vertically aligned above the first phase change material layer; a second phase change material layer vertically aligned above the filament layer; an internal fracture in the filament layer, the internal fracture connecting the first phase change material layer and the second phase change material layer; as well as A top electrode is vertically aligned over the second phase change material layer.
9. The structure according to claim 8, wherein The filament layer includes a high-k dielectric.
10. The structure according to claim 8, wherein The filament layer includes mixed ionic and electronic conductive filaments.
11. The structure according to claim 8, further comprising: include: a first liner vertically aligned between the first phase change material layer and the filament layer; as well as A second pad is vertically aligned between the second phase change material layer and the filament layer.
12. The structure according to claim 11, wherein The first liner and the second liner are each a raised layer.
13. The structure according to claim 11, wherein The first liner and the second liner are each a thermal barrier layer.
14. The structure according to claim 11, wherein The first liner and the second liner are each an adhesive layer.
15. The structure according to claim 9, further comprising: include: a first pad vertically aligned between the first phase change material layer and the bottom electrode; as well as A second pad is vertically aligned between the second phase change material layer and the top electrode.
16. The structure of claim 15, wherein The first liner and the second liner are each a raised layer.
17. The structure of claim 15, wherein The first liner and the second liner are each a thermal barrier layer.
18. The structure of claim 15, wherein The first liner and the second liner are each an adhesive layer.
19. A method of forming a structure, the method include: forming a first phase change material layer over the bottom electrode; forming a dielectric layer over the first phase change material layer; forming an internal electrode in the dielectric layer; forming a second phase change material layer over the dielectric layer, wherein the internal electrode is physically and electrically connected to both the first phase change material layer and the second phase change material layer; A top electrode is formed over the second phase change material layer.
20. The method according to claim 19, further comprising: include: A high voltage pulse is provided to the dielectric layer to form the inner electrode, wherein the dielectric layer includes a dielectric constant greater than or equal to 5.
0.
21. The method according to claim 19, further comprising: include: The structure is reset to the amorphous stage by applying a current to the inner electrodes.