Furyl polyamide and preparation method thereof

By designing furyl polyamide with a trans-arranged carbonyl structure, the problem of poor thermal stability of existing furyl polyamide is solved, high thermal performance and industrial application are achieved, and the biodegradability and environmental protection of the material are improved through green processes.

CN118745245AActive Publication Date: 2024-10-08NANJING TECH UNIV

Patent Information

Application Number
CN202410973130.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-19
Publication Date
2024-10-08
Estimated Expiration
2044-07-19

AI Technical Summary

Technical Problem

The thermal stability of existing furan-based polyamides is poor, which limits the application development of the materials.

Method used

By designing furyl polyamide containing a trans-arranged carbonyl structure and preparing it by the reaction of oxalic acid dibasic ester and aliphatic diamine, the intermolecular hydrogen bond density is increased and the material's low water absorption, high modulus and high melting point properties are improved. , and adopt green and non-toxic process methods.

Benefits of technology

The thermal stability of furan-based polyamide is significantly improved, providing excellent thermal performance and solvent resistance, while realizing the industrial application and biodegradability of the material, and the process is simple and environmentally friendly.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118745245A_ABST
    Figure CN118745245A_ABST
Patent Text Reader

Abstract

The invention belongs to the field of polymer synthetic chemistry, and discloses furyl polyamide and a preparation method thereof, and the furyl polyamide shown in a formula I is prepared by reacting an aliphatic diamine monomer containing an oxalic acid amide group shown in a formula II with a furandicarboxylic acid derivative monomer. The furyl polyamide molecular chain has a special trans-arrangement carbonyl structure, and the hydrogen bond density is greatly increased, so that the furyl polyamide is endowed with the characteristics of low water absorption, high modulus, high melting point and the like, the problem of poor thermal performance of furyl polyamide is solved, and a new thought is provided for industrial application of furyl polyamide. The method provided by the invention is green and non-toxic, is simple to operate, and can obtain furyl polyamide with high molecular weight.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of polymer synthesis chemistry, and in particular to a novel furan-based polyamide and a preparation method thereof. Background Art

[0002] This section merely provides background information related to the present disclosure and is not necessarily prior art.

[0003] Polyamide, commonly known as nylon, refers to the general term for polymers containing amide groups (-NHCO-) ​​in the macromolecular chain segments, which are mainly obtained by the self-polymerization of amino acid lactam or the condensation of dibasic acid and diamine. There are many varieties of polyamide. According to their composition structure, polyamide can be divided into aliphatic polyamide, aromatic polyamide and copolyamide. Due to the presence of amide groups in the nylon molecular chain, stable hydrogen bonds can be formed between the molecular chains, and nylon is easy to crystallize, thus giving it strong mechanical properties and good thermal properties. At the same time, nylon has a higher specific strength than metal, a low friction coefficient, excellent fatigue resistance, chemical resistance and self-lubrication, etc. It is a polymer material with excellent comprehensive properties. Since the development of PA6 by DuPont in the United States in the 1930s, nylon has developed rapidly as a general engineering plastic variety and has extended into a variety of products.

[0004] 2,5-Furandicarboxylic acid (FDCA) is a bio-based dibasic acid monomer obtained from sugar. It is a substitute for PTA and has good biodegradability. It has fewer carbon atoms than benzene rings and weaker aromaticity than benzene rings. Its thermodynamic and mechanical properties are even better than those of terephthalic acid polymers. The use of furan-based aliphatic polyamides to replace traditional aromatic polyamides as high-performance materials has attracted a lot of attention. This not only breaks the dependence of the traditional polyamide synthesis industry on petroleum resources, but also reduces the generation and emission of hazardous waste. However, the thermal stability of the furan-based polyamides reported so far is poor, and they are easily decomposed during high-temperature reactions, which limits the application and development of the material. Therefore, we need to enhance the thermal properties by modifying the structure of furan-based polyamides to provide performance guarantees for expanding the industrial application of polyamides. Summary of the invention

[0005] Purpose of the invention: The technical problem to be solved by the present invention is to provide a highly heat-resistant furan-based semi-aromatic polyamide and a preparation method thereof in view of the deficiencies in the prior art.

[0006] In order to solve the above technical problems, the present invention discloses the following technical solutions:

[0007] In a first aspect, the present invention provides an aliphatic diamine monomer having a designed structure as shown in Formula II;

[0008]

[0009] in,

[0010] R is selected from C 4 -C 12 Alkyl groups, including C 4 -C 12 The term "alkyl" refers to a straight-chain alkyl group and a branched-chain alkylene group.

[0011] In a second aspect, the present invention provides a method for preparing the aliphatic diamine monomer having a designed structure as shown in Formula II, comprising reacting oxalic acid dibasic ester with C 4 -C 12 Reaction of aliphatic diamines.

[0012] The dibasic oxalate includes dimethyl oxalate, diethyl oxalate, dibutyl oxalate, or any combination thereof, preferably diethyl oxalate.

[0013] The C4-C12 aliphatic diamine includes 1,4-butanediamine, 1,5-pentanediamine, 1,6-hexanediamine, 1,8-octanediamine, 1,10-decanediamine, 1,11-diaminoundecane, 1,12-diaminododecane or any combination thereof.

[0014] Wherein, the molar ratio of the oxalic acid dibasic ester to the C4-C12 aliphatic diamine is 0.1-0.3:1, such as 0.15:1, 0.2:1, 0.25:1.

[0015] Wherein, the solvent used in the method is methanol or ethanol, preferably ethanol; the volume ratio of the solvent to the C4-C12 aliphatic diamine is 1:0.8-1.2, preferably 1:1.

[0016] The specific process steps and conditions of the preparation method are as follows:

[0017] First, an excess of diamine is dissolved in a solvent, and then a dibasic oxalate solution is added dropwise under inert gas protection and stirring. Further, after the reaction is completed, suction filtration is performed, washing is performed with ethanol, and the solid is dried to obtain a white aliphatic diamine monomer crude product, which is then recrystallized with butyl acetate, insoluble solids are filtered out, the solution is allowed to stand at low temperature, the precipitated product is washed with ethanol, and the solid is dried to obtain a white aliphatic diamine-containing monomer.

[0018] Wherein, the stirring rotation speed is 50-500rpm, such as 350-500rpm.

[0019] Wherein, the dibasic oxalate solution is added dropwise at a flow rate of 200-400 uL / min.

[0020] After the addition is completed, stirring is continued for 1-3 hours to react. During the esterification, the excess diamine will block the oxalate to obtain the desired product.

[0021] In a third aspect, the present invention uses a designed aliphatic diamine and furan dicarboxylic acid as raw materials to design a furan-based polyamide having an alternating structure in a molecular structure as shown in Formula I;

[0022]

[0023] in,

[0024] R is selected from C 4 -C 12 Alkyl groups, including C 4 -C 12 Straight-chain alkyl and branched alkylene;

[0025] n is any integer selected from 10 to 500.

[0026] The furan-based polyamide of the present invention has a special trans-arranged carbonyl structure on the molecular chain, and the hydrogen bond density is greatly increased, thereby giving it the characteristics of low water absorption, high modulus and high melting point, solving the problem of poor thermal properties of furan-based polyamide, and providing a new idea for the industrial application of furan-based polyamide. The method of the present invention is green and non-toxic, simple to operate, and can obtain high molecular weight furan-based polyamide.

[0027] In a fourth aspect, the present invention discloses a method for preparing the furan-based polyamide as shown in Formula I according to the third aspect.

[0028] The method comprises the steps of reacting an aliphatic diamine monomer containing an oxalic acid amide group as shown in formula II with a furan dicarboxylic acid derivative monomer.

[0029] The furan dicarboxylic acid derivative monomer includes 2,5-furan dicarboxylic acid, 2,5-furan dicarboxylic acid dimethyl ester, 2,5-furan dicarboxylic acid diethyl ester, 2,5-furan dicarboxylic acid dibutyl ester, 2,5-furan dicarboxylic acid chloride, or any combination thereof.

[0030] Wherein, the molar ratio of the aliphatic diamine monomer containing oxalic acid amide group shown in Formula II to the furan dicarboxylic acid derivative monomer is 1-3:1, such as 1.1:1, 1.5:1, 2:1, etc.

[0031] Furthermore, the method comprises adding an aliphatic diamine monomer containing an oxalic acid amide group and a furan dicarboxylic acid derivative monomer shown in formula II into a reaction container under an inert atmosphere, heating the temperature to a first temperature, then gradually heating the temperature to a second temperature and maintaining it for 1-4 hours to carry out an ester exchange reaction, then heating the temperature to a third temperature and adjusting the pressure to a negative pressure and vacuuming for 1-9 hours to carry out a condensation reaction, and cooling the reaction in water after the reaction is completed to obtain the furan-based polyamide.

[0032] Wherein, the first temperature is selected from 110-170°C, preferably 120-160°C; the second temperature is selected from 170-230°C, preferably 180-220°C; the third temperature is selected from 190-260°C, preferably 200-250°C; at the same time, the first temperature < the second temperature < the third temperature; in some embodiments, the second temperature is 40-80°C higher than the first temperature, such as 50°C, 60°C, 70°C; in some embodiments, the third temperature is 20-50°C higher than the second temperature, such as 30°C, 40°C.

[0033] The gradient temperature increase is 3-6°C every ten minutes.

[0034] Among them, the pressure in the vacuum stage is 30-300Pa.

[0035] Wherein, stirring may be performed during the transesterification reaction stage and the polycondensation reaction stage, and the stirring rate is 50-500 rpm, such as 350-500 rpm.

[0036] In a fifth aspect, the present invention discloses the use of the furan-based polyamide represented by the above formula I in the preparation of chemically recyclable materials.

[0037] The novel furan-based polyamide prepared by the present invention is degraded to monomers under certain conditions, thereby realizing closed-loop chemical recycling of polyamide; the monomers include 2,5-furandicarboxylic acid and diamines, such as 1,5-pentanediamine.

[0038] The degradation conditions are as follows: 120-200° C., sodium hydroxide aqueous solution as solvent, and the furan-based polyamide is reacted under this condition for 5-12 hours.

[0039] Furthermore, after the reaction is completed, the degradation solution is adjusted to a pH of 2-3 with hydrochloric acid, during which furandicarboxylic acid is gradually precipitated, the precipitate is collected and washed with ethanol, and pure furandicarboxylic acid is obtained after drying, and the recovery rate of furandicarboxylic acid is 80%-85%. Therefore, the novel furan-based polyamide prepared by the present invention can be completely degraded to monomers without further purification, further expanding the application of bio-based raw material furandicarboxylic acid and opening up a new way for polyamide recovery research.

[0040] In the present invention, the inert gas includes helium, neon, argon, krypton, xenon, carbon dioxide or nitrogen, preferably argon.

[0041] The relative viscosity of the furan-based polyamide shown in formula I of the present invention is 1.3-1.65, such as 1.37-1.58; the glass transition temperature of the furan-based polyamide shown in formula I is 57-142°C, such as 69-130°C; the melting point Tm of the furan-based polyamide shown in formula I is 171-250°C, such as 180-241°C; the initial decomposition temperature Td5% of the furan-based polyamide shown in formula I is 338-412°C, such as 380-412°C; the maximum decomposition temperature Tmax of the furan-based polyamide shown in formula I is 446-486°C, such as 459-473°C; the tensile strength of the furan-based polyamide shown in formula I is 50-124MPa, such as 59-115MPa.

[0042] Beneficial effects:

[0043] (1) The furan-based polyamide provided by the present invention introduces more amide bonds into the repeating units, provides more intermolecular hydrogen bonds, and the internal network formed needs to be destroyed at a higher temperature. Compared with the reported furan-based semi-aromatic polyamide (initial decomposition temperature 367°C), the thermal stability is significantly improved. In addition, the furan-based polyamide provided by the present invention is crystallizable, has a melting point of 180-250°C, and is a semi-crystalline polymer, providing excellent thermal stability and excellent solvent resistance.

[0044] (2) The preparation method of furan-based polyamide provided by the present invention is bulk polymerization, which does not require solvents and catalysts, saves energy and reduces emissions, has a simple and green preparation process, and reduces environmental pollution.

[0045] (3) The furan-based polyamide provided by the present invention can recover the initial monomer from the degradation solution by a simple, efficient, and high-recovery acidification and post-filtration method, thereby realizing closed-loop chemical recovery of polyamide. This work will further expand the application of bio-based raw material furandicarboxylic acid and open up new avenues for polyamide recovery research. BRIEF DESCRIPTION OF THE DRAWINGS

[0046] The present invention will be further described in detail below in conjunction with the accompanying drawings and specific embodiments, and the above and / or other advantages of the present invention will become more clear.

[0047] Figure 1 Aliphatic diamine monomers of the designed structures of Examples 1-4 1 H NMR spectra.

[0048] Figure 2 The polyamide product of Examples 1-4 1 H NMR spectra.

[0049] Figure 3 The polyamide product of Example 4 13 C NMR spectrum.

[0050] Figure 4 This is the TGA diagram of the polyamide product of Example 4.

[0051] Figure 5 The DSC diagram of the polyamide product of Example 4 (at N 2 The second heating curve was scanned from 30°C to 300°C at a heating rate of 10°C / min under an atmosphere.

[0052] Figure 6 This is the X-ray diffraction pattern of the polyamide product of Example 4.

[0053] Figure 7 The polyamide depolymerization product 1,5-pentanediamine and furan dicarboxylic acid of Example 5 1 H NMR spectra. DETAILED DESCRIPTION

[0054] The present invention can be better understood according to the following examples. However, it is easy for those skilled in the art to understand that the contents described in the examples are only used to illustrate the present invention, and should not and will not limit the present invention described in detail in the claims.

[0055] The experimental methods described in the following examples are conventional methods unless otherwise specified; the reagents and materials described are commercially available unless otherwise specified.

[0056] In the following examples, the products were analyzed using a 400 MHz Bruker nuclear magnetic resonance instrument. 1 H NMR measurement: Take 6 mg of polyamide sample and put it into NMR tube, add deuterated trifluoroacetic acid, shake until it is completely dissolved and then measure the sample.

[0057] The products were analyzed using a 400 MHz Bruker NMR instrument. 13 C NMR measurement: Take 20 mg of polyamide sample and put it into NMR tube, add deuterated sulfuric acid, shake until it is completely dissolved and then measure the sample.

[0058] The sample decomposition temperature is measured by TGA 550, which is the temperature at which the mass loss is 5%. 5-10 mg of sample is weighed on a platinum plate, and the temperature is increased at a rate of 20°C / min under the protection of inert gas nitrogen, and the measurement temperature range is 30-800°C.

[0059] The melting temperature of the sample is obtained by the DSC 250 equipment test and obtained through the second temperature scanning curve. Weigh 5-10 mg of sample on a platinum plate, and under the protection of inert gas nitrogen, set the program to heat up first, then cool down, and finally heat up again. The starting temperature of the heating is 30°C, and the final temperature is the temperature when the sample degrades 5% under thermogravimetric analysis; cooling is the sample from the highest temperature back to 30°C. At 10°C min -1 at a rate of .

[0060] The relative viscosity of the furan-based polyamide in the present invention is measured by an Ubbelohde viscometer with an inner diameter of 1.07 mm, using 96% concentrated sulfuric acid as a solvent and a sample concentration of 10 mg / mL.

[0061] Example 1

[0062] At room temperature, 1 mol of 1,4-butanediamine is first dissolved in an equal volume of ethanol, and then 0.2 mol of dibutyl oxalate solution is added dropwise at a flow rate of 300uL / min under nitrogen protection and stirring at a rate of 400rpm. After the addition is completed, stirring is continued for 2 hours. While esterification is being carried out, the excess 1,4-butanediamine will end-cap the oxalate to obtain the desired product. After the reaction is completed, the white solid obtained by suction filtration is washed with ethanol, and the solid is dried to obtain a crude product. The crude product is recrystallized with butyl acetate, the insoluble matter is filtered off, the solution is allowed to stand at low temperature, the precipitated product is washed with ethanol, and the solid is dried to obtain a white aliphatic diamine monomer.

[0063] 1.02 mmol of the above aliphatic diamine monomer and 1 mmol of dimethyl 2,5-furandicarboxylate were added to the reaction vessel. Argon was replaced at room temperature for 10 minutes, and the reaction vessel was heated to 120°C, and then the temperature was gradually increased to 180°C at a rate of 3°C / 10min, and maintained at this temperature for 3 hours. Then the temperature was increased to 200°C, and the vacuum negative pressure was 50Pa for 4 hours.

[0064] After the polycondensation was completed, stirring was stopped, the polymer was discharged into cooling water, placed in an oven at 60°C, and dried for 12 hours to obtain furan-based polyamide, and the relative viscosity of the product was 1.47. g At 120°C, T m 241℃, T d5% 380℃, T max The temperature is 459℃ and the tensile strength is 62MPa.

[0065] Example 2

[0066] At room temperature, 1 mol of 1,5-pentanediamine is first dissolved in an equal volume of ethanol, and then 0.25 mol of diethyl oxalate solution is added dropwise at a flow rate of 200uL / min under nitrogen protection and stirring at a rate of 500rpm. After the addition is completed, stirring is continued for 2 hours. While esterification is being carried out, the excess 1,5-pentanediamine will end-cap the oxalate to obtain the desired product. After the reaction is completed, the white solid obtained by suction filtration is washed with ethanol, and the solid is dried to obtain a crude product. The crude product is recrystallized with butyl acetate, the insoluble matter is filtered out, the solution is allowed to stand at low temperature, the precipitated product is washed with ethanol, and the solid is dried to obtain a white aliphatic diamine monomer.

[0067] 1.04 mmol of the aliphatic diamine monomer of the designed structure and 1 mmol of 2,5-furandicarboxylic acid chloride were added to the reaction vessel. Argon was replaced at room temperature for 10 minutes, and the reaction vessel was heated to 140°C, and then the temperature was gradually increased to 200°C at a rate of 5°C / 10min, and maintained at this temperature for 3 hours. Then the temperature was increased to 220°C, and the vacuum negative pressure was 80Pa for 4 hours.

[0068] After the polycondensation was completed, stirring was stopped, the polymer was discharged into cooling water, placed in an oven at 60°C, and dried for 12 hours to obtain furan-based polyamide, and the relative viscosity of the product was 1.58. g 130℃, T d5% 390℃, T max The temperature is 462℃ and the tensile strength is 39MPa.

[0069] Example 3

[0070] At room temperature, 1.2 mol of 1,6-hexanediamine was first dissolved in an equal volume of ethanol, and then 0.2 mol of diethyl oxalate solution was added dropwise at a flow rate of 400uL / min under nitrogen protection and stirring at a rate of 350rpm. After the addition was completed, stirring was continued for 2 hours. While esterification was being carried out, the excess 1,6-hexanediamine would end-cap the oxalate to obtain the desired product. After the reaction was completed, the white solid obtained by suction filtration was washed with ethanol, and the solid was dried to obtain a crude product. The crude product was recrystallized with butyl acetate, the insoluble matter was filtered out, the solution was allowed to stand at low temperature, the precipitated product was washed with ethanol, and the solid was dried to obtain a white aliphatic diamine monomer with a designed structure.

[0071] 1.01 mmol of the above aliphatic diamine monomer and 1 mmol of dibutyl 2,5-furandicarboxylate were added to the reaction vessel. Argon was replaced at room temperature for 10 minutes, and the reaction vessel was heated to 160°C, and then the temperature was gradually increased to 200°C at a rate of 6°C / 10min, and maintained at this temperature for 3 hours. Then the temperature was increased to 250°C, and the vacuum negative pressure was 120Pa for 5 hours.

[0072] After the polycondensation was completed, stirring was stopped, the polymer was discharged into cooling water, placed in an oven at 60°C, and dried for 12 hours to obtain furan-based polyamide, and the relative viscosity of the product was 1.49. g At 120°C, T m 217℃, T d5% 393℃, T max The temperature is 471℃ and the tensile strength is 55MPa.

[0073] Example 4

[0074] At room temperature, 1 mol of 1,10-decanediamine was first dissolved in an equal volume of ethanol, and then 0.2 mol of diethyl oxalate solution was added dropwise at a flow rate of 250uL / min under nitrogen protection and stirring at a rate of 450rpm. After the addition was completed, stirring was continued for 2 hours. While esterification was being carried out, the excess 1,10-decanediamine would end-cap the oxalate to obtain the desired product. After the reaction was completed, the white solid obtained by filtration was washed with ethanol, and the solid was dried to obtain a crude product. The crude product was recrystallized with butyl acetate, the insoluble matter was filtered out, the solution was allowed to stand at low temperature, the precipitated product was washed with ethanol, and the solid was dried to obtain a white aliphatic diamine monomer with a designed structure.

[0075] 1.03 mmol of the above aliphatic diamine monomer and 1 mmol of diethyl 2,5-furandicarboxylate were added to the reaction vessel. Argon was replaced at room temperature for 10 minutes, and the reaction vessel was heated to 140°C, and then the temperature was gradually increased to 220°C at a rate of 4°C / 10min, and maintained at this temperature for 3 hours. Then the temperature was increased to 250°C, and the vacuum negative pressure was 300Pa for 5 hours.

[0076] After the polycondensation was completed, stirring was stopped, the polymer was discharged into cooling water, placed in an oven at 60°C, and dried for 12 hours to obtain furan-based polyamide, and the relative viscosity of the product was 1.37. g is 69℃, T m is 180℃, T d5% 412℃, T max The temperature is 473℃ and the tensile strength is 49MPa.

[0077] Example 5

[0078] 200 mg of the furanyl polyamide prepared in Example 2 and 5 mL of 1M sodium hydroxide aqueous solution were added to a pressure tube, and the reaction vessel was heated to 180°C and maintained at this temperature for 10 hours. After cooling to room temperature, the filtrate was collected and 1,5-pentanediamine was obtained by vacuum distillation with a yield of about 55%. Aqueous hydrochloric acid was added dropwise to the remaining salt solution after vacuum distillation to adjust the pH to 2-3. Furandicarboxylic acid was precipitated, washed with ethanol, and vacuum dried overnight to obtain pure furandicarboxylic acid with a yield of 81%.

[0079] The above-mentioned embodiments only express several implementation methods of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the scope of the patent of the present invention. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.

Claims

1. A furan-based polyamide as shown in formula I; in, R is selected from C4-C 12 alkyl; n is any integer selected from 10 to 500.

2. The method for preparing the furan-based polyamide according to claim 1, characterized in that: The method comprises reacting an aliphatic diamine monomer containing an oxalic acid amide group as shown in formula II with a furan dicarboxylic acid derivative monomer to prepare a furan-based polyamide as shown in formula I; in, R is selected from C4-C 12 alkyl.

3. The preparation method according to claim 2, characterized in that: The preparation method of the aliphatic diamine monomer containing oxalic acid amide group shown in formula II comprises: reacting oxalic acid dibasic ester with C4-C 12 Reaction of aliphatic diamines.

4. The preparation method according to claim 3, characterized in that: The dibasic oxalate includes dimethyl oxalate, diethyl oxalate, dibutyl oxalate, or any combination thereof; the molar ratio of the dibasic oxalate to the C4-C12 aliphatic diamine is 0.1-0.3:

1.

5. The preparation method according to claim 2, characterized in that: The furan dicarboxylic acid derivative monomer includes 2,5-furan dicarboxylic acid, 2,5-furan dicarboxylic acid dimethyl ester, 2,5-furan dicarboxylic acid diethyl ester, 2,5-furan dicarboxylic acid dibutyl ester, 2,5-furan dicarboxylic acid chloride, or any combination thereof.

6. The preparation method according to claim 2, characterized in that: Under an inert atmosphere, the aliphatic diamine monomer containing oxalic acid amide group shown in formula II and the furan dicarboxylic acid derivative monomer are heated to a first temperature, then heated to a second temperature for ester exchange reaction, and then heated to a third temperature for polycondensation reaction to obtain the furan-based polyamide.

7. The preparation method according to claim 6, characterized in that: The first temperature is selected from 110-170°C, preferably 120-160°C; the second temperature is selected from 170-230°C, preferably 180-220°C; the third temperature is selected from 190-260°C, preferably 200-250°C; at the same time, the first temperature < second temperature < third temperature.

8. The preparation method according to claim 6, characterized in that: The temperature is raised to the second temperature and maintained for 1-4 hours to carry out the ester exchange reaction.

9. The preparation method according to claim 6, characterized in that: The temperature is raised to the third temperature and vacuum is applied for 1-9 hours to carry out polycondensation reaction.

10. Use of the furan-based polyamide according to claim 1 in the preparation of chemically recyclable materials.

Citation Information

Patent Citations

  • Hybrid polyester and preparation method thereof

    CN107189049A

  • A solvent-free melt polycondensation process of making furan-based polyamides

    CN108699240A

  • Pentanediamine ethanedioate and crystal thereof

    CN109265354A

  • Transparent bio-based polyamide and preparation method thereof

    CN111234207A

  • Preparation method of high molecular weight furan polyamide

    CN113429569A

Cited By

  • Aliphatic long-carbon-chain copolyamide resin containing oxamide component and preparation method of aliphatic long-carbon-chain copolyamide resin

    CN119264415A

  • High-pressure-resistant heat-resistant PVC (polyvinyl chloride) insulating electrical conduit and preparation method thereof

    CN120904596A

  • Bio-based polyester amide elastomer, foam and preparation method therefor

    WO2026227683A1