Composition for treating mine soil pollution and preparation method thereof

By using compositions prepared from phosphorus-solubilizing bacteria, papermaking sludge and other materials, the problems of large engineering volume, secondary pollution and long cycle of chemical remediation in mine soil remediation technology have been solved, and the effective degradation of heavy metals and the reduction of environmental risks have been achieved. , suitable for soil treatment of different scales and pollution levels.

CN118745348APending Publication Date: 2024-10-08MINGCHUANG HUIYUAN TECH GRP CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310796255.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-07-02
Publication Date
2024-10-08

AI Technical Summary

Technical Problem

The existing mine soil remediation technology has the problems of large engineering volume, consumption of manpower, material and financial resources, chemical remediation may produce secondary pollution, long phytoremediation cycle and poor processing methods.

Method used

A composition including phosphorus-solubilizing bacteria, papermaking sludge, quicklime, butyl orthosilicate, wheat straw, corn grass and absolute ethanol is prepared through specific mixing and stirring steps to form a composition capable of adsorption, complexation, and precipitation. , redox and ion exchange reaction compositions for controlling mine soil pollution.

Benefits of technology

The composition can reduce the bioavailability of heavy metals, reduce environmental risks, does not produce secondary pollution, is suitable for soil treatment of different sizes and pollution levels, and reduces the harm of heavy metals to the ecological environment and human health.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention relates to the technical field of mine soil pollution treatment, and discloses a preparation method of a composition for treating mine soil pollution, which comprises the following steps: S11, drying paper mill sludge with the humidity of 40-60% until the water content is lower than 10%, and crushing into powder for later use; s13, tetrabutyl orthosilicate and sterile water are sequentially added into absolute ethyl alcohol, then mixing is conducted through a stirring machine, the stirring time is controlled to be 20-57 min, a solution A1 is obtained, soil heavy metal can be refined by additionally and reasonably matching chemical components, the soil heavy metal content is reduced, the soil heavy metal content is reduced, the soil heavy metal content is reduced, and the soil heavy metal content is reduced. Through a series of reactions such as adsorption, complexation, precipitation, oxidation reduction and ion exchange, the chemical form of heavy metal elements in soil is changed, the influence of heavy metal on plants is reduced, and the harm of heavy metal to the ecological environment and human health is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of mine soil pollution control, in particular to a composition for controlling mine soil pollution and a preparation method thereof. Background Art

[0002] Methods for mine soil remediation are generally divided into physical remediation, chemical remediation and biological remediation. However, existing mine soil remediation technologies, whether physical remediation, chemical remediation or phytoremediation, have certain drawbacks. Physical remediation projects are large in scale and consume manpower, material resources and financial resources. Various chemical reagents used in chemical remediation are prone to secondary pollution when applied to the soil. The phytoremediation cycle is long, and there is no good way to deal with plants enriched with heavy metals. Based on the above shortcomings, technicians in this field have proposed a composition for controlling mine soil pollution and a preparation method thereof to solve the above problems. Summary of the invention

[0003] In view of the deficiencies of the prior art, the present invention provides a composition for treating mine soil pollution and a preparation method thereof, which solves the problem of secondary pollution caused by the existing chemical means for treating mine soil pollution.

[0004] To achieve the above purpose, the present invention is implemented through the following technical scheme: a composition for treating mine soil pollution, comprising the following raw materials in parts by weight: 50 to 60 parts of phosphate-solubilizing bacteria, 50 to 90 parts of papermaking sludge, 5 to 30 parts of quicklime, 15 to 25 parts of butyl orthosilicate, 30 to 60 parts of wheat straw, 15 to 35 parts of corn straw, 6 to 8 parts of sterile water, 9 to 20 parts of cosolvent, and 50 to 90 parts of anhydrous ethanol.

[0005] Preferably, the phosphate-dissolving bacteria is prepared by the following steps:

[0006] S1. Take 40-50 g of potassium feldspar and mix it with pure water, shake and incubate at room temperature to obtain a diluted solution A;

[0007] S2. The diluted solution A is mixed with a potassium-free culture medium and the culture time is 50 min to finally obtain phosphate-dissolving bacteria.

[0008] Preferably, in step S2, the culture humidity of the potassium-free culture medium is controlled at 40-55%, and the temperature is set at 55-60°C.

[0009] Preferably, the co-solvent is one or a combination of propylene glycol, ethylene glycol, and chlorinated hydrocarbons.

[0010] A method for preparing a composition for treating mine soil pollution comprises the following steps:

[0011] S11, taking papermaking sludge with a humidity of 40-60%, drying it to a moisture content of less than 10%, and crushing it into powder for later use;

[0012] S12, drying the wheat straw and corn straw in the sun, and crushing them into particles A with a particle size of 5 to 15 mm by a crushing mechanism;

[0013] S13, adding butyl orthosilicate and sterile water to anhydrous ethanol in sequence, and then mixing them by a stirrer, with the stirring time controlled at 20 to 57 minutes to obtain a solution A1;

[0014] S14, adding the particle A to the solution A1 obtained in step S13, stirring and mixing, and finally keeping the temperature at 65° C. for 30 min and standing to obtain a solution B1

[0015] S15, adding the powder obtained in step S11 to solution B1, and then adding a solvent, quicklime and phosphate-dissolving bacteria in sequence, continuing to stir, and adjusting the pH range of the solution to 6.1-7.8, to finally form a composition for treating mine soil pollution.

[0016] Preferably, the drying temperature in step S11 is set to 55-70°C.

[0017] Preferably, in the step S12, the drying days are 5 to 15 days, and the crushing speed of the crushing mechanism is 100 to 200 r / min.

[0018] Preferably, in step S13, the stirring speed of the stirrer is 100-200 r / min, the humidity is adjusted to 30-50%, and the temperature is controlled at 80-100°C.

[0019] Preferably, in step S14, the stirring time is controlled to be 30 to 60 minutes.

[0020] Preferably, in step S15, the specific steps of adjusting the pH of the solution are:

[0021] A1. Place the acid-base detector in the mixed solution and determine whether the pH of the solution is too high or too low;

[0022] A2. If the acidity of the mixed solution is too high, sodium hydroxide is added to the mixed solution. If the acidity of the mixed solution is too low, hydrochloric acid is added to the mixed solution to adjust the pH of the solution to 6.1 to 7.8.

[0023] The present invention provides a composition for treating soil pollution in mines and a preparation method thereof.

[0024] Beneficial effects:

[0025] 1. The present invention uses crop straw as the main material, is easy to use, has a simple preparation method, and is easy to achieve large-scale production. Therefore, it can be widely promoted and applied to reduce the bioavailability of heavy metals, reduce environmental risks, and does not produce secondary pollution.

[0026] 2. The present invention can refine soil heavy metals through a series of reactions such as adsorption, complexation, precipitation, oxidation-reduction and ion exchange, thereby changing the chemical form of heavy metal elements in the soil, reducing the impact of heavy metals on plants, and reducing the harm of heavy metals to the ecological environment and human health. In addition, the composition for treating soil pollution is not only simple and practical, but can also treat soils of different sizes and different degrees of pollution, and is suitable for use by people in my country. DETAILED DESCRIPTION

[0027] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0028] Embodiment 1:

[0029] The embodiment of the present invention provides a composition for treating mine soil pollution, comprising the following raw materials in parts by weight: 48 parts of phosphate-dissolving bacteria, 81 parts of papermaking sludge, 26 parts of quicklime, 19 parts of butyl orthosilicate, 36 parts of wheat straw, 18 parts of corn grass, 7 parts of sterile water, 12 parts of cosolvent, and 86 parts of anhydrous ethanol.

[0030] The phosphate-dissolving bacteria are prepared by the following steps:

[0031] S1. Take 46 g of potassium feldspar and mix it thoroughly with pure water, and shake and incubate it at room temperature to obtain a diluted solution A;

[0032] S2. The diluted solution A is mixed with a potassium-free culture medium and the culture time is 50 min to finally obtain phosphate-solubilizing bacteria. The culture humidity of the potassium-free culture medium is controlled at 49% and the temperature is set at 58°C.

[0033] The cosolvent is one or a combination of propylene glycol, ethylene glycol and chlorinated hydrocarbons.

[0034] A method for preparing a composition for treating mine soil pollution comprises the following steps:

[0035] S11, taking papermaking sludge with a humidity of 46%, drying it to a moisture content of less than 10%, and crushing it into powder for later use, and the drying temperature is set to 68°C.

[0036] S12, drying the wheat straw and corn straw, and then crushing them into particles A with a particle size of 6 mm by a crushing mechanism, the drying time is 7 days, and the crushing speed of the crushing mechanism is 120 r / min

[0037] S13. Add butyl orthosilicate and sterile water to anhydrous ethanol in sequence, and then mix them by a stirrer. The stirring time is controlled at 57 min to obtain solution A1. The stirring speed of the stirrer is 180 r / min, the humidity is adjusted to 45%, and the temperature is controlled at 90°C.

[0038] S14, adding the particle A to the solution A1 obtained in step S13, stirring and mixing, and finally keeping the temperature at 65° C. for 30 min, and letting it stand to obtain a solution B1. In step S14, the stirring time is controlled to 45 min.

[0039] S15, adding the powder obtained in step S11 to solution B1, and then adding a solvent, quicklime and phosphate-dissolving bacteria in sequence, continuing to stir, and adjusting the pH range of the solution to 7.2, to finally form a composition for treating mine soil pollution.

[0040] The specific steps for adjusting the pH of the solution are:

[0041] A1. Place the acid-base detector in the mixed solution and determine whether the pH of the solution is too high or too low;

[0042] A2. If the acidity of the mixed solution is too high, sodium hydroxide is added to the mixed solution. If the acidity of the mixed solution is too low, hydrochloric acid is added to the mixed solution to adjust the pH of the solution to 7.2.

[0043] Embodiment 2:

[0044] The embodiment of the present invention provides a composition for treating mine soil pollution, comprising the following raw materials in parts by weight: 59 parts of phosphate-dissolving bacteria, 80 parts of papermaking sludge, 25 parts of quicklime, 17 parts of butyl orthosilicate, 60 parts of wheat straw, 35 parts of corn straw, 7 parts of sterile water, 12 parts of cosolvent, and 86 parts of anhydrous ethanol. The remaining steps are consistent with the experimental steps and methods of Example 1, and the same method is used for characterization. The final soil cadmium and arsenic contents are shown in Table 1 below.

[0045] Comparative Example 1: The phosphate-dissolving bacteria in a composition for treating mine soil pollution in Example 1 were removed, and the other steps were consistent with the experimental steps and methods of Example 1, and the same method was used for characterization. The final soil cadmium and arsenic contents were shown in Table 1 below.

[0046] Comparative Example 2: The papermaking sludge in the composition for treating mine soil pollution in Example 1 was removed, and the other steps were consistent with the experimental steps and methods of Example 1, and the same method was used for characterization. The final soil cadmium and arsenic contents were shown in Table 1 below.

[0047] Comparative Example 3: The wheat straw and corn straw in the composition for treating mine soil pollution in Example 1 were removed, and the other steps were consistent with the experimental steps and methods of Example 1, and the same method was used for characterization. The final soil cadmium and arsenic contents were shown in Table 1 below.

[0048] Comparative Example 4: The butyl orthosilicate in the composition for treating mine soil pollution in Example 1 was removed, and the other steps were consistent with the experimental steps and methods of Example 1, and the same method was used for characterization. The final soil cadmium and arsenic contents were shown in Table 1 below.

[0049] Comparative Example 5: The phosphate-dissolving bacteria and papermaking sludge in a composition for treating mine soil pollution in Example 1 were removed simultaneously, and the other steps were consistent with the experimental steps and methods of Example 1, and the same method was used for characterization. The final soil cadmium and arsenic contents were shown in Table 1 below.

[0050] Comparative Example 6: The mass fraction of phosphate-dissolving bacteria in a composition for treating mine soil pollution in Example 1 was changed to 53 parts, papermaking sludge to 78 parts, and quicklime to 21 parts. The other steps were consistent with the experimental steps and methods of Example 1, and the same method was used for characterization. The final soil cadmium and arsenic contents were shown in Table 1 below.

[0051] Comparative Example 7: The mass fraction of wheat straw in a composition for treating mine soil pollution in Example 1 was changed to 53 parts, papermaking sludge was 90 parts, and butyl orthosilicate was 17 parts. The other steps were consistent with the experimental steps and methods of Example 1, and the same method was used for characterization. The final soil cadmium and arsenic contents are shown in Table 1 below.

[0052] <![CDATA[Cadmium (kg / m 2 )]]> <![CDATA[Arsenic (kg / m 2 ) <!-- 3 -->]]> Embodiment 1 0.15 0.08 Embodiment 2 0.13 0.13 Comparative Example 3 0.13 0.14 Comparative Example 4 0.21 0.22 Comparative Example 5 0.26 0.21 Comparative Example 6 0.13 0.13 Comparative Example 7 0.17 0.08 Prior art 0.25 0.21

[0053] Table 1

[0054] It can be seen from Table 1 that by adding butyl orthosilicate, phosphate-dissolving bacteria, papermaking sludge, and corn grass components to the composition for treating mine soil pollution in the prior art, a series of reactions such as adsorption, complexation, precipitation, oxidation-reduction, and ion exchange can be performed on soil heavy metals, thereby changing the chemical form of heavy metal elements in the soil, reducing the impact of heavy metals on plants, and reducing the harm of heavy metals such as cadmium and arsenic to the ecological environment and human health. In addition, the composition for treating soil pollution is not only simple and practical, but can also be used to treat soils of different sizes and different degrees of pollution, and is suitable for use by people in my country. At the same time, the present invention uses crop straw as the main material, is easy to use, has a simple preparation method, and is easy to achieve large-scale production. Therefore, it can be widely promoted and applied to reduce the biological effectiveness of heavy metals, reduce environmental risks, and does not produce secondary pollution.

[0055] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A composition for treating mine soil pollution, characterized in that: The invention comprises the following raw materials in parts by weight: 50-60 parts of phosphate-dissolving bacteria, 50-90 parts of papermaking sludge, 5-30 parts of quicklime, 15-25 parts of butyl orthosilicate, 30-60 parts of wheat straw, 15-35 parts of corn straw, 6-8 parts of sterile water, 9-20 parts of cosolvent and 50-90 parts of anhydrous ethanol.

2. A composition for treating mine soil pollution according to claim 1, characterized in that: The phosphate-dissolving bacteria are specifically prepared by the following steps: S1. Take 40-50 g of potassium feldspar and mix it with pure water, and shake it at room temperature to obtain a diluted solution A; S2. The diluted solution A is mixed with a potassium-free culture medium and the culture time is 50 minutes to finally obtain phosphate-dissolving bacteria.

3. A composition for treating mine soil pollution according to claim 2, characterized in that: In the step S2, the culture humidity of the potassium-free culture medium is controlled at 40-55%, and the temperature is set at 55-60°C.

4. The composition for treating mine soil pollution according to claim 1, characterized in that: The co-solvent is one or a combination of propylene glycol, ethylene glycol and chlorinated hydrocarbons.

5. A method for preparing a composition for treating mine soil pollution, characterized in that: A composition for treating mine soil pollution according to any one of claims 1 to 4, comprising the following steps: S11, taking papermaking sludge with a humidity of 40-60%, drying it until the moisture content is less than 10%, and crushing it into powder for later use; S12, drying the wheat straw and corn straw in the sun, and crushing them into particles A with a particle size of 5 to 15 mm by a crushing mechanism; S13, adding butyl orthosilicate and sterile water to anhydrous ethanol in sequence, and then mixing them by a stirrer, with the stirring time controlled at 20 to 57 minutes, to obtain a solution A1; S14, adding the particle A to the solution A1 obtained in step S13, stirring and mixing, and finally keeping the mixture at 65° C. for 30 min and standing to obtain a solution B1; S15, adding the powder obtained in step S11 to solution B1, and then adding a solvent, quicklime and phosphate-dissolving bacteria in sequence, continuing to stir, and adjusting the pH range of the solution to 6.1-7.8, to finally form a composition for treating mine soil pollution.

6. A composition for treating mine soil pollution and a preparation method thereof according to claim 5, characterized in that: In step S11, the drying temperature is set to 55-70°C.

7. The method for preparing a composition for treating mine soil pollution according to claim 5, characterized in that: In the step S12, the drying days are 5 to 15 days, and the crushing speed of the crushing mechanism is 100 to 200 r / min.

8. The method for preparing a composition for treating mine soil pollution according to claim 5, characterized in that: In the step S13, the stirring speed of the stirrer is 100-200 r / min, the humidity is adjusted to 30-50%, and the temperature is controlled at 80-100°C.

9. The method for preparing a composition for treating mine soil pollution according to claim 5, characterized in that: In the step S14, the stirring time is controlled to be 30 to 60 minutes.

10. The method for preparing a composition for treating mine soil pollution according to claim 5, characterized in that: In the step S15, the specific steps of adjusting the pH of the solution are: A1. Place the acid-base detector in the mixed solution and determine whether the pH of the solution is too high or too low; A2. If the acidity of the mixed solution is too high, sodium hydroxide is added to the mixed solution. If the acidity of the mixed solution is too low, hydrochloric acid is added to the mixed solution to adjust the pH of the solution to 6.1 to 7.8.