Bonding device and bonding method

By using multiple annular areas to independently control the adsorption pressure in the substrate processing device, the problem of strain control on the substrate adsorption surface is solved and the bonding accuracy and quality are improved.

CN118748157APending Publication Date: 2024-10-08TOKYO ELECTRON LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410680731.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2018-01-17
Filing Date
2019-01-09
Publication Date
2024-10-08

AI Technical Summary

Technical Problem

The existing technology is difficult to effectively control the strain of the substrate adsorbed on the adsorption surface, affecting the accuracy and quality of substrate bonding.

Method used

A substrate processing device is designed, which uses multiple annular areas as adsorption pressure control areas. The adsorption pressure of each area is independently controlled through a vacuum pump and a vacuum regulator to achieve fine adjustment of multi-region pressure on the substrate adsorption surface.

Benefits of technology

It achieves fine control of the strain on the substrate adsorption surface, reduces the bonding strain during the substrate bonding process, and improves the bonding accuracy and quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118748157A_ABST
    Figure CN118748157A_ABST
Patent Text Reader

Abstract

The invention relates to a bonding apparatus and a bonding method. The substrate processing apparatus is provided with: a holding unit having a circular first region and an annular second region disposed radially outward of the first region on an adsorption surface for adsorbing a substrate, the holding unit serving as a plurality of regions in which adsorption pressures for adsorbing the substrate are individually controlled; a plurality of suction pressure generation units that individually generate a suction pressure in each of a plurality of regions constituting the suction surface; a plurality of adsorption pressure adjustment units that individually adjust the adsorption pressure generated by each of the plurality of adsorption pressure generation units, the adsorption pressure being generated by each of the plurality of adsorption pressure generation units; and a control unit that controls the plurality of suction pressure generation units and the plurality of suction pressure adjustment units, the control unit causing different suction pressures to be generated in at least a part of the first region and at least a part of the second region.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] This application is a divisional application of an application with a filing date of January 9, 2019, application number 201980008044.X, and invention name “Substrate processing device and substrate processing method”. Technical Field

[0002] The present disclosure relates to a substrate processing apparatus and a substrate processing method. Background Art

[0003] The bonding device described in Patent Document 1 includes an upper chuck that sucks the upper substrate from above and a lower chuck that sucks the lower substrate from below, and the two substrates are bonded on the basis of being face to face. Specifically, first, the bonding device presses down the center of the substrate sucked on the upper chuck so that it contacts the center of the substrate sucked on the lower chuck. As a result, the center of the two substrates are bonded to each other due to intermolecular forces, etc. Next, the bonding device expands the bonded bonding area of ​​the two substrates from the center to the periphery.

[0004] Prior art literature

[0005] Patent Literature

[0006] Patent Document 1: Japanese Patent Application Publication No. 2015-095579 Summary of the invention

[0007] Problem that the invention aims to solve

[0008] A technical solution of the present disclosure provides a technology capable of controlling the strain of a substrate adsorbed on an adsorption surface.

[0009] Solutions for solving problems

[0010] A substrate processing device according to a technical solution of the present disclosure comprises:

[0011] A holding portion having a circular first region and an annular second region disposed radially outside the first region on a suction surface for suctioning the substrate, as a plurality of regions in which suction pressure for suctioning the substrate is individually controlled;

[0012] A plurality of adsorption pressure generating units, wherein the plurality of adsorption pressure generating units generate adsorption pressure individually in each of the plurality of regions constituting the adsorption surface;

[0013] a plurality of adsorption pressure adjusting units, wherein the plurality of adsorption pressure adjusting units individually adjust the adsorption pressure generated by each of the plurality of adsorption pressure generating units; and

[0014] a control unit that controls the plurality of adsorption pressure generating units and the plurality of adsorption pressure adjusting units,

[0015] The control unit generates different adsorption pressures in at least a portion of the first region and at least a portion of the second region.

[0016] Effects of the Invention

[0017] According to a technical solution of the present disclosure, the strain of a substrate adsorbed on an adsorption surface can be controlled. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 It is a top view showing a joining system according to one embodiment.

[0019] Figure 2 It is a side view which shows the joining system of one embodiment.

[0020] Figure 3 This is a side view showing a state before the first substrate and the second substrate are bonded together according to one embodiment.

[0021] Figure 4 It is a top view showing a bonding device according to one embodiment.

[0022] Figure 5 It is a side view showing a bonding device according to one embodiment.

[0023] Figure 6 1 is a cross-sectional view showing an upper chuck and a lower chuck according to an embodiment, and is a cross-sectional view showing a state after an upper wafer and a lower wafer are aligned and before being bonded.

[0024] Figure 7 This is a cross-sectional view showing a state in which an upper wafer and a lower wafer are gradually bonded from a center portion toward an outer periphery portion according to one embodiment.

[0025] Figure 8 This is a flowchart showing a part of the processing executed by the joining system according to one embodiment.

[0026] Fig. 9 It is a diagram showing a lower chuck, a vacuum pump, and a vacuum regulator according to one embodiment.

[0027] Fig.10 It is a diagram showing a lower chuck, a vacuum pump, and a vacuum regulator according to a first modified example.

[0028] Fig.11 It is a diagram showing a lower chuck, a vacuum pump, and a vacuum regulator according to a second modified example.

[0029] Fig.12 It is a diagram showing a lower chuck, a vacuum pump, and a vacuum regulator according to a third modified example. DETAILED DESCRIPTION

[0030] Hereinafter, the embodiments of the present disclosure will be described with reference to the accompanying drawings. In each of the accompanying drawings, the same or corresponding structures are marked with the same or corresponding figure marks and the description is omitted. In the following description, the X-axis direction, the Y-axis direction and the Z-axis direction are directions perpendicular to each other, the X-axis direction and the Y-axis direction are horizontal directions, and the positive direction of the Z-axis is the vertical direction. The rotation direction with the vertical axis as the rotation center is also referred to as the θ direction. In this specification, the bottom refers to the vertical bottom, and the top refers to the vertical top.

[0031] <Joint system>

[0032] Figure 1 It is a top view showing a joining system according to one embodiment. Figure 2 It is a side view which shows the joining system of one embodiment. Figure 3 This is a side view showing a state before the first substrate and the second substrate are bonded together according to one embodiment. Figure 1 The bonding system 1 shown in FIG. 1 forms a stacked substrate T (see FIG. 1 ) by bonding a first substrate W1 and a second substrate W2. Figure 7 (b)).

[0033] The first substrate W1 is a substrate on which a plurality of electronic circuits are formed on a semiconductor substrate such as a silicon wafer or a compound semiconductor wafer. In addition, the second substrate W2 is, for example, a bare wafer on which no electronic circuits are formed. The first substrate W1 and the second substrate W2 have substantially the same diameter. In addition, an electronic circuit may also be formed on the second substrate W2.

[0034] In the following, the first substrate W1 is sometimes referred to as “upper wafer W1”, the second substrate W2 is sometimes referred to as “lower wafer W2”, and the overlapping substrate T is sometimes referred to as “overlapping wafer T”. Figure 3 As shown, the plate surface of the upper wafer W1 on the side bonded to the lower wafer W2 is recorded as a "bonding surface W1j", and the plate surface on the opposite side of the bonding surface W1j is recorded as a "non-bonding surface W1n". In addition, the plate surface of the lower wafer W2 on the side bonded to the upper wafer W1 is recorded as a "bonding surface W2j", and the plate surface on the opposite side of the bonding surface W2j is recorded as a "non-bonding surface W2n".

[0035] like Figure 1 As shown, the bonding system 1 includes a feeding station 2 and a processing station 3. The feeding station 2 and the processing station 3 are arranged in the order of the feeding station 2 and the processing station 3 along the positive direction of the X axis. In addition, the feeding station 2 and the processing station 3 are connected as a whole.

[0036] The loading and unloading station 2 includes a loading platform 10 and a conveying area 20. The loading platform 10 includes a plurality of loading plates 11. Boxes CS1, CS2, and CS3 for storing a plurality of (e.g., 25) substrates in a horizontal state are placed on each loading plate 11. For example, box CS1 is a box for storing an upper wafer W1, box CS2 is a box for storing a lower wafer W2, and box CS3 is a box for storing overlapping wafers T.

[0037] The conveying area 20 is arranged adjacent to the mounting table 10 on the positive X-axis direction side of the mounting table 10. The conveying area 20 is provided with a conveying path 21 extending in the Y-axis direction and a conveying device 22 that can move along the conveying path 21. The conveying device 22 can move not only in the Y-axis direction but also in the X-axis direction and can rotate around the Z-axis, and conveys the upper wafer W1, the lower wafer W2, and the overlapping wafer T between the cassettes CS1 to CS3 mounted on the mounting plate 11 and the third processing module G3 of the processing station 3 described later.

[0038] The number of cassettes CS1 to CS3 placed on the placement plate 11 is not limited to the number shown in the figure. In addition, on the placement plate 11, in addition to the cassettes CS1, CS2, and CS3, a cassette for collecting defective substrates may be placed.

[0039] The processing station 3 is provided with a plurality of processing modules including various devices, for example, three processing modules G1, G2, and G3. For example, the first processing module G1 is provided on the front side of the processing station 3 ( Figure 1 The second processing module G2 is provided on the back side of the processing station 3 ( Figure 1 In addition, the third processing module G3 is arranged on the side of the processing station 3 close to the feeding and unfeeding station 2 ( Figure 1 The position on the negative side of the X-axis.

[0040] The first processing module G1 is provided with a surface modification device 30 for modifying the bonding surface W1j of the upper wafer W1 and the bonding surface W2j of the lower wafer W2. The surface modification device 30 modifies the SiO 2 The bonds of W1j and W2j are cut to form single-bonded SiO, thereby modifying the bonding surfaces W1j and W2j to facilitate subsequent hydrophilization.

[0041] In addition, in the surface modification device 30, oxygen or nitrogen as a processing gas is excited to be plasma and ionized, for example, under a reduced pressure atmosphere. Then, the oxygen ions or nitrogen ions are irradiated to the bonding surface W1j of the upper wafer W1 and the bonding surface W2j of the lower wafer W2, so that the bonding surfaces W1j and W2j are plasma-treated and modified.

[0042] The second processing module G2 is provided with a surface hydrophilization device 40 and a bonding device 41. The surface hydrophilization device 40, for example, uses pure water to hydrophilize the bonding surface W1j of the upper wafer W1 and the bonding surface W2j of the lower wafer W2, and cleans the bonding surfaces W1j and W2j. In the surface hydrophilization device 40, for example, while rotating the upper wafer W1 or the lower wafer W2 held on the rotating chuck, pure water is supplied to the upper wafer W1 or the lower wafer W2. Thus, the pure water supplied to the upper wafer W1 or the lower wafer W2 diffuses on the bonding surface W1j of the upper wafer W1 or the bonding surface W2j of the lower wafer W2, so that the bonding surfaces W1j and W2j are hydrophilized.

[0043] The bonding apparatus 41 bonds the hydrophilized upper wafer W1 and the lower wafer W2 together by intermolecular force. The structure of the bonding apparatus 41 will be described later.

[0044] In the third processing module G3, as Figure 2 As shown, the upper wafer W1, the lower wafer W2 and the transfer (TRS) devices 50, 51 of the overlapping wafer T are sequentially arranged from the bottom and arranged in two layers.

[0045] In addition, if Figure 1 As shown, a conveying area 60 is formed in an area surrounded by the first processing module G1, the second processing module G2, and the third processing module G3. A conveying device 61 is arranged in the conveying area 60. The conveying device 61 has, for example, a conveying arm that can move freely in a vertical direction, in a horizontal direction, and around a vertical axis. The conveying device 61 moves in the conveying area 60 and conveys the upper wafer W1, the lower wafer W2, and the overlapping wafer T to the prescribed devices in the first processing module G1, the second processing module G2, and the third processing module G3 adjacent to the conveying area 60.

[0046] In addition, if Figure 1 As shown in FIG. 1 , the joining system 1 includes a control device 70. The control device 70 controls the operation of the joining system 1. The control device 70 is constituted by, for example, a computer. Figure 1 As shown, the control device 70 has a CPU (Central Processing Unit) 71, a storage medium 72 such as a memory, an input interface 73, and an output interface 74. The control device 70 performs various controls by causing the CPU 71 to execute a program stored in the storage medium 72. In addition, the control device 70 receives signals from the outside using the input interface 73 and sends signals to the outside using the output interface 74.

[0047] The program of the control device 70 is stored in an information storage medium and installed from the information storage medium. Examples of the information storage medium include a hard disk (HD), a floppy disk (FD), a compact disk (CD), a magneto-optical disk (MO), and a memory card. In addition, the program can also be downloaded from a server via the Internet and installed.

[0048] <Joining device>

[0049] Figure 4 It is a top view showing a bonding device according to one embodiment. Figure 5 It is a side view showing a bonding device according to one embodiment.

[0050] like Figure 4 As shown, the bonding apparatus 41 has a sealed processing container 100. A delivery port 101 for the upper wafer W1, the lower wafer W2 and the stacked wafer T is formed on the side of the processing container 100 near the transfer area 60, and a shutter 102 is provided at the delivery port 101.

[0051] The interior of the processing container 100 is divided into a conveying area T1 and a processing area T2 by an inner wall 103. The above-mentioned delivery port 101 is formed on the side of the delivery area T1 of the processing container 100. In addition, delivery ports 104 for upper wafers W1, lower wafers W2 and overlapping wafers T are also formed on the inner wall 103.

[0052] In the transport region T1 , the conveyor 110 , the wafer transport mechanism 111 , the reversing mechanism 130 , and the position adjustment mechanism 120 are arranged in the order described above, for example, from the side of the carry-in / carry-out port 101 .

[0053] The conveyor 110 temporarily mounts the upper wafer W1 , the lower wafer W2 , and the overlapping wafer T. The conveyor 110 is formed in two stages, for example, and can mount any two of the upper wafer W1 , the lower wafer W2 , and the overlapping wafer T at the same time.

[0054] like Figure 4 and Figure 5 As shown, the wafer conveying mechanism 111 has, for example, a conveying arm that can move freely in the vertical direction (Z-axis direction), in the horizontal direction (Y-axis direction, X-axis direction) and around the vertical axis. The wafer conveying mechanism 111 can convey the upper wafer W1, the lower wafer W2, and the overlapping wafer T within the conveying area T1 or between the conveying area T1 and the processing area T2.

[0055] The position adjustment mechanism 120 adjusts the horizontal orientation of the upper wafer W1 and the lower wafer W2. Specifically, the position adjustment mechanism 120 has a base 121 and a detection unit 122. The base 121 has a holding unit (not shown) that holds and rotates the upper wafer W1 and the lower wafer W2. The detection unit 122 detects the position of the notch of the upper wafer W1 and the lower wafer W2. The position adjustment mechanism 120 rotates the upper wafer W1 and the lower wafer W2 held on the base 121 while using the detection unit 122 to detect the position of the notch of the upper wafer W1 and the lower wafer W2, thereby adjusting the position of the notch. Thus, the horizontal orientation of the upper wafer W1 and the lower wafer W2 is adjusted.

[0056] The flip mechanism 130 flips the front and back surfaces of the upper wafer W1. Specifically, the flip mechanism 130 has a holding arm 131 for holding the upper wafer W1. The holding arm 131 extends in the horizontal direction (X-axis direction). In addition, holding members 132 for holding the upper wafer W1 are provided at, for example, four locations of the holding arm 131.

[0057] The holding arm 131 is supported by a driving unit 133, for example, including a motor. The holding arm 131 is able to rotate freely around a horizontal axis by means of the driving unit 133. In addition, the holding arm 131 is able to rotate freely around the driving unit 133 and is able to move freely in the horizontal direction (X-axis direction). Another driving unit (not shown), for example, including a motor, is provided below the driving unit 133. By means of the other driving unit, the driving unit 133 can be moved in the vertical direction along a support column 134 extending in the vertical direction.

[0058] Thus, the upper wafer W1 held by the holding member 132 can be rotated around the horizontal axis and can be moved in the vertical direction and the horizontal direction by the driving unit 133. In addition, the upper wafer W1 held by the holding member 132 can be rotated around the driving unit 133 and moved between the position adjustment mechanism 120 and the upper chuck 140 described later.

[0059] An upper chuck 140 and a lower chuck 141 are provided in the processing area T2. The upper chuck 140 holds the upper surface (non-joining surface W1n) of the upper wafer W1 from above by suction, and the lower chuck 141 holds the lower wafer W2 and holds the lower surface (non-joining surface W2n) of the lower wafer W2 from below by suction. The lower chuck 141 is provided below the upper chuck 140 and can be arranged opposite to the upper chuck 140.

[0060] like Figure 5 As shown, the upper chuck 140 is held by an upper chuck holding portion 150 disposed above the upper chuck 140. The upper chuck holding portion 150 is disposed on the top surface of the processing container 100. The upper chuck 140 is fixed to the processing container 100 by the upper chuck holding portion 150.

[0061] The upper chuck holding portion 150 is provided with an upper imaging portion 151 for imaging the upper surface (joining surface W2j) of the lower wafer W2 held by the lower chuck 141. For example, a CCD camera is used as the upper imaging portion 151.

[0062] The lower chuck 141 is supported by the first lower chuck moving part 160 provided below the lower chuck 141. The first lower chuck moving part 160 moves the lower chuck 141 in the horizontal direction (X-axis direction) as described later. In addition, the first lower chuck moving part 160 is configured to allow the lower chuck 141 to move freely in the vertical direction and to rotate around the vertical axis.

[0063] The first lower chuck moving unit 160 is provided with a lower imaging unit 161 (see FIG. 1 ) for imaging the lower surface (joining surface W1 j ) of the upper wafer W1 held by the upper chuck 140 . Figure 5 ). The lower imaging unit 161 uses, for example, a CCD camera.

[0064] The first lower chuck moving part 160 is attached to a pair of guide rails 162, 162 which are provided on the lower surface side of the first lower chuck moving part 160 and extend in the horizontal direction (X-axis direction). The first lower chuck moving part 160 is configured to be movable along the guide rails 162.

[0065] A pair of guide rails 162, 162 are disposed on the second lower chuck moving portion 163. The second lower chuck moving portion 163 is mounted on a pair of guide rails 164, 164 disposed on the lower surface side of the second lower chuck moving portion 163 and extending in the horizontal direction (Y-axis direction). Moreover, the second lower chuck moving portion 163 is configured to be movable in the horizontal direction (Y-axis direction) along the guide rails 164. In addition, the pair of guide rails 164, 164 are disposed on a mounting table 165 disposed on the bottom surface of the processing container 100.

[0066] The first lower chuck moving part 160 and the second lower chuck moving part 163 constitute the position alignment part 166. The position alignment part 166 moves the lower chuck 141 in the X-axis direction, the Y-axis direction, and the θ direction, thereby performing horizontal position alignment between the upper wafer W1 held by the upper chuck 140 and the lower wafer W2 held by the lower chuck 141. In addition, the position alignment part 166 moves the lower chuck 141 in the Z-axis direction, thereby performing vertical position alignment between the upper wafer W1 held by the upper chuck 140 and the lower wafer W2 held by the lower chuck 141.

[0067] In addition, the position alignment unit 166 of the present embodiment performs horizontal position alignment between the upper wafer W1 and the lower wafer W2 by moving the lower chuck 141 in the X-axis direction, the Y-axis direction, and the θ direction, but the technology disclosed in the present invention is not limited to this. The position alignment unit 166 only needs to be able to relatively move the upper chuck 140 and the lower chuck 141 in the X-axis direction, the Y-axis direction, and the θ direction. For example, the position alignment unit 166 may perform horizontal position alignment between the upper wafer W1 and the lower wafer W2 by moving the lower chuck 141 in the X-axis direction and the Y-axis direction, and moving the upper chuck 140 in the θ direction.

[0068] In addition, the position alignment unit 166 of the present embodiment performs vertical position alignment between the upper wafer W1 and the lower wafer W2 by moving the lower chuck 141 in the Z-axis direction, but the technology disclosed in the present invention is not limited to this. The position alignment unit 166 only needs to be able to relatively move the upper chuck 140 and the lower chuck 141 in the Z-axis direction. For example, the position alignment unit 166 may also perform vertical position alignment between the upper wafer W1 and the lower wafer W2 by moving the upper chuck 140 in the Z-axis direction.

[0069] Figure 6 1 is a cross-sectional view showing an upper chuck and a lower chuck according to an embodiment, and is a cross-sectional view showing a state immediately before an upper wafer and a lower wafer are bonded. Figure 7 (a) is a cross-sectional view showing a state in which an upper wafer and a lower wafer are being bonded together according to one embodiment. Figure 7 (b) is a cross-sectional view showing a state where the upper wafer and the lower wafer are bonded to each other in one embodiment. Figure 6 , Figure 7 (a) and Figure 7 In (b), the arrow shown by the solid line indicates the suction direction of the air by the vacuum pump.

[0070] The upper chuck 140 and the lower chuck 141 are, for example, vacuum chucks. The lower chuck 141 corresponds to the holding portion, and the upper chuck 140 corresponds to the opposite holding portion. In addition, as described later, the upper chuck 140 may correspond to the holding portion, and the lower chuck 141 may correspond to the opposite holding portion. The upper chuck 140 has an adsorption surface 140a for adsorbing the upper wafer W1 on the surface (lower surface) opposite to the lower chuck 141. On the other hand, the lower chuck 141 has an adsorption surface 141a for adsorbing the lower wafer W2 on the surface (upper surface) opposite to the upper chuck 140.

[0071] The upper chuck 140 has a chuck base 170. The chuck base 170 has the same diameter as the upper wafer W1 or a larger diameter than the upper wafer W1. The chuck base 170 is supported by a support member 180. The support member 180 is provided to at least cover the chuck base 170 when viewed from above, and is fixed relative to the chuck base 170 by, for example, screwing. The support member 180 is provided on a plurality of support columns 181 (see FIG. 1 ) on the top surface of the processing container 100. Figure 5 The upper chuck holding portion 150 is composed of a supporting member 180 and a plurality of supporting columns 181.

[0072] A through hole 176 is formed in the support member 180 and the chuck base 170, penetrating the support member 180 and the chuck base 170 in the vertical direction. The position of the through hole 176 corresponds to the center of the upper wafer W1 adsorbed and held by the upper chuck 140. The pressing pin 191 of the impactor 190 passes through the through hole 176.

[0073] The impactor 190 is disposed on the upper surface of the support member 180, and includes a pressing pin 191, an actuator unit 192, and a linear motion mechanism 193. The pressing pin 191 is a cylindrical member extending in the vertical direction, and is supported by the actuator unit 192.

[0074] The actuator part 192 generates a certain pressure in a certain direction (here, vertically downward) by using air supplied from an electro-pneumatic regulator, for example. The actuator part 192 can control the pressing load applied to the center of the upper wafer W1 by contacting the center of the upper wafer W1 by using the air supplied from the electro-pneumatic regulator. In addition, the top end of the pressing pin 191 can be freely raised and lowered in the vertical direction by using the air from the electro-pneumatic regulator to penetrate the through hole 176.

[0075] The actuator unit 192 is supported by the linear motion mechanism 193. The linear motion mechanism 193 moves the actuator unit 192 in the vertical direction using a driving unit including a motor, for example.

[0076] The impactor 190 is configured as described above, and the movement of the actuator unit 192 is controlled by the linear motion mechanism 193 , so that the pressing load of the pressing pin 191 on the upper wafer W1 is controlled by the actuator unit 192 .

[0077] The impactor 190 presses the upper wafer W1 sucked and held by the upper chuck 140 and the lower wafer W2 sucked and held by the lower chuck 141 together. Specifically, the impactor 190 deforms the upper wafer W1 sucked and held by the upper chuck 140 to press it together with the lower wafer W2.

[0078] A plurality of pins 171 that contact the non-bonding surface W1n of the upper wafer W1 are provided on the lower surface of the chuck base 170. The upper chuck 140 is composed of the chuck base 170, the plurality of pins 171, etc. The adsorption surface 140a of the upper chuck 140 for adsorbing and holding the upper wafer W1 is divided into a plurality of regions in the radial direction, and the adsorption pressure is generated and released in each divided region as a unit.

[0079] In addition, the lower chuck 141 is preferably constructed in the same manner as the upper chuck 140. The lower chuck 141 has a plurality of pins 204 that contact the non-bonding surface W2n of the lower wafer W2. The adsorption surface 141a of the lower chuck 141 for adsorbing and holding the lower wafer W2 is divided into a plurality of regions in the radial direction, and the adsorption pressure is generated and released in each divided region.

[0080] <Joining method>

[0081] Figure 8 1 is a flowchart showing a portion of the processing performed by the bonding system according to one embodiment. Figure 8 The various processes shown are executed under the control of the control device 70 .

[0082] First, a cassette CS1 containing a plurality of upper wafers W1, a cassette CS2 containing a plurality of lower wafers W2, and an empty cassette CS3 are placed on a predetermined loading plate 11 of the loading / unloading station 2. Then, the upper wafer W1 in the cassette CS1 is taken out by the conveying device 22 and conveyed to the conveying device 50 of the third processing module G3 of the processing station 3.

[0083] Next, the upper wafer W1 is transported to the surface modification device 30 of the first processing module G1 by using the transport device 61. In the surface modification device 30, oxygen gas as a processing gas is excited to be plasma-formed and ionized under a predetermined reduced pressure atmosphere. The oxygen ions are irradiated to the bonding surface W1j of the upper wafer W1, so that the bonding surface W1j is subjected to plasma treatment. As a result, the bonding surface W1j of the upper wafer W1 is modified (step S101).

[0084] Next, the upper wafer W1 is transported to the surface hydrophilization device 40 of the second processing module G2 by using the transport device 61. In the surface hydrophilization device 40, pure water is supplied to the upper wafer W1 while the upper wafer W1 held on the rotating chuck is rotated. Then, the supplied pure water diffuses on the bonding surface W1j of the upper wafer W1, and the hydroxyl group (silanol group) adheres to the bonding surface W1j of the upper wafer W1 modified in the surface modification device 30 to hydrophilize the bonding surface W1j (step S102). In addition, the bonding surface W1j of the upper wafer W1 is cleaned by using the pure water used for the hydrophilization of the bonding surface W1j.

[0085] Next, the upper wafer W1 is transported to the bonding device 41 of the second processing module G2 by the transport device 61. The upper wafer W1 transported to the bonding device 41 is transported to the position adjustment mechanism 120 by the wafer transport mechanism 111 via the conveyor 110. Then, the horizontal orientation of the upper wafer W1 is adjusted by the position adjustment mechanism 120 (step S103).

[0086] After that, the upper wafer W1 is transferred from the position adjustment mechanism 120 to the holding arm 131 of the reversing mechanism 130. Next, in the conveying area T1, the holding arm 131 is reversed to reverse the front and back surfaces of the upper wafer W1 (step S104). That is, the bonding surface W1j of the upper wafer W1 faces downward.

[0087] Thereafter, the holding arm 131 of the reversing mechanism 130 is rotated and moved below the upper chuck 140. Then, the upper wafer W1 is transferred from the reversing mechanism 130 to the upper chuck 140. The non-bonding surface W1n of the upper wafer W1 is held by suction on the upper chuck 140 with the notch facing a predetermined direction (step S105).

[0088] While the upper wafer W1 is being processed in the above-mentioned steps S101 to S105 , the lower wafer W2 is processed. First, the lower wafer W2 in the cassette CS2 is taken out by the transfer device 22 and is transferred to the conveyor device 50 of the processing station 3 .

[0089] Next, the lower wafer W2 is transported to the surface modification device 30 by the transport device 61, and the bonding surface W2j of the lower wafer W2 is modified (step S106). The modification of the bonding surface W2j of the lower wafer W2 in step S106 is the same as the above-mentioned step S101.

[0090] Afterwards, the lower wafer W2 is transported to the surface hydrophilization device 40 by the transport device 61, and the bonding surface W2j of the lower wafer W2 is hydrophilized (step S107). And, the bonding surface W2j is cleaned by the pure water used for the hydrophilization of the bonding surface W2j. In addition, the hydrophilization of the bonding surface W2j of the lower wafer W2 in step S107 is the same as the hydrophilization of the bonding surface W1j of the upper wafer W1 in the above-mentioned step S102.

[0091] Then, the lower wafer W2 is transported to the bonding device 41 by the transport device 61. The lower wafer W2 transported to the bonding device 41 is transported to the position adjustment mechanism 120 by the wafer transport mechanism 111 via the conveyor 110. Then, the horizontal orientation of the lower wafer W2 is adjusted by the position adjustment mechanism 120 (step S108).

[0092] Afterwards, the lower wafer W2 is transported to the lower chuck 141 by the wafer transport mechanism 111 and is held by suction on the lower chuck 141 (step S109). The non-bonding surface W2n of the lower wafer W2 is held by suction on the lower chuck 141 with the notch facing a predetermined direction, i.e., the same direction as the notch of the upper wafer W1.

[0093] Next, the position adjustment in the horizontal direction between the upper wafer W1 held by the upper chuck 140 and the lower wafer W2 held by the lower chuck 141 is performed (step S110). Specifically, the horizontal position (for example, including the X-axis direction position, the Y-axis direction position, and the θ direction position) is adjusted in such a manner that the plurality of alignment marks formed on the bonding surface W1j of the upper wafer W1 and the plurality of alignment marks formed on the bonding surface W2j of the lower wafer W2 overlap when viewed from the vertical direction.

[0094] Next, the vertical position between the upper wafer W1 held on the upper chuck 140 and the lower wafer W2 held on the lower chuck 141 is adjusted (step S111). Specifically, the first lower chuck moving unit 160 moves the lower chuck 141 vertically upward, so that the lower wafer W2 is close to the upper wafer W1. Figure 6 As shown, the interval S between the bonding surface W2 j of the lower wafer W2 and the bonding surface W1 j of the upper wafer W1 is adjusted to a predetermined distance, for example, 50 μm to 200 μm.

[0095] Next, after the upper chuck 140 releases the suction and holding of the center portion of the upper wafer W1 (step S112), Figure 7 As shown in (a), the pressing pin 191 of the impactor 190 is lowered to press down the center of the upper wafer W1 (step S113). The center of the upper wafer W1 contacts the center of the lower wafer W2. When the center of the upper wafer W1 and the center of the lower wafer W2 are pressed with a predetermined force, the pressed center of the upper wafer W1 and the center of the lower wafer W2 begin to be joined. After that, a joining wave is generated that gradually joins the upper wafer W1 and the lower wafer W2 from the center toward the periphery.

[0096] Here, the bonding surface W1j of the upper wafer W1 and the bonding surface W2j of the lower wafer W2 are modified in steps S101 and S106, respectively, so that first, van der Waals force (intermolecular force) is generated between the bonding surfaces W1j and W2j, and the bonding surfaces W1j and W2j are bonded to each other. Moreover, the bonding surface W1j of the upper wafer W1 and the bonding surface W2j of the lower wafer W2 are hydrophilized in steps S102 and S107, respectively, so that the hydrophilic groups between the bonding surfaces W1j and W2j form hydrogen bonds, and the bonding surfaces W1j and W2j are firmly bonded to each other.

[0097] Afterwards, while the center of the upper wafer W1 and the center of the lower wafer W2 are pressed by the pressing pins 191, the upper chuck 140 is released from adsorption and holding of the entire upper wafer W1 (step S114). Figure 7 As shown in (b), the bonding surface W1j of the upper wafer W1 and the bonding surface W2j of the lower wafer W2 are brought into contact with each other to bond the upper wafer W1 and the lower wafer W2. Then, the pressing pins 191 are raised to the upper chuck 140 to release the suction and holding of the lower wafer W2 by the lower chuck 141.

[0098] Thereafter, the overlapped wafer T is transported to the transfer device 51 of the third process module G3 by the transport device 61, and then transported to the cassette CS3 by the transport device 22 of the carry-in / carry-out station 2. In this way, a series of bonding processes are completed.

[0099] <Control of the strain of the lower wafer by the lower chuck>

[0100] Fig. 9 1 is a diagram showing a lower chuck, a vacuum pump, and a vacuum regulator according to one embodiment. Fig. 9 , the horizontal angle of the suction surface 141a of the lower chuck 141 and the lower wafer W2 when sucked on the suction surface 141a are shown (refer to Figure 6 The Miller index used as a directional index or a surface index is negative, and is usually indicated by a “-” (bar) above a number, but in this specification, it is indicated by a minus sign before the number. Fig. 9 In order to facilitate viewing of the drawings, the pin 204 is omitted.

[0101] like Figure 6 As shown in the figures, the lower chuck 141 has a circular first region 210 and an annular second region 220 disposed radially outward of the first region 210 on the adsorption surface 141a for adsorbing the lower wafer W2, as a plurality of regions in which the adsorption pressure (e.g., vacuum pressure) for adsorbing the lower wafer W2 is individually controlled. For example, the lower chuck 141 has an inner peripheral rib 201 that divides the first region 210 and the second region 220 and an outer peripheral rib 202 disposed radially outward of the second region 220 on the adsorption surface 141a.

[0102] The inner rib 201 and the outer rib 202 are concentrically protruded on the upper surface of the chuck base 203. A plurality of pins 204 are protruded and dispersedly provided on the upper surface of the chuck base 203 at the same height as the inner rib 201 and the outer rib 202. The inner rib 201, the outer rib 202 and the plurality of pins 204 have the same height, and keep the lower wafer W2 horizontal.

[0103] In addition, the lower chuck 141 has a plurality of annular regions 221 and 222 formed by dividing the second region 220 in the radial direction, as a plurality of regions where the adsorption pressure for adsorbing the lower wafer W2 is individually controlled. For example, the lower chuck 141 has an annular middle rib 205 on the adsorption surface 141a that divides the radially outer annular region 221 and the radially inner annular region 222. The middle rib 205 is arranged concentrically with the inner peripheral rib 201 and the outer peripheral rib 202. The middle rib 205 has the same height as the inner peripheral rib 201 and the outer peripheral rib 202, and together with the inner peripheral rib 201 and the outer peripheral rib 202, it keeps the lower wafer W2 horizontal.

[0104] In addition, if Fig. 9 As shown, the lower chuck 141 has a plurality of arc regions A1 and A2 formed by dividing the outer peripheral end of the second region 220 (that is, the radially outermost annular region 221) in the circumferential direction, as a plurality of regions where the adsorption pressure for adsorbing the lower wafer W2 is individually controlled. The two arc regions A1 and A2 are alternately and repeatedly arranged in the circumferential direction, for example, four are arranged respectively. For example, the lower chuck 141 has a dividing rib 206 on the adsorption surface 141a that divides the two arc regions A1 and A2. There are a plurality of (e.g., 8) dividing ribs 206 arranged radially. The dividing rib 206 has the same height as the inner rib 201 and the outer rib 202, and together with the inner rib 201 and the outer rib 202, it keeps the lower wafer W2 horizontal. A plurality of pins 204 are dispersedly arranged in each arc region A1 and A2.

[0105] Moreover, the lower chuck 141 has a plurality of arc regions B1 and B2 formed by dividing the radially inner annular region 222 in the circumferential direction, as a plurality of regions where the adsorption pressure for adsorbing the lower wafer W2 is individually controlled. The two arc regions B1 and B2 are alternately and repeatedly arranged in the circumferential direction, for example, four of each are arranged. For example, the lower chuck 141 has a dividing rib 207 on the adsorption surface 141a that divides the two arc regions B1 and B2. There are a plurality of (e.g., 8) dividing ribs 207 radially arranged. The dividing rib 207 has the same height as the inner rib 201 and the outer rib 202, and together with the inner rib 201 and the outer rib 202, it keeps the lower wafer W2 horizontal. A plurality of pins 204 are dispersedly arranged in each arc region B1 and B2.

[0106] The bonding device 41 includes, for example, a plurality of vacuum pumps 231 to 234, 241 as a plurality of adsorption pressure generating units that individually generate adsorption pressure in each of a plurality of regions constituting the adsorption surface 141a of the lower chuck 141. In addition, the bonding device 41 includes, for example, a plurality of vacuum regulators 251 to 254, 261 as a plurality of adsorption pressure adjusting units that individually adjust the adsorption pressure generated by each of the plurality of vacuum pumps 231 to 234, 241.

[0107] A vacuum pump 231 is connected to the four arc areas A1 (at Fig. 9 Only the piping connected to one arc region A1 is shown in the figure. Similarly, one vacuum pump 232 is connected to four arc regions A2 (at Fig. 9 Only the piping connected to one arc region A2 is shown in the figure.) In addition, a vacuum pump 233 is connected to four arc regions B1 via piping with a vacuum regulator 253 provided in the middle (at Fig. 9 Only the piping connected to one arc region B1 is shown in the figure. Similarly, one vacuum pump 234 is connected to four arc regions B2 (at Fig. 9 Only the piping connected to one arc region B2 is shown.) In addition, one vacuum pump 241 is connected to the first region 210 via piping with a vacuum regulator 261 provided in the middle.

[0108] When the control device 70 activates a vacuum pump 231, the vacuum pump 231 generates vacuum pressure in the four arc regions A1, maintains the vacuum pressure at a set value pre-set in the vacuum regulator 251, and generates an adsorption pressure corresponding to the set value in the four arc regions A1. The set value of the vacuum regulator 251 can be changed by the control device 70, and is set in a range of, for example, -80 kPa to -5 kPa based on atmospheric pressure. On the other hand, when the control device 70 stops the operation of the vacuum pump 231, the four arc regions A1 return to atmospheric pressure, and the generation of adsorption pressure in the four arc regions A1 is released. The generation and release of adsorption pressure in the other arc regions A2, arc region B1, arc region B2 and the first region 210 are the same as the generation and release of adsorption pressure in the arc region A1, so the description is omitted.

[0109] The bonding apparatus 41 of this embodiment includes a control device 70 that controls a plurality of vacuum pumps 231 to 234 and 241 and a plurality of vacuum regulators 251 to 254 and 261. The control device 70 Figure 1 In the example above, the control device 70 is provided outside the bonding device 41, but may be provided as a part of the bonding device 41. The control device 70 corresponds to a control unit.

[0110] The control device 70 of this embodiment simultaneously generates different suction pressures in at least a portion of the first region 210 (e.g., the entire first region 210) and at least a portion of the second region 220 (e.g., the arc region A2 and the arc region B1). Thus, the radial distribution of the suction pressure generated on the suction surface 141a can be controlled, and the strain generated on the lower wafer W2 suctioned to the suction surface 141a can be controlled.

[0111] The adsorption pressure generated in the first area 210 and the adsorption pressure generated in the arc area A2 and the arc area B1 may be either larger or smaller. In addition, the adsorption pressure generated in the first area 210 and the adsorption pressure generated in the arc area A1 and the arc area B2 are the same in this embodiment, but either one may be larger or smaller. In addition, it is also possible that no adsorption pressure is generated when the adsorption surface 141a adsorbs the lower wafer W2 in the arc area A1 and the arc area B2. That is, in this embodiment, when the lower wafer W2 is adsorbed, adsorption pressure is generated simultaneously on the entire adsorption surface 141a, but adsorption pressure may be generated only on a part of the adsorption surface 141a.

[0112] According to the present embodiment, the lower wafer W2 and the upper wafer W1 can be joined while the strain generated in the lower wafer W2 is controlled, and the fitting strain (Distortion) between the lower wafer W2 and the upper wafer W1 can be reduced. The fitting strain is represented by, for example, the size of the positional offset remaining when the upper wafer W1 and the lower wafer W2 are relatively moved parallel, rotated, and similarly stretched in a manner that minimizes the positional offset when viewed from above of the multiple alignment marks formed on the upper wafer W1 and the multiple alignment marks formed on the lower wafer W2. It is preferred to repeatedly change the setting of the adsorption pressure, perform the joining according to the changed setting, and measure the fitting strain after joining until the fitting strain is within the allowable range. The change in the distribution of the adsorption pressure is preferably performed based on a plurality of data accumulated previously. The data can be any data that represents the relationship between the setting (or actual condition) of the adsorption pressure and the fitting strain, and can be used by reading the information stored in the information storage medium.

[0113] The inventors have repeatedly conducted in-depth research and found that one of the reasons for the bonding strain is the anisotropy of the physical properties such as the Young's modulus of the lower wafer W2. The physical properties such as the Young's modulus of the lower wafer W2 change periodically in the circumferential direction. The bonding strain caused by this change is more significant from the radial inside of the lower wafer W2 to the radial outside. This is because, from the radial inside of the lower wafer W2 to the radial outside, for example, the circumferential distance between the [0-11] direction and the

[001] direction is greater.

[0114] Therefore, the control device 70 of the present embodiment simultaneously generates different suction pressures in a part of the second region 220 (e.g., the arc region A1 and the arc region B2) arranged radially outside the first region 210 and another part of the second region 220 (e.g., the arc region A2 and the arc region B1). Thus, the strain generated in the lower wafer W2 in the second region 220 deviated from the center of the lower wafer W2 can be controlled.

[0115] The adsorption pressure generated in the arc region A1 and the arc region B2 and the adsorption pressure generated in the arc region A2 and the arc region B1 may be either larger or smaller. In addition, the adsorption pressure generated in the arc region A1 and the adsorption pressure generated in the arc region B2 are the same in this embodiment, but either one may be larger or smaller. Similarly, the adsorption pressure generated in the arc region A2 and the adsorption pressure generated in the arc region B1 are the same in this embodiment, but either one may be larger or smaller.

[0116] The control device 70 of this embodiment simultaneously generates different suction pressures in at least a portion of the radially outer annular region 221 (e.g., arc region A1) and at least a portion of the radially inner annular region 222 (e.g., arc region B1) among the plurality of annular regions 221 and 222 formed by radially dividing the second region 220. Thus, the strain generated in the lower wafer W2 can be controlled based on the radial distance from the center of the lower wafer W2.

[0117] The control device 70 of this embodiment controls the adsorption pressure of each adjacent arc region (here, the arc region A1 and the arc region A2 included in the radially outermost annular region 221) among the plurality of arc regions formed by dividing the outer peripheral end of the second region 220 in the circumferential direction, and makes the adjacent arc regions generate different adsorption pressures at the same time. This is because the physical properties such as the Young's modulus of the lower wafer W2 change periodically in the circumferential direction, and the bonding strain generated by this change is most significant at the outer peripheral end of the lower wafer W2.

[0118] Similarly, the control device 70 may separately control the adsorption pressure of each of the adjacent arc regions (e.g., arc region B1 and arc region B2) in the plurality of arc regions formed by dividing the remaining annular region (here, the radially inner annular region 222) in the circumferential direction, and make the adjacent arc regions simultaneously generate different adsorption pressures. The strain of the lower wafer W2 can be controlled not only in the radially outer annular region 221 but also in the radially inner annular region 222. This is particularly effective when the diameter of the lower wafer W2 is large.

[0119] In addition, the Young's modulus, Poisson's ratio, and shear modulus of a single crystal silicon wafer vary in a 90° period. The directions of the 90° period (0° direction, 90° direction, 180° direction, and 270° direction) based on the [0-11] direction (0° direction) are also collectively referred to as "0° reference 90° period directions". In addition, the directions of the 90° period (45° direction, 135° direction, 225° direction, and 315° direction) based on the [0-10] direction (45° direction) are also collectively referred to as "45° reference 90° period directions". The Young's modulus of a single crystal silicon wafer is highest in the 0° reference 90° period direction and lowest in the 45° reference 90° period direction. In addition, the Poisson's ratio and shear modulus are highest in the 45° reference 90° period direction and lowest in the 0° reference 90° period direction.

[0120] Therefore, when the lower wafer W2 is a single crystal silicon wafer, it is preferred to Fig. 9 As shown, the arc region A1 is arranged in the 90° period direction based on 0°, and the arc region A2 is arranged in the 90° period direction based on 45°. That is, the two arc regions A1 and A2 whose adsorption pressures are independently controlled are alternately and repeatedly arranged in the circumferential direction, for example, four of each are arranged.

[0121] Similarly, when the lower wafer W2 is a single crystal silicon wafer, it is preferred that Fig. 9 As shown, the arc region B1 is arranged in the 90° period direction based on 0°, and the arc region B2 is arranged in the 90° period direction based on 45°. That is, the two arc regions B1 and B2 whose adsorption pressures are independently controlled are alternately and repeatedly arranged in the circumferential direction, for example, four of each are arranged.

[0122] In addition, the control device 70 of the present embodiment causes multiple arc regions with the same angle (e.g., arc region A1 and arc region B1, or arc region A2 and arc region B2) to generate different adsorption pressures at the same time, but the technology disclosed in the present invention is not limited to this. For example, the control device 70 may cause multiple arc regions with different angles (e.g., arc region A1 and arc region B2, or arc region A2 and arc region B1) to generate different adsorption pressures at the same time.

[0123] <Transformation and improvement>

[0124] The above describes the embodiments of the substrate processing device and the substrate processing method of the present disclosure, but the present disclosure is not limited to the above embodiments. Various changes, modifications, substitutions, additions, deletions and combinations can be made within the scope of the claims. These also belong to the technical scope of the present disclosure.

[0125] The control device 70 of the above embodiment causes the adjacent arc regions B1 and B2 to generate different adsorption pressures at the same time, but the technology disclosed in the present invention is not limited to this. The control device 70 may also cause the adjacent arc regions B1 and B2 to generate the same adsorption pressure. In this case, the radially inner annular region 222 does not need to be divided into a plurality of arc regions B1 and B2 in the circumferential direction. Therefore, the control device 70 may be configured as follows: Fig.10 The diagram shows that it is composed of only one annular region B. One annular region B is connected to one vacuum pump 233 via a pipe with a vacuum regulator 253 provided in the middle. The generation and release of the adsorption pressure of the annular region B are the same as those of the arc region A1, so the description is omitted.

[0126] The radially outer annular region 221 and the radially inner annular region 222 of the above embodiment are divided into the same number in the circumferential direction, but they may also be divided into different numbers in the circumferential direction. Fig.11 As shown, the number of divisions of the radially outer annular region 221 is greater than the number of divisions of the radially inner annular region 222. This is because the bonding strain is more likely to be generated from the radial inner side of the lower wafer W2 toward the radial outer side.

[0127] Fig.11 The lower chuck 141 shown has three arc regions A1, A2, and A3 formed by dividing the radially outer annular region 221 in the circumferential direction as a plurality of regions where the adsorption pressure is individually controlled. The arc region A3 is arranged between the arc region A1 arranged in the 90° period direction of the 0° reference and the arc region A2 arranged in the 90° period direction of the 45° reference. Thus, the adsorption pressure distribution of the lower wafer W2 in the circumferential direction can be controlled with higher precision.

[0128] like Fig.11 As shown, the dividing line (e.g., the dividing rib 206) that divides the radially outer annular region 221 into a plurality of arc regions A1, A2, and A3 in the circumferential direction and the dividing line (e.g., the dividing rib 207) that divides the radially inner annular region 222 into a plurality of arc regions B1 and B2 in the circumferential direction may also be staggered in the circumferential direction. The portion where the adsorption pressure discontinuously changes in the radially outer annular region 221 and the portion where the adsorption pressure discontinuously changes in the radially inner annular region 222 can be staggered in the circumferential direction.

[0129] Fig.11 The eight arc areas A3 shown are connected to a vacuum pump 235 by means of a pipe having a vacuum regulator 255 disposed in the middle (at Fig.11 Only the pipe connected to one arc region A3 is shown.) Generation and release of adsorption pressure in the arc region A3 are similar to generation and release of adsorption pressure in the arc region A1, and thus description thereof is omitted.

[0130] Figures 9 to 11 The lower chuck 141 shown has two annular regions 221 and 222 formed by dividing the second region 220 in the radial direction, as multiple regions whose adsorption pressure is controlled separately, but the number of annular regions is not limited to two. The number of annular regions may be one (that is, the second region 220 may not be divided in the radial direction), or the number of annular regions may be three or more.

[0131] Fig.12 It is a diagram showing a lower chuck, a vacuum pump, and a vacuum regulator according to a third modified example. Fig.12 The lower chuck 141 of the illustrated modification example includes four annular regions 221 , 222 , 223 , and 224 formed by dividing the second region 220 in the radial direction, as a plurality of regions whose suction pressures are individually controlled.

[0132] The first annular region 221 from the radial outer side is composed of two circular arc regions A1 and A2 arranged alternately and repeatedly in the circumferential direction. The adsorption pressure of the two adjacent circular arc regions A1 and A2 is controlled separately. Similarly, the second annular region 222 from the radial outer side is composed of two circular arc regions B1 and B2 arranged alternately and repeatedly in the circumferential direction. The adsorption pressure of the two adjacent circular arc regions B1 and B2 is controlled separately.

[0133] In addition, the third annular region 223 from the radial outer side is composed of two circular arc regions C1 and C2 that are alternately arranged in the circumferential direction. The adsorption pressure of the two adjacent circular arc regions C1 and C2 is controlled separately. A vacuum pump 235 is connected to the four circular arc regions C1 (at Fig.12 Only the piping connected to one arc region C1 is shown in the figure.) A vacuum pump 236 is connected to four arc regions C2 via piping with a vacuum regulator 256 provided in the middle (at Fig.12 Only the piping connected to one arc region C2 is shown.) Generation and release of adsorption pressure in the arc regions C1 and C2 are similar to generation and release of adsorption pressure in the arc region A1, and thus description thereof is omitted.

[0134] Furthermore, the fourth annular region 224 from the radially outer side is composed of two circular arc regions D1 and D2 that are alternately arranged in the circumferential direction. The adsorption pressure of the two adjacent circular arc regions D1 and D2 is controlled separately. A vacuum pump 237 is connected to the four circular arc regions D1 by means of a pipe having a vacuum regulator 257 disposed in the middle (at Fig.12 Only the piping connected to one arc region D1 is shown in the figure.) A vacuum pump 238 is connected to four arc regions D2 via piping with a vacuum regulator 258 provided in the middle (at Fig.12Only the piping connected to one arc region D2 is shown.) Generation and release of adsorption pressure in the arc regions D1 and D2 are similar to generation and release of adsorption pressure in the arc region A1, and thus description thereof is omitted.

[0135] also, Fig.12 The lower chuck 141 of the modified example shown has two annular regions 211 and 212 and a circular region 213 formed by radially dividing the first region 210, as multiple regions whose adsorption pressures are individually controlled. The radially outer annular region 211 and the radially inner annular region 212 are divided by an annular rib. In addition, the radially inner annular region 212 and the circular region 213 are divided by an annular rib. The annular rib disposed inside the first region 210 is connected to the inner region 213 of the first region 210. Fig. 9 The inner rib 201 and the outer rib 202 shown in the figure are formed in a concentric circle shape. The annular rib arranged inside the first area 210 has the same height as the pin 204, and together with the pin 204, the lower wafer W2 is kept horizontal. In addition, in this modified example, the two annular areas 211, 212 and the circular area 213 correspond to the divided areas.

[0136] The first annular region 211 counted from the radially outer side in the first region 210 is connected to a vacuum pump 241 via a pipe having a vacuum regulator 261 disposed in the middle. In addition, the second annular region 212 counted from the radially outer side in the first region 210 is connected to a vacuum pump 242 via a pipe having a vacuum regulator 262 disposed in the middle. Furthermore, the third circular region 213 counted from the radially outer side in the first region 210 is connected to a vacuum pump 243 via a pipe having a vacuum regulator 263 disposed in the middle. The generation and release of the adsorption pressure of the annular regions 211, 212 and the circular region 213 are the same as the generation and release of the adsorption pressure of the arc region A1, and therefore the description thereof is omitted.

[0137] The control device 70 of this modified example causes two adjacent divided areas (for example, the radially outer annular area 211 and the radially inner annular area 212, and at least one of the radially inner annular area 212 and the circular area 213) to simultaneously generate different adsorption pressures. Thus, the strain near the center of the lower wafer W2 pressed by the pressing pin 191 of the impactor 190 can be controlled.

[0138] In addition, the number of annular regions constituting the first region 210 is Fig.12 In the embodiment, the number of the first region 210 is two, but the number of the first region 210 may be one or more than three. In addition, the annular region (eg, the annular region 211) constituting the first region 210 may be divided into a plurality of regions in the circumferential direction similarly to the annular region (eg, the annular region 221) constituting the second region 220.

[0139] The lower chuck 141 of the above-mentioned embodiment and the above-mentioned modification example performs vacuum adsorption on the lower wafer W2, but electrostatic adsorption may also be performed. In this case, the adsorption pressure generating unit includes, for example, an internal electrode buried inside the lower chuck 141. On the other hand, the adsorption pressure adjusting unit includes, for example, a power adjusting unit for adjusting the power supplied to the internal electrode. The power adjusting unit is composed of, for example, a step-down DC / DC converter or a step-up DC / DC converter.

[0140] In the above-mentioned embodiment and the above-mentioned modification, the strain generated by the lower wafer W2 adsorbed on the lower chuck 141 is controlled, but the strain generated by the upper wafer W1 adsorbed on the upper chuck 140 can also be controlled. That is, the technology disclosed in the present invention can also be applied to the upper chuck 140, or the upper chuck 140 corresponds to the holding portion, and the lower chuck 141 corresponds to the opposite holding portion. In addition, the technology disclosed in the present invention can also be applied to both the upper chuck 140 and the lower chuck 141. Moreover, the technology disclosed in the present invention can also be applied to devices other than the bonding device 41, such as a cutting device. As long as it is a device with a holding portion for holding a substrate, the technology disclosed in the present invention can be applied.

[0141] This application claims priority based on Japanese Patent Application No. 2018-005987 filed with the Japan Patent Office on January 17, 2018, and the entire contents of Japanese Patent Application No. 2018-005987 are hereby incorporated by reference into this application.

[0142] Description of Reference Numerals

[0143] 41. Bonding device; 70. Control device; 140. Upper chuck (opposite holding portion); 141. Lower chuck (holding portion); 141a. Adsorption surface; 210. First region; 220. Second region; 221. Annular region on the radial outer side; 222. Annular region on the radial inner side; 231 to 234, 241. Vacuum pump (adsorption pressure generating portion); 251 to 254, 261. Vacuum regulator (adsorption pressure adjusting portion); W1. Upper wafer (substrate); W2. Lower wafer (substrate).

Claims

1. A bonding device comprising: A holding portion having a circular first region and an annular second region disposed radially outside the first region on a suction surface for suctioning the substrate, as a plurality of regions in which suction pressure for suctioning the substrate is individually controlled; A plurality of adsorption pressure generating units, wherein the plurality of adsorption pressure generating units generate adsorption pressure individually in each of the plurality of regions constituting the adsorption surface; a plurality of adsorption pressure adjusting units, wherein the plurality of adsorption pressure adjusting units individually adjust the adsorption pressure generated by each of the plurality of adsorption pressure generating units; an opposing holding portion, which is arranged opposite to the holding portion and holds a second substrate separated from the substrate to be joined to the substrate; as well as a control unit that controls the plurality of adsorption pressure generating units and the plurality of adsorption pressure adjusting units, The control unit generates different adsorption pressures in at least a portion of the first region and at least a portion of the second region based on previously accumulated data.

2. The joining device according to claim 1, wherein: The data is the relationship between the setting or actual condition of the adsorption pressure and the fitting strain.

3. The joining device according to claim 1, wherein: The holding portion includes a plurality of regions in the second region in which the adsorption pressure is individually controlled. The control unit generates different adsorption pressures in a part of the second region and in another part of the second region.

4. The joining device according to claim 3, wherein: The holding portion includes a plurality of annular regions formed by dividing the second region in a radial direction as a plurality of regions in which the adsorption pressure is independently controlled. The control unit generates different adsorption pressures in at least a portion of one annular region and at least a portion of another annular region.

5. The joining device according to claim 3 or 4, wherein: The holding portion includes a plurality of arc regions formed by dividing the outer peripheral end of the second region in the circumferential direction, as a plurality of regions in which the adsorption pressure is independently controlled. The control unit generates different adsorption pressures in two adjacent arc regions.

6. The bonding device according to any one of claims 1 to 4, wherein: The holding portion includes a plurality of divided regions formed by dividing the first region in a radial direction as a plurality of regions in which the adsorption pressure is independently controlled. The control unit generates different adsorption pressures in two adjacent divided regions.

7. The bonding device according to any one of claims 1 to 4, wherein: A facing holding portion is provided which is arranged opposite to the holding portion. The pair of facing holding portions holds another substrate to be joined to the substrate.

8. A bonding method, comprising: causing a suction surface for adsorbing a substrate to generate a suction pressure for adsorbing the substrate, so that the substrate adsorbed on the suction surface is bonded face to face with a second substrate separated from the substrate, wherein: The adsorption pressures generated in the circular first region constituting the adsorption surface and the annular second region arranged radially outside the first region are controlled separately, and The adsorption pressure is different between at least a portion of the first region and at least a portion of the second region based on previously accumulated data.

9. The bonding method according to claim 8, wherein: The data is the relationship between the setting or actual condition of the adsorption pressure and the fitting strain.

10. The bonding method according to claim 8, wherein: The adsorption pressures of a part of the second region and other parts of the second region are controlled separately, respectively, so that different adsorption pressures are generated in the part of the second region and other parts of the second region.

11. The bonding method according to claim 10, wherein: The adsorption pressures generated in the plurality of annular regions formed by dividing the second region in the radial direction are controlled individually, and Different adsorption pressures are generated in at least a portion of one of the annular regions and at least a portion of another of the annular regions.

12. The bonding method according to claim 10 or 11, wherein: The adsorption pressures of two adjacent arc regions among a plurality of arc regions formed by dividing the outer peripheral end of the second region in the circumferential direction are controlled individually, and different adsorption pressures are generated in the two adjacent arc regions.

13. The bonding method according to any one of claims 8 to 10, wherein: The adsorption pressures generated in each of a plurality of divided regions formed by dividing the first region in the radial direction are controlled individually, and different adsorption pressures are generated in two adjacent divided regions.

14. The bonding method according to any one of claims 8 to 10, wherein: The substrate adsorbed to the adsorption surface by the adsorption pressure and another substrate are bonded face to face.