Wax smoke treatment system and process in high-temperature alloy casting process

By pre-baking the wax mold shell and combining spray, electrostatic and activated carbon adsorption technology, the wax smoke treatment efficiency and mold shell strength during the high-temperature alloy casting process are improved, and the traditional wax smoke treatment efficiency is low and the mold shell is cracked. problem and extends the life of the equipment.

CN118750994APending Publication Date: 2024-10-11SUZHOU GAOJING NEW MATERIAL TECH CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202410950102.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-16
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

In the high-temperature alloy casting process, the traditional wax smoke treatment efficiency is low and the mold shell is easy to expand and crack, resulting in inclusion defects in the casting and oxidation of the equipment, affecting the service life.

Method used

The moisture in the wax mold shell is evaporated through pre-baking treatment, and the temperature is gradually raised to fully burn the residual wax material and improve the strength of the mold shell. Spraying, electrostatic adsorption and activated carbon adsorption are used to treat the wax smoke, and the temperature of the wax smoke is lowered to improve the treatment efficiency.

Benefits of technology

Significantly improves the wax smoke treatment efficiency to 95%, reduces the problem of mold shell expansion and cracking, extends the service life of the equipment, and reduces the risk of air oxidation during the wax smoke treatment process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118750994A_ABST
    Figure CN118750994A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of casting of castings, in particular to a wax smoke treatment system and process in the high-temperature alloy casting process. The process comprises the following steps: 1) pre-roasting treatment: raising the temperature of a dewaxed wax mold shell to a first set temperature; raising the temperature to a first set temperature, raising the temperature to a second set temperature, and carrying out first heat preservation; after the first heat preservation is completed, the temperature is increased to a third set temperature, and second heat preservation is conducted; after the second heat preservation is completed, the temperature is increased to a fourth set temperature; and (2) wax smoke treatment, wherein wax smoke generated in the dewaxing treatment process and wax smoke generated in the pre-roasting treatment process of the dewaxed wax material mold shell are sequentially subjected to spraying, electrostatic adsorption and activated carbon adsorption. According to the method, moisture in the wax material mold shell is evaporated firstly, then the wax material left after dewaxing is fully combusted, then the temperature is increased to improve the strength of the mold shell, meanwhile, residues in a complex channel are combusted, and finally the temperature is increased again to enable the strength of the mold shell to reach the standard, so that the strength of the mold shell can be effectively improved, and the expansion cracking problem of the mold shell is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of casting, and in particular to a wax smoke treatment system and process in a high-temperature alloy casting process. Background Art

[0002] Complex castings in the aviation field are often made by lost wax casting. Lost wax casting usually refers to making the wax material into the desired pattern, coating the surface of the pattern with several layers of refractory material to make a mold shell, and then melting the pattern and discharging it from the mold shell, thereby obtaining a mold shell without a parting surface.

[0003] Specifically, in the high-temperature alloy investment casting process, nearly 50% of the defects are caused in the shell manufacturing process. Poor treatment of inclusions in the shell will cause product defects in the casting. The filling wax used in the casting process is one of the causes of shell inclusions. Therefore, the cleaner the residual filling wax in the shell cavity is, the fewer inclusions there are, and the fewer inclusion defects in the casting will be.

[0004] During the heating process of the casting process, waxy materials will produce a certain amount of wax smoke with a pungent odor, especially during the dewaxing and pre-baking of the mold shell. Dewaxing is the process of using high-temperature steam to melt the wax material in the mold shell, and then emitting steam to obtain an empty shell. However, a certain amount of wax material will remain, and the mold shell needs to be heated through the pre-baking process to use heat energy to burn out the remaining wax and dry the moisture in the mold shell.

[0005] However, the large amount of wax smoke produced during the burning of wax materials has a current efficiency of only 90% for conventional wax smoke treatment processes. At the same time, because there is moisture in the mold shell, rapid heating will cause the mold shell to change drastically and easily crack. Summary of the invention

[0006] The embodiments of the present invention provide a wax smoke treatment system and process for a high-temperature alloy casting process, so as to reasonably treat the wax smoke generated by filling wax material in the high-temperature alloy casting process, and at the same time improve the technical problem of the expansion and cracking of the existing wax material mold shell.

[0007] In a first aspect, an embodiment of the present invention provides a wax fume treatment process for a high temperature alloy casting process, comprising the steps of: 1) Pre-calcination Heating the dewaxed wax mold shell to a first set temperature to evaporate the water in the wax mold shell; After the temperature is raised to the first set temperature, the temperature is raised to the second set temperature and a first heat preservation is performed to fully burn the wax material remaining after dewaxing; After the first heat preservation is completed, the temperature is raised to the third set temperature and the second heat preservation is performed to improve the strength of the mold shell and burn the residue at the same time; After the second heat preservation is completed, the temperature is raised to the fourth set temperature to ensure that the mold shell strength meets the standard; 2) Wax smoke treatment The wax smoke generated during the dewaxing process and during the pre-baking process of the wax material mold shell after dewaxing is sprayed, electrostatically adsorbed and adsorbed with activated carbon in sequence.

[0008] In an embodiment of the present invention, the moisture in the wax mold is first evaporated, and then the residual wax after dewaxing is fully burned. Then the temperature is increased to improve the strength of the mold, and the residue in the complex channel is burned. Finally, the temperature is increased again to make the mold strength meet the standard. The strength of the mold can be effectively improved and the problem of cracking of the mold can be improved.

[0009] In an embodiment of the present invention, the processing efficiency of wax smoke can be improved by sequentially cooling, electrostatically adsorbing and activated carbon adsorbing the high-temperature wax smoke.

[0010] In one embodiment, the first set temperature is 100-120° C., and the time for heating to the first set temperature is 25-35 minutes; and / or The time for heating to the second set temperature is 65-75 minutes, the second set temperature is 180-220° C., and the first heat preservation time is 18-22 minutes; and / or The third set temperature is 350-450° C., and the second insulation time is 25-35 minutes; and / or The fourth set temperature is 850-950°C.

[0011] In the embodiments of the present invention, the effect of each stage can be effectively controlled by controlling the temperature and time of each stage.

[0012] In one embodiment, the method further comprises: After the wax mold shell is heated to a first set temperature, air is filled into the wax mold shell so that the wax mold shell is in contact with the air; After the second heat preservation is completed, the air filling is stopped.

[0013] In an embodiment of the present invention, by injecting air after the first set temperature and before the second insulation is completed, the wax remaining after dewaxing can be fully burned, while reducing the oxidation of related equipment by air after the second insulation is completed, thereby increasing the service life of the equipment.

[0014] In a second aspect, an embodiment of the present invention provides a wax fume treatment system for a high-temperature alloy casting process, comprising: The dewaxing and roasting device includes a pre-baking furnace and a dewaxing kettle, which is used to first dewax the wax material mold shell and then perform a pre-baking treatment; The wax smoke treatment device comprises a spray tower, an electrostatic precipitator, an activated carbon adsorption tower and an induced draft fan which are connected in sequence. The spray tower is connected to the waste gas discharge ports of the pre-calcining furnace and the dewaxing kettle.

[0015] In the embodiment of the present invention, the processing efficiency of the wax smoke can be improved by successively cooling, electrostatically adsorbing and activated carbon adsorbing the high-temperature wax smoke, and draining the wax smoke through an induced draft fan.

[0016] In one embodiment, the spray tower includes a primary spray tower and a secondary spray tower, the inlet of the spray tower is arranged at the bottom, the outlet of the spray tower is arranged at the top, and the primary spray tower and the secondary spray tower are provided with a water storage area, an atomization layer, a spray layer and a demisting layer in sequence from bottom to top.

[0017] In the embodiment of the present invention, by adopting a vertically designed spray tower, the wax material in the high-temperature and viscous wax smoke is not easy to adhere to the equipment, so it is easy to clean and replace.

[0018] In one embodiment, the atomization layer and the spraying layer are respectively arranged in two layers between the water storage area and the demisting layer.

[0019] In one embodiment, a blower is connected to the pre-baking furnace.

[0020] In an embodiment of the present invention, a blower is used to supply air to the pre-calcining furnace. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative work.

[0022] Figure 1 is a structural schematic diagram of a wax smoke processing system provided by an embodiment of the present invention; Figure 2 It is a schematic diagram of the structure of a primary spray tower and a secondary spray tower provided in an embodiment of the present invention.

[0023] Figure numerals: pre-calcining furnace-1; dewaxing kettle-2; primary spray tower-3; secondary spray tower-4; electrostatic precipitator-5; activated carbon adsorption tower-6; induced draft fan-7; water storage area-8; atomization layer-9; spray layer-10; demisting layer-11. DETAILED DESCRIPTION

[0024] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments in the present invention, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present invention. In addition, it should be understood that the specific implementation methods described herein are only used to illustrate and explain the present invention, and are not used to limit the present invention. In the present invention, unless otherwise specified, the directional words used, such as "upper" and "lower", generally refer to the upper and lower parts of the device in actual use or working state, specifically the drawing direction in the drawings; while "inside" and "outside" refer to the outline of the device. Example 1

[0025] A wax fume treatment process for a high-temperature alloy casting process comprises the following steps: Dewaxing treatment: the wax mold shell is loaded into the dewaxing kettle 2 for dewaxing treatment, wherein the shell making material is selected from silica sol-moly sand, and the steam pressure set in the dewaxing kettle 2 is 0.8-0.9MPa; Pre-baking: put the wax shell after dewaxing treatment into the pre-baking furnace 1, heat it to 100℃ at room temperature, this process takes 30min, then turn on the blower for blowing, then heat it to 200℃ and keep it for 20min, this process takes 90min, then heat it to 400℃ and keep it for 30min, then turn off the wax smoke treatment device and the blower, and then heat it to 850℃; Wax smoke treatment: The wax smoke generated during the dewaxing and pre-baking processes is sprayed, electrostatically adsorbed and adsorbed on activated carbon in turn. Example 2

[0026] A wax fume treatment process for a high-temperature alloy casting process comprises the following steps: Dewaxing treatment: the wax mold shell is loaded into the dewaxing kettle 2 for dewaxing treatment, wherein the shell material is selected from silica sol-corundum powder, and the steam pressure set in the dewaxing kettle 2 is 0.8-0.9MPa; Pre-baking: put the wax shell after dewaxing into the pre-baking furnace 1, heat it to 110℃ at room temperature, this process takes 35min, then turn on the blower to blow air, then heat it to 180℃ and keep it for 22min, this process takes 90min, then heat it to 350℃ and keep it for 35min, then turn off the wax smoke treatment device and the blower, and then heat it to 900℃; Wax smoke treatment: The wax smoke generated during the dewaxing and pre-baking processes is sprayed, electrostatically adsorbed and adsorbed on activated carbon in turn. Example 3

[0027] A wax fume treatment process for a high-temperature alloy casting process comprises the following steps: Dewaxing treatment: the wax mold shell is loaded into the dewaxing kettle 2 for dewaxing treatment, wherein the shell making material is selected from silica sol-corundum powder, and the steam pressure set in the dewaxing kettle 2 is 0.8-0.9MPa; Pre-baking: put the wax shell after dewaxing into the pre-baking furnace 1, heat it to 120℃ at room temperature, this process takes 25min, then turn on the blower to blow air, then heat it to 220℃ and keep it for 18min, this process takes 85min, then heat it to 450℃ and keep it for 25min, then turn off the wax smoke treatment device and the blower, then heat it to 950℃; Wax smoke treatment: The wax smoke generated during the dewaxing and pre-baking processes is sprayed, electrostatically adsorbed and adsorbed on activated carbon in turn.

[0028] The device used in the wax fume treatment method of the high-temperature alloy casting process in the embodiment of the present application is a wax fume treatment system, including a dewaxing device and a wax fume treatment device.

[0029] The dewaxing and roasting device comprises a pre-baking furnace 1 and a dewaxing kettle 2, which are used to first dewax the wax material mold shell and then pre-baking it. A blower is connected to the pre-baking furnace to fill air into the pre-baking furnace.

[0030] The wax smoke treatment device includes a spray tower, an electrostatic precipitator 5, an activated carbon adsorption tower 6 and an induced draft fan 7 connected in sequence, and the spray tower is connected to the exhaust gas discharge port of the pre-calcining furnace 1 and the dewaxing kettle 2. The spray tower includes a primary spray tower 3 and a secondary spray tower 4, the inlet of the spray tower is arranged at the bottom, and the outlet of the spray tower is arranged at the top. The primary spray tower 3 and the secondary spray tower 4 are sequentially provided with a water storage area 8, an atomization layer 9, a spray layer 10 and a demisting layer 11 from bottom to top. The atomization layer 9 and the spray layer 10 are respectively arranged in two layers between the water storage area 8 and the demisting layer 11.

[0031] Table 1 shows the mold shell strength and wax smoke treatment results in Examples 1-3

[0032] It can be seen from Table 1 that the wax fume treatment efficiency of the embodiment of the present application is more than 95% (inlet detection index and exhaust port detection index), which is higher than the traditional wax fume treatment process, and the efficiency of the traditional wax fume treatment process is only 90%.

[0033] The determination of the high temperature flexural strength of the mold shell refers to the industry standard HB 5352.1-2004 "Test method for properties of investment casting mold shell Part 1: Determination of flexural strength".

[0034] The embodiments of the present invention are described in detail above. Specific examples are used herein to illustrate the principles and implementation methods of the present invention. The description of the above embodiments is only used to help understand the method of the present invention and its core idea. At the same time, for those skilled in the art, according to the idea of ​​the present invention, there will be changes in the specific implementation methods and application scope. In summary, the content of this specification should not be understood as a limitation on the present invention.

Claims

1. A wax fume treatment process for high temperature alloy casting, characterized in that: Includes steps: 1) Pre-calcination Heating the dewaxed wax mold shell to a first set temperature to evaporate the water in the wax mold shell; After the temperature is raised to the first set temperature, the temperature is raised to the second set temperature and a first heat preservation is performed to fully burn the wax material remaining after dewaxing; After the first heat preservation is completed, the temperature is raised to the third set temperature and the second heat preservation is performed to improve the strength of the mold shell and burn the residue at the same time; After the second heat preservation is completed, the temperature is raised to the fourth set temperature to ensure that the mold shell strength meets the standard; 2) Wax smoke treatment The wax smoke generated during the dewaxing process and during the pre-baking process of the wax material mold shell after dewaxing is sprayed, electrostatically adsorbed and activated carbon adsorbed in sequence.

2. The wax smoke treatment process for high temperature alloy casting process according to claim 1, characterized in that: The first set temperature is 100-120° C., and the time for heating to the first set temperature is 25-35 minutes; and / or The time for heating to the second set temperature is 65-75 minutes, the second set temperature is 180-220° C., and the first heat preservation time is 18-22 minutes; and / or The third set temperature is 350-450° C., and the second insulation time is 25-35 min; and / or The fourth set temperature is 850-950°C.

3. The wax smoke treatment process of the high temperature alloy casting process according to claim 1 or 2, characterized in that: The method further comprises: After the temperature of the wax mold shell is raised to a first set temperature, air is filled into the wax mold shell so that the wax mold shell is in contact with the air; After the second heat preservation is completed, the air filling is stopped.

4. A wax fume treatment system for a high temperature alloy casting process, characterized in that: include: The dewaxing and roasting device includes a dewaxing kettle and a pre-baking furnace, which is used to first dewax the wax mold shell and then pre-bake it; The wax smoke treatment device comprises a spray tower, an electrostatic precipitator, an activated carbon adsorption tower and an induced draft fan which are connected in sequence. The spray tower is connected to the waste gas discharge ports of the pre-calcining furnace and the dewaxing kettle.

5. The wax fume treatment system for high temperature alloy casting process according to claim 4, characterized in that: The spray tower comprises a primary spray tower and a secondary spray tower, the inlet of the spray tower is arranged at the bottom, the outlet of the spray tower is arranged at the top, and the primary spray tower and the secondary spray tower are sequentially provided with a water storage area, an atomization layer, a spray layer and a demisting layer from bottom to top.

6. The wax fume treatment system for high temperature alloy casting process according to claim 5, characterized in that: The atomization layer and the spraying layer are respectively arranged in two layers between the water storage area and the demisting layer.

7. The wax fume treatment system for high temperature alloy casting process according to claim 4, characterized in that: The pre-baking furnace is connected with a blower.

Citation Information

Patent Citations

  • Precision casting formation process for castings

    CN106077472A

  • Exhaust gas pretreatment device

    CN109248507A

  • Method for preparing mold case for casting beryllium aluminum alloy

    CN110918875A

  • Precision casting process of large thin-wall high-temperature alloy shell casting

    CN112296261A

  • Precision casting waste gas treatment integrated device

    CN214389455U