Display screen protection panel and manufacturing method thereof
By using a protective panel composed of a PMMA diaphragm and an injection molded PC or ABS plastic layer on the elevator display screen, the problem of insufficient impact resistance and explosion-proofness of the glass panel is solved, high transparency and mechanical performance are improved, and production costs are reduced. cost.
Patent Information
- Application Number
- CN202411082837.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-08
- Publication Date
- 2024-10-11
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing glass protective panels on elevator display screens have insufficient impact resistance, drop resistance and explosion-proof properties, and require high process requirements and are fragile.
Use a display protective panel composed of a PMMA diaphragm and an injection molded PC or ABS plastic layer. The acrylic layer and plastic layer are formed through the injection molding process to improve transparency and mechanical properties, and reduce production through the design of the nut mounting part and the melt guide. cost.
It achieves high transparency, impact resistance, drop resistance and explosion-proof properties, while reducing production costs and avoiding the fragility problem of glass panels.
Smart Images

Figure CN118752873A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of display accessories, and in particular to a display screen protection panel and a method for manufacturing the display screen protection panel. Background Art
[0002] The elevator display screen is usually equipped with a transparent protective panel to protect the display screen from physical damage, such as scratches and collisions; it is also used to prevent impurities such as dust and water droplets from entering the display screen and affecting the display effect; the transparency can also make the display screen look neater and more beautiful, and coordinate with the overall design style of the elevator.
[0003] In the prior art, the transparent protective panel on the elevator display screen is usually made of a glass plate, such as an elevator car, an elevator system, a glass display screen and a glass display disclosed in Chinese invention publication number CN208054685U, in which a glass display screen and a glass display disclosed both use a transparent glass substrate.
[0004] However, the above-mentioned solution using glass plates still has the following shortcomings: although the glass plates can ensure transparency, they have high process requirements, are easy to break, and have insufficient impact resistance and explosion-proof capabilities.
[0005] Therefore, how to develop a display screen substrate that is impact-resistant, drop-resistant, explosion-proof, and highly transparent to overcome the above disadvantages has become a topic to be studied by those skilled in the art. Summary of the invention
[0006] The purpose of the present invention is to provide an impact-resistant, drop-resistant, explosion-proof, transparent display screen protection panel and a method for manufacturing the display screen protection panel in view of the deficiencies in the prior art, aiming to ensure high transparency while improving the impact resistance, drop resistance and explosion resistance of the display screen substrate.
[0007] The present invention achieves the above-mentioned purpose through the following technical solutions: A display screen protection panel, comprising: An acrylic layer and a plastic layer arranged on one side of the acrylic layer.
[0008] As a further solution of the present invention: the display screen protection panel is made by injection molding on one side of the acrylic layer, the acrylic layer is a PMMA layer, and the plastic layer is a PC layer or an ABS layer.
[0009] As a further solution of the present invention: the plastic layer includes a main body layer and an edge layer, the main body layer matches and connects with the acrylic layer, the edge layer is arranged on a side of the main body layer away from the acrylic layer, and the outer edge of the edge layer extends out of the main body layer.
[0010] As a further solution of the present invention: a nut mounting portion is provided on a side of the outer edge away from the acrylic layer, and a nut mounting groove is provided on the nut mounting portion; The outer edge is also provided with a bayonet and a hook, and the hook extends out from a side of the outer edge away from the acrylic layer; The side of the outer edge away from the acrylic layer also has a fracture point matched with the melt injection port of the melt guide.
[0011] As a further solution of the present invention: the thickness of the plastic layer accounts for 60% to 90%.
[0012] As a further solution of the present invention: the thickness of the plastic layer accounts for 95% to 99%.
[0013] As a further solution of the present invention: the thickness of the plastic layer is 3.9 mm to 3.95 mm, and the thickness of the acrylic layer is 0.05 mm to 0.1 mm.
[0014] As a further solution of the present invention: a method for manufacturing a display screen protection panel comprises the following steps: Material preparation steps: prepare the injection molding material and the PMMA film of predetermined thickness; Loading step: feeding the injection plastic into the injection molding machine, placing the PMMA film on the front mold cavity of the front mold core of the injection mold on the injection molding machine; Injection molding step: closing the injection mold, the front mold cavity of the front mold core and the rear mold frame cavity of the rear mold core form the cavity of the injection mold, injecting the injection molten material from the front mold frame injection port of the front mold frame plate, the injection molten material enters the molten material buffer cavity of the molten material guide member, and then flows to the molten material drainage channel, and is injected into the cavity of the injection mold from the molten material injection port of the molten material drainage channel, so that the injection plastic and the PMMA diaphragm are thermoplastically fused, and the injection molten material also flows into the molding hole of the rear mold frame cavity position until it is dried, cooled, molded and solidified to obtain a finished product, which includes an acrylic layer corresponding to the PMMA diaphragm and a plastic layer corresponding to the injection molten material; The first mold opening step: the injection mold is opened, the front mold core and the rear mold core are separated, the finished product is located in the rear mold frame cavity of the rear mold core, the nut mounting part of the finished product is inserted into the molding hole, the guide hole column in the molding hole is inserted into the nut mounting groove of the nut mounting part, and the horn waste piece in the melt guide piece is connected with the outer edge of the finished product; The second mold opening step: the ejector plate drives the ejector to eject the finished product, the ejector pushes the guide hole column to insert and press against the nut mounting groove of the nut mounting part, so that the nut mounting part of the finished product is pushed out of the forming hole, the horn waste piece is disconnected and separated from the outer edge of the finished product, so that the outer edge of the finished product forms a fracture point at the disconnection position with the horn waste piece; The first unloading step: pulling out the nut mounting groove on the nut mounting part from the guide hole column, thereby taking out the finished product; The second unloading step: taking out the waste horn piece from the melt guide and resetting the melt guide; Cycle steps: Cycle from the loading step to the second unloading step.
[0015] As a further solution of the present invention: in the material preparation step, preparing the PMMA film of predetermined thickness comprises: stretching the PMMA material or pressing it into a PMMA film of 0.05 mm to 0.1 mm thickness by a high pressure molding machine; The loading step also includes: one side of the PMMA film is pressed against the film receiving position of the front mold cavity; The second unloading step and the circulation step also include: Nut pre-setting steps: place the nut in the nut mounting groove on the nut mounting part and fix it by hot melting.
[0016] As a further solution of the present invention: the material preparation step also includes: a limit clamping opening is provided at the edge of the PMMA diaphragm, a limit clamping protrusion is provided at the edge of the front model cavity which is clamped by the limit clamping opening, a forming hole is provided at the rear mold frame cavity of the rear mold core for forming a nut mounting part on the finished product, and a guide hole column is inserted in the forming hole and used for forming a nut mounting groove.
[0017] Beneficial effects of the present invention: In this solution, a layer of PMMA film is added to the injection molding material, specifically one side of the PMMA film is thermoplastically fused with the injection molding melt formed by the injection molding material, and then formed, so as to obtain a display screen protection panel, including an acrylic layer corresponding to the PMMA film and a plastic layer corresponding to the injection molding material. Furthermore, the transparency of the entire product can be effectively improved, specifically the part covered by the acrylic layer has higher smoothness and transparency. At the same time, compared with the glass substrate of the prior art, the display screen protection panel of this solution has higher impact resistance, drop resistance and explosion resistance, is not easy to break, and has a lower production cost. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 It is a structural schematic diagram of the display screen protection panel of the present invention.
[0019] Figure 2 It is a schematic diagram of the planar structure and partial structure enlargement of the display screen protection panel of the present invention.
[0020] Figure 3 It is a schematic diagram of the structure of the PMMA film of the present invention.
[0021] Figure 4 It is a schematic structural diagram of the injection mold of the present invention in the mold closing state.
[0022] Figure 5It is a structural schematic diagram of the injection mold of the present invention, in which the PMMA film is loaded into the front mold cavity of the front mold core in the mold opening state.
[0023] Figure 6 This is a schematic diagram of the structure of the injection mold of the present invention after the injection molding is completed, in the mold opening state and after the finished product is removed.
[0024] Figure 7 It is a schematic diagram of the structural decomposition of the injection mold of the present invention.
[0025] Figure 8 for Figure 7 Schematic diagram of the structure from another perspective.
[0026] Fig. 9 It is a structural schematic diagram of the melt guide member of the present invention and its exploded schematic diagram.
[0027] Fig.10 It is a schematic structural diagram of the front mold core and the rear mold core of the present invention in a mold closing state.
[0028] Fig.11 It is a schematic structural diagram of the front mold core and the PMMA diaphragm of the present invention.
[0029] Fig.12 The schematic diagram of the structure and the enlarged schematic diagram of the local structure of the finished product taken out from the rear mold core after the injection mold of the present invention is opened.
[0030] Reference numerals include: 1—Display screen protection panel, 11—Acrylic layer, 12—Plastic layer, 121—nut mounting portion, 122—nut mounting groove; 2—Injection mold, 21 - front mold frame, 22 - front mold core, 23 - rear mold frame, 24 - rear mold core, 25 - melt guide, 26 - front mold plate, 27 - runner plate, 28 - ejector plate, 29 - rear mold plate, 211—front mold runner hole, 251—melt buffer chamber, 252—melt drainage channel, 253—horn waste piece, 252a—melt injection port, 261—Front mold injection port, 271—flow channel cavity, 272—flow channel outlet, 281 - thimble, 221—front mold cavity, 221a—diaphragm accommodation position, 221b—edge position, 221c—front mold glue inlet hole, 221e—limiting convex, 241—rear mold cavity, 241a—molding hole, 241b—guide hole column; 3—PMMA film, 31—Limiting card holding opening. DETAILED DESCRIPTION
[0031] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0032] In the description of the present invention, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inside", "outside" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific position, be constructed and operated in a specific position, and therefore cannot be understood as limiting the present invention; the terms "first", "second", and "third" are only used for descriptive purposes, and cannot be understood as indicating or implying relative importance. In addition, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be an indirect connection through an intermediate medium, or it can be a connection between the two elements. For those of ordinary skill in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0033] like Figure 1 to Figure 12 As shown, in an embodiment of the present invention, a display screen protection panel 1 is provided, comprising: an acrylic layer 11 and a plastic layer 12 arranged on one side of the acrylic layer 11 .
[0034] In this solution, a layer of PMMA film 3 is added to the injection molding material, specifically one side of the PMMA film 3 is thermoplastically fused with the injection molding melt formed by the injection molding material and formed, thereby obtaining a display screen protection panel 1, including an acrylic layer 11 corresponding to the PMMA film 3, and a plastic layer 12 corresponding to the injection molding material. Furthermore, the transparency of the entire product can be effectively improved, specifically the part covered by the acrylic layer 11 has higher smoothness and transparency. At the same time, compared with the glass substrate of the prior art, the display screen protection panel 1 of this solution has higher impact resistance, drop resistance and explosion resistance, is not easy to break, and has a lower production cost.
[0035] Among them, the injection molding material adopts PC injection molding material or ABS injection molding material.
[0036] It is worth mentioning that: Polycarbonate is abbreviated as PC in English, also known as PC plastic; it is a high molecular polymer containing carbonate groups in the molecular chain. According to the structure of the ester group, it can be divided into aliphatic, aromatic, aliphatic-aromatic and other types. Among them, the mechanical properties of aliphatic and aliphatic-aromatic polycarbonates are relatively low, which limits their application in engineering plastics.
[0037] ABS plastic is a ternary copolymer of acrylonitrile (A), butadiene (B) and styrene (S). The relative contents of the three monomers can be changed arbitrarily to make various resins.
[0038] In one embodiment, the display screen protection panel 1 is made by injection molding on one side of the acrylic layer 11, the acrylic layer 11 is a PMMA layer, and the plastic layer 12 is a PC layer or an ABS layer. Thus, the transparency of the entire product is further improved, and specifically, the smoothness and transparency of the portion covered by the acrylic layer 11 are further improved. At the same time, compared with the glass substrate of the prior art, the display screen protection panel 1 of this solution further improves the impact resistance, drop resistance and explosion resistance, is not easy to break, and further reduces the production cost.
[0039] In another embodiment, Figure 1 As shown, the plastic layer 12 includes a main body layer and an edge layer, the main body layer matches and is connected to the acrylic layer 11, the edge layer is arranged on the side of the main body layer away from the acrylic layer 11, and the outer edge of the edge layer extends out of the main body layer. Specifically, the nut mounting portion 121 is provided with a nut mounting groove 122 for mounting and placing the nut, and the nut is pressed into the nut mounting groove 122 of the nut mounting portion 121 by hot melting to be fixed, and then the nut is set in the display screen protection panel 1 in advance to further improve the applicability and convenience of assembly. Furthermore, the transparency of the entire product is further improved, specifically the part covered by the acrylic layer 11, its smoothness and transparency are further improved, and at the same time, compared with the glass substrate of the prior art, the display screen protection panel 1 of this solution further improves the impact resistance, drop resistance and explosion resistance, is not easy to break, and further reduces the production cost.
[0040] In another embodiment, a nut mounting portion 121 is provided on a side of the outer edge away from the acrylic layer 11, and a nut mounting groove 122 is provided on the nut mounting portion 121; a bayonet and a hook are provided on the side of the outer edge away from the acrylic layer 11; and a break point is provided on the side of the outer edge away from the acrylic layer 11 to match the melt injection port 252a of the melt guide 25. Thus, the production cost is reduced, and the surface of the finished product will not be damaged to affect the overall aesthetics.
[0041] In another embodiment, the thickness of the plastic layer 12 accounts for 60% to 90%. Specifically, 70% is preferred. In addition, the transparency of the entire product is further improved, specifically the part covered by the acrylic layer 11, and its smoothness and transparency are further improved. At the same time, compared with the glass substrate of the prior art, the display screen protection panel 1 of this solution further improves impact resistance, drop resistance and explosion resistance, is not easy to break, and further reduces the production cost.
[0042] In another embodiment, the thickness of the plastic layer 12 accounts for 95% to 99%. Specifically, 98% is preferred. In addition, the transparency of the entire product is further improved, specifically the part covered by the acrylic layer 11, and its smoothness and transparency are further improved. At the same time, compared with the glass substrate in the prior art, the display screen protection panel 1 of this solution further improves impact resistance, drop resistance and explosion resistance, is not easy to break, and further reduces the production cost.
[0043] In another embodiment, the thickness of the plastic layer 12 is 3.9 mm to 3.95 mm, and the thickness of the acrylic layer 11 is 0.05 mm to 0.1 mm. Specifically, the total thickness of the display screen protection panel 1 is 4 mm. In addition, the transparency of the entire product is further improved, and specifically, the smoothness and transparency of the part covered by the acrylic layer 11 are further improved. At the same time, compared with the glass substrate of the prior art, the display screen protection panel 1 of this solution further improves the impact resistance, drop resistance and explosion resistance, is not easy to break, and further reduces the production cost.
[0044] In another embodiment, a method for manufacturing a display screen protection panel 1 includes the following steps: a material preparation step, a material loading step, an injection molding step, and a material unloading step. Among them: Material preparation step: preparing an injection molding material and a PMMA film 3 of a predetermined thickness, wherein the injection molding material is a PC injection molding material or an ABS injection molding material; Loading steps: see Figure 5 , feeding the injection molding material into the injection molding machine, and placing the PMMA film 3 on the front mold cavity 221 of the front mold core 22 of the injection mold 2 on the injection molding machine; Injection molding steps: see Figure 4, the injection mold 2 is molded together, the front mold cavity 221 of the front mold core 22 and the rear mold frame 23 cavity of the rear mold core 24 form the cavity of the injection mold 2, and the injection molten material is injected from the front mold frame 21 injection port of the front mold frame 21 plate, and the injection molten material enters the melt buffer cavity 251 of the melt guide 25, and then flows to the melt guide channel 252, and is injected into the cavity of the injection mold 2 from the melt injection port 252a of the melt guide channel 252, so that the injection plastic and the PMMA film 3 are thermoplastically fused, and the injection molten material also flows into the molding hole 241a of the cavity position of the rear mold frame 23 until it is dried, cooled, molded and solidified to obtain a finished product, which includes an acrylic layer 11 corresponding to the PMMA film 3 and a plastic layer 12 corresponding to the injection molten material; First mold opening step: the injection mold 2 is opened, the front mold core 22 and the rear mold core 24 are separated, the finished product is located in the cavity of the rear mold frame 23 of the rear mold core 24, the nut mounting portion 121 of the finished product is inserted into the molding hole 241a, the guide hole column 241b in the molding hole 241a is inserted into the nut mounting groove 122 of the nut mounting portion 121, and the horn waste piece 253 in the melt guide 25 is connected to the outer edge of the finished product; Second mold opening step: the ejector plate 28 drives the ejector pin 281 to eject the finished product, and the ejector pin 281 pushes the guide hole column 241b to insert and abut against the nut mounting groove 122 of the nut mounting portion 121, so that the nut mounting portion 121 of the finished product is pushed out of the forming hole 241a, and the horn waste piece 253 is disconnected and separated from the outer edge of the finished product, so that the outer edge of the finished product forms a fracture point at the disconnection position with the horn waste piece 253; First step of cutting: see Fig.12 and Figure 6 , pull out the nut mounting groove 122 on the nut mounting portion 121 from the guide hole column 241b, thereby taking out the finished product; The second unloading step: taking out the waste horn piece 253 from the melt guide 25 and resetting the melt guide 25; Cycle steps: Cycle from the loading step to the second unloading step.
[0045] In this solution, a layer of PMMA film 3 is added to the PC injection plastic, specifically one side of the PMMA film 3 is thermoplastically fused and formed with the PC injection plastic, thereby obtaining a display screen protection panel 1, including an acrylic layer 11 corresponding to the PMMA film 3, and a plastic layer 12 corresponding to the PC injection plastic. Furthermore, the transparency of the entire product can be effectively improved, specifically the part covered by the acrylic layer 11 has higher smoothness and transparency. At the same time, compared with the glass substrate of the prior art, the display screen protection panel 1 of this solution has higher impact resistance, drop resistance and explosion resistance, is not easy to break, and has a lower production cost.
[0046] In another embodiment, in the material preparation step, preparing the PMMA film 3 of the predetermined thickness comprises: stretching the PMMA material or pressing it into a PMMA film 3 with a thickness of 0.05 mm to 0.1 mm using a high pressure molding machine; The loading step also includes: one side of the PMMA film 3 is pressed against the film receiving position 221a of the front mold cavity 221; The second unloading step and the circulation step also include: Nut pre-setting step: place the nut in the nut mounting groove 122 on the nut mounting portion 121, and fix it by hot melting, specifically by hot melting with a hot melting machine. In addition, the transparency of the entire product is further improved, specifically the part covered by the acrylic layer 11, its smoothness and transparency are further improved. At the same time, compared with the glass substrate of the prior art, the display screen protection panel 1 of this solution further improves impact resistance, drop resistance and explosion resistance, is not easy to break, and further reduces the production cost.
[0047] In another embodiment, the edge of the PMMA diaphragm 3 is provided with a limit clamping opening 31, the edge position 221b of the front mold cavity position 221 is provided with a limit clamping protrusion 221e that is clamped by the limit clamping opening 31, and the rear mold frame 23 mold cavity position of the rear mold core 24 is provided with a molding hole 241a for molding the nut mounting portion 121 on the finished product, and a guide hole column 241b inserted in the molding hole 241a. Specifically, the guide hole column 241b is provided in the molding hole 241a, so that the nut mounting portion 121 and the nut mounting groove 122 on the nut mounting portion 121 can be molded during injection molding, and the nut can be fixed to the nut mounting groove 122 in advance by hot melting to improve the convenience of later installation. Furthermore, the transparency of the entire product is further improved, specifically the part covered by the acrylic layer 11, whose smoothness and transparency are further improved. At the same time, compared with the glass substrate in the prior art, the display protection panel 1 of the present solution further improves the impact resistance, drop resistance and explosion resistance, is not easy to break, and further reduces the production cost.
[0048] like Figure 1 to Figure 12 As shown, in the embodiment of the present invention, an injection mold 2 for manufacturing a display screen protection panel 1 is also provided, see FIG. Figure 7 to Figure 12 , including: a front mold plate 26, a runner plate 27, a front mold frame 21, a front mold core 22, a rear mold core 24, a rear mold frame 23, an ejector plate 28, a rear mold plate 29 and a melt guide 25. Among them: The front mold plate 26 is provided with a front mold glue injection port 261; A flow channel plate 27 is provided on one side of the front mold plate 26 and is provided with a flow channel cavity 271 communicating with the front mold injection port 261 and a flow channel outlet 272 on a side away from the front mold plate 26; The front mold frame 21 is disposed on a side of the flow channel plate 27 away from the front mold plate 26 and is provided with a front mold flow channel hole 211 communicating with the flow channel glue outlet 272; The front mold core 22 is arranged on the side wall of the front mold frame 21 away from the flow channel plate 27, and is formed with a front mold cavity 221, wherein the front mold cavity 221 includes a diaphragm accommodating position 221a and an edge position 221b arranged on the outer edge of the diaphragm accommodating position 221a, and the edge position 221b is provided with a front mold glue inlet hole 221c connected to the front mold flow channel hole 211; The rear mold frame 23 is located at a side of the front mold frame 21 away from the flow channel plate 27; The rear mold core 24 is arranged on the side wall of the rear mold frame 23 close to the front mold frame 21, and has a rear mold cavity 241 matching the front mold cavity 221. After the front mold core 22 and the rear mold core 24 are molded together, the front mold cavity 221 and the rear mold cavity 241 constitute the cavity of the injection mold 2; A melt guide 25 is provided on the front mold core 22 and / or the rear mold core 24. A melt buffer cavity 251 and a melt drain channel 252 are provided on the melt guide 25. The melt buffer cavity 251 is communicated with the front mold glue inlet hole 221c and the melt drain channel 252 respectively. The melt drain channel 252 is provided with a certain arc structure. One end of the melt drain channel 252 is communicated with the melt buffer cavity 251, and the other end is communicated with the front mold cavity position 221 and / or the rear mold cavity position 241, so that the injection melt is ejected from the melt drain channel 252 and enters the mold cavity of the injection mold 2; The ejector plate 28 is disposed on a side of the rear mold frame 23 away from the front mold frame 21 and has an ejector pin 281; The rear mold plate 29 is arranged on a side of the ejector plate 28 away from the rear mold frame 23. Specifically, the injection melt is injected from the front mold injection port 261 of the front mold plate 26, enters the runner cavity 271 of the runner plate 27, and enters the front mold runner hole 211 of the front mold frame 21 from the runner outlet 272 of the runner plate 27, and then enters the front mold injection hole 221c of the front mold core 22, and then enters the melt buffer cavity 251 of the melt guide 25 from the front mold injection hole 221c, and then flows into the melt guide 252 of the melt guide 25, and is injected into the cavity of the injection mold 2 from the melt injection port 252a of the melt guide 252.
[0049] In this solution, an injection mold 2 for manufacturing a display screen protection panel 1 is provided, so that the PMMA diaphragm 3 can be placed in the mold cavity of the injection mold 2, specifically in the diaphragm receiving position 221a of the front mold cavity 221 of the front mold core 22, and the mold is closed and the injection molding melt is injected, so that the PMMA diaphragm 3 and the injection molding melt are thermoformed, thereby manufacturing a display screen protection panel 1, which can have higher impact resistance, drop resistance and explosion resistance while ensuring high transparency. Among them, the setting of the melt guide 25 allows the flow rate of the injection molding melt to be buffered by the melt buffer cavity 251 and the melt drainage channel 252 of the melt guide 25 before entering the mold cavity of the injection mold 2. The finished product obtained in this way, that is, the display screen protection panel 1, will not have the appearance of poor effects such as scratches and bubbles on its surface, and the finished product will not be damaged when it is removed to affect the overall aesthetics.
[0050] It should be mentioned that the inventors have repeatedly studied and found that if there is no melt guide 25, a glue inlet bump will be formed at the connection between the finished product and the cavity glue outlet where the injection molding melt is ejected, affecting the overall appearance of the finished product. It is therefore necessary to set up an additional milling step to remove the glue inlet bump. The setting of the molten material guide 25 of the present scheme enables the flow rate of the injection molding molten material to be buffered by the molten material buffer cavity 251 and the molten material drainage channel 252 of the molten material guide 25 before entering the cavity of the injection mold 2. The finished product thus obtained, namely the display screen protection panel 1, will not have the appearance-damaging effects such as punching and bubbles on its surface. Moreover, when the mold is opened, after the ejector plate 28 ejects the display screen protection panel 1, the horn waste piece 253 in the molten material guide 25 can be automatically pulled apart from the display screen protection panel 1, and a tiny fracture point that does not affect the overall appearance is left on the edge layer of the display screen protection panel 1. The production cost is low, the appearance is good, and no glue inlet bump is produced. Therefore, no additional processing step is required to mill off the glue inlet bump of the finished product.
[0051] Production process of display screen protection panel 1: First, in the mold opening state, the PMMA diaphragm 3 is installed on the front mold cavity 221 of the front mold core 22, specifically, in the diaphragm receiving position 221a of the front mold cavity 221, by clamping the limiting clamping opening 31 of the PMMA diaphragm 3 on the limiting clamping protrusion 221e of the front mold cavity 221; Then, the mold is closed, the front mold frame 21 and the rear mold frame 23 are closed, the front mold core 22 and the rear mold core 24 are closed, the front mold cavity 221 of the front mold core 22 and the rear mold cavity 241 of the rear mold core 24 form the cavity of the injection mold 2, and the melt buffer cavity 251 of the melt guide 25 on the rear mold core 24 is connected with the front mold glue inlet hole 221c of the front mold core 22, and the melt guide channel 252 of the melt guide 25 is connected with the cavity of the injection mold 2, so that the melt injection port 252a of the melt guide channel 252 can eject the injection melt toward the front mold cavity 221 of the front mold core 22, specifically, the edge position 221b of the front mold cavity 221; Next, injection molding is performed, and the injection molten material is injected from the front mold injection port 261 of the front mold plate 26. The injection molten material passes through the runner plate 27, the front mold frame 21, and the front mold core 22, and then enters the melt buffer cavity 251 of the melt guide 25 from the front mold injection hole 221c of the front mold core 22, so that the flow rate of the injection molten material can be buffered. Then, the injection molten material flows from the melt buffer cavity 251 of the melt guide 25 to the melt guide channel 252, and is ejected from the melt injection port 252a of the melt guide channel 252, specifically, toward the PMMA diaphragm 3 located on the front mold cavity 221 of the front mold core 22, so that the injection molten material enters the cavity of the injection mold 2 from the melt injection port 252a of the melt guide 25, and is fully hot-melted with the PMMA diaphragm 3; Then, cool for a certain time, specifically 70s to 100s, preferably 80s to 90s, so that the injection molten material in the cavity is cooled and formed; wherein, the injection molten material in the melt buffer cavity 251 and the melt drainage channel 252 in the melt guide 25 will also be cooled together, and the ox-horn waste piece 253 is formed. Since the melt drainage channel 252 is connected to the cavity of the injection mold 2, before the mold is opened, the ox-horn waste piece 253 is connected to the finished product, that is, the outer edge of the display screen protection panel 1; Finally, the mold is opened, the front mold frame 21 and the rear mold frame 23 are opened, and the front mold core 22 and the rear mold core 24 are opened to obtain the finished product, namely the display screen protection panel 1; and since the forming hole 241a is provided on the rear mold cavity 241 of the rear mold core 24, and the guide hole column 241b, namely the ejector pin 281, extends into the forming hole 241a, the display screen protection panel 1 can form the nut mounting portion 121 when the mold is opened, and since the nut mounting groove 122 of the nut mounting portion 121 is formed by the guide hole column 241b, the nut mounting groove 122 of the nut mounting portion 121 is inserted into the guide hole column 241b when the mold is opened, so that the finished product, namely the display screen protection panel, is obtained when the mold is opened. 1 is located on the rear mold cavity 241 of the rear mold core 24, and when the guide hole column 241b is the ejector pin 281, the ejector plate 28 ejects the ejector pin 281, so that the finished product, that is, the display screen protection panel 1, can be ejected from the rear mold cavity 241 of the rear mold core 24, and at the same time, the horn waste piece 253 is disconnected and separated from the display screen protection panel 1, so that the display screen protection panel 1 forms a fracture point at the fracture where it is disconnected from the horn waste piece 253, and finally, the finished product, that is, the display screen protection panel 1, can be removed by the operator; and then the new PMMA membrane 3 can be reinstalled on the front mold cavity 221 of the front mold core 22, so as to injection mold the next new finished product.
[0052] In addition, since the PMMA film 3 is inserted into the limiting clamping protrusion 221e of the front mold cavity 221 through the limiting clamping opening 31, the limiting clamping protrusion 221e can extend out of the PMMA film 3. During injection molding, the limiting clamping protrusion 221e can form a clamping port and a clamping hook on the finished product, so that the finished product, i.e., the display screen protection panel 1, is easier to install on the display screen of the elevator. Specifically, by presetting a buckle portion matching the hook on the outer side of the display screen of the elevator, the hook can be directly aligned with the buckle portion and buckled and engaged during installation, so that the display screen protection panel 1 is fastened to the display screen of the elevator.
[0053] In one embodiment, Fig. 9 As shown, the molten material guide channel 252 is in a bull horn structure, specifically, the channel opening of the molten material guide channel 252 gradually decreases from large to small, the end with the large channel opening is connected to the molten material buffer chamber 251, and the end with the small channel opening is the molten material injection port 252a, which is connected to the cavity of the injection mold 2, that is, connected to the front mold cavity 221 and / or the rear mold cavity 241, so as to inject the injection molten material into the cavity of the injection mold 2. Specifically, since the channel opening at the molten material injection port 252a is small, after the mold is opened, when the ejector plate 28 ejects the display screen protection panel 1, it is easier to separate the display screen protection panel 1 from the bull horn waste piece 253, and the fracture point formed on the display screen protection panel 1 is smaller, so as not to affect the overall appearance.
[0054] Preferably, the melt injection port 252a is oriented toward the edge 221b of the front mold cavity 221 and is adjacent to the edge 221b.
[0055] Preferably, the molten material guide 25 is arranged on the rear mold core 24, and the molten material injection port 252a injects the molten material toward the front mold cavity 221 of the front mold core 22, specifically, toward the edge 221b of the front mold cavity 221. Since the PMMA film 3 is placed in the front mold cavity of the front mold core 22, this arrangement of injection direction makes it easier for the injection molten material and the PMMA film 3 to be fully hot-melted, and the final finished product, i.e., the display screen protection panel 1, will also have better transparency and impact resistance.
[0056] In another embodiment, Figure 5 and Fig.11 As shown, the edge 221 b of the front mold cavity 221 is provided with a limiting protrusion 221 e for matching and engaging with the limiting holding opening 31 of the PMMA film 3 , so that the PMMA film 3 is firmly fixed on the front mold cavity 221 .
[0057] In yet another embodiment, Figure 6 and Fig.12 As shown, a forming hole 241a and a guide hole column 241b inserted in the forming hole 241a are provided at a position opposite to the edge position 221b of the front model cavity 221, so as to be used for forming the nut mounting portion 121 of the display screen protection panel 1. Specifically, the forming hole 241a is used to form the outer contour of the nut mounting portion 121, and the guide hole column 241b forms a nut mounting groove 122 for placing the nut on the nut mounting portion 121, so that the nut can be fixed to the nut mounting groove 122 in advance by hot melting to improve the convenience of later installation, and when the ejector plate 28 ejects the display screen protection panel 1 during mold opening, the guide hole column 241b can still be inserted into the nut mounting groove 122, so that the display screen protection panel 1 will not fall off after being ejected, and is easy for the operator to take. Among them, the guide hole column 241b can be replaced by the ejector pin 281 on the ejector plate 28, or the guide hole column 241b is arranged at the end of the ejector pin 281 on the ejector plate 28, and is pushed by the ejector pin 281 on the ejector plate 28 to expand and contract in the forming hole 241a, that is, the ejector pin 281 and the guide hole column 241b both extend into the forming hole 241a, and when the mold is opened, the ejector pin 281 pushes the guide hole column 241b to eject the finished product.
[0058] Finally, it should be noted that the above is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A display screen protection panel, characterized in that: include: An acrylic layer (11) and a plastic layer (12) arranged on one side of the acrylic layer (11).
2. The display screen protection panel according to claim 1, characterized in that: The display screen protection panel is manufactured by injection molding on one side of the acrylic layer (11); the acrylic layer (11) is a PMMA layer, and the plastic layer (12) is a PC layer or an ABS layer.
3. The display screen protection panel according to claim 1, characterized in that: The plastic layer (12) comprises a main body layer and an edge layer, the main body layer matches the acrylic layer (11) and is connected to the acrylic layer (11), the edge layer is arranged on a side of the main body layer away from the acrylic layer (11), and the outer edge of the edge layer protrudes from the main body layer.
4. The display screen protection panel according to claim 3, characterized in that: A nut mounting portion (121) is provided on a side of the outer edge away from the acrylic layer (11), and the nut mounting portion (121) is provided with a nut mounting groove (122); The outer edge is also provided with a latch and a latch hook, the latch hook extending from a side of the outer edge away from the acrylic layer (11); The side of the outer edge away from the acrylic layer (11) also has a fracture point.
5. The display screen protection panel according to claim 1, characterized in that: The thickness of the plastic layer (12) accounts for 60% to 90%.
6. The display screen protection panel according to claim 5, characterized in that: The thickness of the plastic layer (12) accounts for 95% to 99%.
7. The display screen protection panel according to claim 1, characterized in that: The thickness of the plastic layer (12) is 3.9 mm to 3.95 mm, and the thickness of the acrylic layer (11) is 0.05 mm to 0.1 mm.
8. A method for manufacturing a display screen protection panel, characterized in that: The steps include: Material preparation step: preparing an injection molding material and a PMMA film of a predetermined thickness (3); Loading step: feeding the injection molding material into the injection molding machine, and placing the PMMA film (3) in the front mold cavity (221) of the front mold core (22) of the injection mold; Injection molding step: closing the injection mold, the front mold cavity (221) of the front mold core (22) and the rear mold frame (23) cavity of the rear mold core (24) form a mold cavity of the injection mold, injecting injection molten material from the front mold frame (21) injection port of the front mold frame (21) plate, the injection molten material enters the melt buffer cavity (251) of the melt guide member (25), then flows to the melt guide channel (252), and is injected into the mold cavity of the injection mold from the melt injection port (252a) of the melt guide channel (252), so that the injection plastic and the PMMA film (3) are thermoplastically fused, and the injection molten material also flows into the molding hole (241a) of the mold cavity of the rear mold frame (23) until molding, to obtain a finished product, the finished product comprising an acrylic layer (11) corresponding to the PMMA film (3), and a plastic layer (12) corresponding to the injection molten material; The first mold opening step: the injection mold is opened, the front mold core (22) and the rear mold core (24) are separated, the finished product is located in the mold cavity of the rear mold frame (23) of the rear mold core (24), the nut mounting portion (121) of the finished product is inserted into the molding hole (241a), the guide hole column (241b) in the molding hole (241a) is inserted into the nut mounting groove (122) of the nut mounting portion (121), and the horn waste piece (253) in the melt guide piece (25) is connected to the outer edge of the finished product; The second mold opening step: the ejector plate (28) drives the ejector pin (281) to eject the finished product, and the ejector pin (281) pushes the guide hole column (241b) to insert and press against the nut mounting groove (122) of the nut mounting portion (121), so that the nut mounting portion (121) of the finished product is pushed out of the forming hole (241a), and the ox horn waste piece (253) is disconnected and separated from the outer edge of the finished product, so that the outer edge of the finished product forms a fracture point at the disconnection position with the ox horn waste piece (253); The first unloading step: pulling the nut mounting groove (122) on the nut mounting portion (121) out of the guide hole column (241b), thereby taking out the finished product; The second unloading step: removing the horn waste piece (253) from the melt guide (25) and resetting the melt guide (25); Cycle steps: Cycle from the loading step to the second unloading step.
9. The method for manufacturing a display screen protection panel according to claim 8, characterized in that: In the material preparation step, preparing the PMMA film (3) of predetermined thickness comprises: stretching or pressing the PMMA material into a PMMA film (3) with a thickness of 0.05 mm to 0.1 mm; The loading step also includes: one side of the PMMA film (3) is pressed against the film receiving position (221a) of the front mold cavity (221); The second unloading step and the circulation step also include: Nut pre-setting steps: place the nut in the nut installation groove (122) and fix it by hot melting.
10. The method for manufacturing a display screen protection panel according to claim 8, characterized in that: The edge of the PMMA diaphragm (3) is provided with a limit clamping opening (31), the edge position (221b) of the front mold cavity position (221) is provided with a limit clamping protrusion (221e) that is clamped by the limit clamping opening (31), and the mold cavity position of the rear mold frame (23) of the rear mold core (24) is provided with a molding hole (241a) for molding a nut mounting portion (121) on a finished product, and a guide hole column (241b) inserted into the molding hole (241a).
Citation Information
Patent Citations
Plastic injection mold having angle pin glue feeding structure
CN201012529Y
Transparent panel and vehicle-mounted equipment with information display part
CN203267382U
Domestic appliance panel and have its cooking utensil
CN207492631U
Plastic mold structure for injection molding of sealing copper cover
CN213891049U
Display screen protection panel
CN222972952U