Preparation method of ultrasonic treatment transducer based on PMN-PZT composite material

By adding PMN ceramics to PZT ceramics, a new ternary piezoelectric ceramic material is formed, which solves the problem of low piezoelectric performance of traditional ultrasonic therapy transducers at room temperature and achieves higher dielectric and piezoelectric properties. Improved data accuracy and stability of the device.

CN118754657APending Publication Date: 2024-10-11JIANGSU LEAO INFORMATION TECH CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202410905183.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-08
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

The piezoelectric performance of traditional ultrasound therapy transducers is low at room temperature, which affects the effectiveness of the equipment.

Method used

A new ternary piezoelectric ceramic material composed of adding PMN ceramics to PZT ceramics is used. PMN-PZT composite materials are prepared through high-temperature synthesis, crushing, sieving, ball milling, adding binders and sintering to improve the dielectric properties of the materials. and piezoelectric properties.

Benefits of technology

It is possible to improve the piezoelectric performance of the ultrasonic therapy transducer at room temperature, make data acquisition more accurate and stable, and improve the overall performance of the device.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a preparation method of an ultrasonic treatment transducer based on a PMN-PZT composite material. The PMN-PZT composite material is adopted for manufacturing the ultrasonic treatment transducer. The brand-new ternary system piezoelectric ceramic material is formed by adding PMN ceramic into PZT ceramic, and the purposes that the beneficial performance of the PMN ceramic and the beneficial performance of the PZT ceramic are achieved, and the product performance of an ultrasonic treatment transducer made of the material is improved are achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of production and manufacturing of ultrasonic therapeutic transducers, and in particular to a method for preparing an ultrasonic therapeutic transducer based on a PMN-PZT composite material. Background Art

[0002] Ultrasonic transducers are very important core components in medical ultrasound systems. They convert the system's electrical signals into ultrasonic waves, which are then reflected from the human body and converted back into electrical signals, which are then sent back to the system to form images. Various powerful signal processing algorithms can be used to optimize and shape images, but the quality of the original signal is the most critical basis for improving image quality. Therefore, the preparation of high-quality ultrasound therapy probe materials is one of the research hotspots in the field of ultrasound therapy manufacturing.

[0003] In the traditional manufacturing process, PZT ceramics are generally used. Although PZT ceramic materials have a high Curie temperature, their piezoelectric properties are not high at room temperature, which affects the use of ultrasonic therapeutic transducers.

[0004] At present, there is an urgent need to solve the technical problem of how to improve the piezoelectric properties of materials used to make ultrasonic therapeutic transducers at room temperature.

[0005] The information disclosed in this background technology section is only intended to deepen the understanding of the overall background technology of the present invention, and should not be regarded as acknowledging or suggesting in any form that the information constitutes the prior art already known to those skilled in the art. Summary of the invention

[0006] In order to solve the above technical problems, the present invention proposes a method for preparing an ultrasonic therapeutic transducer based on a PMN-PZT composite material, so as to achieve the purpose of combining the beneficial properties of PMN ceramics and PZT ceramics and improving the product performance of the ultrasonic therapeutic transducer made of this material.

[0007] To achieve the above object, the technical solution of the present invention is as follows:

[0008] A method for preparing an ultrasonic therapeutic transducer based on a PMN-PZT composite material adopts the PMN-PZT composite material to manufacture the ultrasonic therapeutic transducer.

[0009] The invention forms a new ternary piezoelectric ceramic material by adding PMN ceramic to PZT ceramic, thereby achieving the purpose of combining the beneficial properties of PMN ceramic and PZT ceramic and improving the product performance of an ultrasonic therapeutic transducer made of the material.

[0010] Further preferably, the PMN-PZT composite material is made of PbO, MgCO3, Nb2O5, ZrO2, TiO2, A2O3 and PbCO3.

[0011] Further preferably, the PMN-PZT composite material further comprises graphene oxide, wherein the graphene oxide accounts for 1-3% of the total mass ratio.

[0012] Preferably, the preparation steps of the PMN-PZT composite material are as follows:

[0013] 1) Prepare raw materials;

[0014] 2) Dry the raw materials and then perform high temperature synthesis;

[0015] 3) Crush, sieve and ball-mill the high-temperature synthesized materials to make them uniformly mixed;

[0016] 4) Add the binder and then granulate and shape;

[0017] 5) Sintering is performed to obtain the final product.

[0018] As a further preference, the A2O3 is any mixture of any one or more of Y2O3, La2O3, Dy2O3, Nd2O3, and Sm2O3.

[0019] As a further preference, the high temperature synthesis in step 2) is carried out at 700-1000° C. for 1-4 hours.

[0020] Further preferably, the sintering temperature in step 5) is 1150-1250° C., and the sintering time is 1-6 hours; the pressure sintering temperature is 1100-1300° C., the pressure is 40-100 MPa, and the sintering time is 6-15 hours.

[0021] The present invention has the following advantages:

[0022] 1. The present invention forms a new ternary piezoelectric ceramic material by adding PMN ceramic to PZT ceramic, thereby achieving the purpose of combining the beneficial properties of PMN ceramic and PZT ceramic and improving the product performance of the ultrasonic therapeutic transducer made of the material. DETAILED DESCRIPTION

[0023] The technical solutions in the embodiments of the present invention are described clearly and completely below.

[0024] The present invention provides a method for preparing an ultrasonic therapeutic transducer based on a PMN-PZT composite material. The working principle is to add PMN ceramics into PZT ceramics to form a new ternary piezoelectric ceramic material, so as to achieve the purpose of combining the beneficial properties of PMN ceramics and PZT ceramics and improving the product performance of an ultrasonic therapeutic transducer made of the material.

[0025] The present invention is further described in detail below with reference to examples and specific implementation modes.

[0026] A method for preparing an ultrasonic therapeutic transducer based on a PMN-PZT composite material, wherein the PMN-PZT composite material is used to make an ultrasonic therapeutic transducer. The PMN-PZT composite material is a mixture of PMN ceramics and PZT ceramics. That is, PMN is added to PZT ceramics to form a new ternary piezoelectric ceramic material. Since PMN ceramics have higher dielectric and piezoelectric properties, and PZT materials have higher Curie temperatures, the new PMN-PZT composite material has the beneficial properties of both PMN ceramics and PZT ceramics. The ultrasonic therapeutic transducer made of this material is more accurate and stable in acquiring data, thereby improving the performance of the ultrasonic therapeutic transducer.

[0027] The PMN-PZT composite material is made of PbO, MgCO3, Nb2O5, ZrO2, TiO2, A2O3, PbCO3 and graphene oxide. The specific steps are as follows:

[0028] 1) Prepare raw materials;

[0029] 2) After the raw materials are dried, high temperature synthesis is performed, wherein the synthesis temperature is kept at 700-1000°C for 1-4 hours.

[0030] 3) Crush, sieve and ball-mill the high-temperature synthesized materials to make them uniformly mixed;

[0031] 4) Add the binder and then granulate and shape;

[0032] 5) Sintering to obtain the final product, wherein the sintering temperature is 1150-1250° C. and the sintering time is 1-6 hours; the pressure sintering temperature is 1100-1300° C., the pressure is 40-100 MPa, and the sintering time is 6-15 hours.

[0033] Through the above manner, the present invention provides a method for preparing an ultrasonic therapeutic transducer based on a PMN-PZT composite material, which achieves the purpose of combining the beneficial properties of PMN ceramics and PZT ceramics and improving the product performance of an ultrasonic therapeutic transducer made of the material by adding PMN ceramics to PZT ceramics to form a new ternary piezoelectric ceramic material.

[0034] The above is only a preferred embodiment of the method for preparing an ultrasonic therapeutic transducer based on a PMN-PZT composite material disclosed in the present invention. It should be pointed out that, for ordinary technicians in this field, several modifications and improvements can be made without departing from the creative concept of the present invention, which all fall within the scope of protection of the present invention.

Claims

1. A method for preparing an ultrasonic therapeutic transducer based on PMN-PZT composite material, characterized in that: PMN-PZT composite material is used to make ultrasonic therapeutic transducer.

2. The method for preparing an ultrasonic therapeutic transducer based on a PMN-PZT composite material according to claim 1, characterized in that: The PMN-PZT composite material is made of PbO, MgCO3, Nb2O5, ZrO2, TiO2, A2O3 and PbCO3.

3. The method for preparing an ultrasonic therapeutic transducer based on a PMN-PZT composite material according to claim 2, characterized in that: The PMN-PZT composite material also contains graphene oxide, wherein the graphene oxide accounts for 1-3% of the total mass ratio.

4. The method for preparing an ultrasonic therapeutic transducer based on a PMN-PZT composite material according to claim 2, characterized in that: The preparation steps of the PMN-PZT composite material are as follows: 1) Prepare raw materials; 2) Dry the raw materials and then perform high temperature synthesis; 3) Crush, sieve and ball-mill the high-temperature synthesized materials to make them uniformly mixed; 4) Add the binder and then granulate and shape; 5) Sintering is performed to obtain the final product.

5. The method for preparing a PMN-PZT-based transparent electro-optical ceramic material according to claim 4, characterized in that: The A2O3 is any one or more of Y2O3, La2O3, Dy2O3, Nd2O3, and Sm2O3.

6. The method for preparing a PMN-PZT-based transparent electro-optical ceramic material according to claim 4, characterized in that: The high temperature synthesis in step 2) is carried out at 700-1000°C for 1-4 hours.

7. The method for preparing a PMN-PZT-based transparent electro-optical ceramic material according to claim 4, characterized in that: The sintering temperature in step 5) is 1150-1250° C., and the sintering time is 1-6 hours; the pressure sintering temperature is 1100-1300° C., the pressure is 40-100 MPa, and the sintering time is 6-15 hours.

Citation Information

Patent Citations

  • A PMN-PZT-based transparent electro-optic ceramic material and its preparation method

    CN102295456A

  • Piezoelectric body, ultrasound transducer, medical ultrasound diagnostic system, and nondestructive ultrasound test system

    US20120116228A1