PEM electrolytic bath test pole plate and PEM electrolytic bath test device

By using the first sealing ring in the PEM electrolytic cell test device to match the annular groove and sink groove, combined with the collaborative design of the main flow channel and the branch flow channel, the problem of insufficient plate sealing in the existing technology is solved and the gas flow is achieved. Improvements in liquid sealing and distribution efficiency simplify the structure and support rapid single-stack and dual-stack testing.

CN118756243APending Publication Date: 2024-10-11WESTERN METAL MATERIAL
View PDF 0 Cites 3 Cited by

Patent Information

Application Number
CN202410932685.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-12
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

The existing PEM electrolyzer testing device has gap problems in the sealing design of the plates, resulting in air leakage, and the structure is complex, making it difficult to improve gas-liquid sealing and gas-liquid distribution efficiency.

Method used

The first sealing ring is designed to match the annular groove and sinking groove, combined with the collaborative design of the main flow channel and the branch flow channel, to simplify the plate structure, achieve gas-liquid sealing and even distribution of the anode plate and cathode plate, and eliminate the need for additional cover sheets need.

Benefits of technology

It achieves gas-liquid sealing of the anode plate and cathode plate, simplifies the structure, avoids leakage, improves gas-liquid distribution and transmission efficiency, and supports the rapid efficiency of single-stack and double-stack testing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118756243A_ABST
    Figure CN118756243A_ABST
Patent Text Reader

Abstract

The invention discloses a PEM electrolytic bath test polar plate and a PEM electrolytic bath test device, and belongs to the technical field of electrolytic baths. The PEM electrolytic cell test polar plate comprises an anode polar plate and a cathode polar plate which are arranged in parallel, the anode polar plate is provided with an inlet and an outlet, the opposite plate surfaces of the anode polar plate and the cathode polar plate are respectively matched with a first sealing ring, and the opposite plate surfaces of the anode polar plate and the cathode polar plate are respectively provided with a first flow field; the two ends of each first flow field are communicated with channels, the two channels in the anode plate are communicated with the inlet and the outlet respectively, first annular grooves surrounding the inlet, the first flow fields and the outlet together are formed in the opposite plate faces of the anode plate and the cathode plate, and first sinking grooves transversely penetrating through the channels are formed in the corresponding plate faces. According to the PEM electrolytic cell test polar plate, a cover plate does not need to be additionally arranged, the gas-liquid sealing performance of the anode polar plate and the cathode polar plate can be fully ensured only by adopting the first sealing ring, and the structure of the polar plate is simplified.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of electrolyzers, and in particular to a PEM electrolyzer test plate and a PEM electrolyzer test device. Background Art

[0002] Proton Exchange Membrane Electrolyzer Cell (PEMEC), referred to as PEM electrolyzer, is one of the core hydrogen production technologies for realizing carbon-free energy cycle. PEM electrolyzer is generally a water electrolysis hydrogen production device assembled by stacking end plates, separators, plates, membrane electrodes and auxiliary accessories. Among them, the membrane electrode is the main place where the electrochemical reaction occurs, and the membrane electrode is the core component of the entire electrolyzer.

[0003] To study the electrochemical performance of membrane electrodes, it is necessary to reasonably design the structure and stack layout of the remaining components in the electrolyzer, so as to build a stable and reliable PEM electrolyzer test device. The existing PEM electrolyzer test device adopts a design of matching sealing rings and cover sheets on the plate surface. Due to the gap between the sealing ring and the cover sheet, the sealing is insufficient and it is easy to leak after multiple cycles. Summary of the invention

[0004] The purpose of the present invention is to overcome the problems in the prior art and provide a PEM electrolyzer test plate which does not require an additional cover sheet and can fully ensure the gas-liquid sealing of the anode plate and the cathode plate by only using a first sealing ring, thereby simplifying the structure of the plate.

[0005] The present invention provides a PEM electrolyzer test plate, comprising an anode plate and a cathode plate arranged in parallel with each other, the anode plate having an inlet and an outlet, the opposite plate surfaces of the anode plate and the cathode plate are matched with a first sealing ring, the opposite plate surfaces of the anode plate and the cathode plate are provided with a first flow field, both ends of each of the first flow fields are connected with a groove, the two grooves on the anode plate are respectively connected with the inlet and the outlet, the opposite plate surfaces of the anode plate and the cathode plate are provided with a first annular groove that surrounds the inlet, the first flow field and the outlet together, the corresponding plate surfaces are provided with a first sink groove that crosses each groove, each first sink groove is located within the range surrounded by the first annular groove, and both ends of each first sink groove are connected with the first annular groove; the shape of the first sealing ring matches the groove track formed by the first annular groove and the two first sink grooves, and can be simultaneously clamped in the first annular groove and the first sink groove, so that the first sealing ring covers directly above the groove.

[0006] Preferably, the thickness of the first sealing ring is greater than the depth of the first annular groove and the first sink groove; and the width of the first sealing ring is less than or equal to the width of the first annular groove and the first sink groove.

[0007] Preferably, the inlet and the outlet are respectively located at two ends of the first flow field, and the number of corresponding grooves at both ends of the first flow field is multiple, and the multiple grooves are arranged in parallel with each other. The two ends of the first flow field respectively have multiple first main channels with increasing lengths, and the longer the first main channel, the closer it is to the edge of the first flow field, and each first main channel is perpendicular to each groove, and each first main channel is connected to a groove to form an L-shaped channel, and the multiple L-shaped channels located at the same end of the first flow field are parallel to each other; the first flow field also has multiple first branch channels perpendicular to the first main channel, and the longest first main channel at one end of the first flow field and the shortest first main channel at the other end are grouped together, and the second longest first main channel at one end of the first flow field and the second shortest first main channel at the other end are grouped together, and so on, and the two ends of each first branch channel are respectively connected to the ends of two first main channels in the same group.

[0008] Preferably, two transmission layers parallel to the anode plate are provided between the first sealing ring on the anode plate and the first sealing ring on the cathode plate, and a membrane electrode parallel to the anode plate is provided between the two transmission layers. The anode plate and the cathode plate are close to each other, and the first sealing rings are squeezed to achieve sealing, so as to realize single stack testing.

[0009] Preferably, the number of the inlet and the outlet are both two, the two inlets are both located at one end of the anode plate, the two outlets are both located at the other end of the anode plate, the two inlets and the two outlets are respectively located at the four corners of the rectangle, and the two ends of the first flow field on the anode plate are connected to an inlet and an outlet located at the diagonal corners of the rectangle through a groove; the first sealing ring, the transmission layer, the membrane electrode, the transmission layer and the first sealing ring arranged in parallel in sequence constitute a test group, and there are two test groups, both of which are located between the anode plate and the cathode plate, and a bipolar plate parallel to the anode plate is arranged between the two test groups, and both of the bipolar plates are Two plate inlets and two plate outlets are provided which correspond to the two inlets and the two outlets respectively. The bipolar plate and the anode plate have the same structure on the two plate surfaces close to the cathode plate. The bipolar plate and the cathode plate have the same structure on the two plate surfaces close to the anode plate. The two plate surfaces of the bipolar plate are provided with a first flow field which is connected with the plate inlet and the plate outlet. A groove, a first sink groove and a first annular groove are also provided. The straight lines where the inlets and outlets which are connected with each other on the two plate surfaces of the bipolar plate intersect. The anode plate, the bipolar plate and the cathode plate are close to each other and sealed by squeezing each first sealing ring to realize double stack testing.

[0010] The PEM electrolyzer test device includes the PEM electrolyzer test plate, wherein an anode separator and an anode end plate are sequentially arranged on the side of the anode plate away from the cathode plate, and an anode inlet and an anode outlet corresponding to the sub-inlet and the sub-outlet are arranged on the anode separator and the anode end plate, and second annular grooves respectively surrounding the anode inlet and the anode outlet are arranged on each plate surface of the anode separator and the anode end plate, and second annular grooves respectively surrounding the inlet and the outlet are also arranged on the plate surface of the anode plate close to the anode separator, and the same second sealing ring is arranged in two opposite second annular grooves, and the anode end plate, the anode separator and the anode plate are close to each other, and sealing is achieved by squeezing each second sealing ring.

[0011] Preferably, a cathode separator and a cathode end plate parallel to the cathode plate are provided in sequence on one side of the cathode plate away from the anode plate, a plurality of bolt holes are evenly distributed on the edges of the cathode end plate and the anode end plate, a corresponding bolt hole on the cathode end plate and the anode end plate respectively cooperates with the same bolt to achieve fastening, and both side plate surfaces of the anode plate, the bipolar plate and the cathode plate close to one of the bolt holes are provided with a second recessed groove for connecting the detection terminal of the voltage patrol meter.

[0012] Preferably, third sink grooves are provided on the plate surfaces on both sides of the first flow field and parallel to the edges of the first branch flow channel, and two edges of the transmission layer are placed in two third sink grooves in the same first flow field.

[0013] Preferably, multiple coaxial positioning holes are provided on the edges of the anode end plate, the anode separator, the anode plate, the cathode plate, the cathode separator and the cathode end plate, and the multiple coaxial positioning holes cooperate with the same positioning pin to achieve positioning.

[0014] Preferably, the anode end plate and the cathode end plate are provided with a plurality of reinforcing rib grooves for improving strength in the middle of the plate surfaces facing away from each other; the edge of the anode plate has a positive power supply connector, and the edge of the cathode plate has a negative power supply connector.

[0015] Compared with the prior art, the present invention has the following beneficial effects:

[0016] 1. The PEM electrolyzer test plate does not need to add an additional cover plate, eliminating the gap problem caused by adding a cover plate. Only the first sealing ring is needed to fully ensure the gas-liquid sealing of the anode plate and the cathode plate, simplifying the structure of the plate and avoiding the leakage problem;

[0017] 2. Based on the design of the first main flow channel and the first branch flow channel in the first flow field working together, there is no need to set up multiple distribution areas in the flow channel area in the prior art. It is only necessary to arrange the main flow channel and the first branch flow channel in the best proportion into a structure with a self-distribution function to fully ensure the uniformity of gas and liquid, and further simplify the structure of the anode plate and the cathode plate; based on the design of the first flow field on the anode plate and the cathode plate, it is beneficial to promote the distribution and transmission of gas and liquid in the device;

[0018] 3. Dual-stack testing is more efficient than single-stack testing. At the same time, dual-stack or multi-stack testing devices can be combined according to the actual needs of customers and the market. During the combination process, only the corresponding number of test groups and bipolar plates need to be added. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 It is a single pile test assembly diagram of the present invention;

[0020] Figure 2 For the present invention Figure 1 Exploded diagram of

[0021] Figure 3 It is a front schematic diagram of the anode plate of the present invention;

[0022] Figure 4 It is a schematic diagram of the reverse side of the anode plate of the present invention;

[0023] Figure 5 It is a front schematic diagram of the cathode plate of the present invention;

[0024] Figure 6 It is a schematic diagram of the reverse side of the cathode plate of the present invention;

[0025] Figure 7 is a schematic diagram of the first sink of the present invention;

[0026] Figure 8 is a schematic diagram of a first sealing ring of the present invention;

[0027] Fig. 9 It is the explosion diagram of the double pile test of the present invention;

[0028] Fig.10 for Fig. 9 Exploded diagram of

[0029] Fig.11 Schematic diagram of the front and back sides of the bipolar plate of the present invention;

[0030] Fig.12 is a schematic diagram of an anode separator;

[0031] Fig.13 It is a front schematic diagram of the anode terminal plate of the present invention;

[0032] Fig.14 It is a schematic diagram of the reverse side of the anode terminal plate of the present invention;

[0033] Fig.15 is a schematic diagram of a second sealing ring of the present invention;

[0034] Fig.16 is a schematic diagram of a cathode separator of the present invention;

[0035] Fig.17 It is a front schematic diagram of the cathode end plate of the present invention;

[0036] Fig.18 It is a schematic diagram of the reverse side of the cathode end plate of the present invention;

[0037] Fig.19 is a schematic diagram of a third sink of the present invention;

[0038] Fig. 20 Schematic diagram of the transport layer of the present invention.

[0039] Description of reference numerals:

[0040] 1. Inlet, 2. Third trough, 3. First flow field, 4. Membrane electrode, 5. Outlet, 6. First annular groove, 7. Second trough, 8. Second sealing ring, 9. First sealing ring, 10. Transport layer, 11. Sub-inlet, 12. Sub-outlet, 15. Second annular groove, 18. First main channel, 19. First branch channel, 20. Reinforcement rib groove, 30. Anode plate, 31. Groove, 32. First trough, 33. Cathode plate, 34. Bipolar plate, 35. Anode separator, 36. Anode end plate, 37. Cathode separator, 38. Cathode end plate, 39. Bolt hole. DETAILED DESCRIPTION

[0041] In order to make the purpose, technical solution and advantages of the embodiment of the present invention clearer, the technical solution of the embodiment of the present invention will be clearly and completely described below in conjunction with the accompanying drawings of the embodiment of the present invention. Obviously, the described embodiment is a part of the embodiment of the present invention, not all of the embodiments. Based on the described embodiment of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0042] Unless otherwise defined, the technical or scientific terms used herein shall have the usual meanings understood by persons of ordinary skill in the field to which the present invention belongs. "Include" or "comprises" and similar words mean that the elements or objects appearing before the word include the elements or objects listed after the word and their equivalents, without excluding other elements or objects. "Inside", "outside", "upper", "lower", "far", "near", "front", "back", etc. are only used to indicate relative positional relationships. When the absolute position of the described object changes, the relative positional relationship may also change accordingly.

[0043] The drawings in this disclosure are not drawn strictly according to the actual scale, and the specific size and quantity of each structure can be determined according to actual needs. The drawings described in this disclosure are only schematic diagrams of the structures.

[0044] The PEM electrolyzer test plate provided by the present invention is as follows Figure 1-Figure 8 The invention comprises an anode plate 30 and a cathode plate 33 arranged in parallel with each other, wherein the anode plate 30 has an inlet 1 and an outlet 5, and the opposite plate surfaces of the anode plate 30 and the cathode plate 33 are equipped with a first sealing ring 9, and the opposite plate surfaces of the anode plate 30 and the cathode plate 33 are provided with a first flow field 3, and both ends of each first flow field 3 are connected with a groove 31, and the two grooves 31 on the anode plate 30 are connected with the inlet 1 and the outlet 5 respectively, and the opposite plate surfaces of the anode plate 30 and the cathode plate 33 are provided with a common surrounding inlet 1 , the first annular groove 6 of the first flow field 3 and the outlet 5, and the corresponding plate surfaces are provided with first sink grooves 32 that cross each groove 31, each first sink groove 32 is located in the range surrounded by the first annular groove 6, and both ends of each first sink groove 32 are connected to the first annular groove 6; the shape of the first sealing ring 9 matches the groove track formed by the first annular groove 6 and the two first sink grooves 32, and can be simultaneously clamped in the first annular groove 6 and the first sink groove 32, so that the first sealing ring 9 covers directly above the groove 31.

[0045] The reactants first flow in from the inlet 1 on the anode plate 30 and the cathode plate 33, and flow into the first flow field through a corresponding groove 31. After the reaction occurs, the reactants and the products flow out from the outlet 5 through another groove 31.

[0046] The material of the anode plate 30 and the cathode plate 33 is preferably one of the metal plates, more preferably titanium; the thickness of the anode plate 30 and the cathode plate 33 are preferably 1mm~5mm, more preferably 2mm~4mm; the depth of the first flow field 3 is preferably 0.2mm~2.0mm, more preferably 0.4mm~1.0mm; the depth of the first annular groove 6 is preferably 0.2mm~1.0mm, more preferably 0.4mm~0.8mm; the width of the first annular groove 6 is preferably 1mm~8mm, more preferably 2mm~6mm.

[0047] The PEM electrolyzer test plate does not require an additional cover plate, eliminating the problem of gaps caused by adding a cover plate. Only the first sealing ring 9 is needed to fully ensure the gas-liquid sealing of the anode plate 30 and the cathode plate 33, simplifying the structure of the plate and avoiding leakage problems.

[0048] In this embodiment, Figure 7-Figure 8 The thickness of the first sealing ring 9 is greater than the depth of the first annular groove 6 and the first sink groove 32 ; and the width of the first sealing ring 9 is less than or equal to the width of the first annular groove 6 and the first sink groove 32 .

[0049] The purpose is to enable the first sealing ring 9 to be smoothly placed in the first annular groove 6 and the first sink groove 32 , and after the first sealing ring 9 is squeezed, it can better seal the first annular groove 6 and the first sink groove 32 .

[0050] The material of the first sealing ring 9 is preferably one of the insulating materials, preferably a silicone material; the thickness of the first sealing ring 9 is preferably 0.3mm to 3.0mm, more preferably 0.5mm to 2.0mm; the width of the sealing pad 9 is preferably 1mm to 5mm, more preferably 2mm to 4mm. The first sealing ring 9, the first annular groove 6, and the first sink groove 32 form a "single pad + single groove" combination structure, which can fully ensure the sealing performance at the first sink groove 32.

[0051] In this embodiment, Figure 3-Figure 7The inlet 1 and the outlet 5 are respectively located at the two ends of the first flow field 3, and the number of corresponding grooves 31 at the two ends of the first flow field 3 is multiple, and the multiple grooves 31 are arranged in parallel with each other. The two ends of the first flow field 3 are respectively provided with multiple first main channels 18 with increasing lengths. The longer the first main channel 18 is, the closer it is to the edge of the first flow field 3. Each first main channel 18 is respectively perpendicular to each groove 31, and each first main channel 18 is respectively connected to a groove 31 to form an L-shaped channel. The multiple L-shaped channels located at the same end of the first flow field 3 are parallel to each other; the first flow field 3 also has multiple first branch channels 19 perpendicular to the first main channel 18, and the longest first main channel 18 at one end of the first flow field 3 is grouped with the shortest first main channel 18 at the other end, and the second longest first main channel 18 at one end of the first flow field 3 is grouped with the second shortest first main channel 18 at the other end, and so on. The two ends of each first branch channel 19 are respectively connected to the ends of two first main channels 18 in the same group.

[0052] The depth of the first flow field 3 is preferably 0.2mm to 2.0mm, more preferably 0.4mm to 1.8mm. The plate surface between two adjacent grooves 31, between two adjacent first main channels 18 and between two adjacent first branch channels 19 is called a ridge. The height of the ridge between two adjacent first branch channels 19 is preferably 0.2mm to 1.4mm, more preferably 0.4mm to 1.2mm; the width of the first main channel 18 and the first branch channel 19 is preferably 0.5mm to 3.0mm, more preferably 0.5mm to 2.0mm; the width of the ridge between the two grooves 31 is preferably 1.0mm to 4.0mm, more preferably 1.0mm to 3.0mm; the width of the first main channel 18 and the first branch channel 19 in the first flow field 3 must be the width of the first main channel 18 and the first branch channel 19 between the two adjacent first branch channels 19. The height of the ridge between the two first branch channels 19 plus the depth of the first annular groove 6 must be equal to the depth of the first flow field 3; the ratio of the number of the first main channel 18 to the first branch channel 19 is preferably 1:2 to 1:10, and more preferably 1:3 to 1:9; based on the design of the first main channel 18 and the first branch channel 19 cooperating in the first flow field 3, there is no need to set up multiple distribution areas in the flow channel area in the prior art, and the main channel 18 and the first branch channel 19 only need to be arranged in the best proportion into a structure with a distribution function to fully ensure the uniformity of gas and liquid, and further simplify the structure of the anode plate 30 and the cathode plate 33. The design of the first flow field 3 on the anode plate 30 and the cathode plate 33 is conducive to promoting the distribution and transmission of gas and liquid in the device.

[0053] In this embodiment, Figure 2 and Fig. 20Two transmission layers 10 parallel to the anode plate 30 are provided between the first sealing ring 9 on the anode plate 30 and the first sealing ring 9 on the cathode plate 33, and a membrane electrode 4 parallel to the anode plate 30 is provided between the two transmission layers 10. The anode plate 30 and the cathode plate 33 are close to each other, and the first sealing rings 9 are squeezed to achieve sealing, so as to realize single stack testing.

[0054] The material of the transmission layer 10 is preferably one of the porous materials, more preferably titanium felt; the thickness of the transmission layer 10 is preferably 0.1 mm to 1.0 mm, more preferably 0.2 mm to 0.8 mm. Based on the design of the first flow field 3, the transmission layer 10 only needs titanium felt of one porosity to ensure that the gas and liquid are fully diffused inside it, and the structure of the entire single stack test will become simple and compact, and the assembly speed and assembly quality will be significantly improved.

[0055] In this embodiment, Figure 3-Figure 11 The number of the inlet 1 and the outlet 5 is two, the two inlets 1 are located at one end of the anode plate 30, the two outlets 5 are located at the other end of the anode plate 30, the two inlets 1 and the two outlets 5 are respectively located at the four corners of the rectangle, and both ends of the first flow field 3 on the anode plate 30 are connected to an inlet 1 and an outlet 5 located at the diagonal corners of the rectangle through the groove 31; the first sealing ring 9, the transmission layer 10, the membrane electrode 4, the transmission layer 10 and the first sealing ring 9 arranged in parallel in sequence constitute a test group, and there are two test groups, both of which are located between the anode plate 30 and the cathode plate 33, and a bipolar plate 34 parallel to the anode plate 30 is arranged between the two test groups, and the bipolar plate 34 is provided There are two plate inlets and two plate outlets corresponding to the two inlets 1 and the two outlets 5 respectively. The bipolar plate 34 and the anode plate 30 have the same structure on the two plate surfaces close to the cathode plate 33. The bipolar plate 34 and the cathode plate 33 have the same structure on the two plate surfaces close to the anode plate 30. The two plate surfaces of the bipolar plate 34 are provided with a first flow field 3 connected to the plate inlet and the plate outlet, and are also provided with a groove 31, a first sink 32 and a first annular groove 6. The straight lines where the inlets 1 and the outlets 5 connected to each other on the two plate surfaces of the bipolar plate 34 intersect, the anode plate 30, the bipolar plate 34 and the cathode plate 33 are close to each other, and sealing is achieved by squeezing each first sealing ring 9 to achieve double stack testing.

[0056] The bipolar plate 34 is applied to the PEM electrolyzer stack test, and the air tightness reaches 5MPa, and the circulating gas-liquid flow rate can reach 1.0L / min. In addition, from the perspective of macroscopic structure comparison, the bipolar plate 34 on the PEM electrolyzer test device designed by the present invention does not need to add an additional cover plate and set a distribution area, so that the overall structure of the bipolar plate 34 tends to be simplified, which is conducive to its subsequent processing and use; the present invention adopts a design in which the main flow channel 18 and the first branch flow channel 19 work together, and it is only necessary to arrange the main flow channel 18 and the first branch flow channel 19 in a certain proportion into a structure with a self-distribution function to fully ensure the gas-liquid uniformity of the bipolar plate, further simplifying the structure of the bipolar plate.

[0057] The dual-stack test is more efficient than the single-stack test. A dual-stack or multi-stack test device can be combined according to the actual needs of customers and the market. During the combination process, only the corresponding number of test groups and bipolar plates 34 need to be added.

[0058] The PEM electrolyzer test device includes the PEM electrolyzer test plate, such as Figure 2 , Fig. 9 ,like Figure 12-Figure 15 An anode separator 35 and an anode end plate 36 are sequentially provided on the side of the anode plate 30 away from the cathode plate 33. The anode separator 35 and the anode end plate 36 are provided with an anode inlet and an anode outlet corresponding to the sub-inlet 11 and the sub-outlet 12. Second annular grooves 15 respectively surrounding the anode inlet and the anode outlet are provided on the plate surfaces of the anode separator 35 and the anode end plate 36. Second annular grooves 15 respectively surrounding the inlet 1 and the outlet 5 are also provided on the plate surface of the anode plate 30 close to the anode separator 35. The same second sealing ring 8 is padded in the two opposite second annular grooves 15. The anode end plate 36, the anode separator 35 and the anode plate 30 are close to each other, and sealing is achieved by squeezing each second sealing ring 8.

[0059] Two second annular grooves 15 are distributed on the plate surfaces of the anode end plate 36 and the anode separator 35, and the second annular grooves 15 and the second sealing ring 8 are used for sealing between the anode end plate 36 and the anode separator 35; the material of the anode end plate 36 is preferably one of the metal plates, and more preferably an aluminum alloy plate; the material of the anode separator 35 is preferably one of insulating plastic, insulating resin and insulating rubber, and more preferably insulating plastic; the thickness of the anode end plate 36 is preferably 10mm~60mm, and more preferably 10mm~20mm; the thickness of the anode separator 35 is preferably 1mm~6mm, and more preferably 1mm~3mm; the apertures of the sub-inlet 11 and the sub-outlet 12 are preferably 2mm~20mm, and more preferably 2mm~12mm; the depth of the second annular groove 15 is preferably 0.2mm~1.0mm, and more preferably 0.4mm~0.8mm; the width of the second annular groove 15 is preferably 1mm~8mm, and more preferably 2mm~6mm.

[0060] The material of the second sealing ring 8 is preferably one of the insulating materials, more preferably silicone material; the thickness of the second sealing ring 8 is preferably 0.3mm-3.0mm, more preferably 0.5mm-2.0mm; the width of the second sealing ring 8 is preferably 1mm-5mm, more preferably 2mm-4mm. The "single pad + double groove" combination structure composed of the second annular groove 15 + the second sealing ring 8 + the second annular groove 15 can fully ensure the sealing of this connection part in the device.

[0061] In this embodiment, Figure 6 and Figure 16-Figure 18 A cathode separator 37 and a cathode end plate 38 parallel to the cathode plate 33 are provided in sequence on one side of the cathode plate 33 away from the anode plate 30, and multiple bolt holes 39 are evenly distributed on the edges of the cathode end plate 38 and the anode end plate 36. The corresponding bolt holes 39 on the cathode end plate 38 and the anode end plate 36 are fastened with the same bolt, and the two side plate surfaces of the anode plate 30, the bipolar plate 34 and the cathode plate 33 close to one of the bolt holes 39 are provided with a second sink 7 for connecting the detection terminal of the voltage patrol meter.

[0062] The material of the cathode separator 37 is preferably one of insulating plastic, insulating resin and insulating rubber, and more preferably insulating plastic; the thickness of the cathode separator 37 is preferably 1 mm to 6 mm, and more preferably 1 mm to 3 mm. The material of the cathode end plate 38 is preferably one of metal plates, and more preferably aluminum alloy plates; the thickness of the cathode end plate 38 is preferably 10 mm to 60 mm, and more preferably 10 mm to 20 mm.

[0063] The number of bolt holes 39 on the edges of the cathode end plate 38 and the anode end plate 36 is 8. The bolts include a screw rod, a washer and a nut. The test device is fixed by installing the bolts.

[0064] In this embodiment, Figure 7 and Fig.19 Third troughs 2 are provided on the plate surfaces on both sides of the first flow field 3 parallel to the edges of the first branch flow channel 19 , and two edges of the transmission layer 10 are placed in two third troughs 2 in the same first flow field 3 .

[0065] The third sink 2 is used to accurately position the transmission layer 10 and bond / weld it to the surface of the plate flow field, so that during the subsequent assembly process, the transmission layer 10 will not slide or even fall off, which is conducive to improving the assembly quality.

[0066] In this embodiment, Figure 3-Figure 6 and Figure 11-Figure 18 A plurality of coaxial positioning holes are provided on the edges of the anode end plate 36 , the anode separator 35 , the anode plate 30 , the cathode plate 33 , the cathode separator 37 and the cathode end plate 38 . The plurality of coaxial positioning holes cooperate with the same positioning pin to achieve positioning.

[0067] Four positioning through holes 18 are distributed on the anode end plate 36 , the anode separator 35 , the anode plate 30 , the cathode plate 33 , the cathode separator 37 and the cathode end plate 38 for their own positioning.

[0068] In this embodiment, Fig.14 and Fig.18 The anode end plate 36 and the cathode end plate 38 are provided with a plurality of reinforcing rib grooves 20 for improving strength in the middle of the plate surfaces facing away from each other; the edge of the anode plate 30 has a positive power supply connector, and the edge of the cathode plate 33 has a negative power supply connector.

[0069] The reinforcing rib groove 20 is used to enhance the strength of the anode end plate 36 and the cathode end plate 38 while saving materials. The depth of the reinforcing rib groove 20 is preferably 2 mm to 20 mm, more preferably 2 mm to 10 mm.

[0070] The above shows and describes the basic principles, main features and advantages of the present invention. Technical personnel in this industry should understand that the present invention is not limited to the above embodiments. The above embodiments and descriptions are only preferred examples of the present invention and are not used to limit the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention to be protected. The scope of protection of the present invention is defined by the attached claims and their equivalents.

Claims

1. A PEM electrolyzer test plate, comprising an anode plate (30) and a cathode plate (33) arranged parallel to each other, characterized in that: The anode plate (30) is provided with an inlet (1) and an outlet (5). The opposite plate surfaces of the anode plate (30) and the cathode plate (33) are matched with a first sealing ring (9). The opposite plate surfaces of the anode plate (30) and the cathode plate (33) are provided with a first flow field (3). Both ends of each first flow field (3) are connected with a groove (31). The two grooves (31) on the anode plate (30) are respectively connected with the inlet (1) and the outlet (5). The opposite plate surfaces of the anode plate (30) and the cathode plate (33) are provided with a first annular groove (6) which surrounds the inlet (1), the first flow field (3) and the outlet (5). The corresponding plate surfaces are provided with a first sink groove (32) which crosses each groove (31). Each first sink groove (32) is located within the range surrounded by the first annular groove (6), and both ends of each first sink groove (32) are connected with the first annular groove (6). The shape of the first sealing ring (9) matches the groove track formed by the first annular groove (6) and the two first recessed grooves (32), and can be simultaneously clamped in the first annular groove (6) and the first recessed groove (32), so that the first sealing ring (9) covers directly above the groove (31).

2. The PEM electrolyzer test plate according to claim 1, characterized in that: The thickness of the first sealing ring (9) is greater than the depth of the first annular groove (6) and the first recessed groove (32); and the width of the first sealing ring (9) is less than or equal to the width of the first annular groove (6) and the first recessed groove (32).

3. The PEM electrolyzer test plate according to claim 1, characterized in that: The inlet (1) and the outlet (5) are respectively located at two ends of the first flow field (3); the number of the corresponding channels (31) at the two ends of the first flow field (3) is multiple, and the multiple channels (31) are arranged in parallel with each other; the two ends of the first flow field (3) respectively have multiple first main channels (18) of increasing lengths, and the longer the first main channel (18), the closer it is to the edge of the first flow field (3); each first main channel (18) is respectively perpendicular to each channel (31), and each first main channel (18) is respectively connected to a channel (31) to form an L-shaped channel; and the multiple L-shaped channels located at the same end of the first flow field (3) are parallel to each other; The first flow field (3) also has a plurality of first branch flow channels (19) perpendicular to the first main flow channel (18); the first main flow channel (18) with the longest length at one end and the first main flow channel (18) with the shortest length at the other end in the first flow field (3) are grouped together; the first main flow channel (18) with the second longest length at one end and the first main flow channel (18) with the second shortest length at the other end in the first flow field (3) are grouped together; and so on; the two ends of each first branch flow channel (19) are respectively connected to the ends of the two first main flow channels (18) in the same group.

4. The PEM electrolyzer test plate according to claim 1, characterized in that: Two transmission layers (10) parallel to the anode plate (30) are provided between the first sealing ring (9) on the anode plate (30) and the first sealing ring (9) on the cathode plate (33); a membrane electrode (4) parallel to the anode plate (30) is provided between the two transmission layers (10); the anode plate (30) and the cathode plate (33) are brought close to each other and the first sealing rings (9) are squeezed to achieve sealing, so as to realize a single stack test.

5. The PEM electrolyzer test plate according to claim 4, characterized in that: The number of the inlet (1) and the number of the outlet (5) are both two, the two inlets (1) are both located at one end of the anode plate (30), the two outlets (5) are both located at the other end of the anode plate (30), the two inlets (1) and the two outlets (5) are respectively located at the four corners of the rectangle, and both ends of the first flow field (3) on the anode plate (30) are connected to an inlet (1) and an outlet (5) located at diagonally opposite corners of the rectangle through the groove (31); A first sealing ring (9), a transmission layer (10), a membrane electrode (4), a transmission layer (10) and a first sealing ring (9) are sequentially arranged in parallel to form a test group. There are two test groups, both of which are located between the anode plate (30) and the cathode plate (33). A bipolar plate (34) parallel to the anode plate (30) is arranged between the two test groups. The bipolar plate (34) is provided with two plate inlets and two plate outlets corresponding to the two inlets (1) and the two outlets (5), respectively. The bipolar plate (34) and the anode plate (30) are close to the two plate surfaces of the cathode plate (33). The structure is the same as above, the bipolar plate (34) and the cathode plate (33) have the same structure on the two plate surfaces close to the anode plate (30), the two plate surfaces of the bipolar plate (34) are provided with a first flow field (3) connected to the plate inlet and the plate outlet, and are also provided with a groove (31), a first sink groove (32) and a first annular groove (6), the straight lines where the inlet (1) and the outlet (5) connected to each other on the two plate surfaces of the bipolar plate (34) intersect, the anode plate (30), the bipolar plate (34) and the cathode plate (33) are close to each other, and are sealed by squeezing each first sealing ring (9) to realize a double stack test.

6. A PEM electrolyzer testing device, comprising the PEM electrolyzer testing plate according to claim 5, characterized in that: An anode separator (35) and an anode end plate (36) are sequentially arranged on the side of the anode plate (30) away from the cathode plate (33); an anode inlet and an anode outlet corresponding to the sub-inlet (11) and the sub-outlet (12) are arranged on the anode separator (35) and the anode end plate (36); second annular grooves (15) respectively surrounding the anode inlet and the anode outlet are arranged on the plate surfaces of the anode separator (35) and the anode end plate (36); a second annular groove (15) respectively surrounding the inlet (1) and the outlet (5) is also arranged on the plate surface of the anode plate (30) close to the anode separator (35); a second sealing ring (8) is arranged in two opposite second annular grooves (15); the anode end plate (36), the anode separator (35) and the anode plate (30) are close to each other, and sealing is achieved by squeezing each second sealing ring (8).

7. The PEM electrolyzer testing device according to claim 6, characterized in that: A cathode separator (37) and a cathode end plate (38) parallel to the cathode plate (33) are sequentially arranged on one side of the cathode plate (33) away from the anode plate (30); a plurality of bolt holes (39) are evenly distributed on the edges of the cathode end plate (38) and the anode end plate (36); a bolt hole (39) corresponding to each other on the cathode end plate (38) and the anode end plate (36) is fastened with the same bolt; and second recessed grooves (7) for connecting detection terminals of a voltage inspection instrument are arranged on both side surfaces of the anode plate (30), the bipolar plate (34) and the cathode plate (33) near one of the bolt holes (39).

8. The PEM electrolyzer testing device according to claim 6, characterized in that: Third troughs (2) are provided on the plate surfaces on both sides of the first flow field (3) and parallel to the edges of the first branch flow channel (19), and the two edges of the transmission layer (10) are placed in the two third troughs (2) in the same first flow field (3).

9. The PEM electrolyzer testing device according to claim 7, characterized in that: Multiple coaxial positioning holes are provided on the edges of the anode end plate (36), the anode separator (35), the anode plate (30), the cathode plate (33), the cathode separator (37) and the cathode end plate (38), and the multiple coaxial positioning holes are all matched with the same positioning pin to achieve positioning.

10. The PEM electrolyzer testing device according to claim 7, characterized in that: The anode end plate (36) and the cathode end plate (38) are both provided with a plurality of reinforcing rib grooves (20) for increasing strength in the middle of the plate surfaces facing away from each other; the edge of the anode plate (30) has a positive power supply connector, and the edge of the cathode plate (33) has a negative power supply connector.

Citation Information

Cited By

  • PEM electrolytic cell electrochemical performance test system and method

    CN119352053A

  • Flow battery SOC testing device and SOC-OCV calibration method

    CN121164937A

  • Device and method for testing electrochemical performance of anode catalyst

    CN121499615A