Display structure

By combining the anti-reflection layer with gradient refractive index, the phase change layer with low loss and high refractive index and the metal layer with K value compensation in the display structure, the angle sensitivity and color saturation of the reflective display device in the existing technology are solved. problem, achieving high reflectivity, high color saturation and angle-insensitive display effects, which is suitable for a variety of application fields.

CN118759740AActive Publication Date: 2024-10-11HUAZHONG UNIV OF SCI & TECH
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202410960742.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-17
Publication Date
2024-10-11
Estimated Expiration
2044-07-17

AI Technical Summary

Technical Problem

In the existing technology, reflective display devices based on phase change materials are difficult to achieve vivid, highly saturated and dynamically adjustable RGB reflective colors, and have strong angle sensitivity, which affects their application effects.

Method used

A display structure is designed, including an anti-reflective layer with a refractive index gradient, a low-loss, high-refractive index phase change layer, a lossy metal layer that provides K value compensation, and a metal layer that constitutes the FP cavity. Through the phase change material The high refractive index and high extinction properties of the metal layer, combined with multi-layer refractive index gradient media, achieve high reflectivity, high color saturation and angle-insensitive display effects.

Benefits of technology

It achieves high reflectivity, high color saturation, angle-insensitive display effects, simple structure, and dynamic adjustment. It is suitable for micro-nano displays, anti-counterfeiting measures, reflective color filters and other fields, overcoming the limitations of existing structures. limitation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118759740A_ABST
    Figure CN118759740A_ABST
Patent Text Reader

Abstract

The invention provides a display structure, and the structure comprises an anti-reflection layer which comprises a multi-layer medium with a refractive index gradient, the refractive index of the multi-layer medium is gradually increased from top to bottom, the K value of the multi-layer medium is smaller than 0.5, the total thickness and the effective refractive index of the anti-reflection layer meet a certain condition in the three primary colors of red, green and blue, and the effective refractive index of the anti-reflection layer meets a certain condition in the three primary colors of red, green and blue. The upper and lower electric fields of the position of the phase change layer below the anti-reflection layer are 0; the optical loss of a used phase change material is smaller than a first preset threshold value, the refractive index of the used phase change material is larger than a second preset threshold value, and the phase change layer is located below the anti-reflection layer; the first metal layer is lossy metal for providing K value compensation, and the first metal layer is located below the phase change layer; the second metal layer is used for forming an FP cavity, and the second metal layer is located below the first metal layer; and the dielectric layer is positioned below the second metal layer. The reflective phase change display structure is high in reflectivity, high in color saturation, insensitive in angle, dynamically adjustable and simple in structure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of phase change materials, and in particular to a display structure. Background Art

[0002] So far, various types of color filters have been developed, such as those based on subwavelength gratings, nanoresonators, plasmonic nanostructures, photonic crystals, and multilayer thin films. However, these filters are inevitably limited in practical applications because they exhibit angle-sensitive spectral properties, which manifest as spectral shifts of the central wavelength and reduced transmission and reflection efficiencies at oblique incidence.

[0003] For some nanophotonic devices, including metal nanoantenna arrays and plasmonic nanostructures, people have tried to take measures to mitigate their angular sensitivity. However, since complex manufacturing techniques such as electron beam or nanoimprint lithography are inevitably required, reflective displays based on FP (Fabry-Perot) cavity structures have attracted much attention due to their simple structure. Among them, non-volatile displays using phase change materials have attracted much attention due to their advantages such as low power consumption and dynamic adjustability. However, how to use low-loss, high-reflectivity phase change materials to achieve vivid, highly saturated and dynamically adjustable RGB reflective colors remains a challenge. Summary of the invention

[0004] In order to solve the problems existing in the prior art, the present invention provides a display structure.

[0005] The present invention provides a display structure, comprising:

[0006] The anti-reflection layer comprises a multilayer medium with a refractive index gradient, wherein the refractive index of the multilayer medium increases from small to large from top to bottom, the K value of the multilayer medium is less than 0.5, and the total thickness and equivalent refractive index of the anti-reflection layer meet certain conditions when the three primary colors of red, green and blue are used, so that the upper and lower electric fields at the position where the phase change layer below the anti-reflection layer is located are 0;

[0007] The phase change layer, the phase change material used in the phase change layer has an optical loss less than a first preset threshold and a refractive index greater than a second preset threshold, the N value of the phase change material is greater than 1 in the visible light region, the larger the better, and the K value is less than 1 in the visible light region, the smaller the better, the phase change layer is located below the anti-reflection layer;

[0008] A first metal layer, which is a lossy metal providing K value compensation, and the first metal layer is located below the phase change layer;

[0009] A second metal layer, used to form a FP cavity, the second metal layer being located below the first metal layer;

[0010] The dielectric layer is located below the second metal layer.

[0011] According to a display structure provided by the present invention, when the color generated by the display structure is red or blue, the total thickness of the anti-reflection layer is λ0 / (4n);

[0012] When the color generated by the display structure is green, the total thickness of the anti-reflection layer is λ0 / (8n);

[0013] Wherein, λ0 is the wavelength to be suppressed by the anti-reflection layer, and n is the effective refractive index of the anti-reflection layer.

[0014] According to a display structure provided by the present invention, the thickness of the dielectric layer is λ c / (2n1),λ c is the target wavelength of the color generated by the display structure, and n1 is the refractive index of the medium layer.

[0015] According to a display structure provided by the present invention, the effective thickness formed by the thickness of the phase change material and the thickness of the first metal layer is less than λ c / (4n2π),λ c is the target wavelength of the color generated by the display structure, n2 is the effective refractive index of the phase change material and the first metal layer, the K value of the first metal layer is greater than the N value of the first metal layer, and the K value of the first metal layer is greater than 1.

[0016] According to a display structure provided by the present invention, the phase change layer is one or more layers, each phase change layer includes a phase change material and an electrode layer deposited on the lower side of the phase change material, and the voltage threshold of the phase change material in each phase change layer is different;

[0017] The first metal layer is one layer or multiple layers.

[0018] According to a display structure provided by the present invention, the phase change material is an alloy compound composed of a VI main group element and a III to V main group element, and the alloy compound is doped with an Ib main group element.

[0019] According to a display structure provided by the present invention, the phase change material includes one or more alloys such as Sb2Se3 and Sb2S3, wherein the percentage of each atom is adjustable;

[0020] The dielectric layer includes transparent media such as TIO2, Ta2O5 and LaTIO3, and the K value of the media is less than 1 and approaches 0.

[0021] According to a display structure provided by the present invention, the second metal layer is a simple substance formed by one element from main groups III to V or a compound composed of multiple elements in any proportion.

[0022] According to a display structure provided by the present invention, the second metal layer is a metal material having the ability to conduct electricity and generate heat, such as Ag, Al, and W.

[0023] A display structure provided according to the present invention further includes a reflective layer, wherein the reflective layer is located below the dielectric layer, and the thickness of the reflective layer is greater than 50 nm.

[0024] The present invention provides a display structure, a reflective phase change display structure based on a low-loss, high-refractive-index phase change material, which is a thin film composed of a medium, a metal constituting an FP cavity, a lossy metal providing a compensation K value, and a low-loss, high-refractive-index phase change material. It is designed to form a reflective phase change display with high reflectivity, high color saturation, and angle insensitivity. The design mainly utilizes the high refractive index of the phase change material itself and the high extinction coefficient of the metal providing K value compensation to absorb light other than the target area and allow the light in the target area to pass through, and is combined with an anti-reflection layer composed of a top layer of multiple layers of a refractive index gradient medium, thereby achieving the effects of high reflectivity, high color saturation, angle insensitivity, dynamic adjustability, and simple structure. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] In order to more clearly illustrate the technical solutions in the present invention or the prior art, the following briefly introduces the drawings required for use in the embodiments or the description of the prior art. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0026] Figure 1 It is a schematic diagram of the display structure provided by the present invention;

[0027] Figure 2 is a schematic diagram of a spectrum of blue produced by the display structure provided by the present invention;

[0028] Figure 3 It is a schematic diagram of the spectrum of green produced by the display structure provided by the present invention;

[0029] Figure 4 It is a schematic diagram of the spectrum of red generated by the display structure provided by the present invention;

[0030] Figure 5 is a schematic diagram showing the angle insensitivity of the display structure provided by the present invention to produce blue;

[0031] Figure 6 is a schematic diagram of the angle insensitivity of the display structure provided by the present invention to produce green;

[0032] Figure 7It is a schematic diagram of the angle insensitivity of the display structure provided by the present invention to produce red.

[0033] Reference numerals:

[0034] 101: substrate; 102: reflective layer; 103: third dielectric layer; 104: second metal layer; 105: first metal layer; 106: phase change layer; 107: second dielectric layer; 108: first dielectric layer. DETAILED DESCRIPTION

[0035] In order to make the purpose, technical solution and advantages of the present invention clearer, the technical solution of the present invention will be clearly and completely described below in conjunction with the drawings of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0036] Combine the following Figure 1 A display structure of the present invention is described, comprising:

[0037] The anti-reflection layer comprises a multilayer medium with a refractive index gradient, wherein the refractive index of the multilayer medium increases from small to large from top to bottom, the K value of the multilayer medium is less than 0.5, and the total thickness and equivalent refractive index of the anti-reflection layer meet certain conditions when the three primary colors of red, green and blue are used, so that the upper and lower electric fields at the position where the phase change layer below the anti-reflection layer is located are 0;

[0038] The phase change layer 106, the phase change material used in the phase change layer 106 has an optical loss less than a first preset threshold and a refractive index greater than a second preset threshold, the N value of the phase change material is greater than 1 in the visible light region, the larger the better, and the K value is less than 1 in the visible light region, the smaller the better, the phase change layer 106 is located below the anti-reflection layer;

[0039] A first metal layer 105 is a lossy metal for providing K value compensation, and the first metal layer 105 is located below the phase change layer 106;

[0040] A second metal layer 104, used to form a FP cavity, wherein the second metal layer 104 is located below the first metal layer 105;

[0041] The dielectric layer is located below the second metal layer 104 .

[0042] The upper anti-reflection layer may include a first dielectric layer 108 and a second dielectric layer 107, wherein the first dielectric layer 108 is located on the second dielectric layer 107. The K value of each dielectric layer in the anti-reflection layer is less than 0.5, preferably 0.

[0043] To minimize absorption losses and achieve high reflectivity, the top anti-reflection layer can reduce reflection in non-peak areas by introducing an additional resonant cavity.

[0044] The phase change material used in the phase change layer 106 is a low-loss, high-refractive-index phase change material. The low-loss, high-refractive-index phase change material refers to a phase change material whose N value in the visible light region is greater than 1, the larger the better, and whose K value in the visible light region is less than 1, the smaller the better.

[0045] The first metal layer 105 is a high-loss metal that provides K value compensation. The metal that provides K value compensation needs to have a K value greater than the N value and greater than 1. The second metal layer 104 located below the first metal layer 105 is used to form a FP cavity.

[0046] The dielectric layer below the second metal layer 104 is the third dielectric layer 103. Below the third dielectric layer 103 is the reflective layer 102, and below the reflective layer 102 is the substrate 101.

[0047] The phase change material of the phase change layer 106 can be converted between a crystalline state and an amorphous state under electrical stimulation or laser stimulation, thereby changing the transmittance and reflectivity of the phase change layer 106. Metal Ag is deposited under the phase change layer 106, and the phase change layer 106 can control the crystallization state of the phase change material by applying voltage on Ag.

[0048] Specifically, a pulse voltage or laser pulse of medium intensity is applied to the phase change layer 106. Under the action of the current or laser pulse, the temperature of the phase change material rises to a temperature range above the crystallization temperature and below the melting temperature and is maintained for a certain period of time. At this time, the crystal lattice is orderly arranged to form a crystalline state, realizing the transition from amorphous to crystalline.

[0049] A short and strong voltage or laser pulse is applied to the phase change layer 106 to raise the temperature of the phase change material to above the melting temperature, thereby destroying the long-range order of the crystalline state. The pulse falling edge is very short, causing the phase change material to be quickly cooled to below the crystallization temperature, so that the phase change material is fixed in the amorphous state, realizing the transition from the crystalline state to the amorphous state. The grayscale of the display device is controlled by the changes in the transmittance and reflectivity of the phase change material of the phase change layer 106 when converting between the amorphous state and the crystalline state.

[0050] The phase change layer 106 of the phase change filter component has very different N and K in different states. The phase change material is stable in the crystalline and amorphous states, so the voltage or laser can be removed when the phase change material is in a stable state, so the power consumption of the entire display device during the display process is very low.

[0051] The FP structure that produces color based on low-loss, high-refractive-index phase-change materials consists of a dielectric-phase-change material-lossy metal-metal-phase-change material-metal (MDM) cavity or multiple cavities of the same or different types. The cavity should be designed so that the state change of the phase-change material does not change the significant movement of the color peak, but only changes in the corresponding band, that is, changes the grayscale of the display. By applying voltage or heating the electrode layer, the crystal structure of the phase-change material can be changed, thereby adjusting the peak value and position of the cavity.

[0052] Through this design, reflective display devices based on low-loss, high-refractive-index phase-change materials can produce high-reflectivity, high-color-saturation, and angle-insensitive display devices to meet the demand for high-color-saturation and high-reflectivity regulation in the reflective display market based on phase-change materials.

[0053] In this embodiment, the reflective phase change display structure based on the low-loss, high-refractive-index phase change material is a thin film composed of a medium, a metal constituting an FP cavity, a lossy metal providing compensation for the K value, and a low-loss, high-refractive-index phase change material. It is designed to form a reflective phase change display with high reflectivity, high color saturation, and angle insensitivity. The design mainly utilizes the high refractive index of the phase change material itself and the high extinction coefficient of the metal providing K value compensation to absorb light other than the target area, while allowing the light in the target area to pass through, combined with the anti-reflection layer composed of the top layer of multi-layer refractive index gradient medium, thereby achieving the effects of high reflectivity, high color saturation, angle insensitivity, dynamic adjustability, and simple structure. This structure has great application potential in various fields such as micro-nano displays, anti-counterfeiting measures, reflective color filters, and decorations, overcomes the inherent limitations of existing structures, has significant technological advancement significance, and opens up new possibilities for the further development of phase change display technology.

[0054] On the basis of the above embodiment, in this embodiment, when the color generated by the display structure is red or blue, the total thickness of the anti-reflection layer is λ0 / (4n);

[0055] When the color generated by the display structure is green, the total thickness of the anti-reflection layer is λ0 / (8n);

[0056] Wherein, λ0 is the wavelength to be suppressed by the anti-reflection layer, and n is the effective refractive index of the anti-reflection layer.

[0057] This setting causes strong resonance in the target peak region and weakens in the non-target peak region.

[0058] Based on the above embodiment, the thickness of the dielectric layer in this embodiment is λ c / (2n1),λ cis the target wavelength of the color generated by the display structure, and n1 is the refractive index of the medium layer.

[0059] Based on the above embodiment, the effective thickness of the phase change material and the first metal layer 105 in this embodiment is less than λ c / (4n2π),λ c is the target wavelength of the color generated by the display structure, n2 is the effective refractive index of the phase change material and the first metal layer 105, the K value of the first metal layer 105 is greater than the N value of the first metal layer 105, and the K value of the first metal layer 105 is greater than 1.

[0060] The effective thickness of the phase change material in the reflective phase change display structure and the metal thickness providing the compensation K value should be less than λ c / (4n2π), but it cannot be too thin to ensure that the light absorption at the target peak wavelength is small, while the light absorption at the non-target peak wavelength band is large. In this type of design, all low-loss, high-refractive-index phase-change materials can be applied to the design to form a high-reflectivity phase-change display device.

[0061] On the basis of the above embodiments, the phase change layer 106 in this embodiment is one or more layers, each phase change layer 106 includes a phase change material and an electrode layer deposited on the lower side of the phase change material, and the voltage threshold of the phase change material in each phase change layer is different;

[0062] The first metal layer 105 is one layer or multiple layers.

[0063] In this embodiment, there is at least one layer of phase change material and at least one layer of lossy metal that provides compensation K value for the phase change material. The electrode layer between two adjacent layers of phase change material can be shared. The material of the conductive electrode layer can be Ag, Al, W and other metal materials that are conductive and heat-generating.

[0064] On the basis of the above embodiments, the phase change material in this embodiment is an alloy compound composed of elements of the VI main group and elements of the III to V main groups, and the alloy compound is doped with elements of the Ib main group.

[0065] On the basis of the above embodiments, the phase change material in this embodiment may include the following sulfur compounds and their alloys, including but not limited to one or more low-loss, high-refractive-index phase change materials in alloys such as Sb2Se3 and Sb2S3, wherein the percentage of each atom in the above chemical formula is adjustable. The phase change material layer may further include at least one dopant, such as C and N. Preferably, the phase change material is Sb2Se3, which has a large loss in the visible light range, a large refractive index, and good thermal stability.

[0066] Phase change materials must have low loss and high refractive index, that is, the average K value in the visible light band is less than 1, the smaller the better, and the N value in the visible light band is greater than 1, and the larger the better. The metal that provides K value compensation needs to have a K value greater than the N value and greater than 1.

[0067] The thickness of the phase change layer 106 is less than 50nm. Since the increase of the thickness of the phase change layer 106 will reduce the transmittance of visible light and the temperature required for the crystallization of the phase change material is also higher, the more suitable thickness is within 30nm. The phase change material of the phase change layer 106 can be driven by laser or voltage. When driven by voltage, the transparent electrodes on both sides of the phase change layer 106 apply voltage to cause the phase change material to undergo phase change.

[0068] The dielectric layer is composed of low-loss dielectrics (K value is less than 1 and tends to 0) such as TIO2, Ta2O5, LaTIO3, etc.

[0069] On the basis of the above embodiments, the second metal layer constituting the FP cavity in this embodiment is a single substance formed by one element from the main groups III to V or a compound composed of multiple elements in any proportion.

[0070] On the basis of the above embodiments, in this embodiment, the second metal layer is a metal material with electrical conductivity and heat generation such as Ag, Al, and W.

[0071] On the basis of the above embodiments, this embodiment further includes a reflective layer 102, wherein the reflective layer 102 is located below the dielectric layer, and the thickness of the reflective layer 102 is greater than 50 nm.

[0072] The thickness of the first metal layer 105 is less than 15 nm. The main function of this layer is to compensate for the defect of the low-loss, high-refractive-index phase-change material with a small K value, and further improve the color purity.

[0073] The thickness of the second metal layer 104 is less than 30 nm. This layer is mainly used to form a resonant cavity with the third dielectric layer 103. The display structure mainly controls the color change by changing the thickness of Ta2O5 in the bottom third dielectric layer 103, thereby achieving color change within the color range.

[0074] Optionally, Figure 1 The phase change material of the structure shown in the figure is Sb2Se3, the second metal layer 104 is Ag, and the lossy metal used in the first metal layer 105 is Cr, wherein Sb2Se3 is an ultra-thin phase change material with low optical loss and high refractive index, Ag is a high reflectivity material, Cr is a lossy metal with a high extinction coefficient, and the dielectric materials are Ta205 and MgF2.

[0075] like Figure 1As shown, when the reflective display structure produces blue, the substrate 101 of the reflective display structure is silicon or glass or a flexible substrate, the reflective layer 102Ag of the reflective display structure is 100nm, the third dielectric layer 103Ti2O3 of the reflective display structure is 55nm, the second metal layer 104Ag of the reflective display structure is 6nm, the first metal layer 105Cr of the reflective display structure is 5nm, the phase change layer 106Sb2Se3 of the reflective display structure is 6nm, the second dielectric layer 107Ti2O3 of the reflective display structure is 12nm, and the third dielectric layer 108MgF2 of the reflective display structure is 233nm.

[0076] like Figure 1 As shown, when the reflective display produces green, the substrate 101 of the reflective display structure is silicon or glass or a flexible substrate, the reflective layer 102Ag of the reflective display structure is 100nm, the third dielectric layer 103Ti2O3 of the reflective display structure is 70nm, the second metal layer 104Ag of the reflective display structure is 10nm, the first metal layer 105Cr of the reflective display structure is 7nm, the phase change layer 106Sb2Se3 of the reflective display structure is 8nm, the second dielectric layer 107Ti2O3 of the reflective display structure is 14nm, and the third dielectric layer 108MgF2 of the reflective display structure is 140nm.

[0077] like Figure 1 As shown, when the reflective display produces red, the substrate 101 of the reflective display structure is silicon or glass or a flexible substrate, the reflective layer 102Ag of the reflective display structure is 100nm, the third dielectric layer 103Ti2O3 of the reflective display structure is 110nm, the second metal layer 104Ag of the reflective display structure is 15nm, the first metal layer 105Cr of the reflective display structure is 6nm, the phase change layer 106Sb2Se3 of the reflective display structure is 6nm, the second dielectric layer 107Ti2O3 of the reflective display structure is 32nm, and the third dielectric layer 108MgF2 of the reflective display structure is 233nm.

[0078] Figure 2 Shown is Figure 1 Spectral diagram of the structural parameters corresponding to the structure producing blue, with a reflectivity of more than 80%. Figure 3 Shown is Figure 1 The spectrum of the structural parameters corresponding to the structure producing green has a reflectivity of more than 85%. Figure 4 Shown is Figure 1 The spectrum of the structural parameters corresponding to the structure produces red, and the reflectivity is as high as more than 85%.

[0079] like Figure 5 Shown is Figure 1The corresponding structure produces a blue angle-insensitive graph of the structural parameters, and the angle insensitivity is as high as more than 60 degrees. Figure 6 Shown is Figure 1 The corresponding structure produces a green angle-insensitive graph of the structural parameters, and the angle insensitivity is as high as 60 degrees or more. Figure 7 Shown is Figure 1 The corresponding structure produces a red angle-insensitive graph of the structural parameters, and the angle insensitivity is as high as over 60 degrees.

[0080] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A display structure, characterized in that: include: The anti-reflection layer comprises a multilayer medium with a refractive index gradient, wherein the refractive index of the multilayer medium increases from small to large from top to bottom, the K value of the multilayer medium is less than 0.5, and the total thickness and equivalent refractive index of the anti-reflection layer meet certain conditions when the three primary colors of red, green and blue are used, so that the upper and lower electric fields at the position where the phase change layer below the anti-reflection layer is located are 0; The phase change layer, the phase change material used in the phase change layer has an optical loss less than a first preset threshold and a refractive index greater than a second preset threshold, the N value of the phase change material is greater than 1 in the visible light region, the larger the better, and the K value is less than 1 in the visible light region, the smaller the better, the phase change layer is located below the anti-reflection layer; A first metal layer, which is a lossy metal providing K value compensation, and the first metal layer is located below the phase change layer; A second metal layer, used to form a FP cavity, the second metal layer being located below the first metal layer; The dielectric layer is located below the second metal layer.

2. The display structure according to claim 1, characterized in that: When the color generated by the display structure is red or blue, the total thickness of the anti-reflection layer is λ0 / (4n); When the color generated by the display structure is green, the total thickness of the anti-reflection layer is λ0 / (8n); Wherein, λ0 is the wavelength to be suppressed by the anti-reflection layer, and n is the effective refractive index of the anti-reflection layer.

3. The display structure according to claim 1, characterized in that: The thickness of the dielectric layer is λ c / (2n1),λ c is the target wavelength of the color generated by the display structure, and n1 is the refractive index of the medium layer.

4. The display structure according to claim 1, characterized in that: The effective thickness formed by the thickness of the phase change material and the thickness of the first metal layer is less than λ c / (4n2π),λ c is the target wavelength of the color generated by the display structure, n2 is the effective refractive index of the phase change material and the first metal layer, the K value of the first metal layer is greater than the N value of the first metal layer, and the K value of the first metal layer is greater than 1.

5. The display structure according to any one of claims 1 to 4, characterized in that: The phase change layer is one or more layers, each phase change layer comprises a phase change material and an electrode layer deposited on the lower side of the phase change material, and the voltage threshold of the phase change material in each phase change layer is different; The first metal layer is one layer or multiple layers.

6. The display structure according to any one of claims 1 to 4, characterized in that: The phase change material is an alloy compound composed of a VI main group element and a III to V main group element, and the Ib main group element is doped into the alloy compound.

7. The display structure according to claim 6, characterized in that: The phase change material includes one or more of Sb2Se3 and Sb2S3 alloy, wherein the percentage of each atom is adjustable; The dielectric layer includes a dielectric selected from the group consisting of TIO2, Ta2O5 and LaTIO3, and a K value of the dielectric is less than 1 and approaches 0.

8. The display structure according to any one of claims 1 to 4, characterized in that: The second metal layer is a simple substance formed by one element from the main groups III to V or a compound composed of multiple elements in any proportion.

9. The display structure according to claim 8, characterized in that: The second metal layer is a metal material having electrical conductivity and heat generation among Ag, Al and W.

10. The display structure according to any one of claims 1 to 4, characterized in that: It also includes a reflective layer, which is located below the dielectric layer and has a thickness greater than 50 nm.

Citation Information

Patent Citations

  • Display device based on phase-change material

    CN105938261A

  • Optical device

    CN107771301A

  • Fabry-Perot with coated mirrors

    CN1079820A

  • Pixel structure and display driving method thereof

    CN116449629A

  • Color filter structure and pixel array switching control method thereof

    CN116577943A