Antimicrobial protection in post-tanning stage of leather by combining biocidal composition and luminescent additive

By applying the additional step of biocidal compositions and luminescent additives in the post-tanning stage, the problem of ineffective protection of leather after tanning is solved, a longer period of microbial protection is achieved, and the treatment effect is verified by luminescent properties, significantly improving the quality of the leather. protection and longevity.

CN118765369APending Publication Date: 2024-10-11ANCOR TECH CANARIA SL
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380023575.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-02-23
Filing Date
2023-02-21
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

Existing technologies cannot effectively protect leather from microbial pathogens after tanning, and commonly used biocidal methods are highly aggressive to the environment and difficult to ensure that the leather has been effectively treated.

Method used

An additional step is applied in the post-tanning stage that combines a biocidal composition consisting of silver phosphate glass, silicones and aliphatic hydrocarbons with a luminescent additive formed by metal oxides that luminesce under infrared light. Identifies the presence of the composition and ensures antimicrobial protection of leather.

Benefits of technology

This method provides longer-term microbial protection than conventional methods and uses luminescent properties to verify whether the leather has been treated, significantly increasing the lifespan and protection of the leather while reducing its impact on the environment.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The present invention discloses an additional antimicrobial protection step applied to leather in the post-tanning stage, combining a biocidal composition and an additive that allows the presence thereof to be identified by the luminescence effect in addition to using a luminescence encryption technique to demonstrate its authenticity, wherein the composition is added during the tanning process immediately after the addition of a chromium or titanium salt in an amount of between 0.1% and 5% of the weight of the material to be tanned, comprising: between 3% and 5% of a silver phosphate glass; between 1% and 3.5% of a silicone; between 0.1% and 0.30% of an aliphatic hydrocarbon; between 90% and 95% of water, the luminescent additive being added in an amount between 0.1% and 5% of the weight of the material to be tanned, comprising between 20% and 40% of silica relative to the total weight of the luminescent additive; alumina in a proportion between 10% and 30%; between 30% and 50% of calcium fluoride; between 0.5% and 3% of erbium (III) fluoride; between 5% and 15% of ytterbium (III) fluoride; a maximum of 5% thulium (III) fluoride; and a maximum of 5% europium (III) fluoride.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention discloses an additional step of antimicrobial protection applied to leather in the post-tanning phase, combining a biocidal composition and an additive that allows the presence of the biocidal composition to be identified through a luminescent effect, thus providing a guarantee that the leather has been previously treated with said biocidal product, giving the user peace of mind, in addition to proving its authenticity using luminescent encryption technology. Background Art

[0002] Initially, the treatment of raw leather includes a visual inspection to ensure that it meets the required quality requirements, thus preventing its deterioration. Wastewater is generated during the leather receiving step, which comes from the discharge of the moisture contained in the leather. Then, parts of the neck, tail and limbs are cut off. Washing the leather is used for its rehydration, as well as to remove blood residues, excrement and other contained dirt. For this washing, sodium hydroxide, sodium hypochlorite and detergent are used. For the development of this step of the method, water and chemicals (sodium hydroxide, sodium hypochlorite and detergent) are used to wash the leather. The raw leather is cured by salting out or drying the raw leather.

[0003] To disinfect leather, the most common method is to use salt in two forms: brine salting or brine curing. During this operation, large volumes of water are used, dragging along soil and organic matter as well as blood and manure waste.

[0004] Salt water curing is the faster and most commonly used method, the leather is placed in a vat containing disinfectants (mercuric chloride and carbonic acid), biocides (sodium sulfate and boric acid) and a nearly saturated salt solution. It is stirred to improve the contact between the leather and the solution, and after spending about 16 hours in the vat, the leather completely absorbs the salt. The development of this activity requires water, electrical energy for the stirrer, salt and aggressive chemicals (disinfectants and biocides) for the leather, and empty chemical containers, in addition, solid waste with high moisture content from the leather is generated, as well as water and chemicals (sodium hydroxide, sodium hypochlorite and detergent) used to wash the leather.

[0005] After disinfecting the leather, the pickling step begins, which consists in chemically preparing the leather for the tanning process by using mainly formic acid and sulfuric acid solutions. These acids contribute protons that bond to carboxyl groups, allowing the tanning agent to diffuse inside the leather. In this step, chemicals and water are required to prepare the solution. After this step, the tanning step begins, which consists in treating the leather with chromium or titanium salts.

[0006] Previous methods cannot guarantee that the treated skin is protected from the microbial pathogens present on the leather surface, because the applied biocidal components and subsequent treatments (such as tanning and storage) can reduce the disinfection effect previously applied through the tanning reaction. In addition, the disinfectant products used are aggressive to the environment, so there is a need for a disinfection step associated with an appropriate biocide in the post-tanning stage, which is intended to protect the environment and allow the protection of the leather to last longer, thereby preventing the transmission of diseases caused by microbial pathogens from person to person for a longer period of time. In addition, there is a need for an easier, faster, cheaper and more reliable method to determine whether a biocide has been applied to a leather piece and, optionally, that the leather remains protected for a longer period of time.

[0007] As can be seen from patent application WO2008 / 093353, a more environmentally suitable disinfectant composition has been incorporated into the technology, which relates to the use of a combined proteolytic enzyme and a carbolytic enzyme for soaking leather and / or hides, for cleaning dirt adhering to the hides and leathers, so that it allows their disinfection. The soaking of leather and hides is currently achieved by using surfactants, amines and organic solvents. Also in many cases, when hides are tanned to produce leather, biocidal preparations are added to the tanning drum to prevent the deterioration of the leather during storage and transportation, however, the use of surfactants reduces the quality of the resulting product.

[0008] US Patent No. 5,089,414 suggests using soaking enzymes, such as proteases and / or lipases, to reduce or even avoid the use of surfactants or replace organic solvents. Compared with traditional methods, enzyme soaking processes generally improve the quality of the final leather, reduce the use of chemicals, and replace chemicals that have a harmful impact on the environment.

[0009] It has been shown that treatment with enzymes does not reduce the presence of microorganisms in an effective manner, since within a very short time after application, they degrade, losing the biocidal effect, in addition to the associated costs. The present invention discloses a method for antimicrobial protection of leather in a post-tanning stage, wherein an additional step is incorporated into the post-tanning stage, which incorporates a biocidal product based on a controlled source of Ag+ ions, which allows for longer protection than conventional biocides used in pre-tanning steps. Furthermore, a luminescent additive is included in the additional step to ensure that the leather piece has been treated and is free of microorganisms, pathogens, viruses, etc. Summary of the invention

[0010] The present invention discloses a method for the antimicrobial protection of leather in the post-tanning stage, comprising a biocidal composition and a luminescent additive allowing the identification of the biocidal composition. DETAILED DESCRIPTION

[0011] After the tanning step, the post-tanning step begins, consisting of fatliquoring, with the aim of avoiding cracking of the leather, making it soft, strong and flexible. This process consists of impregnating the leather with an emulsified oil which is deposited in the fibers of the leather, adhering to it and giving the desired finish. In fatliquoring, a distinction is made between simple fatliquoring, manual fatliquoring or barrel fatliquoring. Throughout this entire series of treatments, the amount of emulsified oil increases, thereby improving the water tightness and quality of the leather. In the development of this step, emulsified fatliquoring oils (mineral and vegetable) are required. As a result of this activity, there is a risk of potential oil spills.

[0012] The present invention modifies this post-tanning step by incorporating an additional step that incorporates a biocidal composition for disinfecting and protecting the leather that has been tanned, thereby blocking the spread of diseases caused by microbial pathogens for a longer period of time than conventional methods, the composition comprising: between 3% and 5% silver phosphate glass; between 1% and 3.5% silicone; between 0.1% and 0.30% aliphatic hydrocarbons; between 90% and 95% water. This composition is added during the tanning process in an amount between 0.1% and 5% of the weight of the material to be tanned. The biocidal composition provides a sufficient amount of silver ions to maintain the biocidal effect of the Ag(+) ions throughout the useful life of the material after tanning.

[0013] The amount of composition used is estimated to be between 0.5% and 1.0% (always with respect to the weight of the leather to be treated in the process), which will be sufficient for the composition to achieve its antimicrobial function.

[0014] Furthermore, in the post-tanning stage, a luminescent additive is incorporated to indicate that the skin has been previously treated with a biocidal composition. A luminescent additive formed by metal oxides (aluminosilicate glass containing rare earth ions, by means of a dopant) is incorporated into the biocidal composition, which allows the detection and identification of the coating of said composition by infrared light inducing an easily detectable luminescence (green light). This luminescent additive presents a codable emission light pattern that allows the compound to be unavoidably identified, thus proving its authenticity, which distinguishes it with respect to other similar products on the market.

[0015] The luminescent additive acting as a marker allowing the identification of the biocidal composition comprises between 20% and 40% of silicon dioxide and between 10% and 30% of aluminum oxide and between 30% and 50% by weight of calcium fluoride. Materials doped with luminescent "rare earth" ions are added to this mixture, such as between 0.5% and 3% of erbium (III) fluoride; between 5% and 15% of ytterbium (III) fluoride; a maximum of 5% of thulium (III) fluoride; and a maximum of 5% of europium (III) fluoride. All these percentages are with respect to the total weight of the luminescent additive.

[0016] Silicon dioxide is used as luminescent coatings, i.e. they do not involve heat generation, and are particularly useful in the main physical phenomena that allow the generation of light with characteristics such as phosphorescence and fluorescence. In addition, it is used as an insulating coating, forming a thin layer similar to a laminate on the coated surface, protecting and preserving the surface from the action of water, from scratches or other wear damage. Aluminum oxide is used as a selective adsorbent, allowing the level of fluoride in the mixture to be adjusted downward.

[0017] Calcium fluoride significantly increases its fluorescence, with a broad emission that occurs within an acceptable target range. The optically active compound of the additive is formed by a luminescent "rare earth" ion. Ytterbium fluoride increases the absorption of infrared light and the subsequent conversion to visible light by the remaining luminescent elements in the marker composition (erbium fluoride, thulium fluoride and europium fluoride). Erbium-doped silica glass fibers are active elements that amplify the luminescence effect, and in addition, their homogenization is increased due to the presence of aluminum oxide. Ytterbium fluoride also increases the amplification of the material as a luminescent marker, and thulium (III) fluoride is used to improve the up-conversion fluorescence from infrared to ultraviolet and visible in fluoride glass. Europium fluorescence is used to improve the emission color coding effect of the marking additive.

[0018] During the tanning process, the luminescent additive used as an identification marker for the biocidal composition is applied at between 0.1% and 5% by weight of the material treated.

[0019] This luminescent additive (visible only under IR excitation) is formulated to be integrated into the formulation of the material being treated and acts as a marker when illuminated by IR light in the 900 to 990 nanometer range.

[0020] Different tests have established that the luminescent additive of the product presents emission only under invisible infrared light with high intensity brightness, due to the lack of background noise due to zero autofluorescence of the fabric matrix or the surface to which it has been applied. Furthermore, the luminescence intensity ratio between the different visible emission bands (blue, green and red) observed after the conversion of the invisible infrared reading light can be adjusted as desired (by varying the concentration level and type of dopant "rare earth" ions). In other words, by designing and synthesizing on demand at the source, the emitted light is encoded with an irrefutable code, providing a novel and disruptive proof of concept for optical cryptographic security mode.

[0021] The tests applied to the samples during the tanning process are:

[0022] ASTM E2149-20: Standard Test Method for Determining the Activity of Immobilized Antimicrobials under Dynamic Contact Conditions.

[0023] - UNE-EN ISO 18184 - Test methods for determining the antiviral activity of products against specific viruses.

[0024] Biocidal protection of surfaces has been determined to be 12 to 18 months, so leather can be protected for a long time in one application. The product has effective bactericidal protection against various microorganisms such as Escherichia coli, Staphylococcus aureus, Enterococcus aeruginosa, Pseudomonas aeruginosa, Candida albicans and some types of viruses with or without outer packaging.

[0025] As an added value, the luminescence feature of the present invention clearly distinguishes the present invention with respect to the prior art, as it allows the user to visualize where the product is applied and to identify the coded light pattern to indicate that the product is original. A simple and compact portable handheld device (pocket spectrometer / App for smartphone camera) will allow the end user to detect the coded luminescence pattern by illuminating it with a low-cost commercial infrared laser pointer, thus verifying that the applied product is protected with the original biocidal composition. This luminescence technology using infrared light and color coding using "rare earth" ions is at the forefront of anti-counterfeiting light technology, in the line of technology for secure encryption of certification documents (passports, security inks) and for legal tender banknotes. Therefore, its application in the original identification of biocidal composition products undoubtedly constitutes an absolute novelty, which defines a clear and significant difference from other products with similar characteristics on the market. The biocidal product is formulated in an aqueous matrix, so a good drying time is obtained, ranging from 2 to 3 minutes. The product is easy to apply. Using an atomizer, it allows to be effectively applied on the surface with the help of a cloth.

Claims

1. An antimicrobial protection in the post-tanning stage of leather by combining a biocidal composition and a luminescent additive, characterized in that In a post-tanning step of the leather, a biocidal composition is added in an amount between 0.1% and 5% by weight of the material to be tanned, the biocidal composition comprising: between 3% and 5% silver phosphate glass; between 1% and 3.5% silicone; between 0.1% and 0.30% aliphatic hydrocarbons; between 90% and 95% water, and a luminescent additive is added in an amount between 0.1% and 5% by weight of the material to be tanned, the luminescent additive comprising between 20% and 40% silicon dioxide relative to the total weight of the luminescent additive; aluminum oxide in a proportion between 10% and 30%; calcium fluoride between 30% and 50%; erbium (III) fluoride between 0.5% and 3%; ytterbium (III) fluoride between 5% and 15%; a maximum of 5% thulium (III) fluoride; and a maximum of 5% europium (III) fluoride.

2. Antimicrobial protection in the post-tanning stage of leather by combining a biocidal composition and a luminescent additive according to claim 1, characterized in that The luminescent additive acts as a marker when illuminated by IR light in the range of 900 to 990 nanometers.