Riser improvement structure of cylinder sleeve casting and pouring system and pouring method
By using the combined technology of wedge blocks and heating insulation plates in cylinder liner casting, the problems of molten iron temperature control and casting shape in large cylinder liner casting are solved, achieving high-quality output of castings and easy operation.
Patent Information
- Application Number
- CN202411003254.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-25
- Publication Date
- 2024-10-15
AI Technical Summary
During the casting process of large cylinder liners, it is difficult to maintain the molten iron temperature in compliance with the existing technology, resulting in shrinkage and loosening of the upper part of the casting, uneven appearance, and unclear outline. Moreover, the flat and vertical pouring method is difficult to apply to the casting of large parts.
The cylinder liner casting pouring system riser is used to improve the structure and method. By arranging wedge blocks and heating insulation plates in the sand box, it is ensured that the core does not shift during the vertical placement process, and the heating insulation plates are used to generate heat to prevent the upper part of the casting from shrinking. loose to achieve the flatness of the casting shape and the integrity of the contour.
It effectively prevents shrinkage in the upper part of the casting, ensures the smooth appearance and clear and complete outline of the casting, improves the quality of the casting, simplifies the process operation, and reduces the difficulty for workers to repair the sand mold.
Smart Images

Figure CN118768519A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of cylinder liner casting, in particular to an improved riser structure and a casting method of a cylinder liner casting pouring system. Background Art
[0002] In the casting process of large cylinder liners, the vertical casting process is generally adopted, that is, the core is hoisted onto the bottom box by hoisting, and then the sand box with a horizontal parting surface is sequentially inserted into the outside of the core, and finally the sand box is fixed by screws to form a whole. However, this method is complicated to operate and it is difficult for workers to repair the sand mold.
[0003] At present, there is no related document of adopting the casting method of flat making and vertical pouring to cast large cylinder sleeves and the open literature of casting sand mold adopting the casting method of flat making and vertical pouring to be retrieved.
[0004] In addition, during the casting process, the temperature of the molten iron gradually decreases from the bottom to the top, causing shrinkage and loosening of the upper part of the casting; the molten iron splashes on the inner wall of the core, causing the casting to have an uneven shape and unclear and incomplete contours. Therefore, how to keep the temperature of the molten iron in the casting process in accordance with the requirements, ensure that the shape of the casting is flat, the contour is clear and complete, and cast a high-density, high-quality cylinder head casting has become a technical problem that the applicant is committed to solving. Summary of the invention
[0005] The present invention aims to overcome the above-mentioned technical defects and provide an improved riser structure and a pouring method for a cylinder liner casting pouring system, which can ensure that the core will not be displaced or sink in the process of changing from a horizontal state to a vertical state in the sand box, thereby ensuring the casting quality; preventing the upper part of the casting from shrinking and loosening, achieving a shrinkage compensation effect, and ensuring that the casting has a smooth appearance and a clear and complete contour.
[0006] In order to achieve some or all of the above-mentioned purposes or other purposes, the present application provides the following technical solutions: an improved structure of the riser of the cylinder liner casting pouring system, including a first sand box and a second sand box; a first sand core is arranged in the first sand box, and a second sand core is arranged in the second sand box; the first sand box and the second sand box are molded together to form a molded sand box, and the first sand core and the second sand core are molded together to form a molded sand core; a core is arranged in the inner cavity of the molded sand core, and a cavity to be poured is formed between the molded sand core and the core.
[0007] Furthermore, the mold cavity is divided into a casting mold cavity and a riser mold cavity, and a heating and heat preservation plate is arranged on the outer peripheral surface of the riser mold cavity.
[0008] Furthermore, the mold cavity is divided into a casting mold cavity and a riser mold cavity, and the heating and insulation plate is fixedly connected to the first sand core and the second sand core.
[0009] Furthermore, the core comprises a first core head, a riser core and a casting core; the diameter of the connection between the first core head and the riser core is larger than the diameter of the connection between the riser core and the casting core.
[0010] Furthermore, a pouring system is also arranged in the mold sand box; the pouring system includes a straight runner, a cross runner and an ingrown runner; the straight runner is connected to the cross runner, the cross runner is connected to the ingrown runner, the ingrown runner is arranged on the plane where the connection part of the first core head and the riser core is located, and the ingrown runner is connected to the riser cavity.
[0011] Furthermore, a wedge block is also arranged in the mold sand box, and the wedge block is located between the inner wall of the first sand box and the core, the straight edge of the wedge block is against the inner wall of the first sand box, and the oblique edge of the wedge block is against the core; there is at least one wedge block; the core also includes a second core head; the core is composed of a core bone and molding sand, the molding sand is wrapped around the core bone, and one end of the core bone is against the oblique edge of the wedge block.
[0012] Furthermore, a casting method for a cylinder liner casting pouring system riser improved structure is characterized by comprising the following steps: Step 1: Make a casting profile with a riser according to the manufacturing specifications, and prefabricate a loose block that matches the casting profile; Step 2: placing the casting copy and the movable block into the second sand box, setting the movable block at the sealing position of the second core head, and sand-blasting and shaping to form a second sand core in the second sand box; wherein the casting copy and the movable block are both wooden models; Step 3: demolding, pulling out the casting profiling and the live block, the cavity formed by the casting profiling in the second sand box is the second mold cavity, the cavity formed by the live block in the sand box is the operating cavity, and the operating cavity is located in the second sand box; Step 4: making a first sand core to be set in the first sand box, making a wedge-shaped block profile, placing the casting profile and the wedge-shaped block profile into the first sand box, blasting and shaping, and forming the first sand core in the first sand box; Step 5, demolding, shaping the casting and the wedge block, the cavity formed by the shaping of the casting in the first sand box is the first cavity, and the cavity formed by the shaping of the wedge block in the first sand box is used to place the wedge block; Step 6, assembling the core in the first cavity of the first sand box, positioning the cavity through the first core head and the second core head, placing the wedge block between the core bone and the first sand box, so that the wedge block is respectively against the core bone and the inner wall of the first sand box; one end of the core bone is exposed outside the sand mold, and the other end of the core bone extends to the first core head of the core, and the first core head of the core matches the core of the casting system; when the wedge block is placed in the sand box and contacts with the core bone, the inclined surface of the wedge block can fix the integral core and the sand box tightly together without loosening; Step 7: Cover the exposed core bone and wedge block with molding sand; the purpose of this step is to prevent the core bone or wedge block from contacting with molten iron to prevent affecting the quality of the casting. At the same time, this process can make the wedge block full of sand, fix the position of the wedge block, and avoid relative displacement between the wedge block and the sand box or core bone during the vertical placement of the sand box; Step 8: Place the second sand box with the second sand core on the first sand box, close the boxes, and fix the sand box with fastening bolts; this process can ensure that the first sand box and the second sand box will not be misplaced or separated when the sand box is placed from horizontal to vertical; Step nine, sealing the gap between the second core head and the mold cavity through the operating cavity of the second sand box, and filling the operating cavity with molding sand; Step 10, vertically place the assembled sand box so that the outer wall of the sand box close to the wedge block is close to the ground; during the vertical placement process, the sand box can provide support for the wedge block, the wedge block can provide support for the core bone, and the core bone can ensure that the entire core will not be displaced, so that the position of the internal structure of the entire sand box will not be offset during the vertical placement process; Step 11, pouring molten iron; if you want to realize large cylinder liner casting by the horizontal casting and vertical casting method, you need to put the core into two sand boxes and combine them, and then change the combined sand boxes from a horizontal state to a vertical state. In this process, the gravity direction of the core inside the sand box changes, which will inevitably cause changes in the composition of various parts inside the sand box. Therefore, for the casting of small and medium-sized parts, the gravity change in the process of changing the sand box from a horizontal state to a vertical state has little effect on the sand mold inside the sand box, and the horizontal casting and vertical casting method is feasible. However, for the casting of large parts, the positions of the sand mold and the core inside the sand box will be greatly offset in the process of changing the sand box from a horizontal state to a vertical state, which will change the structure of the cavity formed by the sand mold and the core, and the ideal parts cannot be obtained by pouring molten iron. Therefore, in the casting process of large cylinder liners, the horizontal casting and vertical casting process cannot be used; Step 12: Cool, take out the cast casting, and cut off the riser part; the riser part contains impurities generated by the chemical reaction of the heating and insulation board.
[0013] Furthermore, the wedge block is fixedly connected to the side wall of the sand box by bolts. After the wedge block completely fixes the core bone, it is connected to the sand box by bolts, and no vibration or deformation will occur during the erection process.
[0014] Furthermore, the mold cavity is divided into a casting mold cavity and a riser mold cavity, and a heating and insulation plate is arranged on the outer peripheral surface of the riser mold cavity; the step three also includes setting a heating and insulation plate near the riser mold cavity of the second sand core; the step five also includes setting a heating and insulation plate near the riser mold cavity of the first sand core.
[0015] The preparation and use of the active block in step 2 can be obtained by the method described in Chinese invention CN 117047031 A.
[0016] Compared with the prior art, the beneficial effects of the present invention are as follows: by placing a wedge block between the core bone and the sand box, the core is prevented from moving up and down during the vertical placement of the sand box after the box is assembled, and by setting the core head, the core is prevented from moving left and right. Therefore, the technical solution is simple to operate and has a clever design. It can ensure that the cylinder liner is manufactured using the flat-making and vertical pouring process. When the sand box is placed vertically after the box is assembled, the core will not be displaced laterally or longitudinally due to the action of gravity, thereby ensuring the quality of the casting formed by the casting.
[0017] When molten iron flows into the mold cavity from the inner runner, it will not scour the outer wall of the casting core, ensuring that the casting has a flat appearance, clear and complete contours, achieving sequential solidification, and improving the quality of the casting; during the casting pouring process, the molten iron that flows from the bottom to the riser reacts with the heating and insulation plate to generate heat, which is transferred to the position of the casting through the molten iron, preventing the upper part of the casting from shrinking and achieving a shrinkage compensation effect. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 It is a structural schematic diagram of the present invention; Figure 2 It is a schematic diagram of AA; Figure 3 It is a schematic diagram of BB; Figure 4 It is a schematic diagram of the structure after the wedge block and the core are placed in the first sand core; Figure 5 This is a schematic diagram after mold closing; Figure 6 for Figure 4 Schematic cross section; Figure 7 It is a schematic diagram of the wedge block structure; Figure 8 This is a schematic diagram of the structure of placing two wedge blocks in the first sand core.
[0019] In the figure: 1. core bone; 2. molding sand; 3. wedge block; 3.1. straight edge of wedge block; 3.2. oblique edge of wedge block; 4. first sand core; 5. second sand core; 6.1. riser cavity; 6.2. casting cavity; 7. movable block; 8. first core head; 9. second core head; 10. sprue; 11. horizontal runner; 12. inner runner; 13. heating and insulation board. DETAILED DESCRIPTION
[0020] In order to make the structure and function of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the accompanying drawings in the embodiments of the present invention.
[0021] Example 1 refer to Figure 1-Figure 6 The improved riser structure of the cylinder liner casting pouring system includes a first sand box and a second sand box; a first sand core 4 is arranged in the first sand box, and a second sand core 5 is arranged in the second sand box; the first sand box and the second sand box are molded together to form a molded sand box, and the first sand core 4 and the second sand core 5 are molded together to form a molded sand core; a core is arranged in the inner cavity of the molded sand core, and a cavity to be poured is formed between the molded sand core and the core.
[0022] Furthermore, the cavity is divided into a casting cavity 6.2 and a riser cavity 6.1, and a heating and insulation plate 13 is arranged on the outer peripheral surface of the riser cavity 6.1; the heating and insulation plate 13 is mainly composed of aluminum oxide, and the reaction equation of aluminum oxide and iron is: 2Al2O3+Fe→2FeO+3Al, and the reaction of aluminum oxide and iron releases heat; the heating and insulation plate 13 is arranged on the outer peripheral surface of the riser cavity 6.1, and during the casting process, the temperature of the molten iron from the bottom to the top gradually decreases, and the molten iron reaching the riser reacts with the heating and insulation plate 13 to generate heat, and the heat is transferred to the position of the casting through the molten iron, so that the upper part of the casting does not shrink and the shrinkage compensation effect is achieved.
[0023] Furthermore, the heating and heat-insulating plate 13 is fixedly connected to the first sand core 4 and the second sand core 5 .
[0024] Furthermore, the core includes a first core head 8, a riser core and a casting core; the diameter of the connection between the first core head 8 and the riser core is larger than the diameter of the connection between the riser core and the casting core; when molten iron flows into the mold cavity from the ingrowth 12, the molten iron will flow downward from the mold cavity. Since the diameter of the casting core is smaller than the diameter of the mold cavity at the outlet of the ingrowth 12, the molten iron will not flow downward along the outer wall of the casting core, and will not scour the outer wall of the casting core, thereby ensuring that the shape of the casting is smooth, the contour is clear and complete, achieving sequential solidification, and improving the quality of the casting.
[0025] Furthermore, a pouring system is also arranged in the mold sand box; the pouring system includes a straight runner 10, a cross runner 11 and an ingode 12; the straight runner 10 is connected to the cross runner 11, the cross runner 11 is connected to the ingode 12, the ingode 12 is arranged on the plane where the connection part of the first core head 8 and the riser core is located, and the ingode 12 is connected to the riser cavity 6.1.
[0026] Furthermore, a wedge block 3 is also arranged in the mold sand box, and the wedge block 3 is located between the inner wall of the first sand box and the core, the straight edge 3.1 of the wedge block is against the inner wall of the first sand box, and the oblique edge 3.2 of the wedge block is against the core; there is at least one wedge block 3; the core also includes a second core head 9; the core is composed of a core frame 1 and molding sand 2, the molding sand 2 is wrapped outside the core frame 1, and one end of the core frame 1 is against the oblique edge 3.2 of the wedge block.
[0027] Furthermore, a casting method for a cylinder liner casting pouring system riser improved structure is characterized by comprising the following steps: Step 1: Make a casting profile with a riser portion according to the manufacturing specification, and prefabricate a movable block 7 that matches the casting profile; the movable block 7 has an arc-shaped matching surface that contacts the casting profile to ensure that the movable block 7 can be stably placed; Step 2: Put the casting profiling and the movable block 7 into the second sand box, set the movable block 7 at the sealing position of the second core head 9, and sandblast to shape it, so as to form the second sand core 5 in the second sand box; this process can locate the core head sealing position in advance, and ensure that the core head sealing operation can be completed after demolding; Step 3: Demolding, pull out the casting profiling and the movable block 7, the cavity formed by the casting profiling in the second sand box is the second mold cavity, and the cavity formed by the movable block 7 in the sand box is the operating cavity, and the operating cavity is located in the second sand box; Step 4: prepare the first sand core 4 set in the first sand box, prepare the wedge-shaped block 3, put the molded casting and the wedge-shaped block 3 into the first sand box, and blast the sand to shape them, so as to form the first sand core 4 in the first sand box; Step 5, demolding, shaping the casting and the wedge block 3, the cavity formed by the casting shaping in the first sand box is the first cavity, and the cavity formed by the wedge block 3 shaping in the first sand box is used to place the wedge block 3; since the gap between the first sand box 4 and the second core head 9 can be directly sealed, it is not necessary to place the loose block 7 in the first sand box; Step 6: assemble the core into the first cavity of the first sand box, position the cavity by the first core head 8 and the second core head 9, place the wedge block 3 between the core bone 1 and the first sand box, so that the wedge block 3 is respectively against the core bone 1 and the inner wall of the first sand box; when the core is placed in the first sand box, the core head part has the function of supporting the core; Step 7: Cover the exposed core bone 1 and wedge block 3 with molding sand; the purpose of this step is to prevent the core bone 1 or wedge block 3 from contacting with molten iron to prevent affecting the quality of the casting. At the same time, this process can make the wedge block 3 covered with sand, fix the position of the wedge block 3, and avoid relative displacement between the wedge block 3 and the sand box or core bone 1 during the vertical placement of the sand box; Based on the above process, the operator can perform a sealing operation on the first sand box by wrapping the molding sand around the core and the wedge block 3 with hands or other tools. The sealing process is simple and can ensure the shape of the cavity and improve the casting quality. Step 8: Place the second sand box with the second sand core 5 on the first sand box, close the boxes, and fix the sand box with fastening bolts; this process can ensure that the first sand box and the second sand box will not be misplaced or separated when the sand box is placed from horizontal to vertical; Step 9: Seal the gap between the second core head 9 and the mold cavity through the operating cavity of the second sand box, and fill the operating cavity with molding sand; Step 10, vertically place the assembled sand box so that the outer wall of the sand box close to the wedge block 3 is close to the ground; during the vertical placement process, the sand box can provide support for the wedge block 3, the wedge block 3 can provide support for the core bone 1, and the core bone 1 can ensure that the entire core will not be displaced, so that the position of the internal structure of the entire sand box will not be offset during the vertical placement process; Step 11, pouring molten iron; Step 12: Cool, take out the poured casting, and cut off the riser part.
[0028] Furthermore, the step three also includes setting a heating and insulation plate at the second sand core near the riser cavity; the step five also includes setting a heating and insulation plate at the first sand core near the riser cavity.
[0029] Furthermore, the wedge block 3 can also be fixedly connected to the side wall of the sand box by bolts. For the present invention, the straight edge 3.1 of the wedge block is directly in contact with the first sand box 4. It is only necessary to ensure that the relative position of the wedge block 3.1 and the first sand box 4 is fixed to ensure that the wedge block 3 will not move. The present invention uses a sand mold to fix the wedge block 3. In addition to the straight edge 3.1 of the wedge block in contact with the first sand box 4, the oblique edge 3.2 of the wedge block is in contact with the core bone 1, and the rest of the wedge block 3 is fixed by the sand mold. In the process of changing from horizontal placement to vertical placement, the wedge block will only be subjected to the force applied by the core bone. Since the sand mold can support the wedge block, the wedge block will not move, and it can be ensured that the core bone 1 will not move, so that the core and the sand mold will not change in structure or position during the horizontal casting process, thereby improving the casting quality.
[0030] The use of the flat casting and vertical pouring method as described in the present application can greatly reduce the difficulty of workers in trimming the sand mold, while ensuring that the gravity direction inside the sand box will not change during the upright process of the sand box, the core will not sink or deflect, and the quality of the cylinder liner formed by casting is improved.
[0031] Example 2 refer to Figure 8 Embodiment 2 adds a wedge block on the basis of Embodiment 1 to make the sand box more stable during the process of changing from a horizontal placement state to a vertical placement state. The rest of the technical solutions are the same as those of Embodiment 1.
[0032] It should be noted that the parts not described in detail in the present invention are prior art.
[0033] The above disclosure is only the preferred embodiment of the present application, which certainly cannot be used to limit the scope of rights of the present application. Therefore, equivalent changes made according to the claims of the present application are still within the scope covered by the present application.
Claims
1. Improved riser structure of cylinder liner casting pouring system. Features: It includes a first sand box and a second sand box; a first sand core is arranged in the first sand box, and a second sand core is arranged in the second sand box; the first sand box and the second sand box are molded together to form a molded sand box, and the first sand core and the second sand core are molded together to form a molded sand core; a core is arranged in the inner cavity of the molded sand core, and a cavity to be poured is formed between the molded sand core and the core.
2. The improved riser structure of the cylinder liner casting pouring system according to claim 1, Features: The mold cavity is divided into a casting mold cavity and a riser mold cavity, and a heating and heat preservation plate is arranged on the outer peripheral surface of the riser mold cavity.
3. The improved riser structure of the cylinder liner casting pouring system according to claim 2, Features: The heating and heat-insulating plate is fixedly connected to the first sand core and the second sand core.
4. The improved riser structure of the cylinder liner casting pouring system according to claim 1, Features: The core comprises a first core head, a riser core and a casting core; the diameter of the connection between the first core head and the riser core is larger than the diameter of the connection between the riser core and the casting core.
5. The improved riser structure of the cylinder liner casting pouring system according to claim 4, Features: A pouring system is also arranged in the mold sand box; the pouring system includes a straight runner, a cross runner and an ingrate; the straight runner is connected to the cross runner, the cross runner is connected to the ingrate, the ingrate is arranged on the plane where the connection part of the first core head and the riser core is located, and the ingrate is connected to the riser cavity.
6. The improved riser structure of the cylinder liner casting pouring system according to claim 1, Features: A wedge block is also arranged in the mold sand box, and the wedge block is located between the inner wall of the first sand box and the core, the straight edge of the wedge block is against the inner wall of the first sand box, and the oblique edge of the wedge block is against the core; there is at least one wedge block; the core also includes a second core head; the core is composed of a core bone and molding sand, the molding sand is wrapped outside the core bone, and one end of the core bone is against the oblique edge of the wedge block.
7. A casting method using the cylinder liner casting pouring system riser improved structure of claim 6, It is characterized in that The following steps are involved: Step 1: Make a casting profiling with a riser portion according to the production specifications, and prefabricate a live block that matches the casting profiling; Step 2: Put the casting profiling and the live block into the second sand box, the live block is set at the sealing part of the second core head, and the sand is blasted to finalize the shape, so as to form a second sand core in the second sand box; Step 3: Demolding: pull out the casting profiling and the live block, the cavity formed by the casting profiling in the second sand box is the second cavity, and the cavity formed by the live block in the sand box is the operating cavity, and the operating cavity is located in the second sand box; Step 4: Make a first sand core set in the first sand box, make a wedge-shaped block profiling, put the casting profiling and the wedge-shaped block profiling into the first sand box, and sand is blasted to finalize the shape, so as to form a first sand core in the first sand box; Step 5: Demolding: make the casting profiling and the wedge-shaped block profiling, the cavity formed by the casting profiling in the first sand box is the first cavity, and the cavity formed by the wedge-shaped block profiling in the first sand box is used to place the wedge-shaped block; Step 6, assemble the core into the first cavity of the first sand box, locate the cavity by the first core head and the second core head, place the wedge block between the core bone and the first sand box, and make the wedge block respectively abut against the core bone and the inner wall of the first sand box; Step 7, cover the exposed core bone and the outside of the wedge block with molding sand; Step 8, place the second sand box with the second sand core on the first sand box, close the box, and fix the sand box with fastening bolts; Step 9, seal the gap between the second core head and the cavity through the operating cavity of the second sand box, and fill the operating cavity with molding sand; Step 10, place the closed sand box vertically, so that the outer wall of the sand box close to the wedge block is close to the ground; Step 11, pour molten iron; Step 12: Cool, take out the poured casting, and cut off the riser part.
8. The pouring method of the cylinder liner casting pouring system riser improved structure according to claim 7, Features: The mold cavity is divided into a casting mold cavity and a riser mold cavity, and a heating and insulation plate is arranged on the outer peripheral surface of the riser mold cavity; the step three also includes arranging a heating and insulation plate near the riser mold cavity on the second sand core; the step five also includes arranging a heating and insulation plate near the riser mold cavity on the first sand core.
9. The pouring method of the cylinder liner casting pouring system riser improved structure according to claim 7, Features: A heating and insulation plate is arranged on the outer peripheral surface of the riser core; a heating and insulation plate is arranged at the riser core; in step six, the core with the heating and insulation plate fixed is assembled in the first cavity of the first sand box, the cavity is positioned by the first core head and the second core head, and the wedge block is placed between the core bone and the first sand box, so that the wedge block is respectively against the core bone and the inner wall of the first sand box.
Citation Information
Patent Citations
Cutter tooth holder casting mold for crushing machines and horizontally molding-vertically pouring casting process for cutter tooth holders for crushing machines
CN102554138A
Method for preventing sand core head from rubbing against sand
CN108405806A
Sand mold structure for thin-wall casting and casting method
CN116079004A
Anti-run-out casting process
CN117047031A
Medium and high pressure water-cooling cylinder block casting mold
CN204449223U
Cited By
Casting method of one-piece bearing seat
CN120984843A