Method for correcting fixed weight deviation of cutting blank caused by abrasion of copper pipe of continuous casting crystallizer

Through the high-definition infrared sizing system and the copper tube steel passing correction model, the problem of slab weight deviation caused by the wear of the mold copper tube is solved, the yield rate and steel utilization rate of the continuous casting process are improved, and the waste of resources is reduced.

CN118768536AActive Publication Date: 2024-10-15HUNAN VALIN LIANYUAN IRON & STEEL CO LTD +1
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202410984298.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-22
Publication Date
2024-10-15
Estimated Expiration
2044-07-22

AI Technical Summary

Technical Problem

The existing technology fails to effectively consider the impact of the wear of the mold copper tube on the weight accuracy of the casting billet, resulting in weight deviation of the cutting billet, affecting the yield rate of the continuous casting process and the waste of steel materials.

Method used

The high-definition infrared fixed-length system is used to measure the fixed-length length of the cast slab, and a correction model for the amount of steel passed by the copper pipe is set to correct the impact of the wear of the copper pipes in different flows on the cutting fixed-length, and a hydraulic shearing device is used for cutting to achieve the fixed-length length. Accurate correction.

Benefits of technology

It effectively improves the pass rate after cutting the continuous casting billet, reduces the cutting loss of the cast billet, improves the overall yield rate of the continuous casting process, and reduces the waste of steel materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118768536A_ABST
    Figure CN118768536A_ABST
Patent Text Reader

Abstract

The invention provides a correction method for cutting blank constant weight deviation caused by continuous casting crystallizer copper pipe abrasion. The correction method comprises the following steps that firstly, before casting, crystallizer copper pipe replacement information of all flows of a casting machine is checked; 2, steel passing amount data of the crystallizer copper pipe of each flow are accumulated according to the actual steel passing amount in the casting process; thirdly, a steel passing amount correction model is arranged to correct the cutting fixed length of the casting blank; fourthly, the fixed length of the casting blank is measured through a high-definition infrared fixed-length system in the intelligent cutting system, and cutting is conducted through a shearing device; and 5, after each flow of casting blank is cut in a fixed-length mode, online weighing is conducted, the weight is compared with the preset weight, and the follow-up casting blank fixed-length length is fed back and corrected. According to the method, the copper pipe steel passing amount correction model is used for correcting the influence of copper pipe steel passing abrasion of different flows on cutting weight fixing, the percent of pass after continuous casting blank cutting is effectively increased, casting blank cutting loss is reduced, and the overall yield in the continuous casting process is increased.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of continuous casting billet fixed weight and fixed length control, and in particular to a method for correcting the deviation of cut billet fixed weight caused by the wear of the copper tube of the continuous casting crystallizer. Background Art

[0002] The sizing technology of ingot is a technology that cuts the continuous and uninterrupted steel ingot into a fixed length online. It is the last indispensable process of continuous casting production. The cross-sectional specifications of wide and thick plate ingots are about (200-300) mm × (1500-2200) mm. The cross-sectional specifications of ingots are large. According to calculations, if the sizing accuracy of the ingot length direction fluctuates between 20 and 60 mm, the mass of the ingot after sizing will fluctuate by 40 to 300 kg. The quality fluctuation is large. If the sizing of wide and thick plate ingots is inaccurate, it will cause a lot of waste of steel materials.

[0003] The prior art technology for improving the sizing accuracy is to detect the distance between the end of the ingot and the cutting device through infrared rays, encoders, laser rays and other devices, and if the distance is equal to the sizing distance, cutting is performed. However, these technologies all improve the sizing accuracy from the perspective of improving the measurement accuracy of the sizing distance, and do not consider the impact of the wear of the inner cavity of the crystallizer copper tube on the sizing accuracy.

[0004] During the continuous casting and steel drawing process, there is friction between the inner cavity of the copper tube of the crystallizer and the shell of the continuous casting billet. The friction between the inner cavity of the copper tube and the shell of the casting billet causes the inner cavity of the copper tube to wear continuously, thereby causing changes in the shape and section surface of the inner cavity of the copper tube of the crystallizer. The copper tube of the crystallizer of the continuous casting machine is in different steel-passing cycles, which directly affects the degree of wear of the inner cavity of the copper tube, and has a great impact on the stability of the billet weight through cross-sectional changes. The steel rolling process requires that the weight of a single billet is as stable as possible. The huge deviation of the billet weight brings great difficulties to the control of the sizing rate and yield rate of the next process. It is urgent to take a measure to eliminate the impact of cross-sectional changes caused by the wear of the inner cavity of the copper tube.

[0005] Application Contents

[0006] The present application is made in view of the above-mentioned problems, and its purpose is to provide a method for correcting the deviation of the cut billet fixed weight caused by the wear of the copper tube of the continuous casting crystallizer. The fixed length of the billet is measured by a high-definition infrared sizing system, and a copper tube over-steel correction model is set to correct the influence of the copper tube over-steel wear of different flows on the cutting fixed weight, which effectively improves the qualified rate of the continuous casting billet after cutting, reduces the cutting loss of the billet, and improves the overall yield rate of the continuous casting process.

[0007] Specifically, a first aspect of the present application provides a method for correcting the deviation in the weight of cut billets caused by the wear of a continuous casting crystallizer copper tube, comprising the following steps:

[0008] Step 1: Before casting, check the replacement information of the copper tubes of the crystallizer of each stream of the casting machine, and preset the cut length and weight of the ingot;

[0009] The copper tube of the crystallizer is the core component of the continuous casting machine. It plays the role of solidifying and forming molten steel. The quality of the copper tube of the crystallizer has a great impact not only on the output and quality of the ingot, but also on the service life of the copper tube itself. During the continuous casting process, the coating on the inner surface of the copper tube of the crystallizer is in contact with the high-temperature molten steel. It is subject to the combined effects of chemical corrosion, thermal erosion and friction between the molten steel and the shell of the ingot. The copper tube of the crystallizer is prone to thermal deformation and scratches on the surface coating, which affects the normal operation of the continuous casting machine, reduces the continuous casting efficiency, and deteriorates the quality of the ingot. Due to the different steel types of the ingot and the process parameters of the continuous casting machine, the service life of the copper tube of the crystallizer is also different.

[0010] Step 2: During the casting process, the data of the amount of steel passed through the copper tube of the crystallizer of each stream is accumulated according to the actual amount of steel passed through;

[0011] Step 3: Receive the oversteel data through the continuous casting billet fixed weight and fixed length intelligent cutting system, set the oversteel correction model to correct the billet cutting fixed length, the formula is as follows:

[0012] L=133-K*X 2 *10 -3 ;

[0013] Where: L: Corrected length of copper tube for excess steel, mm;

[0014] X: excess steel in copper tube, furnace; K: correction factor;

[0015] In this formula, the unit of the amount of steel flowing through the copper tube X is furnace, which is used to record how many furnaces of molten steel have flowed through the copper tube.

[0016] The main function of the six-strand roller scale is to accurately measure the weight and quantity of steel billets and finished rolled products. This weighing system is an online static weighing and metering system designed, manufactured and installed according to the on-site process, specifically for the special measurement requirements of steel companies for steel billets and finished rolled products during the production process.

[0017] The function of Jiayong's non-contact automatic sizing and positioning system is to use non-contact camera technology to achieve accurate measurement and positioning of plates in wide and thick plate continuous casting machines. The software automatically calculates the actual size of the plate by analyzing the image data captured by the camera, and makes corresponding adjustments and controls, thereby improving the automation level of the production process and the consistency of the product.

[0018] Step 4: measuring the fixed length of the ingot by the high-definition infrared fixed length system in the intelligent cutting system, and cutting by the shearing device when it is detected that the fixed length meets the corrected cutting fixed length;

[0019] Step 5: After each strand of ingot is cut to length, it is weighed online, compared with the preset weight and feedback is used to correct the subsequent ingot length.

[0020] Furthermore, the replacement information of the copper tube of the crystallizer of each stream of the casting machine is checked, specifically including: the steel passing amount data of the stream replaced with a new copper tube is entered as 0, the steel passing amount data of the copper tube subsequently used for maintenance due to an accident is entered according to the number of times before the line is offline, and no changes are made to the copper tubes that have not been replaced.

[0021] Furthermore, the preset cut length of the ingot is positively correlated with the set weight.

[0022] Furthermore, the steel passing data of the copper tube of the crystallizer of each flow is accumulated according to the actual steel passing amount, specifically including: when the flow operates normally, the steel passing data is automatically accumulated; when the flow fails or the flow is blocked as planned, the system monitors that the pulling speed of the flow is 0, and the steel passing amount of the flow is no longer accumulated.

[0023] Furthermore, the correction coefficient K has a value range of 0.35 to 0.6.

[0024] Furthermore, the value of the correction coefficient K shows a decreasing trend as the amount of excess steel increases.

[0025] The basis for selecting the value range is that the wear of the inner cavity of the copper tube during the steel pouring process does not change uniformly with the increase of the amount of steel passed. The real-time wear of the copper tube shows a downward trend with the increase of the amount of steel passed. The wear amount changes significantly every 70 to 100 furnaces of molten steel. The value of the correction coefficient is adjusted accordingly according to the change in wear amount.

[0026] Furthermore, the sizing error of the high-definition infrared sizing system is ±10 mm.

[0027] Furthermore, the shearing device is a hydraulic shearing device.

[0028] The hydraulic shearing device is a machine based on a hydraulic system. It uses a moving upper blade and a fixed lower blade, adopts a reasonable blade gap, and applies shearing force to metal plates of various thicknesses to break and separate the plates according to the required size. It is used for cold shearing of various shapes of steel sections and various metal structures to meet production needs.

[0029] In the second aspect, the present application also provides a computing device, which has the function of implementing the method described in the first aspect above. The beneficial effects can be found in the description of the first aspect, which will not be repeated here. The function can be implemented by hardware, or by executing the corresponding software implementation through hardware. The hardware or software includes one or more modules corresponding to the above functions. In one possible design, the structure of the device includes an acquisition module, a training module, and optionally, a construction module. These modules can implement the function of the training node in the method example of the first aspect above. Please refer to the detailed description in the method example for details, which will not be repeated here.

[0030] In the third aspect, the present application also provides a computing device, which is used to implement the functions of the method described in the first aspect above. The beneficial effects can be found in the description of the first aspect and will not be repeated here. The structure of the computing device includes a processor and a memory, and the memory is used to store instructions and / or data. The memory is coupled to the processor, and when the processor executes the program instructions stored in the memory, the function of the training node in the example of the first aspect above can be implemented. The structure of the computing device also includes a communication interface for communicating with other devices.

[0031] In a fourth aspect, the present application also provides a computer-readable storage medium, in which instructions are stored, and when the computer-readable storage medium is run on a computer, the computer executes the method in the above-mentioned first aspect and various possible designs of the first aspect.

[0032] In a fifth aspect, the present application also provides a computer program product comprising instructions, which, when executed on a computer, enables the computer to execute the method in the above-mentioned first aspect and various possible designs of the first aspect.

[0033] In a sixth aspect, the present application also provides a computing chip, which is connected to a memory, and the chip is used to read and execute a software program stored in the memory, and to execute the methods in the above-mentioned first aspect and various possible implementation methods of the first aspect. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] In order to more clearly illustrate the embodiments of the present drawings or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present drawings. For ordinary technicians in this field, other drawings can be obtained based on the structures shown in these drawings without paying any creative work.

[0035] Figure 1 A flowchart of a method for correcting the deviation in the weight of cut blanks caused by the wear of the copper tube of a continuous casting crystallizer;

[0036] Figure 2 This is a continuous casting data diagram without correction using the present invention;

[0037] Figure 3 The continuous casting data diagram after correction using the present invention;

[0038] Figure 4 This is a comparison chart of weight adjustment during experimental rolling of Ф28~Ф32 steel grades.

[0039] The purpose, features and advantages of this figure will be further described in conjunction with the embodiments with reference to the accompanying drawings. DETAILED DESCRIPTION

[0040] In order to make the purpose, technical solutions and advantages of the present application clearer, the present application is described and illustrated below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present application and are not intended to limit the present application. Based on the embodiments provided in the present application, all other embodiments obtained by ordinary technicians in the field without making creative work are within the scope of protection of the present application.

[0041] Obviously, the drawings described below are only some examples or embodiments of the present application. For ordinary technicians in this field, the present application can also be applied to other similar scenarios based on these drawings without creative work. In addition, it can also be understood that although the efforts made in this development process may be complicated and lengthy, for ordinary technicians in this field related to the content disclosed in this application, some changes in design, manufacturing or production based on the technical content disclosed in this application are just conventional technical means, and should not be understood as insufficient content disclosed in this application.

[0042] Unless otherwise specified, all embodiments and optional embodiments of the present application can be combined with each other to form a new technical solution.

[0043] Unless otherwise specified, all technical features and optional technical features of this application can be combined with each other to form a new technical solution.

[0044] If there is no special explanation, all steps of the present application can be performed sequentially or randomly, preferably sequentially. For example, the method includes steps (a) and (b), which means that the method may include steps (a) and (b) performed sequentially, or may include steps (b) and (a) performed sequentially. For example, the method may further include step (c), which means that step (c) may be added to the method in any order. For example, the method may include steps (a), (b) and (c), or may include steps (a), (c) and (b), or may include steps (c), (a) and (b), etc.

[0045] If there is no special explanation, the "include" and "comprising" mentioned in this application are open-ended or closed-ended. For example, the "include" and "comprising" may mean that other components not listed may also be included or only the listed components may be included or only the listed components may be included.

[0046] If not specifically stated, in this application, the term "or" is inclusive. For example, the phrase "A or B" means "A, B, or both A and B". More specifically, any of the following conditions satisfies the condition "A or B": A is true (or exists) and B is false (or does not exist); A is false (or does not exist) and B is true (or exists); or both A and B are true (or exist).

[0047] In order to better understand the solutions of the embodiments of the present application, some relevant terms and concepts that may be involved in the embodiments of the present application are first introduced below.

[0048] (1) Continuous casting: In the continuous casting process, continuous casting refers to continuous casting, that is, the process of converting molten metal into solid metal material through continuous pouring and cooling. Specifically, continuous casting is to pour the molten metal through a water-cooled crystallizer so that it gradually solidifies into a billet in the crystallizer, and then continuously pull it out from the bottom of the crystallizer to obtain the metal material of the desired shape and size after cooling. In the continuous casting process, the crystallizer is one of the key equipment, and its function is to make the molten metal form a certain shape and size during the cooling and solidification process. The crystallizer is usually made of copper or steel, and is equipped with a cooling water channel inside, and the metal is solidified by the action of cooling water.

[0049] like Figure 1 As shown, in this embodiment, a method for correcting the deviation of the cut blank weight caused by the wear of the copper tube of the continuous casting crystallizer includes the following steps:

[0050] Step 1: Before casting, check the replacement information of the copper tubes of the crystallizer of each stream of the casting machine, and preset the cut length and weight of the ingot;

[0051] The copper tube of the crystallizer is the core component of the continuous casting machine. It plays the role of solidifying and forming molten steel. The quality of the copper tube of the crystallizer has a great impact not only on the output and quality of the ingot, but also on the service life of the copper tube itself. During the continuous casting process, the coating on the inner surface of the copper tube of the crystallizer is in contact with the high-temperature molten steel. It is subject to the combined effects of chemical corrosion, thermal erosion and friction between the molten steel and the shell of the ingot. The copper tube of the crystallizer is prone to thermal deformation and scratches on the surface coating, which affects the normal operation of the continuous casting machine, reduces the continuous casting efficiency, and deteriorates the quality of the ingot. Due to the different steel types of the ingot and the process parameters of the continuous casting machine, the service life of the copper tube of the crystallizer is also different.

[0052] Step 2: During the casting process, the data of the amount of steel passed through the copper tube of the crystallizer of each stream is accumulated according to the actual amount of steel passed through;

[0053] Step 3: Receive the oversteel data through the continuous casting billet fixed weight and fixed length intelligent cutting system, set the oversteel correction model to correct the billet cutting fixed length, the formula is as follows:

[0054] L=133-K*K 2 *10 -3 ;

[0055] Where: L: Corrected length of copper tube for excess steel, mm;

[0056] X: excess steel in copper tube, furnace; K: correction factor;

[0057] In this formula, the unit of the amount of steel flowing through the copper tube X is furnace, which is used to record how many furnaces of molten steel have flowed through the copper tube.

[0058] In this embodiment, the continuous casting billet fixed weight and fixed length intelligent cutting system used includes SCS-5t×6-GDC type six-stream roller scale and Jiayong non-contact automatic sizing and positioning system, and the Jiayong non-contact automatic sizing and positioning system includes a high-definition infrared sizing system and a shearing device.

[0059] The main function of the six-strand roller scale is to accurately measure the weight and quantity of steel billets and finished rolled products. This weighing system is an online static weighing and metering system designed, manufactured and installed according to the on-site process, specifically for the special measurement requirements of steel companies for steel billets and finished rolled products during the production process.

[0060] The function of Jiayong's non-contact automatic sizing and positioning system is to use non-contact camera technology to achieve accurate measurement and positioning of plates in wide and thick plate continuous casting machines. The software automatically calculates the actual size of the plate by analyzing the image data captured by the camera, and makes corresponding adjustments and controls, thereby improving the automation level of the production process and the consistency of the product.

[0061] Step 4: The high-definition infrared sizing system in the intelligent cutting system measures the slab length, and when it is detected that the slab length meets the corrected cutting length, the slab is cut by the shearing device;

[0062] Step 5: After each strand of ingot is cut to length, it is weighed online, compared with the preset weight and feedback is used to correct the subsequent ingot length.

[0063] In this embodiment, Figure 2-3 As shown in the figure, the fixed weight fine-tuning is the feedback correction of the subsequent fixed length of the billet. The fixed weight fine-tuning is calculated by subtracting the theoretical length from the actual length, which is used to fine-tune the fixed length of the billet.

[0064] Furthermore, the replacement information of the copper tube of the crystallizer of each stream of the casting machine is checked, including: the steel passing data of the stream for which the new copper tube is replaced is entered as 0, the steel passing data of the copper tube used subsequently after being taken offline for maintenance due to an accident is entered according to the number of times before the line was taken offline, and no changes are made to the copper tubes that have not been replaced.

[0065] Furthermore, there is a positive correlation between the preset cut length of the ingot and the set weight.

[0066] Furthermore, the data of the amount of steel passed through the copper tube of the crystallizer of each flow are accumulated according to the actual amount of steel passed, specifically including: when the flow operates normally, the steel passing data is automatically accumulated; when the flow fails or the flow is blocked as planned, the system monitors that the pulling speed of the flow is 0, and the steel passing amount of the flow is no longer accumulated.

[0067] Furthermore, the correction coefficient K ranges from 0.35 to 0.6.

[0068] Furthermore, the value of the correction coefficient K shows a downward trend with the increase of excess steel.

[0069] The basis for selecting the value range is that the wear of the inner cavity of the copper tube during the steel pouring process does not change uniformly with the increase of the amount of steel passed. The real-time wear of the copper tube shows a downward trend with the increase of the amount of steel passed. The wear amount changes significantly every 70 to 100 furnaces of molten steel. The value of the correction coefficient is adjusted accordingly according to the change in wear amount.

[0070] In this embodiment, the value of the correction coefficient K is shown in Table 1:

[0071] Table 1. The value of correction coefficient K varies with the amount of steel passed

[0072]

[0073]

[0074] The unit of the amount of steel X is furnace. In this embodiment, the weight of one furnace of molten steel is 100 tons.

[0075] Furthermore, the sizing error of the high-definition infrared sizing system is ±10mm.

[0076] Furthermore, the shearing device is a hydraulic shearing device.

[0077] The hydraulic shearing device is a machine based on a hydraulic system. It uses a moving upper blade and a fixed lower blade, adopts a reasonable blade gap, and applies shearing force to metal plates of various thicknesses to break and separate the plates according to the required size. It is used for cold shearing of various shapes of steel sections and various metal structures to meet production needs.

[0078] In this embodiment, Figure 2 As shown, when the correction method of the present invention is not used to correct the set weight deviation, the absolute values ​​of the deviations between the actual weights of 5 flows and the set weights are 10kg or more, and the absolute value of the maximum deviation reaches 29kg, resulting in a great waste of steel materials.

[0079] like Figure 3 As shown, after using the correction method of the present invention to correct the fixed weight deviation, only one flow has an absolute value of deviation between the actual weight and the set weight of more than 5kg, and the absolute value of the maximum deviation is 9kg, which greatly reduces the deviation rate and deviation degree.

[0080] When the correction method of the present invention is not used to correct the fixed weight deviation, the average qualified rate of the continuous casting process within the absolute value of the deviation of 5kg is only 21%, and the weight fluctuation of a single billet under fixed length control is large, which has a great impact on the subsequent rolling work.

[0081] In this embodiment, after using the correction method of the present invention to correct the fixed weight deviation, the total cutting count of the casting machine with casting machine number C3 is 19465, the weighing count is 19238, the count with the absolute value of deviation within 5kg is 16702, and the qualified rate is 86.82%; the count with the absolute value of deviation within 4kg is 14280, and the qualified rate is 74.23%; the count with the absolute value of deviation within 3kg is 11791, and the qualified rate is 61.29%; the count with the absolute value of deviation within 2kg is 9073, and the qualified rate is 47.16%.

[0082] After the correction method of the present invention is used to correct the fixed weight deviation, the qualified rate of the slabs in the fixed length and fixed weight process in the continuous casting work is greatly improved, the utilization rate of the steel is improved, and the waste of resources is reduced.

[0083] like Figure 4As shown, when the steel grades with specifications of Ф28 to Ф32 are tested for rolling, the weight adjustment distribution of the original fixed-length rolling method is shown as the red curve, and the weight adjustment distribution after using the correction method of the present invention is shown as the blue curve. The black solid line is the target weight, which is 2500kg; the red dotted line is the original weight setting value, which is 2530kg, and the margin is 30kg; the blue dotted line is the setting value after correction and optimization. After correction and optimization, the consistency of the weight of the ingot is improved, and the weight setting point moves left to 2520kg. On average, the cutting loss of each ingot is reduced by 10kg, and the non-size and cutting loss parts are more converted into fixed-length materials. 42 furnaces of steel grades were tested for rolling, and the average yield rate was increased by 0.58%.

[0084] It should be noted that the present application is not limited to the above-mentioned embodiments. The above-mentioned embodiments are only examples, and the embodiments having the same structure as the technical idea and exerting the same effect within the scope of the technical solution of the present application are all included in the technical scope of the present application. In addition, without departing from the scope of the main purpose of the present application, various modifications that can be thought of by those skilled in the art to the embodiments and other methods of combining some of the constituent elements in the embodiments are also included in the scope of the present application.

Claims

1. A method for correcting the deviation of the cut blank weight caused by the wear of the copper tube of the continuous casting crystallizer. It is characterized in that The following steps are involved: Step 1: Before casting, check the replacement information of the copper tubes of the crystallizer of each stream of the casting machine, and preset the cut length and weight of the ingot; Step 2: During the casting process, the data of the amount of steel passed through the copper tube of the crystallizer of each stream is accumulated according to the actual amount of steel passed through; Step 3: Receive the oversteel data through the continuous casting billet fixed weight and fixed length intelligent cutting system, set the oversteel correction model to correct the billet cutting fixed length, the formula is as follows: L=133-K*K 2 *10 -3 ; Where: L: Corrected length of copper tube for excess steel, mm; X: excess steel in copper tube, furnace; K: correction factor; Step 4: The high-definition infrared sizing system in the intelligent cutting system measures the slab length, and when it is detected that the slab length meets the corrected cutting length, the slab is cut by the shearing device; Step 5: After each strand of ingot is cut to length, it is weighed online, compared with the preset weight and feedback is used to correct the subsequent ingot length.

2. A method for correcting the deviation in the weight of cut blanks caused by the wear of the copper tube of the continuous casting crystallizer according to claim 1, It is characterized in that The replacement information of the copper tube of the crystallizer of each stream of the casting machine is checked, specifically including: the steel passing amount data of the stream for which the new copper tube is replaced is entered as 0, the steel passing amount data of the copper tube subsequently used for maintenance due to an accident is entered according to the number of times before the line was put into operation, and no changes are made to the copper tubes that have not been replaced.

3. The method for correcting the deviation of the cut blank weight caused by the wear of the copper tube of the continuous casting crystallizer according to claim 1, It is characterized in that The preset billet cutting length and the set weight are positively correlated.

4. The method for correcting the deviation of the cut blank weight caused by the wear of the copper tube of the continuous casting crystallizer according to claim 1, It is characterized in that The method of accumulating the steel passing data of the copper tube of the crystallizer of each flow according to the actual steel passing data specifically includes: automatically accumulating the steel passing data when the flow operates normally; when the flow fails or the flow is blocked as planned, the system monitors that the pulling speed of the flow is 0, and then no longer accumulates the steel passing data of the flow.

5. The method for correcting the deviation of the cut blank weight caused by the wear of the copper tube of the continuous casting crystallizer according to claim 1, It is characterized in that The correction coefficient K has a value range of 0.35 to 0.

6.

6. A method for correcting the deviation in the weight of cut blanks caused by the wear of the copper tube of the continuous casting crystallizer according to claim 5, It is characterized in that The value of the correction coefficient K shows a decreasing trend as the amount of excess steel increases.

7. The method for correcting the deviation of the cut blank weight caused by the wear of the copper tube of the continuous casting crystallizer according to claim 1, It is characterized in that The sizing error of the high-definition infrared sizing system is ±10 mm.

8. The method for correcting the deviation of the cut blank weight caused by the wear of the copper tube of the continuous casting crystallizer according to claim 1, It is characterized in that The shearing device is a hydraulic shearing device.

Citation Information

Patent Citations

  • Online sizing and weighing system for multi-flow multi-sizing continuous casting slab

    CN104117648A

  • On-line weighing, sizing and correcting method of continuous casting slab

    CN104325105A

  • Direct rolling continuous casting billet sizing dynamic adjusting method

    CN116967414A

  • Method for calculating corrected heating procedure in linear heating

    JP2006218486A

  • Casting piece production system and method

    JP2015058436A