Gluing machine for wood sheets

By using the combined structure of the lower rubber roller and the upper rubber roller and the auxiliary device in the wood thin plate glue coating machine, the problems of insufficient glue layer thickness and plate crushing during the double-sided glue coating process are solved, and the wood thin plate glue coating machine is realized. Efficient double-sided gluing and multi-layer solid wood board increase the strength.

CN118769335APending Publication Date: 2024-10-15JIANGSU CHAONENG NEW MATERIAL TECH CO LTD

Patent Information

Application Number
CN202411100232.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-12
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

Existing wood thin plate gluing equipment has problems such as insufficient glue layer thickness, excessive pressure, excessive temperature and prolonged production cycle during the double-sided gluing process. In addition, the straight lines of the glue roller can easily cause indentation and wear of the plate. Affect the glue coating effect.

Method used

A wood thin plate glue coating machine is designed, which adopts a combined structure of a lower rubber coating roller and an upper rubber coating roller, and uses devices such as a glue dripping pipe, a glue spray pipe, a rubber scraper, a glue brushing plate, and a lateral limit plate to realize the glue coating of wood thin plates. Glue is applied on both sides at the same time to improve the glue application efficiency and connection strength, and the design of the annular hose and roller avoids crushing of the plate and waste of glue.

Benefits of technology

It achieves uniform glue coating on both sides of wooden thin boards, improves the connection strength of multi-layer solid wood boards, reduces production costs and cycles, avoids waste of glue and environmental pollution, and extends the service life of the glue roller.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118769335A_ABST
    Figure CN118769335A_ABST
Patent Text Reader

Abstract

A base frame is sequentially provided with a feeding conveying roller, a glue coating roller set and a discharging conveying rod in the conveying direction of the wood sheets, the glue coating roller set comprises a lower glue coating roller and an upper glue coating roller which are arranged in parallel up and down, and a glue solution pool is arranged at the position, under the lower glue coating roller, of the base frame; a glue dripping pipe is arranged above the side, facing the feeding conveying roller, of the upper glue coating roller on the base frame, a glue solution pool conveys glue solution into the glue dripping pipe through a pump A, and the bottom of the lower glue coating roller is glued through the glue solution pool below the lower glue coating roller. According to the structure, according to the gluing machine for the wood sheet, the two side plate faces of the wood sheet can be glued at the same time under the action of the lower gluing roller and the upper gluing roller, the gluing efficiency can be improved, multiple layers of wood sheets can be more conveniently formed into multiple layers of solid wood boards through hot pressing of the wood sheets subjected to double-face gluing, and the gluing efficiency of the wood sheets is improved. And the connection strength of the multiple layers of solid wood boards is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of wood veneer gluing equipment, in particular to a wood veneer gluing machine. Background Art

[0002] Solid wood multilayer boards are made by hot pressing multiple layers of stacked wood veneers. Before hot pressing, each wood veneer needs to be coated with glue so that a uniform thin glue layer is formed on the surface of each wood veneer. At present, the gluing of wood veneers is achieved by a glue coating machine. The basic structure of the glue coating machine is to pass the wood veneer through the upper and lower rollers with glue on the surface. When the wood veneer passes through the upper and lower rollers, the upper and lower rollers squeeze the wood veneer and press the glue onto the surface of the wood veneer.

[0003] At present, due to the consideration of equipment cost and production cost, enterprises generally adopt single-sided gluing when gluing wood veneers. The single-sided gluing wood veneers can be stacked in sequence and hot pressed into multi-layer solid wood boards. However, since the wood veneers are only glued on one side, the other side that is not glued can only be achieved through hot pressing in order to ensure effective contact with the glue. This results in the hot pressing pressure required for the single-sided glued wood veneers to be relatively larger, the hot pressing temperature is relatively higher, and the hot pressing time is relatively longer, which leads to an increase in subsequent production costs and an extension of the production cycle. Therefore, double-sided gluing equipment for wood veneers has also appeared on the market. The thickness of the glue layer on both sides of the double-sided glued wood veneer is smaller than that of the single-sided glued wood veneer. After the amount of single-sided glue is reduced, the thickness of the glue layer required on the surface of the glue roller will also decrease. After the thickness of the glue layer is reduced, the pressure of the glue roller when rolling the glue on the wood veneer can be relatively reduced, further avoiding the wood veneer from being crushed by the larger rolling force of the glue roller, or maintaining the same extrusion force can make the glue better squeezed into the wood veneer; and after the thickness of the glue layer is reduced, the glue dripping on the surface of the glue roller will be reduced or even avoided. In addition, since the double-sided glued wood veneer also has a glue layer on the bottom, it is necessary to prevent the glue on the bottom of the wood board from dripping or flying off during the transportation of the wood board and polluting the environment.

[0004] For example, the patent with application number 202121362389.6 discloses a roller body structure of a glue coating roller, which has the effects of uniform glue coating, no damage to the veneer layer of the board, and small amount of glue used through the straight lines set on the surface of the roller body. However, the premise that the technical scheme of the above-mentioned prior art does not damage the veneer layer of the board is that there is no mutual pressure between the board and the glue coating roller, and the glue on the surface of the roller body is only rolled on the edge of the wood veneer to be sealed. Once the above-mentioned glue coating roller is used to roll coat the surface of the wood veneer, it will inevitably generate pressure on the surface of the wood veneer. At this time, since the straight lines in the technical scheme of the above-mentioned prior art are directly milled out of the roller body, it will inevitably cause the straight lines of the roller body to press indentations on the wood veneer or even directly damage it.

[0005] In addition, after being used for a long time, the technical solution of the above-mentioned prior art will inevitably cause wear of the straight lines, which will affect the gluing effect of the gluing roller. Summary of the invention

[0006] The purpose of the present invention is to overcome the shortcomings of the prior art and provide a glue coating machine for wood veneers. Through the action of a lower glue coating roller and an upper glue coating roller, both side surfaces of the wood veneer can be coated with glue at the same time, which not only improves the gluing efficiency, but also makes it easier to hot-press the multi-layer wood veneers into multi-layer solid wood boards after double-sided glue coating, thereby improving the connection strength of the multi-layer solid wood boards.

[0007] The technical solution adopted by the present invention is: The glue coating machine for wood veneers comprises a base frame with supporting legs, wherein the base frame is provided with a feed conveying roller, a glue coating roller group and a discharging conveying rod in sequence along the conveying direction of the wood veneers, the glue coating roller group comprises a lower glue coating roller and an upper glue coating roller arranged in parallel up and down, the top rotation direction of the feed conveying roller, the top rotation direction of the lower glue coating roller, the bottom rotation direction of the upper glue coating roller and the top rotation direction of the discharging conveying rod all rotate along the conveying direction of the wood veneers, and the rotation linear speeds are all equal, the spacing between the top of the lower glue coating roller and the bottom of the upper glue coating roller is less than the thickness of the wood veneers, the top of the feed conveying roller is The top of the upper and lower glue coating rollers and the top of the discharge conveying rod are located in the same plane, the base frame is provided with a glue pool directly below the lower glue coating roller, the base frame is provided with a glue dripping tube above the upper glue coating roller facing the feed conveying roller, the glue dripping tube is parallel to the upper glue coating roller, and the glue dripping port provided at the bottom of the glue dripping tube is arranged along the length direction of the glue dripping tube, and the glue in the glue dripping tube drips evenly from the glue dripping port by gravity and is distributed to the upper part of the glue coating roller facing the feed conveying roller. The glue pool transfers the glue to the glue dripping tube through pump A, and the bottom of the lower glue coating roller is glued through the glue pool below.

[0008] A further improvement of the present invention is that a transition conveying roller is also provided on the side of the base frame located at the lower glue coating roller facing the feed conveying roller, the diameter of the transition conveying roller is smaller than the diameter of the feed conveying roller, and the top of the transition conveying roller is located in the same plane as the top of the lower glue coating roller and the top of the feed conveying roller.

[0009] A further improvement of the present invention is that an upper glue roller is provided at the pool mouth of the glue liquid pool, the top of the upper glue roller contacts the bottom of the lower glue coating roller, the lower part of the upper glue roller contacts the glue in the glue liquid pool, the roller surface of the upper glue roller is provided with roller hair, the rotation direction of the upper glue roller is the same as that of the lower glue coating roller, and the linear speed of the upper glue roller is greater than the linear speed of the lower glue coating roller.

[0010] A further improvement of the present invention is that a scraper plate is provided at the lower part of the lower glue coating roller facing the feeding conveying roller, and both sides of the scraper plate are fixedly connected to the corresponding side walls of the glue pool through connecting rods B.

[0011] A further improvement of the present invention is that the lower glue coating roller and the upper glue coating roller have the same structure and both include a central shaft A, the central shaft A is coaxially passed through and fixed to the roller, the circumferential side wall of the roller is coaxially covered with an annular rubber hose, the circumferential side wall surface of the annular rubber hose is coaxially provided with a plurality of annular protrusions, the annular protrusions are evenly spaced along the circumference of the annular rubber hose, the height of the annular protrusion relative to the outer side wall of the annular rubber hose is in the range of 1 to 2 mm, and the axial groove width of the annular glue groove formed between two adjacent annular protrusions is in the range of 2 to 5 mm.

[0012] A further improvement scheme of the present invention is that the base frame is respectively connected to the upper glue coating roller and the glue pool through side frames, a dust cover for the upper glue coating roller is also fixed between the tops of the side frames, and the glue dripping tube is fixedly connected inside the dust cover; a glue spraying tube arranged parallel to the glue dripping tube is also fixedly connected inside the dust cover on the side of the glue dripping tube facing the upper glue coating roller, the glue pool transfers the glue to the inner glue spraying tube through pump B, and the glue sprayed by the glue spraying tube is vertically sprayed onto the upper glue coating roller, and the unit glue spraying amount of the glue spraying tube is in the range of one quarter to one fifth of the unit glue dripping amount of the glue dripping tube.

[0013] A further improvement of the present invention is that a glue brushing plate is provided on the base frame on the side of the lower glue coating roller facing the discharging conveying rod, the top of the glue brushing plate is swingably connected to the connecting vertical rods provided on both sides of the base frame through a swing shaft, the bottom end of the connecting vertical rod is fixedly connected to the inner side of the corresponding side wall of the glue pool, the glue brushing plate is inclined downward along the conveying direction of the wood veneer, and the bottom of the glue brushing plate is provided with bristles along the length direction of the glue brushing plate.

[0014] A further improvement of the present invention is that lateral limit plates are respectively provided on the opposite side end faces of the connecting uprights and at positions corresponding to the positions of the wooden veneers, and the lateral limit plates are respectively connected to the connecting uprights through compression springs, and one end of the lateral limit plate facing the downward glue coating roller is also provided with an inlet surface inclined inwardly along the conveying direction of the wooden veneer.

[0015] A further improvement of the present invention is that the discharging conveying rod includes a central shaft B rotatably connected to the base frame, and a plurality of conveying disks A are coaxially fixed on the central shaft B, and the tops of the conveying disks A are located in the same plane as the tops of the lower glue coating roller and the tops of the feed conveying roller, and the conveying disks A are arranged at equal intervals along the axial direction of the central shaft B, and the edges of the conveying disks A are sharp edges.

[0016] A further improvement scheme of the present invention is that a plurality of discharging conveying rods are provided along the conveying direction of the wood veneer, and a discharging pressure plate rod is also provided on the base frame at a position between two adjacent discharging conveying rods, and the discharging pressure plate rod includes a Zhou Xin shaft rod C rotatably connected to the base frame, and a plurality of conveying disks B are coaxially fixed on the central shaft rod C, and the bottom of the conveying disk B is in contact with the top surface of the passed wood veneer, and the conveying disks B are arranged at equal intervals along the axial direction of the central shaft rod C, and the edges of the conveying disks B are sharp edges.

[0017] A further improvement of the present invention is that the bottom of the glue pool is supported and fixed by a support seat.

[0018] The beneficial effects of the present invention are: First, the gluing machine for wood veneers of the present invention can simultaneously apply glue to both sides of the wood veneers through the action of the lower gluing roller and the upper gluing roller, which not only improves the gluing efficiency, but also makes it easier to hot-press the multi-layer wood veneers into multi-layer solid wood boards after double-sided gluing, thereby improving the connection strength of the multi-layer solid wood boards.

[0019] Secondly, in the gluing machine for wood veneers of the present invention, since the diameters of the feed conveying roller and the lower gluing roller are relatively large, and the lower gluing roller is also provided with a scraper plate and other devices on the side facing the feed conveying roller, the gap between the feed conveying roller and the lower gluing roller will be relatively large, which will cause the end of the wood veneer separated from the last feed conveying roller but not entering the gluing roller group to bend downward under the action of its own gravity. The wood veneer that bends downward before entering the gluing roller group will increase the contact area between the lower end and the lower gluing roller. After the bottom surface of the wood veneer contacts the lower gluing roller in advance before entering the gluing roller group for extrusion, the wood veneer bends downward more severely under the action of the viscosity of the glue. Moreover, when the bottom surface of the wood veneer contacts the glue in advance, it is not squeezed by the glue roller, resulting in the glue only floating on the surface of the wood veneer at this time. Most of the glue floating on the bottom surface of the wood veneer will be directly squeezed out of the wood veneer when it is subsequently squeezed by the lower and upper glue rollers. , it cannot achieve the gluing effect of squeezing more glue into the wood veneer at the same time as it just contacts the glue; in addition, as the downward-bent wood veneer continues to be conveyed as the glue roller group rotates to drive the wood veneer to continue to be conveyed, although the end of the wood veneer will eventually be corrected under the elastic restoring force of the wood veneer itself, the process from bending downward to the corrected level will cause the end of the wood veneer to swing up and down, thereby causing the glue that was contacted in advance on the wood veneer to be thrown off under the action of the swing, which will not only lead to a reduction and waste of the amount of glue on the bottom surface of the wood veneer, but also cause the flying glue to pollute the surrounding environment; through the action of the transition conveyor roller, the wood veneer can still be supported after leaving the last feed conveyor roller to prevent the wood veneer from bending downward, and the gravity at the end of the wood veneer after leaving the transition conveyor roller is not enough to bend the wood veneer, thereby avoiding the above situation.

[0020] Thirdly, the glue coating machine for wood veneers of the present invention can coat the glue on the circumferential side wall surface of the upper glue coating roller more quickly and evenly to form a glue layer, thereby ensuring the glue coating effect on the top surface of the wood veneer, through the action of the glue dripping tube and the glue spraying tube.

[0021] Fourthly, the gluing machine for wood veneer of the present invention can not only apply glue to the bottom of the lower glue coating roller through the action of the upper glue roller, but also the linear speed of the upper glue roller is greater than that of the lower glue coating roller, so that the glue on the surface of the lower glue coating roller can be rolled and brushed evenly while gluing, which not only enables the lower glue coating roller to apply glue quickly and evenly, but also ensures the glue thickness on the surface of the lower glue coating roller, thereby avoiding a large amount of glue dripping caused by applying excessive glue in order to ensure that the entire bottom of the lower glue coating roller can be glued, and avoiding inconsistent glue layer thickness on the surface of the lower glue coating roller due to a large amount of glue dripping.

[0022] Fifth, the glue coating machine for wood veneers of the present invention can make the glue layer on the surface of the lower glue coating roller evenly scraped again through the action of the scraper plate, and if the scraper plate is used as an adjustable mechanism, the thickness of the glue layer on the surface of the lower glue coating roller can be adjusted according to the thickness of the glue required for wood veneers of different thicknesses.

[0023] Sixth, the glue coating machine for wood veneers of the present invention can further evenly brush the glue layer on the top surface of the wood veneers through the action of the glue brushing board, and if the glue brushing board is used as an adjustable mechanism, the thickness of the glue layer on the top surface of the wood veneers can also be adjusted according to the thickness of the glue required for wood veneers of different thicknesses.

[0024] Seventh, the glue coating machine for wood veneers of the present invention can prevent the lateral deviation of the template during the transmission process, which would cause uneven glue coating on the surface of the wood veneer, through the effect of the lateral limit plate. It can also prevent the lateral deviation of the wood veneer, which would cause the glue layer on the surface of the wood veneer to be unevenly scraped by the conveying disk A of the discharge conveying rod and the conveying disk B of the discharge pressure plate rod.

[0025] Eighth, in the wood veneer gluing machine of the present invention, the gluing roller group, the gluing roller, the glue dripping hose, the glue spraying hose, the glue scraping plate, the glue brushing plate and the lateral limiting plates are all above the glue pool, so that the glue dripping produced when the above-mentioned device is working can drip back into the glue pool, avoiding glue waste and environmental pollution.

[0026] Ninth, the glue coating machine for wood veneers of the present invention can quickly stop the shaking of the wood veneers when they pass between two adjacent discharging conveying rods during the discharging process through the action of the discharging pressure plate rod, thereby avoiding the glue layer on the surface of the wood veneer from dripping or flying off.

[0027] Tenth, the glue coating machine for wood veneers of the present invention, through the structure of the discharging conveying roller and the discharging pressing plate rod, contacts the bottom and top surfaces of the wood veneers after gluing through the conveying disc A and the conveying disc B respectively, so as to minimize the contact area and avoid damaging the uniformity of the glue layer of the wood veneers.

[0028] Eleventh, the gluing machine for wood veneers of the present invention, through the effect of the annular protrusions provided on the surface of the annular rubber hose, makes it easier for the outer wall of the annular rubber hose to effectively gather glue, so that a glue layer is formed on the circumferential side wall surface of the annular rubber hose, ensuring that when the gluing roller contacts the board for gluing, sufficient glue is liquid-applied to the board, thereby ensuring the gluing effect, and the provision of the annular rubber hose can prevent the surface of the wood veneer from being crushed by the roller.

[0029] Twelfth, the glue coating machine for wood veneers of the present invention has glue baffles fixed on the outer sides of the end plates at both ends of the roller, which not only enables the two axial ends of the circumferential side wall of the roller to form annular glue collecting grooves for the convenience of collecting excess glue dripping on the roller surface, but also prevents the glue from continuing to spread along the central axis to both ends and contaminating other components, or even affecting the normal operation of the glue coating roller.

[0030] Thirteenth, in the glue coating machine for wood veneers of the present invention, the glue baffle is fixed to the end plate by connecting bolts, which facilitates the disassembly and assembly of the glue baffle, thereby facilitating the maintenance and replacement of the annular rubber hose.

[0031] Fourteenth, in the glue coating machine for wood veneers of the present invention, the bottom diameter of the annular glue collecting groove decreases along the direction facing the glue baffle, and when the excess glue located at the upper part of the roller is located in the annular glue collecting groove, the excess glue can be made to move away from one side of the annular rubber hose as quickly as possible under the action of gravity and drip downward in a concentrated manner, so that more excess glue on the surface of the annular rubber hose can continue to enter the annular glue collecting groove; when the excess glue located at the lower part of the roller is located in the annular glue collecting groove, the excess glue can be made to move close to one side of the annular rubber hose under the action of gravity, and flow along the end of the annular rubber hose and the annular conical surface A and the annular conical surface B to the annular protrusion position of the annular rubber hose in turn and gather the glue through the annular protrusion, thereby ensuring the amount of glue on the surface of the roller.

[0032] Fifteenth, the gluing machine for wood veneers of the present invention realizes axial fixation of the annular rubber hose relative to the roller by setting a limit clamp ring and annular clamping groove, thereby avoiding axial movement of the annular rubber hose during the gluing process and ensuring the gluing effect of the wood veneers.

[0033] Sixteenth, the glue coating machine for wood veneer of the present invention forms a vulcanization layer on the outer surface of the annular rubber hose, thereby improving the strength and wear resistance of the outer surface of the circumferential side wall of the annular rubber hose, extending the service life of the annular rubber hose, and ensuring the strength of the annular protrusion and the use effect of the annular protrusion.

[0034] Seventeenth, the glue coating machine for wood veneer of the present invention, through the arrangement of the annular conical arc surface A and the annular conical arc surface B, can not only facilitate the excess glue on the upper part of the roller to flow to the annular glue collecting grooves at the two axial ends of the roller, but also enable the glue on the lower part of the roller to flow and gather toward the annular raised part. BRIEF DESCRIPTION OF THE DRAWINGS

[0035] Figure 1 This is a schematic cross-sectional view of the main view of the present application.

[0036] Figure 2 It is an enlarged schematic diagram of the side view of the glue coating roller.

[0037] Figure 3 It is an enlarged schematic diagram of the side view of the discharge conveying rod.

[0038] Figure 4 It is an enlarged schematic diagram of the side view of the discharge pressure plate rod. DETAILED DESCRIPTION

[0039] Combination Figure 1~Figure 4 It can be seen that the gluing machine for wood veneers includes a base frame 1 with supporting legs 2, and the base frame 1 is provided with a feed conveying roller 3, a gluing roller group and a discharging conveying rod 8 in sequence along the conveying direction of the wood veneer 22, and the gluing roller group includes a lower gluing roller 4 and an upper gluing roller 5 which are arranged in parallel up and down, and the top rotation direction of the feed conveying roller 3, the top rotation direction of the lower gluing roller 4, the bottom rotation direction of the upper gluing roller 5 and the top rotation direction of the discharging conveying rod 8 are all rotated along the conveying direction of the wood veneer 22, and the rotation linear speeds are all equal, the spacing between the top of the lower gluing roller 4 and the bottom of the upper gluing roller 5 is less than the thickness of the wood veneer 22, and the feed conveying roller 3 is arranged in parallel with the upper gluing roller 5. The top and the top of the lower glue coating roller 4 and the top of the discharge conveying rod 8 are located in the same plane, the base frame 1 is provided with a glue pool 6 directly below the lower glue coating roller 4, and the base frame 1 is provided with a glue dripping tube 7 above the upper glue coating roller 5 facing the feed conveying roller 3. The glue dripping tube 7 is parallel to the upper glue coating roller 5, and the glue dripping port provided at the bottom of the glue dripping tube 7 is arranged along the length direction of the glue dripping tube 7, and the glue in the glue dripping tube 7 drips evenly from the glue dripping port by gravity and is distributed to the upper part of the glue coating roller 5 facing the feed conveying roller 3. The glue pool 6 transfers the glue to the glue dripping tube 7 through pump A, and the bottom of the lower glue coating roller 4 is glued through the glue pool 6 below.

[0040] A transition conveying roller 19 is also provided on the base frame 1 on the side of the lower glue coating roller 4 facing the feed conveying roller 3. The diameter of the transition conveying roller 19 is smaller than the diameter of the feed conveying roller 3, and the top of the transition conveying roller 19 is located in the same plane as the top of the lower glue coating roller 4 and the top of the feed conveying roller 3.

[0041] The feed conveying rollers 3 are arranged in sequence along the conveying direction of the wood veneer 22 .

[0042] An upper glue roller 11 is provided at the pool mouth of the glue pool 6, the top of the upper glue roller 11 contacts the bottom of the lower glue roller 4, the lower part of the upper glue roller 11 contacts the glue in the glue pool 6, the roller surface of the upper glue roller 11 is provided with roller hair, the rotation direction of the upper glue roller 11 is the same as that of the lower glue roller 4, and the linear speed of the upper glue roller 11 is greater than the linear speed of the lower glue roller 4.

[0043] A scraper plate 14 is also provided at the lower part of the lower glue coating roller 4 facing the feeding conveying roller 3 , and both sides of the scraper plate 14 are fixedly connected to the corresponding side walls of the glue pool 6 through connecting rods B15 .

[0044] The lower glue coating roller 4 and the upper glue coating roller 5 have the same structure and both include a central shaft A23, which is coaxially penetrated and fixed to the roller 24, and the circumferential side wall of the roller 24 is coaxially covered with an annular rubber tube 25, and the circumferential side wall surface of the annular rubber tube 25 is coaxially provided with a plurality of annular protrusions 26, which are evenly spaced along the circumference of the annular rubber tube 25, and the height of the annular protrusion 26 relative to the outer side wall of the annular rubber tube 25 is in the range of 1 to 2 mm, and the axial groove width of the annular glue groove formed between two adjacent annular protrusions 26 is in the range of 2 to 5 mm.

[0045] The roller 24 is provided with end plates 27 coaxially at both ends thereof, and an axial spacing is provided between the two ends of the annular rubber tube 25 and the end plates at the corresponding ends of the roller 24 .

[0046] A glue baffle 31 is coaxially fixed to the outer end face of the end plate 27. The diameter of the glue baffle 31 is larger than the diameter of the roller 24 and less than or equal to the diameter of the annular rubber hose 25. The roller 24 is located between the corresponding ends of the glue baffle 31 and the annular rubber hose 25 to form an annular glue collecting groove 32.

[0047] The glue baffle 31 is inserted into and sleeved on the central shaft 23 , and the glue baffle 31 is fixedly connected to the end plate 27 via connecting bolts 33 .

[0048] A sealing ring is also provided on the edge of the end surface of the end plate 27 facing the glue baffle 31 .

[0049] The bottom diameter of the annular glue collecting groove 32 decreases along the direction facing the glue baffle 31 .

[0050] The circumferential side walls of the roller 24 are coaxially provided with limiting clamping rings 28 at positions corresponding to both ends of the annular rubber tube 25 , and the inner wall of the annular rubber tube 25 is provided with matching annular clamping grooves corresponding to the limiting clamping rings 28 .

[0051] The outer surface of the annular rubber tube 25 is a vulcanized layer 30 .

[0052] The vulcanized layer 30 is provided with annular conical arc surfaces B35 at two axial ends corresponding to the annular rubber tube 25 , respectively. The diameter of the annular conical arc surface B35 increases in a direction away from the end where the annular rubber tube 25 is located.

[0053] The diameter of the smaller diameter end of the annular conical arc surface B35 is the diameter of the inner edge of the vulcanized layer 30 .

[0054] The outer edges of the two axial ends of the annular rubber tube 25 are respectively provided with annular conical arc surfaces A34, and the diameter of the annular conical arc surfaces A34 increases along the direction away from the end where the annular rubber tube 25 is located.

[0055] The base frame 1 is connected to the upper glue coating roller 5 and the glue pool 6 respectively through the side frames 12, and a dust cover 13 of the upper glue coating roller 5 is also fixed between the tops of the side frames 12, and the glue dripping tube 7 is fixedly connected in the dust cover 13; the dust cover 13 is also fixedly connected to a glue spraying tube 9 arranged parallel to the glue dripping tube 7 on the side of the glue dripping tube 7 facing the upper glue coating roller 5, and the glue pool 6 transfers the glue to the inner glue spraying tube 9 through the pump B, and the glue sprayed by the glue spraying tube 9 is vertically sprayed onto the upper glue coating roller 5, and the unit glue spraying amount of the glue spraying tube 9 is in the range of one quarter to one fifth of the unit glue dripping amount of the glue dripping tube 7.

[0056] A glue brushing plate 16 is provided on the base frame 1 on the side of the lower glue coating roller 4 facing the discharging conveying rod 8. The top of the glue brushing plate 16 is swingably connected to the connecting vertical rods 18 provided on both sides of the base frame 1 through a swing shaft. The bottom ends of the connecting vertical rods 18 are fixedly connected to the inner sides of the corresponding side walls of the glue pool 6. The glue brushing plate 16 is inclined downward along the conveying direction of the wood veneer 22, and the bottom of the glue brushing plate 16 is provided with bristles along the length direction of the glue brushing plate 16.

[0057] Lateral limit plates 17 are respectively provided on the opposite side end surfaces of the connecting rod 18 and at the positions corresponding to the wooden veneer 22. The lateral limit plates 17 are respectively connected to the connecting rod 18 through compression springs. The end of the lateral limit plate 17 facing the downward glue coating roller 4 is also provided with an inlet surface inclined inwardly along the conveying direction of the wooden veneer 22.

[0058] The discharging conveying rod 8 includes a central shaft B36 rotatably connected to the base frame 1, and a plurality of conveying disks A37 are coaxially fixed on the central shaft B36. The top of the conveying disk A37 is located in the same plane as the top of the lower glue coating roller 4 and the top of the feed conveying roller 3. The conveying disks A37 are arranged at equal intervals along the axial direction of the central shaft B36, and the edges of the conveying disks A37 are sharp edges.

[0059] The discharging conveying rods 8 are provided in plurality along the conveying direction of the wood veneer 22, and a discharging pressure plate rod 20 is also provided on the base frame 1 at a position between two adjacent discharging conveying rods 8, and the discharging pressure plate rod 20 includes a Zhou Xin shaft rod C38 rotatably connected to the base frame 1, and a plurality of conveying disks B39 are coaxially fixed on the central shaft rod C38, and the bottom of the conveying disk B39 is in contact with the top surface of the passed wood veneer 22, and the conveying disks B39 are arranged at equal intervals along the axial direction of the central shaft rod C38, and the edges of the conveying disks B39 are sharp edges.

[0060] The bottom of the glue pool 6 is supported and fixed by a support base 10 .

[0061] During use of the lower glue coating roller 4 and the upper glue coating roller 5 of the present application, when the annular rubber tube 25 on the surface of the roller 24 contacts the glue, the glue infiltrates into the annular glue retaining groove formed between two adjacent annular protrusions 26, and due to the effect of viscosity, the roller 24 can effectively retain the glue in the annular glue retaining groove. In addition, due to the effect of the surface tension of the glue, the glue liquid level in the annular glue retaining groove can exceed the groove wall of the annular glue retaining groove formed by the annular protrusion 26, and the glue in different annular glue retaining grooves is connected together to submerge and cover the corresponding position of the annular protrusion 26, that is, the roller 24 can retain more glue for gluing, thereby ensuring the glue coating amount of the wood veneer 22. When the glue retained on the surface of the roller 24 rotates to be in close contact with the surface of the sheet to be coated with glue due to the rotation of the roller 24, the annular rubber hose 25 is compressed and deformed due to the pressure on the roller 24, so that the glue retained on the surface of the annular rubber hose 25 is pressed against the surface of the sheet. In addition, the elastic restoring force of the annular rubber hose 25 facilitates the glue to penetrate deeper into the sheet through the fibers of the sheet, so that the glue layer of the sheet partially penetrates into the sheet to a certain thickness, so as to ensure the subsequent bonding effect of the sheet.

[0062] When the upper glue roller 5 applies glue to the top surface of the sheet, the sheet contacts the bottom of the upper glue roller 5. At this time, due to the setting of the annular conical arc surface A34 and the annular conical arc surface B35 at the two axial ends of the roller 24, the middle of the bottom edge of the annular rubber tube 25 of the roller 24 contacts the sheet surface. In order to ensure that the entire top surface of the sheet can be glued, it is generally necessary to ensure that the two side edges of the sheet are between the annular conical arc surfaces B35 at the two axial ends of the annular rubber tube 25. When the roller 24 squeezes the glue liquid onto the sheet surface, the excess glue liquid will inevitably be squeezed out from the two side edges of the sheet. However, due to the annular conical arc surface A34 and the annular conical arc surface B35, the glue liquid will not be squeezed out from the two side edges of the sheet. Due to the structure of surface B35, the glue will gather toward the middle part in contact with the board along the annular conical surface A34 and the annular conical surface B35 under the action of its own weight, so that the glue is still located at the position where the annular protrusion 26 is provided on the annular hose 25, ensuring that more glue is used to apply glue to the board surface of the board; after the glue is squeezed out from the two side edges of the wooden veneer 22 to the outer edge, it will contact the supporting components under the wooden veneer 22 through the annular hoses 253 on both sides of the wooden veneer 22, and the glue will be transferred to the supporting components under the wooden veneer 22 under the action of gravity.

[0063] When the lower glue coating roller 4 applies glue to the bottom surface of the plate, the plate contacts the top of the lower glue coating roller 4 . At this time, due to the setting of the annular conical surface A34 and the annular conical surface B35 at the two axial ends of the roller 24, the middle of the top edge of the annular rubber hose 25 of the roller 24 contacts the plate surface. In order to ensure that the top surface of the plate can be fully coated with glue, it is generally necessary to ensure that the two side edges of the plate are between the annular conical surfaces B35 at the two axial ends of the annular rubber hose 53. When the roller 24 squeezes the glue to the plate surface, excess glue will inevitably be squeezed out from the two side edges of the plate. Due to the structure of the annular conical surface A34 and the annular conical surface B35, the glue will flow along the annular conical surface A34 and the annular conical surface B35 to the annular glue collecting groove 32 under the action of its own weight, so that the squeezed excess glue flows to both sides as soon as possible, which is convenient for the centralized recovery of the glue. In addition, due to the action of the glue baffle 31, the glue is prevented from flowing along the central shaft 23 to the shaft end and contacting other components, thereby preventing the glue from polluting other components of the equipment and even affecting the normal operation of other components.

[0064] When the glue dripping tube 7 is applying glue to the upper part of the upper glue coating roller 5, in order to ensure that the glue can be applied to the surface of the roller 24 as quickly and evenly as possible, the upper glue coating roller 5 first rotates to the position of the glue spraying tube 9, and the glue spraying tube 9 sprays the glue evenly to the side wall surface of the roller 24 passing through, so that the side wall surface of the roller 24 is wetted by the mist glue, so that the subsequent glue can quickly and evenly fill the surface of the roller 24 under the wetting effect of the mist glue; in order to ensure that there is still enough glue on the surface of the roller when the glue turns to the bottom and contacts the wood veneer 22, At this time, it is necessary to evenly drop a relatively excessive amount of glue onto the upper surface of the upper glue coating roller 5 along the axial direction. A layer of glue can be gathered on the outer wall of the annular rubber tube 25 at the position of the annular protrusion 26 on the surface of the upper glue coating roller 5. The glue at the positions corresponding to the annular conical surfaces A34 and the annular conical surfaces B35 at both axial ends of the annular rubber tube 25 will flow along the annular conical surfaces A34 and the annular conical surfaces B35 to the annular glue collecting groove 32 under the action of its own weight. The glue in the annular glue collecting groove 32 will drip downward in a concentrated manner under the action of its own weight.

[0065] When the upper glue roller 11 applies glue to the bottom of the lower glue roller 4, in order to ensure that there is enough glue on the surface of the roller 24 when the glue turns to the top and contacts the wooden veneer 22, and in order to prevent the increase of energy consumption of the roller 24 due to excessive glue, the bottom of the upper glue roller 11 contacts the liquid surface of the glue in the glue pool 6, and then the upper glue roller 11 moistened by the glue rotates to the bottom surface of the annular rubber tube 25 of the lower glue roller 4 for gluing. Since the rotation direction of the upper glue roller 11 is the same as that of the lower glue roller 4, and the linear speed of the upper glue roller 11 is greater than the linear speed of the lower glue roller 4, after applying the glue to the bottom surface of the annular rubber tube 25 of the lower glue roller 4, the upper glue roller 11 will brush the glue evenly and remove the excess glue through relative rotation with the lower glue roller 4, and the glue on the surface of the annular rubber tube 25 will be scraped evenly and the excess glue will be scraped off again when passing through the scraper 14.

[0066] The wood veneer 22 is conveyed between the lower glue coating roller 4 and the upper glue coating roller 5 through the feed conveyor roller 3 and the transition conveyor roller 19. The upper and lower surfaces of the wood veneer 22 are coated with a glue layer by the rolling glue of the lower glue coating roller 4 and the upper glue coating roller 5. The wood veneer 22 with the glue layer on the upper and lower surfaces continues to be conveyed to the position of the glue brushing plate 16, and the glue on the top surface of the wood veneer 22 is brushed evenly again to prevent the glue on the top surface of the wood veneer 22 from gathering in the middle of the wood veneer 22 under the action of tension and gravity, and the lateral limit plate 1 7 can limit the wooden veneer 22, ensuring that the wooden veneer 22 is always located in the middle position when passing through the lower glue coating roller 4 and the upper glue coating roller 5, thereby ensuring the gluing effect of the wooden veneer 22; finally, the wooden veneer is discharged and conveyed through the discharge conveying rod 8, and the discharge pressing plate rod 20 is used to avoid the wooden veneer 22 from jumping during the discharge and conveying, thereby preventing the glue on the surface of the wooden veneer 22 from falling off and affecting the amount and uniformity of the glue on the surface of the wooden veneer 22, and also preventing the falling glue from contaminating the site or equipment.

Claims

1. Gluing machine for wood veneer, characterized by: The invention comprises a base frame (1) provided with supporting legs (2), wherein the base frame (1) is provided with a feed conveying roller (3), a glue coating roller group and a discharge conveying rod (8) in sequence along the conveying direction of the wood veneer (22), wherein the glue coating roller group comprises a lower glue coating roller (4) and an upper glue coating roller (5) which are arranged in parallel up and down, wherein the top rotation direction of the feed conveying roller (3), the top rotation direction of the lower glue coating roller (4), the bottom rotation direction of the upper glue coating roller (5) and the top rotation direction of the discharge conveying rod (8) are all along the conveying direction of the wood veneer (22), and the rotation linear speeds are all equal, the spacing between the top of the lower glue coating roller (4) and the bottom of the upper glue coating roller (5) is smaller than the thickness of the wood veneer (22), and the top of the feed conveying roller (3), the lower glue coating roller ( The top of the glue roller (4) and the top of the discharge conveying rod (8) are located in the same plane, the base frame (1) is provided with a glue pool (6) directly below the lower glue coating roller (4), the base frame (1) is provided with a glue dripping tube (7) above the upper glue coating roller (5) facing the feeding conveying roller (3), the glue dripping tube (7) is parallel to the upper glue coating roller (5), and the glue dripping port provided at the bottom of the glue dripping tube (7) is arranged along the length direction of the glue dripping tube (7), and the glue in the glue dripping tube (7) is evenly dripped from the glue dripping port by gravity and distributed to the upper part of the glue coating roller (5) facing the feeding conveying roller (3), the glue pool (6) transfers the glue to the glue dripping tube (7) through the pump A, and the bottom of the lower glue coating roller (4) is glued through the glue pool (6) below.

2. The glue coating machine for wood veneer as claimed in claim 1, characterized in that: A transition conveying roller (19) is also provided on the base frame (1) on the side of the lower glue coating roller (4) facing the feed conveying roller (3); the diameter of the transition conveying roller (19) is smaller than the diameter of the feed conveying roller (3); and the top of the transition conveying roller (19) is located in the same plane as the top of the lower glue coating roller (4) and the top of the feed conveying roller (3).

3. The glue coating machine for wood veneer as claimed in claim 1, characterized in that: An upper glue roller (11) is provided at the pool opening of the glue liquid pool (6), the top of the upper glue roller (11) contacts the bottom of the lower glue coating roller (4), the lower part of the upper glue roller (11) contacts the glue liquid in the glue liquid pool (6), the roller surface of the upper glue roller (11) is provided with roller hair, the rotation direction of the upper glue roller (11) is the same as that of the lower glue coating roller (4), and the linear speed of the upper glue roller (11) is greater than the linear speed of the lower glue coating roller (4).

4. The glue coating machine for wood veneer as claimed in claim 1, characterized in that: A scraper plate (14) is also provided at the lower part of the lower glue coating roller (4) facing the feeding conveying roller (3), and the two sides of the scraper plate (14) are fixedly connected to the corresponding side walls of the glue liquid pool (6) via connecting rods B (15).

5. The wood veneer gluing machine according to claim 1, characterized in that: The lower glue coating roller (4) and the upper glue coating roller (5) have the same structure, and both include a central shaft A (23). The central shaft A (23) is coaxially penetrated and fixed to the roller (24). The circumferential side wall of the roller (24) is coaxially covered with an annular rubber tube (25). The circumferential side wall surface of the annular rubber tube (25) is coaxially provided with a plurality of annular protrusions (26). The annular protrusions (26) are distributed at equal intervals along the circumference of the annular rubber tube (25). The height of the annular protrusions (26) relative to the outer wall of the annular rubber tube (25) is in the range of 1 to 2 mm. The axial groove width of the annular glue groove formed between two adjacent annular protrusions (26) is in the range of 2 to 5 mm.

6. The glue coating machine for wood veneer as claimed in claim 1, characterized in that: The base frame (1) is connected to the upper glue coating roller (5) and the glue pool (6) respectively through the side stand (12); a dust cover (13) of the upper glue coating roller (5) is also fixed between the tops of the side stand (12); the glue dripping tube (7) is fixedly connected inside the dust cover (13); a glue spraying tube (9) arranged parallel to the glue dripping tube (7) is also fixedly connected inside the dust cover (13) on the side of the glue dripping tube (7) facing the upper glue coating roller (5); the glue pool (6) transmits the glue to the inner glue spraying tube (9) through a pump B; the glue sprayed by the glue spraying tube (9) is vertically sprayed onto the upper glue coating roller (5); the unit glue spraying amount of the glue spraying tube (9) is within a range of one quarter to one fifth of the unit glue dripping amount of the glue dripping tube (7).

7. The glue coating machine for wood veneer as claimed in claim 1, characterized in that: A glue brushing plate (16) is provided on the base frame (1) at a side of the lower glue coating roller (4) facing the discharge conveying rod (8); the top of the glue brushing plate (16) is swingably connected to connecting uprights (18) provided on both sides of the base frame (1) via a swing shaft; the bottom ends of the connecting uprights (18) are fixedly connected to the inner sides of corresponding side walls of the glue pool (6); the glue brushing plate (16) is tilted downward along the conveying direction of the wood veneer (22); and bristles are provided on the bottom of the glue brushing plate (16) along the length direction of the glue brushing plate (16).

8. The glue coating machine for wood veneer as claimed in claim 7, characterized in that: Side limit plates (17) are respectively provided on the opposite side end surfaces of the connecting uprights (18) and at positions corresponding to the wood veneers. The side limit plates (17) are respectively connected to the connecting uprights (18) via compression springs. One end of the side limit plates (17) facing the downward glue coating roller (4) is also provided with an introductory surface inclined inwardly along the conveying direction of the wood veneer (22).

9. The wood veneer glue coating machine according to claim 1, characterized in that: The discharging conveying rod (8) comprises a central shaft B (36) rotatably connected to the base frame (1), and a plurality of conveying disks A (37) are coaxially fixed on the central shaft B (36), and the top of the conveying disk A (37) is located in the same plane as the top of the lower glue coating roller (4) and the top of the feeding conveying roller (3), and the conveying disks A (37) are arranged at equal intervals along the axial direction of the central shaft B (36), and the edges of the conveying disks A (37) are sharp edges.

10. The glue coating machine for wood veneer as claimed in claim 9, characterized in that: A plurality of the discharging conveying rods (8) are provided along the conveying direction of the wood veneer (22); a discharging pressure plate rod (20) is also provided on the base frame (1) at a position between two adjacent discharging conveying rods (8); the discharging pressure plate rod (20) comprises a Zhouxin shaft rod C (38) rotatably connected to the base frame (1); a plurality of conveying disks B (39) are coaxially fixed on the central shaft rod C (38); the bottom of the conveying disk B (39) is in contact with the top surface of the passing wood veneer (22); the conveying disks B (39) are arranged at equal intervals along the axial direction of the central shaft rod C (38); and the edges of the conveying disks B (39) are sharp edges.

Citation Information

Patent Citations

  • Two -sided rubber coating device of three -ply board

    CN205731808U

  • Glue spreader of wood working machinery spreading machine

    CN207204478U

  • Gluing device for insulation board processing

    CN211937671U

  • Coating device capable of achieving uniform coating

    CN215542227U

  • Inorganic silicon crystal plate gluing device

    CN217528026U

Cited By

  • Wood sheet double-sided gluing machine

    CN121733664A