Method and device for detecting lithium precipitation starting point potential of soft package battery cell
Through the detection method of the lithium evolution starting point potential of the soft-packed battery cell, the voltage-time curve and the differential voltage-time curve are used to determine the lithium evolution starting point potential, which solves the problem of large error in the detection of the lithium evolution starting point of the soft-packed battery cell in the existing technology, and improves the efficiency The accuracy of testing and the rationality of strategy development.
Patent Information
- Application Number
- CN202410983402.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-22
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2044-07-22
AI Technical Summary
Existing lithium battery lithium evolution window testing methods have large errors in detecting the lithium evolution starting point of soft-packed cells, resulting in unreasonable formulation of subsequent stage charging strategies and affecting the overall testing experience.
Using the lithium evolution starting point potential detection method of soft-packed batteries, by preparing positive and negative electrode test pole pieces, preparing soft-packed batteries, determining the nominal capacity, generating test capacity parameters, and obtaining voltage-time curves and differential voltage-time curves, Differential treatment to determine the starting potential of lithium evolution.
It improves the accuracy of the starting potential of lithium evolution, makes the subsequent step charging strategy more reasonable, and improves the overall testing experience.
Smart Images

Figure CN118777902A_ABST
Abstract
Description
Technical Field
[0001] The present application belongs to the technical field of battery cell testing, and in particular relates to a method and device for detecting the starting potential of lithium deposition of a soft-pack battery cell. Background Art
[0002] The lithium plating window of a lithium battery refers to the voltage range in which the negative electrode material can stably accept and release lithium ions without lithium metal precipitation during the charge and discharge process of a lithium-ion battery. Under normal working conditions, lithium ions are deintercalated from the positive electrode and migrate to the negative electrode through the electrolyte and are embedded in the negative electrode material. However, when the lithium battery is in an overcharged state, high-current rapid charging, or when the lithium ion concentration near the negative electrode surface increases rapidly, it is possible that the lithium ions cannot be effectively embedded in the internal structure of the negative electrode material. At this time, the lithium ions will be reduced to metallic lithium by electrons on the negative electrode surface, and lithium plating will occur.
[0003] At present, the lithium plating window test of lithium batteries mainly uses power cells and makes reference electrodes. The starting point of lithium plating is determined by monitoring the potential of the negative electrode to the reference electrode to be 0 volts. However, this method of determining the starting point of lithium plating is not applicable. For example, for some soft-pack cells, there is a large error between the determined lithium plating starting point and the actual lithium plating starting point, which leads to unreasonable formulation of subsequent step-charging strategies and affects the overall testing experience. Summary of the invention
[0004] This application is to solve the above-mentioned problem of using 0 volts of potential of the negative electrode to the reference electrode as the starting point of lithium precipitation. However, this method of determining the starting point of lithium precipitation is not applicable. For example, there is a large error between the starting point of lithium precipitation determined for some soft-pack batteries and the actual starting point of lithium precipitation, which leads to unreasonable formulation of subsequent step charging strategies and affects the overall test experience. Technical defects, a method and device for detecting the starting point potential of lithium precipitation of soft-pack batteries are proposed, and the technical solution is as follows: In a first aspect, an embodiment of the present application provides a method for detecting a lithium plating starting potential of a soft-pack battery cell, comprising: Performing sample preparation according to at least two electrode materials to obtain positive and negative electrode test electrodes, and preparing soft-pack battery cells according to the positive and negative electrode test electrodes and preset reference electrodes; Based on the soft-pack battery cell and two sets of preset charge and discharge parameters, the nominal capacity is determined; Generate at least two groups of test capacity parameters according to the nominal capacity, and test the soft-pack battery cells in turn according to each group of test capacity parameters to obtain corresponding voltage-time curves and negative electrode to lithium potential curves; Each voltage-time curve is differentiated to obtain the corresponding differential voltage-time curve, and the lithium plating starting potential of the soft-pack battery cell is determined based on all voltage-time curves, all differential voltage-time curves and the negative electrode to lithium potential curve.
[0005] In an optional solution of the first aspect, the positive and negative electrode test electrodes are obtained by sample preparation according to at least two electrode materials, including: Mixing artificial graphite, conductive carbon black, sodium carboxymethyl cellulose and styrene-butadiene rubber latex according to a preset first ratio to obtain a negative electrode slurry; The negative electrode slurry is coated and dried according to a preset first coating surface density, and the negative electrode slurry after the coating and drying is roll-pressed according to a preset first compaction density; Cutting the negative electrode slurry after the roll pressing process according to a preset first size to obtain at least two negative electrode test pole pieces; Mixing lithium iron phosphate, conductive carbon black, polyvinylidene fluoride and carbon nanotubes according to a preset second ratio to obtain a positive electrode slurry; The positive electrode slurry is coated and dried according to a preset second coating surface density, and the positive electrode slurry after the coating and drying is roll-pressed according to a preset second compaction density; The positive electrode slurry after the roll pressing process is cut according to a preset second size to obtain at least two positive electrode test pole pieces.
[0006] In another optional solution of the first aspect, a soft-pack battery cell is prepared according to the positive and negative test electrodes and a preset reference electrode, including: Performing lithium plating treatment on a preset reference electrode according to preset lithium plating parameters; Based on the preset number of stacked layers, the number of negative test electrodes, the number of positive test electrodes, the preset number of reference electrodes after lithium plating, and the number of diaphragms are determined respectively, and according to the number of negative test electrodes, the number of positive test electrodes, the preset number of reference electrodes after lithium plating, and the number of diaphragms, soft-pack battery cells are prepared.
[0007] In another optional solution of the first aspect, the two sets of preset charge and discharge parameters include a discharge parameter consisting of a charge and discharge rate and a discharge cut-off voltage, and a charge parameter consisting of a charge and discharge rate and a charge cut-off voltage, and the discharge cut-off voltage is less than the charge cut-off voltage; Based on the soft-pack battery and two sets of preset charge and discharge parameters, the nominal capacity is determined, including: The soft-pack battery cell is placed in a static state according to a preset static state time, and the soft-pack battery cell is discharged according to a discharge parameter after the static state treatment; The soft-packed battery cells after the discharge treatment are placed in a shelf state according to a preset shelf time, and the soft-packed battery cells after the shelf state are charged according to charging parameters; The soft-packed battery cells after the charge treatment are placed in a shelf state according to a preset placement time, and the soft-packed battery cells after the placement treatment are discharged according to the discharge parameters, so as to use the corresponding discharge capacity as the nominal capacity.
[0008] In yet another optional solution of the first aspect, generating at least two sets of test capacity parameters according to the nominal capacity includes: Obtaining a first set of test capacity parameters based on the nominal capacity, a preset first charging ratio parameter, and a preset relaxation time; Based on the nominal capacity, the preset second charging ratio parameter and the preset relaxation time, a second set of test capacity parameters is obtained; Based on the nominal capacity, the preset third charging ratio parameter and the preset relaxation time, a third set of test capacity parameters is obtained; wherein the difference between the preset second charging ratio parameter and the preset first charging ratio parameter is consistent with the difference between the preset third charging ratio parameter and the preset second charging ratio parameter.
[0009] In another optional scheme of the first aspect, the lithium precipitation starting potential of the soft-pack battery cell is determined according to all voltage-time curves, all differential voltage-time curves and the negative electrode to lithium potential curve, including: When an abnormal slope change is detected in the voltage-time curve corresponding to the nth group of test capacity parameters, it is determined whether there is a characteristic peak in the corresponding differential voltage-time curve; wherein n is a positive integer greater than 1; When a characteristic peak is detected in the differential voltage-time curve, the lithium plating starting potential of the soft-pack battery cell is determined according to the voltage-time curve, the differential voltage-time curve and the negative electrode to lithium potential curve corresponding to the n-1th group of test capacity parameters.
[0010] In another optional scheme of the first aspect, the lithium precipitation starting potential of the soft-pack battery cell is determined according to the voltage-time curve, the differential voltage-time curve and the negative electrode to lithium potential curve corresponding to the n-1th group of test capacity parameters, including: When no abnormal slope change is detected in the voltage-time curve corresponding to the n-1th group of test capacity parameters, it is determined whether there is a characteristic peak in the corresponding differential voltage-time curve; When no characteristic peak is detected in the differential voltage-time curve, a first potential corresponding to the nth group of test capacity parameters and a second potential corresponding to the n-1th group of test capacity parameters are respectively determined in the negative electrode to lithium potential curve; The lithium deposition starting point potential of the soft-pack battery cell is determined according to the potential interval formed by the first potential and the second potential.
[0011] In a second aspect, an embodiment of the present application provides a device for detecting a lithium plating starting point potential of a soft-pack battery cell, comprising: A cell preparation module, used to prepare samples according to at least two electrode materials to obtain positive and negative electrode test electrodes, and to prepare soft-pack cells according to the positive and negative electrode test electrodes and preset reference electrodes; A capacity determination module, used to determine the nominal capacity based on the soft-pack battery cell and two sets of preset charge and discharge parameters; A data generation module is used to generate at least two groups of test capacity parameters according to the nominal capacity, and test the soft-pack battery cells in turn according to each group of test capacity parameters to obtain corresponding voltage-time curves and negative electrode to lithium potential curves; The result determination module is used to perform differentiation processing on each voltage-time curve to obtain the corresponding differential voltage-time curve, and determine the lithium precipitation starting potential of the soft-pack battery cell based on all voltage-time curves, all differential voltage-time curves and the negative electrode to lithium potential curve.
[0012] In a third aspect, an embodiment of the present application further provides a device for detecting a lithium plating starting point potential of a soft-pack battery cell, comprising a processor and a memory; The processor is connected to the memory; A memory for storing executable program codes; The processor runs a program corresponding to the executable program code by reading the executable program code stored in the memory, so as to implement the method for detecting the lithium plating starting point potential of the soft-pack battery cell provided by the first aspect of the embodiment of the present application or any one of the implementation methods of the first aspect.
[0013] In a fifth aspect, an embodiment of the present application provides a computer storage medium, which stores a computer program. The computer program includes program instructions. When the program instructions are executed by a processor, the method for detecting the lithium plating starting point potential of a soft-pack battery cell provided in the first aspect of the embodiment of the present application or any one of the implementation methods of the first aspect can be implemented.
[0014] In an embodiment of the present application, when detecting the lithium deposition starting potential of a soft-pack battery cell, a sample preparation process can be performed according to at least two electrode materials to obtain positive and negative electrode test electrodes, and a soft-pack battery cell can be prepared according to the positive and negative electrode test electrodes and a preset reference electrode; the nominal capacity is determined based on the soft-pack battery cell and two sets of preset charge and discharge parameters; at least two sets of test capacity parameters are generated according to the nominal capacity, and the soft-pack battery cell is tested in turn according to each set of test capacity parameters to obtain a corresponding voltage-time curve and a negative electrode to lithium potential curve; each voltage-time curve is differentiated to obtain a corresponding differential voltage-time curve, and the lithium deposition starting potential of the soft-pack battery cell is determined based on all voltage-time curves, all differential voltage-time curves and the negative electrode to lithium potential curve. By combining a variety of electrode materials and a preset reference electrode, a soft-pack battery cell with a simple process and a shorter cycle can be prepared, and multiple sets of test capacity parameters are generated according to the nominal capacity determined by the soft-pack battery cell, so that the soft-pack battery cell can be tested based on the voltage relaxation method without causing damage to the soft-pack battery cell and wasting time; secondly, the voltage-time curve obtained after the test process and the corresponding differential voltage-time curve can be combined to determine the lithium plating starting potential of the soft-pack battery cell at a specific rate in the negative electrode to lithium potential curve, which can not only ensure the accuracy of the lithium plating starting potential, but also make the subsequent step-charging strategy formulation more reasonable, thereby improving the overall testing experience. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0016] Figure 1 An overall flow chart of a method for detecting the lithium plating starting point potential of a soft-pack battery cell provided in an embodiment of the present application; Figure 2 A schematic diagram of a voltage-time curve and a differential voltage-time curve of a soft-pack battery cell provided in an embodiment of the present application; Figure 3 A schematic diagram of a voltage-time curve and a differential voltage-time curve of another soft-pack battery cell provided in an embodiment of the present application; Figure 4 A schematic diagram of a negative electrode to lithium potential curve of a soft-pack battery provided in an embodiment of the present application; Figure 5 A schematic diagram of the structure of a device for detecting the starting point potential of lithium deposition of a soft-pack battery cell provided in an embodiment of the present application; Figure 6A schematic structural diagram of another device for detecting the lithium plating starting point potential of a soft-pack battery cell provided in an embodiment of the present application. DETAILED DESCRIPTION
[0017] The technical solutions in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application.
[0018] In the following introduction, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance. The following introduction provides multiple embodiments of the present application, and different embodiments can be replaced or combined, so the present application can also be considered to include all possible combinations of the same and / or different embodiments recorded. Therefore, if one embodiment includes features A, B, and C, and another embodiment includes features B and D, then the present application should also be considered to include embodiments containing one or more of all other possible combinations of A, B, C, and D, although the embodiment may not be clearly recorded in the following text.
[0019] The following description provides examples and does not limit the scope, applicability or examples set forth in the claims. Changes may be made to the functions and arrangements of the elements described without departing from the scope of the present application. Various processes or components may be appropriately omitted, substituted or added to each example. For example, the described method may be performed in an order different from the order described, and various steps may be added, omitted or combined. In addition, features described in some examples may be combined in other examples.
[0020] See also Figure 1 , Figure 1 An overall flow chart of a method for detecting the lithium plating starting point potential of a soft-pack battery cell provided in an embodiment of the present application is shown.
[0021] like Figure 1 As shown, the method for detecting the lithium plating starting point potential of the soft-pack battery cell may at least include the following steps: Step 102: Prepare samples using at least two electrode materials to obtain positive and negative electrode test electrodes, and prepare soft-pack cells based on the positive and negative electrode test electrodes and preset reference electrodes.
[0022] In an embodiment of the present application, the method for detecting the lithium deposition starting point potential of a soft-pack battery cell can be but is not limited to being applied to a test terminal, which can establish connections with a battery preparation device and a battery testing device, respectively, to control the battery preparation device to prepare a soft-pack battery cell according to a variety of electrode materials, corresponding electrode parameters and a preset reference electrode, and the soft-pack battery cell can be placed in the battery testing device for testing and processing, so as to determine the lithium deposition starting point potential of the soft-pack battery cell according to the test results fed back by the battery testing device.
[0023] Among them, the battery preparation device can be understood as a collection of processing equipment that coats and dries, rolls, and die-cuts a variety of electrode materials to obtain positive and negative electrode test electrodes, and performs lamination, liquid injection, formation, and volume separation on the positive and negative electrode test electrodes and the preset reference electrodes. It can process the corresponding multiple electrode materials and the preset reference electrode according to the preparation process of the positive and negative electrode test electrodes output by the test terminal and the preparation process of the soft-pack battery cell, and when laminating the positive and negative electrode test electrodes and the preset reference electrode, the preset reference electrode can also be fixed in the middle of the diaphragm corresponding to the positive and negative electrode test electrodes, and the nickel sheet is used as the pole ear of the preset reference electrode, that is, the preset reference electrode is welded to the nickel sheet through a tin bar to ensure the potential stability of the reference electrode. Here, all processing equipment contained in the battery preparation device can be conventional equipment in this field, and its related control procedures or execution principles will not be described in detail.
[0024] Among them, the battery testing device can be understood as a test cabinet and a collection of test equipment for charging and discharging soft-pack batteries. The prepared soft-pack batteries can be placed in the test cabinet through a test terminal or manually, and the soft-pack batteries can be tested according to a variety of test capacity parameters output by the test terminal. For example, but not limited to, the soft-pack batteries are charged and discharged at a specified current rate at a constant current, so that the remaining capacity of the soft-pack batteries meets the specified charging ratio parameter (that is, the ratio of the energy of the battery after current charging to the energy when it is fully charged, referred to as SOC), and the current is cut off. The changing trend of the soft-pack battery cell during the natural relaxation of the voltage as time increases can be recorded in a manner to generate the voltage-time curve of the soft-pack battery cell under different discharge ratio parameters; in addition, the battery testing device can also synchronously record the negative electrode to lithium potential (that is, the voltage between the negative electrode plate of the soft-pack battery cell and the preset reference electrode) of the soft-pack battery cell as time increases through a multi-channel meter during the test process, so as to generate a corresponding negative electrode to lithium potential curve according to the negative electrode to lithium potential, and all the voltage-time curves and the negative electrode to lithium potential curve mentioned above can be fed back to the test terminal. Here, all the test equipment contained in the battery testing device can be conventional equipment in this field, and its related control procedures or execution principles will not be described in detail.
[0025] It can be understood that when the test terminal detects the lithium deposition starting potential of the soft-pack battery cell, it can control the above-mentioned battery preparation device to prepare a soft-pack battery cell with a simple process and a shorter cycle by combining a variety of electrode materials and a preset reference electrode, and generate multiple sets of test capacity parameters according to the nominal capacity determined by the soft-pack battery cell, so as to control the above-mentioned battery testing device to test and process the soft-pack battery cell according to the multiple sets of test capacity parameters, without causing damage to the soft-pack battery cell and consumption; secondly, after receiving all the voltage-time curves and the negative electrode to lithium potential curves fed back by the battery testing device, it is also possible to determine the lithium deposition starting potential of the soft-pack battery cell at a specific rate in the negative electrode to lithium potential curve according to all the voltage-time curves and the corresponding differential voltage-time curves, which can not only ensure the accuracy of the lithium deposition starting potential, but also make the subsequent step charging strategy formulation more reasonable, thereby improving the overall testing experience.
[0026] Specifically, when detecting the lithium plating starting potential of the soft-pack battery cell, the test terminal can, but is not limited to, generate the preparation process of the positive and negative electrode test electrode sheets and the preparation process of the soft-pack battery cell according to the names of the various electrode sheet materials, the preset reference electrode and the preset electrode sheet parameters input by the staff, and can send the preparation process of the positive and negative electrode test electrode sheets and the preparation process of the soft-pack battery cell to the battery preparation device, so that the battery preparation device first coats and dries the various electrode sheet materials according to the preparation process of the positive and negative electrode test electrode sheets, rolls, and die-cuts them, and then stacks, injects, forms and divides the positive and negative electrode test electrode sheets and the preset reference electrode according to the preparation process of the soft-pack battery cell, so as to obtain a soft-pack battery cell with higher stability. Here, the preset electrode sheet parameters can include, but are not limited to, the material ratio, coating surface density, and size parameters corresponding to the positive electrode test electrode sheet, the material ratio, coating surface density, and size parameters corresponding to the negative electrode test electrode sheet, and the number of positive and negative electrode test electrode sheets during the stacking process.
[0027] As an option of the embodiment of the present application, the positive and negative electrode test electrodes are obtained by sample preparation according to at least two electrode materials, including: Mixing artificial graphite, conductive carbon black, sodium carboxymethyl cellulose and styrene-butadiene rubber latex according to a preset first ratio to obtain a negative electrode slurry; The negative electrode slurry is coated and dried according to a preset first coating surface density, and the negative electrode slurry after the coating and drying is roll-pressed according to a preset first compaction density; Cutting the negative electrode slurry after the roll pressing process according to a preset first size to obtain at least two negative electrode test pole pieces; Mixing lithium iron phosphate, conductive carbon black, polyvinylidene fluoride and carbon nanotubes according to a preset second ratio to obtain a positive electrode slurry; The positive electrode slurry is coated and dried according to a preset second coating surface density, and the positive electrode slurry after the coating and drying is roll-pressed according to a preset second compaction density; The positive electrode slurry after the roll pressing process is cut according to a preset second size to obtain at least two positive electrode test pole pieces.
[0028] Specifically, taking the case where the active material of the positive electrode sheet of the soft-pack battery cell to be prepared is lithium iron phosphate and the active material of the negative electrode sheet is artificial graphite as an example, after the test terminal sends the preparation process of the positive and negative electrode test sheets to the battery preparation device, the battery preparation device can first mix the artificial graphite (C), conductive carbon black (SP), sodium carboxymethyl cellulose (CMC) and styrene-butadiene rubber emulsion (SBR) according to the preset first ratio, and use deionized water as a solvent to obtain the negative electrode slurry. The proportions of artificial graphite, conductive carbon black, sodium carboxymethyl cellulose and styrene-butadiene rubber emulsion in the preset first ratio can be, but are not limited to, 96.1%, 1.0%, 1.3% and 1.6%. Of course, in the embodiment of the present application, the proportion of artificial graphite can also be controlled between 94% and 97%, the proportion of conductive carbon black can be controlled between 1% and 3%, the proportion of sodium carboxymethyl cellulose can be controlled between 1% and 3%, and the proportion of styrene-butadiene rubber emulsion can be controlled between 1% and 3%, and are not limited to this.
[0029] Next, after obtaining the negative electrode slurry, the negative electrode slurry can also be coated on a 6 μm thick copper foil by a battery preparation device, and a continuous oven set at a temperature between 60-65° C. is used to coat and dry the negative electrode slurry according to a preset first coating surface density. The preset first coating surface density can be, but is not limited to, 173 g / m 2 , and a roller press with a roller pressure set to 50T can be used to roller press the negative electrode slurry after coating and drying according to a preset first compaction density, and the preset first compaction density can be but is not limited to 1.6g / cm 3 Of course, the first coating surface density preset in the embodiment of the present application can also be controlled within a range of 150-200 g / m 2 Between (for example but not limited to 150g / m 2 , 160g / m 2 , 170g / m 2 , 180g / m 2 , 190g / m 2 Or 200g / m 2 ), the preset first compaction density can also be controlled at 1.4-1.7g / cm 3 Between (for example but not limited to 1.4g / cm 3 , 1.45g / cm 3 , 1.5g / cm3 , 1.55g / cm 3 , 1.6g / cm 3 , 1.65g / cm 3 Or 1.7g / cm 3 ) to ensure the stability of the negative electrode.
[0030] Next, after the negative electrode slurry is rolled, the battery preparation device can also use a cutter to cut the negative electrode slurry after the rolling process according to a preset first size to obtain a plurality of negative electrode test electrodes. The preset first size can be but is not limited to a width of 62 mm and a length of 93 mm, and the number of the negative electrode test electrodes can also be determined according to a preset number of stacking layers input by a user. For example, when the preset number of stacking layers is 12 layers, the number of negative electrode test electrodes can be but is not limited to 13, and is not limited to this.
[0031] Next, after preparing a plurality of negative electrode test electrodes, the battery preparation device can also mix lithium iron phosphate (LiFePO4), conductive carbon black (SP), polyvinylidene fluoride (PVDF) and carbon nanotubes (CNT) according to a preset second ratio, and use N-methylpyrrolidone (NMP) as a solvent to obtain a positive electrode slurry. The proportions of lithium iron phosphate, conductive carbon black, polyvinylidene fluoride and carbon nanotubes in the preset second ratio can be, but are not limited to, 96.5%, 1.0%, 2.0% and 0.5%. Of course, in the embodiment of the present application, the proportion of lithium iron phosphate can also be controlled between 95% and 98%, the proportion of conductive carbon black can also be controlled between 1% and 3%, the proportion of polyvinylidene fluoride can also be controlled between 1% and 3%, and the proportion of carbon nanotubes can also be controlled between 0% and 2%, and are not limited thereto.
[0032] Next, after obtaining the positive electrode slurry, the positive electrode slurry can also be coated on a 14 μm thick carbon-coated aluminum foil by a battery preparation device, and a continuous oven set at a temperature between 100 and 120° C. is used to coat and dry the positive electrode slurry according to a preset second coating surface density. The preset second coating surface density can be, but is not limited to, 370 g / m 2 The negative electrode slurry after the coating and drying treatment can also be subjected to roller pressing treatment by a roller press machine with a roller pressing pressure set to 60T according to a preset second compaction density, and the preset second compaction density can be but is not limited to 2.55g / cm 3 Of course, the second coating surface density preset in the embodiment of the present application can also be controlled within the range of 350-410 g / m 2 Between (for example but not limited to 350g / m 2 , 360g / m 2 , 370g / m2 , 380g / m 2 , 390g / m 2 , 400g / m 2 Or 410g / m 2 ), the preset second compaction density can also be controlled at 2.4-2.8 g / cm 3 Between (for example but not limited to 2.4g / cm 3 , 2.5g / cm 3 , 2.6g / cm 3 , 2.7g / cm 3 , or 2.8g / cm 3 ) to ensure the stability of the positive electrode.
[0033] Next, after the positive electrode slurry is roll-pressed, the battery preparation device can also use a cutting device to cut the positive electrode material after the rolling process according to a preset second size to obtain a plurality of positive electrode test electrodes. The preset second size can be but is not limited to a width of 59 mm and a length of 90 mm, and the number of the positive electrode test electrodes can also be determined according to the preset number of stacking layers input by the user. For example, when the preset number of stacking layers is 12 layers, the number of positive electrode test electrodes can be but is not limited to being set to 12, and is not limited to this.
[0034] As another option of the embodiment of the present application, a soft-pack battery cell is prepared according to the positive and negative test electrodes and the preset reference electrode, including: Performing lithium plating treatment on a preset reference electrode according to preset lithium plating parameters; Based on the preset number of stacked layers, the number of negative test electrodes, the number of positive test electrodes, the preset number of reference electrodes after lithium plating, and the number of diaphragms are determined respectively, and according to the number of negative test electrodes, the number of positive test electrodes, the preset number of reference electrodes after lithium plating, and the number of diaphragms, soft-pack battery cells are prepared.
[0035] Specifically, after preparing a plurality of positive electrode test pole pieces and a plurality of negative electrode test pole pieces respectively, the test terminal can also send the preparation process of the soft-pack battery cell to the battery preparation device, so that the battery preparation device first uses the nickel sheet as the pole ear of the preset reference electrode, welds the nickel sheet to the preset reference electrode through the tin bar, and performs forward charging and reverse discharging lithium plating on the preset reference electrode according to the preset lithium plating parameters, and repeats multiple times until the preset total time or the preset lithium layer thickness is reached, thereby ensuring the potential stability of the preset reference electrode. Here, the preset reference electrode can be but not limited to copper wire, and the preset lithium plating parameters can be but not limited to lithium plating current and lithium plating time, the lithium plating current can be controlled between 5uA-30uA (for example, but not limited to 5uA, 10uA, 15uA, 20uA, 25uA or 30uA), and the lithium plating time can be controlled between 2h-6h (for example, but not limited to 2h, 3h, 4h, 5h or 6h).
[0036] Next, taking the above-mentioned preset number of stacking layers of 12 as an example, it can be determined that the number of negative test sheets is 13, the number of positive test sheets is 12, the number of preset reference electrodes after lithium plating is 12, and the number of diaphragms is 12. The battery preparation device performs stacking treatment on all negative test sheets, all positive test sheets, all preset reference electrodes and all diaphragms, and during the stacking process, a diaphragm is arranged between each positive test sheet and the adjacent negative test sheet, and a preset reference electrode can be fixed in the middle of each diaphragm. A mixed solution can be prepared with, but not limited to, a 1 mol / L lithium hexafluorophosphate (LiPF6) solution as the electrolyte and a solvent with a volume ratio of ethylene carbonate (EC): ethyl carbonate (DMC) = 1:1, so that all sheets after the stacking treatment are injected with the mixed solution, left to stand at room temperature, formed, and divided into different volumes, so as to obtain a soft-pack battery cell. Here, the type of the separator may be a single-sided ceramic polyethylene (PE) based film, but is not limited thereto.
[0037] Of course, in the embodiment of the present application, all negative test electrodes, all positive test electrodes, all preset reference electrodes and all diaphragms can be stacked, and then all preset reference electrodes can be forward charged and reverse discharged for lithium plating, and this can be repeated multiple times until a preset total time or a preset lithium layer thickness is reached. This is also not limited to this.
[0038] Step 104: Determine the nominal capacity based on the soft-pack battery cell and two sets of preset charge and discharge parameters.
[0039] Specifically, after the soft-pack battery cell is prepared by the battery preparation device, the test terminal can, but is not limited to, control the transfer of the soft-pack battery cell to the test cabinet for a period of time manually or according to the automatic control program, and send two sets of preset charge and discharge parameters to the battery test device, so that the battery test device can perform multiple charge and discharge processes on the soft-pack battery cell according to the preset charge and discharge parameters, and use the capacity of the soft-pack battery cell finally discharged as the nominal capacity. Here, the standing time can be, but is not limited to, set to 6 hours.
[0040] As another option of the embodiment of the present application, the two sets of preset charge and discharge parameters include a discharge parameter consisting of a charge and discharge rate and a discharge cut-off voltage, and a charge parameter consisting of a charge and discharge rate and a charge cut-off voltage, and the discharge cut-off voltage is less than the charge cut-off voltage; Based on the soft-pack battery and two sets of preset charge and discharge parameters, the nominal capacity is determined, including: The soft-pack battery cell is placed in a static state according to a preset static state time, and the soft-pack battery cell is discharged according to a discharge parameter after the static state treatment; The soft-packed battery cells after the discharge treatment are placed in a shelf state according to a preset shelf time, and the soft-packed battery cells after the shelf state are charged according to charging parameters; The soft-packed battery cells after the charge treatment are placed in a shelf state according to a preset placement time, and the soft-packed battery cells after the placement treatment are discharged according to the discharge parameters, so as to use the corresponding discharge capacity as the nominal capacity.
[0041] In order to ensure the rationality of charging and discharging, the two sets of preset charging and discharging parameters can be divided into a set of charging parameters and a set of discharging parameters. The charging parameters may include charging and discharging rates and discharge cut-off voltages. The discharging parameters may include charging and discharging parameters and charging cut-off voltages. The charging and discharging rates can be understood as the constant current density corresponding to the specified capacity during the charging and discharging process (for example, one hour charging and discharging xx capacity), for example, which can be set between 0.01C-2C (for example but not limited to 0.01C, 0.1C, 0.2C, 0.5C, 1C or 2C).
[0042] Specifically, when the battery testing device performs multiple charge and discharge treatments on the soft-pack battery cells according to preset charge and discharge parameters, it is also possible but not limited to that after the soft-pack battery cells have been stationary in the test cabinet for a preset standing time (for example, which can be set to 6 hours), the soft-pack battery cells after the standing treatment are discharged according to the discharge parameters, for example, but not limited to discharging at a 1C constant current to a cut-off voltage of 2.5V, and after the discharge treatment of the soft-pack battery cells is completed, the soft-pack battery cells after the discharge treatment are placed for a preset placement time, which can be but not limited to being set to 10 minutes, and then the soft-pack battery cells after the placement treatment are charged according to the charging parameters, for example, but not limited to charging at a 1C constant current to a cut-off voltage of 3.65V.
[0043] Then, after completing one charge and discharge cycle of the soft-pack battery cell, the battery testing device can also perform multiple charge and discharge cycle treatments on the soft-pack battery cell in the above manner (for example but not limited to three times), until the soft-pack battery cell after the shelving treatment is finally discharged according to the discharge parameters, and the capacity corresponding to the final discharge process is used as the nominal capacity.
[0044] It should be noted that the test cabinet in the embodiment of the present application can be but is not limited to the Xinwei test cabinet, and the temperature of the entire charging and discharging process is maintained at about 25°C.
[0045] Step 106: Generate at least two groups of test capacity parameters according to the nominal capacity, and test the soft-pack battery cells in turn according to each group of test capacity parameters to obtain corresponding voltage-time curves and negative electrode to lithium potential curves.
[0046] Specifically, after the nominal capacity of the soft-pack battery cell is determined by the battery testing device, the testing terminal may, but is not limited to, generate multiple groups of test capacity parameters according to the nominal capacity fed back by the battery testing device. Among them, each group of test capacity parameters may include a charging rate corresponding to the nominal capacity, a preset charging ratio parameter and a preset relaxation time, the charging rate can be set between 1C-6C (for example, but not limited to 1C, 2, 3C, 4C, 5C or 6C), the preset charging ratio parameter can be set between the starting charging ratio and the ending charging ratio (the starting charging ratio can be but not limited to 40%, and the ending charging ratio can be but not limited to 70%, 80%, 90% or 100%), the difference between two preset charging ratio parameters in any two adjacent groups of test capacity parameters is fixed and can be set between 1%-15% (for example, but not limited to 1%, 2%, 3%, 5%, 10% or 15%), and the preset relaxation time can be set between 10min-60min (for example, but not limited to 10min, 20min, 30min, 40min, 50min or 60min).
[0047] Of course, each set of test capacity parameters in the embodiment of the present application may also include a discharge rate and a cut-off voltage corresponding to the nominal capacity, that is, after processing according to the above-mentioned charging rate, preset charging ratio parameters and preset relaxation time, the voltage of the soft-pack battery cell must be discharged according to the discharge rate to be consistent with the cut-off voltage, and after a specified shelf time, the test can be performed again according to the next set of test capacity parameters.
[0048] As another option of the embodiment of the present application, at least two groups of test capacity parameters are generated according to the nominal capacity, including: Obtaining a first set of test capacity parameters based on the nominal capacity, a preset first charging ratio parameter, and a preset relaxation time; Based on the nominal capacity, the preset second charging ratio parameter and the preset relaxation time, a second set of test capacity parameters is obtained; Based on the nominal capacity, the preset third charging ratio parameter and the preset relaxation time, a third set of test capacity parameters is obtained; wherein the difference between the preset second charging ratio parameter and the preset first charging ratio parameter is consistent with the difference between the preset third charging ratio parameter and the preset second charging ratio parameter.
[0049] Specifically, taking the number of groups of test capacity parameters as three groups and the nominal capacity represented as C as an example, the test terminal can also, but is not limited to, set the charging rate to 4C according to the nominal capacity, and set the preset first charging ratio parameter to 40%, and the preset relaxation time to 20min, thereby obtaining a first group of test capacity parameters including a charging rate of 4C, a charging ratio parameter of 40%, and a relaxation time of 20min (of course, the first group of test capacity parameters may also include a discharge rate of 1C and a cut-off voltage of 2.5V); then, the difference between any two adjacent charging ratio parameters may be set to 5%, that is, the preset second charging ratio parameter. The parameter is 45%, thereby obtaining the first set of test capacity parameters including a charge rate of 4C, a charge ratio parameter of 45% and a relaxation time of 20min (of course, the second set of test capacity parameters may also include a discharge rate of 1C and a cut-off voltage of 2.5V); then, according to the above setting, the difference between any two adjacent charge ratio parameters is 5%, that is, the preset third charge ratio parameter is 50%, thereby obtaining the third set of test capacity parameters including a charge rate of 4C, a charge ratio parameter of 50% and a relaxation time of 20min (of course, the second set of test capacity parameters may also include a discharge rate of 1C and a cut-off voltage of 2.5V).
[0050] It should be noted that the number of test capacity parameter groups in the embodiment of the present application is not limited to three groups. For example, the charging ratio parameter in the first group of test capacity parameters can be set to 40%, and the charging ratio parameter in the last group of test capacity parameters can be set to 80%. The difference between any two adjacent charging ratio parameters is set to 5%, generating a total of nine groups, and is not limited to this.
[0051] Furthermore, after generating multiple groups of test capacity parameters, the test terminal can also send all the test capacity parameters to the battery testing device, so that the battery testing device can test the soft-pack battery cells according to all the test capacity parameters, and can record the voltage-time curve corresponding to each group of test capacity parameters and the negative electrode to lithium potential curve corresponding to all the test capacity parameters in real time during the test process.
[0052] Here, when the battery testing device tests the soft-pack battery cell according to all the test capacity parameters, it can be but not limited to referring to the above embodiment, so that after the soft-pack battery cell is allowed to stand for 30 minutes, the battery testing device charges it to 40% at a constant current at a charging rate of 4C, with a relaxation time of 20 minutes, and discharges it to 2.5V at a constant current at a discharge rate of 1C; then, the soft-pack battery cell can be left for 30 minutes, charged to 45% at a constant current at a charging rate of 4C, with a relaxation time of 20 minutes, and discharged to 2.5V at a constant current at a discharge rate of 1C; the difference between two adjacent groups of charging ratio parameters in each group of test capacity parameters is set to 5% until it reaches 80%.
[0053] Step 108: Differentiate each voltage-time curve to obtain a corresponding differential voltage-time curve, and determine the lithium deposition starting potential of the soft-pack battery cell based on all voltage-time curves, all differential voltage-time curves, and the negative electrode to lithium potential curve.
[0054] Specifically, after the battery testing device obtains the voltage-time curve corresponding to each set of test capacity parameters, the test terminal can receive all voltage-time curves fed back by the battery testing device, and differentiate each voltage-time curve to obtain the corresponding differential voltage-time curve, so as to determine the lithium plating window of the soft-pack battery cell by combining the voltage-time curve corresponding to each set of test capacity parameters and the differential voltage-time curve, and determine the corresponding lithium plating starting potential in the negative electrode to lithium potential curve according to the lithium plating window. Compared with the prior art that takes the negative electrode to lithium potential of 0V as the lithium plating starting point, it can not only ensure the accuracy of the lithium plating starting potential, but also make the subsequent step charging strategy formulation more reasonable, thereby improving the overall testing experience.
[0055] As another option of the embodiment of the present application, the lithium precipitation starting potential of the soft-pack battery cell is determined according to all voltage-time curves, all differential voltage-time curves and the negative electrode to lithium potential curve, including: When an abnormal slope change is detected in the voltage-time curve corresponding to the nth group of test capacity parameters, it is determined whether there is a characteristic peak in the corresponding differential voltage-time curve; wherein n is a positive integer greater than 1; When a characteristic peak is detected in the differential voltage-time curve, the lithium plating starting potential of the soft-pack battery cell is determined according to the voltage-time curve, the differential voltage-time curve and the negative electrode to lithium potential curve corresponding to the n-1th group of test capacity parameters.
[0056] Specifically, when determining the lithium plating starting potential of the soft-pack battery cell, the test terminal may, but is not limited to, perform feature point recognition processing on the voltage-time curve corresponding to each set of test capacity parameters, identify multiple continuous feature points corresponding to each voltage-time curve, and calculate multiple slopes according to the coordinates of two consecutive feature points in the corresponding voltage-time curve, and use the difference between two adjacent slopes as the slope change to determine whether there is a platform in the corresponding voltage-time curve by using whether the slope change is abnormal, that is, indicating that lithium plating may occur. Here, the basis for judging whether the slope change is abnormal may be, but is not limited to, when it is detected that the difference between any two adjacent slope changes exceeds a preset difference threshold, or when it is detected that any slope change is not in a preset slope change interval, it can be determined that the slope change is abnormal, otherwise it is not abnormal, and it is not limited to this.
[0057] Next, when an abnormal slope change is detected in the voltage-time curve corresponding to any set of test capacity parameters, the test terminal can identify the characteristic peak of the corresponding differential voltage-time curve to determine whether the corresponding test capacity parameter has caused lithium deposition in the soft-pack battery cell by judging whether the differential voltage-time curve has a characteristic peak. It is understandable that the method of identifying the characteristic peak of the differential voltage-time curve can also be determined by calculating the slope of the characteristic points, or by judging whether the differential voltage-time curve has an inflection point, etc., which will not be elaborated here. Next, when the presence of a characteristic peak is identified in the corresponding differential voltage-time curve, it indicates that when the soft-pack battery cell is tested according to the corresponding test capacity parameters, lithium deposition has occurred in the soft-pack battery cell, and then the voltage-time curve and the differential voltage-time curve determined when the soft-pack battery cell is tested by combining the previous set of test capacity parameters can be used to further determine whether lithium deposition has occurred in the soft-pack battery cell. It is understandable that when the current set of test capacity parameters is used to test the soft-pack battery cell and it is determined that no lithium deposition has occurred, it can be indicated that the lithium deposition window of the soft-pack battery cell is between the preset charging ratio parameters corresponding to the previous set of test capacity parameters and the preset charging ratio parameters corresponding to the current set of test capacity parameters.
[0058] As another option of the embodiment of the present application, the lithium precipitation starting potential of the soft-pack battery cell is determined according to the voltage-time curve, the differential voltage-time curve and the negative electrode to lithium potential curve corresponding to the n-1 group of test capacity parameters, including: When no abnormal slope change is detected in the voltage-time curve corresponding to the n-1th group of test capacity parameters, it is determined whether there is a characteristic peak in the corresponding differential voltage-time curve; When no characteristic peak is detected in the differential voltage-time curve, a first potential corresponding to the nth group of test capacity parameters and a second potential corresponding to the n-1th group of test capacity parameters are respectively determined in the negative electrode to lithium potential curve; The lithium deposition starting point potential of the soft-pack battery cell is determined according to the potential interval formed by the first potential and the second potential.
[0059] Specifically, when analyzing and processing the voltage-time curve and the differential voltage-time curve corresponding to the n-1 group of test capacity parameters, you can but are not limited to referring to the above embodiments, which will not be described in detail here. When it is determined that no abnormal slope change is detected in the voltage-time curve corresponding to the n-1 group of test capacity parameters, and no characteristic peak is detected in the differential voltage-time curve, it indicates that the lithium precipitation window of the soft-pack battery cell is between the charging ratio parameters in the n-1 group of test capacity parameters and the charging ratio parameters in the nth group of test capacity parameters. Then, the test terminal can find out the first potential corresponding to the charging ratio parameters in the nth group of test capacity parameters and the second potential corresponding to the charging ratio parameters in the n-1 group of test capacity parameters in the negative electrode to lithium potential curve. At this time, the lithium precipitation starting potential of the soft-pack battery cell is within the potential interval formed by the first potential and the second potential.
[0060] Next, after obtaining the potential interval formed by the first potential and the second potential, the test terminal can also, but is not limited to, use any potential within the potential interval as the starting potential for lithium deposition of the soft-pack battery cell. Of course, the median corresponding to the potential interval can also be used as the starting potential for lithium deposition of the soft-pack battery cell, but is not limited to this.
[0061] Also see here Figure 2 A schematic diagram showing a voltage-time curve and a differential voltage-time curve of a soft-pack battery cell provided in an embodiment of the present application is shown, and Figure 3 Schematic diagram of voltage-time curve and differential voltage-time curve of another soft-pack battery cell provided in an embodiment of the present application is shown. Figure 2 As shown in 3, Figure 2 The voltage-time curve and differential voltage-time curve in the figure can be obtained by testing the test capacity parameter with a charging ratio parameter of 60%. Figure 2 The voltage-time curve in the figure does not have abnormal slope change, and the differential voltage-time curve does not have a characteristic peak; Figure 3 The voltage-time curve and differential voltage-time curve in the figure can be obtained by testing the test capacity parameter with a charging ratio parameter of 65%. Figure 3 The voltage-time curve in the graph has an abnormal slope change, and the differential voltage-time curve has a characteristic peak, that is, the lithium plating window of the soft-pack battery cell is when the charging ratio parameter is set between 60% and 65%.
[0062] Also see here Figure 4 The schematic diagram of the negative electrode to lithium potential curve of a soft-pack battery cell provided in an embodiment of the present application is shown in FIG. Figure 4 As shown, combined with the above Figure 2 as well as Figure 3 The lithium plating window of the soft-pack battery cell is determined to be between 60% and 65% of the charging ratio parameter setting. Figure 4 The potential corresponding to the charging ratio parameter of 60% (-0.048V in the figure) and the potential corresponding to the charging ratio parameter of 65% (-0.055V in the figure) are found respectively, and it can be concluded that the starting potential of lithium precipitation of the soft-pack battery cell is between -0.048V and -0.055V. It should be noted that if the existing technology is used to take the negative electrode potential of 0 V as the starting potential of lithium precipitation of the battery cell, then combined with Figure 2 , Figure 3 as well as Figure 4 It can be inferred that the corresponding lithium precipitation window should be smaller than the charging ratio parameter set at 40% (according to Figure 4 The potential corresponding to the charging ratio parameter of 40% is -0.02V), which is quite different from the actual lithium plating window, which may easily lead to unreasonable formulation of subsequent step-charging strategies and affect the overall testing experience.
[0063] See also Figure 5 , Figure 5 A structural schematic diagram of a lithium plating starting point potential detection device for a soft-pack battery cell provided in an embodiment of the present application is shown.
[0064] like Figure 5 As shown, the lithium plating starting point potential detection device of the soft-pack battery cell may at least include a battery cell preparation module 501, a capacity determination module 502, a data generation module 503 and a result determination module 504, wherein: The battery cell preparation module 501 is used to prepare samples according to at least two electrode materials to obtain positive and negative electrode test electrodes, and to prepare soft-pack battery cells according to the positive and negative electrode test electrodes and preset reference electrodes; A capacity determination module 502, configured to determine a nominal capacity based on the soft-pack battery cell and two sets of preset charge and discharge parameters; The data generation module 503 is used to generate at least two groups of test capacity parameters according to the nominal capacity, and test the soft-pack battery cells in turn according to each group of test capacity parameters to obtain corresponding voltage-time curves and negative electrode to lithium potential curves; The result determination module 504 is used to perform differentiation processing on each voltage-time curve to obtain a corresponding differential voltage-time curve, and determine the lithium precipitation starting potential of the soft-pack battery cell based on all voltage-time curves, all differential voltage-time curves and the negative electrode to lithium potential curve.
[0065] In some possible embodiments, the positive and negative electrode test electrodes are obtained by sample preparation according to at least two electrode materials, including: Mixing artificial graphite, conductive carbon black, sodium carboxymethyl cellulose and styrene-butadiene rubber latex according to a preset first ratio to obtain a negative electrode slurry; The negative electrode slurry is coated and dried according to a preset first coating surface density, and the negative electrode slurry after the coating and drying is roll-pressed according to a preset first compaction density; Cutting the negative electrode slurry after the roll pressing process according to a preset first size to obtain at least two negative electrode test pole pieces; Mixing lithium iron phosphate, conductive carbon black, polyvinylidene fluoride and carbon nanotubes according to a preset second ratio to obtain a positive electrode slurry; The positive electrode slurry is coated and dried according to a preset second coating surface density, and the positive electrode slurry after the coating and drying is roll-pressed according to a preset second compaction density; The positive electrode slurry after the roll pressing process is cut according to a preset second size to obtain at least two positive electrode test pole pieces.
[0066] In some possible embodiments, a soft-pack battery cell is prepared according to the positive and negative test electrodes and a preset reference electrode, including: Performing lithium plating treatment on a preset reference electrode according to preset lithium plating parameters; Based on the preset number of stacked layers, the number of negative test electrodes, the number of positive test electrodes, the preset number of reference electrodes after lithium plating, and the number of diaphragms are determined respectively, and according to the number of negative test electrodes, the number of positive test electrodes, the preset number of reference electrodes after lithium plating, and the number of diaphragms, soft-pack battery cells are prepared.
[0067] In some possible embodiments, the two sets of preset charge and discharge parameters include a discharge parameter consisting of a charge and discharge rate and a discharge cut-off voltage, and a charge parameter consisting of a charge and discharge rate and a charge cut-off voltage, and the discharge cut-off voltage is less than the charge cut-off voltage; Based on the soft-pack battery and two sets of preset charge and discharge parameters, the nominal capacity is determined, including: The soft-pack battery cell is placed in a static state according to a preset static state time, and the soft-pack battery cell is discharged according to a discharge parameter after the static state treatment; The soft-packed battery cells after the discharge treatment are placed in a shelf state according to a preset shelf time, and the soft-packed battery cells after the shelf state are charged according to charging parameters; The soft-packed battery cells after the charge treatment are placed in a shelf state according to a preset placement time, and the soft-packed battery cells after the placement treatment are discharged according to the discharge parameters, so as to use the corresponding discharge capacity as the nominal capacity.
[0068] In some possible embodiments, at least two groups of test capacity parameters are generated according to the nominal capacity, including: Obtaining a first set of test capacity parameters based on the nominal capacity, a preset first charging ratio parameter, and a preset relaxation time; Based on the nominal capacity, the preset second charging ratio parameter and the preset relaxation time, a second set of test capacity parameters is obtained; Based on the nominal capacity, the preset third charging ratio parameter and the preset relaxation time, a third set of test capacity parameters is obtained; wherein the difference between the preset second charging ratio parameter and the preset first charging ratio parameter is consistent with the difference between the preset third charging ratio parameter and the preset second charging ratio parameter.
[0069] In some possible embodiments, the lithium precipitation starting potential of the soft-pack battery cell is determined according to all voltage-time curves, all differential voltage-time curves, and the negative electrode to lithium potential curve, including: When an abnormal slope change is detected in the voltage-time curve corresponding to the nth group of test capacity parameters, it is determined whether there is a characteristic peak in the corresponding differential voltage-time curve; wherein n is a positive integer greater than 1; When a characteristic peak is detected in the differential voltage-time curve, the lithium plating starting potential of the soft-pack battery cell is determined according to the voltage-time curve, the differential voltage-time curve and the negative electrode to lithium potential curve corresponding to the n-1th group of test capacity parameters.
[0070] In some possible embodiments, the lithium precipitation starting potential of the soft-pack battery cell is determined according to the voltage-time curve, the differential voltage-time curve, and the negative electrode to lithium potential curve corresponding to the n-1th group of test capacity parameters, including: When no abnormal slope change is detected in the voltage-time curve corresponding to the n-1th group of test capacity parameters, it is determined whether there is a characteristic peak in the corresponding differential voltage-time curve; When no characteristic peak is detected in the differential voltage-time curve, a first potential corresponding to the nth group of test capacity parameters and a second potential corresponding to the n-1th group of test capacity parameters are respectively determined in the negative electrode to lithium potential curve; The lithium deposition starting point potential of the soft-pack battery cell is determined according to the potential interval formed by the first potential and the second potential.
[0071] Those skilled in the art can clearly understand that the technical solutions of the embodiments of the present application can be implemented with the help of software and / or hardware. The "unit" and "module" in this specification refer to software and / or hardware that can independently complete or cooperate with other components to complete specific functions, where the hardware can be, for example, a field programmable gate array (FPGA), an integrated circuit (IC), etc.
[0072] See also Figure 6 , Figure 6 A structural schematic diagram of another soft-pack battery cell lithium plating starting point potential detection device provided in an embodiment of the present application is shown.
[0073] like Figure 6 As shown, the lithium plating starting point potential detection device 600 for the soft-pack battery cell may include at least one processor 601 , at least one network interface 604 , a user interface 603 , a memory 605 and at least one communication bus 602 .
[0074] The communication bus 602 may be used to realize the connection and communication among the above-mentioned components.
[0075] The user interface 603 may include buttons, and the optional user interface may also include a standard wired interface or a wireless interface.
[0076] The network interface 604 may include, but is not limited to, a Bluetooth module, an NFC module, a Wi-Fi module, etc.
[0077] Among them, the processor 601 may include one or more processing cores. The processor 601 uses various interfaces and lines to connect the various parts of the lithium starting potential detection device 600 for the soft-pack battery cell, and executes various functions and processes data of the lithium starting potential detection device 600 for the routing soft-pack battery cell by running or executing instructions, programs, code sets or instruction sets stored in the memory 605, and calling the data stored in the memory 605. Optionally, the processor 601 can be implemented in at least one hardware form of DSP, FPGA, and PLA. The processor 601 can integrate one or a combination of CPU, GPU, modem, etc. Among them, the CPU mainly processes the operating system, user interface, and application programs; the GPU is responsible for rendering and drawing the content to be displayed on the display screen; the modem is used to process wireless communications. It can be understood that the above-mentioned modem may not be integrated into the processor 601, but may be implemented by a single chip.
[0078] The memory 605 may include a RAM or a ROM. Optionally, the memory 605 includes a non-transitory computer-readable medium. The memory 605 may be used to store instructions, programs, codes, code sets or instruction sets. The memory 605 may include a program storage area and a data storage area, wherein the program storage area may store instructions for implementing an operating system, instructions for at least one function (such as a touch function, a sound playback function, an image playback function, etc.), instructions for implementing the above-mentioned various method embodiments, etc.; the data storage area may store data involved in the above-mentioned various method embodiments, etc. The memory 605 may optionally be at least one storage device located away from the aforementioned processor 601. As Figure 6 As shown, the memory 605 as a computer storage medium may include an operating system, a network communication module, a user interface module, and an application program for detecting the lithium plating starting potential of the soft-pack battery cell.
[0079] Specifically, the processor 601 can be used to call the lithium plating starting point potential detection application for the soft-pack battery cell stored in the memory 605, and specifically perform the following operations: Performing sample preparation according to at least two electrode materials to obtain positive and negative electrode test electrodes, and preparing soft-pack battery cells according to the positive and negative electrode test electrodes and preset reference electrodes; Based on the soft-pack battery cell and two sets of preset charge and discharge parameters, the nominal capacity is determined; Generate at least two groups of test capacity parameters according to the nominal capacity, and test the soft-pack battery cells in turn according to each group of test capacity parameters to obtain corresponding voltage-time curves and negative electrode to lithium potential curves; Each voltage-time curve is differentiated to obtain the corresponding differential voltage-time curve, and the lithium plating starting potential of the soft-pack battery cell is determined based on all voltage-time curves, all differential voltage-time curves and the negative electrode to lithium potential curve.
[0080] In some possible embodiments, the positive and negative electrode test electrodes are obtained by sample preparation according to at least two electrode materials, including: Mixing artificial graphite, conductive carbon black, sodium carboxymethyl cellulose and styrene-butadiene rubber latex according to a preset first ratio to obtain a negative electrode slurry; The negative electrode slurry is coated and dried according to a preset first coating surface density, and the negative electrode slurry after the coating and drying is roll-pressed according to a preset first compaction density; Cutting the negative electrode slurry after the roll pressing process according to a preset first size to obtain at least two negative electrode test pole pieces; Mixing lithium iron phosphate, conductive carbon black, polyvinylidene fluoride and carbon nanotubes according to a preset second ratio to obtain a positive electrode slurry; The positive electrode slurry is coated and dried according to a preset second coating surface density, and the positive electrode slurry after the coating and drying is roll-pressed according to a preset second compaction density; The positive electrode slurry after the roll pressing process is cut according to a preset second size to obtain at least two positive electrode test pole pieces.
[0081] In some possible embodiments, a soft-pack battery cell is prepared according to the positive and negative test electrodes and a preset reference electrode, including: Performing lithium plating treatment on a preset reference electrode according to preset lithium plating parameters; Based on the preset number of stacked layers, the number of negative test electrodes, the number of positive test electrodes, the preset number of reference electrodes after lithium plating, and the number of diaphragms are determined respectively, and according to the number of negative test electrodes, the number of positive test electrodes, the preset number of reference electrodes after lithium plating, and the number of diaphragms, soft-pack battery cells are prepared.
[0082] In some possible embodiments, the two sets of preset charge and discharge parameters include a discharge parameter consisting of a charge and discharge rate and a discharge cut-off voltage, and a charge parameter consisting of a charge and discharge rate and a charge cut-off voltage, and the discharge cut-off voltage is less than the charge cut-off voltage; Based on the soft-pack battery and two sets of preset charge and discharge parameters, the nominal capacity is determined, including: The soft-pack battery cell is placed in a static state according to a preset static state time, and the soft-pack battery cell is discharged according to a discharge parameter after the static state treatment; The soft-packed battery cells after the discharge treatment are placed in a shelf state according to a preset shelf time, and the soft-packed battery cells after the shelf state are charged according to charging parameters; The soft-packed battery cells after the charge treatment are placed in a shelf state according to a preset placement time, and the soft-packed battery cells after the placement treatment are discharged according to the discharge parameters, so as to use the corresponding discharge capacity as the nominal capacity.
[0083] In some possible embodiments, at least two groups of test capacity parameters are generated according to the nominal capacity, including: Obtaining a first set of test capacity parameters based on the nominal capacity, a preset first charging ratio parameter, and a preset relaxation time; Based on the nominal capacity, the preset second charging ratio parameter and the preset relaxation time, a second set of test capacity parameters is obtained; Based on the nominal capacity, the preset third charging ratio parameter and the preset relaxation time, a third set of test capacity parameters is obtained; wherein the difference between the preset second charging ratio parameter and the preset first charging ratio parameter is consistent with the difference between the preset third charging ratio parameter and the preset second charging ratio parameter.
[0084] In some possible embodiments, the lithium precipitation starting potential of the soft-pack battery cell is determined according to all voltage-time curves, all differential voltage-time curves, and the negative electrode to lithium potential curve, including: When an abnormal slope change is detected in the voltage-time curve corresponding to the nth group of test capacity parameters, it is determined whether there is a characteristic peak in the corresponding differential voltage-time curve; wherein n is a positive integer greater than 1; When a characteristic peak is detected in the differential voltage-time curve, the lithium plating starting potential of the soft-pack battery cell is determined according to the voltage-time curve, the differential voltage-time curve and the negative electrode to lithium potential curve corresponding to the n-1th group of test capacity parameters.
[0085] In some possible embodiments, the lithium precipitation starting potential of the soft-pack battery cell is determined according to the voltage-time curve, the differential voltage-time curve, and the negative electrode to lithium potential curve corresponding to the n-1th group of test capacity parameters, including: When no abnormal slope change is detected in the voltage-time curve corresponding to the n-1th group of test capacity parameters, it is determined whether there is a characteristic peak in the corresponding differential voltage-time curve; When no characteristic peak is detected in the differential voltage-time curve, a first potential corresponding to the nth group of test capacity parameters and a second potential corresponding to the n-1th group of test capacity parameters are respectively determined in the negative electrode to lithium potential curve; The lithium deposition starting point potential of the soft-pack battery cell is determined according to the potential interval formed by the first potential and the second potential.
[0086] The present application also provides a computer-readable storage medium on which a computer program is stored, and when the program is executed by a processor, the steps of the above method are implemented. The computer-readable storage medium may include, but is not limited to, any type of disk, including a floppy disk, an optical disk, a DVD, a CD-ROM, a micro drive, and a magneto-optical disk, a ROM, a RAM, an EPROM, an EEPROM, a DRAM, a VRAM, a flash memory device, a magnetic card or an optical card, a nanosystem (including a molecular memory IC), or any type of medium or device suitable for storing instructions and / or data.
[0087] In the several embodiments provided in the present application, it should be understood that the disclosed devices can be implemented in other ways. For example, the device embodiments described above are only schematic, such as the division of units, which is only a logical function division. There may be other division methods in actual implementation, such as multiple units or components can be combined or integrated into another system, or some features can be ignored or not executed. Another point is that the mutual coupling or direct coupling or communication connection shown or discussed can be through some service interfaces, and the indirect coupling or communication connection of devices or units can be electrical or other forms.
[0088] In addition, each functional unit in each embodiment of the present application may be integrated into one processing unit, or each unit may exist physically separately, or two or more units may be integrated into one unit. The above-mentioned integrated unit may be implemented in the form of hardware or in the form of software functional units.
[0089] If the integrated unit is implemented in the form of a software functional unit and sold or used as an independent product, it can be stored in a computer-readable memory. Based on this understanding, the technical solution of the present application, or the part that contributes to the prior art, or all or part of the technical solution can be embodied in the form of a software product. The computer software product is stored in a memory, including a number of instructions to enable a computer device (which can be a personal computer, server or network device, etc.) to execute all or part of the steps of the various embodiments of the present application. The aforementioned memory includes: U disk, read-only memory (ROM), random access memory (RAM), mobile hard disk, disk or optical disk and other media that can store program codes.
Claims
1. A method for detecting the starting potential of lithium deposition of a soft-pack battery cell, characterized in that: include: Performing sample preparation according to at least two electrode materials to obtain positive and negative electrode test electrodes, and preparing soft-pack battery cells according to the positive and negative electrode test electrodes and preset reference electrodes; Determining a nominal capacity based on the soft-pack battery cell and two sets of preset charge and discharge parameters; Generate at least two groups of test capacity parameters according to the nominal capacity, and test the soft-pack battery cells in turn according to each group of test capacity parameters to obtain corresponding voltage-time curves and negative electrode to lithium potential curves; Each of the voltage-time curves is differentiated to obtain a corresponding differential voltage-time curve, and the lithium precipitation starting potential of the soft-pack battery cell is determined based on all the voltage-time curves, all the differential voltage-time curves and the negative electrode to lithium potential curve.
2. The method according to claim 1, characterized in that The method of preparing samples according to at least two electrode materials to obtain positive and negative electrode test electrodes comprises: Mixing artificial graphite, conductive carbon black, sodium carboxymethyl cellulose and styrene-butadiene rubber latex according to a preset first ratio to obtain a negative electrode slurry; Performing coating and drying treatment on the negative electrode slurry according to a preset first coating surface density, and performing roller pressing treatment on the negative electrode slurry after coating and drying treatment according to a preset first compaction density; Cutting the negative electrode slurry after the rolling process according to a preset first size to obtain at least two negative electrode test pole pieces; Mixing the lithium iron phosphate, the conductive carbon black, the polyvinylidene fluoride and the carbon nanotubes according to a preset second ratio to obtain a positive electrode slurry; The positive electrode slurry is coated and dried according to a preset second coating surface density, and the positive electrode slurry after the coating and drying is roll-pressed according to a preset second compaction density; The positive electrode slurry after the rolling process is cut according to a preset second size to obtain at least two positive electrode test pole pieces.
3. The method according to claim 2, characterized in that The method of preparing a soft-pack battery cell according to the positive and negative test electrodes and a preset reference electrode comprises: Performing lithium plating treatment on a preset reference electrode according to preset lithium plating parameters; Based on the preset number of stacked layers, the number of negative electrode test sheets, the number of positive electrode test sheets, the preset number of reference electrodes after lithium plating, and the number of diaphragms are determined respectively, and according to the number of negative electrode test sheets, the number of positive electrode test sheets, the preset number of reference electrodes after lithium plating, and the number of diaphragms, a soft-pack battery cell is prepared.
4. The method according to claim 1, characterized in that: The two sets of preset charge and discharge parameters include a discharge parameter consisting of a charge and discharge ratio and a discharge cut-off voltage, and a charge parameter consisting of the charge and discharge ratio and the charge cut-off voltage, wherein the discharge cut-off voltage is less than the charge cut-off voltage; The method of determining the nominal capacity based on the soft-pack battery cell and two sets of preset charge and discharge parameters includes: The soft-pack battery cell is subjected to a static treatment according to a preset static time, and the soft-pack battery cell is discharged according to the discharge parameters after the static treatment; Performing a shelf treatment on the soft-pack battery cell after the discharge treatment according to a preset shelf time, and performing a charging treatment on the soft-pack battery cell after the shelf treatment according to the charging parameters; The soft-packed battery cell after the charging process is placed on hold according to the preset placement time, and the soft-packed battery cell after the placement process is discharged according to the discharge parameter, so as to use the corresponding discharge capacity as the nominal capacity.
5. The method according to claim 1, characterized in that The generating at least two groups of test capacity parameters according to the nominal capacity comprises: Based on the nominal capacity, a preset first charging ratio parameter, and a preset relaxation time, a first set of test capacity parameters is obtained; Based on the nominal capacity, the preset second charging ratio parameter and the preset relaxation time, obtaining a second set of test capacity parameters; Based on the nominal capacity, the preset third charging ratio parameter and the preset relaxation time, a third set of test capacity parameters is obtained; wherein the difference between the preset second charging ratio parameter and the preset first charging ratio parameter is consistent with the difference between the preset third charging ratio parameter and the preset second charging ratio parameter.
6. The method according to claim 1, characterized in that The step of determining the lithium deposition starting potential of the soft-pack battery cell according to all the voltage-time curves, all the differential voltage-time curves and the negative electrode to lithium potential curve comprises: When an abnormal slope change is detected in the voltage-time curve corresponding to the nth group of test capacity parameters, it is determined whether there is a characteristic peak in the corresponding differential voltage-time curve; wherein n is a positive integer greater than 1; When the characteristic peak is detected in the differential voltage-time curve, the lithium precipitation starting potential of the soft-pack battery cell is determined according to the voltage-time curve corresponding to the test capacity parameters of the n-1th group, the differential voltage-time curve and the negative electrode to lithium potential curve.
7. The method according to claim 6, characterized in that The step of determining the lithium deposition starting potential of the soft-pack battery cell according to the voltage-time curve, the differential voltage-time curve, and the negative electrode to lithium potential curve corresponding to the test capacity parameter of the n-1th group includes: When no abnormal slope change is detected in the voltage-time curve corresponding to the test capacity parameter of the n-1th group, determining whether there is a characteristic peak in the corresponding differential voltage-time curve; When the absence of the characteristic peak is detected in the differential voltage-time curve, a first potential corresponding to the nth group of test capacity parameters and a second potential corresponding to the n-1th group of test capacity parameters are respectively determined in the negative electrode to lithium potential curve; The lithium deposition starting point potential of the soft-pack battery cell is determined according to the potential interval formed by the first potential and the second potential.
8. A device for detecting the starting potential of lithium deposition of a soft-pack battery cell, characterized in that: include: A cell preparation module, used to prepare samples according to at least two electrode materials to obtain positive and negative electrode test electrodes, and to prepare soft-pack cells according to the positive and negative electrode test electrodes and preset reference electrodes; A capacity determination module, used to determine the nominal capacity based on the soft-pack battery cell and two sets of preset charge and discharge parameters; A data generation module, used to generate at least two groups of test capacity parameters according to the nominal capacity, and test the soft-pack battery cells in turn according to each group of test capacity parameters to obtain corresponding voltage-time curves and negative electrode to lithium potential curves; The result determination module is used to perform differentiation processing on each of the voltage-time curves to obtain a corresponding differential voltage-time curve, and determine the lithium precipitation starting potential of the soft-pack battery cell based on all the voltage-time curves, all the differential voltage-time curves and the negative electrode to lithium potential curve.
9. A device for detecting the starting potential of lithium deposition of a soft-pack battery cell, characterized in that: including a processor and a memory; The processor is connected to the memory; The memory is used to store executable program code; The processor runs a program corresponding to the executable program code by reading the executable program code stored in the memory, so as to execute the steps of the method according to any one of claims 1 to 7.
10. A computer-readable storage medium having a computer program stored thereon, characterized in that: The computer-readable storage medium stores instructions, and when the instructions are executed on a computer or a processor, the computer or the processor executes the steps of the method according to any one of claims 1 to 7.
Citation Information
Patent Citations
Preparation method of three-electrode battery and lithium precipitation test method of three-electrode battery
CN114497693A
Method and device for determining lithium precipitation potential of lithium ion battery and electronic equipment
CN116008827A
Three-electrode-based lithium ion battery lithium precipitation critical point test method and application method
CN117347891A
Method and device for testing lithium precipitation window of negative electrode material button half cell
CN118169589A
Cited By
Battery standing tool
CN119108656A
Lithium ion battery lithium precipitation repair method and device, electronic equipment and storage medium
CN119481362A