Display module, manufacturing method thereof and electronic equipment
By performing simultaneous photolithography processing on the first inorganic layer and the first substrate in the frame area of the display module, and introducing the second inorganic layer and organic layer, the problem of difficulty in realizing narrow frame requirements in traditional designs is solved, and the frame area is realized The stability and precise control avoid dark spots and shadow effects.
Patent Information
- Application Number
- CN202410741126.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-07
- Publication Date
- 2024-10-15
AI Technical Summary
The traditional compression design distance solution cannot meet the market demand for narrow frames, resulting in black spots or black lines that may appear in the bending area, and the shadow effect of the packaging layer and the accuracy of the incoming materials limit the frame design.
By performing synchronous photolithography on the first inorganic layer and the first substrate in the frame area of the display module to make the side walls on the same plane, and introducing the second inorganic layer and the organic layer into the packaging layer, photolithography is performed simultaneously Processed to control boundaries and ensure consistent shrinkage during heating.
It avoids the generation of black spots or black lines in the bending area, and eliminates the shadow effect of the packaging layer in traditional display modules and the problem of incoming material accuracy, achieving more precise control over the frame design and achieving a narrow frame.
Smart Images

Figure CN118785784A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of display technology, and in particular to a display module, a manufacturing method thereof, and an electronic device. Background Art
[0002] As the market demand for narrow bezels of electronic products increases, the new technical requirements for narrow bezels of mobile phones are also increasing. However, the traditional solution of compressing the design distance can no longer meet the market demand for narrow bezels. Summary of the invention
[0003] Based on this, it is necessary to provide a display module and a manufacturing method thereof and an electronic device to solve the problem of how to achieve a narrow frame.
[0004] A display module comprises a display panel, an encapsulation layer arranged on one side of the display panel, and a touch layer located on a side of the encapsulation layer away from the display panel; wherein:
[0005] The display panel includes a display area and a frame area, the display area includes a bending area, and the frame area is located on one side of the bending area;
[0006] The encapsulation layer comprises a first inorganic layer, and the orthographic projection of the first inorganic layer on the display panel covers at least a portion of the frame area;
[0007] The touch layer comprises a first substrate and a first touch electrode layer which are sequentially stacked in a direction away from the encapsulation layer, and the orthographic projection of the first substrate on the display panel covers at least a portion of the frame area;
[0008] The first substrate located in the border area covers the first inorganic layer, and the sidewall surfaces of the first inorganic layer and the first substrate located in the border area are on the same plane.
[0009] The display module using the technical solution of the present invention can ensure that the first inorganic layer located in the border area and the first substrate have the same shrinkage amount during the heating process of the display module, since the first inorganic layer located in the border area is on the same plane as the side wall surface of the first substrate, thereby avoiding the generation of black spots or black lines in the bending area. In addition, the boundary between the first inorganic layer of the encapsulation layer and the first substrate of the touch layer can be synchronously and accurately controlled, which can remove the shadow effect of the first inorganic layer in the traditional display module and the limitations of the material accuracy problem on the border design, thereby achieving a narrow border.
[0010] In a feasible implementation, the touch layer further includes a second substrate and a second touch electrode layer sequentially stacked on one side of the first touch electrode layer in a direction away from the encapsulation layer, the orthographic projection of the second substrate on the display panel covers at least a portion of the frame area, and the second substrate located in the frame area covers the first substrate, wherein the sidewall surfaces of the first inorganic layer, the first substrate, and the second substrate located in the frame area are on the same plane;
[0011] Preferably, the first inorganic layer, the first substrate and the second substrate are made of the same material.
[0012] In a feasible implementation, the encapsulation layer further includes a second inorganic layer and an organic layer located between the first inorganic layer and the second inorganic layer; the orthographic projection of the second inorganic layer on the display panel covers at least a portion of the frame area;
[0013] Preferably, the second inorganic layer is located on a side of the organic layer facing the display panel; preferably, the first inorganic layer located in the frame area covers the second inorganic layer, and the sidewall surfaces of the second inorganic layer and the first inorganic layer located in the frame area are on the same plane;
[0014] Preferably, the second inorganic layer and the first inorganic layer are made of the same material.
[0015] In a feasible implementation, the thickness of the first inorganic layer is 0.4 μm to 1 μm; the thickness of the first substrate is 0.2 μm to 0.5 μm.
[0016] In a feasible implementation, the first inorganic layer and the first substrate are an integrated structure;
[0017] Preferably, the total thickness of the first inorganic layer and the first substrate is 0.4 μm to 1.5 μm.
[0018] In a feasible implementation, the first inorganic layer and the first substrate are made of the same material;
[0019] Preferably, the material of the first inorganic layer and the first substrate is at least one of silicon nitride and silicon oxide.
[0020] A method for manufacturing a display module comprises the following steps:
[0021] A display panel is provided, wherein the display panel comprises a display area and a frame area, wherein the display area comprises a bending area, and the frame area is located on one side of the bending area;
[0022] A first inorganic layer of an encapsulation layer and a first substrate of a touch layer are formed on the display panel, wherein the orthographic projections of the first inorganic layer and the first substrate on the display panel both cover at least a portion of the frame area, and the first substrate located in the frame area covers the first inorganic layer;
[0023] forming a first touch electrode layer on the first substrate; and
[0024] The first substrate and the first inorganic layer located in the border area are simultaneously subjected to photolithography processing, so that the sidewall surfaces of the first substrate and the first inorganic layer located in the border area are on the same plane.
[0025] In the method for manufacturing a display module using the technical solution of the present invention, since the first substrate and the first inorganic layer are simultaneously photolithographically processed in the border area of the display module, the side wall surfaces of the first substrate and the first inorganic layer located in the border area are on the same plane; therefore, during the heating process of the display module, the shrinkage amounts of the first inorganic layer and the first substrate located in the border area can be ensured to be consistent, thereby avoiding the generation of black spots or black lines in the bending area; in addition, the boundary between the first inorganic layer of the encapsulation layer and the first substrate of the touch layer can be synchronously and accurately controlled, eliminating the restrictions on the border design caused by the shadow effect of the first inorganic layer and the problem of incoming material accuracy, thereby achieving a narrow border.
[0026] In a feasible implementation, the step of forming a first inorganic layer of an encapsulation layer and a first substrate of a touch layer on the display panel includes:
[0027] Firstly, a first inorganic layer of an encapsulation layer is formed on the display panel, and then a first substrate of a touch layer is formed on the first inorganic layer; or
[0028] The first inorganic layer and the first substrate are simultaneously formed on the display panel by using a CVD process, and the first inorganic layer and the first substrate are an integrated structure.
[0029] In a feasible implementation, before forming the first inorganic layer of the encapsulation layer, the following steps are also included:
[0030] forming a second inorganic layer of an encapsulation layer on the display panel; and
[0031] forming an organic layer on a side of the second inorganic layer away from the display panel;
[0032] Preferably, the step of performing photolithography processing includes: performing photolithography processing on the second inorganic layer, the first inorganic layer and the first substrate located in the frame area simultaneously, so that the sidewall surfaces of the second inorganic layer, the first inorganic layer and the first substrate located in the frame area are on the same plane; preferably, before performing photolithography processing, the following steps are also included: forming a second substrate on a side of the first touch electrode layer away from the first substrate;
[0033] Preferably, the method further comprises the following steps: forming a second touch electrode layer on a side of the second substrate away from the first touch electrode layer;
[0034] Preferably, the step of performing photolithography processing includes: simultaneously performing photolithography processing on the second substrate, the first substrate, the first inorganic layer and the second inorganic layer located in the border area, so that the side wall surfaces of the second substrate, the first substrate, the first inorganic layer and the second inorganic layer are all on the same plane.
[0035] An electronic device comprises the display module in any one of the above embodiments.
[0036] In an electronic device using the technical solution of the present invention, since the side wall surfaces of the first inorganic layer and the first substrate are on the same plane, the boundary between the first inorganic layer of the encapsulation layer and the first substrate of the touch layer can be synchronously and precisely controlled, so that during the heating process of the display module, the shrinkage of the first inorganic layer and the first substrate in the border area can be ensured to be consistent, thereby effectively avoiding the generation of black spots or black lines in the bending area; in addition, the restrictions on the border design caused by the shadow effect of the first inorganic layer and the material accuracy problem in the traditional display module can be removed, thereby achieving a narrow border. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] Figure 1 is a schematic diagram of a display module according to a first embodiment of the present invention;
[0038] Figure 2 is a schematic diagram of a display module according to a second embodiment of the present invention;
[0039] Figure 3 is a schematic diagram of a display module according to a third embodiment of the present invention;
[0040] Figure 4 is a schematic diagram of a display module according to a fourth embodiment of the present invention;
[0041] Figure 5 is a flow chart of a method for manufacturing a display module according to an embodiment of the present invention;
[0042] Figure 6 is a schematic diagram of a display panel during the manufacturing process of a display module according to a first embodiment of the present invention;
[0043] Figure 7 It is a schematic diagram of a display module after forming a first touch electrode layer in the manufacturing process of the first embodiment of the present invention;
[0044] Figure 8 It is a schematic diagram of the display module after photolithography processing in the manufacturing process of the first embodiment of the present invention;
[0045] Fig. 9 is a schematic diagram of a display panel during the manufacturing process of a display module according to a second embodiment of the present invention;
[0046] Fig.10 It is a schematic diagram of a display module after forming a first touch electrode layer in the manufacturing process of the second embodiment of the present invention;
[0047] Fig.11 It is a schematic diagram of a display module after photolithography processing in the manufacturing process of the second embodiment of the present invention;
[0048] Fig.12 is a schematic diagram of a display panel during the manufacturing process of a display module according to a third embodiment of the present invention;
[0049] Fig.13 It is a schematic diagram of a display module after forming a second touch electrode layer in the manufacturing process of the third embodiment of the present invention;
[0050] Fig.14 It is a schematic diagram of a display module after photolithography processing in the manufacturing process of the third embodiment of the present invention;
[0051] Fig.15 is a schematic diagram of a display panel during the manufacturing process of a display module according to a fourth embodiment of the present invention;
[0052] Fig.16 It is a schematic diagram of a display module after forming a second touch electrode layer in the manufacturing process of the fourth embodiment of the present invention;
[0053] Fig.17 FIG. 4 is a schematic diagram of a display module after photolithography processing is performed during the manufacturing process of the display module according to the fourth embodiment of the present invention. DETAILED DESCRIPTION
[0054] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the specific embodiments of the present invention are described in detail below in conjunction with the accompanying drawings. In the following description, many specific details are set forth to facilitate a full understanding of the present invention. However, the present invention can be implemented in many other ways different from those described herein, and those skilled in the art can make similar improvements without violating the connotation of the present invention, so the present invention is not limited by the specific embodiments disclosed below.
[0055] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art of the present invention. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more related listed items.
[0056] See also Figure 1 The display module 100 of the first embodiment of the present invention includes a display panel 110 , an encapsulation layer 120 disposed on one side of the display panel 110 , and a touch layer 130 located on a side of the encapsulation layer 120 away from the display panel 110 .
[0057] The display panel 110 includes a display area 111 and a frame area 112. The display area 111 includes a bending area 113. The frame area 112 is located on one side of the bending area 113. It is worth noting that during the display process of the display panel 110, the bending area 113 also displays, such as a curved screen or a four-curved screen in the related art.
[0058] Among them, the encapsulation layer 120 includes a first inorganic layer 121, and the orthographic projection of the first inorganic layer 121 on the display panel 110 covers at least part of the frame area 112. The present invention does not limit the number of inorganic layers in the encapsulation layer 120, wherein the first inorganic layer 121 is an inorganic layer in the encapsulation layer 120 that is closest to the touch layer 130. The encapsulation layer 120 is used to encapsulate the display panel 110, and plays a role in blocking external factors such as water vapor and protecting the internal functional layers. Of course, in other embodiments, there are other film layers between the first inorganic layer 121 and the touch layer 130, which are not specifically limited in this application.
[0059] The touch layer 130 includes a first substrate 131 and a first touch electrode layer 132 which are sequentially stacked in a direction away from the encapsulation layer 120 , and the orthographic projection of the first substrate 131 on the display panel 110 covers at least a portion of the frame area 112 .
[0060] Among them, the first substrate 131 located in the border area 112 covers the first inorganic layer 121, and the side wall surfaces of the first inorganic layer 121 and the first substrate 131 located in the border area 112 are on the same plane, and the range covered by the two in the border area 112 tends to be consistent, so that during the heating process of the display panel 110, the shrinkage of the first inorganic layer 121 and the first substrate 131 located in the border area 112 can be guaranteed to be consistent, thereby avoiding the generation of black spots or black lines in the bending area 113; at the same time, the boundary between the first inorganic layer 121 of the encapsulation layer 120 and the first substrate 131 of the touch layer 130 can be synchronously and accurately controlled, which can remove the restrictions on the border design caused by the shadow effect of the first inorganic layer in the traditional display module and the problem of incoming material accuracy, thereby achieving a narrow border. It is worth noting that, since the display panel 110 has a bent display area, the stress of the relevant film layer of the display module 100 is the greatest in the bent area 113. If there is a large difference in the coverage of the first inorganic layer 121 and the first substrate 131 in the frame area 112, the shrinkage amount of the film layer is inconsistent when heated, resulting in a difference in the stress on the display panel 110, which easily causes black spots or black lines in the bent area 113. The shadow effect refers to the problem of uneven thickness of the film layer formed in the edge area corresponding to the mask opening when the film layer is prepared, which is affected by the mask opening.
[0061] On the basis of the above-mentioned embodiment, the encapsulation layer 120 further includes a second inorganic layer 122 and an organic layer 123 located between the first inorganic layer 121 and the second inorganic layer 122, and the second inorganic layer 122 is disposed close to the display panel 110. Similarly, the present invention does not limit the number of layers of the organic layer 123, and an organic layer is located between two adjacent inorganic layers.
[0062] Preferably, the sidewall surfaces of the second inorganic layer 122 and the first inorganic layer 121 located in the border area 112 are on the same plane. At this time, the boundary between the second inorganic layer 122 and the first inorganic layer 121 can be etched using the same photolithography process. In this embodiment, the sidewall surfaces of the second inorganic layer 122, the first inorganic layer 121 and the first substrate 131 are on the same plane, so that the display module 100 can ensure that the second inorganic layer 122, the first inorganic layer 121 and the first substrate 131 located in the border area 112 shrink in the same amount during the heating process, thereby avoiding the generation of black spots or black lines in the bending area 113; in addition, in the display module 100 of this embodiment, the boundary between the first inorganic layer 121 and the second inorganic layer 122 of the encapsulation layer 120 can be synchronously and accurately controlled, removing the shadow effect of the first inorganic layer 121 and the second inorganic layer 122 and the limitation of the frame design caused by the material precision problem, thereby realizing a narrow frame.
[0063] On the basis of the above-mentioned embodiment, the thickness of the first inorganic layer 121 is 0.4 μm to 1 μm; the thickness of the first substrate 131 is 0.2 μm to 0.5 μm. The thickness of the first inorganic layer 121 may be, but not limited to, 0.4 μm, 0.5 μm, 0.6 μm, 0.7 μm, 0.8 μm, 0.9 μm or 1 μm, etc.; the thickness of the first substrate 131 may be, but not limited to, 0.2 μm, 0.3 μm, 0.4 μm or 0.5 μm, etc.
[0064] On the basis of the foregoing embodiment, the display panel 110 includes an array substrate 114 and a display unit 115, and the display unit 115 is located between the array substrate 114 and the encapsulation layer 120. In a feasible implementation, the array substrate 114 includes a substrate, a buffer layer, a gate insulating layer, an interlayer dielectric layer, a flat layer and a pixel definition layer stacked in sequence. In a feasible implementation, the display unit 115 includes a first electrode layer, a first functional layer, a light-emitting layer, a second functional layer and a second electrode layer stacked in sequence. In a feasible implementation, the first electrode layer is a cathode, the second electrode layer is an anode, the first functional layer is selected from at least one of an electron transport layer and an electron injection layer, and the second functional layer is selected from at least one of a hole transport layer and a hole injection layer. In another feasible implementation, the first electrode layer is an anode, the second electrode layer is a cathode, the first functional layer is selected from at least one of a hole transport layer and a hole injection layer, and the second functional layer is selected from at least one of an electron transport layer and an electron injection layer. Furthermore, the present invention does not limit the materials and thicknesses of the functional layers of the array substrate 114 and the display unit 115 , and the materials and thicknesses may be commonly used in the art.
[0065] In the display module 100 of the above embodiment, there is a clear interface between the first inorganic layer 121 and the first substrate 131, and the first inorganic layer 121 and the first substrate 131 are manufactured in two steps. However, the display module of the present invention is not limited thereto, and the first inorganic layer and the first substrate may also be an integrated structure.
[0066] See also Figure 2 The display module 200 of the second embodiment of the present invention includes a display panel 210 , an encapsulation layer 220 disposed on one side of the display panel 210 , and a touch layer 230 located on a side of the encapsulation layer 220 away from the display panel 210 .
[0067] The display panel 210 includes a display area 211 and a frame area 212 . The display area 211 includes a bending area 213 . The frame area 212 is located at one side of the bending area 213 .
[0068] The encapsulation layer 220 includes a first inorganic layer 221 , and the orthographic projection of the first inorganic layer 221 on the display panel 210 covers at least a portion of the frame area 212 . Specifically, the first inorganic layer 221 is disposed close to the touch layer 230 .
[0069] The touch layer 230 includes a first substrate 231 and a first touch electrode layer 232 which are sequentially stacked in a direction away from the encapsulation layer 220 , and the orthographic projection of the first substrate 231 on the display panel 210 covers at least a portion of the frame area 212 .
[0070] In the display module 200 of this embodiment, the first inorganic layer 221 and the first substrate 231 are an integrated structure. When manufacturing the display module 200 of this embodiment, a CVD (Chemical Vapor Deposition) process is used to simultaneously form the first inorganic layer 221 and the first substrate 231, that is, the two are one film layer, without physical boundaries, and can reduce processes and reduce production costs.
[0071] Among them, the side wall surfaces of the first inorganic layer 221 and the first substrate 231 located in the border area 212 are on the same plane, and the range covered by the two in the border area 212 tends to be consistent, so that during the heating process of the display panel 210, the shrinkage of the first inorganic layer 221 and the first substrate 231 located in the border area 212 can be guaranteed to be consistent, thereby avoiding the generation of black spots or black lines in the bending area 213; in addition, the boundary between the first inorganic layer 221 of the encapsulation layer 220 and the first substrate 231 of the touch layer 230 can be synchronously and accurately controlled, which can remove the shadow effect of the first inorganic layer in the traditional display module and the limitations of the material accuracy problem on the border design, thereby achieving a narrow border.
[0072] On the basis of the above-mentioned embodiment, the encapsulation layer 220 further includes a second inorganic layer 222 and an organic layer 223 located between the first inorganic layer 221 and the second inorganic layer 222, and the second inorganic layer 222 is disposed close to the display panel 210. Similarly, the present invention does not limit the number of layers of the organic layer 223, and an organic layer is provided between two adjacent inorganic layers.
[0073] Preferably, the first inorganic layer 221 located in the border area 212 covers the second inorganic layer 222, and the sidewalls of the second inorganic layer 222 and the first inorganic layer 221 located in the border area 212 are on the same plane. At this time, the boundary between the second inorganic layer 222 and the first inorganic layer 221 can be etched using the same photolithography process. In this embodiment, the sidewalls of the second inorganic layer 222 and the first inorganic layer 221 (first substrate 231) are on the same plane, which can ensure that the second inorganic layer 222 located in the border area 212 and the first inorganic layer 221 (first substrate 231) have the same shrinkage amount, thereby avoiding the generation of black spots or black lines in the bending area 213; in addition, in the display module 200 of this embodiment, the boundary between the first inorganic layer 221 and the second inorganic layer 222 of the encapsulation layer 220 can be synchronously and accurately controlled, removing the shadow effect of the first inorganic layer 221 and the second inorganic layer 222 and the limitation of the frame design caused by the material precision problem, thereby realizing a narrow frame.
[0074] Based on the above embodiment, the total thickness of the first inorganic layer 221 and the first substrate 231 is 0.4 μm to 1.5 μm. Further, the total thickness of the first inorganic layer 221 and the first substrate 231 can be, but is not limited to, 0.4 μm, 0.5 μm, 0.6 μm, 0.7 μm, 0.8 μm, 0.9 μm, 1 μm, 1.1 μm, 1.2 μm, 1.3 μm, 1.4 μm or 1.5 μm.
[0075] On the basis of the above-mentioned embodiments, the display panel 210 includes an array substrate 214 and a display unit 215 . The display unit 215 is located between the array substrate 214 and the encapsulation layer 220 .
[0076] In addition, the display module of the present invention is not limited to the above-mentioned embodiment, and the touch layer may further include a second substrate and a second touch electrode layer.
[0077] See also Figure 3 The display module 300 of the third embodiment of the present invention includes a display panel 310 , an encapsulation layer 320 disposed on one side of the display panel 310 , and a touch layer 330 located on a side of the encapsulation layer 320 away from the display panel 310 .
[0078] The display panel 310 includes a display area 311 and a frame area 312 . The display area 311 includes a bending area 313 . The frame area 312 is located at one side of the bending area 313 .
[0079] The encapsulation layer 320 includes a first inorganic layer 321 , and the orthographic projection of the first inorganic layer 321 on the display panel 310 covers at least a portion of the frame area 312 . Specifically, the first inorganic layer 321 is disposed close to the touch layer 330 .
[0080] The touch layer 330 includes a first substrate 331, a first touch electrode layer 332, a second substrate 333, and a second touch electrode layer 334 which are sequentially stacked in a direction away from the encapsulation layer 320. The orthographic projections of the first substrate 331 and the second substrate 333 on the display panel 310 both cover at least a portion of the frame area 312, and the second substrate 333 located in the frame area 312 covers the first substrate 331. The first touch electrode layer 332 is a sensing electrode layer, and the second touch electrode layer 334 is a driving electrode layer.
[0081] Among them, the side walls of the first inorganic layer 321, the first substrate 331 and the second substrate 333 located in the border area 312 are on the same plane, and the range covered by the three in the border area 312 tends to be consistent, so that during the heating process of the display panel 310, the shrinkage of the first inorganic layer 321, the first substrate 331 and the second substrate 333 located in the border area 312 can be guaranteed to be consistent, thereby avoiding the generation of black spots or black lines in the bending area 313; in addition, the boundaries of the first inorganic layer 321 of the encapsulation layer 320 and the first substrate 331 and the second substrate 333 of the touch layer 330 can be synchronously and accurately controlled, which can remove the restrictions on the border design caused by the shadow effect of the first inorganic layer in the traditional display module and the problem of incoming material accuracy, thereby achieving a narrow border.
[0082] On the basis of the above-mentioned embodiment, the encapsulation layer 320 further includes a second inorganic layer 322 and an organic layer 323 located between the first inorganic layer 321 and the second inorganic layer 322 , and the second inorganic layer 322 is disposed close to the display panel 310 .
[0083] Preferably, the first inorganic layer 321 located in the border area 312 covers the second inorganic layer 322, and the sidewall surfaces of the second inorganic layer 322 and the first inorganic layer 321 located in the border area 312 are on the same plane. At this time, the boundary between the second inorganic layer 322 and the first inorganic layer 321 can be etched using the same photolithography process. In this embodiment, the sidewall surfaces of the second inorganic layer 322, the first inorganic layer 321, the first substrate 331 and the second substrate 333 in the border area 312 are on the same plane, so that the range covered by the four in the border area 312 tends to be consistent, so that the display panel 310 can ensure that the second inorganic layer 322, the first inorganic layer 321, the first substrate 331 and the second substrate 333 in the border area 312 shrink in the same amount during the heating process, thereby avoiding the generation of black spots or black lines in the bending area 313. In addition, in the display module 300 of this embodiment, the boundary between the first inorganic layer 321 and the second inorganic layer 322 of the encapsulation layer 320 can be synchronously and precisely controlled, removing the restrictions on the frame design caused by the shadow effect of the first inorganic layer 321 and the second inorganic layer 322 and the problem of incoming material accuracy, thereby achieving a narrow frame.
[0084] On the basis of the above-mentioned embodiments, the display panel 310 includes an array substrate 314 and a display unit 315 . The display unit 315 is located between the array substrate 314 and the encapsulation layer 320 .
[0085] See also Figure 4 The display module 400 of the fourth embodiment of the present invention includes a display panel 410 , an encapsulation layer 420 disposed on one side of the display panel 410 , and a touch layer 430 located on a side of the encapsulation layer 420 away from the display panel 410 .
[0086] The display panel 410 includes a display area 411 and a frame area 412 . The display area 411 includes a bending area 413 . The frame area 412 is located at one side of the bending area 413 .
[0087] The encapsulation layer 420 includes a first inorganic layer 421 , and the orthographic projection of the first inorganic layer 421 on the display panel 410 covers at least a portion of the frame area 412 . Specifically, the first inorganic layer 421 is disposed close to the touch layer 430 .
[0088] The touch layer 430 includes a first substrate 431, a first touch electrode layer 432, a second substrate 433, and a second touch electrode layer 434 which are sequentially stacked in a direction away from the encapsulation layer 420. The orthographic projections of the first substrate 431 and the second substrate 433 on the display panel 410 both cover at least a portion of the frame area 412, and the second substrate 433 located in the frame area 412 covers the first substrate 431. The first touch electrode layer 432 is a sensing electrode layer, and the second touch electrode layer 434 is a driving electrode layer.
[0089] In the display module 400 of this embodiment, the first inorganic layer 421 and the first substrate 431 are an integrated structure. When manufacturing the display module 400 of this embodiment, a CVD (Chemical Vapor Deposition) process is used to simultaneously form the first inorganic layer 421 (first substrate 431).
[0090] Among them, the side walls of the first inorganic layer 421 (first substrate 431) and the second substrate 433 located in the border area 412 are on the same plane, so that the range covered by the two in the border area 412 tends to be consistent, so that during the heating process of the display panel 410, the shrinkage of the first inorganic layer 421 (first substrate 431) and the second substrate 433 located in the border area 412 can be ensured to be consistent, thereby avoiding the generation of black spots or black lines in the bending area 413; in addition, in this way, the boundaries of the first inorganic layer 421 (first substrate 431) and the second substrate 433 of the encapsulation layer 420 can be synchronously and accurately controlled, which can remove the restrictions on the border design caused by the shadow effect of the first inorganic layer in the traditional display module and the problem of incoming material accuracy, thereby achieving a narrow border.
[0091] Based on the above-mentioned embodiment, the encapsulation layer 420 also includes a second inorganic layer 422 and an organic layer 423 located between the first inorganic layer 421 and the second inorganic layer 422. The second inorganic layer 422 is arranged close to the display panel 410, and the orthographic projection of the second inorganic layer 422 on the display panel 410 covers at least part of the border area 412. The first inorganic layer 421 located in the border area 412 covers the second inorganic layer 422.
[0092] Preferably, the sidewall surfaces of the second inorganic layer 422 and the first inorganic layer 421 in the border area 412 are on the same plane. At this time, the boundary between the second inorganic layer 422 and the first inorganic layer 421 can be etched using the same photolithography process. In this embodiment, the sidewall surfaces of the second inorganic layer 422, the first inorganic layer 421 (the first substrate 431) and the second substrate 433 in the border area 412 are on the same plane, so that the range covered by the three in the border area 412 tends to be consistent, so that the display panel 410 can ensure that the second inorganic layer 422, the first inorganic layer 421 (the first substrate 431) and the second substrate 433 in the border area 412 shrink in the same amount during the heating process, thereby avoiding the generation of black spots or black lines in the bending area 413. In the display module 400 of this embodiment, the boundaries between the first inorganic layer 421 and the second inorganic layer 422 of the encapsulation layer 420 can be synchronously and precisely controlled, removing the restrictions on the frame design caused by the shadow effect of the first inorganic layer 421 and the second inorganic layer 422 and the material precision problem, thereby achieving a narrow frame.
[0093] On the basis of the above-mentioned embodiments, the display panel 410 includes an array substrate 414 and a display unit 415 . The display unit 415 is located between the array substrate 414 and the encapsulation layer 420 .
[0094] In the display module using the technical solution of the present invention, since the side wall surface of the first inorganic layer and the first substrate are on the same plane, the boundary between the first inorganic layer of the encapsulation layer and the first substrate of the touch layer can be synchronously and accurately controlled, eliminating the restrictions on the frame design caused by the shadow effect of the first inorganic layer and the material accuracy problem, thereby achieving a narrow frame.
[0095] It is worth noting that the materials of the first substrate, the second substrate, the first inorganic layer, and the second inorganic layer in the above embodiments are the same, and can be at least one of silicon nitride or silicon oxide, for example, all are silicon nitride.
[0096] See also Figure 5 A method for manufacturing a display module according to an embodiment of the present invention comprises the following steps:
[0097] S10. Provide a display panel, wherein the display panel includes a display area and a frame area. The display area includes a bending area, and the frame area is located on one side of the bending area.
[0098] The display panel includes an array substrate and a display unit, and the display unit is located between the array substrate and the packaging layer.
[0099] S20, forming a first inorganic layer of the encapsulation layer and a first substrate of the touch layer on the display panel, wherein the orthographic projections of the first inorganic layer and the first substrate on the display panel both cover at least a portion of the frame area, and the first substrate located in the frame area covers the first inorganic layer.
[0100] In step S20, the step of forming a first inorganic layer of an encapsulation layer and a first substrate of a touch layer on the display panel includes:
[0101] Firstly, a first inorganic layer of an encapsulation layer is formed on the display panel, and then a first substrate of a touch layer is formed on the first inorganic layer; or
[0102] A first inorganic layer and a first substrate are formed on the display panel simultaneously by using a CVD process, and the first inorganic layer and the first substrate are an integrated structure.
[0103] Among them, the operation of synchronously forming the first inorganic layer and the first substrate by using a CVD (Chemical Vapor Deposition) process can reduce one CVD (Chemical Vapor Deposition) process and improve production efficiency.
[0104] In a feasible implementation, before forming the first inorganic layer of the encapsulation layer, the following steps are also included:
[0105] forming a second inorganic layer of an encapsulation layer on the display panel; and
[0106] An organic layer is formed on a side of the second inorganic layer away from the display panel.
[0107] The second inorganic layer and the organic layer may be formed by conventional means in the art.
[0108] In a feasible implementation, the step of performing photolithography processing includes: simultaneously performing photolithography processing on the second inorganic layer, the first inorganic layer and the first substrate located in the border area, so that the side wall surfaces of the second inorganic layer, the first inorganic layer and the first substrate located in the border area are on the same plane.
[0109] S30, forming a first touch electrode layer on the first substrate.
[0110] The first touch electrode layer may be a sensing electrode layer. The first touch electrode layer may be formed on the first substrate by conventional means in the art, for example, first forming a film by PVD (Physical Vapor Deposition) and then etching to obtain a patterned first touch electrode layer.
[0111] S40, performing photolithography processing on the first substrate and the first inorganic layer located in the frame area simultaneously, so that the sidewall surfaces of the first substrate and the first inorganic layer located in the frame area are on the same plane.
[0112] The photolithography process in step S40 is preferably a yellow light process, which includes the steps of coating, soft baking, exposure, development and hard baking.
[0113] In step S40, since the first substrate and the first inorganic layer are simultaneously photolithographically processed at the border of the display module, the first inorganic layer located in the border area and the side wall surface of the first substrate are on the same plane. During the heating process of the display module, the shrinkage amount of the first inorganic layer and the first substrate in the border area can be ensured to be consistent, thereby avoiding the generation of black spots or black lines in the bending area. In addition, the boundary of the first inorganic layer of the encapsulation layer can be synchronously and accurately controlled to remove the restrictions on the border design caused by the shadow effect of the first inorganic layer and the accuracy of the incoming materials, thereby achieving a narrow border.
[0114] In a feasible implementation, before the photolithography process is performed, the following step is also included: forming a second substrate on the first touch electrode layer and the first substrate. Preferably, the following step is also included: forming a second touch electrode layer on the second substrate. The second touch electrode layer may be a drive electrode layer. The second touch electrode layer may be formed on the second substrate by conventional means in the art, for example, first forming a film by PVD (Physical Vapor Deposition), and then etching to obtain a patterned second touch electrode layer.
[0115] In a feasible implementation, the step of performing photolithography processing includes: simultaneously performing photolithography processing on the second substrate, the first substrate, the first inorganic layer and the second inorganic layer located in the border area, so that the side wall surfaces of the second substrate, the first substrate, the first inorganic layer and the second inorganic layer are all on the same plane.
[0116] The manufacturing method of the display module of the present invention is described below in conjunction with specific embodiments.
[0117] See also Figure 1 , Figure 6 to Figure 8 The manufacturing method of the display module 100 of the first embodiment includes the following steps:
[0118] A display panel 110 is provided, the display panel 110 includes a display area 111 and a frame area 112, the display area 111 includes a bending area 113, and the frame area 112 is located on one side of the bending area 113; the display panel 110 includes an array substrate 114 and a display unit 115 which are stacked, such as Figure 6 As shown;
[0119] The second inorganic layer 122 of the encapsulation layer 120, the organic layer 123, the first inorganic layer 121 and the first substrate 131 of the touch layer 130 are sequentially formed on the display panel 110, and the orthographic projections of the second inorganic layer 122, the first inorganic layer 121 and the first substrate 131 on the display panel 110 all cover at least part of the frame area 112, and then the first touch electrode layer 132 is formed on the first substrate 131. Figure 7 As shown;
[0120] The first substrate 131, the first inorganic layer 121 and the second inorganic layer 122 located in the border area 112 are Figure 8 The position of the middle arrow is simultaneously subjected to photolithography processing, and the Figure 1 The display module 100 is shown.
[0121] See also Figure 2 , Figures 9 to 11 The manufacturing method of the display module 200 of the second embodiment includes the following steps:
[0122] A display panel 210 is provided, the display panel 210 includes a display area 211 and a frame area 212, the display area 211 includes a bending area 213, and the frame area 212 is located on one side of the bending area 213; the display panel 210 includes an array substrate 214 and a display unit 215 which are stacked, such as Fig. 9 As shown;
[0123] The second inorganic layer 222 and the organic layer 223 of the encapsulation layer 220 are sequentially formed on the display panel 210, and then the first inorganic layer 221 is synchronously formed by a CVD process. The first inorganic layer 221 is reused as the first substrate 231 of the touch layer 230, that is, the two are an integrated structure, wherein the orthographic projection of the first inorganic layer 221 (first substrate 231) on the display panel 210 covers at least part of the frame area 212, and then the first touch electrode layer 232 is formed on the first inorganic layer 221 (first substrate 231), as shown in FIG. Fig.10 As shown;
[0124] The first inorganic layer 221 (first substrate 231) and the second inorganic layer 222 located in the border area 212 are Fig.11 The position of the middle arrow is simultaneously subjected to photolithography processing, and the Figure 2 The display module 200 is shown.
[0125] In the manufacturing method of the display module 200 of the second embodiment, the first inorganic layer 221 and the first substrate 231 are formed simultaneously by using a CVD (Chemical Vapor Deposition) process, which can reduce one CVD (Chemical Vapor Deposition) process and improve production efficiency.
[0126] See also Figure 3 , Figure 12 to Figure 14 The manufacturing method of the display module 300 of the third embodiment includes the following steps:
[0127] A display panel 310 is provided, the display panel 310 includes a display area 311 and a frame area 312, the display area 311 includes a bending area 313, and the frame area 312 is located on one side of the bending area 313; the display panel 310 includes an array substrate 314 and a display unit 315 stacked, such as Fig.12 As shown;
[0128] The second inorganic layer 322 of the encapsulation layer 320, the organic layer 323, the first inorganic layer 321 and the first substrate 331 of the touch layer 330 are sequentially formed on the display panel 310, and then the first touch electrode layer 332 is formed on the first substrate 331, and then the second substrate 333 is formed on the first touch electrode layer 332, and then the second touch electrode layer 334 is formed on the second substrate 333. The orthographic projections of the first inorganic layer 321, the first substrate 331 and the second substrate 333 on the display panel 310 all cover at least part of the frame area 312, as shown in FIG. Fig.13 As shown;
[0129] The second substrate 333, the first substrate 331, the first inorganic layer 321 and the second inorganic layer 322 located in the frame area 312 are Fig.14 The position of the middle arrow is simultaneously subjected to photolithography processing, and the Figure 3 The display module 300 is shown.
[0130] See also Figure 4 , Figure 15 to Figure 17 The manufacturing method of the display module 400 of the fourth embodiment includes the following steps:
[0131] A display panel 410 is provided, the display panel 410 includes a display area 411 and a frame area 412, the display area 411 includes a bending area 413, and the frame area 412 is located on one side of the bending area 413; the display panel 410 includes an array substrate 414 and a display unit 415 stacked, such as Fig.15 As shown;
[0132] The second inorganic layer 422 and the organic layer 423 of the encapsulation layer 420 are sequentially formed on the display panel 410, and then the first inorganic layer 421 (reused as the first substrate 431 of the touch layer 430) is simultaneously formed by a CVD process, and then the first touch electrode layer 432 is formed on the first inorganic layer 421, and then the second substrate 433 is formed on the first touch electrode layer 432, and then the second touch electrode layer 434 is formed on the second substrate 433. The orthographic projections of the second inorganic layer 422, the first inorganic layer 421 (the first substrate 431) and the second substrate 433 on the display panel 410 all cover at least part of the frame area 412, as shown in FIG. Fig.16 As shown;
[0133] The second substrate 433, the first inorganic layer 421 (the first substrate 431) and the second inorganic layer 422 located in the frame area 412 are Fig.17 The position of the middle arrow is simultaneously subjected to photolithography processing, and the Figure 4 The display module 400 is shown.
[0134] In the manufacturing method of the display module 400 of the fourth embodiment, the first inorganic layer 421 and the first substrate 431 are formed simultaneously by using a CVD (Chemical Vapor Deposition) process, which can reduce one CVD (Chemical Vapor Deposition) process and improve production efficiency.
[0135] In the display module of this embodiment, the boundary between the first inorganic layer and the second inorganic layer of the encapsulation layer can be synchronously and precisely controlled, removing the restrictions on the frame design caused by the shadow effect of the first inorganic layer and the second inorganic layer and the problem of material precision, thereby achieving a narrow frame. In addition, it should be noted that in some cases, the boundary of the second inorganic layer itself is within the design boundary that requires photolithography processing, and there is no need to perform photolithography processing on the boundary of the second inorganic layer.
[0136] In the method for manufacturing a display module using the technical solution of the present invention, since the first substrate and the first inorganic layer are simultaneously photolithographically processed at the frame of the display module, the boundary between the first inorganic layer of the encapsulation layer and the first substrate of the touch layer can be synchronously and accurately controlled, which can remove the restrictions on the frame design caused by the shadow effect of the first inorganic layer and the material accuracy problem in the traditional display module, thereby achieving a narrow frame.
[0137] An electronic device according to one embodiment includes the display module according to any one of the above embodiments.
[0138] In an electronic device using the technical solution of the present invention, since the side wall surface of the first inorganic layer and the first substrate are on the same plane, the boundary between the first inorganic layer of the encapsulation layer and the first substrate of the touch layer can be synchronously and accurately controlled, which can remove the restrictions on the frame design caused by the shadow effect of the first inorganic layer and the material accuracy problem in the traditional display module, thereby achieving a narrow frame.
[0139] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0140] The above-mentioned embodiments only express several implementation methods of the present invention, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, and these all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.
Claims
1. A display module, characterized in that: It comprises a display panel, an encapsulation layer arranged on one side of the display panel, and a touch layer located on a side of the encapsulation layer away from the display panel; wherein, The display panel includes a display area and a frame area, the display area includes a bending area, and the frame area is located on one side of the bending area; The encapsulation layer comprises a first inorganic layer, and the orthographic projection of the first inorganic layer on the display panel covers at least a portion of the frame area; The touch layer comprises a first substrate and a first touch electrode layer which are sequentially stacked in a direction away from the encapsulation layer, and the orthographic projection of the first substrate on the display panel covers at least a portion of the frame area; The first substrate located in the border area covers the first inorganic layer, and the sidewall surfaces of the first inorganic layer and the first substrate located in the border area are on the same plane.
2. The display module according to claim 1, characterized in that: The touch layer further includes a second substrate and a second touch electrode layer sequentially stacked on one side of the first touch electrode layer in a direction away from the encapsulation layer, the orthographic projection of the second substrate on the display panel covers at least a portion of the frame area, and the second substrate located in the frame area covers the first substrate, wherein the sidewall surfaces of the first inorganic layer, the first substrate, and the second substrate located in the frame area are on the same plane; Preferably, the first inorganic layer, the first substrate and the second substrate are made of the same material.
3. The display module according to claim 1, characterized in that: The encapsulation layer further includes a second inorganic layer and an organic layer located between the first inorganic layer and the second inorganic layer; the orthographic projection of the second inorganic layer on the display panel covers at least a portion of the frame area; Preferably, the second inorganic layer is located on a side of the organic layer facing the display panel; Preferably, the first inorganic layer located in the border region covers the second inorganic layer, and the sidewall surfaces of the second inorganic layer and the first inorganic layer located in the border region are on the same plane; Preferably, the second inorganic layer and the first inorganic layer are made of the same material.
4. The display module according to claim 1, characterized in that: The thickness of the first inorganic layer is 0.4 μm to 1 μm; the thickness of the first substrate is 0.2 μm to 0.5 μm.
5. The display module according to claim 1, characterized in that: The first inorganic layer and the first substrate are an integrated structure; Preferably, the total thickness of the first inorganic layer and the first substrate is 0.4 μm to 1.5 μm.
6. The display module according to claim 1, characterized in that: The first inorganic layer and the first substrate are made of the same material; Preferably, the material of the first inorganic layer and the first substrate is at least one of silicon nitride and silicon oxide.
7. A method for manufacturing a display module, characterized in that: The steps include: A display panel is provided, wherein the display panel comprises a display area and a frame area, wherein the display area comprises a bending area, and the frame area is located on one side of the bending area; A first inorganic layer of an encapsulation layer and a first substrate of a touch layer are formed on the display panel, wherein the orthographic projections of the first inorganic layer and the first substrate on the display panel both cover at least a portion of the frame area, and the first substrate located in the frame area covers the first inorganic layer; forming a first touch electrode layer on the first substrate; as well as The first substrate and the first inorganic layer located in the frame area are simultaneously subjected to photolithography processing, so that the sidewall surfaces of the first substrate and the first inorganic layer located in the frame area are on the same plane.
8. The method for manufacturing a display module according to claim 7, characterized in that: The step of forming a first inorganic layer of an encapsulation layer and a first substrate of a touch layer on the display panel includes: Firstly forming a first inorganic layer of an encapsulation layer on the display panel, and then forming a first substrate of a touch layer on the first inorganic layer; or The first inorganic layer and the first substrate are simultaneously formed on the display panel by using a CVD process, and the first inorganic layer and the first substrate are an integrated structure.
9. The method for manufacturing a display module according to claim 7, characterized in that: Before forming the first inorganic layer of the encapsulation layer, the following steps are also included: forming a second inorganic layer of an encapsulation layer on the display panel; and forming an organic layer on a side of the second inorganic layer away from the display panel; Preferably, the step of performing photolithography processing includes: performing photolithography processing on the second inorganic layer, the first inorganic layer and the first substrate located in the frame area simultaneously, so that the sidewall surfaces of the second inorganic layer, the first inorganic layer and the first substrate located in the frame area are on the same plane; Preferably, before the photolithography process is performed, the method further includes the following steps: forming a second substrate on a side of the first touch electrode layer away from the first substrate; Preferably, the method further comprises the following steps: forming a second touch electrode layer on a side of the second substrate away from the first touch electrode layer; Preferably, the step of performing photolithography processing includes: simultaneously performing photolithography processing on the second substrate, the first substrate, the first inorganic layer and the second inorganic layer located in the border area, so that the side wall surfaces of the second substrate, the first substrate, the first inorganic layer and the second inorganic layer are all on the same plane.
10. An electronic device, characterized in that: A display module comprising any one of claims 1 to 6, or a display module prepared by the preparation method according to any one of claims 7 to 9.