New sanitary ceramic product research and development method
By using 3D software design and CNC equipment to produce plaster profiling products in the research and development of sanitary ceramic products, combined with functional testing and three-dimensional scanning optimization design, the problems of long research and development cycles and high testing costs in the existing technology have been solved, and a more complete solution has been achieved. Efficient product shaping and cost reduction.
Patent Information
- Application Number
- CN202410926659.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-11
- Publication Date
- 2024-10-18
AI Technical Summary
Existing sanitary ceramic products have long development cycles, high testing costs, and low efficiency.
Adopt a new sanitary ceramics product development method, including 3D software design, CNC equipment to produce plaster copy products, functional testing, modifications based on test results, 3D scanning optimization design, making experimental molds, small batch production and testing, until the product until qualified.
It greatly shortens the product finalization time, reduces the input of materials and equipment in the pilot stage, reduces costs, and facilitates structural adjustment through the flexibility of gypsum materials, improving the efficiency of product design.
Smart Images

Figure CN118789663A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of ceramic production, and in particular relates to a new sanitary ceramic product research and development method. Background Art
[0002] Ceramic companies need to constantly update their products, especially sanitary ceramic companies. In order to improve product competitiveness, they have been constantly creating improvements from appearance to function. The design of each new product will affect the functionality of the product accordingly. Therefore, new products must undergo functional testing before they can be finalized for production.
[0003] In the existing technology, it takes at least two months for new product development from design to determination of production model. The general process is: 1) product 3D design; 2) product prototype design based on 3D design; 3) CNC product prototype (gypsum product model) is made according to the product prototype; 4) product mold is reproduced; 5) product mold is dried and small-scale product test is carried out. Product small-scale test refers to the use of product molds to produce a part of products in small batches, including using product molds for grouting, drying, glazing and firing of product ceramic blanks after demolding, and then testing the product. If the test failure rate is high, it is necessary to return to the prototype design or mold reproduction process to find the problem, and conduct small-scale production tests again. Finally, after passing the small-scale test, the line mold is determined and the product is produced.
[0004] Since each small test is equivalent to a complete production process, it requires a large investment in material and equipment costs, and the cycle of each small test is very long, so the efficiency of determining the product master mold is extremely low, which makes the R&D design cycle longer. Summary of the invention
[0005] The technical problem to be solved by the present invention is the long R&D cycle, high testing cost and low efficiency of existing products.
[0006] The present invention solves the above-mentioned problem by adopting the following technical solution: A new sanitary ceramic product development method, comprising: S1: Product design, using 3D software to create three-dimensional product products; S2: Based on the finished three-dimensional product, make plaster imitation products through CNC equipment; S3: Apply waterproof coating on the surface of the gypsum profiling product, and then dry the gypsum profiling product; S4: Perform a functional test on the dried gypsum profiling product. If the functional test fails, proceed to the next step. If the functional test passes, skip the next step. S5: modifying the gypsum profiling product according to the functional defects shown by the test results, performing waterproof repair on the modified gypsum profiling product, and then performing step S4 again; S6: Perform three-dimensional scanning on the gypsum profiling products that have passed the test, input the scanning results into 3D software, modify the three-dimensional product to form a three-dimensional finalized product; S7: Use the three-dimensional finalized product to carry out product prototype design; S8: Make experimental molds based on product prototypes; S9: Use the experimental mold to carry out small batch grouting production to obtain the product experimental green body; S10: Drying, glazing and firing the product experimental green body to form a primary product; S11: Check the dimensions and deformation of the primary product. If it is qualified, the experimental mold will be used as the product master mold and the product will be officially finalized for production.
[0007] Compared with the prior art, the present invention adopting the above structure has the following beneficial effects: 1) The present invention greatly advances the time for functional testing, shortens the product's small-scale test and modification cycle, and can greatly speed up the product finalization time; 2) The present invention uses waterproof coating to enable gypsum profiling products to meet the conditions for functional testing, reduces the material and equipment investment in the small-scale test stage, and greatly reduces costs; 3) The present invention uses gypsum to make product profiling, and the gypsum material is relatively soft, so that structural modifications can be made, which is convenient for adjusting products that have problems found after testing.
[0008] As a preferred embodiment, a further technical solution of the above structure is: Preferably, the range of the surface of the gypsum profiling product brushed with waterproof coating is the surface of the product functional test.
[0009] Preferably, the waterproof coating is a material that forms a film with a smooth surface after drying.
[0010] Modifications to plaster profiling products include one or more of the following: 1) Polish the inner surface of the pot body partially and fill other parts with plaster to modify the curve shape of the pot body surface; 2) Grind the wall of the sewage pipe to increase the diameter of the sewage pipe; 3) Use gypsum to thicken the sewage pipe wall, thereby reducing the diameter of the sewage pipe; 4) Increase or decrease the size of the injection hole; 5) Grind or add on the outer edge of the baffle to adjust the height or width of the baffle; 6) Modify the curvature of the sewage pipe or waterway to adjust the water seal height; 7) Modify the number, size, angle and shape of the holes to adjust the flushing capacity of the product; 8) Modify the pipe shape, size, hole size, water flow direction and size to change the siphoning capacity of the product.
[0011] Preferably, the product prototype is obtained by adding shrinkage and pre-deformation to the three-dimensional final product to obtain the product prototype design, and the gypsum prototype is manufactured according to the product prototype design. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] Figure 1 It is a finished product picture of a three-dimensional product of the present invention; Figure 2 It is a schematic diagram of the gypsum profiling product of the present invention; Figure 3 It is a schematic diagram of the product prototype of the present invention; Figure 4 3D product finished product and product prototype of the present invention, the dotted line in the figure represents the product prototype, the solid line represents; 3D product finished product Figure 5 It is a schematic diagram of the experimental mold of the present invention; Figure 6 It is a schematic diagram of modifying the pot body of the gypsum profiling product according to the present invention; Figure 7 It is a schematic diagram of the present invention of grinding the wall of a sewage pipe of a gypsum profiling product to expand its diameter; Figure 8 It is a schematic diagram of the present invention for reducing the diameter of the sewage pipe wall thickened by the gypsum profiling product; Fig. 9 It is a schematic diagram of enlarging and modifying the ring hole of the gypsum profiling product according to the present invention; Fig.10 It is a schematic diagram of the present invention for enlarging and modifying the injection hole of the gypsum profiling product; Fig.11 It is a schematic diagram of modifying the curvature of a sewage pipe by using a gypsum profiling product according to the present invention; Fig.12 It is a production flow chart of the present invention.
[0013] In the figure: 1. pot body; 2. drain pipe; 3. ring hole; 4. injection hole; 5. baffle. DETAILED DESCRIPTION
[0014] The present invention will be further described below in conjunction with embodiments, the purpose of which is only to provide a better understanding of the content of the present invention. Therefore, the examples given do not limit the protection scope of the present invention.
[0015] The research and development of new products must first meet the functional requirements. After the breakthrough product design, functionality is often the most unstable factor. There are many factors that affect the functionality of the finished product, mainly the following: 1) New product design problems, including unreasonable design parameters and mismatched design parts. Usually, the functional unqualified products caused by this reason account for 80%-90%; 2) Inconsistent operation of workers, or failure to operate according to technical requirements, resulting in an unqualified inspection rate of 5%-10%; 3) Product deformation leads to functional instability, including product deformation during firing and molding, accounting for 5%-10%.
[0016] The product prototype (three-dimensional product finished product) is the starting point of new product research and development, and the test result is the end point. Since the existing technology requires a complete production process from the product design prototype to the testing of the product, when the test result is unqualified, it is necessary to find the problem in the entire production process to determine the cause. If it is a problem with the original design of the prototype, the design prototype should be modified and adjusted; if the prototype made according to the three-dimensional product finished product does not completely restore the design, the prototype needs to be remade; if there is an error in the mold making during the mold remodeling, or there are unchecked bumps and cracks during the drying of the original blank, or the firing process is unqualified, a new batch of test products must be produced again. Therefore, functional testing is the most time-consuming and resource-consuming work stage in the product development process.
[0017] Among the above factors that affect the product function test structure, the product design prototype is the source and also the factor with the highest frequency of problems. Therefore, if the correctness of the "source" can be determined first, the efficiency of product design finalization will inevitably be greatly improved.
[0018] The method for developing new sanitary ceramic products provided by the present invention comprises: S1: Product design, use 3D software to create three-dimensional product products, see Figure 1 .
[0019] S2: Based on the finished three-dimensional product, the CNC equipment is used to make plaster imitation products, see Figure 2 .
[0020] S3: Brush waterproof coating on the surface of the gypsum profiling product, and then dry the gypsum profiling product.
[0021] S4: Perform a functional test on the dried gypsum profiling product. If the functional test fails, proceed to the next step. If the functional test passes, skip the next step.
[0022] S5: According to the functional defects shown in the test results, the gypsum profiling product is modified, the modified gypsum profiling product is waterproofed, and then step S4 is performed again; for specific modifications, see Figure 6-Figure 11 .
[0023] S6: Perform three-dimensional scanning on the gypsum profiling products that have passed the test, input the scanning results into 3D software, modify the three-dimensional product to form a three-dimensional finalized product; S7: Using the three-dimensional finalized product, the product prototype is designed after setting the scale and pre-deformation. Figure 3 , Figure 4 .
[0024] S8: Design and manufacture experimental molds according to product prototypes. Figure 5 .
[0025] S9: Use the experimental mold to carry out small batch grouting production to obtain the product experimental green body.
[0026] S10: Drying, glazing and firing the product experimental green body to form a primary product.
[0027] S11: Check the dimensions and deformation of the primary product. If it is qualified, the experimental model will be used as the product master mold and the product will be officially finalized for production.
[0028] Preferably, the surface of the gypsum profiling product is painted with waterproof coating, which is a material that forms a smooth film after drying, such as shellac, polyurethane waterproof coating, acrylic waterproof coating, waterproof emulsion coating or silicone waterproof coating.
[0029] Functional test structure and inspection items comparison table: Test Type Inspection items Miso test The shape of the pot, the diameter and flow direction of the pipe, the size of the spray hole, the height of the baffle, the shape of the water tank, the water channel space and flow direction, the size of the sewage outlet, the height of the water seal and the size of the water seal area PP ball test The shape of the pot, the diameter and flow direction of the pipe, the size of the spray hole, the height of the baffle; the shape of the water tank, the water channel space and flow direction, the size and angle of the ring, the size of the sewage outlet, the height and size of the water seal Particle and pellet testing The shape of the pot, the diameter and flow direction of the pipe, the size of the spray hole, the height of the baffle; the shape of the water tank, the waterway space and flow direction, the size and angle of the ring, the size of the sewage outlet Splash Pot shape, product water outlet angle and size, water belt width and position, ring edge width, water seal height and size Sponge and paper The shape of the pot, the diameter and flow direction of the pipe, the size of the spray hole, the height of the baffle; the shape of the water tank, the waterway space and flow direction, the size and angle of the ring, the size of the sewage outlet Casing test Pot shape, pipe diameter and flow direction, water outlet angle and size, baffle height, water tank shape, waterway space and flow direction, eye size and angle, drain outlet size, water seal height and size Water seal area Pot shape, water seal height Water seal height Pipe size, pot shape, baffle height Inkblot test Water outlet angle and size Sawdust test Water outlet angle and size, waterway space and flow direction, water hose width and position, 18m pipeline transportation test The shape of the pot, the diameter and flow direction of the pipe, the size of the spray hole, the height of the baffle; the shape of the water tank, the water channel space and flow direction, the size and angle of the ring, the size of the sewage outlet, the height and size of the water seal Product paper test The shape of the pot, the diameter and flow direction of the pipe, the size of the spray hole, the height of the baffle; the shape of the water tank, the waterway space and flow direction, the size and angle of the ring, the size of the sewage outlet, the height and size of the water seal, Product replacement testing Water storage capacity, pot shape, water seal height and size, pipe diameter Pipe ball Pipe diameter Product water consumption Tank shape, water channel space and flow direction, pipe diameter and flow direction Product water level Water tank shape Follow-up water Pot shape, pipe diameter and flow direction Product flushing The number, size, angle of holes and the shape of the hose Products through newspapers Number, size, angle of holes, shape of pot Product siphoning capacity Pipe shape and size, hole size, waterway direction and size After the gypsum profiling products have gone through the above-mentioned test items, a test result report will be issued. Based on the unqualified items, the problems with the product prototype can be judged. Taking the production and development of toilets as an example, the modifications and adjustments to the product include but are not limited to the following situations: 1) If the sample sticks to the pot body 1 during the miso test and obvious water splashing occurs during the water splash test, the inner surface of the pot body 1 is partially polished and other parts are thickened with plaster to modify the inner surface curve shape, see Figure 6 .
[0030] 2) If the sample is discharged slowly or not completely during the taste increment test, or if there are small balls remaining in the pot body 1 during the PP ball test, particle and small ball test, grind the wall of the sewage pipe 2 to increase the diameter of the sewage pipe 2, see Figure 7 .
[0031] 3) If the toilet does not have enough suction on the test sample during the odor increment test, use plaster to thicken the wall of the sewage pipe 2 to reduce the diameter of the sewage pipe 2; see Figure 8 .
[0032] 4) If the PP ball test or the sponge plus paper test shows that the flushing water flow rate is too slow or the flushing water pressure is too high, increase or decrease the size of the spray hole 4, see Fig.10 .
[0033] 5) If the direction of the water spray and the width of the water flow are found to be not as expected during the casing test, water seal test and product paper-passing test, grind or add to the outer edge of the baffle 5 to adjust the height or width of the baffle 5, see Fig.11 .
[0034] 6) If there is residual medium in the casing test and the 18-meter pipeline transportation test, modify the curvature of the sewage pipe 2 or the waterway to enhance the flushing effect; see Fig.11 .
[0035] 7) Modify the number, size, angle and shape of the ring holes 3 to adjust the flushing capacity of the product, see Fig. 9 .
[0036] 8) Modify the pipe shape, size, hole size, water flow direction and size to change the siphoning capacity of the product.
[0037] Preferably, the product prototype design is based on the three-dimensional finalized product, and the shape is increased in shrinkage and pre-deformed according to the drying deformation rate of the grouting green body.
[0038] Experimental mold drying can be done by drying the moisture in the mold quickly, so as to quickly absorb moisture from the ceramic blank during production and accelerate the forming of the blank after grouting. The mold grouting is carried out on the production line to facilitate workers' operation.
[0039] The experimental mold is formed by grouting, the wet blank is dried, glazed and fired. The test refers to injecting mud into the mold to form a wet blank, which is then dried to form a dry blank. Glaze is sprayed and fired on the basis of the dry blank to form a ceramic product, and then the finished product is tested.
[0040] The product production master mold is actually made using the experimental mold that has passed all tests and is a production mold made for the convenience of mass production of products.
[0041] Compared with traditional development methods, the sanitary ceramic research and development method provided by the present invention puts product testing in advance. First, it avoids multiple product modifications due to unqualified functions during small-batch experiments, which prolongs the development time. Second, the finished product function test is carried out through product gypsum, which is more accurate and the results are faster than using software simulation analysis. Third, compared with 3D printing resin materials, gypsum materials are easier to modify quickly and know the functional results. Fourth, compared with modifying the model, the modification of the product gypsum finished product does not need to consider requirements such as the thickness of the product blank. The change is faster and more intuitive, and the data is more accurate, so that the research and judgment of the new product function can be completed quickly.
[0042] The above description is only a preferred feasible embodiment of the present invention, and does not limit the scope of rights of the present invention. All equivalent changes made using the contents of the present invention specification and its drawings are included in the scope of rights of the present invention.
Claims
1. A new sanitary ceramic product development method, comprising: S1: Product design, using 3D software to create three-dimensional product products; S2: Based on the finished three-dimensional product, make plaster imitation products through CNC equipment; Features: S3: Apply waterproof coating on the surface of the gypsum profiling product, and then dry the gypsum profiling product; S4: Perform a functional test on the dried gypsum profiling product. If the functional test fails, proceed to the next step. If the functional test passes, skip the next step. S5: modifying the gypsum profiling product according to the functional defects shown by the test results, waterproofing the modified gypsum profiling product, and then performing step S4 again; S6: Perform three-dimensional scanning on the gypsum profiling products that have passed the test, input the scanning results into 3D software, modify the three-dimensional product to form a three-dimensional finalized product; S7: Use the three-dimensional final product to design product prototypes; S8: Make experimental molds based on product prototypes; S9: Use the experimental mold to carry out small batch grouting production to obtain the product experimental green body; S10: Drying, glazing and firing the product experimental green body to form a primary product; S11: Check the dimensions and deformation of the primary product. If it is qualified, the experimental mold will be used as the product master mold and the product will be officially finalized for production.
2. The method for developing new sanitary ceramic products according to claim 1, characterized in that: The range of the waterproof coating on the surface of the gypsum profiling product is the surface for the functional test of the product.
3. The method for developing new sanitary ceramic products according to claim 1, characterized in that: Waterproof coatings are materials that form a smooth film after drying.
4. The method for developing new sanitary ceramic products according to claim 1, characterized in that: Modifications to plaster profiling products include one or more of the following: 1) Polish the inner surface of the pot body partially and fill other parts with plaster to modify the curve shape of the pot body surface; 2) Grind the wall of the sewage pipe to increase the diameter of the sewage pipe; 3) Use gypsum to thicken the sewage pipe wall, thereby reducing the diameter of the sewage pipe; 4) Increase or decrease the size of the injection hole; 5) Grind or add on the outer edge of the baffle to adjust the height or width of the baffle; 6) Modify the curvature of the sewage pipe or waterway to adjust the water seal height; 7) Modify the number, size, angle and shape of the holes to adjust the flushing capacity of the product; 8) Modify the pipe shape, size, hole size, water flow direction and size to change the siphoning capacity of the product.
5. The method for developing new sanitary ceramic products according to claim 1, characterized in that: The product prototype is a plaster prototype made by adding shrinkage and pre-deformation to the three-dimensional final product to obtain the product prototype design.